Coating device and method for manufacturing mesh with coating film
By arranging a partition member and an independent coating liquid supply flow path in the coating device, the problems of coating width adjustment and productivity reduction in the prior art are solved, efficient coating width control and coating liquid flow management are achieved, and ensuring Improvement of coating quality and productivity.
Patent Information
- Application Number
- CN202380025049.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-15
- Filing Date
- 2023-02-07
- Publication Date
- 2024-10-22
AI Technical Summary
The existing coating device can easily cause wrinkles and reduce productivity when adjusting the coating width, and it cannot independently control the flow rate of the upstream and downstream coating liquids, affecting the coating quality.
A coating device was designed. By arranging a partition member vertically below the coating rod, and arranging containers on the upstream and downstream sides, independent coating liquid supply flow paths were formed, and the structures of the inclined surfaces and holes were used to adjust The flow rate of the coating liquid and the coating width ensure the formation of non-coated parts at the ends of the mesh and improve productivity.
It realizes the formation of non-coated parts under any coating conditions, improves the flexibility of adjusting the coating width and productivity, avoids the problems of coating liquid adhering to the coating rod and air bubbles biting in, and ensures coating quality.
Smart Images

Figure CN118829488A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a coating device and a method for producing a web with a coating film. Background Art
[0002] Conventionally, as a method for uniformly coating a coating liquid on the surface of a web such as a thermoplastic resin film being conveyed, there is a rod coating method. This method is a method in which a coating bar extending in the width direction of the web is pressed against the lower surface of the traveling web, and the coating bar is rotated by utilizing the frictional force generated between the web and the coating bar or by a driving force provided by a motor, so that the excess coating liquid previously supplied to the web is scraped off (measured).
[0003] However, in the case of coating liquid application based on the rod coating method, bubbles are trapped in the coating film when the coating liquid is scraped off, which may cause streaks and defects. The reason for this is that: under the influence of the air accompanying the moving web, air is drawn into the coating liquid when the upstream side of the coating portion begins to wet; under the influence of the air accompanying the rotating coating rod, air is drawn into the coating liquid at the gas-liquid interface near the coating rod; and so on. In response to this, as disclosed in Patent Document 1, it is generally known that there is a device structure that prevents the entrainment of air by supplying liquid to each of the upstream and downstream sides of the coating rod. For example, when the speed of the web moving from the upstream side to the downstream side is high, the entrainment of air accompanying the moving web is prevented by increasing the liquid supply from the upstream side, and when the rotation speed of the coating rod rotating in the positive direction relative to the moving web is high, the entrainment of air accompanying the rotation of the rotating coating rod is prevented by increasing the liquid supply from the downstream side. By adjusting the amount of coating liquid supplied to the upstream and downstream sides of the coating rod in accordance with the coating conditions, the air is prevented from being drawn in. In addition, the coating rod is usually cylindrical with a diameter of tens of mm and a length of hundreds to thousands of mm, so it is easy to bend due to its own weight and the force received from the net. As a method for preventing this bending, as disclosed in Patent Document 1, most of them adopt a structure in which a support body with a V-shaped or arc-shaped cross-section extending in the width direction of the coating rod contacts the coating rod from below to support it, and the structure is a structure in which the upstream and downstream sides of the coating rod are separated by the support body. By separating the upstream side and the downstream side, the coating liquid supplied from the upstream side is supplied to the upstream side of the coating rod, and the coating liquid supplied from the downstream side is supplied to the downstream side of the coating rod, and the amount of the coating liquid supplied to each can be adjusted separately, so the amount of the coating liquid can be easily adjusted for the aforementioned air entrainment.
