Welding pool crystallization synchronization x-ray in-situ imaging characterization device and method
The welding pool crystallization synchronized X-ray in-situ imaging characterization device solves the problem of difficulty in observing the CET mechanism of welding pool solidification, enables high-resolution observation of the dynamic crystallization process of the welding pool, and improves the depth and depth of welding performance research. efficiency.
Patent Information
- Application Number
- CN202410754679.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-12
- Publication Date
- 2024-10-11
AI Technical Summary
It is difficult to observe and understand the Columnarto EquiaxedTransition (CET) mechanism during the solidification process of the welding pool with the existing technology, causing the mechanical properties and service performance of the weld to be affected.
A device for synchronous X-ray in-situ imaging characterization of welding pool crystallization was designed, including an X-ray transmission channel, a synchronous X-ray generator, a shutter, a glassy carbon plate, a scintillator, an objective lens and a high-speed camera. Select appropriate scintillator materials to achieve high-resolution observation of the dynamic crystallization process in the weld pool.
It provides detailed observation of the dynamic evolution of the microstructure of the welding pool, fills the gap in the field of in-situ observation of grain growth, and is of great significance. It provides new ideas for studying the welding CET mechanism and simplifies the operation process.
Smart Images

Figure CN118758979A_ABST
Abstract
Description
Technical field:
[0001] The invention relates to the field of welding molten pool solidification and in-situ synchronous X-ray imaging characterization, and in particular to a welding molten pool crystallization synchronous X-ray in-situ imaging characterization device and method. Background technology:
[0002] After the solidification process of the welding molten pool, the columnar crystal structure pointing from the edge of the molten pool to the center will be formed after the crystallization occurs. When the columnar crystal grows close to the center of the molten pool, the equiaxed crystal in the center of the molten pool will mechanically block the columnar crystal to prevent it from continuing to grow. This process of transformation from columnar crystal to equiaxed crystal during the solidification process of the molten pool is called Columnarto Equiaxed Transition, or CET for short. When there are a large number of long and thick columnar crystals in the structure, it will lead to problems such as high sensitivity to crystallization cracks, high degree of element segregation, and extremely uneven chemical composition, which will seriously affect the mechanical properties and performance of the weld. It is generally believed that by promoting the CET process of molten pool solidification, the formation of long and thick columnar crystals can be effectively avoided, and a large number of fine equiaxed grains can be nucleated, which is conducive to grain refinement and grain boundary strengthening. At the same time, the sensitivity to crystallization cracks is reduced, and the purpose of improving performance is finally achieved. A full understanding of the CET mechanism of welding molten pool solidification is the basis for formulating measures to promote the CET process of molten pool solidification, refine the structure, and improve the comprehensive mechanical properties.
[0003] However, the solidification of the welding molten pool has the characteristics of overheating (average temperature can reach 1870℃), fast cooling rate (average value can reach 100℃ / s), large temperature gradient (generally 10 higher than casting 4 Due to the characteristics of large size and small molten pool volume, it is difficult to observe the molten pool crystallization process using conventional experimental methods, which brings great difficulties to revealing the CET mechanism of welding molten pool solidification.
[0004] Since X-rays have the dual nature of wave and particle, when X-rays penetrate an object, their amplitude and phase will change. The interaction between materials and X-rays can be described by the complex refractive index. Combined with matching information processing methods (software and equipment), it is possible to use X-rays to complete microscopic dynamic in-situ imaging of some specific objects, and synchrotron radiation X-rays have the advantages of high energy, high brightness, high resolution and good monochromaticity. Therefore, this field urgently needs a synchrotron X-ray in-situ imaging characterization device for the crystallization process of the welding molten pool, which can provide an effective way for the experimental observation of the dynamic crystallization process of the welding molten pool, and is of great significance to the study of the welding CET mechanism. Summary of the invention:
[0005] The purpose of the present invention is to provide a device and method for in-situ imaging characterization of weld pool crystallization by synchronous X-ray, so as to solve the problem that the existing conventional methods cannot observe the dynamic crystallization process of weld pool, and achieve the technical goal of observing and understanding the CET mechanism of weld pool solidification.
