A precast bridge material and its preparation method
By using modified bamboo fiber mixed with fly ash as an admixture and in conjunction with specific additives, precast bridge materials were prepared, which solved the problem of decreased material durability, improved the mechanical properties and corrosion resistance of the materials, and extended their service life.
Patent Information
- Application Number
- CN202411031410.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-07-30
AI Technical Summary
Precast bridge materials are susceptible to environmental erosion and load effects during use, leading to decreased durability and affecting the safety and service life of the bridge.
Modified bamboo fiber and fly ash are mixed in a specific ratio as admixtures, and a specific type of additive is used to prepare precast bridge materials, which improves the interfacial adhesion between fibers and other materials and enhances the mechanical properties of the materials.
This improved the mechanical properties and acid and alkali corrosion resistance of precast bridge materials, extending their durability and service life.
Smart Images

Figure BDA0004970019980000041 
Figure BDA0004970019980000061 
Figure BDA0004970019980000071
Abstract
Description
Technical Field
[0001] This application relates to the technical field of concrete, specifically to a precast bridge material and its preparation method. Background Technology
[0002] Precast bridge materials typically refer to the materials used in bridge components that are pre-produced, processed, and cured to a certain strength in a factory or prefabrication site. Once these components reach the required design strength, they are transported to the construction site for installation to build the complete bridge structure. The selection of precast bridge materials has a significant impact on the quality, durability, safety, and construction efficiency of bridges.
[0003] In summary, the selection of precast bridge materials should be based on a comprehensive consideration of specific engineering needs, geographical environment, and usage conditions to ensure the safety and economy of the bridge structure.
[0004] Currently, the main problem with precast bridge materials is that they may be affected by environmental erosion, loads, and other factors during use, leading to a decrease in material durability, which may seriously affect the safety and service life of the bridge. Summary of the Invention
[0005] To address the aforementioned technical problems, this application provides a precast bridge material and its preparation method.
[0006] This application provides a precast bridge material, specifically comprising the following components in parts by weight: 380-420 parts cement, 140-166 parts water, 800-820 parts river sand, 1000-1060 parts crushed stone, 82-90 parts admixture, and 6.2-7.6 parts additives; The preparation method of the admixture is as follows: bamboo fiber is soaked in an aqueous solution of 1-5 wt% sodium hydroxide and reacted at 20-40℃ for 8-10 hours. After the reaction, the bamboo fiber is removed and dried. Then, it is placed in an aqueous solution containing 5-9 wt% trifluoromethanesulfonic acid and 10-16 wt% inorganic phosphoric acid and reacted at 40-60℃ for 60-90 minutes. After the reaction, the bamboo fiber is removed and dried to obtain modified bamboo fiber. The modified bamboo fiber is mixed with fly ash at a weight ratio of 1-5:5 to obtain the admixture. The additive is composed of a mixture of polycarboxylate superplasticizer, water-soluble silicate, and triethanolamine in a weight ratio of 1-3:6-11:1-3.
[0007] This application utilizes the above-mentioned technical solution to treat bamboo fibers with an alkaline solution, which can promote the removal of some amorphous components in the fibers, reduce the degree of fiber aggregation, increase the surface roughness of bamboo fibers, increase the interface between fibers and other materials, and improve the good adhesion and bonding of bamboo fibers in the mixed system. Then, the alkaline-treated bamboo fibers are modified with an aqueous solution containing trifluoromethanesulfonic acid and inorganic phosphoric acid, which further increases the specific surface area of the fibers and can effectively improve the activity of hydroxyl groups on the fiber surface, making them more tightly bound to other raw materials and enhancing their improvement effect on precast bridge materials.
[0008] During the experiment, the inventors discovered that mixing modified bamboo fiber with fly ash in the above weight ratio as an admixture can increase the specific surface area of fly ash. The two have a synergistic effect, and the adhesion between the mixture and other raw materials is further strengthened, which is beneficial to improving the mechanical properties and durability of precast bridge materials.
[0009] Preferably, the precast bridge material specifically comprises the following components in parts by weight: 390-410 parts cement, 150-160 parts water, 805-815 parts river sand, 1020-1040 parts crushed stone, 84-88 parts admixture, and 6.6-7.2 parts additives.
