Quartz product grinding method
By adopting multi-step methods of rough grinding, semi-fine grinding and fine grinding, spray cooling lubricant and ultrasonic vibration technology in the grinding of quartz products, the problems of low grinding efficiency and difficulty in ensuring surface quality are solved, and efficient quartz products are achieved. Product grinding.
Patent Information
- Application Number
- CN202410818185.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-24
- Publication Date
- 2024-10-15
AI Technical Summary
Existing quartz product grinding technology has problems such as low grinding efficiency and difficulty in ensuring surface quality, especially when using ordinary three-axis machining centers, copper-bonded grinding heads and oily cutting fluids.
The three-step grinding method of rough grinding, semi-finishing grinding and fine grinding is adopted, using roughing grinding head, semi-finishing grinding head and finishing grinding head respectively, and spraying grinding fluid containing coolant and lubricant during the grinding process. Cutting fluid, combined with ultrasonic vibration technology, optimizes grinding speed and axial, radial, and deep hole grinding methods.
It effectively improves the grinding efficiency, ensures the flatness and smoothness of the quartz product surface, reduces thermal damage, and achieves efficient processing of double-sided grinding.
Smart Images

Figure CN118769034A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a semiconductor processing technology, and more particularly to a quartz product grinding method. Background Art
[0002] With the continuous development of semiconductor technology, quartz products are increasingly used, and higher requirements are placed on the quality of quartz products. At present, when grinding quartz products, ordinary three-axis machining centers, copper-bonded grinding heads, oily cutting fluids, and spindles with too low linear speeds are used to grind products or deep holes, resulting in low grinding efficiency and difficulty in ensuring surface quality. Summary of the invention
[0003] In order to overcome the above-mentioned shortcomings, the present invention provides a quartz product grinding method, which can effectively improve the grinding efficiency and ensure the flatness and smoothness of the surface of the quartz product after grinding.
[0004] In order to solve the above technical problems, the present invention adopts the following technical solutions: a quartz product grinding method, comprising the following steps: S1, loading the quartz product onto a workbench; S2, rough grinding, grinding the surface of the quartz product with a rough grinding head; S3, semi-finishing grinding, grinding the surface of the quartz product with a semi-finishing grinding head; S4, fine grinding, grinding the surface of the quartz product with a fine grinding head; S5, unloading the quartz product to complete the grinding process.
[0005] When the quartz product is ground, it is loaded on the workbench for positioning. The grinding process is divided into three steps: rough grinding, semi-finishing grinding, and fine grinding. In these three steps, the rough grinding head, semi-finishing grinding head, and fine grinding head are used to perform the grinding operation. Using different grinding head distributions for grinding is conducive to improving the grinding effect and ensuring the flatness and smoothness of the surface of the quartz product after grinding.
[0006] The quartz product grinding method disclosed in this patent application can effectively improve the grinding efficiency while ensuring the flatness and smoothness of the surface of the quartz product after grinding.
[0007] Preferably, grinding fluid is sprayed toward the grinding position during the process from S2 to S4.
[0008] During the grinding process, spraying grinding fluid onto the grinding position plays a role in heat dissipation, reducing thermal damage to the surface of the quartz product, and taking away the grinding chips, which is beneficial to improving the grinding effect and grinding efficiency.
[0009] Preferably, the grinding fluid contains a coolant and a lubricant.
[0010] The grinding fluid includes coolant and lubricant. The coolant has good heat dissipation effect, and the lubricant is beneficial to improve the lubrication performance of the grinding fluid, avoiding excessive friction between the grinding head and the surface of the quartz product during the grinding process, which may cause damage to the surface of the quartz product.
[0011] Preferably, the coolant comprises cerium oxide abrasive, deionized water and hydrogen peroxide, wherein the concentration of cerium oxide abrasive is 7-12wt%, the concentration of hydrogen peroxide is 5-9wt%, and the rest is deionized water.
[0012] The composition of the coolant is set reasonably. Cerium oxide abrasive has a very high polishing efficiency, which can quickly remove stains and defects on the surface of quartz products, reducing polishing time and cost. Cerium oxide abrasive has good chemical and physical stability and will not decompose or produce pollution during the polishing process. Hydrogen peroxide plays an oxidative corrosion role, grinding the surface of quartz products.
