Manufacturing method of touch screen FPC

Through the method of layered processing of FPC cables and double-sided EMI attachment, the problems of assembly difficulty and high damage rate caused by the FPC cable structure in the existing technology are solved, achieving easier assembly of the whole machine and lower damage rate. loss rate.

CN118829094APending Publication Date: 2024-10-22STARRY ELECTRONIC TECH SHENZHEN CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310460326.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-04-21
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

The linear cable arrangement structure of the existing touch screen FPC results in a lack of reserved space during the assembly process of the whole machine, which can easily cause the customer case to press onto the protruding position of the TP cable, affecting the ease of assembly and the damage rate.

Method used

Using the method of layered processing of FPC cables and double-sided EMI attachment, chemically thinning the SENSOR functional sheet and constructing an FPC double-layer cable structure, the protruding size of the FPC bending position is reduced, and the avoidance space is reserved to avoid customer casing Press it to the protruding position of the TP cable.

Benefits of technology

It improves the simplicity of the overall assembly of the touch screen, reduces the damage rate, and ensures the protection of the internal structure of the product and the stability of the entire machine.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118829094A_ABST
    Figure CN118829094A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of touch screens, in particular to a touch screen FPC manufacturing method which comprises the following steps that S1, touch screen FPC accessories are prepared; s2, carrying out layering treatment on the FPC flat cable; and S3, the double-sided EMI is attached to the FPC flat cable, so that the wire outlet space of the TX wiring at the bottom layer of the FPC is saved. In the preparation process of the touch screen FPC accessory, the overall thickness of the touch screen FPC accessory is reduced through a processing mode of chemically thinning a SENSOR functional sheet, an FPC double-layer flat cable structure is constructed through a specific method for preparing an FPC flat cable, then a protruding part after an FPC is bent serves as an important component of a touch display screen, double-sided EMI is attached to the FPC flat cable, and therefore the touch screen FPC accessory can be manufactured. By means of the manufacturing method, the wire outlet space of the TX wiring at the bottom layer of the FPC is saved, on the premise that the internal structure of a product is protected, the protruding size of the bending position of the FPC is reduced, the avoiding space is reserved for the whole machine, the situation that a client machine shell is pressed to the protruding position of the TP wiring is avoided, the overall assembling simplicity of the touch screen is guaranteed, and the damage rate is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of touch screens, and in particular to a method for manufacturing a touch screen FPC. Background Art

[0002] A touch screen is a professional tool used in electronic devices such as mobile phones and tablet computers to collect, identify and display information. In the structure of existing touch screens, the FPC cables are often assembled in a linear structure, resulting in a lack of reserved space at the FPC position during the assembly of the touch screen. This can easily cause the client's case to press on the protruding position of the TP cable, which requires improvement. Summary of the invention

[0003] The purpose of the present invention is to solve the shortcomings in the prior art and to propose a method for manufacturing a touch screen FPC.

[0004] In order to achieve the above object, the present invention adopts the following technical solution: a method for manufacturing a touch screen FPC, comprising the following steps:

[0005] S1: Prepare touch screen FPC accessories;

[0006] S2: FPC cable layering processing;

[0007] S3: Attach the double-sided EMI to the FPC cable to save the outlet space of the TX wiring on the bottom layer of the FPC.

[0008] As a further solution of the present invention, in S1, the touch screen FPC accessories include a cover plate, a SENSOR functional sheet, double-sided EMI and FPC cables, the FPC cables include FPC bottom layer TX routing and FPC top layer RX routing, and the SENSOR functional sheet is divided into a SENSOR TX layer and a SENSOR RX layer based on the upper and lower surfaces.

[0009] As a further solution of the present invention, in S2, the steps of layering the FPC cable are specifically as follows:

[0010] S210: Divide the FPC cable into TX layer and RX layer;

[0011] S220: The TX layer and the RX layer are divided into three-stage binding methods;

[0012] The TX layer and the RX layer refer to the TX wiring on the bottom layer of the FPC and the RX wiring on the top layer of the FPC respectively.

