Nickel iron ammonium phosphate electrocatalyst as well as preparation method and application thereof

By using a hydrothermal method guided by aminated carbon nanotubes to synthesize nanoscale nickel iron ammonium phosphate electrocatalysts in the electrocatalytic oxygen evolution reaction, the problems of large-scale preparation and insufficient loading of existing OER catalysts have been solved, and high efficiency has been achieved. , stable electrocatalytic oxygen evolution reaction, and reduced production costs.

CN118756194APending Publication Date: 2024-10-11BEIJING UNIV OF CHEM TECH
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411038751.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing OER catalysts have difficulties in large-scale preparation and loading capacity, resulting in insufficient efficiency and stability in practical applications, and high costs, making it difficult to replace precious metal catalysts.

Method used

Aminated carbon nanotubes are used as conductive agents, and nanoscale nickel iron ammonium phosphate electrocatalysts are synthesized at lower temperatures through hydrothermal methods, and their excellent performance in electrocatalytic oxygen evolution reactions are used to improve the efficiency of electrolysis of water.

Benefits of technology

It achieves an efficient and stable electrocatalytic oxygen evolution reaction, reduces production costs, and finely controls the size and shape of nanoparticles by adjusting reaction conditions, improving the application potential of the material.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118756194A_ABST
    Figure CN118756194A_ABST
Patent Text Reader

Abstract

The invention discloses a nickel iron ammonium phosphate electrocatalyst and a preparation method and application thereof. The method comprises the following steps: mixing nickel salt, ferrous salt, phosphorus salt, a conductive agent and a pH regulator, adding a solvent, stirring and dissolving to obtain a mixed solution, then pouring the mixed solution into a reaction kettle, reacting at 160-200 DEG C for 4-8 hours, cooling to room temperature, centrifugally washing, and drying to obtain the composite material. Compared with preparation of a traditional solid-phase transition metal phosphate electrocatalyst, the preparation method has the advantages that the aminated carbon nanotubes are introduced, so that a conductive effect is achieved, reaction at a relatively low temperature is facilitated, and material sintering caused by high temperature is avoided. The synthesized nickel iron ammonium phosphate as a catalyst shows excellent catalytic performance and stability in the aspect of water electrolysis oxygen evolution, the water electrolysis efficiency is effectively improved, and strong support is provided for clean energy production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of inorganic nanomaterial synthesis and water electrolysis, and specifically relates to a high-activity ammonium nickel iron phosphate electrocatalyst and a preparation method thereof and application in electrocatalytic oxygen evolution. Background Art

[0002] Oxygen evolution (OER) is a key reaction in the water electrolysis process, which releases oxygen from water molecules through an electrochemical reaction at the anode. This process is an important step in hydrogen production because it is directly related to the efficiency of decomposing water into hydrogen and oxygen.

[0003] The water electrolysis process can be summarized as: Oxygen evolution reaction occurs at the anode (positive electrode) to produce oxygen: 2H2O→O2+4H + +4e - The cathode (negative electrode) undergoes hydrogen evolution reaction: 2H + +2e - →H2 The efficiency and stability of oxygen evolution by water electrolysis is one of the key challenges for its commercial application. During the water electrolysis process, the efficiency of OER directly affects the energy conversion efficiency and economy of the entire system. Therefore, the development of efficient and low-cost OER catalysts is a hot topic in scientific research. Ideal OER catalysts need to have low overpotential, high activity, excellent stability, and low cost and availability. Currently, common OER catalysts include precious metals such as iridium and ruthenium-based catalysts, but due to their high cost, researchers have been exploring more economical alternative materials.

[0004] The high-performance OER catalysts reported in existing literature or patents are mainly structured, that is, in-situ growth of catalysts on nickel foam, copper foam or carbon fiber paper. Although such catalysts have shown excellent performance, their biggest disadvantages are that they are difficult to prepare in large quantities and have low catalyst loading (the loading of most structured OER catalysts is ≤2 mg / cm 2 ), which seriously limits the practical application of this type of material. The biggest advantage of powder materials is that they can be scaled up for production and the catalyst loading per unit area can be increased through coating processes. Therefore, it is more urgent to explore a more efficient powder OER electrocatalyst. Summary of the invention

[0005] The present invention provides a green, simple and efficient method for preparing nano-sized ammonium nickel iron phosphate and applying the method to electrocatalytic oxygen evolution. Compared with the preparation of traditional solid-phase transition metal phosphate electrocatalysts, the present invention introduces amino carbon nanotubes, which not only play a conductive role, but also facilitate the reaction at a lower temperature, avoiding material sintering caused by high temperature. The synthesized ammonium nickel iron phosphate is used as a catalyst in the electrolysis of water for oxygen evolution and shows excellent catalytic performance and stability, effectively improving the efficiency of electrolysis of water and providing strong support for clean energy production.

