8H-dibenzacridine derivative and electroluminescent device thereof
By designing 8H-dibenzoacridine derivatives as TADF materials and using their structural characteristics to apply them in OLED devices, we solve the problem of replacing green TADF materials in the existing technology, achieve high luminous efficiency and stability, and prolong It improves the device life and provides a basis for research on green light materials.
Patent Information
- Application Number
- CN202410836872.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-26
- Publication Date
- 2024-10-11
AI Technical Summary
In the existing technology, green TADF materials used in OLED devices are difficult to replace heavy metal iridium complexes, and there are problems of unsustainability and environmental unfriendliness of rare metals. There is a lack of efficient green TADF material solutions.
An 8H-dibenzoacridine derivative was designed as a TADF material, using its structural characteristics to use benzoxazole, pyrimidine, pyrazine, etc. as substituents to reduce intermolecular stacking, improve device stability, and perform in OLED devices In applications, the host and guest luminescent materials are combined to improve luminous efficiency and stability.
It significantly improves the luminous efficiency of the OLED device, reduces the startup voltage and energy consumption, and extends the working life of the device. The color coordinate is in the range of yellow-green light to green light, laying the foundation for the research of green light materials.
Smart Images

Figure CN118754883A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of organic light-emitting materials and semiconductors, and specifically relates to an 8H-dibenzoacridine derivative and an electroluminescent device thereof. Background Art
[0002] In recent years, organic light-emitting diodes (OLEDs) have become a hot research direction in the field of lighting and display due to their excellent properties such as self-luminescence, high brightness, high contrast, see-through, wearable, foldable, low energy consumption, wide viewing angle, and low temperature resistance. With the development of science and technology, researchers have developed the third generation of OLED luminescent materials - thermally activated delayed fluorescence (TADF) materials. TADF materials have a small singlet-triplet energy level difference (ΔEst), and triplet excitons can effectively realize the conversion of triplet excitons to singlet excitons through the reverse intersystem crossing (RISC) process, and obtain an internal quantum efficiency of nearly 100%. Therefore, TADF materials have attracted much attention as emerging materials for OLED devices.
[0003] Typically, organic TADF materials use the DA configuration to reduce the overlap between HOMO / LUMO, thereby producing the smallest ΔEst. In general, TADF molecules are pure organic push-pull electron systems containing electron donors (donor, D) and electron acceptors (acceptor, A). By changing the structure, number, substituents and positions of the donor and acceptor units, the singlet-triplet energy level difference, frontier orbital distribution, aggregated state structure, electroluminescent color and performance of the TADF molecule can be adjusted. At the same time, the substituents play a very important role in regulating the push-pull electron capabilities of the donor and acceptor units and the physical and chemical properties of the TADF material, such as the molecular configuration, aggregated state structure and stability.
[0004] In order to manufacture high-efficiency OLEDs, the TADF materials used therein must have a small ΔEst and a high electroluminescent quantum yield (PLQY). Generally, for OLED devices to achieve full-color display, materials that emit red, green, and blue light are required. Among the three primary electroluminescent materials, green light emitting materials are currently mainly phosphorescent materials of heavy metal iridium complexes. However, due to the high price of heavy metal complexes, the unsustainable development of rare metals, and the environmental unfriendliness, people have been looking for friendly alternatives to the above materials.
[0005] In 2021, the patent number applied by Deshan Company of South Korea is US11088330B2 and the chemical formula is published The invention has created a series of high-performance green light materials, which contributes to the field of OLED light-emitting materials. However, the series of compounds disclosed in this invention are difficult to be used as TADF materials.
[0006] Therefore, how to design and develop high-efficiency green light TADF materials for OLED devices is very necessary and of great strategic significance. Summary of the invention
[0007] The purpose of the present invention is to overcome the deficiencies of the above-mentioned prior art and provide an 8H-dibenzoacridine derivative and an electroluminescent device thereof, wherein the 8H-dibenzoacridine derivative is used as a TADF material.
[0008] In order to solve the technical problem, the technical solution of the present invention is:
[0009] Preferably, a 8H-dibenzoacridine derivative, the general structural formula of the 8H-dibenzoacridine derivative includes general formula 1:
[0010]
[0011] Where:
[0012] n is an integer selected from 1, 2, and 3;
[0013] Y1 is selected from H, C1-C8 alkyl, C1-C8 alkoxy;
[0014] L is selected from C3~C 20 heteroaryl;
[0015] Ar1, Ar2 are independently selected from H, deuterium, C1-C 30 Alkyl, C6~C 40 Substituted or unsubstituted aryl, C5~C 30 The substituted or unsubstituted substituent is selected from: C1 to C 10 Alkyl, C3~C 10 Cycloalkyl, C5~C 20 Heteroaryl, C6~C 20 One or more of aryl, dimethylamino, trimethylsilyl, triphenylsilyl, and morpholinyl;
[0016] The heteroatoms in the heteroaryl group include O, S, N, P, B, and Si. The heteroaryl group includes a monocyclic heteroaryl group and a polycyclic heteroaryl group.
