Heating cigarette preparation method and heating cigarette

By using thermally conductive films instead of steel strips in the production of heated cigarettes, the problems of low strength and uneven thickness of tobacco sheets are solved, higher quality heated cigarettes are produced, and product stability and user experience are ensured.

CN118805945APending Publication Date: 2024-10-22NANTONG CIGARETTE FILTER +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411232148.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

The tobacco sheets produced by the existing thick slurry method have low strength and are easy to break, and the high-temperature baking of the steel strip causes uneven thickness, which affects the quality of heated cigarettes.

Method used

A thermally conductive film is used instead of a steel strip. The thick cigarette slurry is applied to the thermally conductive film and dried to form a tobacco sheet, which is then wrapped with cigarette paper to form a cigarette core rod, reducing the risk of breakage.

Benefits of technology

It improves the strength and thickness uniformity of tobacco sheets, enhances the structural strength of cigarette core rods, and ensures the product quality of heated cigarettes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118805945A_ABST
    Figure CN118805945A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of novel tobacco products, and discloses a heating cigarette preparation method and a heating cigarette. The heating cigarette preparation method comprises the following steps that S100, cigarette thick paste and a heat conduction film are provided, a tape casting platform of the cigarette thick paste is formed by the heat conduction film, and the cigarette thick paste is smeared to the tape casting platform; and S200, the cigarette thick paste on the casting platform is dried, and the dried cigarette thick paste and the heat conduction film are bonded together to form the tobacco sheet. And S300, cigarette paper is provided, and the cigarette paper wraps the tobacco sheets to form the cigarette core rod. And S400, the cigarette core rod is cut into sections according to the preset length. And S500, providing a filter end, and combining the cut cigarette core rod with the filter end to form the heated cigarette. According to the heating cigarette preparation method, the strength of the tobacco sheets can be enhanced, the thickness uniformity is improved, and breakage of the tobacco sheets in the production process is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of novel tobacco products, and in particular to a method for preparing heated cigarettes and heated cigarettes. Background Art

[0002] Heated cigarettes, also known as heat-not-burn cigarettes, are a type of new tobacco. They are the most rapidly developing and promising type of new tobacco. They are characterized by heating tobacco rather than burning it. The vast majority of tobacco materials for heated cigarettes are used in the form of tobacco flakes (reconstituted tobacco leaves), which are the core material for heat-not-burn cigarette products. The thick slurry method is a common method for making reconstituted tobacco leaves used in heated cigarettes. This method usually involves evenly spreading the thick slurry on a steel belt for primary drying, which is then scraped off with a shovel and then dried again for the second level to form flakes. The flakes are then rolled up with paper rolls to form cigarette core rods, which are finally compounded with a cooling section and a filter section to form heated cigarettes.

[0003] However, the thin sheets produced by the thick slurry method in the prior art are entirely bonded to the tobacco powder by adhesives, so their own strength is relatively low and is greatly affected by the moisture after drying. Too little moisture will cause brittle fracture. In addition, the steel belts used by most companies will produce ups and downs after long-term high-temperature baking, which directly affects the uniformity of the thick slurry laying, resulting in uneven thickness of the thick slurry thin sheets after drying, and the weak points in the thin parts are very likely to break when winding. In addition, the thin sheets are easily damaged by the peeling action of the scraper, affecting their tensile strength.

[0004] Therefore, there is an urgent need for a method for preparing a heated cigarette and a heated cigarette to solve the above problems. Summary of the invention

[0005] An object of the present invention is to provide a method for preparing heated cigarettes, which can enhance the strength of tobacco sheets, improve the uniformity of thickness, and reduce the breakage of tobacco sheets during the production process.

