Aluminum pipe extrusion forming device with combined mold core
Through the trifurcated base and multi-specification forming core column of the combined core device, the problems of core connection damage and specification diversity in aluminum pipe extrusion are solved, achieving diversified production of aluminum pipes and saving mold costs.
Patent Information
- Application Number
- CN202410949852.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-10-22
AI Technical Summary
The existing aluminum tube extrusion forming device is easily damaged at the mold core connection under high pressure, causing the mold to be unable to continue to be used, and there is a lack of technology to easily replace the mold to produce aluminum tubes of different specifications.
A combined mold core device is used, including a trifurcated base, a baffle, a molding core column and a core tooth sleeve. The tension of the molding core column is evenly distributed through the connection between the trifurcated base and the upper mold shunt bridge, and the detachable design And multi-specification molding core columns and core tooth sleeves can be used to realize working belts of different lengths and thicknesses, reducing connection damage and mold manufacturing costs.
It effectively reduces the connection damage caused by the force in the center of the upper mold, allows the replacement of the base instead of the entire upper mold, reduces the mold manufacturing cost, and supports the production of aluminum tubes of different specifications.
Smart Images

Figure CN118808364A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of extrusion molding, in particular to an aluminum tube extrusion molding device with a combined mold core. Background Art
[0002] Aluminum extrusion molding is a plastic processing method that applies strong pressure to the metal billet placed in the die, forcing the metal billet to produce directional plastic deformation and extrude it from the extrusion die, thereby obtaining parts or semi-finished products with the desired cross-sectional shape, size and certain mechanical properties.
[0003] The working conditions of the extrusion mold are poor, and the blank is in a nearly closed state during extrusion, so the mold core needs to withstand very high pressure. This leads to the mold core being damaged due to excessive force during the extrusion molding of the aluminum tube. At the same time, the mold core is usually subjected to high temperature and high friction during hot extrusion, which greatly affects the strength and service life of the mold and needs to be replaced frequently. In the prior art, most of the mold cores are fixed to the center of the upper mold to solve the technical problem of needing to be replaced, but this technical solution has certain defects. Usually, the production cost of the mold is high, and under the action of high pressure, the mold core is directly fixed to the center of the upper mold. Due to the presence of the diverter hole in the upper mold, the connection at the center of the upper mold is difficult to withstand huge pressure. Once the thread at the connection is damaged, the entire upper mold cannot be used. The prior art also lacks a technology that can easily replace the mold to produce aluminum tubes of different specifications. Summary of the invention
[0004] 1. Technical issues to be resolved
[0005] In view of the above-mentioned shortcomings and deficiencies of the prior art, the present invention provides an aluminum tube extrusion forming device with a combined mold core, which solves the technical problem that during the aluminum tube extrusion forming process, the connection structure between the replaceable mold core and the upper mold is destroyed under the action of high pressure, resulting in the upper mold as a whole being unable to continue to be used, and also solves the problem of the convertibility of the working belt.
[0006] (II) Technical solution
[0007] In order to achieve the above object, the main technical solutions adopted by the present invention include:
[0008] The embodiment of the present invention provides an aluminum tube extrusion forming device with a combined die core, comprising an upper die, a lower die, a die core assembly, a feed barrel and an extrusion rod. The die core assembly is detachably connected to a central cavity formed by coaxially opposing upper and lower dies, the feed side of the upper die is connected to one end of the feed barrel, and the extrusion rod is slidably connected in the feed barrel.
[0009] The mold core assembly includes a trident base, a trident baffle, a forming core column and a core tooth sleeve. The trident base is fixedly connected to the trilobate groove on the side of the central chamber of the diverter bridge on the upper mold. The trident baffle covers the top of the trident base and is pressed by the lower mold. The bottom end of the forming core column passes through the center of the trident baffle and is connected to the center of the trident base. The core tooth sleeve is inserted into the step hole opened in the center of the lower mold; the outer contour of the core tooth sleeve presents a large and a small stepped shaft shape, and a through inner hole is provided along its axial direction. The top of the forming core column has a forming core tooth; the forming core tooth and the core tooth sleeve are coaxially matched with each other, and the gap constitutes the working belt of the extrusion molding.