[0017] Preferably, the general formula 1 includes chemical formulas 1 to 8, and the specific structural formula is as follows:
[0018]
[0019] Where:
[0020] n is an integer selected from 1, 2, and 3;
[0021] Ar1, Ar2 are independently selected from H, deuterium, C1-C 30Alkyl, C6~C 40 Substituted or unsubstituted aryl, C5~C 30 The substituted or unsubstituted substituent is selected from: C1 to C 10 Alkyl, C3~C 10 Cycloalkyl, C5~C 20 Heteroaryl, C6~C 20 One or more of aryl, dimethylamino, trimethylsilyl, triphenylsilyl, and morpholinyl;
[0022] R1, R2 are independently selected from H, cyano, trifluoromethyl, C6-C 20 The aromatic group;
[0023] The heteroatoms in the heteroaryl group include O, S, N, P, B, and Si. The heteroaryl group includes a monocyclic heteroaryl group and a polycyclic heteroaryl group.
[0024] Preferably, an electroluminescent device comprises a cathode, an anode and an organic layer located between the cathode and the anode, wherein the organic layer comprises any one of the compounds 1 to 216 of the present invention.
[0025] Preferably, the organic layer comprises a hole transport layer, a light emitting layer and an electron transport layer, and the light emitting layer comprises any one of the compounds 1 to 216 of the present invention.
[0026] Preferably, the light-emitting layer comprises a host light-emitting material and a guest light-emitting material, wherein the host light-emitting material is selected from
[0027] The guest luminescent material comprises any one of the compounds 1 to 216 of the present invention, and the mass ratio of the host luminescent material to the guest luminescent material is in the range of 97:3 to 80:20.
[0028] Preferably, the mass ratio of the host luminescent material to the guest luminescent material is 90:10.
[0029] Compared with the prior art, the advantages of the present invention are:
[0030] (1) The present invention uses 8H-dibenzoacridine structure as a fixed core and benzoxazole, pyrimidine, pyrazine, triazine, pteridine, benzothiazole, benzoquinoxaline, etc. as fixed substituents (electron acceptor A). Such substituents have low reduction potentials, which are conducive to accepting electrons and thus facilitate electron transmission. At the same time, the main skeleton of the 8H-dibenzoacridine molecule (electron donor D) is conducive to hole transmission. Therefore, materials of this type of structure can be used as TADF materials.
[0031] (2) The present invention uses 8H-dibenzoacridine structure as electron donor, and uses benzene, diphenyl and terphenyl as bridges to connect electron acceptors with different substituents. This structure is beneficial to reduce intermolecular stacking and aggregation quenching, thereby improving device stability.
[0032] (3) The 8H-dibenzoacridine derivative described in the present invention is used as a TADF material in the light-emitting layer of an OLED device, and has excellent thermal stability and thin film stability, which is beneficial to the preparation of the device. At the same time, it significantly improves the luminous efficiency of the device, reduces the starting voltage and energy consumption, and improves the device working life and device stability.
[0033] (4) The color coordinates of the OLED device prepared from the preferred 8H-dibenzoacridine structure derivative of the present invention are in the range of yellow-green to green light, which lays a certain foundation for the later research on OLED green light materials. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 , a cross-sectional view of an electroluminescent device of the present invention;
[0035] Figure 2 , the NMR spectrum of compound 6 of the present invention;
[0036] Figure 3 , the NMR spectrum of compound 11 of the present invention;
[0037] Figure 4 , the NMR spectrum of compound 69 of the present invention;
[0038] Figure 5 , the NMR spectrum of compound 167 of the present invention.
[0039] Description of reference numerals:
[0040] 1. Conductive glass, 2. Anode, 3. Hole injection layer, 4. Hole transport layer, 5. Light-emitting layer, 6. Electron transport layer, 7. Electron injection layer, 8. Cathode. DETAILED DESCRIPTION
[0041] The specific implementation mode of the present invention is described below in conjunction with examples. The raw materials and reagents described in the present invention are all commercially available.
