Etching uniformity detection and judgment method

By combining graphic design with a three-dimensional measuring instrument, the problem of large data volume and high limitations in etching uniformity testing is solved, accurate measurement and evaluation of different design line widths and spacings is achieved, and production efficiency and product quality are improved.

CN118765040APending Publication Date: 2024-10-11AKM ELECTRONICS TECH SUZHOU
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202410842191.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-27
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

The existing technology has the problems of large data volume, cumbersome processing, and high limitations in etching uniformity detection. It cannot effectively evaluate the line width and spacing of different designs, and the measurement accuracy is insufficient, especially for testing fine lines.

Method used

Using a method that combines graphic design with a three-dimensional measuring instrument, after going through the process of film application, exposure, development, etching, and film removal, a three-dimensional measuring instrument is used to measure line width and line spacing, calculate the line width distribution map, screen out abnormal points, and adjust parameters. Provide compensation recommendations.

Benefits of technology

It improves the measurement accuracy and efficiency, can quickly determine abnormal areas, comprehensively evaluate etching uniformity, significantly improves production efficiency and product quality, especially the control of fine lines is more precise.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118765040A_ABST
    Figure CN118765040A_ABST
Patent Text Reader

Abstract

The invention relates to an etching uniformity detection and judgment method. The etching uniformity detection and judgment method comprises the following steps: S1, selecting a copper-clad plate meeting conditions as a to-be-detected plate; step S2, pretreatment: carrying out pretreatment on the to-be-tested plate; s3, pattern transfer: attaching a dry film to the to-be-tested plate, exposing and developing the to-be-tested plate, and forming an anti-corrosion layer pattern on the to-be-tested plate; step S3, etching: etching the non-circuit pattern under a specified etching parameter; s4, a film removing step: removing the dry film on the etched to-be-tested board, and forming a circuit pattern on the left copper surface; and S5, a measuring step: measuring the line width and the line distance of the line pattern through a three-dimensional measuring instrument. According to the method, the measurement accuracy and the measurement efficiency are improved, the etching uniformity is rapidly judged through the method of combining the graphic design and the three-dimensional measurement instrument, proper adjustment suggestions are provided according to results, and the method has the advantages of being high in speed, large in data size and small in deviation and can truly reflect the actual levels of different design line widths.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of PCB manufacturing, and in particular to a method for detecting and judging etching uniformity. Background Art

[0002] In the manufacturing process of printed circuit boards (PCBs), etching technology is crucial and has a direct impact on the quality and performance of products. Etching uniformity is a key indicator in the etching process and is directly related to the accuracy and stability of PCB circuits. Detecting etching uniformity is an important step to ensure product quality and performance, because uneven etching may lead to problems such as unstable electrical performance, reduced reliability, insufficient accuracy, and low production efficiency. Therefore, detecting etching uniformity is not only a key step to ensure product quality, but also an important means to improve production efficiency and reduce production costs. At present, vacuum two-fluid etching technology is a new method to improve etching uniformity. It provides a more uniform etching effect, higher etching speed and accuracy by simultaneously ejecting a mixture of gas and liquid for etching. However, even with this advanced technology, the detection and adjustment of etching uniformity is still indispensable to ensure the stability of product quality and performance. At present, copper thickness measurement is one of the commonly used etching uniformity evaluation methods, which evaluates etching uniformity by measuring the thickness of the copper layer in different areas of the copper clad laminate. Usually, instruments such as CMI (Copper Micro-etch Instrument) are used to perform multi-point measurements on the copper clad laminate to obtain copper layer thickness data.

[0003] However, this method has several major disadvantages. 1. Large amount of data and cumbersome processing: It is necessary to measure multiple locations (121), which results in large amount of data and complex processing, increasing the workload and time cost. 2. High limitations: It can only reflect the distribution of copper layer thickness of the entire plate, and cannot evaluate the line width and spacing of actual lines of different designs, resulting in incomplete evaluation.

