Converter steelmaking process

By cleaning scrap steel with ultrasonic waves, controlling the composition of molten iron and oxygen blowing pressure, adding zinc-manganese alloy and stirring with inert gas, the problem of no scrap steel pretreatment and inaccurate oxygen blowing in the converter steelmaking process has been solved, and the quality of finished products and the steelmaking effect have been significantly improved. .

CN118773393APending Publication Date: 2024-10-15HEBEI IRON AND STEEL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411076445.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-07
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

The existing converter steelmaking process fails to effectively pretreat scrap steel, resulting in poor quality of finished products, and the oxygen blowing process cannot be accurately controlled, affecting the steelmaking effect.

Method used

Use ultrasonic waves to clean scrap steel, control the composition of molten iron and oxygen blowing pressure, add zinc-manganese alloy, use inert gas stirring to ensure clean molten steel and full contact with oxygen, and form high-quality steel billets through mold cooling.

Benefits of technology

It improves the cleanliness of scrap steel and the quality of finished products, ensures precise control of the oxygen blowing process, improves the steelmaking effect and the structural strength of finished products, avoids the entry of external impurities, and significantly improves the overall application effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118773393A_ABST
    Figure CN118773393A_ABST
Patent Text Reader

Abstract

The invention discloses a converter steelmaking process, which belongs to the technical field of converter steelmaking, and comprises the following steps: preparing molten iron for steelmaking and scrap steel, and adding the molten iron and the scrap steel into a converter; according to the method, the obtained waste steel is pretreated, the cleanliness of the waste steel can be guaranteed, the surface of the waste steel is free of oil stains and impurities, and therefore the quality of a final finished product can be guaranteed, meanwhile, the oxygen blowing process in the converter can be accurately controlled in different time periods, and therefore blown-in oxygen can effectively circulate; and in the method, the components of the molten steel are controlled, and the zinc-manganese alloy can be effectively fused in the molten steel, so that the structural strength of the final finished product can be improved, and when the molten steel is finally tapped, the molten steel can be continuously tapped by introducing inert gas for stirring and the like. External impurities can be effectively prevented from entering molten steel, the quality of cooled steel billets is guaranteed, and the overall method is good in practical application effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of converter steelmaking, and in particular relates to a converter steelmaking process. Background Art

[0002] The converter steelmaking process is a common steelmaking process, and it is also a complex and delicate process that requires strict control and management of each link. By continuously improving and optimizing the process methods, we can improve steelmaking efficiency and product quality, reduce production costs and energy consumption, and achieve sustainable development of the steel industry.

[0003] A Chinese patent (CN105714011A) discloses a converter steelmaking process, which includes the following steps: the carbon of the molten steel before the furnace filling is ≥0.03%, and the tapping temperature is ≤1220℃; first prepare the pig iron block, put the pig iron block in, and immediately shake the furnace 80-90° and stay for 3-5 minutes; then take out the converter, and leave all the slag after the molten steel; then the converter is tilted to the front of the converter lining, and the pig iron blocks are poured into the tilted converter. The converter stays at this position for 2-3 minutes, and the angle of the furnace is shaken at 50-65° when the pig iron blocks are added, and the slag splashing and furnace protection begins. This process can solve the scouring and mechanical wear of the furnace lining caused by adding molten iron and scrap steel by standardizing the requirements, parameter conditions and precautions of each step, reduce the use of furnace materials and the time of furnace filling after stopping the furnace, and has good economic benefits. Although the current converter steelmaking process can also complete steelmaking operations, it does not pre-treat the scrap steel, resulting in a large number of impurities in the scrap steel, resulting in poor quality of the final product. In addition, the oxygen blowing process is not precisely controlled, resulting in the inability to guarantee the oxygen supply effect in the furnace, which also has a significant adverse effect on steelmaking. The overall method has poor actual application effect, and a converter steelmaking process is urgently needed. Summary of the invention

[0004] The purpose of the present invention is to solve the problem that although the current converter steelmaking process can complete the steelmaking operation, the scrap steel is not pre-treated, resulting in a large amount of impurities in the scrap steel, resulting in poor quality of the final product, and the oxygen blowing process is not accurately controlled, resulting in the oxygen supply effect in the furnace cannot be guaranteed, which also has a great adverse effect on steelmaking, and the overall method has a poor actual application effect. A converter steelmaking process is proposed.

