Aerosol generating device, preparation method thereof and aerosol generating system
By using a hollow device formed by a composite layer in the aerosol generating device, the smoke layer composed of loaded particles and adhesives solves the problem of high smoke temperature in heat-not-burn cigarettes, increases the amount of aerosol released, and improves consumption experience.
Patent Information
- Application Number
- CN202411124055.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-10-11
AI Technical Summary
In heat-not-burn cigarettes, the smoke temperature of the aerosol generating device is relatively high, which causes the smoke-generating body in the aerosol matrix to partially condense, reducing the smoke concentration and affecting the consumer experience.
The hollow device formed by the composite layer includes a base material and a smoke-generating layer located on the surface of the base material. The smoke-generating layer is composed of loaded particles and a binder. The loaded particles include a porous particle carrier and a smoke layer loaded on the porous particle carrier. The first smoke-generating agent is made of pipe fittings through a composite layer to reduce the leakage of the smoke-generating agent and increase the smoke concentration.
It reduces the flue gas temperature of the aerosol generating device, increases the amount of aerosol released, and improves the consumer experience.
Smart Images

Figure CN118749705A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of heat-not-burn cigarettes, and in particular to an aerosol generating device and a preparation method thereof, and an aerosol generating system. Background Art
[0002] As a new type of tobacco product, heat-not-burn cigarettes have a heating temperature of 200℃~400℃, which is lower than the combustion temperature of traditional cigarettes of 600℃~900℃. The harmful components produced by the high-temperature combustion of tobacco are greatly reduced. Therefore, it has developed rapidly in recent years.
[0003] In order to simulate the "smoking" effect of traditional cigarettes, it is necessary to add a smoke-generating body to the aerosol matrix of heat-not-burn cigarettes. In order to pursue a more intense smoking effect, a higher smoke-generating body content and a higher heating temperature are usually used. Heat-not-burn cigarettes are used in conjunction with heating devices for heating. When heated by heating devices, there are usually two ways: peripheral heating and center heating. The temperature of the central heating element is set at about 350°C, and the temperature of the circumferential heating element is set at about 250°C. The smoke-generating body and other substances in the aerosol matrix migrate into the smoke through physical changes such as evaporation and distillation at high temperatures. These high-temperature aerosols will reduce the consumer experience. In order to reduce the smoke temperature of heat-not-burn cigarettes, it is usually adopted to add a hollow tubular element after the aerosol matrix, so that the aerosol generated by heating can reduce the smoke temperature when it flows through the hollow tubular element. However, while the aerosol flows through the hollow tubular element to reduce the temperature, it will partially condense on the inner wall of the hollow tubular element, causing the cigarette smoke concentration to decrease, which will also reduce the consumer experience. Summary of the invention
[0004] Based on this, it is necessary to provide an aerosol generating device and a preparation method and an aerosol generating system that can reduce the smoke temperature of the aerosol generating device and increase the aerosol release amount.
[0005] The technical solution proposed in this application is as follows:
[0006] In a first aspect, the present application provides an aerosol generating device, comprising a filter body, a hollow device and an aerosol matrix connected in sequence; wherein the hollow device is formed by a composite layer, the composite layer comprises a substrate and a smoke-generating layer arranged on the inner surface of the substrate, the smoke-generating layer comprises loaded particles and an adhesive, the loaded particles comprise a porous particle carrier and a first smoke-generating agent loaded on the porous particle carrier.
[0007] The aerosol generating device of the present application includes a filter body, a hollow device and an aerosol matrix connected in sequence; the hollow device is formed by a composite layer, the composite layer includes a substrate and a smoke-generating layer arranged on the surface of the substrate, the smoke-generating layer includes loaded particles and an adhesive, the loaded particles include a porous particle carrier and a first smoke-generating agent loaded on the porous particle carrier. After the composite layer of the present application is made into a pipe, it is used in the aerosol generating device. On the one hand, the loaded particles adsorbed with the first smoke-generating agent are combined with the adhesive, which can reduce the content of the smoke-generating agent in the aerosol matrix accordingly, inhibit or reduce the yellow spot problem caused by the extravasation of the smoke-generating agent in the aerosol matrix smoke-generating material; on the other hand, the loaded particles can also adsorb the smoke generated by the aerosol matrix during the suction process, and cooperate with the first smoke-generating agent to be attached to the composite layer, so that the aerosol generated by high temperature can flow through the hollow device to reduce the temperature while increasing the smoke concentration of the aerosol generating device during the suction process.
[0008] In some of the embodiments, one end of the hollow device abuts against the aerosol matrix, and the other end abuts against or is close to the filter.