[0006] To achieve this object, the present invention adopts the following technical solutions:

[0007] A method for preparing a heated cigarette is provided, comprising the following steps:

[0008] S100, providing a cigarette slurry and a heat-conductive film, wherein the heat-conductive film forms a casting platform for the cigarette slurry, and applying the cigarette slurry onto the casting platform;

[0009] S200, drying the cigarette slurry on the casting platform, so that the dried cigarette slurry is bonded to the heat conductive film to form a tobacco sheet together;

[0010] S300, providing cigarette paper, wherein the cigarette paper wraps the tobacco sheet to form a cigarette core rod;

[0011] S400, dividing the cigarette core rod into segments according to preset lengths;

[0012] S500, providing a filter end, and combining the divided cigarette core rod with the filter end to form a heated cigarette.

[0013] As an optional solution of the method for preparing heated cigarettes, in step S300, the tobacco sheet is divided into a plurality of cigarette rods, and the cigarette paper wraps the plurality of cigarette rods to form the cigarette core rod.

[0014] As an optional solution of the method for preparing heated cigarettes, the width of each tobacco rod is 0.8 mm-1.2 mm.

[0015] As an optional solution of the method for preparing heated cigarettes, in step S300, the tobacco sheet is folded and wrapped in the cigarette paper.

[0016] As an optional solution of the method for preparing heated cigarettes, the folding width between adjacent folds of the tobacco sheet is 0.8 mm-1.2 mm.

[0017] As an optional solution of the method for preparing heated cigarettes, the heat-conductive film is a metal film.

[0018] As an optional solution for the method for preparing heated cigarettes, the thickness of the thermally conductive film is 0.01 mm-0.05 mm.

[0019] As an optional solution of the method for preparing heated cigarettes, the heat-conductive film includes an anti-corrosion layer and a high-temperature resistant layer, and the anti-corrosion layer is connected to the high-temperature resistant layer.

[0020] As an optional solution of the method for preparing heated cigarettes, the thermally conductive film further includes a detection layer, the detection layer is connected between the anti-corrosion layer and the high temperature resistant layer, and the detection layer includes a temperature detection element.

[0021] Another object of the present invention is to provide a heated cigarette that can improve the strength of tobacco sheets and ensure the production quality of heated cigarettes.

[0022] To achieve this object, the present invention adopts the following technical solutions:

[0023] Provided is a heated cigarette manufactured by the heated cigarette manufacturing method.

[0024] Beneficial effects of the present invention:

[0025] The present invention provides a method for preparing heated cigarettes, which uses a heat-conductive film to replace the steel belt in the prior art, and applies the cigarette slurry on a casting platform formed by the heat-conductive film, thereby avoiding the uneven thickness of the cigarette slurry due to the uneven surface of the steel belt, thereby improving the problem of uneven local strength of the cigarette slurry after drying, and improving the strength of the cigarette slurry. After the cigarette slurry is dried, it can be bonded with the heat-conductive film to form a tobacco sheet, so that the heat-conductive sheet can support and connect the cigarette slurry, reduce the sheet peeling process by a scraper, and further improve the strength of the tobacco sheet. The tobacco sheet, i.e., the cigarette slurry and the heat-conductive sheet, are wrapped with cigarette paper to form a cigarette core rod, thereby avoiding the problem of the tobacco sheet breaking during the formation of the cigarette core rod, and ensuring the product quality of the heated cigarette.

[0026] The present invention also provides a heated cigarette, which is prepared by the above-mentioned heated cigarette preparation method, improves the structural strength of the cigarette core rod, and ensures the product quality of the heated cigarette. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 The present invention is a flow chart of the method for preparing heated cigarettes. DETAILED DESCRIPTION

[0028] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.

[0029] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0030] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0031] In the description of this embodiment, the terms "upper", "lower", "right", etc., directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.

[0032] like Figure 1 As shown, the method for preparing a heated cigarette in this embodiment includes the following steps:

[0033] S100, providing cigarette slurry and a thermal conductive film, wherein the thermal conductive film forms a casting platform for the cigarette slurry, and applying the cigarette slurry onto the casting platform;

[0034] S200, drying the cigarette slurry on the casting platform so that the dried cigarette slurry is bonded to the heat conductive film to form a tobacco sheet;

[0035] S300, providing cigarette paper, wherein the cigarette paper wraps the tobacco sheet to form a cigarette core rod;

[0036] S400, dividing the cigarette core rod into segments according to a preset length;

[0037] S500, providing a filter end, and combining the divided cigarette core rod with the filter end to form a heated cigarette.