[0013] As a further solution of the present invention, the three-stage binding method is specifically:

[0014] S221: Bind the RX layer to the top layer, and the RX trace on the top layer of the FPC is bound to the side of the cover through the SENSOR RX layer of the SENSOR functional chip;

[0015] S222: Bind the TX layer to the bottom layer, and the TX trace of the FPC bottom layer is bound to the back of the SENSOR function slice through the SENSOR TX layer of the SENSOR function slice;

[0016] S223: Extend the TX wiring on the bottom layer of the FPC to the back of the SENSOR functional chip.

[0017] As a further solution of the present invention, in S1, the step of preparing the touch screen FPC accessories further includes:

[0018] S110: Preparation of SENSOR functional slices;

[0019] S120: Double-sided EMI preparation;

[0020] S130: FPC cable preparation.

[0021] As a further solution of the present invention, it is characterized in that in S110, the steps of preparing the SENSOR functional sheet are specifically as follows:

[0022] S111: preparing a large glass substrate;

[0023] S112: forming a sensor area on the glass substrate corresponding to the sensor range by laser engraving or chemical etching;

[0024] S113: bonding the two corresponding glass substrates forming the sensor area so that the sensor area is in a sealed state;

[0025] S114: using a chemical thinning method to reduce the overall thickness of the two glass substrates;

[0026] S115: Cut and split the bonding position of the glass substrate to obtain a single sensor functional sheet.

[0027] As a further solution of the present invention, the chemical thinning method is specifically to place the two bonded glass substrates into an etching solution for immersion treatment, the etching solution is composed of one or more of hydrofluoric acid, concentrated nitric acid, and concentrated hydrochloric acid, and the immersion treatment time is 25 minutes.

[0028] As a further solution of the present invention, in 120, the steps of preparing the double-sided EMI are specifically as follows:

[0029] S121: preparing a flexible substrate as a base structure for double-sided EMI;

[0030] S122: Arranging a copper foil layer on the double-sided EMI substrate structure, and forming an EMI circuit on the surface of the copper foil layer by exposure and etching;

[0031] S123: A protective film is attached to the surface of the EMI circuit, and copper is exposed at the interface end of the EMI circuit;

[0032] S124: Attach shielding film to the exposed copper position of the EMI circuit.

[0033] As a further solution of the present invention, in S130, the FPC cable preparation specifically refers to FPC double-layer cable preparation, and the steps of the FPC double-layer cable preparation are specifically as follows:

[0034] S131: forming a polyimide matrix film on the FPC cable substrate by casting or coating a liquid polyimide resin;

[0035] S132: forming a crystal planting layer on the polyimide substrate film by sputtering;

[0036] S133: forming a resist pattern of a reverse pattern of the circuit on the implant layer by photolithography to obtain a plating-resistant layer;

[0037] S134: forming a conductor circuit by electroplating in the blank part, removing the anti-etching layer and unnecessary planting layer, and forming a first layer circuit;

[0038] S135: Casting or coating liquid polyimide resin on the first layer circuit;

[0039] S136: Repeat steps S132-S134 to form a double-layer FPC wiring structure, thereby obtaining a TX wiring on the bottom layer of the FPC and a RX wiring on the top layer of the FPC.

[0040] As a further solution of the present invention, the step of forming the anti-etching layer pattern of the inverse pattern of the circuit by photolithography is specifically to form the anti-etching layer pattern of the inverse pattern of the circuit by sequentially performing exposure, development, etching and stripping.