[0005] In order to achieve the above object, the present invention adopts the following technical solutions: A converter steelmaking process comprises the following steps: S1, prepare molten iron for steelmaking; S2, prepare scrap steel and add the two into the converter; S3, using an oxygen blowing gun to blow oxygen into the converter; S4. Control the pressure of oxygen blowing; S5, controlling the temperature of the molten steel and filling the slag inside; S6. Control the composition of molten steel; S7. Find a suitable mold; S8, introducing molten steel into the mold, introducing inert gas into the mold, and continuously stirring for a period of time; S9, waiting for the molten steel to cool and form a steel billet.

[0006] As a further description of the above technical solution: In S1, molten iron for steelmaking is prepared, the temperature of the molten iron is ≥1250°C, P≤0.15%, Cr≤0.35% in the molten iron is ensured, and the molten iron is free of impurities.

[0007] As a further description of the above technical solution: In S2, scrap steel is prepared, firstly the scrap steel is added into an ultrasonic cleaning device, a cleaning liquid at 60-70°C is added, the scrap steel is ultrasonically cleaned, and the scrap steel is segmented, firstly molten iron is added into a converter, and after 5-10 minutes, the segmented scrap steel is added into the converter, and the mass ratio of molten iron to scrap steel is 1:2.

[0008] As a further description of the above technical solution: In S3, oxygen is blown into the converter by using an oxygen blowing lance. During the oxygen blowing process, the angle and position of the oxygen blowing lance are adjusted every 1-2 minutes to ensure that oxygen is in full contact with the molten pool.

[0009] As a further description of the above technical solution: In S4, the pressure of oxygen blowing is controlled, and the specific control scheme is: the oxygen pressure is controlled to be 0.8-1.0 MPa during 0-10 minutes of oxygen blowing, the oxygen pressure is controlled to be 1.4-1.7 MPa during 11-15 minutes, the oxygen pressure is controlled to be 1.3-1.5 MPa during 16-20 minutes, and the oxygen pressure is controlled to be 1.6-1.9 MPa during 21-26 minutes.

[0010] As a further description of the above technical solution: In S5, the temperature of the molten steel is controlled to 1500-1700°C, and slag is filled therein, wherein the slag is lime and light-burned dolomite, wherein the filled slag accounts for 10-15% of the total mass of the molten steel, and the mass ratio of lime to light-burned dolomite in the slag is 1.2:2.3.

[0011] As a further description of the above technical solution: In S6, the composition of the molten steel is controlled by adding alloy elements into the molten steel. During this process, the molten steel needs to be sampled and analyzed to monitor the composition changes of the molten steel in real time. The added alloy element is zinc-manganese alloy.

[0012] As a further description of the above technical solution: In S7, a suitable mold is found and the inside of the mold is cleaned.

[0013] As a further description of the above technical solution: In the step S8, molten steel is introduced into the mold, and an inert gas is introduced thereinto, and stirring is continued for 5-10 minutes, wherein the deoxidizing gas introduced is argon.

[0014] As a further description of the above technical solution: In S9, the molten steel is cooled and formed into a billet, samples are taken from the formed billet, and the chemical composition, mechanical properties and appearance quality of the samples are tested to ensure that the product quality meets the standards, wherein the water cooling temperature is 40-60°C.

[0015] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are: In the present invention, the method can ensure the cleanliness of the scrap steel by pre-treating the obtained scrap steel, and the surface is free of oil stains and impurities, thereby ensuring the quality of the final product. At the same time, the oxygen blowing process in the converter can be accurately controlled in different time periods, so that the blown oxygen can be effectively circulated, thereby ensuring the overall steelmaking effect and improving the quality of the final product. The composition of molten steel is also controlled in the method, and zinc-manganese alloy can be effectively integrated into it, thereby improving the structural strength of the final product. When the molten steel is finally tapped, external impurities can be effectively prevented from entering the molten steel by introducing inert gas stirring and the like, thereby ensuring the quality of the billet after cooling. The overall method has good practical application effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 The present invention is a flow chart of a converter steelmaking process. DETAILED DESCRIPTION