[0009] In some of the embodiments, based on the total mass of the supported particles, the mass of the first smoke agent accounts for 10% to 65%, and the mass of the porous particle carrier accounts for 35% to 90%.
[0010] In some embodiments, the loaded particles further include a flavoring agent loaded on the porous particle carrier. Based on the total mass of the loaded particles, the mass of the first smoke agent accounts for 10% to 60%, the mass of the porous particle carrier accounts for 35% to 80%, and the mass of the flavoring agent accounts for 0.1% to 10%.
[0011] In some embodiments, the mass ratio of the binder to the total mass of the supported particulate matter is (0.5-10):1.
[0012] In some embodiments, the supported particles satisfy at least one of the conditions (1) to (5):
[0013] (1) The porous particle carrier comprises at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon, molecular sieves and gel particles;
[0014] (2) the first smoke generating agent comprises at least one of glycerol, propylene glycol, ethylene glycol, dipropylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, oleyl alcohol, xylitol and erythritol;
[0015] (3) The flavoring agent includes at least one of a mint flavoring agent, a blueberry flavoring agent, a cantaloupe flavoring agent, an orange flavoring agent, a coffee flavoring agent, and a tea flavoring agent;
[0016] (4) The adhesive comprises at least one of gum, cellulose adhesive, polysaccharide, organic acid and conjugate alkali salt of organic acid.
[0017] In some embodiments, the aerosol matrix includes a second smoking agent, and the second smoking agent includes glycerin; and / or
[0018] The particle size of the porous particle carrier is 20 mesh to 200 mesh.
[0019] In some embodiments, the composite layer further includes an anti-permeation layer, which is disposed on a surface of the substrate facing away from the smoke-generating layer; relative to the substrate, the anti-permeation layer is located on the outside of the hollow device.
[0020] In some of the embodiments, the aerosol generating device further comprises a wrapping layer, wherein the wrapping layer wraps the outer surface of the filter body, the hollow device and the aerosol matrix which are connected in sequence.
[0021] In a second aspect, the present application provides a method for preparing an aerosol generating device, comprising the following steps:
[0022] The smoke-generating layer is formed on the surface of the substrate to obtain the composite layer; the smoke-generating layer comprises supported particles and a binder, and the supported particles comprise a porous particle carrier and a first smoke-generating agent supported on the porous particle carrier;
[0023] Rolling the composite layer to form the hollow device;
[0024] The filter body, the hollow device and the aerosol matrix are connected in sequence to obtain an aerosol generating device.
[0025] In some embodiments, the coating amount of the smoke-generating layer is 5 g / m 2 ~60g / m 2 .
[0026] In a third aspect, the present application provides an aerosol generating system, comprising the above-mentioned aerosol generating device and a heating device.
[0027] In some embodiments, the heating device includes a heating component, a battery component, a control component and a housing, the battery component is a battery component for powering the heating device, the control component is used to control the battery component, and the housing is used to accommodate the heating component, the battery component and the control component. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 This is a schematic diagram of an aerosol generating device according to one embodiment of the present application;
[0029] Figure 2 This is a schematic diagram of an aerosol generating device according to another embodiment of the present application;
[0030] Figure 3 This is a schematic diagram of the cross-sectional structure of a hollow device according to one embodiment of the present application;
[0031] Figure 4 This is a schematic diagram of the cross-sectional structure of a hollow device according to another embodiment of the present application;
[0032] Figure 5 This is a schematic diagram of the cross-sectional structure of a hollow device according to another embodiment of the present application.
[0033] Description of reference numerals:
[0034] 10. Aerosol generating device; 100. Aerosol matrix; 200. Hollow device; 300. Filter body; 400. Wrapping layer; 210. Composite layer; 211. Smoke-generating layer; 212. Base material; 213. Anti-permeation layer; 213A. Anti-permeation material layer; 213B. First paper layer; 214. Second paper layer. DETAILED DESCRIPTION
[0035] In order to make the above-mentioned purposes, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present application. However, the present application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present application, so the present application is not limited by the specific embodiments disclosed below.
[0036] In the description of the present application, it should be understood that if the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc. appear, the orientation or position relationship indicated by these terms is based on the orientation or position relationship shown in the accompanying drawings, which is only for the convenience of describing the present application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application.
[0037] In addition, if the terms "first" or "second" appear, these terms are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of this application, if the term "plurality" appears, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0038] In this application, unless otherwise clearly specified and limited, if the terms "installed", "connected", "connected", "fixed" and the like appear, these terms should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integrated connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to the specific circumstances.
