Glass laminate and method for producing glass laminate
By forming and laser processing the printing layer on the second main surface of the glass laminate, the problem of unclear boundary lines between the glass substrate and the printing layer is solved, and the boundary lines are clearly displayed and the visibility of the display device is improved.
Patent Information
- Application Number
- CN202380023142.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-08-10
- Filing Date
- 2023-02-17
- Publication Date
- 2024-10-15
AI Technical Summary
The existing glass laminate has light leakage on the boundary line between the glass substrate and the printing layer, resulting in unclear boundary lines.
By forming a printing layer on the second main surface of the glass substrate and removing part of the printing layer using laser processing, a boundary line end portion with a peak and valley value of less than 20 μm and a slope of more than 0.1 is formed to clearly display the boundary line. The wavelength of the laser is 300nm~1100nm, and the scanning speed is 1000mm/s~8000mm/s.
The boundary line between the glass substrate and the printing layer is clear, the visibility and design of the display device are improved, and the boundary line between the printing layer and the display area is ensured to be clear.
Smart Images

Figure CN118786101A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a glass laminate and a method for producing the glass laminate. Background Art
[0002] In display devices such as car navigation devices and smart phones, cover materials are used as front panels of touch panels and display panels. As such cover materials, it is known that a glass laminate is used, and the glass laminate has a light-shielding printed layer (decorative layer) on the periphery of one main surface of a glass substrate (transparent plate) (for example, refer to Patent Document 1). For the glass laminate described in Patent Document 1, a technology is disclosed in which a convex and concave shape is provided at the end of the printed layer in a top view of one main surface to reduce the color difference of the boundary between the glass substrate and the printed layer so that it becomes inconspicuous.
[0003] Prior art literature
[0004] Patent Literature
[0005] Patent Document 1: Japanese Patent Application Publication No. 2019-010871 Summary of the invention
[0006] However, in the technology of Patent Document 1, light leakage occurs at the boundary between the glass substrate and the printed layer, so the boundary line becomes unclear, and there is room for improvement in this respect.
[0007] The present invention has been made in view of the above-mentioned problems, and an object of the present invention is to provide a glass laminate and a method for producing the glass laminate, which can provide a clear boundary line between a glass base and a printed layer in a plan view.
[0008] In order to solve the above-mentioned problems and achieve the purpose, the glass laminate of the present invention comprises: a glass substrate having a first main surface and a second main surface, and a first printed layer laminated on a portion of the second main surface; in a top view of the first printed layer observed from the second main surface side, the PV value of the end of the first printed layer forming a boundary line with the second main surface is less than 20 μm, in a cross-sectional view of the first printed layer, the average thickness of the first printed layer is greater than 2.0 μm, and the value obtained by dividing the thickness direction distance by the horizontal direction distance between two different points set at the end is greater than 0.1.
[0009] In order to solve the above-mentioned problems and achieve the purpose, the manufacturing method of the glass laminate of the present invention has the following steps: for a glass substrate having a first main surface and a second main surface, a first printed layer is formed on the second main surface, and the first printed layer is irradiated with a laser to remove a part of the first printed layer to form an end portion serving as a boundary line with the second main surface; the irradiation conditions of the above-mentioned laser when forming the end portion are a wavelength of 300nm to 1100nm, an irradiation interval of less than 100μm, and a scanning speed of 1000mm / s to 8000mm / s.
[0010] According to the present invention, the boundary line between the glass substrate and the printed layer can be made clear in a plan view. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 This is a schematic diagram showing a vehicle-mounted display device including the glass laminate according to the present embodiment.
[0012] Figure 2 It is a cross-sectional view schematically showing a glass laminate.
[0013] Figure 3 This is a plan view of the glass base body viewed from the second main surface side.
[0014] Figure 4 is the magnified representation equivalent to Figure 3 Electron micrograph of part A.
[0015] Figure 5 This is a graph showing an example of the relationship between the film thickness of the printed layer and the horizontal distance from the end portion.
[0016] Figure 6 This is a schematic diagram showing the configuration of a laser irradiation device for removing the remaining portion of the printed layer to form an edge portion.
[0017] Figure 7 It is a schematic cross-sectional view showing the step of forming a printed layer on a glass substrate by transfer decoration.
[0018] Figure 8 It is a schematic cross-sectional view showing the step of forming a printed layer on a glass substrate by transfer decoration.
[0019] Fig. 9 This is a plan view showing an example of a printed layer in which openings are formed.
[0020] Fig.10 It is a schematic cross-sectional view showing a decorative printed layer which is stacked on the printed layer and fills the opening. DETAILED DESCRIPTION
[0021] The preferred embodiment of the present invention is described in detail below with reference to the accompanying drawings. It should be noted that the present invention is not limited to the embodiment. In addition, when there are multiple embodiments, an embodiment composed of a combination of the embodiments is also included. In addition, the numerical value includes a rounded range. In addition, in this specification, the expression of a numerical range such as "α to β" means "above α and below β".
[0022] (In-vehicle display device)
[0023] Figure 1 Schematic diagram showing a vehicle-mounted display device having a glass laminate according to the present embodiment. Figure 1 As shown, the vehicle-mounted display device 2 is a display device installed in a vehicle, for example, installed in front of the steering shaft 1 in the vehicle. The vehicle-mounted display device 2 includes a display panel 3 and a glass laminate 10. The display panel 3 displays images such as a car navigation screen, various instruments such as a speedometer, and a start button. The glass laminate 10 is used as a cover material for the surface (front) of the display panel 3. However, Figure 1 The configuration is an example, and the vehicle-mounted display device using the glass laminate 10 can have any configuration. In addition, the glass laminate 10 is not limited to being used as a cover material for the surface of a vehicle-mounted display device, and can also be used for any purpose including a cover material for a display device such as a smartphone.