[0041] Compared with the prior art, the advantages and positive effects of the present invention are:

[0042] In the present invention, the overall thickness of the SENSOR functional sheet is reduced by chemically thinning the sheet, and a specific method for preparing the FPC cable is used to construct an FPC double-layer cable structure, and then the protruding portion after the FPC is bent is used as an important component of the touch display screen. Under the premise of protecting the internal structure of the product, this manufacturing method is used to reduce the protruding size of the FPC bending position, reserve avoidance space for the entire machine, and avoid the client shell from pressing on the protruding position of the TP cable, thereby ensuring the simplicity of the overall assembly of the touch screen and reducing the damage rate. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 A schematic diagram of the main steps of a method for manufacturing a touch screen FPC is provided in the present invention;

[0044] Figure 2 A schematic diagram of the structure of a touch screen FPC accessory for a touch screen FPC manufacturing method proposed in the present invention;

[0045] Figure 3 A detailed schematic diagram of step 2 of a method for manufacturing a touch screen FPC is provided in the present invention;

[0046] Figure 4 A detailed schematic diagram of step 220 of a method for manufacturing a touch screen FPC is provided for the present invention;

[0047] Figure 5 A detailed schematic diagram of step 1 of a method for manufacturing a touch screen FPC is provided in the present invention;

[0048] Figure 6 A detailed schematic diagram of step 110 of a method for manufacturing a touch screen FPC is provided in the present invention;

[0049] Figure 7 A detailed schematic diagram of step 120 of a method for manufacturing a touch screen FPC is provided for the present invention;

[0050] Figure 8 The present invention provides a detailed schematic diagram of step 130 of a method for manufacturing a touch screen FPC.

[0051] In the figure: 1. Cover plate; 2. SENSOR functional chip; 3. Double-sided EMI; 4. TX wiring on the bottom layer of FPC; 5. RX wiring on the top layer of FPC. DETAILED DESCRIPTION

[0052] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0053] In the description of the present invention, it should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, in the description of the present invention, "multiple" means two or more, unless otherwise clearly and specifically defined.

[0054] Embodiment 1

[0055] See also Figure 1 The present invention provides a technical solution: a method for manufacturing a touch screen FPC, comprising the following steps:

[0056] S1: Prepare touch screen FPC accessories;

[0057] S2: FPC cable layering processing;

[0058] S3: Attach the double-sided EMI3 to the FPC cable to save the outlet space of the TX trace 4 on the bottom layer of the FPC.

[0059] Specifically, the overall thickness of the SENSOR functional sheet 2 is reduced by chemically thinning it, and a specific method for preparing the FPC cable is used to construct a double-layer FPC cable structure. The protruding part after the FPC is bent is used as an important component of the touch display screen. Under the premise of protecting the internal structure of the product, this production method is used to reduce the protruding size of the FPC bending position, reserve avoidance space for the entire machine, and prevent the client shell from pressing on the protruding position of the TP cable.

[0060] See also Figure 2 In S1, the touch screen FPC accessories include a cover plate 1, a SENSOR functional sheet 2, a double-sided EMI 3 and an FPC cable. The FPC cable includes an FPC bottom layer TX trace 4 and an FPC top layer RX trace 5. The SENSOR functional sheet 2 is divided into a SENSOR TX layer and a SENSOR RX layer based on the upper and lower surfaces.

[0061] See also Figure 3 In S2, the steps of FPC cable layering are as follows:

[0062] S210: Divide the FPC cable into TX layer and RX layer;

[0063] S220: The TX layer and the RX layer are divided into three-stage binding methods;

[0064] The TX layer and the RX layer refer to the TX trace 4 on the bottom layer of the FPC and the RX trace 5 on the top layer of the FPC respectively.

[0065] See also Figure 4 , the three-stage binding method is as follows:

[0066] S221: Bind the RX layer to the top layer, and the FPC top layer RX trace 5 is bound to the side of the cover plate 1 through the SENSOR RX layer of the SENSOR functional sheet 2;

[0067] S222: Bind the TX layer to the bottom layer, and the FPC bottom layer TX trace 4 is bound to the back of the SENSOR function slice 2 through the SENSOR TX layer of the SENSOR function slice 2;

[0068] S223: Extend the TX wiring 4 on the bottom layer of the FPC to the back of the SENSOR functional sheet 2.