[0039] In the present application, unless otherwise clearly specified and limited, if there is a description that a first feature is "above" or "below" a second feature, etc., or similar descriptions appear, it may mean that the first and second features are in direct contact, or that the first and second features are in indirect contact through an intermediate medium. Moreover, the first feature being "above", "above" and "above" the second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. The first feature being "below", "below" and "below" the second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0040] It should be noted that if an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be a central element. If an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. If any, the terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used in this application are for illustrative purposes only and do not represent the only implementation method.
[0041] Except as shown in the operating examples or otherwise indicated, all numbers used in the specification and claims to indicate the amount of ingredients, physicochemical properties, etc. are understood to be adjusted by the term "about" in all cases. For example, therefore, unless otherwise indicated, the numerical parameters listed in the above specification and the attached claims are approximate values, and those skilled in the art can use the teachings disclosed herein to seek to obtain the desired properties and appropriately change these approximate values. The use of numerical ranges expressed as endpoints includes all numbers within the range and any range within the range, for example, 1 to 5 includes 1, 1.1, 1.3, 1.5, 2, 2.75, 3, 3.80, 4 and 5, etc.
[0042] See also Figure 1 and Figure 2 In one embodiment of the present application, an aerosol generating device 10 is provided, comprising a filter body 300, a hollow device 200 and an aerosol matrix 100 which are connected in sequence.
[0043] See also Figure 3 The hollow device is formed by a composite layer 210, the composite layer 210 includes a substrate 212 and a smoke-generating layer 211 disposed on the inner surface of the substrate 212, the smoke-generating layer 211 includes supported particles and an adhesive, the supported particles include a porous particle carrier and a first smoke-generating agent supported on the porous particle carrier, and the adhesive is used to bond the supported particles to form the smoke-generating layer 211. That is, with respect to the substrate 212, the smoke-generating layer 211 is located on the inner side of the hollow device 200.
[0044] The aerosol generating device 10 of the present application comprises a filter body 300, a hollow device 200 and an aerosol substrate 100 connected in sequence; the hollow device 200 comprises a composite layer 210, the composite layer 210 comprises a substrate 212 and supported particles and an adhesive arranged on the surface of the substrate 212, the supported particles comprising a porous particle carrier and a first smoke generating agent supported on the porous particle carrier, after the composite layer 210 of the present application is made into a hollow device 200, it is used in the aerosol generating device 10, on the one hand, the first smoke generating agent adsorbed on the composite layer 210 is adsorbed on the composite layer 210, and the first smoke generating agent is adsorbed on the composite layer 210. The combination of loaded particles and adhesive can reduce the content of smoke agent in the aerosol matrix 100 accordingly, inhibit or reduce the yellow spot problem caused by the extravasation of smoke agent in the aerosol matrix smoke material. On the other hand, the loaded particles can also adsorb the smoke generated by the aerosol matrix 100 during the smoking process, and cooperate with the first smoke agent to be attached to the composite layer 210, so that the aerosol generated by high temperature can flow through the hollow device 200 to reduce the temperature, while increasing the smoke concentration of the aerosol generating device during the smoking process, thereby increasing the aerosol release amount.
[0045] In some of these examples, see Figure 4The composite layer 210 further includes an anti-permeation layer 213 , which is disposed on a surface of the substrate 212 facing away from the smoke-generating layer 211 . For the substrate 212 , the anti-permeation layer 213 is located on the outside of the hollow device 200 .
[0046] Furthermore, the anti-permeability layer 213 includes a first paper layer 213B and an anti-permeability material layer 213A; the anti-permeability material layer 213A is disposed on the first paper layer 213B, and the components of the anti-permeability material layer 213A include any one of silicone oil and metal.
[0047] Furthermore, the anti-permeability material layer 213A is located between the first paper layer 213B and the substrate 212 .
[0048] It can be understood that, on the one hand, the above-mentioned anti-permeability layer 213 can inhibit or reduce the yellow spot problem caused by the extravasation of the first smoke agent or flavoring agent in the composite layer 210. On the other hand, since the composite layer 210 contains the first smoke agent or flavoring agent, as the hollow device 200 continues to be heated, the first smoke agent or flavoring agent in the composite layer 210 is further released, and the above-mentioned anti-permeability layer 213 can play a role in preserving the fragrance.
[0049] In some embodiments, the anti-permeability layer 213 and the composite layer 210 are connected by an adhesive.
[0050] In some embodiments, the type of binder includes carboxymethyl cellulose.
[0051] See also Figure 5 , Figure 5 The composite layer 210 further includes a second paper layer 214 . Furthermore, the second paper layer 214 is located between the anti-permeability material layer 213 and the substrate 212 .