[0004] In addition, the disclosed Chinese patent CN110719697A provides a PCB etching uniformity detection and adjustment method, which proposes to use AOI (automatic optical inspection) to measure the line width of the anti-corrosion layer pattern with different line directions to determine the etching uniformity. However, this method has the following disadvantages: 1. Single line width and spacing design: It cannot reflect the etching conditions of different types of line widths and spacings, and it is difficult to fully evaluate the etching uniformity. Moreover, the surface copper used in the above two methods is greater than 1OZ, that is, the line width designed by this method is relatively large, and it is impossible to evaluate the test results of fine lines; 2. AOI measurement data limitations: the amount of data is small, and it cannot be exported to Excel for further analysis, and there is a large optical deviation (±10%), so the accuracy of the measurement results cannot be guaranteed. Summary of the invention

[0005] To this end, the technical problem to be solved by the present invention is to overcome the deficiencies in the prior art, provide an etching uniformity detection and judgment method, solve the key problem of etching uniformity detection in the manufacturing process of printed circuit boards (PCBs), and aim at the shortcomings of the existing copper thickness measurement method, such as large data volume, cumbersome processing, and high limitations. Through a method combining graphic design with a three-dimensional measuring instrument, rapid judgment of etching uniformity is achieved, and appropriate adjustment suggestions are provided based on the results. After the board to be tested undergoes the film pre-treatment, film pasting, exposure, development, etching, and film removal processes, circuits with different line width spacings are obtained, and the line width and line spacing of different design units are measured by a three-dimensional measuring instrument to obtain the line width spacing of different circuit designs. By comparing the line width changes of the same unit design at different positions, the etching uniformity differences in different areas can be clearly evaluated.

[0006] In order to solve the above technical problems, the present invention provides an etching uniformity detection and judgment method, comprising:

[0007] Step S1, a material cutting step, selecting a copper clad laminate that meets the conditions as a board to be tested;

[0008] Step S2, a pre-processing step, pre-processing the board to be tested;

[0009] Step S3, a pattern transfer step, attaching a dry film to the board to be tested, exposing and developing the board to be tested, and forming a resist layer pattern on the board to be tested;

[0010] Step S3, etching step, etching the non-circuit pattern under specified etching parameters;

[0011] Step S4, a film removal step, removing the dry film on the board to be tested after etching, and the remaining copper surface forms a circuit pattern;

[0012] Step S5, a measuring step, measuring the line width and line spacing of the circuit pattern by a three-dimensional measuring instrument;

[0013] Step S6, data collection and processing step, collecting the measurement data of the line width and line spacing, screening outliers, calculating the line width and line spacing of different design units in different arrays, and obtaining a line width distribution diagram;

[0014] Step S7, analysis and adjustment step, adjusting the parameters of the etching step according to the line width distribution diagram, and then testing again.

[0015] In one embodiment of the present invention, in step S3, etching is performed by spraying, and the etching speed is 2-5.6 m / min.

[0016] In one embodiment of the present invention, in step S6, the average value, range and standard deviation of multiple groups of different line width data are calculated to obtain the optimal compensation amount.

[0017] In one embodiment of the present invention, in the step S2, the pre-treatment step includes S21, removing oxides and impurities on the copper surface of the board to be tested, and roughening the copper surface of the board to be tested.

[0018] In one embodiment of the present invention, the pre-treatment step further includes step S22, wherein the dry film is attached to the surface of the test board by a film attaching machine, the film attaching temperature is 100-120°C, the film attaching speed is 2m / min, and the film attaching pressure is 3.5kg / cm2.

[0019] In one embodiment of the present invention, the pre-processing step further includes step S23, transferring the pattern to the board to be tested by an exposure machine.

[0020] In one embodiment of the present invention, in step S6, 4 sets of line width and spacing in the unit are measured, and the measurement starts from the unit with a compensation of 8. Each array can obtain 91 sets of line width and spacing, and 6 arrays are measured.

[0021] In one embodiment of the present invention, in step S7, the method for adjusting the etching step includes adjusting the pressure value of the upper nozzle, the pressure value of the lower spray pressure, the spray position and distance of the upper spray of the compensation etching section, and the spray position and distance of the lower spray of the compensation etching section.

[0022] In one embodiment of the present invention, in the step S4, the dry film is stripped off by using NaOH film stripping solution.

[0023] In one embodiment of the present invention, the surface copper thickness of the copper clad laminate is less than or equal to 18 microns.

[0024] The above technical solution of the present invention has the following advantages compared with the prior art:

[0025] The present invention discloses an etching uniformity detection and judgment method, wherein a copper clad laminate to be tested is selected as a test board, and after the board to be tested undergoes film pre-treatment, film pasting, exposure, development, etching, and film removal processes, circuits with different line widths and spacings are obtained, and then a three-dimensional measuring instrument is used to measure the line widths and line spacings of different design units to obtain the line width spacings of different circuit designs. By comparing the line width changes of the same unit design at different positions, the etching uniformity differences in different areas can be clearly evaluated.

