Raw gas conveying pipeline and using method thereof

By using a composite lining structure of refractory brick support layer, sealing layer and heat insulation layer in the coke oven high temperature raw gas transportation pipeline, the problems of tar deposition and thermal insulation performance degradation in the coke oven high temperature raw gas transportation pipeline are solved, and the Stable transportation of high-temperature waste gas and investment savings.

CN118793852APending Publication Date: 2024-10-18ACRE COKING & REFRACTORY ENG CONSULTING CORP DALIAN MCC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411155392.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-22
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

Existing high-temperature waste gas transmission pipelines for coke ovens are prone to problems such as tar deposition and blockage, reduced thermal insulation performance, and high investment costs under high temperatures and corrosive environments. Moreover, commonly used lining structures are prone to shortened service life in long-term high-temperature environments. .

Method used

A composite sealed and insulated lining composed of a refractory brick support layer, a sealing layer and a heat insulation layer is used. The pipe body is made of ordinary carbon steel. The refractory brick support layer and sealing layer prevent tar penetration. The heat insulation layer provides heat preservation function and Set a circumferential expansion joint on the outside to compensate for thermal expansion, reduce investment and extend the life of the pipe lining.

Benefits of technology

It achieves long-distance stable transportation of high-temperature raw gas, avoids tar deposition and degradation of thermal insulation performance, reduces investment costs, and extends the service life of the pipeline lining.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118793852A_ABST
    Figure CN118793852A_ABST
Patent Text Reader

Abstract

The invention relates to a raw gas conveying pipeline and a using method thereof. The raw gas conveying pipeline comprises a pipeline body and a composite sealing heat insulation lining arranged in the pipeline body. The pipeline body is made of carbon steel, and the composite sealing heat insulation lining is composed of a refractory brick supporting layer, a sealing layer and a heat insulation layer which are sequentially arranged from inside to outside. According to the invention, while the pipeline investment is reduced and the service life of the pipeline lining is greatly prolonged, the problem that the heat insulation effect of the pipeline is invalid due to the fact that substances such as tar in the high-temperature raw gas permeate into the heat insulation layer is avoided, and long-distance stable conveying of the high-temperature raw gas in the direct reforming process is realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of coking production, and in particular to a coke oven high-temperature raw gas transmission pipeline and a use method thereof. Background Art

[0002] In order to cope with global climate change, the demand for hydrogen by production enterprises has increased dramatically. The high-temperature raw gas of 650-800℃ released during the coking process contains a large amount of H2, CH4, etc., which can be used as one of the low-cost sources of hydrogen. The existing raw gas treatment process is to spray the high-temperature raw gas from the coke oven with ammonia water to cool it down to 80-90℃, then send it to the chemical production unit for purification, and finally reform the purified clean gas; the process is complicated, the investment is high, and a large amount of sensible heat in the high-temperature raw gas is wasted.

[0003] The process of directly sending the high-temperature raw coal gas from the coke oven into the reforming furnace for direct reforming without cooling and purification can not only shorten the process flow and reduce equipment investment, but also utilize the sensible heat of the high-temperature raw coal gas itself to reduce production energy consumption; in addition, impurities such as tar and coking coal powder in the raw coal gas can be reformed to greatly increase the output of synthesis gas H2 and CO, which is a very promising hydrogen production technology.

[0004] The direct reforming process of high-temperature raw coal gas requires that the high-temperature raw coal gas be led out of the coke oven and directly transported to the reforming furnace. The composition of high-temperature raw coal gas is complex. In addition to combustible gases such as H2, CH4, and CO, it also contains tar, coal tar dust, and corrosive impurities such as H2S, NH3, and HCl. In order to prevent the heat loss of high-temperature raw coal gas and the deposition of substances such as tar to block the pipeline, a jacketed raw coal gas transmission pipeline structure is often used (such as Chinese patent applications with publication numbers CN 110778842 A and CN 114923123A). The raw coal gas is insulated and transported by passing heating fuel gas or high-temperature gas into the jacket. The jacket structure using refractory bricks is complex, the project investment is large, and it is easy to have problems such as leakage and even high-temperature graphite formation, which affects the safety of the combustible gas transportation in the pipeline. Since the temperature of high-temperature raw coal gas can reach 650-800℃, and the condensation temperature of tar therein is 400-565℃ under normal pressure, even if the jacket structure is not adopted, it is only necessary to adopt a reasonable insulation structure and control the flow rate of the raw coal gas to ensure that the temperature of the high-temperature raw coal gas before entering the reforming furnace is above 565℃, so as to avoid the tar in the high-temperature raw coal gas from being deposited in the pipeline.