[0013] Preferably, during the processes S2 to S4, the roughing grinding head, semi-finishing grinding head and finishing grinding head are successively connected to the ultrasonic vibration main shaft, and the ultrasonic vibration main shaft rotates and generates vibration to achieve rough grinding, semi-finishing grinding and finishing grinding of the quartz product.
[0014] Ultrasonic assisted grinding technology is used to promote effective contact between abrasive particles and the surface of quartz products through the micro-impact and micro-friction generated by ultrasonic vibration, thereby improving grinding efficiency. Ultrasonic equipment uses a built-in ultrasonic system integrated with the grinder, including a transducer, an amplifier rod, a tool head, and an ultrasonic spring collet chuck. By applying a certain vibration frequency to the grinding head, the surface of the workpiece is crushed, and the grinding head can easily remove the material.
[0015] Preferably, the vibration frequency of the ultrasonic vibration main shaft is 20 kHz to 50 kHz.
[0016] The vibration frequency of 20 kHz to 50kHz has a good effect on crushing the surface of quartz products.
[0017] Preferably, the binder used for the roughing grinding head is silver, and the binder used for the semi-finishing grinding head and the finishing grinding head is resin.
[0018] Diamond itself is self-sharpening, and the use of silver binder can improve the wear resistance and processing efficiency of the rough machining grinding head and reduce processing costs. The binder of the fine machining grinding head is resin, and the tool bar is made of carbide steel. It is completed on an ultra-precision lathe to ensure concentricity and circular runout with the grinding head.
[0019] Preferably, the grinding methods in processes S2 to S4 are divided into axial grinding, radial grinding, and deep hole grinding, with the axial grinding speed Vc=800~1150 m / min, the radial grinding speed Vc=400~600 m / min, and the deep hole grinding speed Vc=55~120 m / min.
[0020] Vc represents the linear speed of the grinding wheel. Different grinding speeds are used for different grinding methods to ensure the grinding effect.
[0021] Preferably, after S1, a dial indicator is installed on the spindle, the dial indicator contact is fitted to the side wall of the quartz product, and the spindle is rotated and moved and adjusted along the X and Y directions until the display of the dial indicator is stable and there is no jump. At this time, the spindle and the quartz product are in a coaxial state.
[0022] In many cases, the grinding of quartz products needs to ensure that it is coaxial with the grinding head. The circular runout of the side wall of the quartz product is measured by a dial indicator to determine whether the two are concentric. The judgment is accurate and reliable.
[0023] Preferably, a lifting suction cup and a flipping suction cup are provided on the workbench. In S1, the quartz product is first loaded on the lifting suction cup, and the lifting suction cup adsorbs and positions the quartz product. After the upper surface of the quartz product completes the processing of steps S2 to S4, the flipping suction cup flips to the top of the quartz product and adsorbs the upper surface of the quartz product. Thereafter, the lifting suction cup removes the adsorption effect on the quartz product and moves downward. The flipping suction cup flips 180 degrees, and the lower surface of the quartz product is processed by steps S2 to S4.
[0024] The quartz product can be double-sided ground by loading it once, which is beneficial to improve the grinding efficiency.
[0025] Compared with the prior art, the beneficial effects of the present invention are: (1) The quartz product grinding method of the patent application can effectively improve the grinding efficiency, while ensuring the flatness and smoothness of the surface of the quartz product after grinding; (2) During the grinding process, the grinding fluid sprayed toward the grinding position plays a heat dissipation role, reduces the thermal damage to the surface of the quartz product, and takes away the grinding chips, which is beneficial to improving the grinding effect and improving the grinding efficiency; (3) The ultrasonic assisted grinding technology is adopted, and the micro-impact and micro-friction generated by ultrasonic vibration promote the effective contact between the abrasive particles and the surface of the quartz product, thereby improving the grinding efficiency; (4) Double-sided grinding of quartz products can be achieved with one loading, which is beneficial to improving the grinding efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a grinding schematic diagram of the present invention.