[0052] In some of the embodiments, one end of the hollow device 200 abuts against the aerosol matrix 100 , and the other end abuts against or is close to the filter 300 .
[0053] It can be understood that one of the benefits of the above-mentioned hollow device abutting the above-mentioned aerosol matrix is that the temperature of the aerosol matrix segment is higher during inhalation. According to the heat conduction effect, the temperature close to the aerosol matrix segment is also higher, which is beneficial for the hollow segment containing the first smoke agent particles to release the smoke aerosol when heated, thereby improving consumer experience; another benefit is that, similarly, the hollow segment containing the first smoke agent particles to release the smoke aerosol when heated will absorb heat and reduce the temperature of the smoke aerosol, thereby also improving consumer experience; the benefit of the above-mentioned hollow device abutting the above-mentioned filter body is: usually this cigarette structure is adopted, the structure is simple, if there are other components in the middle, the other components will adsorb the smoke aerosol and thus reduce the amount of smoke aerosol, resulting in a worse consumer experience.
[0054] In some of the embodiments, based on the total mass of the supported particles, the mass of the first smoke agent accounts for 10% to 65%, and the mass of the porous particle carrier accounts for 35% to 90%.
[0055] In some embodiments, based on the total mass of the supported particles, the mass of the first smoke agent accounts for 20% to 60%, and the mass of the porous particle carrier accounts for 40% to 80%.
[0056] In some of the embodiments, based on the total mass of the supported particles, the mass of the first smoke agent accounts for 30% to 55%, and the mass of the porous particle carrier accounts for 45% to 70%.
[0057] In some embodiments, the loaded particles further include a flavoring agent loaded on the porous particle carrier. Based on the total mass of the loaded particles, the mass of the first smoke agent accounts for 10% to 60%, the mass of the porous particle carrier accounts for 35% to 80%, and the mass of the flavoring agent accounts for 0.1% to 10%.
[0058] In some embodiments, the mass ratio of the binder to the total mass of the supported particulate matter is (0.05-0.1):1.
[0059] In some embodiments, the mass ratio of the binder to the total mass of the supported particulate matter is (0.01-0.08):1.
[0060] In some embodiments, the mass ratio of the binder to the total mass of the supported particulate matter is (0.02-0.05):1.
[0061] Further controlling the ratio of the components of the smoke-generating layer 211 can reduce the smoke temperature of the aerosol generating device 10 and increase the aerosol release amount, thereby achieving a better effect.
[0062] In some of the embodiments, the porous particle carrier includes at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon, molecular sieves and gel particles.
[0063] Optionally, the above-mentioned natural porous mineral material includes at least one of diatomaceous earth, montmorillonite, sepiolite and kaolin.
[0064] Optionally, the metal oxide includes at least one of calcium oxide, calcium carbonate, calcium hydroxide and calcium sulfate.
[0065] Preferably, the porous particle carrier is diatomaceous earth or gel particles.
[0066] In some embodiments, the first smoke generating agent includes at least one of glycerin, propylene glycol, ethylene glycol, dipropylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, oleyl alcohol, xylitol and erythritol.
[0067] In some embodiments, the flavoring agent includes at least one of mint flavoring, blueberry flavoring, cantaloupe flavoring, and orange flavoring.
[0068] In some embodiments, the type of the above-mentioned binder includes at least one of gum, cellulose binder, polysaccharide, organic acid and conjugate alkali salt of organic acid.
[0069] Optionally, the gum includes at least one of guar gum, xanthan gum, gum arabic and locust bean gum.
[0070] Optionally, the cellulose binder includes at least one of hydroxypropyl cellulose, carboxymethyl cellulose, hydroxyethyl cellulose, methyl cellulose and ethyl cellulose.
[0071] Optionally, the polysaccharide comprises starch.
[0072] Optionally, the organic acid includes alginic acid.
[0073] Optionally, the conjugate salt of the organic acid includes at least one of sodium alginate, agar and pectin.
[0074] Preferably, the above-mentioned binder comprises carboxymethyl cellulose.
[0075] In some embodiments, the substrate 212 includes paper.
[0076] In some embodiments, the porous particle carrier has a particle size of 20 mesh to 200 mesh, for example, 20 mesh, 25 mesh, 30 mesh, 35 mesh, 40 mesh, 45 mesh, 50 mesh, 60 mesh, 80 mesh, 100 mesh, 120 mesh, 150 mesh, 170 mesh, or 200 mesh.
[0077] Optionally, the particle size of the porous particle carrier is 40 mesh to 100 mesh; further optionally, the particle size of the porous particle carrier is 60 mesh to 80 mesh.