[0026] In addition, the present invention improves the measurement accuracy and efficiency. The measurement using a three-dimensional measuring instrument has the advantages of fast speed, large data volume (1000 sets of data can be provided in 10 minutes), and small deviation (the measurement of a high-power camera is more accurate), and can truly reflect the actual level of different design line widths. This efficient and accurate measurement method significantly improves the measurement efficiency and accuracy.

[0027] In addition, the present invention can quickly judge the abnormal area. Through the line width change curve, the abnormal area can be quickly judged. The multi-PITCH multi-compensation design can avoid abnormal processing caused by single-point problems and ensure that the overall etching uniformity evaluation is more comprehensive and accurate.

[0028] Furthermore, the present invention can also improve production efficiency and reduce waste. For a stable etching line, if an abnormality occurs, by comparing the line width change curve each time, it is possible to quickly determine which area block has a problem; it can give early warning reminders for the production process of fine lines, increase the probability of the first qualified piece in the production process, significantly improve production efficiency, and reduce waste.

[0029] Furthermore, the present invention can also improve the control of line width accuracy. Specifically, by designing resist patterns for different line compensations, the actual level of line width can be accurately detected. For any new dry film and line design, by adjusting the etching speed, the method can quickly give the best compensation interval and etching parameters, thereby effectively improving production efficiency and product quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] In order to make the content of the present invention more clearly understood, the present invention is further described in detail below according to specific embodiments of the present invention in conjunction with the accompanying drawings, wherein:

[0031] Figure 1 It is a fine line of different pitches of an Array in the Panel.

[0032] Figure 2 It is a diagram of a Panel that contains multiple Arrays.

[0033] Figure 3 It is a flowchart of a preferred embodiment of the present invention.

[0034] Figure 4 It is a line width distribution diagram measured with different compensations in a specific embodiment.

[0035] Figure 5 is a line width distribution diagram obtained by measuring different compensations in another specific embodiment. DETAILED DESCRIPTION

[0036] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments so that those skilled in the art can better understand the present invention and implement it, but the embodiments are not intended to limit the present invention.

[0037] Embodiment 1

[0038] Reference Figure 1 as well as Figure 2 As shown, firstly, LDI (Laser Direct Imaging) data is used to design fine lines of different pitches, including but not limited to designs with pitches of 50, 60, and 70 microns. In designs with different pitches, the graphics in the unit are designed in straight lines, and different units have different line compensations, which start from 0 and increase by 2 microns until the upper limit of the resolution is reached.

[0039] The present invention discloses a method for detecting and judging etching uniformity, combining Figure 3 As shown, the method includes:

[0040] Step S1, a material cutting step, selecting a copper clad laminate that meets the conditions as a board to be tested;

[0041] Step S2, a pre-processing step, pre-processing the board to be tested;

[0042] Step S3, pattern transfer step, first, a dry film is attached to the surface of the board to be tested, the board to be tested is exposed, and the pattern is transferred to the side board using 33MJ energy; then, development is performed to remove the unexposed dry film and leave the photosensitive part, thereby forming a resist layer pattern on the board to be tested;

[0043] Step S3, etching step, under specified etching parameters, using etching liquid to etch the copper surface of the non-circuit pattern part. Since the copper surface located under the dry film is not in contact with the etching liquid, it will not be etched. The etching parameters include but are not limited to etching pressure and etching speed.

[0044] Step S4, a film removal step, removing the dry film on the board to be tested after etching, so that the remaining copper surface forms a circuit pattern;

[0045] Step S5, a measuring step, measuring the line width and line spacing of the circuit pattern by a three-dimensional measuring instrument;

[0046] Step S6, data collection and processing step, collecting the measurement data of the line width and line spacing, screening outliers, calculating the line width and line spacing of different design units in different arrays, and obtaining a line width distribution diagram;

[0047] Step S7, analysis and adjustment step, adjusting the etching step according to the line width distribution diagram, and then testing again.

[0048] It can be known from this that the etching uniformity detection and judgment method to be protected by the present invention selects the copper clad board to be tested as the test board, and obtains lines with different line widths and spacings after the board to be tested undergoes film pre-treatment, film pasting, exposure, development, etching, and film removal processes, and then uses a three-dimensional measuring instrument to measure the line width and line spacing of different design units to obtain the line width spacing of different circuit designs. By comparing the line width changes of the same unit design at different positions, the etching uniformity differences in different areas can be clearly evaluated.