[0024] (Glass Laminate)
[0025] Figure 2 : is a cross-sectional view showing an overview of a glass laminate. Figure 2 As shown in FIG. 1 , the glass laminate 10 is a transparent plate-shaped glass component, comprising a glass base (glass substrate) 11, an AG layer 12, an AR layer 13, an AFP layer 14, and a printed layer (first printed layer) 15. In the figure, the stacking direction of each layer is referred to as a thickness direction, and the direction perpendicular to the thickness direction and parallel to the main surface of the glass base 11 described later is referred to as a horizontal direction.
[0026] The glass substrate 11 includes a first main surface 11A and a second main surface 11B facing each other. An AG layer 12, an AR layer 13, and an AFP layer 14 are sequentially stacked on the first main surface 11A. In addition, a printed layer 15 is stacked on the periphery of the second main surface 11B. When the glass laminate 10 is mounted on a vehicle-mounted display device 2 (mounted object), for example, the first main surface 11A side is exposed to the outside, and the second main surface 11B side faces the mounted object (display panel 3). It should be noted that transparency here means transmission of visible light.
[0027] The glass substrate 11 is formed of general glass. Specifically, the glass substrate 11 can use alkali-free glass, soda-lime glass, soda-lime silicate glass, aluminosilicate glass, borosilicate glass, lithium aluminosilicate glass, borosilicate glass, etc. In addition, when used for the glass laminate 10, the glass substrate 11 is preferably aluminosilicate glass or lithium aluminosilicate glass, which can be easily applied with large stress through strengthening treatment even if the thickness is thin, and high-strength glass can be obtained. The glass substrate 11 is preferably strengthened by chemical strengthening treatment, for example. This chemical strengthening treatment is usually performed by immersing the glass substrate 11 formed into a predetermined shape in a molten salt containing an alkali metal.
[0028] The shape of the glass substrate 11 used for the glass laminate 10 may be not only Figure 2 The flat shape shown may also be a complex three-dimensional curved shape including one or more curved or bent portions. In this case, the AG layer 12, AR layer 13, AFP layer 14 and printed layer 15 stacked on the glass substrate 11 deform according to the shape of the glass substrate 11.
[0029] The thickness of the glass substrate 11 is preferably 0.3 mm to 5.0 mm, more preferably 0.8 mm to 3.0 mm, and further preferably 1.0 mm to 2.5 mm. By setting the thickness within this range, it is possible to achieve both lightweight and strength of the glass substrate 11, and to form a cover material for a vehicle-mounted display device with improved design. It should be noted that the thickness of the glass substrate 11 refers to the distance in the normal direction between the first main surface 11A and the second main surface 11B.
[0030] The AG (Anti-Glare) layer 12 is an anti-glare layer provided on the first main surface 11A side of the glass substrate 11 to impart anti-glare properties to the glass laminate 10. The AG layer 12 has a concavo-convex shape formed on the first main surface 11A side of the glass substrate 11. The concavo-convex shape may be formed directly on the first main surface 11A of the glass substrate 11, or may be formed by a layer composed of a material different from the glass substrate 11. The surface roughness (root mean square roughness, RMS) of the concavo-convex shape is preferably 15nm to 1000nm, and more preferably 10nm to 500nm. It should be noted that the AG layer 12 may be realized by imparting a concavo-convex shape by subjecting the first main surface 11A of the glass substrate 11 to an anti-glare treatment and an etching treatment. In addition, the AG layer 12 may be realized by using a coating film in which particles having an arbitrary refractive index are dispersed on the first main surface 11A of the glass substrate 11, or by forming a concavo-convex shape on the main surface of a bonded transparent resin film.
[0031] The AR (Anti-Reflection) layer 13 is an anti-reflection layer that reduces the reflectivity of the glass laminate 10. In addition to reducing the glare caused by the reflection of light, it also improves the visibility of the display device when used in a display device. The composition of the AR layer 13 is not particularly limited as long as it can suppress the reflection of light. For example, it can be a composition formed by alternating layers of a high refractive index layer with a refractive index of 1.9 or more at a wavelength of 550nm and a low refractive index layer with a refractive index of 1.6 or less at a wavelength of 550nm. The AR layer 13 is provided on the first main surface 11A side of the glass substrate 11. Figure 2 In the example shown in FIG. 1 , the AR layer 13 is provided on the AG layer 12 , but may be provided directly on the first main surface 11A of the glass substrate 11 .
[0032] The AFP (Anti-Finger-Print) layer 14 is an anti-fouling layer that has the function of inhibiting the adhesion of various dirt such as fingerprints, sweat, and dust, making the dirt less noticeable, and keeping the display surface clean. The AFP layer 14 is arranged on the first main surface 11A side of the glass substrate 11, but from the perspective of the characteristics of the anti-fouling layer, it is preferably formed on the outermost surface of the glass laminate 10. The AFP layer 14 is preferably composed of a fluorine-containing organic compound (a compound having a fluorine-containing organic group) that can impart anti-fouling properties, water repellency, and oil repellency. As the fluorine-containing organic compound, for example, a fluorine-containing organic silicon compound can be cited.