[0038] The method for preparing heated cigarettes uses a heat-conductive film to replace the steel belt in the prior art to form a casting platform, and applies the cigarette slurry on the casting platform, thereby avoiding the uneven thickness of the cigarette slurry due to the uneven surface of the steel belt, thereby improving the problem of uneven local strength of the cigarette slurry after drying, and improving the strength of the cigarette slurry. After the cigarette slurry is dried, it can be bonded with the heat-conductive film to form a tobacco sheet, so that the heat-conductive sheet can support and connect the cigarette slurry, reduce the sheet peeling process by the scraper, and further improve the strength of the tobacco sheet. The tobacco sheet, i.e., the cigarette slurry and the heat-conductive sheet, are wrapped with cigarette paper to form a cigarette core rod, thereby avoiding the problem of the tobacco sheet breaking during the formation of the cigarette core rod, and ensuring product quality.

[0039] When producing heated cigarettes, it is necessary to first prepare cigarette slurry. Generally, cigarette slurry is composed of water, tobacco powder, fiber, smoke-generating agent and adhesive and other raw materials. The specific preparation method is as follows:

[0040] S1, drying the tobacco leaves and crushing them into 2mm-6mm pieces, and then crushing them into fine tobacco powder with a mesh size of more than 200 by a fine grinder;

[0041] S2, preparing a dispersion of a smoke-generating agent by mixing an adhesive and a smoke-generating agent in a ratio of 1:2 to 1:4, illustratively, the smoke-generating agent may use glycerol, propylene glycol, etc., and the adhesive generally includes an adhesive and other additives, such as guar gum, xanthan gum, carrageenan, konjac gum, CMC, phosphoric acid, etc.;

[0042] S3, transferring the above-mentioned smoke agent dispersion into an aqueous solution with a fiber concentration of 0%-1.5%, to prepare a mixed solution with a smoke agent dispersion concentration of 3%-6%. For example, the fiber concentration in the aqueous solution may be 0%, 0.5%, 1% or 1.5%, and the concentration of the smoke agent dispersion in the mixed solution may be 3%, 4%, 5% or 6%, etc.;

[0043] S4, continue to add fine tobacco powder to the mixed solution to prepare a cigarette slurry with a solid content of 15%-30%, thereby completing the preparation of the cigarette slurry. For example, the solid content of the cigarette slurry can be 15%, 20%, 25% or 30%.

[0044] Furthermore, the cigarette slurry is evenly coated on the thermal conductive film, and the thickness of the coated cigarette slurry is 0.4mm-1.5mm. When the thickness of the cigarette slurry is less than 0.4mm, the heating efficiency of the tobacco sheet is too fast, the working duration of the cigarette is short, and the user experience cannot be guaranteed; if the thickness of the cigarette slurry is greater than 1.5mm, the thickness of the cigarette slurry is too large to be fully heated, resulting in product waste. Optionally, the thickness of the coated cigarette slurry can be 0.4mm, 0.8mm, 1.2mm or 1.5mm, etc.

[0045] Optionally, when coating, there are two coating methods: gravity casting and extrusion casting. Specifically, when using gravity casting, it is necessary to use a scraper to cooperate with the casting platform, the scraper and the thermal conductive film are set at intervals, and the interval distance is the thickness of the cigarette slurry, and the cigarette slurry is cast from the interval between the scraper and the thermal conductive film. When using the extrusion casting method, the cigarette slurry can be directly extruded according to a certain thickness using an extrusion device, without the need to use a scraper to control the thickness of the cigarette slurry. It should be noted that when using the gravity casting method, in order to ensure that the cigarette slurry has sufficient fluidity, the solid content in the cigarette slurry is 15%-22%, while in the extrusion casting method, the solid content in the cigarette slurry is 22%-30%. For example, when using the gravity casting method, the solid content in the cigarette slurry is 15%, 18%, 20% or 22%, etc.; when using the extrusion casting method, the solid content in the cigarette slurry is 22%, 25%, 28% or 30%, etc.