[0006] A synchronous X-ray in-situ imaging characterization device for a welding molten pool crystallization process, comprising
[0007] X-ray transmission channel;
[0008] and a synchronous X-ray generating device, a shutter, a glass carbon plate, a scintillator, an objective lens, and a high-speed camera which are sequentially arranged on the center line of the X-ray transmission channel;
[0009] Setting the welding equipment to correspond to the workpiece placed between the glassy carbon plates;
[0010] All components are coupled and connected with the X-ray light transmission channel as the central axis.
[0011] Furthermore, the x-ray light transmission channel is a cylindrical light transmission channel, and the high-energy x-rays generated by the synchronous x-ray generating device enter the in-situ characterization device from the front end of the light transmission channel, and the shutter clamps are mounted on the upper and lower sides of the light transmission channel.
[0012] Furthermore, a substrate is provided at the bottom of the device, and two glass carbon plates are fixed on the substrate, and their length directions are adjusted to be parallel to each other, perpendicular to the light transmission channel, and the midpoint is located in the light transmission channel;
[0013] Furthermore, the spacing between the glass carbon plates can be adjusted within a range of 0.5-2 mm.
[0014] Furthermore, a small gantry device is installed on both sides of the substrate parallel to the light-transmitting channel. The interior of the gantry column is hollow, and a travel track of the welding gun of the welding equipment is arranged in the crossbeam at the top of the gantry, so as to facilitate the translation of the clamping device of the welding gun in this direction, thereby driving the translation of the welding gun;
[0015] A stepper motor is fixed on the outer wall of one side of the gantry column. The stepper motor is connected to the clamping device through a wire to control the movement of the welding gun. The wire is placed in the hollow column of the gantry.
[0016] The welding gun of the welding equipment is fixed on the clamping device, and the rest of the parts including the welding power supply are placed in the gantry column on the other side. The control panel is placed on the outside to facilitate the adjustment of welding parameters.
[0017] Welding equipment has basic welding components, including welding gun, protector, and welding power source.
[0018] Furthermore, the light transmission channel needs to pass through the scintillator, the objective lens and the high-speed camera, which are assembled and matched, with the objective lens receiving the X-rays in front to improve the quality of the rays, and then transmitting them to the high-speed camera;
[0019] A CMOS high-speed camera was selected for high-speed imaging and placed at the end of the entire device to record imaging information. The distance between the high-speed camera and the sample was controlled at 17 cm.
[0020] Furthermore, the entire device is encapsulated in a metal shell, leaving four free interactive windows, one for switching welding guns, one for adjusting welding parameters, one for controlling the stepper motor, and one for replacing the scintillator material; in addition, a light inlet is provided at one end of the device and a data output port is provided at the other end.
[0021] A synchronous X-ray in-situ imaging characterization test method for a welding molten pool crystallization process comprises the following steps:
[0022] Step 1: Prepare multiple groups of welding specimens with different thicknesses;
[0023] Step 2: Grind and clean the surface of the sample to be welded. After completion, fix the sample to be welded in the device with a glass carbon plate and move it to the target position;
[0024] Step 3: Start all devices to gain power control.
[0025] Step 4: Select a suitable welding gun, install it firmly and stably on the fixture, and adjust the welding parameters;
[0026] Step 5: Select the energy of the synchrotron radiation X-ray according to the material of the sample to be welded, and replace the scintillator that matches the material properties;
[0027] Step 6: Control the clamping, adjust the upper and lower positions of the welding gun, and move it to the target position;
[0028] Step 7: Use the stepper motor to preset the welding gun's travel trajectory and travel speed;
[0029] Step 8: Adjust the temporal and spatial resolution of the high-speed camera device;
[0030] Step 9: Start the synchrotron radiation X-ray generator, and after the optical path is stable, start the welding power supply to start welding.
[0031] Compared with the prior art, the present invention has the following advantages:
[0032] 1) The present invention combines synchrotron radiation X-rays to dynamically observe the microstructure, providing a new idea for the analysis of the microstructure evolution of the molten pool during the welding process.