[0042] The present invention discloses an 8H-dibenzoacridine derivative, wherein the structure of the 8H-dibenzoacridine is as shown in general formula 1:
[0043]
[0044] Wherein, n is an integer selected from 1, 2, and 3;
[0045] Y1 is selected from H, C1-C8 alkyl, C1-C8 alkoxy;
[0046] L is selected from C3~C 20 A substituted or unsubstituted heteroaryl group;
[0047] Ar1, Ar2 are independently selected from H, deuterium, C1-C 30 Alkyl, C6~C 40 Substituted or unsubstituted aryl, C5~C 30 The substituted or unsubstituted substituent is selected from: C1 to C 10 Alkyl, C3~C 10 Cycloalkyl, C5~C 20 Heteroaryl, C6~C 20 One or more of aryl, dimethylamino, trimethylsilyl, triphenylsilyl, and morpholinyl;
[0048] The heteroatom in the term "heteroaryl" includes O, S, N, P, B, and Si, and the heteroaryl includes a monocyclic heteroaryl and a polycyclic heteroaryl.
[0049] Preferably, the general formula 1 includes chemical formulas 1 to 8, and the specific structural formulas are as follows:
[0050]
[0051] Wherein, n is an integer selected from 1, 2, and 3;
[0052] Ar1, Ar2 are independently selected from H, deuterium, C1-C 30 Alkyl, C6~C 40 Substituted or unsubstituted aryl, C5~C 30 The substituted or unsubstituted substituent is selected from: C1 to C 10 Alkyl, C3~C 10 Cycloalkyl, C5~C 20 Heteroaryl, C6~C 20 One or more of aryl, dimethylamino, trimethylsilyl, triphenylsilyl, and morpholinyl;
[0053] R1, R2 are independently selected from H, cyano, trifluoromethyl, C6~C 20 The aromatic group;
[0054] The heteroatom in the term "heteroaryl" includes O, S, N, P, B, and Si, and the heteroaryl includes a monocyclic heteroaryl and a polycyclic heteroaryl.
[0055] The 8H-dibenzoacridine derivatives specifically include but are not limited to compounds 1 to 216, and the specific structural formula is:
[0056]
[0057]
[0058]
[0059]
[0060]
[0061]
[0062]
[0063]
[0064]
[0065]
[0066]
[0067]
[0068]
[0069] Preferably, an electroluminescent device comprises a cathode, an anode and an organic layer located between the cathode and the anode, wherein the organic layer comprises any one of the compounds 1 to 216 of the present invention.
[0070] Preferably, the organic layer comprises a hole transport layer, a light emitting layer and an electron transport layer, and the light emitting layer comprises any one of the compounds 1 to 216 of the present invention.
[0071] Preferably, the light-emitting layer includes a host light-emitting material and a guest light-emitting material, the host light-emitting material is selected from one or a combination of at least two of PH-1, PH-2, PH-3, PH-4 and PH-5 with high triplet energy, the guest light-emitting material contains any one of the compounds 1 to 216 of the present invention, and the mass ratio of the host light-emitting material to the guest light-emitting material is in the range of 97:3 to 80:20.
[0072] Preferably, the mass ratio of the host luminescent material to the guest luminescent material is 90:10.
[0073] The synthesis process of the 8H-dibenzoacridine derivatives (compounds 1 to 216) of the present invention is described as follows: The structures of some key intermediates used in the implementation process are shown in Table 1:
[0074]
[0075] The synthesis process of some intermediates is as follows:
[0076] 1. Synthesis steps of key intermediate M1:
[0077] Step 1:
[0078]
[0079] Operation process: under nitrogen protection, add 1.571 kg of N-(8-bromobenzonaphthyl-9-yl)acetamide to a 20L three-necked flask, add 10L of a mixed solution of THF and H2O with a volume ratio of 4:1, and 2.073 kg of K2CO3, stir and heat to 40°C, add 4173 g of Pd(PPh3) after the solution is clarified, and after the addition, the reaction solution is heated to 80°C and the reaction is continued for 12 hours until the reaction is completed. The reaction solution is cooled to room temperature, EA is added for multiple extractions, the organic phases are combined, dried over anhydrous magnesium sulfate, filtered and concentrated, and passed through a silica gel column to obtain 1.366 kg of a white solid M1-1, with a yield of 80%, a HPLC content of 98%, and a molecular weight of 342.10 shown by LC-MS.