[0017] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Example 1

[0018] See also Figure 1 The present invention provides a technical solution: a converter steelmaking process, comprising the following steps: S1. Prepare molten iron for steelmaking, make the temperature of molten iron ≥1250℃, ensure P≤0.15%, Cr≤0.35% in molten iron, and ensure that the molten iron is free of impurities; S2, prepare scrap steel, first add the scrap steel into an ultrasonic cleaning device, add a 60°C cleaning solution, perform ultrasonic cleaning on the scrap steel, and segment the scrap steel, first add molten iron into the converter, and after 5 minutes, add the segmented scrap steel into the converter, with the mass ratio of molten iron to scrap steel being 1:2; S3. Use an oxygen lance to blow oxygen into the converter. During the oxygen blowing process, adjust the angle and position of the oxygen lance every 2 minutes to ensure that the oxygen is in full contact with the molten pool. S4. Control the pressure of oxygen blowing. The specific control scheme is: control the oxygen pressure to 0.8MPa during 0-10min of oxygen blowing, control the oxygen pressure to 1.4MPa during 11-15min, control the oxygen pressure to 1.3MPa during 16-20min, and control the oxygen pressure to 1.6MPa during 21-26min; S5, controlling the temperature of the molten steel to 1500°C, and filling slag into the molten steel, wherein the slag is lime and light-burned dolomite, wherein the filling slag accounts for 10% of the total mass of the molten steel, and the mass ratio of lime to light-burned dolomite in the slag is 1.2:2.3; S6. By adding alloying elements into the molten steel, the composition of the molten steel is controlled. In this process, the molten steel needs to be sampled and analyzed to monitor the composition changes of the molten steel in real time. The added alloying element is zinc-manganese alloy; S7. Find a suitable mold and clean the inside of the mold; S8, introducing molten steel into the mold, introducing inert gas therein, and continuously stirring for 5 minutes, wherein the deoxidizing gas introduced is argon; S9, water cooling at 40℃, waiting for the molten steel to cool and form a billet, sampling the formed billet, and testing the chemical composition, mechanical properties and appearance quality of the samples to ensure that the product quality meets the standards.

[0019] In this embodiment, the method can ensure the cleanliness of the scrap steel by pre-treating the scrap steel obtained, and ensure that the surface is free of oil stains and impurities, thereby ensuring the quality of the final product. Example 2

[0020] See also Figure 1 The present invention provides a technical solution: a converter steelmaking process, comprising the following steps: S1. Prepare molten iron for steelmaking, make the temperature of molten iron ≥1250℃, ensure P≤0.15%, Cr≤0.35% in molten iron, and ensure that the molten iron is free of impurities; S2, prepare scrap steel, first add the scrap steel into an ultrasonic cleaning device, add a 60°C cleaning solution, perform ultrasonic cleaning on the scrap steel, and segment the scrap steel, first add molten iron into the converter, and after 7 minutes, add the segmented scrap steel into the converter, with the mass ratio of molten iron to scrap steel being 1:2; S3. Use an oxygen lance to blow oxygen into the converter. During the oxygen blowing process, adjust the angle and position of the oxygen lance every 1 minute to ensure that the oxygen is in full contact with the molten pool. S4. Control the pressure of oxygen blowing. The specific control scheme is: control the oxygen pressure to 0.9MPa during 0-10min of oxygen blowing, control the oxygen pressure to 1.5MPa during 11-15min, control the oxygen pressure to 1.4MPa during 16-20min, and control the oxygen pressure to 17MPa during 21-26min; S5, controlling the temperature of the molten steel to 1600°C, and filling slag into the molten steel, wherein the slag is lime and light-burned dolomite, wherein the filling slag accounts for 15% of the total mass of the molten steel, and the mass ratio of lime to light-burned dolomite in the slag is 1.2:2.3; S6. By adding alloying elements into the molten steel, the composition of the molten steel is controlled. In this process, the molten steel needs to be sampled and analyzed to monitor the composition changes of the molten steel in real time. The added alloying element is zinc-manganese alloy; S7. Find a suitable mold and clean the inside of the mold; S8, introducing molten steel into the mold, introducing inert gas therein, and continuously stirring for 8 minutes, wherein the deoxidizing gas introduced is argon; S9, water cooling at 45℃, waiting for the molten steel to cool and form a billet, sampling the formed billet, and testing the chemical composition, mechanical properties and appearance quality of the samples to ensure that the product quality meets the standards.

