Far infrared ray radioactive material, manufacturing method and application thereof

By manufacturing far-infrared radioactive materials with high emissivity, the problem of limited use of far-infrared rays in daily life has been solved, and its wide application in human correction equipment, tableware and other fields has been achieved, improving health effects and material performance.

CN118754633APending Publication Date: 2024-10-11DONGGUAN CHENGCHENGMEI TRADING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411020210.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The use of far-infrared rays in daily life is limited. It requires a specific location and is expensive, making it difficult to popularize it in daily life.

Method used

Using a far-infrared radioactive material including caustic soda, silicon oxide, aluminum oxide, titanium oxide, iron oxide, calcium oxide, magnesium oxide, potassium oxide and sodium oxide, through crushing, stirring, ceramic slurry mixing, molding and The high-temperature sintering process produces powerful far-infrared base materials with an emissivity of over 90%.

Benefits of technology

Far-infrared materials have been widely used in daily life, such as human body correction equipment, tableware and conveying pipe fittings, to promote health, reduce diseases, and improve the wear resistance, antioxidant capacity and service life of the material.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a far infrared ray radioactive material, a manufacturing method and application thereof, and relates to the field of manufacturing of far infrared ray radioactive materials. Comprising the following raw materials in percentage by weight: 3%-5% of burning soda, 65%-75% of silicon oxide, 18%-25% of aluminum oxide, 0.03%-0.07% of titanium oxide, 0.1%-0.3% of ferric oxide, 0.3%-0.5% of calcium oxide, 0.2%-0.4% of magnesium oxide, 2.5%-4% of potassium oxide and 1%-2% of sodium oxide. As far infrared rays can promote health and reduce diseases, products made of the material can be widely applied to daily life, for example, human body correction equipment (such as spectacle lenses, protective films and the like), tableware utensils, conveying pipe fittings (such as pipe fittings for liquid such as oil, water and the like), even energy stones capable of changing water quality and the like. Therefore, far infrared rays can be conveniently used in daily life.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of far-infrared radioactive material manufacturing, in particular to a far-infrared radioactive material, a manufacturing method and application thereof. Background Art

[0002] Infrared refers to light waves with a wavelength ranging from 15 to 1000 microns, which is a part of infrared. In addition to its applications in science and technology and astronomy, far infrared is also widely used in medicine and health care. The wavelength of its emission is between 4 and 14 microns, and it can produce a resonance frequency of 300,000 times per second. Far infrared of this wavelength and frequency has "resonance absorption" and "penetration", so it is easily absorbed by many substances, resulting in thermal reactions. When far infrared penetrates into the internal tissues of the human body, it can cause the water molecules in the cells of the human body to resonate. In addition, carbon dioxide molecules in the microvessels can also absorb far infrared of different wavelengths. The energy and heat released by these molecules after enhanced vibration will cause blood vessels to dilate, enhance the exchange and transportation capacity of microvessels, accelerate blood circulation, promote enzyme production, give cells vitality, activate metabolism, enhance tissue regeneration ability, and improve the body's immunity. Far infrared rays have a good health-care effect, can promote blood circulation, and achieve the effect of health care. In real life, if people want to achieve health-care effects or treat diseases through infrared rays, they must go to specific places, such as hospitals, to receive corresponding treatments. This is not only troublesome but also requires a certain amount of money, thus limiting the use of far infrared rays in daily life. Summary of the invention

[0003] The purpose of the present invention is to provide a far-infrared radioactive material, a manufacturing method and its application in order to solve the problems raised in the above-mentioned background technology.

[0004] To achieve the above-mentioned purpose, the present invention provides the following technical solution: a far-infrared radioactive material, comprising the following raw materials in weight ratio: 3% to 5% by weight of caustic soda, 65% to 75% by weight of silicon oxide, 18% to 25% by weight of aluminum oxide, 0.03% to 0.07% by weight of titanium oxide, 0.1% to 0.3% by weight of iron oxide, 0.3% to 0.5% by weight of calcium oxide, 0.2% to 0.4% by weight of magnesium oxide, 2.5% to 4% by weight of potassium oxide and 1% to 2% by weight of sodium oxide.

[0005] A method for manufacturing a far-infrared radioactive material comprises the following steps: Step 1: prepare the following materials, 3% to 5% by weight of caustic soda, 65% to 75% by weight of silicon oxide, 18% to 25% by weight of aluminum oxide, 0.03% to 0.07% by weight of titanium oxide, 0.1% to 0.3% by weight of iron oxide, 0.3% to 0.5% by weight of calcium oxide, 0.2% to 0.4% by weight of magnesium oxide, 2.5% to 4% by weight of potassium oxide, and 1% to 2% by weight of sodium oxide; Step 2: respectively crushing and sieving the caustic soda, silicon oxide, aluminum oxide, titanium oxide, iron oxide, calcium oxide, magnesium oxide, potassium oxide and sodium oxide weighed by weight to obtain raw material powders; Step 3: Add the raw material powders obtained in step 2 into a stirrer and mix them using the stirrer; Step 4: When the raw materials are mixed in the blender, ceramic slurry is added until the raw material powders and the ceramic slurry are fully mixed and uniformly mixed into a plastic semi-solid state; Step 5: Molding: Molding the mixed semi-solid raw materials into a semi-finished product of a specific shape; Step 6: high temperature sintering: the semi-finished product is sintered at high temperature by sintering technology, the sintering temperature is 1200~-1500 degrees Celsius, and the sintering time is continuous 7-10 hours; Step 7: Cooling to form a strong far-infrared substrate: After high-temperature sintering, the substrate is naturally cooled to obtain a finished product of the strong far-infrared substrate, and the emissivity of the strong far-infrared substrate is more than 90%.

