Aluminum plate machining and bending device and method

Through the hydraulic bending device and automatic control system, combined with high-strength engineering plastics and aerosol spray ends, the problems of mold material influence and low processing efficiency in aluminum plate bending are solved, and an efficient and high-quality aluminum plate bending process is realized.

CN118808385AInactive Publication Date: 2024-10-22LINYI JIYU BUILDING MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410696956.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-05-31
Publication Date
2024-10-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the existing aluminum plate processing technology, the bottom material of the mold is not suitable, which affects the bending quality of the aluminum plate. Moreover, the spraying protective film and heating process increase the handling procedures of workers and reduce the processing efficiency.

Method used

The hydraulic bending device is combined with the automatically controlled aluminum plate processing and bending device, including the bottom of the bending head and the aerosol spray end made of high-strength engineering plastics. Through the automation of hydraulic pressure and spray heating procedures, the aluminum plate is ensured during the bending process. Medium shape hold and surface protection.

Benefits of technology

It improves the processing efficiency and surface quality of aluminum plate bending, ensures the integrity of the internal crystal structure of the aluminum plate, reduces workers' handling steps, and improves the overall processing efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118808385A_ABST
    Figure CN118808385A_ABST
Patent Text Reader

Abstract

The invention discloses an aluminum plate machining bending device which comprises a bending machine body and a master control end, the bending machine body comprises a bending die end and a hydraulic bending device, and an aluminum plate positioned and placed at the bending die end is made to form a needed shape through downward pressing of the hydraulic bending device; the aluminum plate spraying end is used for performing spraying protection treatment on the surface of the aluminum plate, and the aluminum plate spraying end is conveyed to the bending mold end through the conveying end; and meanwhile, an aerial fog spraying end used for spraying aerial fog to the surface of the aluminum plate is arranged at the bottom of the hydraulic bending device. The invention further discloses an aluminum plate bending method. Spraying and heating procedures are combined together through automatic control, and the machining efficiency can be improved; meanwhile, high-strength engineering plastic is adopted as the material of the bottom end of the bending head, so that the bending surface quality of the aluminum plate can be improved while the strength is ensured; and a high-pressure spraying structure is arranged at the bottom of the bending head, so that the bending effect of the aluminum plate can be further improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of aluminum plate processing, and in particular to an aluminum plate processing and bending device and method. Background Art

[0002] The hardness of aluminum plate is relatively high. If the pressure of the mold is not well controlled during bending, or the bottom of the mold is processed roughly, the bending quality of the aluminum plate will be affected. In the existing technology, the commonly used technology is to spray a layer of protective film on the surface of the aluminum plate and heat the aluminum plate appropriately. However, because it involves three processes, workers need to increase the handling procedure, which will affect the processing efficiency. In addition, experience has shown that the material of the bottom of the mold is critical to the quality of the aluminum plate bending. If it is too hard, it will destroy the internal crystal structure of the aluminum plate, and if it is too soft, it will not achieve the purpose of bending. Therefore, it is necessary to improve the existing technology. Summary of the invention

[0003] The present invention aims at the above-mentioned problems and proposes an aluminum plate processing and bending device and method to solve the above-mentioned problems.

[0004] In order to achieve the above technical objectives, the present invention adopts an aluminum plate processing and bending device, including a bending machine body for bending aluminum plates, and a general control end. The bending machine body includes a bending mold end for bending and shaping the aluminum plate, and a hydraulic bending device for bending the mold. The aluminum plate positioned on the bending mold end is formed into a desired shape by pressing down the hydraulic bending device; it also includes an aluminum plate spraying end for spraying a protective treatment on the surface of the aluminum plate, and the aluminum plate spraying end is transmitted to the bending mold end through the transmission end; at the same time, an aerosol spraying end for spraying aerosol onto the surface of the aluminum plate is provided at the bottom of the hydraulic bending device.

[0005] Preferably, the aluminum plate spraying end comprises: a spraying room, the rear of which is provided with a first conveying end for conveying the aluminum plate to be sprayed to the spraying room;

[0006] The upper end of the spraying room is provided with a spraying mechanism based on multi-directional rotation adjustment; the bottom surface of the spraying room is provided with a positioning and conveying end capable of positioning and conveying the aluminum plate to be sprayed; the left side of the spraying room is provided with a drying room for drying the sprayed aluminum plate, and the bottom surface of the drying room is provided with a second conveying end for placing and conveying the sprayed aluminum plate;

[0007] The left side of the drying chamber is provided with a third conveying end which is connected to the second conveying end and can convey the aluminum plate after spraying and drying to the bending mold end.

