Processing technology method of super back seal
By adding CMP processing and controlling CVD film growth to the super back sealing process, the problem of silicon wafer surface defects is solved and the product yield and surface quality are significantly improved.
Patent Information
- Application Number
- CN202410857979.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-10-22
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of silicon wafer back seal processing, and in particular to a processing method of a super back seal. Background Art
[0002] In the semiconductor manufacturing industry, the surface quality of silicon wafers is crucial to the performance of the final product. In the chemical vapor deposition (CVD) process, the quality of the silicon wafer surface is particularly critical to the subsequent processing flow and the performance of the final product. However, in the prior art, silicon wafers often leave defects, scratches, marks, etc. on the surface during the CVD thermal process.
[0003] In the super back-sealing process (SiO2 LTO film + Poly Si film), two CVD processes are performed, so the risk of defects on the silicon wafer surface is further increased, and serious products may be scrapped. If the first CVD process (LTO film) leaves defects on the wafer surface, they will be wrapped in the poly film after the second layer of Poly film is deposited. It is difficult to completely remove them during subsequent polishing, which reduces the yield of the final product. Summary of the invention
[0004] The present invention mainly solves the deficiencies in the prior art and provides a super back-sealing processing method, which adds a CMP between two CVD processes in the super back-sealing product processing process, and then performs a final CMP after the back-sealing process is completed, thereby improving the front-side marks, scratches, stains and other defects of the wafer. This makes the front-side defects of the processed silicon wafers less and the product yield is greatly improved.
[0005] The above technical problems of the present invention are mainly solved by the following technical solutions: A super back seal processing method includes the following steps: The first step: the first APCVD process is performed on the double-sided polished silicon wafer to coat a layer of silicon dioxide film, namely LTO film, on the back of the silicon wafer with a thickness of 0.3 to 0.6 μm.
[0006] Step 2: After the silicon wafer with the first layer of silicon dioxide film is cleaned, the front side of the silicon wafer is subjected to chemical mechanical polishing (CMP), so that stains, marks and other defects on the front side of the silicon wafer are initially removed to facilitate the next step of processing.
[0007] Step 3: Perform a second LPCVD process to coat the silicon wafer with a layer of polycrystalline silicon film, namely Poly film, with a thickness of about 0.3 to 0.8 μm.
[0008] Step 4: Perform a second CMP process on the front side of the silicon wafer to obtain a finished super back-sealed polished wafer.
[0009] The polysilicon film remaining on the front side during the second LPCVD process is removed, and a final polished wafer that is flat, smooth, and free of appearance defects is obtained through final chemical mechanical polishing.
[0010] CMP in silicon wafer processing uses polishing liquid and polishing cloth, and uses chemical corrosion and mechanical grinding to remove the damaged layer on the surface of the silicon wafer. Preferably, the silicon dioxide film processed by the first APCVD is polished to remove 0.1 to 0.5 μm.
[0011] Preferably, the polishing removal amount of the second CMP process is about 0.5-1 μm.
[0012] Preferably, during APCVD processing, a certain amount of silane and oxygen are introduced into the APCVD equipment, and a chemical reaction occurs through heating to form a silicon dioxide film. By real-time control of the temperature in the reaction area, the film growth rate at different positions is effectively affected, thereby improving the uniformity of the film.
[0013] Preferably, the ratio of silane and oxygen introduced into the APCVD equipment during the reaction is 2:19, and the tray running speed is 325-355 mm / min.
[0014] The present invention can achieve the following effects: The present invention provides a super back-sealing processing method. Compared with the prior art, a CMP is added between two CVD processes in the super back-sealing product processing process, and a final CMP is performed after the back-sealing process is completed, thereby improving the defects such as imprints, scratches, and stains on the front of the wafer. This makes the front defects of the processed silicon wafers less and the product yield is greatly improved. DETAILED DESCRIPTION
[0015] The technical solution of the invention is further specifically described below through embodiments.
[0016] Embodiment: A processing method of a super back seal comprises the following steps: Step 1: Perform the first APCVD process on the double-sided polished silicon wafer to coat a layer of silicon dioxide film, namely LTO film, on the back of the silicon wafer with a thickness of 0.45 μm.
[0017] Step 2: After the silicon wafer with the first layer of silicon dioxide film is cleaned, the front side of the silicon wafer is subjected to chemical mechanical polishing (CMP). The amount of silicon dioxide film removed by the first APCVD polishing is 0.3 μm.
[0018] Step 3: Perform a second LPCVD process to coat the silicon wafer with a layer of polycrystalline silicon film, namely Poly film, with a thickness of about 0.55μm.
[0019] Step 4: Perform a second CMP process on the front side of the silicon wafer, and the polishing removal amount of the second CMP process is about 0.6 μm. A finished product of a super back-sealed polished wafer is obtained.
[0020] During APCVD processing, a certain amount of silane and oxygen are introduced into the APCVD equipment. During the reaction, the ratio of silane and oxygen introduced into the APCVD equipment is 2:19, and the tray running speed is 345mm / min. A silicon dioxide film is formed by a chemical reaction through heating. The real-time control of the temperature in the reaction area effectively affects the film growth rate at different positions, thereby improving the uniformity of the film.
[0021] In summary, the processing method of the super back seal is to add a CMP between the two CVD processes in the processing of the super back seal product, and then perform the final CMP after the back seal process is completed, so as to improve the defects such as imprints, scratches, and stains on the front of the wafer. This makes the front defects of the processed silicon wafers less and the product yield is greatly improved.
[0022] The above description is only a specific embodiment of the present invention, but the structural features of the present invention are not limited thereto. Any changes or modifications made by any technician in the field of the present invention are included in the patent scope of the present invention.
Claims
1. A processing method for super back seal, characterized in that The steps are as follows: Step 1: Perform the first APCVD process on the double-sided polished silicon wafer to coat a layer of silicon dioxide film, i.e., LTO film, on the back of the silicon wafer, with a thickness of 0.3 to 0.6 μm; Step 2: After the silicon wafer with the first layer of silicon dioxide film is cleaned, the front side of the silicon wafer is subjected to chemical mechanical polishing (CMP); Step 3: Perform the second LPCVD process to coat the silicon wafer with a layer of polycrystalline silicon film, i.e., Poly film, with a thickness of about 0.3 to 0.8 μm; Step 4: Perform a second CMP process on the front side of the silicon wafer to obtain a finished super back-sealed polished wafer.
2. The processing method of the super back seal according to claim 1, characterized in that: The amount of silicon dioxide film removed by polishing during the first APCVD process is 0.1 to 0.5 μm.
3. The processing method of the super back seal according to claim 2 is characterized in that: The polishing removal amount of the second CMP process is about 0.5 to 1 μm.
4. The processing method of the super back seal according to claim 1 is characterized in that: During APCVD processing, a certain amount of silane and oxygen are introduced into the APCVD equipment, and a chemical reaction occurs through heating to form a silicon dioxide film. By real-time control of the temperature in the reaction area, the film growth rate at different positions is effectively affected, thereby improving the uniformity of the film.
5. The processing method of the super back seal according to claim 4 is characterized in that: During the reaction, the ratio of silane and oxygen introduced into the APCVD equipment was 2:19, and the tray running speed was 325-355 mm / min.