[0006] The preparation method of the ammonium nickel iron phosphate electrocatalyst is as follows: nickel salt, ferrous salt, phosphate salt, conductive agent and pH regulator are mixed, a solvent is added, stirred and dissolved to obtain a mixed solution, and then poured into a reactor to react at 160-200°C for 4-8 hours, cooled to room temperature, centrifuged and washed, and dried to obtain the ammonium nickel iron phosphate electrocatalyst.

[0007] The nickel salt is selected from one or more of nickel phosphate, nickel nitrate, nickel chloride, nickel acetate and nickel sulfate.

[0008] The concentration of nickel ions in the mixed solution is 0.05 - 0.2 mol / L.

[0009] The ferrous salt is ferrous sulfate and / or ferrous nitrate.

[0010] The molar ratio of the ferrous salt to the nickel salt is 0.5-1.5.

[0011] The pH regulator is selected from one or more of urea, sodium hydroxide, potassium hydroxide, and hexamethylenetetramine.

[0012] The molar ratio of the pH regulator to the nickel salt is 3-5.

[0013] The pH value of the mixed solution is 8-10.

[0014] The conductive agent is amino-modified carbon nanotubes.

[0015] The concentration of the conductive agent in the mixed solution is 3-15 g / L.

[0016] The solvent is deionized water.

[0017] The phosphate salt is sodium hypophosphite.

[0018] Application of the ammonium nickel iron phosphate electrocatalyst prepared as above in electrocatalytic oxygen evolution reaction.

[0019] Beneficial effects of the present invention: (1) The preparation process is simple and controllable: The traditional high-temperature solid-phase reaction method has the disadvantages of high energy consumption, difficulty in temperature control, uneven phase purity and particle size distribution, and long reaction time; the chemical vapor deposition method has the disadvantages of high equipment cost, slow production speed, high temperature and specific gas precursors, and sometimes involving toxic gases; while the present invention only needs to dissolve nickel salt, ferrous salt, conductive agent, and pH adjuster in a common solvent, and react in a hydrothermal kettle to obtain nano-scale nickel iron ammonium phosphate powder. The present invention reacts at a lower temperature, the reaction conditions are mild, which is conducive to preserving sensitive components and is environmentally friendly; the present invention can also finely control the size and shape of nanoparticles by adjusting the reaction conditions.

[0020] (2) Excellent electrochemical stability: The prepared nano-sized ammonium nickel iron phosphate was applied to the electrocatalytic oxygen evolution reaction. -2 The voltage can be kept stable for 24 hours at a current density of , showing excellent electrocatalytic effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is the XRD pattern of ammonium nickel iron phosphate prepared in Example 1.

[0022] Figure 2 This is the SEM image of the ammonium nickel iron phosphate prepared in Example 1.

[0023] Figure 3 This is the XRD pattern of the material prepared in Comparative Example 1.

[0024] Figure 4 This is the XRD pattern of the material prepared in Comparative Example 2.

[0025] Figure 5 This is the LSV diagram of the ammonium nickel iron phosphate prepared in Application Example 1 during the electrocatalytic oxygen evolution process.

[0026] Figure 6 The prepared ammonium nickel iron phosphate in Application Example 1 was subjected to 100 mA·cm -2 Voltage-time diagram at current density of . DETAILED DESCRIPTION

[0027] Embodiment 1: Weigh 2.63 g nickel phosphate, 1.39 g ferrous sulfate, 4.59 g sodium hypophosphite, 2.7 g urea, and 0.5 g amino-modified multi-walled carbon nanotubes and place them in 80 mL deionized water. After magnetic stirring at room temperature for 20 minutes, pour the solution into a hydrothermal reactor, react at 180 °C for 6 hours, and then cool to room temperature. Wash with deionized water and anhydrous ethanol by centrifugation, and dry the precipitate in a 60 °C forced air oven for 12 hours to obtain ammonium nickel iron phosphate powder. Figure 1This is the XRD pattern of ammonium nickel iron phosphate. Figure 2 This is the SEM image of ammonium nickel iron phosphate. It can be seen from the figure that the obtained ammonium nickel iron phosphate is spherical and the particle size is about 180nm. Comparative Example 1:

[0028] In order to demonstrate the role of the aminated carbon nanotubes in the synthesis, in this comparative example, except for the absence of aminated carbon nanotubes, other reaction conditions were consistent with those in Example 1. Figure 3 The XRD diagram of the prepared sample and the sample prepared in Example 1 shows that the sample prepared in Comparative Example 1 does not show the characteristic diffraction peak of ammonium nickel iron phosphate, indicating that ammonium nickel iron phosphate is not formed. Through Example 1 and Comparative Example 1, it is proved that the amino carbon nanotubes play a key role in the formation of ammonium nickel iron phosphate. Comparative Example 2:

[0029] In order to demonstrate the role of the aminated carbon nanotubes in the synthesis, in this comparative example, except that non-aminated carbon nanotubes were added to replace the aminated carbon nanotubes, other reaction conditions were the same as those in Example 1.