[0078] It is understandable that the particle size of the porous particle carrier is controlled within the above-mentioned specific range, wherein if the particle size is too large, it is easy to fall off after coating or during processing; if the particle size is too small, the coating is relatively dense, which is not conducive to the thermal release of the first smoke agent.
[0079] In some of the embodiments, the aerosol generating device 10 further includes a wrapping layer 400 , and the wrapping layer 400 wraps the outer surface of the filter body 300 , the hollow device 200 , and the aerosol matrix 100 which are sequentially connected.
[0080] In a specific example, the material of the wrapping layer 400 includes paper.
[0081] In some embodiments, the anti-permeation layer 213 is located between the wrapping layer 400 and the composite layer 210 .
[0082] Heat-not-burn cigarettes are used as an example of the aerosol generating device 10. In one example, the aerosol generating device 10 can be a heat-not-burn cigarette, but is not limited thereto.
[0083] The present application also provides a method for preparing the above-mentioned aerosol generating device 10, comprising steps S10 to S30.
[0084] Step S10: forming the above-mentioned smoke-generating layer 211 on the surface of the substrate 212 to obtain the composite layer 210; the smoke-generating layer 211 includes supported particles and a binder, and the supported particles include a porous particle carrier and a first smoke-generating agent supported on the above-mentioned porous particle carrier.
[0085] Specifically, the above steps of preparing the composite layer include steps S11 to S14.
[0086] Step S11: performing a first mixing process on the first smoke generating agent and the flavor enhancer to prepare a first mixture.
[0087] Step S12: performing a second mixing treatment on the first mixture and the porous particle carrier to prepare a second mixture.
[0088] Step S13: performing a third mixing process on the second mixture and the adhesive to prepare a smoke-generating slurry.
[0089] In some of the embodiments, the above-mentioned adhesive is used to bond the loaded particles to form the smoke-generating layer 211 .
[0090] The types and proportions of the porous particle carrier, the first smoke generating agent, the flavoring agent and the adhesive have been described in detail above and will not be repeated here.
[0091] Step S14: The smoke-generating slurry is loaded onto the substrate 212 and dried to prepare the composite layer 210 .
[0092] Optionally, the step of loading the smoke slurry onto the substrate 212 includes a step of coating treatment.
[0093] In some embodiments, the coating amount of the smoke-generating layer 211 is 5 g / m 2 ~60g / m 2 For example, it can be 5 g / m 2 , 10 g / m 2 , 15 g / m 2 , 20 g / m2 , 25 g / m 2 , 30 g / m 2 , 35 g / m 2 , 40 g / m 2 , 45 g / m 2 , 50 g / m 2 , 55 g / m 2 , 60 g / m 2 .
[0094] Optionally, the coating amount of the smoke-generating layer 211 is 10 g / ㎡~50 g / ㎡; further optionally, the coating amount of the supported particles and the adhesive is 20 g / ㎡~30 g / ㎡.
[0095] It is understandable that the coating amount of the smoke-generating layer 211 is controlled within the above-mentioned specific range. If the coating amount is too small, the first smoke agent contained is relatively small and the effect is not obvious; if the coating amount is too large, the processing difficulty increases, and the utilization rate of the first smoke agent contained therein is not high, which is not economical.
[0096] In some embodiments, the composite layer 210 further includes an anti-permeation layer 213 , and the anti-permeation layer 213 is disposed on a surface of the substrate 212 facing away from the smoke-generating layer 211 .
[0097] In some embodiments, step S10 of the preparation method further includes the following step: forming the anti-permeability layer 213 on the surface of the substrate 212 facing away from the smoke-generating layer 211 .
[0098] Furthermore, the anti-permeation layer 213 includes a first paper layer 213B and an anti-permeation material layer 213A. The anti-permeation material layer 213A is disposed on the first paper layer 213B. The anti-permeation material layer 213 includes any one of silicone oil and metal.
[0099] In some embodiments, the anti-permeability layer 213 may be a paper layer.
[0100] In some embodiments, the anti-permeability layer 213 may be one layer or two layers.
[0101] In a specific example, the composite layer 210 further includes a second paper layer 214 , and the second paper layer 214 is located between the anti-permeability material layer 213 and the substrate 212 .
[0102] Step S20 : rolling the composite layer 210 to form a hollow device 200 .
[0103] Step S30 : connecting the filter 300 , the hollow device 200 , and the aerosol matrix 100 in sequence to prepare the aerosol generating device 10 .
[0104] The aerosol generating device 10 prepared by the above preparation method can reduce the smoke temperature of the aerosol generating device and increase the aerosol release amount.