[0008] Further preferably, the aerosol spray end includes: a socket part installed on the bottom of the hydraulic bending device and socketed on the bottom of the bending head, the socket part includes: a socket body whose shape is adapted to the shape of the bottom of the bending head, the upper end of the socket body is a pressure-bearing surface made of pressure-bearing material, and the upper end of the pressure-bearing surface is provided with a snap-fitting part that forms a snap connection with the bottom and both sides of the bending head; a liquid containing cavity is provided in the socket body, and the bottom of the liquid containing cavity is also located at the lower end of the pressure-bearing surface; a small-diameter atomizing spray hole is provided at the bottom of the liquid containing cavity; a liquid atomizer is provided in the liquid containing cavity, and the liquid atomizer passes through the upper end of the liquid containing cavity through the connecting pipe at the upper end, and is connected to a liquid storage end located outside the bending machine body.

[0009] More preferably, the diameter of the small-diameter atomizing spray holes is 0.2-0.4 mm, the spacing between the small-diameter atomizing spray holes is 0.6-0.8 mm, and semicircular protrusions for contacting the surface of the aluminum plate are provided between the small-diameter atomizing spray holes; the diameter of the semicircular protrusions is 0.2-0.4 mm.

[0010] More preferably, the socket body is made of high-strength engineering plastics, and the high-strength engineering plastics are mixed with polyamide and glass fiber in a certain proportion.

[0011] More preferably, the space between the bending die end and the hydraulic bending device of the bending machine body is provided with a heating device capable of heating the space between the bending die end and the hydraulic bending device to 50-70° within 3-5 minutes, and the heating device forms a control connection with the main control end.

[0012] Furthermore, an electromagnetic suction cup device capable of sucking and positioning the aluminum plate is provided at the lower part of the bending die end, and the electromagnetic suction cup device is connected to the main control end in a control manner.

[0013] The present invention also discloses an aluminum plate bending method, comprising the following steps:

[0014] Step 1: In the spray room, spray the surface of the aluminum plate;

[0015] Step 2: The sprayed aluminum plate is conveyed into the bending machine body through a conveyor belt for heating;

[0016] Step 3: After the heated aluminum plate is left to stand for a period of time, it is bent using the bending die end;

[0017] Preferably, in step three, the standing time is 2-3 minutes, and the bending pressure of the bending mold is 12-15 tons.

[0018] After adopting the above technical improvements, the present invention has the following advantages:

[0019] 1. The present invention combines the spraying and heating procedures together by automatic control, which can improve the processing efficiency;

[0020] 2. The present invention also uses high-strength engineering plastic as the bottom end material of the bending head, which can ensure the strength while improving the bending surface quality of the aluminum plate;

[0021] 3. The present invention provides a high-pressure spray structure at the bottom of the bending head, which can further improve the bending effect of the aluminum plate. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 Shown is a schematic diagram of the overall structure of the present invention;

[0023] Figure 2 Shown is a schematic diagram of the structure of the aerosol spray end of the present invention;

[0024] Figure 3 Shown is a schematic diagram of the bottom structure of the sleeve body of the present invention;

[0025] Among them, 1. bending machine body; 2. total control end; 3. bending die end; 4. hydraulic bending device; 5. spraying room; 6. first conveying end; 7. spraying mechanism; 8. positioning conveying end; 9. drying room; 10. second conveying end; 11. third conveying end; 12. bending head; 13. sleeve joint; 14. sleeve body; 15. pressure-bearing surface; 16. buckle joint; 17. liquid-containing cavity; 18. small-caliber atomizing spray hole; 19. liquid atomizer; 20. connecting pipe; 21. liquid storage end. 22. semicircular convex block; 23. heating device; 24. electromagnetic suction cup device. DETAILED DESCRIPTION

[0026] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments.