[0080] Step 2:
[0081]
[0082] Operation process: Under nitrogen protection, add M1-1 (1.366 kg) and 6.0 L of dichloromethane into a 20L three-necked flask, stir and cool to 0°C, add 4.6 L of dichloromethane solution of boron tribromide (1.0 mol / L) dropwise into the system, after the addition is complete, the reaction solution is heated to room temperature and reacted for 18 hours. After the reaction is completed, the reaction solution is cooled to 0°C, slowly added with ice water to quench, and concentrated sodium bicarbonate solution is added dropwise until the reaction solution is weakly alkaline. The organic phase is separated and then washed with water in small amounts several times until neutral. The organic phase is dried and concentrated under reduced pressure, and recrystallized with dichloromethane / petroleum ether to obtain an off-white solid M1-2 weighing 1.152 kg, with a yield of 88%, an HPLC content of 98%, and a molecular weight of 328.03 shown by LC-MS.
[0083] Step 3:
[0084]
[0085] Operation process: Under nitrogen protection, add 1.146 kg of M1-2 into a 20L three-necked flask, add 8L of a mixed solution of ethanol and 80% hydrazine hydrate in a volume ratio of 5:3, and heat to reflux for 40 hours. After the reaction is completed, the reaction solution is cooled to room temperature, extracted with dichloromethane, dried over anhydrous magnesium sulfate, and passed through a silica gel column to obtain an off-white solid M1-3, weighing 842 g, with a yield of 90%, HPLC content of 98%, and LC-MS showing a molecular weight of 268.00.
[0086] Step 4:
[0087]
[0088] Operation process: under nitrogen protection, add M1-30.866kg, p-chlorobromobenzene 0.620kg, and toluene 8.0L into a 20L three-necked flask, stir until the solution is clear, add Pd2(dba) 359g, Am-phos 33g, and sodium tert-butoxide 0.623g, and heat the reaction solution to 120°C for 10h. After the reaction is completed, filter it while hot using diatomaceous earth, cool the filtrate to room temperature, add purified water for washing, retain the organic phase after separation, extract the aqueous phase with ethyl acetate, combine the organic phases, dry over anhydrous magnesium sulfate, concentrate, and pass through a column to obtain an off-white solid M1 weighing 1.004kg, with a yield of 82%, an HPLC content of 99%, and a molecular weight of 377.99 shown by LC-MS.
[0089]
[0090] Operation process: Under inert atmosphere, add 0.982kg of M1-4, 0.792kg of biboric acid pinacol ester, 0.561kg of potassium acetate, and 10L of 1,4-dioxane into a 20L three-necked flask, start stirring and heat to
[0091] After 60-65°C, add 21g of Pd(dppf)Cl2, and then continue to heat up to reflux reaction for 6-8h until M1-4 reacts completely. Filter the reaction solution directly, collect the filtrate, concentrate under reduced pressure to dryness, dissolve in 2000mL of toluene, and then wash with water. After the organic phase passes through the silica gel column, the column liquid is again concentrated under reduced pressure until solid precipitates, then stop, cool to 10-15°C, filter after crystallization, and dry to obtain 0.964kg of white solid M2, with a yield of 79%.
[0092] HPLC content 99%, LC-MS molecular weight 470.12.
[0093] 2. Synthesis of key intermediate M2:
[0094]
[0095] Operation process: Under nitrogen protection, add M1: 235g, 2,4-dichlorobenzoxazole 94g, 1,4-dioxane 1500mL, potassium carbonate 138g, deionized water 60mL, Pd(PPh3)4 12g into a 3L three-necked flask, and heat the system to reflux for 15-18h until the reaction is complete. Wash the reaction solution with water and separate the liquids. Collect the filtrate after the organic phase passes through a diatomaceous earth funnel, and concentrate under reduced pressure to obtain a solid crude product. Add 500mL of ethanol to disperse and slurry, and then filter to obtain 164g of off-white solid M2, with a yield of 66%, HPLC content of 99%, and LC-MS molecular weight of 495.16.
[0096] 3. Synthesis of key intermediate M3:
[0097]
[0098] Operation process: referring to the synthesis process of M2, 92 g of 2,4,5-trichloropyrimidine was added to obtain 164 g of off-white solid M3, with a yield of 67%, HPLC content of 99%, and LC-MS molecular weight of 490.00.
[0099] 4. Synthesis of key intermediate M4:
[0100]
[0101] Operation process: referring to the synthesis process of M2, 92 g of 2,3,5-trichloropyrazine was added to obtain 167 g of off-white solid M4, with a yield of 68%, HPLC content of 99%, and LC-MS molecular weight of 490.03.