[0027] Figure 2 Schematic diagram of the vacuum suction cup of Example 1 of the present invention.
[0028] Figure 3 Schematic diagram of the vacuum suction cup of embodiment 2 of the present invention.
[0029] Figure 4 Schematic diagram of the vacuum suction cup of Example 3 of the present invention.
[0030] In the figure: 1. quartz product, 2. workbench, 3. transducer, 4. amplifier rod, 5. tool head, 6. vacuum suction cup, 7. vacuum adsorption hole, 8. ring groove, 9. closing ring, 10. adsorption surface, 11. centering piston cylinder, 12. ball head, 13. lifting suction cup, 14. flip suction cup, 15. lifting correction piston cylinder, 16. lifting correction column, 17. lifting correction hole, 18. lifting piston cylinder, 19. support plate, 20. flip correction piston cylinder, 21. flip correction column, 22. flip correction hole, 23. rotating shaft, 24. rib plate. DETAILED DESCRIPTION
[0031] The technical solution of the present invention is further described in detail below through specific embodiments and in conjunction with the accompanying drawings: Embodiment 1: A method for grinding a quartz product (see attached Figure 1 , Attachment Figure 2 ), including the following steps: S1, loading the quartz product 1 onto the workbench 2; S2, rough grinding, using a rough grinding head to grind the surface of the quartz product 1; the rough grinding head is installed on the main shaft of the grinder, and the main shaft rotates so that the rough grinding head and the surface of the quartz product 1 are in contact with each other for grinding; S3, semi-finishing grinding, using a semi-finishing grinding head to grind the surface of the quartz product 1; the semi-finishing grinding head is installed on the main shaft of the grinder, and the main shaft rotates so that the semi-finishing grinding head and the surface of the quartz product 1 are in contact with each other for grinding; S4, fine grinding, using a fine grinding head to grind the surface of the quartz product 1; the fine grinding head is installed on the main shaft of the grinder, and the main shaft rotates so that the fine grinding head and the surface of the quartz product 1 are in contact with each other for grinding; S5, unloading the quartz product 1, and completing the grinding process.
[0032] The binder used for the roughing grinding head is silver, which binds the diamond abrasives together to form a roughing grinding head. The binder used for the semi-finishing grinding head and the finishing grinding head is resin, which binds the diamond abrasives together to form a semi-finishing grinding head and a finishing grinding head. The abrasive grains of the roughing grinding head, semi-finishing grinding head, and finishing grinding head are #170, #400, and #800 respectively.
[0033] During the grinding process, the quartz product 1 is loaded on the workbench 2 for positioning. The grinding process is divided into three steps: rough grinding, semi-finishing grinding, and fine grinding. In these three steps, a rough grinding head, a semi-finishing grinding head, and a fine grinding head are used to perform the grinding operation. Using different grinding head distributions for grinding is conducive to improving the grinding effect and ensuring the flatness and smoothness of the surface of the quartz product 1 after grinding.
[0034] During S2 to S4, a grinding fluid is sprayed toward the grinding position, and the grinding fluid contains a coolant and a lubricant. The ratio of the coolant to the lubricant is (20-30):1, and in this embodiment, the ratio of the coolant to the lubricant is 24:1. The coolant composition includes cerium oxide abrasive, deionized water and hydrogen peroxide, wherein the concentration of the cerium oxide abrasive is 7-12wt%, the concentration of the hydrogen peroxide is 5-9wt%, and the rest is deionized water.
[0035] During the grinding process, spraying grinding fluid onto the grinding position plays a role in heat dissipation, reduces thermal damage to the surface of the quartz product 1, and takes away the grinding chips, which is beneficial to improving the grinding effect and grinding efficiency. The grinding fluid includes coolant and lubricant. The coolant has a good heat dissipation effect, and the lubricant is beneficial to improving the lubrication performance of the grinding fluid, avoiding excessive friction between the grinding head and the surface of the quartz product 1 during the grinding process, which may cause damage to the surface of the quartz product 1. The composition of the coolant is reasonably set, and the cerium oxide abrasive has a very high polishing efficiency, which can quickly remove stains and defects on the surface of the quartz product 1, reducing polishing time and cost. Cerium oxide abrasive has good chemical stability and physical stability, and will not decompose or produce pollution during the polishing process. Hydrogen peroxide plays a role in oxidative corrosion, grinding the surface of the quartz product 1.