[0105] One embodiment of the present application also provides an aerosol generating system, comprising the above-mentioned aerosol generating device and a heating device.
[0106] In some of the embodiments, the heating device includes a heating component, a battery component for powering the heating device, a control component for controlling the battery component, and a housing for accommodating the heating component, the battery component, and the control component.
[0107] The present application does not impose any particular limitation on the heating component, battery component, control component and housing, and they may be selected from materials and shapes commonly used in the art.
[0108] The aerosol generating system of the present application has the characteristics of being able to reduce the smoke temperature of the aerosol generating device and increase the aerosol release amount.
[0109] The following is a detailed description in conjunction with specific examples. The following examples do not include other components except for inevitable impurities unless otherwise specified. The reagents and instruments used in the examples are conventionally selected in the art unless otherwise specified. The experimental methods for which specific conditions are not specified in the examples are implemented according to conventional conditions, such as the conditions described in the literature, books, or methods recommended by the manufacturer.
[0110] Example 1
[0111] 1. Preparation of hollow devices
[0112] (1) Preparing a smoking slurry. A glycerol mixture including glycerol, ethylene glycol and mint flavoring agent is mixed with activated carbon (average diameter is less than or equal to 0.075 mm, i.e., less than 200 mesh) to obtain fully wetted particles, and then a carboxymethyl cellulose aqueous solution is used to prepare a slurry to obtain a smoking slurry. Based on the total mass of the loaded particles, the mass proportions of glycerol, ethylene glycol and mint flavoring agent are 30%, 5% and 2.5% respectively, the mass proportion of activated carbon is 62.5%, and the mass ratio of carboxymethyl cellulose to the total mass of the loaded particles is 0.02.
[0113] (2) The smoke-generating slurry is quantitatively coated on one side of the substrate paper and dried. The coating weight after drying is 30 g / ㎡, and a smoke-generating layer is formed on one side of the substrate paper.
[0114] (3) Providing an anti-permeation layer. The anti-permeation layer includes a first paper layer and an anti-permeation material layer disposed on a surface of the first paper layer, wherein the anti-permeation material layer is a silicone oil layer.
[0115] (4) The inner paper layer having the smoke-generating layer is connected to the silicone oil layer side of the anti-permeation layer by polyacrylic acid to form a composite layer.
[0116] (5) The composite layer is wound with the anti-permeation layer on the outside to form a hollow device.
[0117] 2. Preparation of heat-not-burn cigarettes
[0118] The filter body, the above-mentioned hollow device and the aerosol matrix are connected in order, wrapped with paper on the outside, and assembled into a heat-not-burn cigarette, wherein one end of the hollow device abuts the aerosol matrix, and the other end abuts the filter body.
[0119] Example 2
[0120] 1. Preparation of hollow devices
[0121] (1) Preparing a smoke-generating slurry. A glycerol mixture including glycerol and propylene glycol is mixed with activated carbon (average diameter is less than or equal to 0.075 mm, i.e., less than 200 mesh) to obtain fully wetted and balanced loaded particles, and then a carboxymethyl cellulose aqueous solution is used to prepare a slurry to obtain a smoke-generating slurry. Based on the total mass of the loaded particles, the mass proportions of glycerol and propylene glycol are 40% and 5% respectively, the mass proportion of activated carbon is 55%, and the mass ratio of carboxymethyl cellulose to the total mass of the loaded particles is 0.02.
[0122] (2) The smoke-generating slurry is quantitatively coated on one side of the substrate paper and dried. The coating weight after drying is 45.5 g / ㎡, and a smoke-generating layer is formed on one side of the substrate paper.
[0123] (3) Providing an anti-permeation layer. The anti-permeation layer includes a first paper layer and an anti-permeation material layer disposed on a surface of the first paper layer, wherein the anti-permeation material layer is a silicone oil layer.
[0124] (4) Providing a second paper layer. The second paper layer is located between the anti-permeation material layer and the substrate.
[0125] (4) The inner paper layer with the smoke-generating layer is bonded to one side of the second paper layer by polyacrylic acid, and the other side of the second paper layer is bonded to one side of the silicone oil layer of the anti-permeation layer by polyacrylic acid to form a composite layer.
[0126] (5) The composite layer is wound with the anti-permeation layer on the outside to form a hollow device.
[0127] 2. Preparation of heat-not-burn cigarettes
[0128] The filter body, the above-mentioned hollow device and the aerosol matrix are connected in order, wrapped with paper on the outside, and assembled into a heat-not-burn cigarette, wherein one end of the hollow device abuts the aerosol matrix, and the other end abuts the filter body.