[0102] 5. Synthesis of key intermediate M5
[0103]
[0104] Operation process: referring to the synthesis process of M2, 111 g of 2,6-dichloro-4-diethylaminopyrazine was added to obtain 184 g of off-white solid M5 with a yield of 70%, HPLC content of 99%, and LC-MS molecular weight of 527.06.
[0105] 6. Synthesis of key intermediate M6
[0106]
[0107] Operation process: referring to the synthesis process of M2, 101 g of 2,4-dichloropteridine was added to obtain 175 g of off-white solid M6 with a yield of 69%, HPLC content of 99%, and LC-MS molecular weight of 508.12.
[0108] 7. Synthesis of key intermediate M7
[0109]
[0110] Operation process: referring to the synthesis process of M2, 102 g of 2,4-dichlorobenzothiazole was added to obtain 177 g of off-white solid M7, with a yield of 69%, HPLC content of 99%, and LC-MS molecular weight of 511.13.
[0111] Using the above key intermediates, the synthesis implementation process of the preferred compound 6, compound 11, compound 56, compound 69, compound 109, compound 150, and compound 167 is exemplified as follows:
[0112] Synthesis of compound 6:
[0113]
[0114] Operation process: Under nitrogen protection, add M2 (5.0 g), 2.0 g of cyclohexylphenylboronic acid, and a mixed solution of DMF and H2O (V DMF :V H2O =6:1)50mL, stirred until the solution was clear, added Pd2(dba)30.18g, X-Phos 0.24g, K3PO44.2g, the reaction solution was heated to 97°C and continued to react for 8h~10h until the reaction was completed, filtered while hot using diatomaceous earth, the filtrate was cooled to room temperature, purified water was added to wash the filter cake, the filtrate was extracted with ethyl acetate, the organic phases were combined, dried over anhydrous magnesium sulfate, concentrated, and passed through a column to obtain an off-white solid compound 6, weighing 4.9g, with a yield of 79%, HPLC content of 99%, and LC-MS showing a molecular weight of 619.25.
[0115] Synthesis of compound 11:
[0116]
[0117] Operation process: refer to the synthesis process of compound 6, add 5.0g M2 and 2.2g 9-phenanthreneboric acid to obtain 4.8g of compound 11 as an off-white solid with a yield of 76%, HPLC content of 99%, and LC-MS molecular weight of 637.21.
[0118] Synthesis process of compound 56:
[0119]
[0120] Operation process: Referring to the synthesis process of compound 6, 4.9 g of M3 and 2.4 g of 2,6-dimethyl-4-morpholinophenylboronic acid were added to obtain 6.1 g of compound 56 as an off-white solid with a yield of 76%, HPLC content of 99%, and LC-MS molecular weight of 780.40.
[0121] Synthesis process of compound 69:
[0122]
[0123] Operation process: refer to the synthesis process of compound 6, add 4.9 g of M4 and 1.7 g of 2-naphthalene-phenylboronic acid to obtain 5.3 g of compound 69, an off-white solid, with a yield of 78%, HPLC content of 99%, and LC-MS molecular weight of 674.25.
[0124] Synthesis process of compound 109:
[0125]
[0126] Operation process: refer to the synthesis process of compound 6, add 5.3g of M5 and 1.7g of 4-(dimethylamino)phenylboronic acid to obtain 4.5g of compound 109 as an off-white solid with a yield of 73%, HPLC content of 99%, and LC-MS molecular weight of 612.25.
[0127] Synthesis process of compound 150:
[0128]
[0129] Operation process: refer to the synthesis process of compound 6, add 5.1g of M6 and 4.5g of 4-(9,9-diphenylacridine-10-(9H)-yl)phenylboronic acid to obtain 5.0g of compound 150 as an off-white solid with a yield of 70%, HPLC content of 99%, and LC-MS molecular weight of 717.28.
[0130] Synthesis process of compound 167:
[0131]
[0132] Operation process: refer to the synthesis process of compound 6, add 5.1 g of M7 and 2.9 g of 4-(9H-carbazole-9-yl)phenylboronic acid to obtain 5.1 g of compound 167 as an off-white solid with a yield of 71%, HPLC content of 99%, and LC-MS molecular weight of 718.23.
[0133] The synthesis process of other compounds was completed by referring to compound 6, and the key reactants used are summarized in Tables 2 and 3.