[0036] In the process from S2 to S4, the roughing grinding head, the semi-finishing grinding head and the finishing grinding head are successively connected to the ultrasonic vibration main shaft, and the ultrasonic vibration main shaft rotates and generates vibration to realize the rough grinding, semi-finishing grinding and finishing grinding of the quartz product 1. The vibration frequency of the ultrasonic vibration main shaft is 20 kHz to 50kHz.
[0037] Ultrasonic assisted grinding technology is used to promote effective contact between abrasive particles and the surface of the quartz product 1 through the micro-impact and micro-friction generated by ultrasonic vibration, thereby improving grinding efficiency. The ultrasonic equipment uses a built-in ultrasonic system integrated with the grinder, including a transducer 3, an amplifier rod 4, a tool head 5, and an ultrasonic spring collet chuck. By applying a certain vibration frequency to the grinding head, the surface of the workpiece is crushed, and the grinding head can easily remove the material.
[0038] The grinding methods in the process from S2 to S4 are divided into axial grinding, radial grinding, and deep hole grinding. The axial grinding speed Vc=800~1150 m / min, the radial grinding speed Vc=400~600 m / min, and the deep hole grinding speed Vc=55~120 m / min. Vc represents the linear speed of the grinding wheel. Different grinding speeds are used for different grinding methods to ensure the grinding effect.
[0039] In S1, the quartz product 1 is loaded onto the vacuum suction cup 6 on the workbench 2. The vacuum suction cup 6 is provided with a plurality of circles of vacuum adsorption holes 7. An annular groove 8 is provided on the lower surface of the vacuum suction cup 6 and corresponds to each circle of vacuum adsorption holes 7. The open end of the annular groove 8 is connected to a closed ring 9, and the annular groove 8 is connected to a vacuum pipeline. The vacuum adsorption holes 7 at the corresponding positions are selected according to the different sizes of the quartz products 1. The annular groove 8 corresponding to the vacuum adsorption holes 7 is connected to the vacuum pipeline to form a negative pressure, thereby realizing the vacuum adsorption positioning of the quartz product 1.
[0040] After S1, a dial indicator is installed on the spindle, and the dial indicator contact is attached to the side wall of the quartz product 1. The spindle rotates and moves along the X and Y directions until the dial indicator display is stable and there is no jump. At this time, the spindle and the quartz product 1 are in a coaxial state. In many cases, the grinding of the quartz product 1 needs to ensure that it is coaxial with the grinding head. The circular runout of the side wall of the quartz product 1 is measured by the dial indicator to determine whether the two are concentric, and the judgment is accurate and reliable.
[0041] Embodiment 2: A method for grinding a quartz product (see attached Figure 1 , Attachment Figure 3 ), including the following steps: S1, loading the quartz product 1 onto the workbench 2; S2, rough grinding, using a rough grinding head to grind the surface of the quartz product 1; the rough grinding head is installed on the main shaft of the grinder, and the main shaft rotates so that the rough grinding head and the surface of the quartz product 1 are in contact with each other for grinding; S3, semi-finishing grinding, using a semi-finishing grinding head to grind the surface of the quartz product 1; the semi-finishing grinding head is installed on the main shaft of the grinder, and the main shaft rotates so that the semi-finishing grinding head and the surface of the quartz product 1 are in contact with each other for grinding; S4, fine grinding, using a fine grinding head to grind the surface of the quartz product 1; the fine grinding head is installed on the main shaft of the grinder, and the main shaft rotates so that the fine grinding head and the surface of the quartz product 1 are in contact with each other for grinding; S5, unloading the quartz product 1, and completing the grinding process.
[0042] The binder used for the roughing grinding head is silver, which binds the diamond abrasives together to form a roughing grinding head. The binder used for the semi-finishing grinding head and the finishing grinding head is resin, which binds the diamond abrasives together to form a semi-finishing grinding head and a finishing grinding head. The abrasive grains of the roughing grinding head, semi-finishing grinding head, and finishing grinding head are #170, #400, and #800 respectively.