[0004] As applicable objects of the rod coating method, there are an online coating method and an offline coating method, wherein the online coating method is a method of coating and drying a web in the process of film making by introducing the coating method in the middle of the web film-making line, and the offline coating method is a method of coating and drying a web being transported by introducing the coating method in the middle of a line having a mechanism for unwinding and a mechanism for winding the web wound into a roll shape. Among them, it is known that in the online coating method, the web, especially in a stretch film such as a PET film and a PP film, is coated before being transported to a tenter oven that heats the web while holding the ends of the web with clamps and pins and stretching the web in the width direction. In the online coating method, since the ends of the web are held with clamps, pins, etc., it is important not to apply the coating liquid to the ends to avoid affecting the holding. Furthermore, since the web width varies depending on the product, the coating device is required to have a mechanism that can appropriately adjust the width of the coating liquid (hereinafter referred to as the coating width) and the width of the non-coating liquid (hereinafter referred to as the non-coating width).
[0005] In the above-mentioned off-line coating method, there is also a case where the coating width is adjusted according to the product width so that the end portion is set to non-coating in order not to consume more coating liquid than necessary. It is important for the coating device to have a function of adjusting the coating width in order to improve productivity.
[0006] Therefore, for example, in Patent Document 2, a method is disclosed in which both ends of the net are lifted by a member or the like so as to be non-contacted with the coating device, thereby forming a non-coating width at the end. In addition, in Patent Document 3, a coating device having a structure capable of changing the width of the device in accordance with the coating width is disclosed. In addition, in Patent Document 4, a method for adjusting the width of the accumulated liquid in the container is disclosed. The method disclosed in Patent Document 4 has good operability and can freely adjust the coating width during coating, so the coating width can be changed in a manner that does not deteriorate productivity.
[0007] Prior art literature
[0008] Patent Literature
[0009] Patent Document 1: Japanese Patent Application Publication No. 2004-74147
[0010] Patent Document 2: Japanese Patent Application Publication No. 2020-961
[0011] Patent Document 3: Japanese Patent Application Publication No. 2009-160552
[0012] Patent Document 4: Japanese Patent Application Publication No. 2007-326080 Summary of the invention
[0013] Problems to be solved by the invention
[0014] However, in the method disclosed in Patent Document 2, wrinkles may sometimes be generated on the web, which may have an adverse effect on transportation. In addition, in the coating device disclosed in Patent Document 3, when switching the type of product, the coating device must be disassembled and reassembled, which will deteriorate productivity. In addition, in the method disclosed in Patent Document 4, in the sliding range of the component for changing the coating width, since the upstream container and the downstream container are connected, it is impossible to separate the upstream side and the downstream side. As a result, it is impossible to adjust the flow rate of the coating liquid supplied to the upstream side and the downstream side of the coating rod according to the coating width.
[0015] The present invention provides a coating device and a coating method which can control the flow rate of coating liquid upstream and downstream of a coating rod respectively, can form a non-coated part at the end of a web, and can adjust the coating width in a manner that does not reduce productivity.
[0016] Means for solving problems
[0017] The present invention for solving the above-mentioned problems is a coating device for applying a coating liquid to a traveling web, wherein the coating device comprises: a coating rod extending in the web width direction; a partition member arranged vertically below the coating rod and extending in the web width direction; an upstream container and a downstream container for storing the coating liquid, the upstream container and the downstream container having side plates arranged on the inner side in the web width direction compared with both ends of the partition member in the web width direction, and respectively arranged on the upstream side and the downstream side in the web conveying direction with the partition member clamped therein, the partition member being a member for separating the upstream container from the downstream container, and forming a flow path for discharging the coating liquid from a position within the web width range and on the outer side in the web width direction compared with the side plates.
[0018] The coating device of the present invention is preferably any one or more of the following (1) to (6).
[0019] (1) The flow path for discharging the coating liquid is a plane that is inclined vertically downward from a position vertically below the coating rod toward the upstream side or the downstream side in the web conveying direction.
[0020] (2) The flow channel for discharging the coating liquid is one or more grooves whose bottom surface is inclined vertically downward from a position vertically below the coating rod toward the upstream side or the downstream side in the web conveying direction.
[0021] (3) The flow path for discharging the coating liquid is one or more holes that penetrate the interior of the partition member from a position vertically below the coating rod and reach the side surface of the partition member on the upstream side or the downstream side in the web conveying direction.
[0022] (4) The side plates are slidable in the web width direction.
[0023] (5) The partition member supports the coating rod from below.