[0006] As a further solution of the present invention: the pulverizing described in step 2 is to add each raw material into a ball mill separately, and crush each raw material by the grinding medium in the ball mill, and crush each raw material into powder.

[0007] As a further solution of the present invention: the screening described in step 2 is to screen the raw materials ground into powder by vibrating the mesh screen, and the qualified raw material powders that pass through the mesh screen are reserved, and the unqualified raw materials that do not pass through the mesh screen are further crushed until they are completely qualified. The mesh number of the mesh screen is 2000 mesh.

[0008] As a further solution of the present invention: the molding described in step five is to inject the semi-solid raw material into two halves of a molding mold that can be opened and closed, and the mold in the closed state shapes the semi-solid raw material.

[0009] An application of far-infrared radioactive materials, which are made into various utensils after the far-infrared radioactive materials are effectively solidified.

[0010] Compared with the prior art, the present invention has the following beneficial effects: 1. Since far infrared rays can promote health and reduce diseases, products made from this material can be widely used in daily life, for example, to make human body correction equipment (such as eyeglass lenses, protective films, etc.), tableware, conveying pipes (such as pipes for oil, water and other liquids), and even energy stones that can change water quality, etc., thus facilitating the use of far infrared rays in daily life. DETAILED DESCRIPTION

[0011] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0012] In an embodiment of the present invention, a far-infrared radioactive material includes the following raw materials in weight ratio: 3% to 5% by weight of caustic soda, 65% to 75% by weight of silicon oxide, 18% to 25% by weight of aluminum oxide, 0.03% to 0.07% by weight of titanium oxide, 0.1% to 0.3% by weight of iron oxide, 0.3% to 0.5% by weight of calcium oxide, 0.2% to 0.4% by weight of magnesium oxide, 2.5% to 4% by weight of potassium oxide, and 1% to 2% by weight of sodium oxide.

[0013] In this embodiment: silicon oxide (silicon dioxide) produces far-infrared radiation effect after high-temperature sintering, aluminum oxide (aluminum oxide) improves the wear resistance and corrosion resistance of the substrate and extends the service life, titanium oxide (titanium dioxide) has excellent photocatalytic properties and can effectively decompose organic pollutants, iron oxide (iron oxide) improves the antioxidant ability of the substrate and enhances durability, calcium oxide (calcium monoxide) helps to improve the sintering performance of the material and increases the density and hardness of the substrate, magnesium oxide (magnesium monoxide) improves the refractoriness of the substrate and reduces the thermal expansion coefficient, potassium oxide (potassium monoxide) enhances the toughness and elasticity of the substrate and improves the impact resistance, and sodium oxide (sodium monoxide) improves the melting characteristics of the substrate and optimizes the manufacturing process.

[0014] A method for manufacturing a far-infrared radioactive material comprises the following steps: Step 1: prepare the following materials, 3% to 5% by weight of caustic soda, 65% to 75% by weight of silicon oxide, 18% to 25% by weight of aluminum oxide, 0.03% to 0.07% by weight of titanium oxide, 0.1% to 0.3% by weight of iron oxide, 0.3% to 0.5% by weight of calcium oxide, 0.2% to 0.4% by weight of magnesium oxide, 2.5% to 4% by weight of potassium oxide, and 1% to 2% by weight of sodium oxide; Step 2: respectively crushing and sieving the caustic soda, silicon oxide, aluminum oxide, titanium oxide, iron oxide, calcium oxide, magnesium oxide, potassium oxide and sodium oxide weighed by weight to obtain raw material powders; Step 3: Add the raw material powders obtained in step 2 into a stirrer and mix them using the stirrer; Step 4: When the raw materials are mixed in the blender, ceramic slurry is added until the raw material powders and the ceramic slurry are fully mixed and uniformly mixed into a plastic semi-solid state; Step 5: Molding: Molding the mixed semi-solid raw materials into a semi-finished product of a specific shape; Step 6: high temperature sintering: the semi-finished product is sintered at high temperature by sintering technology, the sintering temperature is 1200~-1500 degrees Celsius, and the sintering time is continuous 7-10 hours; Step 7: Cooling to form a strong far-infrared substrate: After high-temperature sintering, the substrate is naturally cooled to obtain a finished product of the strong far-infrared substrate, and the emissivity of the strong far-infrared substrate is more than 90%.