[0033] 2) The present invention can use a variety of methods to carry out welding experiments, which fills the gap in the field of in-situ observation of grain growth and is of great significance to the study of welding CET mechanism.
[0034] 3) The present invention is easy to operate. It only needs to adjust the welding method, welding parameters, workpiece size, and scintillator material of the in-situ characterization device to achieve in-situ imaging observation of the dynamic crystallization process of the welding molten pool. Description of the drawings:
[0035] Figure 1 Schematic diagram of the structural principle of the in-situ characterization device for dynamic crystallization of welding molten pool under synchrotron X-ray radiation.
[0036] Figure 2 It is a two-dimensional plan view schematic diagram of the side view structure of the characterization device.
[0037] Figure 3 It is a two-dimensional plan view schematic diagram of the front view structure of the characterization device;
[0038] The reference numerals are: synchronous X-ray generator-1, shutter-2, glass carbon plate-3, workpiece-4, stepper motor-5, travel track-6, small gantry-7, clamping-8, welding equipment-9, scintillator-10, objective lens-11, high-speed camera-12, substrate-13. (The transparent column is the light transmission channel of X-rays).
[0039] Figure 4 It is a schematic diagram of the macroscopic melt flow of the macroscopic welding pool captured by high-speed photography, where Figure a is a schematic diagram of the underwater arc welding pool; Figure b is a schematic diagram of the arc welding pool in an air environment.
[0040] Figure 5 It is a schematic diagram of the microscopic dynamic crystallization of the welding molten pool under high-speed photography, where Figure a is a schematic diagram of dendrite growth; Figure b is a schematic diagram of dendrite melting and fragmentation; Figure c is a schematic diagram of the movement of broken dendrites under the action of flow field. Specific implementation method:
[0041] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below, but it is not intended to limit the present invention. The present invention covers any substitution, modification, equivalent method and scheme made on the essence and scope of the present invention as defined by the claims. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0042] A synchronous X-ray in-situ imaging characterization device for a welding molten pool crystallization process, comprising
[0043] X-ray transmission channel;
[0044] and a synchronous X-ray generating device, a shutter, a glass carbon plate, a scintillator, an objective lens, and a high-speed camera which are sequentially arranged on the center line of the X-ray transmission channel;
[0045] Setting the welding equipment to correspond to the workpiece placed between the glassy carbon plates;
[0046] All components are coupled and connected with the X-ray light transmission channel as the central axis.
[0047] Furthermore, the x-ray light transmission channel is a cylindrical light transmission channel, and the high-energy x-rays generated by the synchronous x-ray generating device enter the in-situ characterization device from the front end of the light transmission channel, and the shutter clamps are mounted on the upper and lower sides of the light transmission channel.
[0048] A substrate is provided at the bottom of the device, and two glass carbon plates are fixed on the top of the substrate. The length directions are adjusted to be parallel to each other, perpendicular to the light transmission channel and the midpoint is located in the light transmission channel; the spacing of the glass carbon plates can be adjusted, and the adjustment range is 0.5-2mm. A small gantry device is installed on both sides of the substrate parallel to the light transmission channel. The interior of the gantry column is hollow, and the travel track of the welding gun of the welding equipment is arranged in the crossbeam at the top of the gantry, which is convenient for the translation of the clamping device of the welding gun in this direction, thereby driving the translation of the welding gun; a stepper motor is fixed on the outer wall of one side of the gantry column, and the stepper motor is connected to the clamping device through a wire to control the movement of the welding gun, and the wire is placed in the hollow gantry column; the welding gun of the welding equipment is fixed on the clamping device, and the rest of the parts including the welding power supply are placed in the gantry column on the other side, and the control panel is placed on the outside to facilitate the regulation of welding parameters; the welding equipment has basic welding components, including a welding gun, a protector, and a welding power supply. The light transmission channel needs to pass through the scintillator, the objective lens and the high-speed camera, and the two are assembled and matched. The objective lens first receives X-rays in front to improve the quality of the rays, and then transmits them to the high-speed camera. A CMOS high-speed camera is selected for high-speed video recording and placed at the end of the entire device to record imaging information. The distance between the high-speed camera and the sample is controlled at 17 cm. The entire device is encapsulated in a metal shell, leaving four free interactive windows, one for switching welding guns, one for adjusting welding parameters, one for controlling stepper motors, and one for replacing scintillator materials; in addition, a light inlet is provided at one end of the device and a data output port is provided at the other end.