[0027] Depend on Figure 1 It can be seen that an aluminum plate processing and bending device includes a bending machine body 1 for bending aluminum plates, and a main control terminal 2. A heating device 23 is provided in the space between the bending die end 3 and the hydraulic bending device 4 of the bending machine body 1, which can heat the space between the bending die end 3 and the hydraulic bending device 4 to 50-70° within 3-5 minutes. The heating device 23 and the main control terminal 2 form a control connection.

[0028] The bending machine body 1 includes a bending die end 3 for bending and shaping the aluminum plate, and a hydraulic bending device 4 for bending the die. The aluminum plate positioned and placed on the bending die end 3 is formed into a desired shape by pressing down the hydraulic bending device 4. An electromagnetic suction cup device 24 capable of sucking and positioning the aluminum plate is provided at the lower part of the bending die end 3, and the electromagnetic suction cup device 24 is controlled and connected to the main control end 2.

[0029] The present invention also includes an aluminum plate spraying end for spraying and protecting the surface of the aluminum plate, which is transmitted to the bending mold end through the transmission end; at the same time, an aerosol spraying end for spraying aerosol onto the surface of the aluminum plate is provided at the bottom of the hydraulic bending device 4.

[0030] In the present invention, the preferred aluminum plate spraying end includes: a spraying room 5, the rear part of which is provided with a first conveying end 6 for conveying the aluminum plate to be sprayed to the spraying room 5; a spraying mechanism 7 based on multi-directional rotation adjustment is provided at the upper end of the spraying room 5; the bottom surface of the spraying room 5 is provided with a positioning conveying end 8 that can position and convey the aluminum plate to be sprayed; the left side of the spraying room 5 is provided with a drying chamber 9 for drying the aluminum plate after spraying, and the bottom surface of the drying chamber 9 is provided with a second conveying end 10 for placing and conveying the aluminum plate after spraying.

[0031] A third conveying end 11 connected to the second conveying end 10 is provided on the left side of the drying chamber 9 and can convey the aluminum plate after spraying and drying to the bending mold end.

[0032] The structure of the present invention combines the spraying and heating procedures together by automatic control, thereby improving the processing efficiency.

[0033] Depend on Figure 2 It can be seen that in the present invention, the preferred aerosol spray end includes: a socket part 13 installed at the bottom of the hydraulic bending device 4 and socketed at the bottom of the bending head 12, and the socket part 13 includes: a socket body 14 whose shape is adapted to the shape of the bottom of the bending head 12. In the present invention, the socket body 14 is made of high-strength engineering plastic, and the high-strength engineering plastic is a mixture of polyamide and glass fiber in a certain proportion.

[0034] The present invention adopts high-strength engineering plastic as the bottom end material of the bending head, which can ensure the strength and improve the bending surface quality of the aluminum plate.

[0035] The upper end of the sleeve body 14 is a pressure-bearing surface 15 made of pressure-bearing material, and the upper end of the pressure-bearing surface 15 is provided with a buckling portion 16 that forms a buckle connection with the bottom and both sides of the bending head 12; a liquid containing cavity 17 is provided in the sleeve body 14, and the bottom of the liquid containing cavity 17 is also located at the lower end of the pressure-bearing surface 15; a small-caliber atomizing spray hole 18 is provided at the bottom of the liquid containing cavity 17; a liquid atomizer 19 is provided in the liquid containing cavity 17, and the liquid atomizer 19 passes through the upper end of the liquid containing cavity through the upper connecting pipe 20, and is connected to a liquid storage end 21 located outside the bending machine body.

[0036] Depend on Figure 3It can be seen that in the present invention, the diameter of the small-diameter atomizing nozzle 18 is 0.2-0.4 mm, the spacing between the small-diameter atomizing nozzles 18 is 0.6-0.8 mm, and semicircular protrusions 22 for contacting the surface of the aluminum plate are provided between the small-diameter atomizing nozzles 18; the diameter of the semicircular protrusions is 0.2-0.4 mm.

[0037] In the above structure of the present invention, a high-pressure spray structure is provided at the bottom of the bending head 12, which can further improve the bending effect of the aluminum plate.

[0038] The present invention also discloses an aluminum plate bending method, comprising the following steps:

[0039] Step 1: In the spray room, spray the surface of the aluminum plate;

[0040] Step 2: The sprayed aluminum plate is conveyed into the bending machine body through a conveyor belt for heating;

[0041] Step 3: After the heated aluminum plate is left to stand for a period of time, it is bent using the bending die end;

[0042] In step three, the standing time is 2-3 minutes, and the bending pressure of the bending mold 3 is 12-15 tons.