[0021] In this embodiment, the method can accurately control the oxygen blowing process in the converter at different time periods, so that the blown oxygen can circulate effectively, thereby ensuring the overall steelmaking effect and improving the quality of the final product. Example 3

[0022] See also Figure 1 The present invention provides a technical solution: a converter steelmaking process, comprising the following steps: S1. Prepare molten iron for steelmaking, make the temperature of molten iron ≥1250℃, ensure P≤0.15%, Cr≤0.35% in molten iron, and ensure that the molten iron is free of impurities; S2, prepare scrap steel, first add the scrap steel into an ultrasonic cleaning device, add a cleaning liquid at 70°C, perform ultrasonic cleaning on the scrap steel, and segment the scrap steel, first add molten iron into a converter, and after 10 minutes, add the segmented scrap steel into the converter, with the mass ratio of molten iron to scrap steel being 1:2; S3. Use an oxygen lance to blow oxygen into the converter. During the oxygen blowing process, adjust the angle and position of the oxygen lance every 2 minutes to ensure that the oxygen is in full contact with the molten pool. S4. Control the pressure of oxygen blowing. The specific control scheme is: control the oxygen pressure to 1.0MPa during 0-10min of oxygen blowing, control the oxygen pressure to 1.7MPa during 11-15min, control the oxygen pressure to 1.5MPa during 16-20min, and control the oxygen pressure to 1.9MPa during 21-26min; S5, controlling the temperature of the molten steel to 1700°C, and filling slag into the molten steel, wherein the slag is lime and light-burned dolomite, wherein the filling slag accounts for 13% of the total mass of the molten steel, and the mass ratio of lime to light-burned dolomite in the slag is 1.2:2.3; S6. By adding alloying elements into the molten steel, the composition of the molten steel is controlled. In this process, the molten steel needs to be sampled and analyzed to monitor the composition changes of the molten steel in real time. The added alloying element is zinc-manganese alloy; S7. Find a suitable mold and clean the inside of the mold; S8, introducing molten steel into the mold, introducing inert gas therein, and continuously stirring for 10 minutes, wherein the deoxidizing gas introduced is argon; S9, 50℃ water cooling, waiting for the molten steel to cool and form a billet, sampling the formed billet, and testing the chemical composition, mechanical properties and appearance quality of the samples to ensure that the product quality meets the standards.

[0023] In this embodiment, the method also controls the composition of the molten steel, and can effectively integrate zinc-manganese alloy into it, thereby improving the structural strength of the final product. When the molten steel is finally tapped, external impurities can be effectively prevented from entering the molten steel by introducing inert gas stirring, thereby ensuring the quality of the steel billet after cooling. The overall method has good practical application effect. Example 4

[0024] See also Figure 1 The present invention provides a technical solution: a converter steelmaking process, comprising the following steps: S1. Prepare molten iron for steelmaking, make the temperature of molten iron ≥1250℃, ensure P≤0.15%, Cr≤0.35% in molten iron, and ensure that the molten iron is free of impurities; S2, prepare scrap steel, first add the scrap steel into an ultrasonic cleaning device, add a cleaning solution at 65°C, perform ultrasonic cleaning on the scrap steel, and segment the scrap steel, first add molten iron into a converter, and after 10 minutes, add the segmented scrap steel into the converter, with the mass ratio of molten iron to scrap steel being 1:2; S3. Use an oxygen lance to blow oxygen into the converter. During the oxygen blowing process, adjust the angle and position of the oxygen lance every 2 minutes to ensure that the oxygen is in full contact with the molten pool. S4. Control the pressure of oxygen blowing. The specific control scheme is: control the oxygen pressure to 1.0MPa during 0-10min of oxygen blowing, control the oxygen pressure to 1.7MPa during 11-15min, control the oxygen pressure to 1.5MPa during 16-20min, and control the oxygen pressure to 1.8MPa during 21-26min; S5, controlling the temperature of the molten steel to 1700°C, and filling the slag therein, wherein the slag is lime and light-burned dolomite, wherein the filling slag is 14% of the total mass of the molten steel, and the mass ratio of lime to light-burned dolomite in the slag is 1.2:2.3; S6. By adding alloying elements into the molten steel, the composition of the molten steel is controlled. In this process, the molten steel needs to be sampled and analyzed to monitor the composition changes of the molten steel in real time. The added alloying element is zinc-manganese alloy; S7. Find a suitable mold and clean the inside of the mold; S8, introducing molten steel into the mold, introducing inert gas therein, and continuously stirring for 8 minutes, wherein the deoxidizing gas introduced is argon; S9, water cooling at 60℃, waiting for the molten steel to cool and form a billet, sampling the formed billet, and testing the chemical composition, mechanical properties and appearance quality of the samples to ensure that the product quality meets the standards.