[0005] Due to the high temperature and corrosive characteristics of high-temperature crude gas, when the insulation structure is set on the outside of the pipeline, the material requirements of the pipeline itself are very high, and special heat-resistant stainless steel is required, which will greatly increase the investment cost. If the insulation and anti-corrosion resistant material lining is set on the inside of the crude gas transmission pipeline, the pipeline can be made of ordinary carbon steel, which greatly reduces the investment. The commonly used lining structure is the castable lining structure, which is connected to the pipeline through anchor nails. However, due to the inconsistency of the expansion coefficients of the anchor nails and the castable, the castable layer is prone to cracking and falling off in a long-term high temperature environment, causing the service life of the crude gas transmission pipeline to drop sharply. For the lining structure using refractory bricks + insulation bricks, since tar will penetrate into the pores inside the insulation bricks through the ash joints and expansion joints of the heavy refractory bricks, the insulation performance of the insulation bricks will decrease, so the insulation performance of the crude gas transmission pipeline will also decrease rapidly, eventually leading to tar deposition and clogging of the pipeline. Summary of the invention

[0006] The present invention provides a raw coal gas transmission pipeline and a method for using the same. The pipeline adopts a composite sealing and heat-insulating lining composed of a refractory brick support layer, a sealing layer and a heat-insulating layer. The pipeline body is made of ordinary carbon steel. While reducing pipeline investment and greatly extending the life of the pipeline lining, it avoids the problem of failure of the pipeline insulation effect due to the penetration of tar and other substances in the high-temperature raw coal gas into the heat-insulating layer, thereby realizing the long-distance and stable transportation of high-temperature raw coal gas in the direct reforming process.

[0007] In order to achieve the above object, the present invention adopts the following technical solutions:

[0008] A raw gas transmission pipeline comprises a pipeline body and a composite sealing and heat-insulating lining arranged in the pipeline body; the pipeline body is made of carbon steel, and the composite sealing and heat-insulating lining consists of a refractory brick supporting layer, a sealing layer and a heat-insulating layer arranged in sequence from the inside to the outside.

[0009] Furthermore, the refractory brick support layer is a cylindrical structure formed by a number of high-strength refractory bricks, and the mortar joint is 2 to 3 mm; two adjacent high-strength refractory bricks are connected by groove and tongue bite; the thickness of the refractory brick support layer is at least 80 mm, and the high-strength refractory bricks are silicon-aluminum refractory bricks with a compressive strength of not less than 20 MPa.

[0010] Furthermore, the sealing layer is a cylindrical structure composed of sealing refractory bricks, the circumferential size of the sealing refractory bricks is larger than the circumferential size of the high-strength refractory bricks, the thickness of the sealing refractory bricks is not less than 50 mm, and the compressive strength is not less than 10 MPa; the sealing refractory bricks and the high-strength refractory bricks of the supporting layer are staggered.

[0011] Furthermore, the sealing layer is a cylindrical structure composed of refractory castables, the thickness of the sealing layer is not less than 50 mm, and the room temperature flexural strength of the refractory castables is not less than 2 MPa.

[0012] Furthermore, the sealing layer is a cylindrical structure made of a heat-resistant stainless steel plate, the thickness of the heat-resistant stainless steel plate is 0.2 to 2.0 mm; and the overlapping width of the heat-resistant stainless steel plate is at least 75 mm.

[0013] Furthermore, the thermal insulation layer is a cylindrical structure composed of thermal insulation bricks or thermal insulation castables, the thermal conductivity of the thermal insulation bricks or thermal insulation castables is less than 0.6W / m·K, and the thickness of the thermal insulation layer is not less than 50mm.

[0014] Furthermore, the refractory brick support layer and the sealing layer are provided with an axial expansion joint every 1 to 2 m along the axial direction of the pipeline, and the axial expansion joint is filled with a ceramic fiber blanket; the axial expansion joint of the refractory brick support layer and the axial expansion joint of the sealing layer are spaced more than 50 mm apart and are staggered.

[0015] Furthermore, an annular expansion joint is provided between the insulation layer and the sealing layer of the composite sealing insulation lining, or between the insulation layer and the pipeline body. The width of the annular expansion joint is 5 to 10 mm, and the ceramic fiber blanket is filled in the annular expansion joint.