[0033] The AG layer 12, AR layer 13, and AFP layer 14 are examples and can be appropriately changed within the scope of the functions of each layer. In addition, the AG layer 12, AR layer 13, and AFP layer 14 are not necessarily required structures, and depending on the structure of the glass laminate 10, a part of the AG layer 12, AR layer 13, and AFP layer 14 may not be provided.
[0034] (Printing layer)
[0035] Figure 3 This is a top view of the glass substrate observed from the second main surface side. Figure 3 As shown, the printed layer 15 is provided on the second main surface 11B of the glass substrate 11. The printed layer 15 is provided on at least a portion of the peripheral portion of the second main surface 11B. The peripheral portion of the second main surface 11B refers to a band-shaped area from an edge portion away from the center of the second main surface 11B toward the center of the second main surface 11B. The printed layer 15 is formed on the entire periphery of the peripheral portion, or at least a portion of the peripheral portion. Usually, the printed layer 15 is formed in a band shape surrounding the outer periphery of the glass substrate 11. Figure 3In the example of FIG. 1 , the printed layer 15 surrounds the entire periphery of the second main surface 11B, and the area surrounded by the printed layer 15 becomes a display area 16 (also referred to as an opening). The printed layer 15 is formed, for example, to hide wiring components disposed in the periphery of the display panel 3 so that the outside of the display area 16 cannot be seen from the observer side, thereby improving the design of the display device.
[0036] The printed layer 15 has an end portion 15A at an inner side of the center portion (display region 16) of the second main surface 11B. When the printed layer 15 is viewed from the second main surface 11B, the end portion 15A forms a boundary 17 between the exposed second main surface 11B (display region 16) and the printed layer 15.
[0037] The printed layer 15 can be formed, for example, by a method of printing ink. The printing method is not particularly limited, and preferred methods include inkjet printing, screen printing, and transfer decoration. Ink can be used without particular limitation. As ink, inorganic inks containing ceramic calcined bodies and organic inks containing colorants such as dyes or pigments and organic resins can be used. It should be noted that the printed layer 15 is formed, for example, in black, but if the light-shielding property is high, it is not limited to black, and can also be printed with patterns such as wood grain.
[0038] The printing layer 15 is formed to have a film thickness (thickness) greater than 2.0 μm using the above-mentioned printing method. The film thickness of the printing layer 15 is an average thickness. If the film thickness of the printing layer 15 is greater than 2.0 μm, the light shielding property of the printing layer 15 is sufficient, visibility can be properly guaranteed, and poor contact between various components and the printing surface can be prevented. The film thickness is preferably 20.0 μm or less. If the film thickness is 20.0 μm or less, when the glass substrate 11 and the display panel 3 ( Figure 1 ), bubbles are not easily left due to the printing step difference. The lower limit of the film thickness of the printed layer 15 is preferably 2.5 μm or more, more preferably 3.0 μm or more, further preferably 5.0 μm or more, and particularly preferably greater than 5.0 μm. In addition, the upper limit is more preferably 15.0 μm or less. That is, the film thickness is preferably formed to be greater than 2.0 μm and less than 20.0 μm, more preferably formed to be 5.0 μm to 15.0 μm, and further preferably formed to be greater than 5.0 μm and less than 15.0 μm.
[0039] As described above, the printed layer 15 preferably has the end 15A exposed, thereby forming the boundary line 17 with the second main surface 11B (display area 16), so that the boundary line 17 is made clear. The inventors have found a configuration in which the boundary line 17 is made clear by designing the shape of the end 15A. The shape of the end 15A of the printed layer 15 is described below. Figure 4 is the magnified representation equivalent to Figure 3 Electron micrograph of part A. Figure 5 1 is a graph showing an example of the relationship between the film thickness of the printed layer 15 and the horizontal distance from the end. Figure 5 In FIG. 1 , a curve equivalent to the cross-sectional shape of the printed layer 15 is shown by plotting the relationship between the film thickness of the printed layer 15 and the horizontal distance from the end portion 15A.
[0040] like Figure 4 As shown, in the top view observed from the second main surface 11B side, continuous projections and depressions 20 are formed at the end 15A of the printed layer 15. The projections and depressions 20 are projections and depressions to a degree that cannot be seen by the naked eye. In this configuration, the PV (Peak to Valley) value of the projections and depressions 20 is less than 20 μm. The PV value is a value representing the difference between the peak and the valley of the projections and depressions 20 in the reference length in the top view observed from the second main surface 11B side (maximum height value). By making the PV value less than 20 μm, it is possible to suppress light leakage from the end 15A of the printed layer 15 and make the boundary line 17 clear. The PV value of the projections and depressions 20 is preferably less than 13 μm, and more preferably less than 10 μm. It should be noted that the smaller the PV value of the projections and depressions 20, the better, so the lower limit is not particularly limited, for example, it is greater than 0 μm, and can be greater than 0.1 μm.
[0041] On the other hand, if the thickness of the printed layer 15 in the end 15A is thin, that is, the slope of the thickness in the end 15A is gentle, the light shielding property is reduced even if the PV value of the concavo-convex 20 is less than 20 μm, thereby easily causing light leakage and blurring the boundary line.