[0134]
[0135]
[0136] (Note: Reactants A1~A 30 Sequentially react with intermediate M2 to generate compounds 1 to 30, reactants A1 to A 30 Sequentially react with intermediate M3 to generate compounds 31 to 60, reactants A1 to A 30 Sequentially react with intermediate M4 to generate compounds 61 to 90, reactants A1 to A 30 Sequentially react with intermediate M5 to generate compounds 91 to 120, reactants A1 to A 30 Sequentially react with intermediate M6 to generate compounds 121 to 150, reactants A1 to A 30The intermediate M7 reacts with the intermediate M7 to generate compounds 151 to 180. The reactants A1, A2, A9, and A 24 Sequentially react with intermediate M10 to generate compounds 213 to 216)
[0137]
[0138]
[0139]
[0140] (Note: Reactants B1~B 30 Sequentially react with intermediate M9 to generate compounds 180 to 210, reactant B 32 , B 33 Sequentially react with intermediate M8 to generate compound 211 and compound 212.)
[0141] like Figures 2 to 5 Shown are the NMR spectra of compound 6, compound 11, compound 69, and compound 167.
[0142] Based on the above 8H-dibenzoacridine derivatives 1 to 216, the preferred compounds are used as TADF materials (guest luminescent materials) in the test device samples. The basic structure and preparation method of the device adopt the device preparation process technology currently recognized by the industry. The device structure schematic diagram is shown in Figure 1 The specific introduction of the device is as follows:
[0143] The test device used in the experimental process includes five parts: an anode, a hole transport layer (HTL), an emitting layer (EML), an electron transport layer (ETL) and a cathode. Among them, one or more combinations of the above-mentioned preferred 8H-dibenzoacridine derivatives are used in the EML region to be used as a TADF material for the evaluation experimental process.
[0144] The specific device preparation is briefly described as follows:
[0145] Preferably, a substrate can be used below the first electrode or above the second electrode, and the substrate is ITO conductive glass with mechanical strength. In addition, the substrate used as a display can also be provided with thin film transistor (TFT) positive rows and a specific display image formed by the positive row combination.
[0146] Preferably, the organic layer includes a hole transport layer, a light-emitting layer and an electron transport layer, the hole transport layer is located between the anode and the light-emitting layer, and the electron transport layer is located between the cathode and the light-emitting layer. The light-emitting layer includes a host light-emitting material and a guest light-emitting material. The host light-emitting material is selected from one or a combination of at least two of PH-1, PH-2, PH-3, PH-4 and PH-5 with higher triplet energy, and the guest light-emitting material used in combination can be any one of the 8H-dibenzoacridine derivatives 1 to 216 of the present invention, and the host light-emitting material and the guest light-emitting material are matched at a mass ratio of 90:10.
[0147] Specifically, the anode can be made of transparent conductive oxide materials such as indium tin oxide (ITO), indium zinc oxide (IZO), tin dioxide (SnO2), zinc oxide (ZnO) and any combination thereof. The cathode can also be made of metals or alloys such as magnesium (Mg), silver (Ag), aluminum (Al), aluminum-lithium (Al-Li), calcium (Ca), magnesium-aluminum (Mg-Al), magnesium-silver (Mg_Ag) and their organic combinations.
[0148] The functional organic layer can be formed on the electrode by vacuum thermal evaporation, spin coating, printing and the like. The compound used as the organic layer can be organic small molecules, organic macromolecules and polymers, and combinations thereof.
[0149] The hole transport layer can be divided into a single-layer hole transport layer (HTL) and a composite hole transport layer. In order to simplify the device structure, the present invention selects hole transport layer materials HT-1,
[0150] Any one of HT-2 and HT-3 or a combination of at least two of them is used as a single-layer hole transport layer. The light-emitting layer is located between the hole transport layer and the electron transport layer. The main light-emitting material is selected from one of PH-1, PH-2, PH-3, PH-4 or PH-5 with higher triplet energy or a combination of at least two of them. The guest light-emitting material used in combination is selected from any one of the 8H-dibenzoacridine derivatives 1 to 216 of the present invention for matching test, and the main light-emitting material and the guest light-emitting material are composited in a mass ratio of 90:10. After the preparation of the above-mentioned functional layer for realizing organic light-emitting is completed, the electron transport material is continuously evaporated on the light-emitting layer. The electron transport material can be realized by one or more combinations of ET-1, ET-2 or ET-3 with excellent industry performance. After the electron transport material is evaporated, the electron injection material is evaporated, followed by sputtering of the metal cathode. Finally, the device is packaged using the industry-standard device packaging method. The samples used to test the device are prepared into 30mm×30mm samples, and then the luminescence performance indicators and device efficiency of the above samples are tested. Compared with conventional luminescent materials, the device luminescence performance and efficiency are better.