[0016] Furthermore, an outer insulation layer is provided on the outside of the pipeline body.

[0017] A method for using a raw gas transmission pipeline comprises the following steps: before use, an external heat source is used to bake a composite sealing and heat-insulating lining; when the temperature of a refractory brick support layer reaches above 600°C, nitrogen is introduced to replace the gas inside the pipeline, and then the pipeline is put into use; during use, the flow rate of the high-temperature raw gas in the pipeline is controlled at 10 to 30 m / s.

[0018] Compared with the prior art, the present invention has the following beneficial effects:

[0019] (1) By adopting a composite sealing and heat-insulating lining composed of a refractory brick support layer, a sealing layer and a heat-insulating layer, and increasing the raw gas flow rate in the pipeline, the temperature of the high-temperature raw gas before entering the reforming furnace is ensured to be above 565°C, thereby preventing the tar in the high-temperature raw gas from being deposited in the pipeline;

[0020] (2) The pipeline lining structure has the function of heat insulation, which can eliminate the heating gas heating and heat preservation measures commonly used in high-temperature raw gas transmission pipelines;

[0021] (3) The pipe body can be made of ordinary carbon steel, which saves a lot of investment compared with pipes made of heat-resistant stainless steel;

[0022] (4) Compared with the conventional lining structure of the raw gas transmission pipeline, the problem of failure of the pipeline insulation due to the penetration of tar and other substances in the high-temperature raw gas into the insulation layer can be avoided, and the long-distance stable transmission of high-temperature raw gas can be achieved, which is conducive to the smooth operation of the reforming furnace production. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a schematic diagram of the cross-sectional structure of a raw gas transmission pipeline described in the present invention.

[0024] Figure 2 It is a schematic diagram of the cross-sectional structure of the high-temperature raw coal gas transmission pipeline in Example 1 of the present invention.

[0025] Figure 3 yes Figure 2 AA section view in.

[0026] Figure 4 It is a schematic diagram of the cross-sectional structure of the high-temperature raw coal gas transmission pipeline in Example 2 of the present invention.

[0027] Figure 5 It is a schematic diagram of the cross-sectional structure of the high-temperature raw coal gas transmission pipeline in Example 3 of the present invention.

[0028] In the figure: 1. Refractory brick support layer 2. Sealing layer 21. Sealing refractory brick 22. Refractory castable 23. Heat-resistant stainless steel plate 3. Insulation layer 4. Circumferential expansion joint 5. Pipeline body 6. Axial expansion joint DETAILED DESCRIPTION

[0029] The specific implementation of the present invention will be further described below in conjunction with the accompanying drawings:

[0030] like Figure 1 As shown, the raw gas transmission pipeline of the present invention is composed of a pipe body 5 made of ordinary carbon steel and a composite sealing and heat-insulating lining inside thereof. The composite sealing and heat-insulating lining is composed of a refractory brick support layer 1, a sealing layer 2, and a heat-insulating layer 3 from the inside to the outside. Among them, the refractory brick support layer 1 supports the composite sealing and heat-insulating lining, and the main function of the sealing layer 2 is to prevent tar and other substances in the high-temperature raw gas from penetrating through the refractory brick support layer 1 to the heat-insulating layer 3, and the heat-insulating layer 3 plays a role of heat insulation.

[0031] The refractory brick support layer 1 of the present invention is a cylindrical structure built by a number of high-strength refractory bricks. The mortar joints between the bricks are controlled at 2 to 3 mm, and the bricks are connected by grooves and tongues to ensure the structural stability of the refractory brick support layer 1. High-strength refractory bricks are preferably silicon-aluminum refractory bricks. The thickness of the refractory brick support layer 1 is at least 80 mm, and the compressive strength is not less than 20 MPa to ensure the structural strength of the refractory support layer 1 and the overall life of the composite sealing and thermal insulation lining. If the refractory brick support layer 1 is cast with castables, its life is generally less than 5 years, and it needs to be regularly inspected and replaced; while the present invention uses high-strength refractory bricks for masonry, which can ensure a service life of more than 20 years and greatly reduce the maintenance workload.

