Ceramic high-flux powder blending system and method
Through the ceramic high-throughput powder mixing system, the microfluidic feeding device and the powder spraying device are used to achieve efficient powder mixing of multi-component ceramic powder and the formation of spherical composite powder, which solves the problem of long trial and error cycles and problems in the existing technology. The problem of unsatisfactory powder shape improves R&D efficiency and molding quality.
Patent Information
- Application Number
- CN202410749323.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-05
- Publication Date
- 2024-10-15
AI Technical Summary
The existing research and development of ceramic composite powders suffers from long trial and error cycles, low work efficiency, high production costs, and difficulty in obtaining spherical powders, which affects the quality of the molding and sintering processes.
Design a high-throughput ceramic powder dispensing system that utilizes microfluidic feeding devices, powder spraying devices and receiving devices to achieve efficient dispensing of multi-component ceramic powders and form spherical composite powders through highly precise control of process parameters. The system includes a syringe pump, a peristaltic pump, an inert gas bottle, a powder spraying device and a conductive metal receiving tank. The slurry is solidified into composite ceramic microspheres through a high-voltage electric field, followed by drying and sintering.
It significantly improves the development efficiency and quality of new materials, reduces research and development costs, and obtains high-density spherical composite powder, which is suitable for subsequent molding and sintering processes.
Smart Images

Figure HSA0000299526050000011 
Figure HSA0000299526050000021
Abstract
Description
Technical Field
[0001] The invention relates to a batch material configuration system and method, and in particular to a ceramic high-throughput powder configuration system and method. Background Art
[0002] The composition of new ceramics and their composite materials is often very complex, and several or even dozens of additives are often added as modified ingredients, or multiple additional phases are added to improve the performance of new ceramics. In the research and development experiments of new ceramics, in order to explore the best formula, the number of tests for any combination of multi-level formulas has increased exponentially. The existing single-variable controlled composite powder research and development has problems such as long trial and error cycle, low work efficiency, and high production cost. At the same time, it is difficult to obtain statistically reliable experimental results with a limited number of tests. Therefore, it is very important to design a high-throughput ceramic powder mixing system and method with multi-channel continuous gradient component changes.
[0003] In addition, the subsequent molding and sintering processes put forward requirements for the powder particle shape of new ceramics, such as additive manufacturing of chopped carbon fiber reinforced silicon carbide ceramics, plasma spraying of multi-rare earth ion doped ceramics, etc. Spherical is the most ideal condition for ceramic powders, because the spherical shape has good fluidity and high packing density, which is conducive to molding and sintering. Therefore, if spherical composite powders can be obtained while efficiently mixing powders, it is of great significance to improve the performance of new ceramics. Summary of the invention
[0004] In order to solve the problems of the prior art, the purpose of the present invention is to overcome the shortcomings of the existing technology and provide a ceramic high-throughput powder mixing system and method, which utilizes the high-precision control of the process parameters of a microfluidic feeding device to greatly improve the powder mixing efficiency of multi-component ceramic powders, so that experiments that originally took several months can be completed within a few hours, greatly improving the development efficiency and quality of new materials and significantly reducing the research and development costs of new materials.
[0005] To achieve the above-mentioned purpose, the present invention provides a ceramic high-throughput powder preparation system, which is composed of a microfluidic feeding device, a powder spraying device and a receiving device; the microfluidic feeding device is one or a mixture of a syringe pump, a peristaltic pump, an inert gas cylinder or compressed air; the powder spraying device is composed of a slurry syringe, a slurry mixing conduit, a needle, a high-voltage power supply and positive and negative electrode wires; the receiving device is a conductive metal receiving tank, which is placed directly below the needle; when a composite powder composed of n powders with different components is configured, the total number of syringe pumps, peristaltic pumps, inert gas cylinders and / or compressed air is n, the number of slurry syringes is n, the number of metal receiving tanks is m, and the number of other devices is 1, n≥1 and is an integer, and m≥1 and is an integer.