[0010] Preferably, the modified bamboo fiber is prepared by: soaking bamboo fiber in a 2-4 wt% sodium hydroxide aqueous solution and reacting it at 20-40℃ for 8-10 hours. After the reaction, the bamboo fiber is removed and dried. Then, it is placed in an aqueous solution containing 6-8 wt% trifluoromethanesulfonic acid and 12-14 wt% inorganic phosphoric acid and reacted at 40-60℃ for 60-90 minutes. After the reaction, the bamboo fiber is removed and dried to obtain the blend.
[0011] Preferably, in the preparation method of the admixture, the weight ratio of the modified bamboo fiber to the fly ash is 2-4:5.
[0012] In some specific implementations, the weight ratio of the modified bamboo fiber to the fly ash can be 1-2:5, 1-3:5, 1-4:5, 2-3:5, 2-4:5, 2-5:5, 3-4:5, 3-5:5, or 4-5:5.
[0013] In one specific implementation, the weight ratio of the modified bamboo fiber to the fly ash can be 1:5, 2:5, 3:5, 4:5, or 5:5.
[0014] Experiments have shown that the modified bamboo fiber and fly ash mixed in the above weight ratio to form the admixture can further improve the mechanical properties and durability of precast bridge materials.
[0015] Preferably, in the preparation method of the admixture, the inorganic phosphate substance is selected from one or more of sodium hexametaphosphate, disodium hydrogen phosphate, sodium tripolyphosphate, sodium pyrophosphate, and sodium dihydrogen phosphate.
[0016] Preferably, the additive is composed of a polycarboxylate superplasticizer, a water-soluble silicate, and triethanolamine in a weight ratio of 1-3:7-10:1-3.
[0017] Experiments have shown that the additives composed of polycarboxylate superplasticizer, water-soluble silicate, and triethanolamine in the above weight ratio can further improve the mechanical properties and durability of precast bridge materials.
[0018] Preferably, the water-soluble silicate is selected from one or more of sodium silicate, potassium silicate, and lithium silicate.
[0019] Preferably, the performance parameters of the fly ash are: Class F, Grade I, fineness 6.8-7.2%, loss on ignition 4.0-4.4%, and water requirement ratio 93-96%.
[0020] Preferably, the performance parameters of the crushed stone are: mud content 0.7-0.9%, mud lump content 0.17-0.23%, crushing index value 8.0-10.0%, and needle-like and flaky content 10-12%.
[0021] Secondly, this application provides a method for preparing the aforementioned precast bridge material, specifically including the following steps: Weigh out the appropriate amounts of each raw material, and mix the cement, river sand, and crushed stone evenly to obtain a dry material; add the admixture to the water to form a liquid material; The dry material and the liquid material are stirred and mixed evenly to obtain a premix; the appropriate weight parts of the admixture are added to the premix, stirred and mixed evenly, and cured to obtain the precast bridge material.
[0022] In summary, the technical solution of this application has the following effects: This application utilizes modified bamboo fiber and fly ash mixed in a specific ratio as an admixture, along with additives of a specific type, and other raw materials to prepare precast bridge materials, thereby obtaining precast bridge materials with high mechanical properties; moreover, the precast bridge materials prepared by this application have good resistance to acid and alkali corrosion, which is beneficial to improving the durability and service life of the materials.
[0023] This application further improves the mechanical properties and durability of precast bridge materials by further optimizing the composition of admixtures and additives. Detailed Implementation
[0024] The specifications or properties of the raw materials used in this application are as follows: Fly ash: Class F, Grade I, fineness 7.0%, loss on ignition 4.2%, water requirement ratio 95%; The polycarboxylate superplasticizer in the admixture has a water reduction rate of 31%, a 1-day compressive strength ratio of 230%, a 3-day compressive strength ratio of 2000%, a 28-day compressive strength ratio of 160%, and good compatibility with cement. River sand: mud content 2.4%, mud lump content 0.5%, fineness modulus 2.9; Crushed stone: mud content 0.8%, mud lump content 0.2%, crushing index value 9.0%, needle-like and flaky content 11%; Bamboo fiber: average length 13-17mm, average diameter 0.15-0.25mm.
[0025] The present application will be further described in detail below with reference to embodiments, comparative examples and performance test results. These embodiments should not be construed as limiting the scope of protection claimed in this application. Example
[0026] Examples 1-3 Examples 1-3 each provide a prefabricated bridge material.