[0049] A synchronous X-ray in-situ imaging characterization test method for a welding molten pool crystallization process, the welding molten pool crystallization in-situ characterization method comprising the following steps:
[0050] Step 1: Prepare multiple groups of welding specimens with different thicknesses;
[0051] Step 2: Grind and clean the surface of the sample to be welded. After completion, fix the sample to be welded in the device with a glass carbon plate and move it to the target position;
[0052] Step 3: Start all devices to gain power control.
[0053] Step 4: Select a suitable welding gun, install it firmly and stably on the fixture, and adjust the welding parameters;
[0054] Step 5: Select the energy of the synchrotron radiation X-ray according to the material of the sample to be welded, and replace the scintillator that matches the material properties;
[0055] Step 6: Control the clamping, adjust the upper and lower positions of the welding gun, and move it to the target position;
[0056] Step 7: Use the stepper motor to preset the welding gun's travel trajectory and travel speed;
[0057] Step 8: Adjust the temporal and spatial resolution of the high-speed camera device;
[0058] Step 9: Start the synchrotron radiation X-ray generator, and after the optical path is stable, start the welding power supply to start welding.
[0059] Furthermore, the synchronous X-ray generator needs to be initially set to emit monochromatic energy X-rays.
[0060] Furthermore, the size of the welding experiment workpiece sample is controlled to be 20mm*7mm (length*height), and the width can be adjusted according to the needs of the actual welding process. The width is the thickness in the X-ray transmission direction; the workpiece welding surface needs to be ground and polished before the experiment to ensure that it is clean and free of impurities;
[0061] Furthermore, the glass carbon plate is used to encapsulate the workpiece, with a size of 30mm*10mm*0.5mm (length*height*width), to ensure that the workpiece is clamped and fixed during the experiment, that is, the workpiece will not swing or move down during the entire welding process. The main component of the glass carbon plate is SiO2. In order not to affect the transmission of imaging information, the composition of the glass carbon plate must be uniform and free of defects (such as pores, impurity particles, etc.).
[0062] The thickness of the scintillator is 0.25mm, which converts the X-rays carrying the workpiece information into visible light and focuses it. The choice of scintillator depends on the material properties of the experimental workpiece. For example, single crystal cadmium tungstate is selected for Al-Cu alloy, and LuAG:Ce is selected for Al-Si alloy.
[0063] Furthermore, the welding equipment is adapted to select tungsten inert gas arc welding or laser welding, and is fixed above the workpiece by a small gantry device to control the height of the welding gun so that the welding operation is performed on the upper surface of the workpiece. The stepper motor on the side controls the movement of the welding gun along the set track during the experiment.
[0064] The shutter is composed of a fast shutter and a slow shutter, which controls the X-ray exposure time, protects the detector, and ultimately makes the received synchronous X-ray energy more stable and concentrated.
[0065] The objective lens is used to receive visible light, improve the quality of the converted light, and facilitate the collection of the next step of information. The CMOS high-speed camera is placed at the end of the entire device to record imaging information and control its spatial resolution and time resolution. This enables the entire process of dynamic crystallization of the molten pool to be clearly obtained within the minimum amount of data information.
[0066] The synchrotron X-ray generator is provided by the Shanghai Synchrotron Radiation Source Center, and the beamline is BL13HB-X-ray Imaging and Biomedical Applications Beamline, which is used to generate single or multiple beams of synchrotron X-rays with specific required energy, which can be selected within a wide spectral range.
[0067] Example 1
[0068] The sample material is Al-Cu alloy, in which the Al content is 85% and the Cu content is 15%. The sample is a rectangular solid with a size of 20mm*7mm (length*height) and a density of 7.5g / cm 3 , the welding method is selected as tungsten inert gas welding.