[0069] See also Figure 5 In S1, the step of preparing the touch screen FPC accessories also includes:

[0070] S110: Preparation of SENSOR functional sheet 2;

[0071] S120: Double-sided EMI3 preparation;

[0072] S130: FPC cable preparation.

[0073] See also Figure 6 , characterized in that, in S110, the steps of preparing the SENSOR functional sheet 2 are specifically as follows:

[0074] S111: preparing a large glass substrate;

[0075] S112: forming a sensor area on the glass substrate corresponding to the sensor range by laser engraving or chemical etching;

[0076] S113: bonding the two corresponding glass substrates forming the sensor area so that the sensor area is in a sealed state;

[0077] S114: using a chemical thinning method to reduce the overall thickness of the two glass substrates;

[0078] S115: Cut and separate the bonding positions of the glass substrate to obtain a single-piece SENSOR functional sheet 2.

[0079] The chemical thinning method is to place the two bonded glass substrates into an etching solution for immersion treatment. The etching solution is composed of one or more of hydrofluoric acid, concentrated nitric acid, and concentrated hydrochloric acid. The immersion treatment time is 25 minutes.

[0080] See also Figure 7 In 120, the steps of preparing double-sided EMI3 are specifically as follows:

[0081] S121: preparing a flexible substrate as a base structure of double-sided EMI3;

[0082] S122: Arranging a copper foil layer on the double-sided EMI3 substrate structure, and forming an EMI circuit on the surface of the copper foil layer by exposure and etching;

[0083] S123: A protective film is attached to the surface of the EMI circuit, and copper is exposed at the interface end of the EMI circuit;

[0084] S124: Attach shielding film to the exposed copper position of the EMI circuit.

[0085] See also Figure 8 In S130, the FPC cable preparation specifically refers to the FPC double-layer cable preparation, and the steps of the FPC double-layer cable preparation are specifically as follows:

[0086] S131: forming a polyimide matrix film on the FPC cable substrate by casting or coating a liquid polyimide resin;

[0087] S132: forming a crystal planting layer on the polyimide substrate film by sputtering;

[0088] S133: forming a resist pattern of a reverse pattern of the circuit on the implant layer by photolithography to obtain a plating-resistant layer;

[0089] S134: forming a conductor circuit by electroplating in the blank part, removing the anti-etching layer and unnecessary planting layer, and forming a first layer circuit;

[0090] S135: Casting or coating liquid polyimide resin on the first layer circuit;

[0091] S136: Repeat steps S132-S134 to form a double-layer FPC wiring structure, thereby obtaining a TX wiring 4 on the bottom layer of the FPC and a RX wiring 5 on the top layer of the FPC.

[0092] The step of forming the resist pattern of the reverse pattern of the circuit by photolithography is specifically to form the resist pattern of the reverse pattern of the circuit by sequentially performing exposure, development, etching, and stripping.