[0032] The sealing layer 2 of the present invention can be built with sealing refractory bricks 21, and the sealing refractory bricks 21 are large arc-shaped bricks to reduce the number of mortar joints. The thickness of the sealing layer 2 using the sealing refractory bricks 21 is not less than 50 mm, and the compressive strength of the sealing refractory bricks 21 used is not less than 10 MPa to ensure the overall strength of the sealing layer 2 and prevent it from being crushed by the refractory brick support layer 1. The sealing refractory bricks 21 and the high-strength refractory bricks of the refractory brick support layer 1 are staggered to avoid the formation of through seams between the two layers to prevent the tar in the high-temperature raw coal gas from penetrating inward.

[0033] The sealing layer 2 described in the present invention can also be formed by a refractory castable 22. The thickness of the sealing layer 2 using the refractory castable 22 is not less than 50 mm, and the room temperature flexural strength of the refractory castable 22 is not less than 2 MPa to ensure the overall structural strength of the sealing layer 2 and avoid it from breaking.

[0034] The sealing layer 2 of the present invention can also be made of a heat-resistant stainless steel plate 23. The thickness of the sealing layer 2 using the heat-resistant stainless steel plate 23 is 0.2 to 2.0 mm, and the overlap width of the heat-resistant stainless steel plate 23 is at least 75 mm to prevent high-temperature raw coal gas from leaking from the joints of the heat-resistant stainless steel plate 23. In order to ensure the structural stability of the sealing layer 2 using the heat-resistant stainless steel plate 23, two adjacent heat-resistant stainless steel plates 23 can be fixed with stainless steel rivets.

[0035] The thermal insulation layer 3 of the present invention is composed of thermal insulation bricks or thermal insulation castables, the thermal conductivity of the thermal insulation bricks or thermal insulation castables is less than 0.6W / m·K, and the thickness of the thermal insulation layer 3 is not less than 50mm to ensure the thermal insulation effect and structural strength.

[0036] The refractory brick support layer 1 and the sealing layer 2 are both provided with an axial expansion joint 6 at intervals of 1 to 2 m along the axial direction of the pipeline. The width of the axial expansion joint 6 is 5 to 10 mm, and a ceramic fiber blanket is filled inside to compensate for thermal expansion. The axial expansion joint of the refractory brick support layer 1 and the axial expansion joint of the sealing layer 2 are staggered, and the interval between the two is more than 50 mm to prevent tar and other substances in the high-temperature raw gas from penetrating into the thermal insulation layer 3 through the axial expansion joint 6.

[0037] The composite sealing heat-insulating lining of the present invention is provided with a 5-10 mm wide annular expansion joint 4 inside or between the composite sealing heat-insulating lining and the pipe body 5, and a ceramic fiber blanket is filled inside to absorb the annular expansion of the composite sealing heat-insulating lining. The annular expansion joint 4 can be provided between the pipe body 5 and the heat-insulating layer 3, or between the heat-insulating layer 3 and the sealing layer 2.

[0038] In addition to the composite sealing and heat-insulating lining on the inner side of the pipeline body 5 of the present invention, an outer insulation layer may also be provided on the outer side thereof to further reduce the temperature of the outer wall of the pipeline.

[0039] Before the raw gas transmission pipeline of the present invention is put into use, the composite sealing and heat-insulating lining needs to be baked with an external heat source. When the temperature of the internal refractory brick support layer 1 reaches above 600°C, nitrogen is used to replace the gas inside the pipeline, and then it can be put into use; when in use, the high-temperature raw gas flow rate in the pipeline is preferably controlled between 10 and 30 m / s. Preheating the pipeline lining can prevent the high-temperature raw gas from condensing on the surface after direct contact with the high-strength refractory bricks of the refractory brick support layer 1, and controlling the high-temperature raw gas flow rate in the pipeline can prevent dust in the high-temperature raw gas from settling and clogging the pipeline.

[0040] The refractory brick support layer 1 of the present invention is built into a cylindrical structure with high-strength refractory bricks to form a high-strength and long-life support layer, while preventing the erosion of the pipeline by raw gas; the sealing layer 2 is made of sealing refractory bricks 21, refractory castables 22 or heat-resistant stainless steel plates 23, which can prevent tar and other substances in the raw gas from penetrating into the insulation layer 3; the insulation layer 3 is composed of insulation bricks or insulation castables, which plays a role in heat insulation and heat preservation. By setting a composite lining structure composed of refractory brick support layer 1-sealing layer 2-insulation layer 3 in the pipeline, the structural strength of the lining is enhanced, the service life of the lining is extended, and at the same time, tar and other substances in the raw gas are prevented from penetrating into the insulation layer 3 to cause the insulation layer 3 to fail, which can play a role in long-term heat insulation and heat preservation.