[0006] A ceramic high-throughput powder preparation method, characterized by comprising the following steps:
[0007] (1) preparing n kinds of ceramic powders with different compositions, respectively mixing them with polymers and solvents to form n groups of slurries, wherein the ceramic powders are main crystalline ceramic powders and / or reinforcing phases, the polymers are polyethersulfone, chitosan or cellulose acetate, the solvents are N-methylpyrrolidone, acetylacetone, acetone or dimethylacetamide, the mass fraction of the ceramic powders is 20-50%, the mass fraction of the polymers is 40-65%, and the mass fraction of the solvents is 5-15%;
[0008] (2) respectively loading the prepared n groups of slurries into n slurry syringes, using n microfluidic feeding devices to push the slurries in the respective slurry syringes into the slurry mixing conduit, and independently adjusting the slurry flow rate of each slurry syringe by controlling the parameters of each microfluidic feeding device, thereby obtaining slurries of different components in the mixing conduit, and forming a continuous state of fluid entering the needle, wherein the pressure of the microfluidic feeding device is the driving pressure of the peristaltic pump, the driving pressure of the syringe pump, the inert gas flow rate or the air pressure of compressed air;
[0009] (3) connecting the positive electrode of a high-voltage power supply to the needle, and the negative electrode of the power supply to a conductive metal receiving tank, wherein the solution in the conductive metal receiving tank is one of water, glycerol, and ethanol or a mixture thereof, turning on the high-voltage power supply, wherein the voltage of the high-voltage power supply is 20 to 25 kV, and the mixed slurry forms droplets in the nozzle under a high-voltage electric field and solidifies in the solution in the receiving tank to obtain a composite ceramic microsphere green body composed of a mixture of n different components;
[0010] (4) replacing the receiving device, changing the pressure of the microfluidic feeding device to adjust the feeding rate of the slurry in each slurry syringe, obtaining a high-throughput mixed powder with a continuous gradient change of m number components and forming a composite microsphere green body;
[0011] (5) The prepared composite microsphere green body is dried in an air environment for 24 hours, and then placed in a muffle furnace for sintering at a sintering temperature of 800-1300° C. and a sintering time of 2-6 hours to obtain complex component ceramic microspheres.
[0012] The main crystalline phase ceramic powder includes oxide ceramics and / or non-oxide ceramics, the oxide ceramics are any one or a mixture of rare earth-doped zirconium oxide, rare earth oxide, silicon oxide, aluminum oxide, magnesium oxide, zinc oxide, titanium oxide, iron oxide, silver oxide, cerium oxide, calcium oxide, manganese oxide, hafnium oxide or lanthanum oxide, the non-metallic ceramics are any one or a mixture of silicon carbide, zirconium carbide, boron carbide or silicon nitride, and the reinforcing phase is any one or a mixture of chopped carbon fiber, chopped aluminum oxide fiber, chopped silicon oxide fiber, chopped silicon carbide fiber, chopped silicon nitride fiber, carbon nanotube, graphene, diamond, silicon carbide whisker or silicon carbide nanowire.
[0013] Compared with the prior art, the present invention has the following beneficial effects: (1) The ceramic high-throughput powder mixing system provided by the present invention has a simple equipment structure, convenient operation, low cost, and can realize automated production; (2) The ceramic high-throughput powder mixing method provided by the present invention can significantly improve the research and development efficiency of complex component powders, and provide a solution for achieving multiple goals of establishing the "component-process-structure-performance" relationship of powders without missing out; (3) The composite powder prepared by the ceramic high-throughput powder mixing method provided by the present invention has a spherical structure and a very high powder packing density, which can avoid the bridging phenomenon caused by irregular powder shape, and is beneficial to subsequent molding processes, such as ceramic additive manufacturing, coating spraying, etc.; (4) The ceramic high-throughput powder mixing method provided by the present invention can realize the uniform compounding of ceramic main crystal phase powder and reinforcement phase powder, avoiding the occurrence of uneven dispersion, agglomeration, etc. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 This is a schematic diagram of a ceramic high-throughput powder preparation system according to Example 1 of the present invention;
[0015] The figures are marked as follows: 1-1. Peristaltic pump No. 1; 1-2. Peristaltic pump No. 2; 1-3. Peristaltic pump No. 3; 2. Slurry syringe; 3. Catheter; 4. Slurry mixing catheter; 5. Needle; 6. Electrode wire; 7. High voltage power supply; 8. Receiving device.
[0016] Figure 2 It is a schematic diagram of a ceramic high-throughput powder preparation system of Example 2 of the present invention.