[0010] Optionally, the forming core column includes a plurality of different specifications, and the forming core teeth thereon have different radial lengths or axial lengths, and the core tooth sleeve also includes a plurality of different specifications, and the inner hole thereon has different radial lengths and axial lengths. Selecting forming core columns and core tooth sleeves of different specifications can form working belts with different lengths or thicknesses.
[0011] Optionally, the surface of the forming core column and the core tooth sleeve is coated with a coating thickness of 0.-0.um, using high-temperature plasma spraying, the spraying temperature is set at 900-000 degrees, and the coating composition is WC: 90%, Co: 9.%, YG6: 0.175%, YG8: 0.175%, Ln: 0.0%, Ce: 0.0%.
[0012] Optionally, a plurality of diversion openings are evenly distributed along the circumferential direction of the center of the upper mold, and the plurality of diversion openings are connected by a diversion bridge. The top shape of each diversion opening is elliptical, the bottom shape is V-shaped, and the connection is smoothly transitioned.
[0013] Optionally, along the extension direction of the shunt bridge, a plurality of connection holes for fixing the trident base are evenly arranged at the bottom of the trilobate groove. Countersunk holes are opened at positions on the trident base corresponding to the connection holes, and the countersunk holes are fixed to the connection holes by a connector.
[0014] Optionally, a first groove is provided on one end surface of the feed barrel, a first annular flange is provided on the feed side of the upper die, and the first groove is connected to the first annular flange in a concave-convex manner. The discharge side of the upper die has three first bosses cut by the three-leaf groove, the edge of the three-fork baffle has three second bosses, the three first bosses and the three second bosses together form a second annular flange, and the second annular flange is connected to the second groove in a concave-convex manner.
[0015] Optionally, a tapered hole with a larger upper portion and a smaller lower portion is provided at one end of the lower die along its axial direction, the angle between the generatrix of the tapered hole and its central axis is 60°, and a stepped hole is provided at the bottom of the tapered hole. The large hole diameter of the stepped hole is the same as the large end diameter of the outer contour of the core gear sleeve, and the small hole diameter of the stepped hole is the same as the small end diameter of the outer contour of the core gear sleeve.
[0016] The bottom end of the forming core column is provided with an external thread, and the center of the trident-shaped base is provided with an internal thread matched with the external thread.
[0017] The aluminum tube extrusion molding method of the aluminum tube extrusion molding device comprises the following steps:
[0018] S1: Place the upper die and lower die on the workbench and fix them;
[0019] S2: Insert the core tooth sleeve into the stepped hole of the lower die, and fix the trident base into the trilobate groove of the upper die through a connecting piece;
[0020] S3: Pass the formed core column through the through hole in the center of the trident-shaped baffle and connect it to the trident-shaped base through threads, and simultaneously clamp the trident-shaped baffle into the trilobate-shaped groove;
[0021] S4: close the lower die to the upper die and press the trident-shaped baffle;
[0022] S5: After the feed barrel is connected to the upper die, the high-temperature treated aluminum material is added, and then the extrusion rod is operated to extrude to obtain the finished aluminum tube.
[0023] Furthermore, before the S2 operation, a forming core tooth column and a core tooth sleeve of corresponding specifications are selected according to the working zone required for forming the aluminum tube to be processed.
[0024] (III) Beneficial effects
[0025] The beneficial effects of the present invention are as follows: the aluminum tube extrusion forming device with a combined mold core of the present invention adopts a base as a connecting transition piece between the molding core column and the upper mold. Compared with the prior art, it can evenly disperse the pulling force of the molding core column on the center of the upper mold to the radial diversion bridge of the upper mold, greatly reducing the connection damage caused by the force on the center of the upper mold. At the same time, due to the presence of the base, even if the connection is damaged, the base can be replaced instead of making the entire upper mold unusable, which greatly saves the manufacturing cost of the mold.
[0026] Furthermore, different combined core mold components can be selected according to the different compositions of aluminum alloy materials, working temperature, and pressure to form working belts of different lengths and thicknesses, thereby enabling the production of aluminum tubes in a diverse and efficient manner. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a three-dimensional exploded schematic diagram of an embodiment of the present invention;
[0028] Figure 2 for Figure 1 A schematic cross-sectional view along the central axis of FIG.