[0041] In order to make the purpose, technical scheme and technical effect of the present invention clearer, the technical scheme in the embodiment of the present invention is now clearly and completely described. However, the embodiments described below are only part of the embodiments of the present invention, not all of the embodiments. In combination with the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0042] [Example 1]

[0043] like Figure 2-Figure 3 As shown, in this embodiment, the pipe body 5 of the raw gas transmission pipeline is made of ordinary carbon steel, and the composite sealing and heat-insulating lining is composed of a refractory brick support layer 1, a sealing layer 2 built of refractory bricks, and a heat-insulating layer 3 built of heat-insulating bricks.

[0044] In this embodiment, the high-strength refractory bricks of the refractory brick support layer 1 are clay bricks, and the bricks are connected by groove and tongue bite. The thickness of the refractory brick support layer 1 is 200 mm, and the compressive strength is not less than 25 MPa.

[0045] In this embodiment, the sealing refractory bricks 21 of the sealing layer 2 are made of floating bead bricks, which are large curved bricks with an outer arc length of 300 mm, a thickness of 65 mm, and a compressive strength of 10 MPa. The floating bead bricks and the clay bricks of the refractory brick support layer 1 are staggered to avoid the generation of through seams.

[0046] In this embodiment, the heat insulation layer 3 is built of heat insulation bricks, the thermal conductivity of the heat insulation bricks is not greater than 0.15 W / m·K, and the thickness of the heat insulation layer 3 is 90 mm.

[0047] In this embodiment, the refractory brick support layer 1 and the sealing layer 2 are both provided with an axial expansion joint 6 every 1500 mm, the width of the axial expansion joint 6 is 7 mm, and the ceramic fiber blanket is filled in it. The axial expansion joint of the refractory brick support layer 1 and the axial expansion joint of the sealing layer 2 are staggered by 75 mm. A 6 mm wide annular expansion joint 4 is provided between the insulation layer 3 and the pipeline body 5, and the ceramic fiber blanket is filled in it.

[0048] [Example 2]

[0049] like Figure 4 As shown, in this embodiment, the pipe body 5 of the raw gas transmission pipeline is made of ordinary carbon steel, and the composite sealing and insulating lining is composed of a refractory brick support layer 1, a sealing layer 2 cast by refractory castable 22, and an insulating layer 3 built by insulating bricks.

[0050] In this embodiment, the high-strength refractory bricks of the refractory brick support layer 1 are high-alumina bricks, and a groove-tongue bite structure is adopted between the bricks. The thickness of the brick layer is 150 mm, and the compressive strength is not less than 40 MPa.

[0051] In this embodiment, the sealing layer 2 is cast by a refractory castable 22, the model of the refractory castable 22 is CN-130, the thickness of the sealing layer 2 is 50 mm, and the flexural strength at room temperature is not less than 4 MPa.

[0052] In this embodiment, the heat insulation layer 3 is built with heat insulation bricks, the thermal conductivity of the heat insulation bricks is not greater than 0.3 W / m·K, and the thickness is 113 mm.

[0053] In this embodiment, the refractory brick support layer 1 and the sealing layer 2 are both provided with an axial expansion joint 6 every 1500 mm, the width of the axial expansion joint 6 is 7 mm, and a 7 mm ceramic fiber blanket is filled inside. The axial expansion joint of the refractory brick support layer 1 and the axial expansion joint of the sealing layer 2 are staggered by 100 mm. A 5 mm wide annular expansion joint 4 is provided between the sealing layer 2 and the insulation layer 3, and a ceramic fiber blanket is filled inside.

[0054] [Example 3]

[0055] like Figure 5 As shown, in this embodiment, the pipe body 5 of the raw gas transmission pipeline is made of ordinary carbon steel, and the composite sealing and insulating lining is composed of a refractory brick support layer 1, a sealing layer 2 made of a heat-resistant stainless steel plate 23, and an insulating layer 3 built of insulating bricks.

[0056] In this embodiment, the high-strength refractory bricks of the refractory brick support layer 1 are mullite bricks, and the bricks are connected by groove and tongue bite. The thickness of the refractory brick support layer is 110 mm, and the compressive strength is not less than 65 MPa.

[0057] In this embodiment, the sealing layer 2 is composed of several square heat-resistant stainless steel plates 23 with a thickness of 0.3 mm and a side length of 1 m. The heat-resistant stainless steel plates 23 are made of 304 stainless steel plates. The heat-resistant stainless steel plates 23 are overlapped with each other, the overlap width is 75 mm, and the overlap positions are fixed with stainless steel rivets.