[0017] The figures are marked as follows: 1-1. Inert gas cylinder No. 1; 1-2. Inert gas cylinder No. 2; 1-3. Inert gas cylinder No. 3; 1-4. Inert gas cylinder No. 4; 2. Slurry syringe; 3. Catheter; 4. Slurry mixing catheter; 5. Needle; 6. Electrode wire; 7. High-voltage power supply; 8. Receiving device. DETAILED DESCRIPTION
[0018] The present invention is further illustrated below in conjunction with specific embodiments. It should be understood that these embodiments are only used for the present invention and are not used to limit the scope of the present invention. After reading the present invention, various equivalent forms of modifications to the present invention by those skilled in the art are all within the scope of the claims attached to this application.
[0019] Embodiment 1
[0020] An embodiment of the present invention provides a high-throughput powder preparation system and method for high-throughput configuration of a composite ceramic powder composed of silicon carbide powder with an average particle size of 0.5 μm, silicon carbide powder with an average particle size of 20 μm, and chopped carbon fibers with an average length of 10 μm for laser selective sintering additive manufacturing printing.
[0021] like Figure 1As shown, a ceramic high-throughput powder preparation system is composed of a microfluidic feeding device, a powder spraying device and a receiving device; the microfluidic feeding device is a peristaltic pump; the powder spraying device is composed of a slurry syringe, a slurry mixing conduit, a needle, a high-voltage power supply and positive and negative electrode wires; the receiving device is a conductive metal receiving tank, which is placed directly below the needle; this embodiment is configured with a composite powder composed of 3 powders of different components, the total number of peristaltic pumps is 3, the number of slurry syringes is 3, the number of metal receiving tanks is 9, and the number of other devices is 1.
[0022] A ceramic high-throughput powder preparation method, characterized by comprising the following steps:
[0023] (1) preparing three ceramic powders of different compositions, and respectively preparing three groups of slurries with polymers and solvents, wherein the ceramic powders are silicon carbide powder with an average particle size of 0.5 μm, silicon carbide powder with an average particle size of 20 μm, and chopped carbon fibers with an average length of 10 μm, the polymer is polyethersulfone, and the solvent is N-methylpyrrolidone; in the first group of slurries, the mass fraction of silicon carbide powder with an average particle size of 0.5 μm is 40%, the mass fraction of polymer is 50%, and the mass fraction of solvent is 10%; in the second group of slurries, the mass fraction of silicon carbide powder with an average particle size of 20 μm is 20%, the mass fraction of polymer is 65%, and the mass fraction of solvent is 15%; in the third group of slurries, the mass fraction of chopped carbon fibers with an average length of 10 μm is 30%, the mass fraction of polymer is 55%, and the mass fraction of solvent is 15%;
[0024] (2) The three groups of prepared slurries are respectively loaded into three slurry syringes, and the slurries in the respective slurry syringes are respectively pushed into the slurry mixing conduit by three peristaltic pumps, and the slurry flow rate of each slurry syringe is independently adjusted by controlling the driving pressure of each peristaltic pump, so as to obtain slurries of different components in the mixing conduit, and form a continuous state fluid to enter the needle;
[0025] (3) connecting the positive electrode of a high-voltage power supply to the needle, and the negative electrode of the power supply to a conductive metal receiving tank, wherein the solution in the conductive metal receiving tank is one of water, glycerol, and ethanol or a mixture thereof, turning on the high-voltage power supply, and the voltage of the high-voltage power supply is 25 kV, and the mixed slurry forms droplets in the nozzle under the high-voltage electric field and solidifies in the receiving tank solution to obtain a composite ceramic microsphere green body composed of a mixture of silicon carbide powder with an average particle size of 0.5 μm, silicon carbide powder with an average particle size of 20 μm, chopped carbon fibers with an average length of 10 μm, and chopped carbon fibers with an average length of 30 μm;
[0026] (4) replacing the receiving device, and each group of peristaltic pumps respectively changes three driving pressures to adjust the feeding rate of the slurry in each slurry syringe, thereby obtaining a high-throughput silicon carbide powder and chopped carbon fiber mixed powder with a continuous gradient change in nine quantity components and forming a composite microsphere green body;
[0027] (5) The prepared composite microsphere green body is dried in an air environment for 24 hours, and then placed in a muffle furnace for sintering at a sintering temperature of 800° C. for a sintering time of 2 hours to obtain complex component ceramic microspheres.