[0025] In this embodiment, the method can ensure the cleanliness of the scrap steel by pre-treating the obtained scrap steel, and the surface is free of oil and impurities, thereby ensuring the quality of the final product. At the same time, the oxygen blowing process in the converter can be accurately controlled in different time periods, so that the blown oxygen can be effectively circulated, thereby ensuring the overall steelmaking effect and improving the quality of the final product. The composition of the molten steel is also controlled in the method, and zinc-manganese alloy can be effectively integrated into it, thereby improving the structural strength of the final product. When the molten steel is finally tapped, external impurities can be effectively prevented from entering the molten steel by introducing inert gas stirring, thereby ensuring the quality of the billet after cooling. The overall method has good practical application effect.

[0026] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A converter steelmaking process, characterized in that: The steps include: S1, prepare molten iron for steelmaking; S2, prepare scrap steel and add the two into the converter; S3, using an oxygen blowing gun to blow oxygen into the converter; S4. Control the pressure of oxygen blowing; S5, controlling the temperature of the molten steel and filling the slag inside; S6. Control the composition of molten steel; S7. Find a suitable mold; S8, introducing molten steel into the mold, introducing inert gas into the mold, and continuously stirring for a period of time; S9, waiting for the molten steel to cool and form a steel billet.

2. A converter steelmaking process according to claim 1, characterized in that: In S1, molten iron for steelmaking is prepared, and the temperature of the molten iron is ≥1250° C., and the mass content of P in the molten iron is ≤0.15%, and Cr is ≤0.35%.

3. A converter steelmaking process according to claim 1, characterized in that: In S2, scrap steel is prepared, firstly the scrap steel is added into an ultrasonic cleaning device, a cleaning liquid at 60-70° C. is added, the scrap steel is ultrasonically cleaned, and the scrap steel is segmented; First add molten iron into the converter, and after 5-10 minutes, add the segmented scrap steel into the converter, with the mass ratio of molten iron to scrap steel being 1:

2.

4. A converter steelmaking process according to claim 1, characterized in that: In S3, oxygen is blown into the converter by using an oxygen blowing lance. During the oxygen blowing process, the angle and position of the oxygen blowing lance are adjusted every 1-2 minutes to ensure that oxygen is in full contact with the molten pool.

5. The converter steelmaking process according to claim 1, characterized in that: In S4, the pressure of oxygen blowing is controlled, and the specific control scheme is: the oxygen pressure is controlled to be 0.8-1.0 MPa during 0-10 minutes of oxygen blowing, the oxygen pressure is controlled to be 1.4-1.7 MPa during 11-15 minutes, the oxygen pressure is controlled to be 1.3-1.5 MPa during 16-20 minutes, and the oxygen pressure is controlled to be 1.6-1.9 MPa during 21-26 minutes.

6. A converter steelmaking process according to claim 1, characterized in that: In S5, the temperature of the molten steel is controlled to 1500-1700°C, and slag is filled therein, wherein the slag is lime and light-burned dolomite, wherein the filled slag accounts for 10-15% of the total mass of the molten steel, and the mass ratio of lime to light-burned dolomite in the slag is 1.2:2.

3.

7. The converter steelmaking process according to claim 1, characterized in that: In S6, the composition of the molten steel is controlled by adding alloy elements into the molten steel. During this process, the molten steel is sampled and analyzed to monitor the composition changes of the molten steel in real time. The added alloy element is zinc-manganese alloy.

8. The converter steelmaking process according to claim 1, characterized in that: In S7, a suitable mold is found and the inside of the mold is cleaned.

9. The converter steelmaking process according to claim 1, characterized in that: In the step S8, molten steel is introduced into the mold, and an inert gas is introduced thereinto, and stirring is continued for 5-10 minutes, wherein the inert gas introduced is argon.

10. The converter steelmaking process according to claim 1, characterized in that: In S9, the molten steel is cooled and formed into a billet, samples are taken from the formed billet, and the chemical composition, mechanical properties and appearance quality of the samples are tested to ensure that the product quality meets the standards, wherein the water cooling temperature is 40-60°C.