[0069] Step 1: Prepare multiple sets of welding specimens with different thicknesses, ranging from 0.5 to 2 mm;
[0070] Step 2: Pre-treat the workpiece to be welded, grind the surface of the workpiece to be welded with an angle grinder, and then clean the surface with 95% industrial alcohol to remove oil stains and rust. After the pre-treatment is completed, fix the sample to be welded with a glass carbon plate at the specified position of the light transmission channel of the device;
[0071] Step 3: Ensure that the welding machine and each adjustment device are firmly and stably installed, and that the movement or rotation of each adjustment device in the up and down, left and right directions can be performed normally. Start all equipment to obtain power control.
[0072] Step 4: Select a tungsten inert gas welding gun, firmly and stably install it on the chuck, and adjust the welding parameters, including current and voltage;
[0073] Step 5: Since the material of the sample to be welded is Al-Cu alloy, the monochromatic energy mode of the synchrotron radiation X-ray is selected, and 0.25 mm single crystal cadmium tungstate is selected as the scintillator;
[0074] Step 6: Control the chuck to adjust the up and down position of the welding gun and move it to the target position;
[0075] Step 7: Use the stepper motor to preset the welding gun's travel trajectory (welding direction) and travel speed along the length direction;
[0076] Step 8: Adjust the time and space resolution of the high-speed camera device, control its space resolution to 5.5 / pixel and frame rate to 30fps;
[0077] Step 9: Start the synchrotron radiation X-ray generator, and after the optical path is stable, start the welding power supply to start welding.
[0078] Step 10: Use high-speed video to collect dynamic crystallization imaging information of the molten pool during the entire welding process. Select different resolutions according to different experimental requirements to obtain dynamic in-situ characterization at different scales. The flow of the molten metal inside the molten pool during welding can be observed at the macroscopic scale, such as Figure 4 ; The dynamic crystallization process inside the molten pool during welding can be observed at the microscopic scale;
[0079] Subsequently, the information collection and recording of the entire crystallization process in the welding pool was completed, including solid-liquid interface instability, co-crystallization, competitive growth, CET, etc., with an emphasis on recording CET process data such as dendrite melting, equiaxed crystal nucleation, solid grain movement, collision, aggregation and growth.
[0080] After processing multiple sets of experimental data, it was found that when the Al-Cu alloy sample was 1mm thick and the high-speed camera controlled its spatial resolution to 5.5 / pixel and the frame rate to 30fps, the entire process of dynamic crystallization of the molten pool was clearly obtained within the minimum amount of data information.
[0081] Although the preferred embodiments of the present invention have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.
[0082] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the design concept of the present invention should be included in the protection scope of the present invention.
Claims
1. A synchronous X-ray in-situ imaging characterization device for welding molten pool crystallization, It is characterized in that include X-ray light transmission channel; and a synchronous X-ray generating device, a shutter, a glass carbon plate, a scintillator, an objective lens, and a high-speed camera which are sequentially arranged on the center line of the X-ray transmission channel; Setting the welding equipment to correspond to the workpiece placed between the glassy carbon plates; All components are coupled and connected with the X-ray light transmission channel as the central axis.
2. The synchronous X-ray in-situ imaging characterization device for welding molten pool crystallization according to claim 1, It is characterized in that The x-ray light transmission channel is a cylindrical light transmission channel. The high-energy x-rays generated by the synchronous x-ray generating device enter the in-situ characterization device from the front end of the light transmission channel. The shutter clamps are mounted on the upper and lower sides of the light transmission channel.
3. The synchronous X-ray in-situ imaging characterization device for welding molten pool crystallization according to claim 1, It is characterized in that A substrate is provided at the bottom of the device, and two glass carbon plates are fixed on the substrate, and their length directions are adjusted to be parallel to each other, perpendicular to the light transmission channel, and the midpoint is located in the light transmission channel; The spacing between the glass carbon plates can be adjusted within a range of 0.5-2mm.