[0043] During the grinding process, the quartz product 1 is loaded on the workbench 2 for positioning. The grinding process is divided into three steps: rough grinding, semi-finishing grinding, and fine grinding. In these three steps, a rough grinding head, a semi-finishing grinding head, and a fine grinding head are used to perform the grinding operation. Using different grinding head distributions for grinding is conducive to improving the grinding effect and ensuring the flatness and smoothness of the surface of the quartz product 1 after grinding.
[0044] During S2 to S4, a grinding fluid is sprayed toward the grinding position, and the grinding fluid contains a coolant and a lubricant. The ratio of the coolant to the lubricant is (20-30):1, and in this embodiment, the ratio of the coolant to the lubricant is 24:1. The coolant composition includes cerium oxide abrasive, deionized water and hydrogen peroxide, wherein the concentration of the cerium oxide abrasive is 7-12wt%, the concentration of the hydrogen peroxide is 5-9wt%, and the rest is deionized water.
[0045] During the grinding process, spraying grinding fluid onto the grinding position plays a role in heat dissipation, reduces thermal damage to the surface of the quartz product 1, and takes away the grinding chips, which is beneficial to improving the grinding effect and grinding efficiency. The grinding fluid includes coolant and lubricant. The coolant has a good heat dissipation effect, and the lubricant is beneficial to improving the lubrication performance of the grinding fluid, avoiding excessive friction between the grinding head and the surface of the quartz product 1 during the grinding process, which may cause damage to the surface of the quartz product 1. The composition of the coolant is reasonably set, and the cerium oxide abrasive has a very high polishing efficiency, which can quickly remove stains and defects on the surface of the quartz product 1, reducing polishing time and cost. Cerium oxide abrasive has good chemical stability and physical stability, and will not decompose or produce pollution during the polishing process. Hydrogen peroxide plays a role in oxidative corrosion, grinding the surface of the quartz product 1.
[0046] In the process from S2 to S4, the roughing grinding head, the semi-finishing grinding head and the finishing grinding head are successively connected to the ultrasonic vibration main shaft, and the ultrasonic vibration main shaft rotates and generates vibration to realize the rough grinding, semi-finishing grinding and finishing grinding of the quartz product 1. The vibration frequency of the ultrasonic vibration main shaft is 20 kHz to 50kHz.
[0047] Ultrasonic assisted grinding technology is used to promote effective contact between abrasive particles and the surface of the quartz product 1 through the micro-impact and micro-friction generated by ultrasonic vibration, thereby improving grinding efficiency. The ultrasonic equipment uses a built-in ultrasonic system integrated with the grinder, including a transducer 3, an amplifier rod 4, a tool head 5, and an ultrasonic spring collet chuck. By applying a certain vibration frequency to the grinding head, the surface of the workpiece is crushed, and the grinding head can easily remove the material.
[0048] The grinding methods in the process from S2 to S4 are divided into axial grinding, radial grinding, and deep hole grinding. The axial grinding speed Vc=800~1150 m / min, the radial grinding speed Vc=400~600 m / min, and the deep hole grinding speed Vc=55~120 m / min. Vc represents the linear speed of the grinding wheel. Different grinding speeds are used for different grinding methods to ensure the grinding effect.
[0049] In S1, the quartz product 1 is loaded onto the vacuum suction cup 6 on the workbench 2. A circle of vacuum adsorption holes 7 are arranged on the vacuum suction cup 6. An annular groove 8 is arranged on the lower surface of the vacuum suction cup 6 corresponding to the vacuum adsorption holes 7. The open end of the annular groove 8 is connected to a closed ring 9, and the annular groove 8 is connected to a vacuum pipeline. The vacuum suction cup 6 is annular in structure. An annular adsorption surface 10 is arranged on the vacuum suction cup 6. A plurality of centering piston cylinders 11 are evenly installed around the outer periphery of the adsorption surface 10 on the vacuum suction cup 6. The end of the telescopic rod of the centering piston cylinder 11 is connected to a ball head 12. The telescopic rod of the centering piston cylinder 11 extends outward so that the ball head 12 presses against the outer wall of the quartz product 1 to realize the centering and positioning of the quartz product 1. The annular groove 8 corresponding to the vacuum adsorption hole 7 is connected to the vacuum pipeline to form a negative pressure, thereby realizing the vacuum adsorption and positioning of the quartz product 1.