[0028] This embodiment can achieve high-throughput, rapid and uniform mixing of composite powders of multiple groups of different silicon carbide powders and short-cut carbon fibers, significantly improving the powder mixing efficiency, while solving the problems of uneven dispersion and aggregation of carbon fibers and silicon carbide powders caused by inconsistent density and shape of silicon carbide fibers and short-cut carbon fibers. The obtained composite powder microspheres have a very high sphericity and can obtain excellent fluidity, which is beneficial to the subsequent laser selective sintering additive manufacturing powder spreading process.
[0029] Embodiment 2
[0030] The embodiment of the present invention provides a method for high-throughput configuration for solid phase sintering synthesis of Er 3+ , Yb 3+ 、Eu 3+ Three kinds of Y2O3 phosphorescent powders doped with different rare earth ions (Y2O3: Er 3+ , Yb 3+ ,Eu 3+ ) is a raw material high-throughput powder mixing system and method composed of four oxide nanopowders of Er2O3, Yb2O3, Eu2O3 and Y2O3.
[0031] The present invention provides a ceramic high-throughput powder preparation system, which is composed of a microfluidic feeding device, a powder spraying device and a receiving device; the microfluidic feeding device is an inert gas cylinder; the powder spraying device is composed of a slurry syringe, a slurry mixing conduit, a needle, a high-voltage power supply and positive and negative electrode wires; the receiving device is a conductive metal receiving slot, which is placed directly below the needle; when the composite powder composed of 4 powders with different components is configured in this embodiment, the total number of inert gas cylinders is 4, the number of slurry syringes is 4, the number of metal receiving slots is 16, and the number of other devices is 1.
[0032] A ceramic high-throughput powder preparation method, characterized by comprising the following steps:
[0033] (1) preparing four ceramic powders of different compositions, and preparing four groups of slurries with polymers and solvents respectively, wherein the ceramic powders are Er2O3, Yb2O3, Eu2O3 and Y2O3, the polymer is polyethersulfone, and the solvent is N-methylpyrrolidone. In each group of slurries, the mass fraction of the ceramic powder is 40%, the mass fraction of the polymer is 50%, and the mass fraction of the solvent is 10%;
[0034] (2) The four groups of prepared slurries are respectively loaded into four slurry syringes, and the slurries in the respective slurry syringes are respectively pushed into the slurry mixing conduit by four microfluidic feeding devices (inert gas), and the slurry flow rate of each slurry syringe is independently adjusted by controlling the parameters (gas flow rate) of each microfluidic feeding device, so as to obtain slurries of different components in the mixing conduit, and form a continuous state of fluid entering the needle;
[0035] (3) connecting the positive electrode of a high-voltage power supply to the needle, and the negative electrode of the power supply to a conductive metal receiving tank, wherein the solution in the conductive metal receiving tank is one of water, glycerol, and ethanol or a mixture thereof, turning on the high-voltage power supply, and the voltage of the high-voltage power supply is 20 kV, and the mixed slurry forms droplets in the nozzle under the high-voltage electric field and solidifies in the receiving tank solution to obtain a composite ceramic microsphere green body composed of four different components of Er2O3, Yb2O3, Eu2O3, and Y2O3;
[0036] (4) replacing the receiving device and changing the pressure of the microfluidic feeding device to adjust the feeding rate of the slurry in each slurry syringe to obtain a high-throughput mixed powder with continuous gradient changes of 16 components and form a composite microsphere green body;
[0037] (5) The prepared composite microsphere green body is dried in air environment for 24 hours, and then placed in a muffle furnace for sintering at a sintering temperature of 800-1300°C and a sintering time of 2-6 hours to obtain a complex component Y2O3:Er 3+ , Yb 3+ ,Eu 3+ Phosphorescent powder microspheres.