[0042] Therefore, in this configuration, the PV value of the concavo-convex 20 is specified and the appropriate slope of the end portion 15A is specified. Figure 5 To illustrate, when the printed layer 15 is observed in cross section, two different points P1 and P2 in the thickness direction are set at the end 15A of the printed layer 15, and the value obtained by dividing the distance Lt (μm) in the thickness direction by the horizontal distance Lh (μm) between the two points P1 and P2 is used as the slope of the end 15A. In this configuration, the value representing the slope of the end 15A is 0.1 or more. The value representing the slope of the end 15A is preferably 0.5 or more, and more preferably 1.0 or more. The larger the value representing the slope of the end 15A, the clearer the boundary, so the upper limit is not particularly limited, for example, 40 or less. It should be noted that the two points P1 and P2 can also be arbitrary points, but in order to accurately calculate the slope of the end 15A, in this embodiment, point P1 is set to a point where the thickness reaches 10% of the film thickness t from the second main surface 11B, and point P2 is set to a point where the thickness reaches 50% of the film thickness t from the second main surface 11B.
[0043] Thus, by making the PV value of the concavo-convex 20 formed at the end 15A of the printed layer 15 less than 20 μm and making the value obtained by dividing the thickness direction distance Lt by the horizontal direction distance Lh between two different points P1 and P2 set in the thickness direction of the end 15A of the printed layer 15 to be 0.1 or more, it is possible to suppress bleeding of the edge of the boundary line 17. Therefore, the boundary line 17 between the printed layer 15 and the display area can be made clear.
[0044] Thus, the end 15A of the printed layer 15 is required to be flat in a plan view and have a steep slope in a cross-sectional view. In this configuration, after the printed layer 15 is formed, for example, the remaining portion of the printed layer 15 can be removed (trimmed) by laser processing to form the end 15A into an appropriate shape. Laser processing is described below.
[0045] (Method for producing glass laminate)
[0046] Next, a method for manufacturing the glass laminate 10 is described. In this embodiment, the method includes the following steps: for a glass substrate having a first main surface and a second main surface, a first printed layer is formed on the second main surface, and a laser is irradiated on the first printed layer to remove a portion of the first printed layer to form an end portion that becomes a boundary line with the second main surface.
[0047] First, a glass substrate 11 is prepared in which the AG layer 12, the AR layer 13, and the AFP layer 14 are sequentially laminated on the first main surface 11A of the glass substrate 11. In this case, the glass substrate 11 is bent into a predetermined shape (three-dimensional shape) in advance and then subjected to chemical strengthening treatment.
[0048] Next, in the prepared glass substrate 11, a printed layer 15 is formed on the second main surface 11B of the glass substrate 11 (a process of forming a first printed layer). As a method for forming the printed layer 15, an inkjet method can be cited. The inkjet method refers to the process of ejecting tiny droplets of liquid ink from a nozzle in a pulsed state to form a predetermined pattern on the second main surface 11B. Specifically, the glass substrate 11 is positioned with the origin of the nozzle as a reference, and based on the command from the control device, the nozzle is ejected while moving the ink on the second main surface 11B of the glass substrate 11 approximately parallel to the second main surface 11B. As a result, dot-shaped ink is continuously formed to form a printed layer 15 of a predetermined pattern.
[0049] The inkjet method generally forms a pattern while moving the nozzle linearly in one direction. Figure 3When the printed layer 15 shown is in the shape of a frame, it is preferably printed in four linear patterns constituting each side of the frame. At this time, the linear patterns are all printed to be wider than the actual width of the pattern of the printed layer 15, that is, the remaining part is included in the end side close to the central part of the second main surface 11B. The thickness of the printed layer 15 can be adjusted by controlling the ejection amount or ejection interval of the ink ejected from the nozzle. In the case of thickening, it is sufficient to increase the ejection amount or narrow the ejection interval. In the case of thinning, it is sufficient to reduce the ejection amount or increase the ejection interval. Thereafter, the printed layer 15 is formed by drying and calcining the ink to solidify the ink. It should be noted that the order of forming each layer is not limited to this, and after the printed layer 15 is formed on the second main surface 11B of the glass substrate 11, the AG layer 12, the AR layer 13 and the AFP layer 14 can be formed on the first main surface 11A of the glass substrate 11.
[0050] Next, the printed layer 15 is irradiated with laser light to perform laser processing to remove the remaining portion, which is a part of the printed layer 15, thereby forming the end portion 15A of the printed layer 15 (the step of forming the end portion). Figure 6 The laser irradiation device 30 shown in the figure. The laser irradiation device 30 irradiates the printed layer 15 with a laser beam L having a wavelength that the printed layer 15 absorbs from the first main surface 11A side to remove the remaining portion of the printed layer 15. In this configuration, the laser beam L is irradiated to the printed layer 15 from the first main surface 11A side opposite to the second main surface 11B on which the printed layer 15 is formed. As a result, the PV value of the concavo-convex 20 formed at the end 15A of the printed layer 15 can be more effectively reduced. It should be noted that the laser beam L may be irradiated to the printed layer 15 from the second main surface 11B side.
[0051] The laser irradiation device 30 irradiates the printed layer 15 with a laser beam L having absorption properties, thereby performing ablation processing on the printed layer 15. The laser irradiation device 30 is composed of a laser oscillator 31, a scanner 32, and a focusing lens 33. The laser oscillator 31 oscillates a laser beam L having a wavelength that is absorbed by the printed layer 15 at a predetermined irradiation time based on a control signal from a control device (not shown). The focusing lens 33 focuses the laser beam L oscillated from the laser oscillator 31 and guides it to the printed layer 15. The scanner 32 is disposed between the laser oscillator 31 and the focusing lens 33, and deflects the optical axis of the laser beam L oscillated from the laser oscillator 31 toward the focusing lens 33. The scanner 32 includes a reflecting mirror (not shown), and by rotating the reflecting mirror around an axis, the laser beam L deflected by the reflecting mirror is scanned on the printed layer 15. As a result, as Figure 6 As shown, by irradiation with the laser beam L, the remaining portion 15B of the printed layer 15 is removed, and an end portion 15A serving as a boundary line with the second main surface 11B is formed.