[0050] After S1, a dial indicator is installed on the spindle, and the dial indicator contact is attached to the side wall of the quartz product 1. The spindle rotates and moves along the X and Y directions until the dial indicator display is stable and there is no jump. At this time, the spindle and the quartz product 1 are in a coaxial state. In many cases, the grinding of the quartz product 1 needs to ensure that it is coaxial with the grinding head. The circular runout of the side wall of the quartz product 1 is measured by the dial indicator to determine whether the two are concentric, and the judgment is accurate and reliable.
[0051] Embodiment 3: A method for grinding a quartz product (see attached Figure 1 , Attachment Figure 4 ), including the following steps: S1, loading the quartz product 1 onto the workbench 2; S2, rough grinding, using a rough grinding head to grind the surface of the quartz product 1; the rough grinding head is installed on the main shaft of the grinder, and the main shaft rotates so that the rough grinding head and the surface of the quartz product 1 are in contact with each other for grinding; S3, semi-finishing grinding, using a semi-finishing grinding head to grind the surface of the quartz product 1; the semi-finishing grinding head is installed on the main shaft of the grinder, and the main shaft rotates so that the semi-finishing grinding head and the surface of the quartz product 1 are in contact with each other for grinding; S4, fine grinding, using a fine grinding head to grind the surface of the quartz product 1; the fine grinding head is installed on the main shaft of the grinder, and the main shaft rotates so that the fine grinding head and the surface of the quartz product 1 are in contact with each other for grinding; S5, unloading the quartz product 1, and completing the grinding process.
[0052] The binder used for the roughing grinding head is silver, which binds the diamond abrasives together to form a roughing grinding head. The binder used for the semi-finishing grinding head and the finishing grinding head is resin, which binds the diamond abrasives together to form a semi-finishing grinding head and a finishing grinding head. The abrasive grains of the roughing grinding head, semi-finishing grinding head, and finishing grinding head are #170, #400, and #800 respectively.
[0053] During the grinding process, the quartz product 1 is loaded on the workbench 2 for positioning. The grinding process is divided into three steps: rough grinding, semi-finishing grinding, and fine grinding. In these three steps, a rough grinding head, a semi-finishing grinding head, and a fine grinding head are used to perform the grinding operation. Using different grinding head distributions for grinding is conducive to improving the grinding effect and ensuring the flatness and smoothness of the surface of the quartz product 1 after grinding.
[0054] During S2 to S4, a grinding fluid is sprayed toward the grinding position, and the grinding fluid contains a coolant and a lubricant. The ratio of the coolant to the lubricant is (20-30):1, and in this embodiment, the ratio of the coolant to the lubricant is 24:1. The coolant composition includes cerium oxide abrasive, deionized water and hydrogen peroxide, wherein the concentration of the cerium oxide abrasive is 7-12wt%, the concentration of the hydrogen peroxide is 5-9wt%, and the rest is deionized water.
[0055] During the grinding process, spraying grinding fluid onto the grinding position plays a role in heat dissipation, reduces thermal damage to the surface of the quartz product 1, and takes away the grinding chips, which is beneficial to improving the grinding effect and grinding efficiency. The grinding fluid includes coolant and lubricant. The coolant has a good heat dissipation effect, and the lubricant is beneficial to improving the lubrication performance of the grinding fluid, avoiding excessive friction between the grinding head and the surface of the quartz product 1 during the grinding process, which may cause damage to the surface of the quartz product 1. The composition of the coolant is reasonably set, and the cerium oxide abrasive has a very high polishing efficiency, which can quickly remove stains and defects on the surface of the quartz product 1, reducing polishing time and cost. Cerium oxide abrasive has good chemical stability and physical stability, and will not decompose or produce pollution during the polishing process. Hydrogen peroxide plays a role in oxidative corrosion, grinding the surface of the quartz product 1.