[0027] The difference between the above embodiments is that the amount of admixture is different, as shown in Table 1.
[0028] The preparation method of the admixture is as follows: 100g of bamboo fiber is soaked in 500g of 3wt% sodium hydroxide aqueous solution and reacted at 30℃ for 9h. After the reaction, the bamboo fiber is taken out and dried at 80℃. Then, it is placed in 500g of an aqueous solution containing 7wt% trifluoromethanesulfonic acid and 13wt% sodium pyrophosphate inorganic phosphoric acid and reacted at 50℃ for 75min. After the reaction, the bamboo fiber is taken out and dried at 80℃ to obtain modified bamboo fiber. The modified bamboo fiber is mixed with fly ash at a weight ratio of 3:5 to obtain the admixture. Weigh out the appropriate amounts of each raw material, and mix the cement (P·O42.5), river sand, and crushed stone evenly to obtain a dry material; add the admixture (composed of polycarboxylate superplasticizer, water-soluble silicate potassium silicate, and triethanolamine in a weight ratio of 2:9:2) to water to form a liquid material; The dry and liquid materials are mixed evenly to obtain a premix; the appropriate weight of admixtures are added to the premix, and the mixture is stirred evenly. The mixture is then poured into a mold, and the concrete is compacted using a vibrating device. The surface of the concrete is then smoothed manually with a trowel, and finally, the surface of the concrete is polished. The concrete is then steam-cured using a high-temperature steam method. The concrete is then demolded and discharged to obtain the precast bridge material.
[0029] Table 1. Amounts of each raw material in the precast bridge materials of Examples 1-3 and Comparative Examples 1-2. Examples 4-10 Examples 4-10 each provide a prefabricated bridge material.
[0030] The difference between the above embodiment and Embodiment 2 is that the preparation method of the admixture is different, as shown below.
[0031] In Example 4, the preparation method of the admixture is as follows: 100g of bamboo fiber is soaked in 500g of 1wt% sodium hydroxide aqueous solution and reacted at 30℃ for 9h. After the reaction, the bamboo fiber is taken out and dried at 80℃. Then, it is placed in 500g of an aqueous solution containing 5wt% trifluoromethanesulfonic acid and 16wt% sodium pyrophosphate inorganic phosphoric acid and reacted at 50℃ for 75min. After the reaction, the bamboo fiber is taken out and dried at 80℃ to obtain modified bamboo fiber. The modified bamboo fiber is mixed with fly ash at a weight ratio of 3:5 to obtain the admixture.
[0032] In Example 5: The preparation method of the admixture is as follows: 100g of bamboo fiber is soaked in 500g of 5wt% sodium hydroxide aqueous solution and reacted at 30℃ for 9h. After the reaction, the bamboo fiber is taken out and dried at 80℃. Then, it is placed in 500g of an aqueous solution containing 9wt% trifluoromethanesulfonic acid and 10wt% sodium pyrophosphate inorganic phosphoric acid and reacted at 50℃ for 75min. After the reaction, the bamboo fiber is taken out and dried at 80℃ to obtain modified bamboo fiber. The modified bamboo fiber is mixed with fly ash at a weight ratio of 3:5 to obtain the admixture.
[0033] In Example 6: In the preparation method of the admixture: the inorganic phosphate substance is sodium hexametaphosphate.
[0034] In Example 7: In the preparation method of the admixture: the inorganic phosphate substance is disodium hydrogen phosphate.
[0035] In Example 8: In the preparation method of the admixture: the inorganic phosphoric acid substance is sodium tripolyphosphate.
[0036] In Example 9: In the preparation method of the admixture: the weight ratio of modified bamboo fiber to fly ash is 1:5.
[0037] In Example 10: In the preparation method of the admixture: the weight ratio of modified bamboo fiber to fly ash is 5:5 (i.e., 1:1).
[0038] The amounts of other raw materials, the types of each raw material, and the preparation methods of the precast bridge materials in the above embodiments and Embodiment 2 are all the same.
[0039] Examples 11-14 Examples 11-14 each provide a prefabricated bridge material.
[0040] The difference between the above embodiment and Embodiment 2 is that the types of admixtures are different, as detailed below.
[0041] In Example 11: the admixture is composed of a mixture of polycarboxylate superplasticizer, water-soluble silicate potassium silicate, and triethanolamine in a weight ratio of 1:6:3.