[0052] In the present embodiment, the processing conditions of the laser processing are a wavelength of 300 nm to 1100 nm, an irradiation interval of less than 100 μm, and a scanning speed of 1000 mm / s to 8000 mm / s. The wavelength of the laser light L is preferably 500 nm to 1100 nm. In addition, the irradiation interval of the laser light L is preferably less than 70 μm. In addition, the scanning speed is preferably 1000 mm / s to 4000 mm / s. The irradiation interval is the interval between laser marks intermittently irradiated to the printed layer 15 when scanning on the printed layer 15, and is calculated by dividing the scanning speed by the irradiation frequency of the laser light L.
[0053] Thus, in this embodiment, by making the wavelength, irradiation interval, and scanning speed of the laser light L all within the prescribed range, the PV value of the end 15A of the printed layer 15 processed by laser can be made less than 20 μm, and the value obtained by dividing the thickness direction distance Lt by the horizontal direction distance Lh between two different points P1 and P2 set in the thickness direction of the end 15A of the printed layer 15 can be made greater than 0.1. In addition, by irradiating the printed layer 15 with the laser light L from the first main surface 11A side, the PV value of the end 15A of the printed layer 15 can be more effectively reduced. Therefore, the boundary line 17 between the printed layer 15 and the display area can be made clear.
[0054] In this embodiment, it is preferred to further remove the printing layer residue. When the remaining portion of the printing layer 15 is trimmed by laser, a portion of the printing layer 15 may not be completely removed and may remain as printing layer residue. Such printing layer residue may be seen as dirt under strong external light, so it is preferred to remove it. By removing the printing layer residue, the appearance of the opening is improved, and the image displayed by the display is easier to see.
[0055] The printed layer residue is removed by, for example, irradiating the second main surface with plasma. Preferably, oxygen radicals are used as plasma. By irradiating the printed layer residue with oxygen radicals, carbon in the printed layer residue reacts with the oxygen radicals, and the printed layer residue is decomposed and removed.
[0056] The treatment temperature of the glass during plasma irradiation is not particularly limited, but is preferably 100 to 220 degrees. When the treatment temperature is within the above range, the treatment of the printed layer residue can be promoted, and damage to the printed layer 15 itself due to heat can be suppressed.
[0057] (Variation Example)
[0058] Next, a modification of the present embodiment will be described.
[0059] (Example of forming a printed layer by transfer decoration)
[0060] In the above-mentioned embodiment, the method of forming the printed layer by the inkjet method has been described, but the present invention is not limited thereto, and the printed layer may be formed by the screen printing method or the transfer decoration method. Figure 7-8 2 is a schematic cross-sectional view showing the steps of forming a printed layer on a glass substrate by transfer decoration. Figure 7 , 8 In the figure, the AG layer 12, the AR layer 13, and the AFP layer 14 stacked on the glass substrate 11 are omitted.
[0061] In the transfer decoration method, a transfer sheet 40 having a printed layer 15 is brought into close contact with a glass substrate 11 under heating conditions to transfer the printed layer 15 to the glass substrate 11. Figure 7 As shown, the transfer substrate (e.g., film) 41 and the print layer 15 are stacked to form a structure. The transfer substrate 41 is formed of a resin material or the like and supports the print layer 15. The transfer substrate 41 is preferably formed to a thickness of 20 μm to 100 μm. The print layer 15 of this embodiment is formed in a planar shape of a pattern to be transferred and is supported on the transfer substrate 41. The print layer 15 is preferably formed to a thickness of 1 μm to 20 μm.
[0062] like Figure 7 As shown, the glass substrate 11 and the transfer sheet 40 are arranged so that the second main surface 11B of the glass substrate 11 faces the printed layer 15 of the transfer sheet 40. Next, the transfer sheet 40 (transfer substrate 41) is softened by heating the transfer sheet 40. The heating method may be infrared rays, superheated steam, a hot plate, etc.
[0063] In this state, when the space between the glass substrate 11 and the transfer sheet 40 is decompressed to be substantially vacuum, the softened transfer sheet 40 is shaped by the differential pressure and comes into close contact with the second main surface 11B of the glass substrate 11 .
[0064] Finally, if Figure 8 As shown, by peeling the transfer base material 41 of the transfer sheet 40 from the glass base 11 , the printed layer 15 remains on the second main surface 11B, and the printed layer 15 can be transferred to the second main surface 11B.
[0065] In the transfer decoration method, accurate alignment of the glass substrate 11 and the printed layer 15 is required, but since the excess portion can be removed by the above-mentioned laser processing, the necessity of laser processing increases, and the printed layer 15 can be easily and accurately formed by transfer decoration.
[0066] (Example of overlapping printing of logo etc.)
[0067] Fig. 9 It is a plan view showing an example of the printed layer 15 in which the openings 19 are formed. Fig.101 is a schematic cross-sectional view showing a decorative printed layer stacked on the printed layer and filling the opening. In recent years, a logo or a logo of a product or company is displayed on the printed layer 15. In this case, Fig. 9 As shown, a portion of the printed layer 15 is removed to form an opening 19 along the shape of a logo or emblem, and therefore, it is required to improve the visibility of the edge of the opening 19. It should be noted that the opening in this embodiment refers to a portion where the printed layer 15 is not formed.