[0049] In addition, the present invention improves the measurement accuracy and efficiency. The measurement using a three-dimensional measuring instrument has the advantages of fast speed, large data volume (1000 sets of data can be provided in 10 minutes), and small deviation (the measurement of a high-power camera is more accurate), and can truly reflect the actual level of different design line widths. This efficient and accurate measurement method significantly improves the measurement efficiency and accuracy.

[0050] In addition, the present invention can quickly judge the abnormal area. Through the line width change curve, the abnormal area can be quickly judged. The multi-PITCH multi-compensation design can avoid abnormal processing caused by single-point problems and ensure that the overall etching uniformity evaluation is more comprehensive and accurate.

[0051] Furthermore, the present invention can also improve production efficiency and reduce waste. For a stable etching line, if an abnormality occurs, by comparing the line width change curve each time, it is possible to quickly determine which area block has a problem; it can give early warning reminders for the production process of fine lines, increase the probability of the first qualified piece in the production process, significantly improve production efficiency, and reduce waste.

[0052] Furthermore, the present invention can also improve the control of line width accuracy. Specifically, by designing resist patterns for different line compensations, the actual level of line width can be accurately detected. For any new dry film and line design, by adjusting the etching speed, the method can quickly give the best compensation interval and etching parameters, thereby effectively improving production efficiency and product quality.

[0053] In the step S3, etching is performed by spraying, and the etching speed is 2-5.6 m / min. As a preferred embodiment, the etching speed is 4.5 m / min.

[0054] In step S6, the average value, range and standard deviation of multiple groups of different line width data are calculated to obtain the optimal compensation amount.

[0055] Furthermore, in the step S2, the pre-treatment step includes S21, removing oxides and impurities on the copper surface of the board to be tested, and roughening the copper surface of the board to be tested.

[0056] Furthermore, the pre-treatment step also includes step S22, attaching the dry film on the surface of the test board by a film sticking machine, with a film sticking temperature of 100-120°C, a film sticking speed of 2m / min, and a film sticking pressure of 3.5kg / cm2.

[0057] In detail, the pre-processing step also includes step S23, transferring the pattern to the board to be tested by an exposure machine.

[0058] As a preferred implementation, in step S6, 4 sets of line width and spacing in the unit are measured, and the measurement starts from the unit with a compensation of 8. Each array can obtain 91 sets of line width and spacing, and 6 arrays are measured.

[0059] In step S7, the method for adjusting the etching step includes adjusting the pressure value of the upper nozzle, the pressure value of the lower spray pressure, the spray position and distance of the upper spray of the compensation etching section, and the spray position and distance of the lower spray of the compensation etching section.

[0060] In the step S4, the dry film is stripped off by using NaOH film stripping solution.

[0061] As a preferred implementation, the surface copper thickness of the copper clad laminate is less than or equal to 18 microns.

[0062] A specific implementation method is introduced below.

[0063] 1. Cutting: Select copper-clad laminate with surface copper of 12 microns and size of 510*610mm as the board to be tested; 2. Pretreatment: remove oxides, grease, and impurities on the copper surface and roughen the copper surface;

[0064] 3. Film laminating: The temperature of the film laminating machine is 115℃, the speed is 2m / min, and the pressure is 3.5kg / cm 2 Next, apply XX-1215 dry film;

[0065] 4. Exposure: Use 33MJ energy to transfer the pattern to the copper-clad board (exposure scale 11 grids);

[0066] 5. Remove the unexposed dry film and leave the photosensitive part;

[0067] 6. Etching: At an etching speed of 4.5 m / min, the etching solution etches away the copper surface of the non-circuit pattern part, while the copper under the dry film cannot be etched;

[0068] 7. Film removal: After the dry film is stripped off with NaOH film removal solution, the remaining copper forms a circuit;

[0069] 8. Line width and spacing measurement: Use a 3D measuring instrument to measure the 4 sets of line width and spacing in the unit. The measurement starts from the unit with a compensation of 8. Each array can obtain 91 sets of line width and spacing, and a total of 6 arrays are measured;

[0070] 9. Data collection and processing: Since the measured line width spacing is fixed in the PITCH value, abnormal points in the process can be quickly screened. Use EXCEL to calculate the line width spacing of different design units in different ARRAYs, taking the design of 35 / 35 (pitch 70, compensation 18 microns) as an example:

[0071] Average value (T surface, compensation 18 microns) = 36.63 microns, range (T surface, compensation 18 microns) = 4.47 microns, standard deviation (T surface, compensation 18 microns) = 1.71 microns,