[0046] Furthermore, after the cigarette slurry is dried by hot air drying, steam drying or infrared drying, the tobacco sheet formed by bonding the cigarette slurry and the heat-conductive film is processed and wrapped in cigarette paper to form a cigarette core rod.

[0047] Optionally, the cigarette core rod can be prepared by cutting tobacco sheets. When preparing cigarette rods by cutting, the tobacco sheets are cut into multiple cigarette rods according to a preset width, and then the multiple cigarette rods are wrapped with cigarette paper, and then cut into cigarette core rods according to a preset length after wrapping.

[0048] Optionally, the cigarette core rod can also be prepared by folding the tobacco sheets. When preparing the cigarette core rod by folding, there are two ways to fold the tobacco sheets. The first way is to directly fold the tobacco sheets according to a preset width, and wrap the folded tobacco sheets in cigarette paper to form a cigarette core rod, so as to ensure the tight collection of the cigarette slurry in the cigarette core rod, so that the tobacco rod has a better fixing effect in the cigarette core rod, and increase the thermal conductivity. In the second folding method, a plurality of through holes are evenly arranged on the tobacco sheet along the direction in which the crease extends to form a dotted crease, and two dotted creases spaced apart from each other can be arranged, and the two dotted creases are staggered with each other, so that the edges of adjacent cigarette rods are connected in multiple sections, which is easier to fold.

[0049] It should be noted that when preparing cigarette core rods, the tobacco sheets can first be divided into tobacco rods according to a preset width and a preset length, and then the divided tobacco rods are arranged in a certain order to prepare cigarette core rods. The process sequence of manufacturing cigarette core rods can be adjusted according to actual conditions to improve production efficiency.

[0050] Preferably, when the tobacco sheet is divided into multiple tobacco rods, the width of each tobacco rod is 0.8mm-1.2mm, or when the tobacco sheet is folded and wrapped in cigarette paper, the folding width between adjacent folds of the tobacco sheet is 0.8mm-1.2mm, so as to ensure heating efficiency. Optionally, the width of the tobacco rod can be set to 0.8mm, 0.9mm, 1.0mm, 1.1mm or 1.2mm, and the folding width can be set to 0.8mm, 0.9mm, 1.0mm, 1.1mm or 1.2mm, etc.

[0051] Optionally, the length of the cigarette core rod is set to 10 mm-20 mm. Exemplarily, the length of the cigarette core rod can be set to 10 mm, 12 mm, 15 mm or 20 mm, etc.

[0052] To ensure that the thermally conductive film has good thermal conductivity, a metal film can be used. When the cigarette core rod is heated, the metal film can quickly conduct heat and save preheating time. Optionally, the thermally conductive film can be a single-layer metal film, which can be a film made of copper, aluminum, iron, or an alloy film made of copper, aluminum, iron, nickel, magnesium, chromium, carbon and other elements to ensure thermal conductivity and improve user experience. Of course, the thermally conductive film can also be made of non-metallic materials, such as graphite, silicone, etc.

[0053] Optionally, the thermally conductive film can also be made of a composite of multiple layers of metal films. When the thermally conductive film uses a multi-layer metal composite film, the thermally conductive film includes an anti-corrosion layer, a high temperature resistant layer and a detection layer. The detection layer is connected between the anti-corrosion layer and the high temperature resistant layer. The detection layer includes a temperature detection element that can feedback the heating temperature of the thermally conductive film. When the metal film has a multi-layer structure, it can be heated by inserting a resistive heating rod into the cigarette core rod, or by electromagnetic heating, so that the heating process is simpler and easier to operate. In addition, different metal elements can be selected to prepare corresponding alloy films depending on whether electromagnetic heating is used, which is conducive to ensuring thermal conductivity efficiency and improving user experience.