[0038] This embodiment can achieve efficient and complete preparation of different Er 3+ , Yb 3+ 、Eu 3+ Rare earth ion doped Y2O3 phosphorescent powder, thus obtaining Y2O3 with the best phosphorescent performance: Er 3+ , Yb 3+ ,Eu 3+ The obtained composite powder microspheres have high sphericity and can obtain excellent fluidity, which is beneficial to the subsequent dry pressing or plasma spraying process for preparing ceramic phosphorescent coatings.
Claims
1. A ceramic high-throughput powder preparation system, consisting of a microfluidic feeding device, a powder spraying device and a receiving device; the microfluidic feeding device is one or a mixture of a syringe pump, a peristaltic pump or compressed air; the powder spraying device is composed of a slurry syringe, a slurry mixing conduit, a needle, a high-voltage power supply and positive and negative electrode wires; the receiving device is a conductive metal receiving tank, which is placed directly below the needle; when a composite powder composed of n powders with different components is configured, the total number of syringe pumps, peristaltic pumps, inert gas cylinders and / or compressed air is n, the number of slurry syringes is n, the number of metal receiving tanks is m, and the number of other devices is 1, n ≥ 1 and is an integer, m ≥ 1 and is an integer.
2. A high-throughput ceramic powder preparation method, Features The following steps are involved: (1) preparing n kinds of ceramic powders with different compositions, respectively mixing them with polymers and solvents to form n groups of slurries, wherein the ceramic powders are main crystalline ceramic powders and / or reinforcing phases, the polymers are polyethersulfone, chitosan or cellulose acetate, the solvents are N-methylpyrrolidone, acetylacetone, acetone or dimethylacetamide, the mass fraction of the ceramic powders is 20-50%, the mass fraction of the polymers is 40-65%, and the mass fraction of the solvents is 5-15%; (2) respectively loading the prepared n groups of slurries into n slurry syringes, using n microfluidic feeding devices to push the slurries in the respective slurry syringes into the slurry mixing conduit, and independently adjusting the slurry flow rate of each slurry syringe by controlling the parameters of each microfluidic feeding device, thereby obtaining slurries of different components in the mixing conduit, and forming a continuous state of fluid entering the needle, wherein the pressure of the microfluidic feeding device is the driving pressure of the peristaltic pump, the driving pressure of the syringe pump, the inert gas flow rate or the air pressure of compressed air; (3) connecting the positive electrode of a high-voltage power supply to the needle, and the negative electrode of the power supply to a conductive metal receiving tank, wherein the solution in the conductive metal receiving tank is one of water, glycerol, and ethanol or a mixture thereof, turning on the high-voltage power supply, wherein the voltage of the high-voltage power supply is 20 to 25 kV, and under a high-voltage electric field, the mixed slurry forms droplets at the nozzle and solidifies in the solution of the receiving tank to obtain a composite ceramic microsphere green body composed of a mixture of n different components; (4) replacing the receiving device, changing the pressure of the microfluidic feeding device to adjust the feeding rate of the slurry in each slurry syringe, obtaining a high-throughput mixed powder with a continuous gradient change of m number components and forming a composite microsphere green body; (5) The prepared composite microsphere green body is dried in an air environment for 24 hours, and then placed in a muffle furnace for sintering at a sintering temperature of 800-1300° C. and a sintering time of 2-6 hours to obtain complex component ceramic microspheres.
3. A ceramic high-throughput powder preparation method according to claim 2, It is characterized in that The main crystalline phase ceramic powder includes oxide ceramics and / or non-oxide ceramics, the oxide ceramics are any one or a mixture of rare earth-doped zirconium oxide, rare earth oxide, silicon oxide, aluminum oxide, magnesium oxide, zinc oxide, titanium oxide, iron oxide, silver oxide, cerium oxide, calcium oxide, manganese oxide, hafnium oxide or lanthanum oxide, the non-metallic ceramics are any one or a mixture of silicon carbide, zirconium carbide, boron carbide or silicon nitride, and the reinforcing phase is any one or a mixture of chopped carbon fiber, chopped aluminum oxide fiber, chopped silicon oxide fiber, chopped silicon carbide fiber, chopped silicon nitride fiber, carbon nanotube, graphene, diamond, silicon carbide whisker or silicon carbide nanowire.
Citation Information
Cited By
Fe2O3, Ag2O and La0. 67Ca0. 33MnO3 three-phase co-composite ceramic and preparation method thereof
CN120518394A