[0029] Figure 3 It is a three-dimensional schematic diagram of the connection effect of the upper mold and the mold core assembly in this embodiment;
[0030] Figure 4 is a schematic diagram of the three-dimensional structure of the base in this embodiment;
[0031] Figure 5 It is a schematic diagram of the three-dimensional structure of the core tooth sleeve in this embodiment.
[0032] [Description of Reference Numerals]
[0033] 1: upper die; 11: special-shaped groove; 12: diversion port; 13: diversion bridge; 14: first annular flange; 15: first boss; 16: second annular flange; 17: connecting hole;
[0034] 2: lower die; 21: stepped hole; 22: second groove; 23: tapered hole;
[0035] 3: mold core assembly; 31: base; 32: baffle; 33: molding core column; 34: core tooth sleeve; 311: countersunk hole; 321: second boss; 331: molding core tooth; 341: inner hole;
[0036] 4: central chamber;
[0037] 5: working belt;
[0038] 6: feed barrel; 61: first groove;
[0039] 7: Squeeze rod. DETAILED DESCRIPTION
[0040] In order to better explain the present invention and facilitate understanding, the present invention is described in detail below through specific implementation modes in conjunction with the accompanying drawings.
[0041] The aluminum tube extrusion forming device with a combined mold core provided in the embodiment of the present invention can evenly disperse the pulling force of the forming core column on the center of the upper mold through the combined mold core assembly, thereby reducing the connection damage caused by the concentrated force on the center of the upper mold. At the same time, due to the presence of the trident base, even if the connection is damaged, the trident base can be replaced instead of making the entire upper mold unusable, which greatly saves the manufacturing cost of the mold.
[0042] In order to better understand the above technical solution, exemplary embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present invention are shown in the accompanying drawings, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided to enable a clearer and more thorough understanding of the present invention and to fully convey the scope of the present invention to those skilled in the art.
[0043] Reference Figure 1 and Figure 2The present invention proposes an aluminum tube extrusion forming device with a combined mold core, comprising an upper mold 1, a lower mold 2, a core assembly 3, a feed barrel 6 and an extrusion rod 7. The core assembly 3 is detachably connected to a central chamber 4 formed by the upper mold 1 and the lower mold 2 coaxially opposed to each other, the feed side of the upper mold 1 is connected to one end of the feed barrel 6, and the extrusion rod 7 is slidably connected in the feed barrel 6. The core assembly 3 comprises a trident base 31, a trident baffle 32, a molding core column 33 and a core tooth sleeve 34.
[0044] The trident base 31 is fixedly connected to the trilobate groove 11 of the diverter bridge 13 on the upper mold 1 on one side of the central chamber 4, and the trident baffle 32 covers the top of the trident base 31 and is pressed by the lower mold 2 to ensure that the high-temperature aluminum material does not leak.
[0045] In this embodiment, the branch lengths of the trident base 31 and the trident baffle 32 are the same. Of course, each branch of the trident base 31 can be extended accordingly at the same time until the edge of the upper mold 1, and the three-leaf groove 11 should also be extended accordingly, so that the concentrated force can be better dispersed and the effect is better.
[0046] It should be noted that the upper mold 1 in this embodiment has three diverter bridges 13, so a three-pronged base 31 and a three-pronged baffle 32 are selected. If the number of diverter bridges 13 changes, corresponding grooves need to be opened on the upper mold 1 and matching bases and baffles need to be selected.
[0047] The bottom end of the forming core column 33 passes through the center of the trident-shaped baffle 32 and is connected to the center of the trident-shaped base 31, and the core tooth sleeve 34 is inserted into the step hole 21 opened in the center of the lower mold 2; the outer contour of the core tooth sleeve 34 presents a stepped shaft shape with one large and one small, and a penetrating inner hole 341 is provided along its axial direction.
[0048] It should be noted that the trident-shaped baffle 32 is limited by the shoulder on the forming core column 33. When the forming core column 33 is fixed to the trident-shaped base 31, the center of the trident-shaped baffle 32 can be firmly pressed, effectively preventing the fluid aluminum from entering the trident-shaped base 31, thereby blocking the connection hole 311 and making the trident-shaped base 31 unable to be disassembled.