[0043] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the technical principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. An aluminum plate processing and bending device, comprising a bending machine body for bending aluminum plates, and a general control end, wherein the bending machine body comprises a bending die end for bending and shaping the aluminum plate, and a hydraulic bending device for bending the die, wherein the aluminum plate positioned and placed on the bending die end is formed into a desired shape by pressing down the hydraulic bending device; characterized in that: It also includes an aluminum plate spraying end for spraying protective treatment on the surface of the aluminum plate, and the aluminum plate spraying end is transmitted to the bending mold end through the transmission end; at the same time, an aerosol spraying end for spraying aerosol onto the surface of the aluminum plate is provided at the bottom of the hydraulic bending device.

2. The aluminum plate processing and bending device according to claim 1, characterized in that: The aluminum plate spraying end comprises: a spraying room, the rear of which is provided with a first conveying end for conveying the aluminum plate to be sprayed to the spraying room; The upper end of the spraying room is provided with a spraying mechanism based on multi-directional rotation adjustment; the bottom surface of the spraying room is provided with a positioning and conveying end capable of positioning and conveying the aluminum plate to be sprayed; the left side of the spraying room is provided with a drying room for drying the sprayed aluminum plate, and the bottom surface of the drying room is provided with a second conveying end for placing and conveying the sprayed aluminum plate; The left side of the drying chamber is provided with a third conveying end which is connected to the second conveying end and can convey the aluminum plate after spraying and drying to the bending mold end.

3. The aluminum plate processing and bending device according to claim 1, characterized in that: The aerosol spray end includes: a socket part installed on the bottom of the hydraulic bending device and socketed on the bottom of the bending head, the socket part includes: a socket body whose shape is adapted to the shape of the bottom of the bending head, the upper end of the socket body is a pressure-bearing surface made of pressure-bearing material, and the upper end of the pressure-bearing surface is provided with a snap-fitting part that forms a snap connection with the bottom and both sides of the bending head; a liquid containing cavity is provided in the socket body, and the bottom of the liquid containing cavity is also located at the lower end of the pressure-bearing surface; a small-caliber atomizing spray hole is provided at the bottom of the liquid containing cavity; a liquid atomizer is provided in the liquid containing cavity, and the liquid atomizer passes through the upper end of the liquid containing cavity through the connecting pipe at the upper end, and is connected to a liquid storage end located outside the bending machine body.

4. The aluminum plate processing and bending device according to claim 3, characterized in that: The diameter of the small-diameter atomizing spray holes is 0.2-0.4 mm, the spacing between the small-diameter atomizing spray holes is 0.6-0.8 mm, and semicircular protrusions for contacting the surface of the aluminum plate are arranged between the small-diameter atomizing spray holes; the diameter of the semicircular protrusions is 0.2-0.4 mm.

5. The aluminum plate processing and bending device according to claim 3, characterized in that: The sleeve body is made of high-strength engineering plastics, which is a mixture of polyamide and glass fiber in a certain proportion.

6. The aluminum plate processing and bending device according to claim 1, characterized in that: The space between the bending die end and the hydraulic bending device of the bending machine body is provided with a heating device capable of heating the space between the bending die end and the hydraulic bending device to 50-70° within 3-5 minutes, and the heating device forms a control connection with the main control end.

7. The aluminum plate processing and bending device according to claim 1, characterized in that: An electromagnetic suction cup device capable of sucking and positioning the aluminum plate is provided at the lower part of the bending die end, and the electromagnetic suction cup device forms a control connection with the main control end.

8. A method for bending an aluminum plate as claimed in claims 1 to 7, characterized in that: The following steps are included: Step 1: In the spray room, spray the surface of the aluminum plate; Step 2: The sprayed aluminum plate is conveyed into the bending machine body through a conveyor belt for heating; Step 3: After the heated aluminum plate is left to stand for a while, bend it with the bending die end.

9. The aluminum plate bending method according to claim 8, characterized in that: In the step three, the standing time is 2-3 minutes, and the bending pressure of the bending mold is 12-15 tons.