[0056] In the process from S2 to S4, the roughing grinding head, the semi-finishing grinding head and the finishing grinding head are successively connected to the ultrasonic vibration main shaft, and the ultrasonic vibration main shaft rotates and generates vibration to realize the rough grinding, semi-finishing grinding and finishing grinding of the quartz product 1. The vibration frequency of the ultrasonic vibration main shaft is 20 kHz to 50kHz.
[0057] Ultrasonic assisted grinding technology is used to promote effective contact between abrasive particles and the surface of the quartz product 1 through the micro-impact and micro-friction generated by ultrasonic vibration, thereby improving grinding efficiency. The ultrasonic equipment uses a built-in ultrasonic system integrated with the grinder, including a transducer 3, an amplifier rod 4, a tool head 5, and an ultrasonic spring collet chuck. By applying a certain vibration frequency to the grinding head, the surface of the workpiece is crushed, and the grinding head can easily remove the material.
[0058] The grinding methods in the process from S2 to S4 are divided into axial grinding, radial grinding, and deep hole grinding. The axial grinding speed Vc=800~1150 m / min, the radial grinding speed Vc=400~600 m / min, and the deep hole grinding speed Vc=55~120 m / min. Vc represents the linear speed of the grinding wheel. Different grinding speeds are used for different grinding methods to ensure the grinding effect.
[0059] A lifting suction cup 13 and a flipping suction cup 14 are provided on the workbench 2. During S1, the quartz product 1 is first loaded onto the lifting suction cup 13, and the lifting suction cup 13 adsorbs and positions the quartz product 1. After the upper surface of the quartz product 1 completes the processing of steps S2 to S4, the flipping suction cup 14 flips to the top of the quartz product 1 and adsorbs the upper surface of the quartz product 1. Then, the lifting suction cup 13 removes the adsorption effect on the quartz product 1 and moves downward. The flipping suction cup 14 flips 180 degrees, and the lower surface of the quartz product 1 is processed through steps S2 to S4.
[0060] A plurality of lifting and correcting piston cylinders 15 are arranged at intervals on the periphery of the lifting suction cup 13 on the workbench 2. The telescopic rod of the lifting and correcting piston cylinder 15 is connected to the lifting and correcting column 16. The end of the lifting and correcting column 16 is tapered. Lifting and correcting holes 17 are arranged on the outer wall of the lifting suction cup 13 and corresponding to the lifting and correcting column 16. The lifting and correcting column 16 is inserted into the lifting and correcting hole 17 to correct and position the lifting suction cup 13. A lifting piston cylinder 18 is installed below the lifting suction cup 13 on the workbench 2. The telescopic rod of the lifting piston cylinder 18 is fastened to the support plate 19, and the support plate 19 is fixedly connected to the lifting suction cup 13.
[0061] A plurality of tilting correction piston cylinders 20 are arranged at intervals around the periphery of the tilting suction cup 14 on the workbench 2. The telescopic rod of the tilting correction piston cylinder 20 is connected to the tilting correction column 21. The end of the tilting correction column 21 is tapered. A tilting correction hole 22 is arranged on the outer wall of the tilting suction cup 14 and the tilting correction column 21. The tilting correction column 21 is inserted into the tilting correction hole 22 to correct the tilting of the tilting suction cup 14. A rotating shaft 23 driven by a motor is installed on the workbench 2. The rotating shaft 23 and the tilting suction cup 14 are fixedly connected by a rib plate 24.
[0062] A circle of vacuum adsorption holes 7 are arranged on both the lifting suction cup 13 and the flipping suction cup 14. An annular groove 8 is arranged on the lower surface of the lifting suction cup 13 corresponding to the vacuum adsorption hole 7. The open end of the annular groove 8 is connected to the closed ring 9, and the annular groove 8 is connected to the vacuum pipeline. An annular groove 8 is arranged on the lower surface of the flipping suction cup 14 corresponding to the vacuum adsorption hole 7. The open end of the annular groove 8 is connected to the closed ring 9, and the annular groove 8 is connected to the vacuum pipeline. The annular groove 8 corresponding to the vacuum adsorption hole 7 is connected to the vacuum pipeline to form a negative pressure, thereby realizing the vacuum adsorption positioning of the quartz product 1.