[0129] Embodiments 3 to 17
[0130] The preparation methods of the heat-not-burn cigarettes in Examples 3 to 17 are basically the same as those in Example 1, and the only difference is the relevant parameters in Tables 1 and 2, wherein the specific parameters and the mixed slurry ratios are shown in Tables 1 and 2 below.
[0131] The other steps and conditions are the same as those in Example 1.
[0132] Embodiment 18
[0133] The preparation method of the heat-not-burn cigarette in Example 18 is basically the same as that in Example 1, except that:
[0134] 1. Preparation of hollow devices
[0135] (1) Preparation of smoke-generating slurry. Glycerol and activated carbon (average diameter less than or equal to 0.075 mm, i.e., less than 200 mesh) are mixed and fully wetted to prepare loaded particles, and then the loaded particles are prepared into a slurry with an aqueous solution of carboxymethyl cellulose to obtain a smoke-generating slurry. Based on the total mass of the loaded particles, the mass of glycerol accounts for 60%, the mass of activated carbon accounts for 40%, and the mass ratio of carboxymethyl cellulose to the total mass of the loaded particles is 0.02.
[0136] (2) The smoke-generating slurry is quantitatively coated on one side of the substrate paper, that is, half of it is coated near the aerosol matrix position, and then dried. The coating weight after drying is 60 g / ㎡, and a smoke-generating layer is formed on one side of the substrate paper.
[0137] (3) Providing an anti-permeation layer. The anti-permeation layer includes a first paper layer and an anti-permeation material layer disposed on a surface of the first paper layer, wherein the anti-permeation material layer is a silicone oil layer.
[0138] (4) The inner paper layer having the smoke-generating layer is connected to the silicone oil layer side of the anti-permeation layer by polyacrylic acid to form a composite layer.
[0139] (5) The composite layer is wound with the anti-permeation layer on the outside to form a hollow device.
[0140] 2. Preparation of heat-not-burn cigarettes
[0141] The filter body, the above-mentioned hollow device and the aerosol matrix are connected in sequence, wrapped with paper on the outside, and assembled into a heat-not-burn cigarette, wherein one end of the hollow device abuts the aerosol matrix and the other end is close to the filter body.
[0142] Comparative Example 1~2
[0143] The preparation methods of the heat-not-burn cigarettes in Comparative Examples 1-2 are basically the same as those in Example 1, and the only difference is: the relevant parameters in Tables 1-2, wherein the specific parameters and the mixed slurry ratios are shown in Tables 1-2 below.
[0144] The other steps and conditions are the same as those in Example 1.
[0145] test:
[0146] The heat-not-burn cigarettes prepared in the above-mentioned Examples 1 to 14 and Comparative Examples 1 to 2 were smoked using a linear smoking machine, using an ambient heating method, with the heating temperature set at 220° C. The smoking parameters of the cigarettes were as follows:
[0147] Puffing capacity: 55mL; Puffing time: 2s; Puffing interval: 30s; Number of puffs: 8 times; Preheating time: 18s; Puffing curve: bell-shaped.
[0148] After 8 puffs using the electronic cigarette device, the GC-TCD method was used. Specifically, Wang Kang, Liu Jun, Xiao Shaohong, et al. GC-TCD method simultaneously detects the moisture content of heat-not-burn cigarette aerosol, and the release of nicotine, glycerol, 1,2-propylene glycol, triacetin and menthol [J]. Tobacco Science and Technology, 2019, 52 (3): 63-68. The glycerol content released was tested; and the temperature of the smoke aerosol after the third puff was measured. The results are shown in Tables 1 and 2.
[0149] Table 1
[0150]
[0151] Table 2
[0152]
[0153] The smoke temperature and glycerol release rate of the third puff of the heat-not-burn cigarette in Examples 1 to 19 and Comparative Examples 1 to 2 are shown in Tables 1 and 2. It can be seen that when the total amount of glycerol is the same, the glycerol release rate of the heat-not-burn cigarette prepared by the technical solution of the present application is significantly improved; when the total amount of glycerol is the same as or slightly lower than that of the comparative example, the glycerol release of the heat-not-burn cigarette prepared by the technical solution of the present application is higher than that of the comparative example; the smoke temperature of the heat-not-burn cigarette prepared by the technical solution of the present application is lower than that of the comparative example. Among them, Examples 18 and 19 are partially coated, that is, half of the coating is close to the aerosol matrix position. The advantage is that, compared with Example 16, the partial coating close to the aerosol matrix position has a high thermal utilization rate, so when the total amount of glycerol is the same, the glycerol release amount and release efficiency are higher. This method has a high preparation process difficulty.