[0068] In this example, the opening 19 is formed by removing a portion of the printed layer 15 by laser processing as described above. Therefore, by making the PV value of the end 15A of the printed layer 15 constituting the outline of the opening 19 less than 20 μm, and making the value obtained by dividing the thickness direction distance Lt by the horizontal direction distance Lh between two different points P1 and P2 set in the thickness direction of the end 15A of the printed layer 15 to be 0.1 or more, the boundary line between the printed layer 15 and the display area can be made clear, thereby improving visibility.
[0069] In addition, if Fig.10 As shown, a decorative printed layer (second printed layer) 18 may be stacked on the printed layer 15. The decorative printed layer 18 may be stacked on the printed layer 15. Fig.10 As shown, the opening 19 may also be filled. The decorative printed layer 18 is a printed layer with different optical properties from the printed layer 15. The different optical properties refer to different color perception in the visible light region or different transmittance at a certain wavelength. For example, when the opening 19 is a logo or a logo, a decorative printed layer 18 of a color (white) that scatters visible light is used. Thus, by making the logo or logo clearly illuminated, visibility can be improved.
[0070] In addition, for example, by providing a decorative printed layer 18 with high infrared transmittance in the same color (black) as the printed layer 15 in the opening 19, a light-transmitting area for receiving infrared light or other operating light from a remote controller can be formed. Thus, a fingerprint authentication sensor, for example, can be provided in the light-transmitting area.
[0071] (Effect)
[0072] As described above, the glass laminate 10 of the present embodiment includes: a glass substrate 11 having a first main surface 11A and a second main surface 11B, and a printed layer 15 partially laminated on the second main surface 11B; in a plan view of the printed layer 15 viewed from the second main surface 11B side, the PV value of the end 15A of the printed layer 15 forming the boundary line 17 with the second main surface 11B is less than 20 μm, in a cross-sectional view of the printed layer 15, the average thickness of the printed layer 15 is greater than 2.0 μm, and the value obtained by dividing the distance Lt in the thickness direction by the distance Lh in the horizontal direction between two different points P1 and P2 set at the end 15A is 0.1 or more. As a result, the shape of the end 15A can be flat in a plan view and formed at a steep angle in a cross-sectional view, so that the boundary line between the printed layer 15 and the display area can be clear, thereby improving visibility.
[0073] In the glass laminate 10 of the present embodiment, when the average thickness of the printed layer 15 is greater than 5.0 μm, the light shielding property of the printed layer 15 can be sufficiently ensured, and the boundary between the printed layer 15 and the display area can be made clear, thereby improving visibility.
[0074] In the glass laminate 10 of this embodiment, if a decorative printed layer 18 having optical properties different from those of the printed layer 15 is provided on the printed layer 15 , various decoration methods can be realized, for example, by filling the decorative printed layer 18 in the opening 19 formed in the printed layer 15 .
[0075] In addition, in the glass laminate 10 of the present embodiment, if the AR layer 13 as the antireflection layer is provided on the first main surface 11A, glare due to reflection of light can be reduced, thereby improving visibility.
[0076] In addition, in the glass laminate 10 of the present embodiment, if the first main surface 11A has a concavo-convex shape with a surface roughness of 15 nm to 1000 nm, an anti-glare property can be imparted.
[0077] In the glass laminate 10 of the present embodiment, if the AFP layer 14 composed of a compound having a fluorine-containing organic group is provided on the first main surface 11A, adhesion of various dirt such as fingerprints to the glass laminate 10 can be suppressed, and the surface can be kept clean.
[0078] In addition, the manufacturing method of the glass laminate 10 of the present embodiment includes the following steps: for the glass substrate 11 having the first main surface 11A and the second main surface 11B, forming the printed layer 15 on the second main surface 11B, and irradiating the printed layer 15 with laser light to remove a part of the printed layer 15 to form an end 15A which becomes the boundary line 17 with the second main surface 11B; the irradiation conditions of the laser light when forming the end 15A are a wavelength of 300nm to 1100nm, an irradiation interval of less than 100μm, and a scanning speed of 1000mm / s to 8000mm / s. According to this configuration, the PV value of the end 15A of the printed layer 15 processed by laser light can be made less than 20μm, and the value obtained by dividing the thickness direction distance Lt by the horizontal direction distance Lh between two different points P1 and P2 set in the thickness direction of the end 15A of the printed layer 15 can be made 0.1 or more. Therefore, the boundary line 17 between the printed layer 15 and the display area can be made clear, thereby improving visibility.
[0079] In the method for manufacturing the glass laminate 10 of the present embodiment, when forming the end 15A, by irradiating the laser from the first main surface 11A side, the PV value of the end 15A of the printed layer 15 can be more effectively reduced, thereby improving the accuracy of laser processing.
[0080] In addition, in the manufacturing method of the glass laminate 10 of the present embodiment, when forming the printed layer 15, if the printed layer 15 is formed on the transfer substrate 41, the surface of the transfer substrate 41 on which the printed layer 15 is formed is brought into contact with the second main surface 11B of the glass base 11, and the printed layer 15 is transferred to the second main surface 11B, the printed layer 15 can be easily formed on the second main surface 11B.
[0081] The present disclosure describes the following inventions, but it should be noted that the inventions are not limited to these.
[0082] (1) A glass laminate comprising: a glass substrate having a first main surface and a second main surface, and a first printed layer laminated on a portion of the second main surface; in a top view of the first printed layer observed from the second main surface side, a PV value of an end portion of the first printed layer forming a boundary line with the second main surface is less than 20 μm, in a cross-sectional view of the first printed layer, an average thickness of the first printed layer is greater than 2.0 μm, and a value obtained by dividing a thickness direction distance by a horizontal direction distance between two different points set at the end portion is greater than 0.1.