[0042] In Example 12: the admixture is composed of a polycarboxylate superplasticizer, a water-soluble silicate potassium silicate, and triethanolamine in a weight ratio of 3:11:1.
[0043] In Example 13: the admixture is composed of a polycarboxylate superplasticizer, a water-soluble silicate sodium silicate, and triethanolamine in a weight ratio of 2:9:2.
[0044] In Example 14: the admixture is composed of a polycarboxylate superplasticizer, a water-soluble silicate lithium silicate, and triethanolamine in a weight ratio of 2:9:2.
[0045] The amounts of other raw materials, the types of each raw material, and the preparation methods of the precast bridge materials in the above embodiments and Embodiment 2 are all the same.
[0046] Comparative Example Comparative Examples 1-2 Comparative Examples 1 and 2 each provide a prefabricated bridge material.
[0047] The difference between the above comparative example and Example 2 is that the amount of admixture is different, as shown in Table 1.
[0048] The amounts of other raw materials, the types of each raw material, and the preparation methods of the precast bridge materials in the above comparative example and Example 2 are all the same.
[0049] Comparative Examples 3-6 Comparative Examples 3-2 each provide a prefabricated bridge material.
[0050] The difference between the above embodiment and embodiment 2 is as follows.
[0051] In Comparative Example 3, the method for preparing the admixture is as follows: unmodified bamboo fiber and fly ash are mixed at a weight ratio of 3:5 to obtain the admixture.
[0052] In Comparative Example 4: The preparation method of the admixture is as follows: 100g of bamboo fiber is soaked in 500g of 3wt% sodium hydroxide aqueous solution and reacted at 30℃ for 9h. After the reaction, the bamboo fiber is taken out and dried at 80℃. Then, it is placed in 500g of an aqueous solution containing 7wt% trifluoromethanesulfonic acid and 13wt% ethylenediaminetetramethylenephosphonic acid, an organophosphate, and reacted at 50℃ for 75min. After the reaction, the bamboo fiber is taken out and dried at 80℃ to obtain modified bamboo fiber. The modified bamboo fiber is mixed with fly ash at a weight ratio of 3:5 to obtain the admixture.
[0053] In Comparative Example 5: The preparation method of the admixture is as follows: 100g of bamboo fiber is soaked in 500g of 3wt% sodium hydroxide aqueous solution and reacted at 30℃ for 9h. After the reaction is completed, the bamboo fiber is taken out and dried at 80℃. Then it is placed in 500g of 13wt% sodium ethyl pyrophosphate aqueous solution and reacted at 50℃ for 75min. After the reaction is completed, the bamboo fiber is taken out and dried at 80℃ to obtain modified bamboo fiber. The modified bamboo fiber is mixed with fly ash at a weight ratio of 3:5 to obtain the admixture.
[0054] In Comparative Example 6: the admixture was a polycarboxylate superplasticizer.
[0055] The amounts of other raw materials, the types of each raw material, and the preparation methods of the precast bridge materials in the above comparative example and Example 2 are all the same.
[0056] Performance testing Performance and mechanical properties of the mixture: The performance and mechanical properties of the precast bridge materials were tested in accordance with GB / T50080-2016 "Standard for Test Methods of Performance of Ordinary Concrete Mixtures" and GB / T50081-2019 "Standard for Test Methods of Physical and Mechanical Properties of Ordinary Concrete".
[0057] Corrosion resistance: An 80mm×80mm×2mm square plate sample (after 28 days of curing) was immersed in a 6% hydrochloric acid and a 6% sodium hydroxide solution for 30 days. The change rate of compressive strength before and after immersion was then measured, and its acid and alkali corrosion resistance was calculated. The corrosion resistance calculation formula is: Corrosion resistance = Compressive strength of the sample after corrosion resistance test / Compressive strength of the original sample after 28 days of curing × 100%.
[0058] Test results are shown in Table 2.