[0058] In this embodiment, the heat insulation layer 3 is built of heat insulation bricks, the thermal conductivity of the heat insulation bricks is not more than 0.15W / m·K, and the thickness is 113mm. The refractory brick support layer 1 is provided with an axial expansion joint 6 every 1500mm, the width of the axial expansion joint 6 is 7mm, and a 7mm ceramic fiber blanket is filled inside. A 5mm wide annular expansion joint 4 is provided between the sealing layer 2 and the heat insulation layer 3, and a ceramic fiber blanket is filled inside.

[0059] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A raw gas transmission pipeline, characterized in that: It includes a pipeline body and a composite sealing and heat-insulating lining arranged in the pipeline body; the pipeline body is made of carbon steel, and the composite sealing and heat-insulating lining is composed of a refractory brick supporting layer, a sealing layer and a heat-insulating layer arranged in sequence from the inside to the outside.

2. A raw gas transmission pipeline according to claim 1, characterized in that: The refractory brick support layer is a cylindrical structure built by a number of high-strength refractory bricks, with a masonry mortar joint of 2 to 3 mm; two adjacent high-strength refractory bricks are connected by groove and tongue bite; the thickness of the refractory brick support layer is at least 80 mm, and the high-strength refractory bricks are silicon-aluminum refractory bricks with a compressive strength of not less than 20 MPa.

3. A raw gas transmission pipeline according to claim 1, characterized in that: The sealing layer is a cylindrical structure composed of sealing refractory bricks. The circumferential size of the sealing refractory bricks is larger than that of the high-strength refractory bricks. The thickness of the sealing refractory bricks is not less than 50 mm, and the compressive strength is not less than 10 MPa. The sealing refractory bricks and the high-strength refractory bricks of the supporting layer are staggered.

4. A raw gas transmission pipeline according to claim 1, characterized in that: The sealing layer is a cylindrical structure composed of refractory castables, the thickness of the sealing layer is not less than 50 mm, and the room temperature flexural strength of the refractory castables is not less than 2 MPa.

5. The raw gas transmission pipeline according to claim 1, characterized in that: The sealing layer is a cylindrical structure made of heat-resistant stainless steel plates, the thickness of the heat-resistant stainless steel plates is 0.2-2.0 mm, and the overlap width of the heat-resistant stainless steel plates is at least 75 mm.

6. The raw gas transmission pipeline according to claim 1, characterized in that: The heat insulation layer is a cylindrical structure composed of heat insulation bricks or heat insulation castables. The thermal conductivity of the heat insulation bricks or heat insulation castables is less than 0.6W / m·K, and the thickness of the heat insulation layer is not less than 50mm.

7. The raw gas transmission pipeline according to claim 1, characterized in that: The refractory brick support layer and the sealing layer are both provided with an axial expansion joint every 1 to 2 m along the axial direction of the pipeline, and the axial expansion joint is filled with a ceramic fiber blanket; the axial expansion joint of the refractory brick support layer and the axial expansion joint of the sealing layer are spaced more than 50 mm apart and are staggered.

8. The raw gas transmission pipeline according to claim 1, characterized in that: An annular expansion joint is arranged between the insulation layer and the sealing layer of the composite sealing insulation lining, or between the insulation layer and the pipeline body. The width of the annular expansion joint is 5 to 10 mm, and the ceramic fiber blanket is filled in the annular expansion joint.

9. The raw gas transmission pipeline according to claim 1, characterized in that: An outer heat-insulating layer is also provided on the outside of the pipeline body.

10. The method for using the raw gas transmission pipeline according to any one of claims 1 to 9, characterized in that: Before use, the composite sealing and thermal insulation lining is baked with an external heat source. When the temperature of the refractory brick support layer reaches above 600°C, nitrogen is introduced to replace the gas inside the pipeline, and then it is put into use. During use, the flow rate of the high-temperature raw coal gas in the pipeline is controlled at 10-30m / s.

Citation Information

Patent Citations

  • High-temperature raw gas conveying method and pipeline system

    CN113958868A

  • Raw gas conveying pipeline

    CN222992396U

  • Heat exchanger for cooling hot high pressure gases - with tubes conducting gases through coolant chamber from gas inlet chamber

    FR2284852A1

  • Flange coupling

    US4475749A