[0151] Device Comparison Examples 1 to 3:
[0152] The organic electroluminescent device was prepared by following the steps below:
[0153] Under high vacuum conditions, on the cleaned glass (conductive glass 1) substrate, 25nm thick indium tin oxide (anode 2) and 20nm thick MoO3 were sequentially deposited as hole injection layer 3, and 26nm thick HT-3 was deposited as hole transport layer 4. After the hole transport material was deposited, a 40nm thick light-emitting layer 5 was prepared, and its structure included PH-1 (Comparative Example 1) or PH-2 (Comparative Example 2) or PH-3 (Comparative Example 3) used in the OLED light-emitting layer as the main light-emitting material, and compound P4-33 in US11088330B2 was used as the guest light-emitting material, and the mass ratio of the two was 90:10. On the light-emitting layer, ET-3 was evaporated, and the vacuum-deposited film thickness of the material was 26nm, which was used as the electron transport layer 6. On the electron transport layer, a 16nm thick LiQ layer was prepared by a vacuum evaporation device, which was the electron injection layer 7. On the electron injection layer, a Mg-Al electrode layer with a thickness of 50 nm is made by vacuum evaporation equipment. This layer is the cathode layer (cathode 8). Finally, the test device is packaged after evaporation of the cover layer material to complete the test device preparation process. Figure 1 The device shown.
[0154] The detailed preparation scheme is as follows:
[0155] Comparative Example 1: Conductive glass / indium tin oxide (25nm) / MoO3 (20nm) / HT-3 (26nm) / PH-1:P4-33=90:10 (40nm) / ET-3 (26nm) / LiQ (16nm) / Mg-Al (50nm);
[0156] Comparative Example 2: Conductive glass / indium tin oxide (25nm) / MoO3 (20nm) / HT-3 (26nm) / PH-2:P4-33=90:10 (40nm) / ET-3 (26nm) / LiQ (16nm) / Mg-Al (50nm);
[0157] Comparative Example 3: Conductive glass / indium tin oxide (25nm) / MoO3 (20nm) / HT-3 (26nm) / PH-3:P4-33=90:10 (40nm) / ET-3 (26nm) / LiQ (16nm) / Mg-Al (50nm);
[0158] Examples of using the compound of the present invention as a doping material:
[0159] Device Examples 1 to 13:
[0160] The preparation method of device comparison example 1 was followed, except that the guest luminescent material p4-33 was replaced with the 8H-dibenzoacridine derivatives described in the present invention in sequence: compound 6, compound 19, compound 30, compound 36, compound 56, compound 74, compound 90, compound 96, compound 109, compound 120, compound 150, compound 175, and compound 205. The device test data are shown in Table 4.
[0161] The conventional materials used in the above device preparation process involve the following functional layer material structure:
[0162]
[0163]
[0164] US11088330B2 patent: Compound P4-33 Table 4 Device test data
[0165]
[0166]
[0167] (Note: SM is the abbreviation of compound)
[0168] As shown in Table 4, from the device test data, the test device prepared by using the preferred compound of the present invention as the TADF material is compared with the preferred luminescent material in the comparative document (US11088330B2 patent), the driving voltage is significantly reduced, the thermal stability is significantly improved, the service life is extended by nearly 50%, and the overall device efficiency is effectively improved; at the same time, under the condition of higher doping (10% doping rate), a relatively narrow half-peak width can be maintained, which will be beneficial to the high-definition display of OLED devices. It can be seen that the use of the preferred compound of the present invention as a TADF material plays a substantial role in improving the performance of the device, and has potential value for its promotion and application. The OLED device prepared by the preferred 8H-dibenzoacridine structure derivative of the present invention has a color coordinate in the range of yellow-green light to green light, which lays a certain foundation for the later research on OLED green light materials.
[0169] The color coordinates of the OLED device prepared from the preferred 8H-dibenzoacridine structure derivative of the present invention are in the range of yellow-green light to green light, which lays a certain foundation for the later research on OLED green light materials.
[0170] The present invention uses the main skeleton of 8H-dibenzoacridine molecule as a fixed core, and uses benzoxazole, pyrimidine, pyrazine, triazine, pteridine, benzothiazole, and phenanthroline as fixed substituents, and such substituents are conducive to electron transmission; at the same time, the main skeleton of 8H-dibenzoacridine molecule is conducive to hole transmission. The 8H-dibenzoacridine derivative of the present invention is used as a TADF material in the light-emitting layer of an OLED device, has excellent thermal stability and film stability, is conducive to the preparation of the device, and makes the OLED device more stable when working, significantly improves the luminous efficiency of the device, reduces the starting voltage and energy consumption, and prolongs the working life of the device.