[0059] Table 2 Performance test results of precast bridge materials in Examples 1-14 and Comparative Examples 1-6 Referring to Table 2, by comparing the performance test results of the precast bridge materials in Examples 1-14 and Comparative Examples 1-6, it can be seen that this application uses modified bamboo fiber and fly ash mixed in a specific ratio as admixtures, and at the same time, it uses a specific weight ratio of polycarboxylate superplasticizer, water-soluble silicate, and triethanolamine as additives, combined with other raw materials to prepare precast bridge materials, thus obtaining precast bridge materials with high mechanical properties; moreover, the precast bridge materials prepared by this application have good resistance to acid and alkali corrosion, which is beneficial to improving the durability and service life of the materials.
[0060] Although the present invention has been described in detail above with general descriptions and specific embodiments, modifications or improvements can be made to it, which will be obvious to those skilled in the art. Therefore, all such modifications or improvements made without departing from the spirit of the present invention fall within the scope of protection claimed by the present invention.
Claims
1. A precast bridge material, characterized in that, Specifically, it includes the following components by weight: 380-420 parts cement, 140-166 parts water, 800-820 parts river sand, 1000-1060 parts crushed stone, 82-90 parts admixture, and 6.2-7.6 parts additives; The preparation method of the admixture is as follows: bamboo fiber is soaked in an aqueous solution of 1-5 wt% sodium hydroxide and reacted at 20-40℃ for 8-10 hours. After the reaction, the bamboo fiber is taken out and dried. Then, it is placed in an aqueous solution containing 5-9 wt% trifluoromethanesulfonic acid and 10-16 wt% inorganic phosphoric acid and reacted at 40-60℃ for 60-90 minutes. After the reaction, the bamboo fiber is taken out and dried to obtain modified bamboo fiber. The modified bamboo fiber is mixed with fly ash at a weight ratio of 1-5:5 to obtain the admixture. The inorganic phosphate is selected from one or more of sodium hexametaphosphate, disodium hydrogen phosphate, sodium tripolyphosphate, sodium pyrophosphate, and sodium dihydrogen phosphate. The additive is composed of a mixture of polycarboxylate superplasticizer, water-soluble silicate, and triethanolamine in a weight ratio of 1-3:6-11:1-3. The water-soluble silicate is selected from one or more of sodium silicate, potassium silicate, and lithium silicate.
2. The precast bridge material according to claim 1, characterized in that, Specifically, it includes the following components by weight: 390-410 parts cement, 150-160 parts water, 805-815 parts river sand, 1020-1040 parts crushed stone, 84-88 parts admixture, and 6.6-7.2 parts additives.
3. The precast bridge material according to claim 1, characterized in that, The modified bamboo fiber is prepared by immersing bamboo fiber in a 2-4 wt% sodium hydroxide aqueous solution and reacting it at 20-40℃ for 8-10 hours. After the reaction, the bamboo fiber is removed and dried. Then, it is placed in an aqueous solution containing 6-8 wt% trifluoromethanesulfonic acid and 12-14 wt% inorganic phosphoric acid and reacted at 40-60℃ for 60-90 minutes. After the reaction, the bamboo fiber is removed and dried to obtain the modified bamboo fiber.
4. The precast bridge material according to claim 1, characterized in that, In the preparation method of the admixture, the weight ratio of the modified bamboo fiber to the fly ash is 2-4:
5.
5. The precast bridge material according to claim 1, characterized in that, The additive is composed of a mixture of polycarboxylate superplasticizer, water-soluble silicate, and triethanolamine in a weight ratio of 1-3:7-10:1-3.
6. The precast bridge material according to claim 1, characterized in that, The performance parameters of the fly ash are: Class F, Grade I, fineness 6.8-7.2%, loss on ignition 4.0-4.4%, and water requirement ratio 93-96%.
7. The precast bridge material according to claim 1, characterized in that, The performance parameters of the crushed stone are as follows: mud content 0.7-0.9%, mud lump content 0.17-0.23%, crushing index value 8.0-10.0%, and needle-like and flaky content 10-12%.
8. A method for preparing the precast bridge material according to any one of claims 1-7, characterized in that, Specifically, the following steps are included: Weigh out the appropriate amounts of each raw material, and mix the cement, river sand, and crushed stone evenly to obtain a dry material; add the admixture to the water to form a liquid material; The dry material and the liquid material are stirred and mixed evenly to obtain a premix; the appropriate weight parts of the admixture are added to the premix, stirred and mixed evenly, and cured to obtain the precast bridge material.
Citation Information
Patent Citations
Concrete used for bridges
CN106517905A
Preparation method for concrete for bridges
CN106565160A