[0083] (2) The glass laminate according to (1), wherein the average thickness of the first printed layer is thicker than 5.0 μm.
[0084] (3) The glass laminate according to (1) or (2), further comprising a second printed layer having optical properties different from those of the first printed layer on the first printed layer.
[0085] (4) The glass laminate according to any one of (1) to (3), further comprising an antireflection layer on the first main surface side.
[0086] (5) The glass laminate according to any one of (1) to (4), which has a concavo-convex shape on the first main surface side.
[0087] (6) The glass laminate according to any one of (1) to (5), further comprising an antifouling layer on the first main surface side, wherein the antifouling layer is composed of a compound having a fluorine-containing organic group.
[0088] (7) A method for manufacturing a glass laminate, comprising the following steps: for a glass substrate having a first main surface and a second main surface, forming a first printed layer on the second main surface, and irradiating the first printed layer with a laser to remove a portion of the first printed layer to form an end portion that serves as a boundary line with the second main surface; the laser irradiation conditions for forming the end portion are a wavelength of 300nm to 1100nm, an irradiation interval of less than 100μm, and a scanning speed of 1000mm / s to 8000mm / s.
[0089] (8) The method for producing a glass laminate according to (7), wherein the laser beam is irradiated from the first main surface side when the edge portion is formed.
[0090] (9) A method for manufacturing a glass laminate according to (7) or (8), wherein, when forming the first printed layer, the first printed layer is formed on a transfer substrate, the surface of the transfer substrate on which the first printed layer is formed is brought into contact with the second main surface of the glass substrate, and the first printed layer is transferred to the second main surface.
[0091] (10) The method for producing a glass laminate according to any one of (7) to (9), further comprising the step of irradiating the second main surface with plasma after irradiating the laser beam to remove residues of the printed layer.
[0092] Example
[0093] Next, examples will be described. It should be noted that the embodiments may be modified as long as the effects of the invention are exhibited.
[0094] First, an example of a glass laminate 10 is described. In this example, the visibility of the printed layer is evaluated for various glass laminates. The glass laminate used in the evaluation has a printed layer formed on the main surface of a glass substrate having a thickness of 1.1 mm by an inkjet method. In addition, the end of the printed layer is trimmed by laser processing. The conditions of the laser processing in this case are that the wavelength of the laser light is 1064 nm, the scanning speed is 2000 mm / s, and the irradiation frequency is 100 kHz.
[0095] Furthermore, the glass laminates of Examples 1 to 6 shown in Table 1 were prepared by varying the film thickness of the printed layer, the PV value of the concavity and convexity at the end, and the slope of the end.
[0096] [Table 1]
[0097]
[0098] The evaluation of visibility is determined by the OD value (Optical Density) at a position 20 μm away from the end 15A of the printed layer 15. The larger the OD value, the higher the visibility. In this embodiment, if the OD value is 5 or more, the visibility is good and the evaluation is expressed as A. In addition, if the OD value is 10 or more, the visibility is particularly good and the evaluation is expressed as A. + .
[0099] The film thickness distribution of the printed layer was measured by non-contact measurement based on a stage scanning laser probe method using NH-3MAS manufactured by Mitaka Optical Instruments Co., Ltd. Specifically, the second main surface 11B of the glass substrate 11 was used as a horizontal reference, and the film thickness was measured in the vertical direction at the boundary between the printed layer 15 and the second main surface 11B to obtain the following: Figure 5 The film thickness distribution curve shown in the example is changed according to the measurement position of the printed layer 15. Therefore, it is preferred that, for example, Figure 5 The film thickness distribution curves are obtained at different positions of the printed layer 15 moving in the paper direction. In this embodiment, the film thickness distribution curves are obtained at different multiple (5) positions in the printed layer 15.
[0100] The thickness of the printed layer was determined by averaging the thickness values at points 5 mm horizontally shifted from the rising start point at the end of the printed layer in the obtained plurality of (5) thickness distribution curves.
[0101] like Figure 5 As shown, when the printed layer 15 is observed in cross section, the slope of the end 15A of the printed layer 15 is a value obtained by setting two different points P1 and P2 in the thickness direction at the end 15A of the printed layer 15, and dividing the distance Lt in the thickness direction by the horizontal distance Lh between the two points P1 and P2. In this case, point P1 is a point where the thickness reaches 10% of the film thickness t from the second main surface 11B, and point P2 is a point where the thickness reaches 50% of the film thickness t from the second main surface 11B. In this embodiment, as described above, a plurality of (5) curves of film thickness distribution at different positions of the printed layer 15 are obtained. Therefore, the average value of the slope of the end 15A in each cross section (curve) of the printed layer 15 is used as the value of the slope of the end 15A.
[0102] The PV value is measured using an optical microscope (digital microscope VHX6000 manufactured by KEYENCE). Specifically, the boundary line 17 is photographed in a top view of the printed layer 15 at a magnification of 500 times and with incident illumination. In the shape of the concave-convex 20 of the boundary line 17 in the shooting area of 510μm×680μm, a predetermined center line (zero line) is set, for example. The point farthest from the center line is selected from the multiple convex vertices of the concave-convex 20, and the point farthest from the center line is selected from the multiple concave vertices, and the distance in the direction orthogonal to these center lines is set as the PV value. In this configuration, the PV value in each shooting area is measured for multiple locations (for example, 5 points) on the boundary line 17, and the average value is used as the PV value.