[0049] The top end of the forming core column 33 is provided with a forming core tooth 331 , and the forming core tooth 331 is coaxially matched with the core tooth sleeve 34 with a clearance, and the clearance forms an extrusion-formed working belt 5 .
[0050] Furthermore, the forming core column 33 includes a plurality of different specifications, and the forming core teeth 331 thereon have different radial lengths or axial lengths, and the core tooth sleeve 34 also includes a plurality of different specifications, and the inner hole 341 thereon has different radial lengths and axial lengths. By selecting forming core columns 33 and core tooth sleeves 34 of different specifications, working belts 5 with different lengths or thicknesses can be formed.
[0051] During the extrusion molding process, it is often necessary to produce aluminum tubes of different diameters. In addition, the pre-treatment temperature and material composition ratio of the aluminum alloy are different. Different lengths and thicknesses of the working belt 5 are required to ensure that the surface quality of the aluminum tube after extrusion molding meets the standards. In this embodiment, the multi-specification forming core column 33 and the core tooth sleeve 34 can be combined to form a variety of diameter working belts for selection (a series of specifications with a length of 1.5-2.4mm and a thickness of 1-1.2mm are provided in this embodiment).
[0052] The surfaces of the forming core column 33 and the core tooth sleeve 34 are coated with a coating thickness of 0.2-0.3um by high-temperature plasma spraying. The spraying temperature is set at 900-1000 degrees. The coating composition is WC: 90%, Co: 9.5%, YG6: 0.175%, YG8: 0.175%, Ln: 0.10%, Ce: 0.05%.
[0053] During the extrusion molding process, the molding parts are subjected to severe wear and tear in a high temperature and high pressure working environment. Therefore, the use of certain wear-resistant treatments can greatly increase the service life. In this embodiment, plasma spraying treatment is used.
[0054] Multiple diversion ports 12 are evenly distributed along the circumferential direction of the center of the upper mold 1. The multiple diversion ports 12 are connected by diversion bridges 13. The top shape of each diversion port 12 is elliptical, the bottom shape is V-shaped, and the connection is smooth. Compared with traditional circular diversion ports, the elliptical diversion holes can make the feeding more sufficient and uniform.
[0055] Along the extension direction of the shunt bridge 13, a plurality of connection holes 17 for fixing the trident base 31 are evenly arranged at the bottom of the trident groove 11. Countersunk holes 311 are opened at positions corresponding to the connection holes 17 on the trident base 31, and the countersunk holes 311 are fixed to the connection holes 17 by a connector.
[0056] Specifically, three countersunk holes 311 are arranged on each branch of the trident-shaped base 31, and nine connecting holes 17 are arranged at the bottom of the corresponding trilobal groove 11. The countersunk holes 311 and the connecting holes 17 are connected with high-strength alloy screws.
[0057] A first groove 61 is provided on one end face of the feed barrel 6, and a first annular flange 14 is provided on the feed side of the upper mold 1, and the first groove 61 is connected with the first annular flange 14 in a concave-convex manner. The discharge side of the upper mold 1 has three sections of first bosses 15 cut by the trilobate groove 11, and the edge of the trident-shaped baffle 32 has three second bosses 321, and the three first bosses 15 and the three second bosses 321 together form a second annular flange 16, and the second annular flange 16 is connected with the second groove 22 in a concave-convex manner.
[0058] A tapered hole 23 with a larger upper portion and a smaller lower portion is provided at one end of the lower die 2 along its axial direction. The angle between the generatrix of the tapered hole 23 and its central axis is 60°, which is more conducive to the forming of high-temperature fluid aluminum. A stepped hole 21 is provided at the bottom of the tapered hole 23. The large hole diameter of the stepped hole 21 is the same as the large end diameter of the outer contour of the core gear sleeve 34, and the small hole diameter of the stepped hole 21 is the same as the small end diameter of the outer contour of the core gear sleeve 34.
[0059] It should be noted here that the diameters of the outer contours of the core tooth sleeves 34 of different specifications are all the same, and they can be fully inserted into the step hole 21 while having a certain interference fit to ensure that they will not fall off during the movement of the lower mold 2.