[0024] (6) Support bodies that support the coating rod from below are arranged at intervals in the web width direction.
[0025] However, the coating device of the present invention does not include a web to be coated.
[0026] In the method for manufacturing a coated web of the present invention, the coating device of the present invention is used to supply coating liquid to the upstream container and the downstream container while pressing the coating rod against the web being transported from the upstream side to the downstream side at a specified speed to apply the coating liquid to the web.
[0027] Next, the meanings of the terms in the present invention are explained.
[0028] The "web conveying direction" refers to the direction in which the web coated by the coating device is conveyed.
[0029] The "web width direction" refers to the direction of the width of the web coated by the coating device.
[0030] The term "upstream side" refers to the side that is disposed toward the direction in which the web is transported when the coating device is disposed in the web transport path.
[0031] The term "downstream side" refers to the side that is disposed toward the direction in which the web is transported when the coating device is disposed in the web transport path.
[0032] In each figure of the present application, the longitudinal direction of the coating device is set as the Y direction, the direction perpendicular to the Y direction is set as the X direction, and the direction perpendicular to the X direction and the Y direction is set as the Z direction. The X direction is equivalent to the conveying direction of the web, and the Z direction is equivalent to the up-down direction of the coating device.
[0033] Effects of the Invention
[0034] According to the coating device and method of the present invention, the coating liquid will not be discharged from the coating device and adhere to the coating rod at the outer side compared to the coating width. Therefore, a non-coated part can be formed at the end of the web under any coating conditions, and the coating width can be adjusted in a manner that does not reduce productivity. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] [ Figure 1 ] is a schematic three-dimensional diagram of the first coating device of the present invention.
[0036] [ Figure 2 ]for Figure 1 A cross-sectional view of the coating device taken along an XZ plane at a position closer to the outside than the side plate.
[0037] [ Figure 3 ]for Figure 1 Top view of the coating device.
[0038] [ Figure 4 ]for Figure 1 A schematic three-dimensional view of a coating device with a coating rod removed.
[0039] [ Figure 5 ] is a schematic three-dimensional diagram of the second coating device of the present invention.
[0040] [ Figure 6 ] is a diagram illustrating a state in which a coating liquid is supplied to the second coating device of the present invention, and the coating rod is omitted in the diagram.
[0041] [ Figure 7 ] is a cross-sectional view of the XZ plane of the conventional coating device at the outer side compared to the side plate.
[0042] [ Figure 8 ] is a diagram showing a state in which a coating liquid is supplied to a conventional rod coating device, and the coating rod is omitted in the diagram.
[0043] [ Fig. 9 ] is a schematic three-dimensional diagram of the third coating device of the present invention.
[0044] [ Fig.10 ] is a schematic three-dimensional diagram of the fourth coating device of the present invention.
[0045] [ Fig.11 ]for Fig.10 A cross-sectional view of the coating device taken along the XZ plane at a portion where the support body is present.
[0046] [ Fig.12 ]for Fig.10 A schematic three-dimensional view of a portion of a coating device where a support body is present.
[0047] [ Fig.13 ] is a cross-sectional view of the coating device in the XZ plane, illustrating the coating state when the coating liquid supplied to the upstream container is insufficient.
[0048] [ Fig.14 ] is a cross-sectional view of the coating device in the XZ plane, illustrating the coating state when the coating liquid supplied to the downstream container is insufficient.
[0049] [ Fig.15 ] is a schematic three-dimensional diagram of the coating device of Patent Document 4 with the coating rod removed. DETAILED DESCRIPTION
[0050] Hereinafter, examples of embodiments of the present invention will be described with reference to the drawings.
[0051] [First coating device]
[0052] The device configuration of the first coating device of the present invention will be described. Figure 1 is a schematic three-dimensional diagram of a first coating device, Figure 2 It is a cross-sectional view of the first coating device taken along the XZ plane, and is a cross-sectional view showing a state in which the coating liquid is discharged outwardly from the side plate in the longitudinal direction of the coating device. Figure 3 This is a plan view of the first coating device viewed from vertically above in the XY plane.