[0030] 2.63 g nickel phosphate, 1.39 g ferrous sulfate, 4.59 g sodium hypophosphite, 2.7 g urea, and 0.5 g carbon nanotubes were weighed and placed in 80 mL deionized water. After magnetic stirring at room temperature for 20 minutes, the solution was poured into a hydrothermal reactor and reacted at 180 °C for 6 hours. After cooling to room temperature, the solution was washed by centrifugation with deionized water and anhydrous ethanol, and the precipitate was dried in a 60 °C forced air oven for 12 hours. Figure 4 The XRD patterns of the prepared samples and the samples prepared in Example 1 are shown in Table 1. Figure 4 It can be seen that the sample prepared in Comparative Example 2 does not show the characteristic diffraction peak of pure ammonium nickel iron phosphate, and the formed compound has a complex composition. Through Example 1 and Comparative Example 2, it is further proved that the amino carbon nanotubes play a key role in the formation of ammonium nickel iron phosphate. Application Example 1:

[0031] Weigh 0.01 g of ammonium nickel iron phosphate prepared in Example 1 and 0.001 g of conductive carbon black in a 3 mL centrifuge tube, and add 1.5 mL of anhydrous ethanol and 20 μL of Nafion to the centrifuge tube. After ultrasonication for 30 minutes, evenly drop it on a 3 cm × 3 cm carbon cloth and dry it in a 60 ° C blast oven. Cut a 1 cm × 1.5 cm carbon cloth as a working electrode, a Hg / HgO electrode as a reference electrode, and a graphite electrode as a counter electrode, and perform electrochemical testing in a 1 M KOH solution. Under the premise of 85% IR compensation, LSV test was performed in a voltage range of 0 V-1.6 V. Figure 5This is the LSV diagram of the nickel iron ammonium phosphate prepared in Example 1 during the electrocatalytic oxygen evolution process. -2 The stability test was carried out at a current density of 2.5 %. Figure 6 The nickel iron ammonium phosphate prepared in Example 1 is 100 mA·cm -2 Voltage-time diagram at current density of .

Claims

1. A method for preparing ammonium nickel iron phosphate electrocatalyst, characterized in that: The specific operation of the preparation method is: nickel salt, ferrous salt, phosphate salt, conductive agent, pH regulator are mixed, solvent is added to stir and dissolve to obtain a mixed solution, and then poured into a reactor to react at 160-200 ° C for 4-8 hours, cooled to room temperature, centrifuged and washed, and dried to obtain nickel iron ammonium phosphate electrocatalyst.

2. The preparation method according to claim 1, characterized in that: The nickel salt is selected from one or more of nickel phosphate, nickel nitrate, nickel chloride, nickel acetate, and nickel sulfate; the concentration of nickel ions in the mixed solution is 0.05-0.2 mol / L.

3. The preparation method according to claim 1, characterized in that: The ferrous salt is ferrous sulfate and / or ferrous nitrate; the molar ratio of the ferrous salt to the nickel salt is 0.5-1.

5.

4. The preparation method according to claim 1, characterized in that: The pH regulator is selected from one or more of urea, sodium hydroxide, potassium hydroxide, and hexamethylenetetramine.

5. The preparation method according to claim 1, characterized in that: The molar ratio of the pH regulator to the nickel salt is 3-5.

6. The preparation method according to claim 1, characterized in that: The pH value of the mixed solution is 8-10.

7. The preparation method according to claim 1, characterized in that: The conductive agent is amino carbon nanotubes; the concentration of the conductive agent in the mixed solution is 3-15 g / L.

8. The preparation method according to claim 1, characterized in that: The solvent is deionized water.

9. The preparation method according to claim 1, characterized in that: The phosphate salt is sodium hypophosphite.

10. Use of the ammonium nickel iron phosphate electrocatalyst prepared according to the method according to any one of claims 1 to 9 in electrocatalytic oxygen evolution reaction.

Citation Information

Cited By

  • Carbon nanotube loaded ferronickel phytate OER catalyst and preparation method thereof

    CN119733569A