[0060] The bottom end of the forming core column 33 is provided with an external thread, and the center of the trident-shaped base 31 is provided with an internal thread matching the external thread. The threaded connection is detachable, which is convenient and quick to replace different specifications.
[0061] The aluminum tube extrusion molding method of the aluminum tube extrusion molding device comprises the following steps:
[0062] S1: Place the upper mold 1 and the lower mold 2 on the workbench and fix them;
[0063] S2: Insert the core tooth sleeve 34 into the stepped hole 21 of the lower die 2, and fix the trident base 31 into the trilobate groove 11 of the upper die 1 through a connecting piece;
[0064] S3: The forming core column 33 passes through the through hole in the center of the trident-shaped baffle 32 and is connected to the trident-shaped base 31 by means of threads, and the trident-shaped baffle 32 is simultaneously inserted into the trilobate groove 11;
[0065] S4: closing the lower mold 2 onto the upper mold 1 and pressing the trident-shaped baffle 32;
[0066] S5: After the feed barrel 6 is connected to the upper mold 1, the high-temperature treated aluminum material is added, and then the extrusion rod 7 is operated to extrude to obtain a finished aluminum tube.
[0067] It should be added here that before the operation of S2, it is necessary to select the molding core tooth column 33 and the core tooth sleeve 34 of corresponding specifications according to the working belt 5 required for molding the aluminum tube to be processed.
[0068] In the description of the present invention, it should be understood that the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0069] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium; it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0070] In the present invention, unless otherwise clearly specified and limited, when a first feature is “on” or “below” a second feature, it may be that the first and second features are in direct contact, or that the first and second features are in indirect contact through an intermediate medium. Moreover, when a first feature is “above”, “above” or “above” a second feature, it may be that the first feature is directly above or obliquely above the second feature, or it may simply mean that the first feature is higher in level than the second feature. When a first feature is “below”, “below” or “below” a second feature, it may be that the first feature is directly below or obliquely below the second feature, or it may simply mean that the first feature is lower in level than the second feature.
[0071] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may alter, modify, replace and modify the above embodiments within the scope of the present invention.
Claims
1. An aluminum tube extrusion molding device with a combined mold core, comprising an upper mold (1), a lower mold (2), a mold core assembly (3), a feed barrel (6) and an extrusion rod (7), wherein the mold core assembly (3) is detachably connected to a central chamber (4) formed by the upper mold (1) and the lower mold (2) coaxially opposed to each other, the feed side of the upper mold (1) is connected to one end of the feed barrel (6), and the extrusion rod (7) is slidably connected to the feed barrel (6), characterized in that: The core mold assembly (3) comprises a trident-shaped base (31), a trident-shaped baffle (32), a molding core column (33) and a core tooth sleeve (34); The trident-shaped base (31) is fixedly connected to the trilobate groove (11) of the diverter bridge (13) on the upper mold (1) and located on one side of the central chamber (4); the trident-shaped baffle (32) covers the top of the trident-shaped base (31) and is pressed by the lower mold (2); The bottom end of the molding core column (33) passes through the center of the trident-shaped baffle (32) and is connected to the center of the trident-shaped base (31); the core tooth sleeve (34) is inserted into the stepped hole (21) opened in the center of the lower mold (2); the outer contour of the core tooth sleeve (34) is in the shape of a stepped shaft with one large and one small, and an inner hole (341) is provided along its axial direction; The top end of the molding core column (33) is provided with a molding core tooth (331), and the molding core tooth (331) is coaxially gap-matched with the core tooth sleeve (34), and the gap constitutes an extrusion-molded working belt (5).
2. The aluminum tube extrusion forming device with a combined mold core according to claim 1, characterized in that: The forming core column (33) includes a plurality of different specifications, and the forming core teeth (331) thereon have different radial lengths or axial lengths; the core tooth sleeve (34) also includes a plurality of different specifications, and the inner hole (341) thereon has different radial lengths and axial lengths; By selecting the molding core column (33) and the core tooth sleeve (34) of different specifications, a working belt (5) with different lengths or thicknesses can be formed.