[0063] After S1, a dial indicator is installed on the spindle, and the dial indicator contact is attached to the side wall of the quartz product 1. The spindle rotates and moves along the X and Y directions until the dial indicator display is stable and there is no jump. At this time, the spindle and the quartz product 1 are in a coaxial state. In many cases, the grinding of the quartz product 1 needs to ensure that it is coaxial with the grinding head. The circular runout of the side wall of the quartz product 1 is measured by the dial indicator to determine whether the two are concentric, and the judgment is accurate and reliable.
[0064] The above-described embodiments are only preferred solutions of the present invention and are not intended to limit the present invention in any form. Other variations and modifications are possible without exceeding the technical solutions described in the claims.
Claims
1. A quartz product grinding method, characterized in that: The following steps are involved: S1, loading the quartz product onto the workbench; S2, rough grinding, using a rough grinding head to grind the surface of the quartz product; S3, semi-finishing grinding, using a semi-finishing grinding head to grind the surface of the quartz product; S4, fine grinding, using a fine grinding head to grind the surface of the quartz product; S5, unloading the quartz product and completing the grinding process.
2. A quartz product grinding method according to claim 1, characterized in that: During S2 to S4, grinding fluid is sprayed toward the grinding position.
3. A quartz product grinding method according to claim 2, characterized in that: Grinding fluid contains coolant and lubricant.
4. A quartz product grinding method according to claim 3, characterized in that: The coolant comprises cerium oxide abrasive, deionized water and hydrogen peroxide, wherein the concentration of the cerium oxide abrasive is 7-12wt%, the concentration of the hydrogen peroxide is 5-9wt%, and the rest is deionized water.
5. A quartz product grinding method according to claim 1, characterized in that: In the process from S2 to S4, the roughing grinding head, semi-finishing grinding head and finishing grinding head are successively connected to the ultrasonic vibration main shaft, and the ultrasonic vibration main shaft rotates and generates vibration to realize the rough grinding, semi-finishing grinding and finishing grinding of the quartz product.
6. A quartz product grinding method according to claim 5, characterized in that: The vibration frequency of the ultrasonic vibration spindle is 20 kHz to 50 kHz.
7. A quartz product grinding method according to claim 1, characterized in that: The binder used for roughing grinding heads is silver, and the binder used for semi-finishing grinding heads and finishing grinding heads is resin.
8. A quartz product grinding method according to claim 1, characterized in that: The grinding methods in the process from S2 to S4 are divided into axial grinding, radial grinding, and deep hole grinding. The axial grinding speed Vc=800~1150 m / min, the radial grinding speed Vc=400~600 m / min, and the deep hole grinding speed Vc=55~120 m / min.
9. A quartz product grinding method according to any one of claims 1 to 8, characterized in that: After S1, install the dial indicator on the spindle, and fit the dial indicator contact to the side wall of the quartz product. The spindle rotates and moves along the X and Y directions until the dial indicator display is stable and there is no jump. At this time, the spindle and the quartz product are in a coaxial state.
10. A quartz product grinding method according to any one of claims 1 to 8, characterized in that: A lifting suction cup and a flipping suction cup are set on the workbench. In S1, the quartz product is first loaded on the lifting suction cup, and the lifting suction cup adsorbs and positions the quartz product. After the upper surface of the quartz product completes the processing of steps S2 to S4, the flipping suction cup flips to the top of the quartz product and adsorbs the upper surface of the quartz product. Then, the lifting suction cup removes the adsorption effect on the quartz product and moves downward. The flipping suction cup flips 180 degrees, and the lower surface of the quartz product is processed by steps S2 to S4.
Citation Information
Patent Citations
Composite grinding method for large-caliber quartz glass substrate
CN101797709A
Double-face grinding device for quartz product and double-face grinding method for quartz product
CN107917113A
Polishing process of novel optical glass material H-FK61
CN111531432A
Quartz hemispherical harmonic oscillator machining tool and method
CN111843634A
Grinding tool setting method suitable for blind hole hard anodizing film layer
CN115635420A