[0093] Working principle: Prepare the touch screen FPC accessories (including cover plate 1, SENSOR function sheet 2, double-sided EMI 3 and FPC cable, FPC cable includes FPC bottom TX line 4 and FPC top RX line 5, SENSOR function sheet 2 is divided into SENSORTX layer and SENSOR based on the upper and lower sides. RX layer) [SENSOR functional sheet 2 preparation (prepare a large glass substrate, form a sensor area in the glass substrate corresponding to the sensor range by laser engraving or chemical etching, bond the two glass substrates corresponding to the sensor area so that the sensor area is in a sealed state, and use chemical thinning to immerse the two bonded glass substrates in an etching solution for treatment. The etching solution is composed of one or more of hydrofluoric acid, concentrated nitric acid, and concentrated hydrochloric acid. The immersion time is 25 minutes, and the overall thickness of the two glass substrates is reduced. The glass substrate bonding position is cut and split to obtain a single SENSOR functional sheet 2), double-sided EMI3 preparation (prepare a flexible substrate as the base structure of double-sided EMI3, arrange a copper foil layer on the base structure of double-sided EMI3, and form an EMI circuit on the surface of the copper foil layer by exposure and etching, attach a protective film to the surface of the EMI circuit, and expose copper at the interface end of the EMI circuit, and attach a shielding film to the copper exposed position of the EMI circuit), FPC cable preparation (on On the FPC wiring substrate, a polyimide substrate film is formed by casting or coating a liquid polyimide resin, a planting crystal layer is formed on the polyimide substrate film by sputtering, and a resist layer pattern of the reverse pattern of the circuit is formed on the planting crystal layer by photolithography, based on the method of sequentially performing exposure, development, etching, and film stripping to obtain a plating-resistant layer, and a conductor circuit is formed by electroplating in the blank part, and the resist layer and unnecessary planting crystal layer are removed to form a first layer circuit, and a liquid polyimide resin is cast or coated on the first layer circuit, and then the first layer circuit is re- Repeat steps S132-S134 to form a double-layer FPC wiring structure, thereby obtaining the FPC bottom TX wiring 4 and the FPC top RX wiring 5)]; FPC wiring layering processing [dividing the FPC wiring into a TX layer and an RX layer, the TX layer and the RX layer refer to the FPC bottom TX wiring 4 and the FPC top RX wiring 5 respectively, and the TX layer and the RX layer are divided into three-stage binding methods (binding the RX layer to the top layer, and the FPC top RX wiring 5 is bound to the side of the cover plate 1 through the SENSOR RX layer of the SENSOR functional chip 2, and the TX layer is bound to the bottom layer, and the FPC bottom TX wiring 4 is bound to the SENSOR functional chip 2 through the SENSOR TX layer of the SENSOR functional chip 2 on the back of the SENSOR functional chip 2, and the FPC bottom TX wiring 4 is extended from the back of the SENSOR functional chip 2)];The double-sided EMI3 is attached to the FPC cable to save the outlet space of the TX wiring 4 at the bottom of the FPC. The overall thickness of the SENSOR functional sheet 2 is reduced by chemical thinning. The FPC double-layer cable structure is constructed by the specific method of preparing the FPC cable. The protruding part after the FPC is bent is used as an important part of the touch display screen. Under the premise of protecting the internal structure of the product, this production method is used to reduce the protruding size of the FPC bending position, reserve avoidance space for the whole machine, and avoid the client shell from pressing the protruding position of the TP cable. ;

[0094] The above are only preferred embodiments of the present invention and are not intended to limit the present invention in other forms. Any technician familiar with the profession may use the technical contents disclosed above to change or modify them into equivalent embodiments with equivalent changes and apply them to other fields. However, any simple modification, equivalent change and modification made to the above embodiments based on the technical essence of the present invention without departing from the technical solution of the present invention still falls within the protection scope of the technical solution of the present invention.

Claims

1. A method for manufacturing a touch screen FPC, characterized in that: The following steps are involved: S1: Prepare touch screen FPC accessories; S2: FPC cable layering processing; S3: Attach the double-sided EMI (3) to the FPC cable to save the outlet space of the TX wiring (4) on the bottom layer of the FPC.

2. The method for manufacturing a touch screen FPC according to claim 1, characterized in that: In S1, the touch screen FPC accessories include a cover plate (1), a SENSOR functional sheet (2), a double-sided EMI (3) and an FPC cable, the FPC cable includes an FPC bottom layer TX wiring (4) and an FPC top layer RX wiring (5), and the SENSOR functional sheet (2) is divided into a SENSORTX layer and a SENSORRX layer based on the upper and lower surfaces.