3. The aluminum tube extrusion forming device with a combined mold core according to claim 1, characterized in that: The surfaces of the forming core column (33) and the core tooth sleeve (34) are coated with a coating thickness of 0.2-0.3um by high-temperature plasma spraying, with the spraying temperature set at 900-1000 degrees, and the coating composition is WC: 90%, Co: 9.5%, YG6: 0.175%, YG8: 0.175%, Ln: 0.10%, Ce: 0.05%.
4. The aluminum tube extrusion forming device with a combined mold core according to claim 1, characterized in that: A plurality of diversion openings (12) are evenly distributed along the circumferential direction of the center of the upper mold (1), and the plurality of diversion openings (12) are connected by the diversion bridge (13). The top shape of each diversion opening (12) is elliptical, and the bottom shape is V-shaped, with a smooth transition at the connection.
5. The aluminum tube extrusion forming device with a combined mold core according to claim 1, characterized in that: A plurality of connection holes (17) for fixing the trident-shaped base (31) are evenly arranged at the bottom of the trilobate groove (11) along the extension direction of the diverter bridge (13); Countersunk holes (311) are provided at positions on the trident-shaped base (31) corresponding to the connecting holes (17) one by one, and the countersunk holes (311) and the connecting holes (17) are fixed via a connecting piece.
6. The aluminum tube extrusion forming device with a combined mold core according to claim 1, characterized in that: A first groove (61) is provided on one end surface of the feed barrel (6), a first annular flange (14) is provided on the feed side of the upper mold (1), and the first groove (61) is connected to the first annular flange (14) in a concave-convex matching manner; The discharge side of the upper mold (1) has three sections of first bosses (15) cut by the three-leaf groove (11), and the edge of the three-pronged baffle (32) has three second bosses (321). The three first bosses (15) and the three second bosses (321) together form a second annular flange (16), and the second annular flange (16) and the second groove (22) are connected in a concave-convex manner.
7. The aluminum tube extrusion forming device with a combined mold core according to claim 1, characterized in that: One end of the lower die (2) is provided with a tapered hole (23) which is larger at the top and smaller at the bottom along its axial direction, the angle between the generatrix of the tapered hole (23) and its central axis is 60°, and the stepped hole (21) is provided at the bottom of the tapered hole (23); The large hole diameter of the step hole (21) is the same as the large end diameter of the outer contour of the core gear sleeve (34), and the small hole diameter of the step hole (21) is the same as the small end diameter of the outer contour of the core gear sleeve (34).
8. The aluminum tube extrusion forming device with a combined mold core according to claim 1, characterized in that: The bottom end of the molding core column (33) is provided with an external thread, and the center of the trident-shaped base (31) is provided with an internal thread matching the external thread.
9. An aluminum tube extrusion molding method using the aluminum tube extrusion molding device according to any one of claims 1 to 8, comprising the following steps: S1: placing the upper mold (1) and the lower mold (2) on a workbench respectively and fixing them; S2: inserting the core tooth sleeve (34) into the stepped hole (21) of the lower die (2), and fixing the trident-shaped base (31) into the trilobate-shaped groove (11) of the upper die (1) via a connecting piece; S3: passing the forming core column (33) through the through hole in the center of the trident-shaped baffle (32) and connecting it to the trident-shaped base (31) via threads, and simultaneously inserting the trident-shaped baffle (32) into the trilobate-shaped groove (11); S4: closing the lower mold (2) onto the upper mold (1) and pressing the trident-shaped baffle (32); S5: After the feed barrel (6) is docked with the upper mold (1), high-temperature treated aluminum material is added, and then the extrusion rod (7) is operated to extrude to obtain a finished aluminum tube.
10. The aluminum tube extrusion molding method of the aluminum tube extrusion molding device according to claim 9, characterized in that: Before the operation S2, the molding core tooth column (33) and the core tooth sleeve (34) of corresponding specifications are selected according to the working belt (5) required for molding the aluminum tube to be processed.
Citation Information
Patent Citations
Aluminum alloy hot extrusion die and assembling method thereof
CN112718905A
Disc drawing round pipe mold capable of being used by joint
CN113578994A
Hard alloy milling cutter with high impact resistance and preparation method thereof
CN113621892A
Semi-enclosed tubular aluminum profile hot-extrusion die
CN203737740U
Skylight guide rail profile mold for locally eliminating air hole structure through secondary extrusion of fixed mold
CN218555179U