[0015] In this embodiment: the ceramic slurry acts as a binder to bond the raw material powders together without causing the raw materials to disperse. After the raw material powders are fully mixed in the ceramic slurry, the performance of the ceramic slurry can be improved while retaining its own performance.

[0016] The pulverization described in step 2 is to add each raw material into a ball mill respectively, and crush each raw material by the grinding medium in the ball mill, and crush each raw material into powder.

[0017] In this embodiment, the raw materials are in the ball mill. As the ball mill rotates, the grinding media (steel balls) fully grind and crush the raw materials to avoid uneven grinding of the raw materials.

[0018] The screening described in step 2 is to screen the raw materials ground into powder by vibrating the mesh screen, and the qualified raw material powders passing through the mesh screen are reserved, and the unqualified raw materials that do not pass the mesh screen are further crushed until they are completely qualified. The mesh number of the mesh screen is 2000 mesh.

[0019] In this embodiment: after the grinding is completed, each powdered raw material is discharged through a cyclone separator, and then vibrated and screened to select qualified powdered materials.

[0020] The molding described in step five is to inject the semi-solid raw material into two halves of a molding mold that can be opened and closed, and the mold in the closed state shapes the semi-solid raw material.

[0021] In this embodiment: a slurry containing various raw material powders is shaped by a shaping mold, and sintered and hardened after shaping to achieve dehydration and solidification of the slurry.

[0022] After the far-infrared radioactive material is effectively solidified, it is made into various utensils.

[0023] In this embodiment: the products made of this material can be widely used in daily life, for example, human body correction equipment (such as eyeglass lenses, protective films, etc.), tableware, conveying pipes (such as pipes for oil, water and other liquids), and even energy stones that can change water quality.

[0024] What is described above is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A far-infrared radioactive material, characterized in that: The invention comprises the following raw materials in weight ratio: 3% to 5% caustic soda by weight, 65% to 75% silicon oxide by weight, 18% to 25% aluminum oxide by weight, 0.03% to 0.07% titanium oxide by weight, 0.1% to 0.3% iron oxide by weight, 0.3% to 0.5% calcium oxide by weight, 0.2% to 0.4% magnesium oxide by weight, 2.5% to 4% potassium oxide by weight and 1% to 2% sodium oxide by weight.

2. A method for producing the far-infrared radiating material according to claim 1, characterized in that: The following steps are involved: Step 1: prepare the following materials, 3% to 5% by weight of caustic soda, 65% to 75% by weight of silicon oxide, 18% to 25% by weight of aluminum oxide, 0.03% to 0.07% by weight of titanium oxide, 0.1% to 0.3% by weight of iron oxide, 0.3% to 0.5% by weight of calcium oxide, 0.2% to 0.4% by weight of magnesium oxide, 2.5% to 4% by weight of potassium oxide, and 1% to 2% by weight of sodium oxide; Step 2: respectively crushing and sieving the caustic soda, silicon oxide, aluminum oxide, titanium oxide, iron oxide, calcium oxide, magnesium oxide, potassium oxide and sodium oxide weighed by weight to obtain raw material powders; Step 3: Add the raw material powders obtained in step 2 into a stirrer and mix them using the stirrer; Step 4: When the raw materials are mixed in the blender, ceramic slurry is added until the raw material powders and the ceramic slurry are fully mixed and uniformly mixed into a plastic semi-solid state; Step 5: Molding: Molding the mixed semi-solid raw materials into a semi-finished product of a specific shape; Step 6: high temperature sintering: the semi-finished product is sintered at high temperature by sintering technology, the sintering temperature is 1200~-1500 degrees Celsius, and the sintering time is continuous 7-10 hours; Step 7: Cooling to form a strong far-infrared substrate: After high-temperature sintering, natural cooling is completed to obtain the strong far-infrared substrate. The finished product of the outer ray base material, and the emissivity of this strong far infrared base material is over 90%.

3. The method for producing a far-infrared radioactive material according to claim 2, characterized in that: The pulverization described in step 2 is to add each raw material into a ball mill respectively, and crush each raw material by the grinding medium in the ball mill, and crush each raw material into powder.

4. The method for producing a far-infrared radioactive material according to claim 3, characterized in that: The screening described in step 2 is to screen the raw materials ground into powder by vibrating the mesh screen, and the qualified raw material powders passing through the mesh screen are reserved, and the unqualified raw materials that do not pass the mesh screen are further crushed until they are completely qualified. The mesh number of the mesh screen is 2000 mesh.

5. The method for producing a far-infrared radioactive material according to claim 4, characterized in that: The molding described in step five is to inject the semi-solid raw material into two halves of a molding mold that can be opened and closed, and the mold in the closed state shapes the semi-solid raw material.

6. Use of the far-infrared radioactive material according to any one of claims 2 to 5, characterized in that: After the far-infrared radioactive material is effectively solidified, it is made into various utensils.