4. The synchronous X-ray in-situ imaging characterization device for welding molten pool crystallization according to claim 1, It is characterized in that Small gantry devices are installed on both sides of the substrate parallel to the light-transmitting channel. The interior of the gantry column is hollow. The travel track of the welding gun of the welding equipment is arranged in the crossbeam at the top of the gantry, which facilitates the translation of the clamping device of the welding gun in this direction, thereby driving the translation of the welding gun; A stepper motor is fixed on the outer wall of one side of the gantry column. The stepper motor is connected to the clamping device through a wire to control the movement of the welding gun. The wire is placed in the hollow column of the gantry. The welding gun of the welding equipment is fixed on the clamping device, and the rest of the parts including the welding power supply are placed in the gantry column on the other side. The control panel is placed on the outside to facilitate the adjustment of welding parameters. The welding equipment has basic welding components, including a welding gun, a protector, and a welding power source.
5. The synchronous X-ray in-situ imaging characterization device for welding molten pool crystallization according to claim 1, It is characterized in that The light transmission channel needs to pass through the scintillator, objective lens and high-speed camera. The two are assembled and matched. The objective lens receives the X-rays in front to improve the quality of the rays, and then transmits them to the high-speed camera. A CMOS high-speed camera was selected for high-speed imaging and placed at the end of the entire device to record imaging information. The distance between the high-speed camera and the sample was controlled at 17 cm.
6. The synchronous X-ray in-situ imaging characterization device for welding molten pool crystallization according to claim 1, It is characterized in that The entire device is encapsulated in a metal shell, leaving four free interactive windows, one for switching welding guns, one for adjusting welding parameters, one for controlling the stepper motor, and one for replacing the scintillator material; in addition, a light inlet is provided at one end of the device and a data output port is provided at the other end.
7. A synchronous X-ray in-situ imaging characterization test method for the crystallization process of the welding molten pool. It is characterized in that The welding molten pool crystallization in-situ imaging characterization test method is carried out using the welding molten pool crystallization synchronous X-ray in-situ imaging characterization device according to any one of claims 1 to 8; The in-situ characterization method for welding molten pool crystallization comprises the following steps: Step 1: Prepare multiple groups of welding specimens with different thicknesses; Step 2: Grind and clean the surface of the sample to be welded. After completion, fix the sample to be welded in the device with a glass carbon plate and move it to the target position; Step 3: Start all devices to obtain power control; Step 4: Select a suitable welding gun, install it firmly and stably on the fixture, and adjust the welding parameters; Step 5: Select the energy of the synchrotron radiation X-ray according to the material of the sample to be welded, and replace the scintillator that matches the material properties; Step 6: Control the clamping, adjust the upper and lower positions of the welding gun, and move it to the target position; Step 7: Use the stepper motor to preset the welding gun's travel trajectory and travel speed; Step 8: Adjust the temporal and spatial resolution of the high-speed camera device; Step 9: Start the synchrotron radiation X-ray generator, and after the optical path is stable, start the welding power supply to start welding.
8. The synchronous X-ray in-situ imaging characterization test method for the crystallization process of the welding molten pool according to claim 7, It is characterized in that The synchronous X-ray generating device needs to be initially set to emit monochromatic energy X-rays.
9. The synchronous X-ray in-situ imaging characterization test method for the crystallization process of the welding molten pool according to claim 7, It is characterized in that The sample size of the welding workpiece in the welding experiment is controlled to be 20mm*7mm in length*height. The width can be adjusted according to the needs of the actual welding process. The width is the thickness in the X-ray transmission direction. The welding surface of the workpiece needs to be ground and polished before the experiment to ensure that it is clean and free of impurities. The size of the glass carbon plate is controlled at 30mm*10mm*0.5mm in length*height*width to ensure the clamping and fixation of the workpiece during the experiment. The composition is SiO 2 ; The scintillator has a thickness of 0.25 mm and its area needs to be larger than the area of the light-transmitting channel to ensure that all X-rays are converted into visible light.
10. The synchronous X-ray in-situ imaging characterization test method for the crystallization process of the welding molten pool according to claim 7, It is characterized in that Tungsten inert gas welding or laser welding is selected for welding equipment adaptation. It is fixed above the workpiece through a small gantry device to control the height of the welding gun so that the welding gun can perform welding operations on the upper surface of the workpiece. The stepper motor on the side controls the movement of the welding gun along the set track during the experiment.