3. The method for manufacturing a touch screen FPC according to claim 1, characterized in that: In S2, the steps of layering the FPC cable are specifically as follows: S210: Divide the FPC cable into TX layer and RX layer; S220: The TX layer and the RX layer are divided into three-stage binding methods; The TX layer and the RX layer refer to the FPC bottom layer TX wiring (4) and the FPC top layer RX wiring (5) respectively.

4. The method for manufacturing a touch screen FPC according to claim 3, characterized in that: The three-stage binding method is specifically as follows: S221: Bind the RX layer to the top layer, and the RX trace (5) on the top layer of the FPC is bound to the side of the cover plate (1) through the SENSOR RX layer of the SENSOR functional sheet (2); S222: Bind the TX layer to the bottom layer, and the FPC bottom layer TX trace (4) is bound to the back of the SENSOR function chip (2) through the SENSORTX layer of the SENSOR function chip (2); S223: Extend the TX wiring (4) on the bottom layer of the FPC to the back of the SENSOR functional chip (2).

5. The method for manufacturing a touch screen FPC according to claim 1, characterized in that: In S1, the step of preparing the touch screen FPC accessories also includes: S110: Preparation of SENSOR functional sheet (2); S120: Double-sided EMI (3) preparation; S130: FPC cable preparation.

6. The method for manufacturing a touch screen FPC according to claim 5, characterized in that: In S110, the steps of preparing the SENSOR functional sheet (2) are specifically as follows: S111: preparing a large glass substrate; S112: forming a sensor area on the glass substrate corresponding to the sensor range by laser engraving or chemical etching; S113: bonding the two corresponding glass substrates forming the sensor area so that the sensor area is in a sealed state; S114: using a chemical thinning method to reduce the overall thickness of the two glass substrates; S115: Cut and separate the bonding positions of the glass substrate to obtain a single SENSOR functional sheet (2).

7. The method for manufacturing a touch screen FPC according to claim 6, characterized in that: The chemical thinning method is specifically to place the two bonded glass substrates into an etching solution for immersion treatment, wherein the etching solution is composed of one or more of hydrofluoric acid, concentrated nitric acid, and concentrated hydrochloric acid, and the immersion treatment time is 25 minutes.

8. The method for manufacturing a touch screen FPC according to claim 5, characterized in that: In the above 120, the steps of preparing the double-sided EMI (3) are specifically as follows: S121: preparing a flexible substrate as a base structure for double-sided EMI (3); S122: Arranging a copper foil layer on the double-sided EMI (3) substrate structure, and forming an EMI circuit on the surface of the copper foil layer by exposure and etching; S123: A protective film is attached to the surface of the EMI circuit, and copper is exposed at the interface end of the EMI circuit; S124: Attach shielding film to the exposed copper position of the EMI circuit.

9. The method for manufacturing a touch screen FPC according to claim 5, characterized in that: In S130, the FPC cable preparation specifically refers to the FPC double-layer cable preparation, and the steps of the FPC double-layer cable preparation are specifically as follows: S131: forming a polyimide matrix film on the FPC cable substrate by casting or coating a liquid polyimide resin; S132: forming a crystal planting layer on the polyimide substrate film by sputtering; S133: forming a resist pattern of a reverse pattern of the circuit on the implant layer by photolithography to obtain a plating-resistant layer; S134: forming a conductor circuit by electroplating in the blank part, removing the anti-etching layer and unnecessary planting layer, and forming a first layer circuit; S135: Casting or coating liquid polyimide resin on the first layer circuit; S136: Repeat steps S132-S134 to form an FPC double-layer wiring structure, thereby obtaining a FPC bottom layer TX wiring (4) and a FPC top layer RX wiring (5).

10. The method for manufacturing a touch screen FPC according to claim 9, characterized in that: In the S133, the step of forming the anti-etching layer pattern of the reverse pattern of the circuit by the photolithography method is specifically to form the anti-etching layer pattern of the reverse pattern of the circuit by sequentially performing exposure, development, etching, and stripping.