[0072] Average value (B surface, compensation 18 microns) = 32.61 microns, range (B surface, compensation 18 microns) = 2.03 microns, standard deviation (B surface, compensation 18 microns) = 0.71 microns; From the measurement results, it can be seen that: the best compensation of 35 / 35 design is about 18±2 microns; there are differences in the etching amount of TB surface; compared with B surface, the line width range and standard deviation of T surface are larger;

[0073] 10. Combine Figure 4 As shown, Figure 4 It is the line width distribution diagram measured with different compensations. The trend lines on both sides show an increasing trend. ARRAY 1, 5, and 7 are in the board-entering direction, and ARRAY 8, 11, and 14 are in the board-outgoing direction. It can be clearly seen that: a. The etching amount in the board-entering direction is too large; b. The etching amount on the left side, i.e., Array 1 and 8, is too large; the etching amount on the cT surface is too large.

[0074] Adjustment: Adjust the spraying position and distance of the etching liquid on the compensation etching section, adjust the nozzles 1 and 8 into the board to 50mm, spray 50mm, adjust the nozzles 2-7 into the board to 60mm, spray 420mm; increase the nozzle pressure on the right side by 0.02MPa / time, and check whether the nozzle on the right side is blocked; during the etching process, increase the lower spray pressure by 0.02MPA / time, and conduct a secondary test.

[0075] In another specific embodiment,

[0076] 1. Cutting: Choose copper clad laminate with surface copper of 15 microns and size of 510*610mm;

[0077] 2. Pretreatment: remove oxides, grease, impurities on the copper surface and roughen the copper surface;

[0078] 3. Film laminating: The temperature of the film laminating machine is 115℃, the speed is 2m / min, and the pressure is 3.5kg / cm 2 Next, apply XX-1215 dry film;

[0079] 4. Exposure: Use 33MJ energy to transfer the pattern to the copper-clad board (exposure scale 11 grids);

[0080] 5. Development: remove the unexposed dry film and leave the photosensitive part;

[0081] 6. Etching: At an etching speed of 3.5 m / min, the etching solution etches away the copper surface of the non-circuit pattern part, while the copper under the dry film cannot be etched;

[0082] 7. Film removal: After the dry film is stripped off with NaOH film removal solution, the remaining copper forms a circuit;

[0083] 8. Line width and spacing measurement: Use a 3D measuring instrument to measure the 4 sets of line width and spacing in the unit. The measurement starts from the unit with a compensation of 8. Each array can obtain 91 sets of line width and spacing, and a total of 6 arrays are measured;

[0084] 9. Data collection and processing: Since the measured line width spacing has a fixed PITCH value, abnormal points in the process can be quickly screened. Figure 3 The 35 / 35 compensation 24 design can be screened out. Use EXCEL to calculate the line width spacing of different design units in different ARRAYs. Take the 35 / 35 (pitch 70 microns, compensation 18 microns) design as an example. The average value (T surface, compensation 18 microns) = 37.54 microns, the range (T surface, compensation 18 microns) = 1.80 microns, the standard deviation (T surface, compensation 18 microns) = 0.71 microns, the average value (B surface, compensation 18 microns) = 32.60 microns, the range (B surface, compensation 18 microns) = 1.10 microns, the standard deviation (B surface, compensation 18 microns) = 0.36 microns; From the above set of measurement results, it can be seen that the best compensation for the 35 / 35 design is about 18±2 microns; there are differences in the etching amount of the TB surface.

[0085] 10. Analysis and adjustment, combined Figure 5 Come and see, Figure 5 It is the line width distribution diagram measured with different compensations. The trend lines on both sides are relatively flat, and the T-side line width is slightly higher than the B-side line width. Adjustment: fine-tune the lower spray pressure by 0.02MPa and conduct a second test.

[0086] It should be noted that the line PITCH diversity: the line PITCH in UNIT includes but is not limited to 25 / 25 micron, 30 / 30 micron, 35 / 35 micron, and may also include 20 / 20 micron, 40 / 40 micron, etc., which can be adjusted according to the factory's capabilities;

[0087] Diversity of graphic design: UNIT graphics include but are not limited to straight lines such as circular lines, horizontal lines, vertical lines, and oblique lines;

[0088] High-density ARRAY: In the above embodiment, there are only 14 arrays. In actual production, the number of arrays is not limited to 14. The increased number of ARRAYs improves the accuracy of data collection.