[0171] The present invention uses 8H-dibenzoacridine structure as a fixed core, and uses benzoxazole, pyrimidine, pyrazine, triazine, pteridine, benzothiazole, benzoquinoxaline, etc. as fixed substituents (electron acceptor A). Such substituents have low reduction potentials, which are conducive to accepting electrons and thus facilitate electron transmission. At the same time, the main skeleton of the 8H-dibenzoacridine molecule (electron donor D) is conducive to hole transmission. Therefore, materials of this type of structure can be used as TADF materials.
[0172] The present invention uses 8H-dibenzoacridine structure as electron donor, and uses benzene, diphenyl and terphenyl as bridges to connect electron acceptors with different substituents. This structure is beneficial to reducing intermolecular stacking and aggregation quenching, thereby improving device stability.
[0173] The 8H-dibenzoacridine derivative described in the present invention is applied as a TADF material to the light-emitting layer of an OLED device, has excellent thermal stability and thin film stability, is beneficial to the preparation of the device, and at the same time significantly improves the luminous efficiency of the device, reduces the starting voltage and energy consumption, and improves the device service life and device stability.
[0174] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of ordinary technicians in this field without departing from the purpose of the present invention.
[0175] Many other changes and modifications may be made without departing from the concept and scope of the present invention.It should be understood that the present invention is not limited to the specific embodiments, and the scope of the present invention is defined by the appended claims.
Claims
1. An 8H-dibenzoacridine derivative, characterized in that: The general structural formula of the 8H-dibenzoacridine derivatives includes general formula 1: Where: n is an integer selected from 1, 2, and 3; Y1 is selected from H, C1-C8 alkyl, C1-C8 alkoxy; L is selected from C3~C 20 heteroaryl; Ar1, Ar2 are independently selected from H, deuterium, C1-C 30 Alkyl, C6~C 40 Substituted or unsubstituted aryl, C5~C 30 The substituted or unsubstituted substituent is selected from: C1 to C 10 Alkyl, C3~C 10 Cycloalkyl, C5~C 20 Heteroaryl, C6~C 20 One or more of aryl, dimethylamino, trimethylsilyl, triphenylsilyl, and morpholinyl; The heteroatoms in the heteroaryl group include O, S, N, P, B, and Si. The heteroaryl group includes a monocyclic heteroaryl group and a polycyclic heteroaryl group.
2. An 8H-dibenzoacridine derivative according to claim 1, characterized in that: The general formula 1 includes chemical formulas 1 to 8, and the specific structural formula is as follows: Where: n is an integer selected from 1, 2, and 3; Ar1, Ar2 are independently selected from H, deuterium, C1-C 30 Alkyl, C6~C 40 Substituted or unsubstituted aryl, C5~C 30 The substituted or unsubstituted substituent is selected from: C1 to C 10 Alkyl, C3~C 10 Cycloalkyl, C5~C 20 Heteroaryl, C6~C 20 One or more of aryl, dimethylamino, trimethylsilyl, triphenylsilyl, and morpholinyl; R1, R2 are independently selected from H, cyano, trifluoromethyl, C6-C 20 The aromatic group; The heteroatoms in the heteroaryl group include O, S, N, P, B, and Si. The heteroaryl group includes a monocyclic heteroaryl group and a polycyclic heteroaryl group.
3. An 8H-dibenzoacridine derivative according to any one of claims 1 and 2, characterized in that: The 8H-dibenzoacridine derivatives specifically include but are not limited to compounds 1 to 216, and the specific structural formula is:
4. An electroluminescent device comprising a cathode, an anode and an organic layer located between the cathode and the anode, characterized in that: The organic layer contains any one of the compounds 1 to 216 of the 8H-dibenzoacridine derivative according to claim 3.
5. The electroluminescent device according to claim 4, wherein the organic layer comprises a hole transport layer, a light emitting layer and an electron transport layer, wherein: The light-emitting layer comprises any one of compounds 1-216.
6. The electroluminescent device according to claim 5, wherein the light-emitting layer comprises a host light-emitting material and a guest light-emitting material, wherein: The host luminescent material is selected from The guest light-emitting material comprises any one of compounds 1 to 216, and the mass ratio of the host light-emitting material to the guest light-emitting material is in the range of 97:3 to 80:
20.
7. An electroluminescent device according to claim 6, characterized in that: The preferred mass ratio of the host luminescent material to the guest luminescent material is 90:10.
Citation Information
Cited By
Organic luminescent compound and organic electroluminescent device thereof
CN119661546A
Naphthalimide compound as well as preparation method and application thereof
CN119841809A