[0154] Compared with the heat-not-burn cigarettes prepared in the comparative example, the heat-not-burn cigarettes prepared in the present application have lower aerosol substrate usage, lower smoke temperature, and higher aerosol release.
[0155] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0156] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be construed as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent application shall be subject to the attached claims.
Claims
1. An aerosol generating device, characterized in that: It comprises a filter body, a hollow device and an aerosol matrix connected in sequence; wherein the hollow device is formed by a composite layer, the composite layer comprises a substrate and a smoke-generating layer arranged on the inner surface of the substrate, the smoke-generating layer comprises loaded particles and an adhesive, and the loaded particles comprise a porous particle carrier and a first smoke-generating agent loaded on the porous particle carrier.
2. The aerosol generating device according to claim 1, characterized in that: One end of the hollow device abuts against the aerosol matrix, and the other end abuts against or is close to the filter body.
3. The aerosol generating device according to claim 1, characterized in that: Based on the total mass of the supported particles, the mass of the first smoke agent accounts for 10% to 65%, and the mass of the porous particle carrier accounts for 35% to 90%.
4. The aerosol generating device according to claim 3, characterized in that: The loaded particles also include a flavoring agent loaded on the porous particle carrier. Based on the total mass of the loaded particles, the mass of the first smoke agent accounts for 10% to 60%, the mass of the porous particle carrier accounts for 35% to 80%, and the mass of the flavoring agent accounts for 0.1% to 10%.
5. The aerosol generating device according to claim 3, characterized in that: The mass ratio of the binder to the total mass of the supported particulate matter is (0.05-0.1):
1.
6. The aerosol generating device according to claim 5, characterized in that: The supported particles satisfy at least one of the conditions (1) to (5): (1) The porous particle carrier comprises at least one of natural porous mineral materials, metal oxides, hydroxides, carbonates, sulfates, activated carbon, molecular sieves and gel particles; (2) the first smoke generating agent comprises at least one of glycerol, propylene glycol, ethylene glycol, dipropylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, oleyl alcohol, xylitol and erythritol; (3) The flavoring agent includes at least one of a mint flavoring agent, a blueberry flavoring agent, a cantaloupe flavoring agent, an orange flavoring agent, a coffee flavoring agent, and a tea flavoring agent; (4) The adhesive comprises at least one of gum, cellulose adhesive, polysaccharide, organic acid and conjugate alkali salt of organic acid.
7. The aerosol generating device according to any one of claims 1 to 6, characterized in that: The aerosol matrix includes a second smoking agent, and the second smoking agent includes glycerol; and / or The particle size of the porous particle carrier is 20 mesh to 200 mesh.
8. The aerosol generating device according to any one of claims 1 to 6, characterized in that: The composite layer further comprises an anti-permeation layer, which is arranged on the surface of the substrate facing away from the smoke-generating layer; relative to the substrate, the anti-permeation layer is located on the outside of the hollow device.
9. The aerosol generating device according to claim 8, characterized in that: The aerosol generating device further comprises a wrapping layer, and the wrapping layer wraps the outer surfaces of the filter body, the hollow device and the aerosol matrix which are connected in sequence.
10. The method for preparing an aerosol generating device according to any one of claims 1 to 9, characterized in that: The steps include: The smoke-generating layer is formed on the surface of the substrate to obtain the composite layer; the smoke-generating layer comprises supported particles and a binder, and the supported particles comprise a porous particle carrier and a first smoke-generating agent supported on the porous particle carrier; Rolling the composite layer to form the hollow device; The filter body, the hollow device and the aerosol matrix are connected in sequence to obtain an aerosol generating device.
11. The method for preparing an aerosol generating device according to claim 10, characterized in that: The coating amount of the smoke-generating layer is 5 g / m 2 ~60g / m 2 .
12. An aerosol generating system, characterized in that: It comprises the aerosol generating device and heating device as described in any one of claims 1 to 8.
13. The aerosol generating system according to claim 12, characterized in that: The heating device includes a heating component, a battery component, a control component and a shell, the battery component is used to supply power to the heating device, the control component is used to control the battery component, and the shell is used to accommodate the heating component, the battery component and the control component.
Citation Information
Patent Citations
Paper filter material provided with active adsorption layer
CN102987560A
Heated non-burning herbaceous plant smoke bomb and assembling method thereof
CN110141007A
Perfuming particle for electronic cigarette, and preparation method and application thereof
CN112159719A
Heating non-combustion fuming particle mixture capable of avoiding caking
CN112806603A
Fuming section based on multi-particle fuming, cigarette comprising same and preparation method
CN113331469A