[0054] It should be noted that in the prior art, it is usually necessary to insert a heating rod into the cigarette core rod for heating. The insertion of the heating rod makes the inside of the cigarette core rod tighter, which easily leads to the risk of unexpected blockage of the smoke channel, affecting the use effect. However, for the heated cigarette of this embodiment, when the thermal conductive film is made of a multi-layer metal film, the metal film can be heated by electromagnetic means, and there is no need to insert the heating rod into the cigarette core rod separately, which ensures the user experience and safety of use, and also avoids the problem that the outer periphery cannot be heated due to heating in the center of the cigarette core rod, and the center is over-carbonized near the heating rod.

[0055] Optionally, the thickness of the thermally conductive film is 0.01 mm-0.05 mm, which can have sufficient strength, avoid material waste, and save production costs. Exemplarily, the thickness of the thermally conductive film can be 0.01 mm, 0.02 mm, 0.03 mm, 0.04 mm or 0.05 mm.

[0056] This embodiment also provides a heated cigarette, which is prepared by the above-mentioned heated cigarette preparation method. The tobacco sheet is supported and connected by a heat-conductive film, which improves the structural strength of the cigarette core rod and ensures the product quality of the heated cigarette.

[0057] When using the heated cigarette proposed in this embodiment, the thermally conductive film has good thermal conductivity and each part of the tobacco sheet can contain the thermally conductive film, which can make the heat evenly transferred in the cigarette core rod during smoking, so that the thick slurry sheet can release the tobacco substance more fully and evenly, satisfying the smoking sensation.

[0058] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the embodiments here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the claims of the present invention.

Claims

1. A method for preparing a heated cigarette, characterized in that: The steps include: S100, providing a cigarette slurry and a heat-conductive film, wherein the heat-conductive film forms a casting platform for the cigarette slurry, and applying the cigarette slurry onto the casting platform; S200, drying the cigarette slurry on the casting platform, so that the dried cigarette slurry is bonded to the heat conductive film to form a tobacco sheet together; S300, providing cigarette paper, wherein the cigarette paper wraps the tobacco sheet to form a cigarette core rod; S400, dividing the cigarette core rod into segments according to preset lengths; S500, providing a filter end, and combining the divided cigarette core rod with the filter end to form a heated cigarette.

2. The method for preparing a heated cigarette according to claim 1, characterized in that: In step S300, the tobacco sheet is divided into a plurality of cigarette rods, and the cigarette paper wraps the plurality of cigarette rods to form the cigarette core rod.

3. The method for preparing a heated cigarette according to claim 2, characterized in that: The width of each of the tobacco rods is 0.8 mm to 1.2 mm.

4. The method for preparing a heated cigarette according to claim 1, characterized in that: In step S300, the tobacco sheet is folded and wrapped in the cigarette paper.

5. The method for preparing a heated cigarette according to claim 4, characterized in that: The folding width between adjacent folds of the tobacco sheet is 0.8 mm to 1.2 mm.

6. The method for preparing a heated cigarette according to claim 1, characterized in that: The thermally conductive film is a metal film.

7. The method for preparing a heated cigarette according to claim 1, characterized in that: The thickness of the thermally conductive film is 0.01 mm-0.05 mm.

8. The method for preparing a heated cigarette according to any one of claims 1 to 7, characterized in that: The heat-conducting film comprises an anti-corrosion layer and a high-temperature resistant layer, and the anti-corrosion layer is connected to the high-temperature resistant layer.

9. The method for preparing a heated cigarette according to claim 8, characterized in that: The thermally conductive film further comprises a detection layer, wherein the detection layer is connected between the anti-corrosion layer and the high temperature resistant layer, and the detection layer comprises a temperature detection element.

10. A heated cigarette, characterized in that: The heated cigarette is manufactured by the method for preparing a heated cigarette as described in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Smoke generation device of low temperature cigarette and manufacturing method thereof

    CN107411178A

  • Heat-not-burn cigarette cut tobacco module and preparation method thereof

    CN109567258A

  • Graphene-based composite filter material applied to filter stick for cigarette

    CN109875112A

  • Heat-conducting porous ceramic atomizing core as well as preparation method and application thereof

    CN116711887A

  • Thermally enhanced aerosol-forming substrate

    CN117545377A