[0053] See also Figure 1 and Figure 3 The first coating device 100 includes: a coating rod 1 extending in the web width direction relative to the web 9; a partition member 2 arranged vertically below the axial center of the coating rod 1 and extending in the web width direction; an upstream main plate 3 and a downstream main plate 4 arranged in parallel on the upstream and downstream sides of the web conveying direction respectively with the partition member 2 interposed therebetween; a side plate 5 arranged on the inner side of the web width direction compared with both ends of the partition member 2 in the web width direction; a bottom plate (not shown) arranged in a manner connected to the partition member 2, the upstream main plate 3, the downstream main plate 4 and the side plate 5, and constituting an upstream container 20 and a downstream container 21 together with the partition member 2, the upstream main plate 3, the downstream main plate 4 and the side plate 5. The coating liquid 12 is supplied to the upstream container 20 and the downstream container 21 from the coating liquid supply port 10 and the coating liquid supply port 11 of the upstream container, respectively. The width L2 between the two side plates 5 is the width of the coating liquid applied to the web 9, that is, the width set as the desired coating width. The side plate 5 may be configured to be slidable in the web width direction. In this case, the sliding range of the side plate 5 becomes the adjustment range of the coating width.
[0054] See also Figure 2 and Figure 4 . Figure 4This is a schematic three-dimensional diagram of the first coating device in a state where the coating rod is removed. The partition member 2 is a plate-like member, and a V-shaped support portion 2a is formed on the side supporting the coating rod 1, and the coating rod 1 is supported by the support portion 2a. In the first coating device 100, the support portion 2a is set to be V-shaped, but it can also be an arc shape as long as it can support the coating rod 1. In addition, an inclined surface 6 is formed on the support portion 2a of the partition member 2, which discharges the coating liquid from a position within the range of the web width L1 of the web 9 as the coating object and on the outside of the web width direction compared to the side plate 5. The inclined surface 6 is formed by cutting a notch in the surface constituting the downstream side of the support portion 2a, and functions as a flow path for the coating liquid to flow out from between the coating rod 1 and the support portion 2a. The inclined surface 6 is formed in a manner that it tilts vertically downward from a position vertically below the coating rod 1 toward the downstream side of the web conveying direction. The inclined surface 6 may also be a plane that is inclined vertically downward as it moves upstream in the web conveying direction, as long as the coating liquid can be discharged from between the coating rod 1 and the partition member 2. In addition, in the present embodiment, both ends of the partition member 2 are all set as inclined surfaces, but the inclined surface 6 may be set only around the side plate 5, and the inclined surface 6 may not be formed on the end side to maintain the state of the support portion 2a.
[0055] [Coating rod]
[0056] As the coating rod 1, for example, a winding rod with a groove formed by winding a wire on the outer circumference of the rod, a rolling rod with a groove formed on the outer circumference of the rod by rolling, a small-diameter gravure roller, etc. can be used. The material of the coating rod 1 is preferably stainless steel, and SUS304 or SUS316 is particularly preferred. The surface of the coating rod 1 can also be subjected to surface treatments such as hard chrome plating. When the diameter of the coating rod 1 is too large, it is easy to produce streak-shaped coating defects along the conveying direction, which are called rib streaks. When the diameter is too small, the deflection of the coating rod 1 becomes larger, so, for example, the diameter of the coating rod is preferably 4 to 20 mm. In addition, the rotation of the coating rod is a state of so-called driven rotation in which the coating rod 1 is pressed against the net 9 and rotated by the friction force with the net 9, or it can be rotated by a driving device such as a motor. In the case of rotating it by a driving device, in order to prevent damage to the net 9, it is preferred to rotate the coating rod 1 along the conveying direction of the net 9 at a speed substantially the same as the conveying speed of the net 9. Here, "substantially the same speed" means that the coating rod 1 is rotated in such a manner that the speed difference between the peripheral speed of the coating rod 1 and the conveying speed of the web 9 is within the range of ±10%. However, depending on the use of the product, if damage to the web is not a problem, the coating rod 1 may be rotated at a speed different from the conveying speed of the web 9 and in a direction opposite to the conveying direction.