[0089] Flexibility of copper thickness on copper clad boards: The copper thickness of copper clad boards can be any thickness below 18 microns, and the appropriate pitch can be selected according to the thickness. Generally speaking, the thinner the copper surface, the higher the level of the circuit that can be etched, and the more data will be collected;

[0090] Figure 3 and Figure 4 Just taking the 35 / 35 design as an example, in fact, in order to better reflect the distribution situation, it is necessary to combine the line width distribution diagrams of all designs. At the same time, the different pitch designs in the graph can be replaced with one design, so that a more accurate line width distribution curve can be drawn.

[0091] The three-dimensional measuring instrument has the characteristics of fast measuring speed and small error. For example, it only takes 10 minutes to measure 1,000 data.

[0092] The line width distribution diagrams with different compensations mentioned in the present invention can quickly screen out abnormal points according to the measured line width range.

[0093] The dry film involved in the present invention has a resolution of 8 / 8 microns, so it can etch 25 / 25 microns when the surface copper is 12 microns, so that a 25 / 25 micron line width distribution diagram can be drawn. When using a dry film with poor resolution or thick surface copper, it is necessary to focus on the line width distribution diagram of high PITCH.

[0094] In the description of the embodiments of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "setting" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0095] In the description of the present invention, it should be understood that the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0096] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium; it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0097] Obviously, the above embodiments are merely examples for the purpose of clear explanation and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the present invention.

Claims

1. A method for detecting and judging etching uniformity, characterized in that: include: Step S1, a material cutting step, selecting a copper clad laminate that meets the conditions as a board to be tested; Step S2, a pre-processing step, pre-processing the board to be tested; Step S3, a pattern transfer step, attaching a dry film to the board to be tested, exposing and developing the board to be tested, and forming a resist layer pattern on the board to be tested; Step S3, etching step, etching the non-circuit pattern under specified etching parameters; Step S4, a film removal step, removing the dry film on the board to be tested after etching, and the remaining copper surface forms a circuit pattern; Step S5, a measuring step, measuring the line width and line spacing of the circuit pattern by a three-dimensional measuring instrument; Step S6, data collection and processing step, collecting the measurement data of the line width and line spacing, screening outliers, calculating the line width and line spacing of different design units in different arrays, and obtaining a line width distribution diagram; Step S7, analysis and adjustment step, adjusting the parameters of the etching step according to the line width distribution diagram, and then testing again.

2. The etching uniformity detection and judgment method according to claim 1, characterized in that: In the step S3, etching is performed by spraying, and the etching speed is 2-5.6 m / min.

3. The etching uniformity detection and judgment method according to claim 1, characterized in that: In step S6, the average value, range and standard deviation of multiple groups of different line width data are calculated to obtain the optimal compensation amount.

4. The etching uniformity detection and judgment method according to claim 1, characterized in that: In the step S2, the pre-treatment step includes S21, removing oxides and impurities on the copper surface of the board to be tested, and roughening the copper surface of the board to be tested.

5. The etching uniformity detection and judgment method according to claim 4, characterized in that: The pre-treatment step also includes step S22, attaching the dry film on the surface of the test board by a film sticking machine, with a film sticking temperature of 100-120° C., a film sticking speed of 2 m / min, and a film sticking pressure of 3.5 kg / cm 2 .

6. The etching uniformity detection and judgment method according to claim 5, characterized in that: The pre-processing step also includes step S23, transferring the pattern to the board to be tested by an exposure machine.

7. The etching uniformity detection and judgment method according to claim 1, characterized in that: In step S6, 4 sets of line width and spacing are measured in the unit, and the measurement starts from the unit with a compensation of 8. Each array can obtain 91 sets of line width and spacing, and 6 arrays are measured.

8. The etching uniformity detection and judgment method according to claim 1, characterized in that: In step S7, the method for adjusting the etching step includes adjusting the pressure value of the upper nozzle, the pressure value of the lower spray pressure, the spray position and distance of the upper spray of the compensation etching section, and the spray position and distance of the lower spray of the compensation etching section.

9. The etching uniformity detection and judgment method according to claim 1, characterized in that: In the step S4, the dry film is stripped off by using NaOH film stripping solution.

10. The etching uniformity detection and judgment method according to claim 1, characterized in that: The surface copper thickness of the copper clad laminate is less than or equal to 18 microns.

Citation Information

Cited By

  • Simplified test method for etching uniformity

    CN120141385A

  • Wet etching equipment and metal mask

    CN121295182A