[0103] (Evaluation results)
[0104] As can be seen from Table 1, the glass laminate of Example 1 as an embodiment satisfies the prescribed conditions in terms of average film thickness, the value of the slope of the end 15A, and the PV value, so the OD value is above the prescribed threshold value, and good visibility can be ensured. In particular, in the glass laminate of Example 6 as an embodiment, the average film thickness of the printed layer 15 is 6.9 μm, and the value of the slope of the end 15A is 3.5, so that particularly good visibility can be ensured. On the other hand, since the glass laminates of Examples 2 to 5 as comparative examples do not satisfy the prescribed conditions, the OD values are smaller than the prescribed threshold value, and good visibility cannot be obtained.
[0105] (Printing layer residue removal experiment)
[0106] An experiment for removing the printed layer residue generated was conducted for the example where the printed layer residue was generated. Using an atmospheric pressure plasma device, the printed layer residue on the second main surface was irradiated with plasma under the following conditions.
[0107] <Plasma irradiation conditions>
[0108] Nozzle width: 20mm
[0109] Scanning speed: 50mm / s
[0110] Irradiation distance: 5mm
[0111] Processing temperature: 200 degrees
[0112] As a result of the irradiation, the printed layer residue on the second main surface was removed and could not be visually recognized even under observation with an optical microscope at a magnification of 500 times.
[0113] The above is a description of the embodiments of the present invention, but the embodiments are not limited to the contents of the embodiments. In addition, the above-mentioned constituent elements include elements that can be easily thought of by a person skilled in the art, substantially the same elements, and so-called elements of equivalent scope. Furthermore, the above-mentioned constituent elements can be appropriately combined. Furthermore, various omissions, substitutions or changes can be made to the constituent elements without departing from the scope of the above-mentioned embodiments. For example, in the present embodiment, the trimming of the end 15A of the printed layer 15 is performed by irradiation with the laser light L, but it can also be performed by dry etching using an etching gas that is reactive with the ink of the printed layer 15, for example.
[0114] The present invention is described in detail with reference to specific embodiments, but it is clear to those skilled in the art that various changes and modifications can be made without departing from the spirit and scope of the present invention. This application is based on Japanese patent applications (Japanese patent application 2022-027979) filed on February 25, 2022 and Japanese patent applications (Japanese patent application 2022-127965) filed on August 10, 2022, the contents of which are incorporated herein by reference.
[0115] Explanation of symbols
[0116] 10 Glass laminate
[0117] 11Glass substrate (glass substrate)
[0118] 11A 1st main surface
[0119] 11B Second main surface
[0120] 12AG layer (anti-glare layer)
[0121] 13AR layer (anti-reflection layer)
[0122] 14AFP layer (antifouling layer)
[0123] 15 printing layers (1st printing layer)
[0124] 15A terminal
[0125] 15B Remaining part
[0126] 16 display areas
[0127] 17Border Line
[0128] 18 Decorative printing layer (second printing layer)
[0129] 19 Opening
[0130] 20 Bump
[0131] 40 transfer film
[0132] 41 transfer substrate (film)
[0133] LLaser beam
[0134] Lh horizontal distance
[0135] Lt thickness direction distance
[0136] P1 point
[0137] P2 point
[0138] t Film thickness
Claims
1. A glass laminate comprising: a glass substrate having a first main surface and a second main surface, and a first printed layer laminated on a portion of the second main surface, In a plan view of the first printed layer viewed from the second main surface, a PV value of an end portion of a boundary line between the first printed layer and the second main surface is less than 20 μm. In a cross-sectional view of the first printed layer, the first printed layer has an average thickness greater than 2.0 μm, and a value obtained by dividing a thickness direction distance by a horizontal direction distance between two different points set at the end is greater than or equal to 0.
1.
2. The glass laminate according to claim 1, wherein: The first printed layer has an average thickness of more than 5.0 μm.
3. The glass laminate according to claim 1 or 2, wherein: A second printed layer having optical properties different from those of the first printed layer is provided on the first printed layer.
4. The glass laminate according to claim 1 or 2, wherein: An antireflection layer is provided on the first main surface side.
5. The glass laminate according to claim 1 or 2, wherein: The first main surface has a concavo-convex shape.
6. The glass laminate according to claim 1 or 2, wherein: An antifouling layer is provided on the first main surface side, and the antifouling layer is composed of a compound having a fluorine-containing organic group.
7. A method for manufacturing a glass laminate, comprising the following steps: For a glass substrate having a first main surface and a second main surface, a first printed layer is formed on the second main surface, and irradiating the first printed layer with laser light to remove a portion of the first printed layer to form an end portion that becomes a boundary line with the second main surface; The irradiation conditions of the laser when forming the end portion are a wavelength of 300 nm to 1100 nm, an irradiation interval of less than 100 μm, and a scanning speed of 1000 mm / s to 8000 mm / s.
8. The method for producing a glass laminate according to claim 7, wherein: When forming the end portion, the laser beam is irradiated from the first main surface side.
9. The method for producing a glass laminate according to claim 7 or 8, wherein: When forming the first printed layer, forming the first printing layer on the transfer substrate, The surface of the transfer base material on which the first printed layer is formed is brought into contact with the second main surface of the glass substrate, and the first printed layer is transferred onto the second main surface.
10. The method for producing a glass laminate according to claim 7 or 8, wherein: The further steps include: After the laser irradiation, the second main surface is irradiated with plasma to remove the residue of the printed layer.