[0057] [Side panel]
[0058] In order to improve the airtightness of the container as much as possible and not to impair the sliding property, it is preferred that the gap between the side plate 5 and each component be set to 0.3 mm or less so that the coating liquid does not leak to the outside of the coating width. In addition, the material is not particularly limited, but a resin material with high sliding property is preferred. The mechanism for sliding the side plate 5 in the width direction can use a motor, a cylinder, or can be performed manually. By enabling the side plate 5 to slide without disassembling the device in advance, the coating width can be easily adjusted when switching between production varieties.
[0059] [Separation member]
[0060] The partition member 2 is provided to separate the flow paths of the coating liquid supplied to the upstream side and the downstream side relative to the web conveying direction of the coating rod 1. As long as the amount of the coating liquid supplied to the upstream side and the downstream side can be adjusted, the shape is not particularly limited, and as long as it is sufficiently close to the coating rod 1, it is not necessary to contact it, and the gap at the closest part to the coating rod is preferably less than 1 mm.
[0061] [Second coating device]
[0062] See also Figure 5 . Figure 5 It is a schematic three-dimensional diagram of the second coating device 100A of the present invention. In the second coating device 100A, four grooves 7 are provided in the support portion 2a of the partition member 2A as a flow path for discharging the coating liquid, and the bottom surface thereof is inclined vertically downward from the position vertically below the coating rod 1 toward the downstream side in the web conveying direction. At least one groove 7 is provided within the range of the web width of the partition member 2A and on the outside of the web width direction compared with the side plate 5, and it is preferably provided at both ends of the web width of the partition member 2A and on the outside of the web width direction compared with the side plate 5. The four grooves 7 are provided in the second coating device 100A to cope with the change of the web width, and more than four grooves 7 may be provided. The bottom surface of the groove 7 may also be inclined vertically downward toward the upstream side in the web conveying direction. The size of the groove 7 may be determined according to the flow rate of the coating liquid discharged. The shape of the cross section of the groove 7 in the web width direction may be rectangular, elliptical, etc., and is not particularly limited as long as the discharge function is satisfied. In the case where there is a portion where the coating rod 1 is not supported within the range of adjusting the coating width, if the adjustment range of the coating width is significantly expanded, there is a risk that the coating rod 1 will bend more at the portion and the coating quality will deteriorate. In the second coating device 100A, the partition member 2A directly contacts and supports the coating rod 1 from below over the entire coating width, so the coating rod 1 is not supported at the portion where the groove 7 is formed, but this is only a partial lack of support and will not have a significant impact on the deflection of the coating rod 1. Therefore, even within the range of adjusting the coating width, the coating quality can be stably coated without reducing it, and the range of adjusting the coating width is greatly expanded.
[0063] See also Figure 6 . Figure 6 The figure shows the state in which the coating liquid 12 is supplied to the second coating device 100A, and the coating rod 1 is omitted for illustration. The coating liquid 12 supplied from the coating liquid supply port 10 of the upstream container and the coating liquid supply port 11 of the downstream container is accumulated in the upstream container 20 and the downstream container 21, respectively, and spreads from the upper surface of the partition member 2A toward both ends in the web width direction along the support portion 2a. Since the support portion 2a of the partition member 2A has a groove 7 on the outside of the web width direction compared to the side plate 5, the coating liquid is discharged from the groove 7 to the outside of each container, and the coating liquid does not accumulate on the upper surface of the partition member 2A. Therefore, the coating rod 1 is not wetted by the coating liquid at the outside of the web width direction compared to the groove 7 from which the coating liquid is discharged, and a non-coated portion can be formed.
[0064] See also Figure 7 , Figure 8 . Figure 7 It is a cross-sectional view of the XZ plane at the width direction end of the conventional coating device 100 ′. Figure 8 This is a diagram showing a state where a coating liquid is supplied to a conventional coating device 100', and the coating rod 1 is omitted. Figure 7 As shown, in the conventional coating device 100', the support portion 2a of the partition member 2' supporting the coating rod 1 extends in the same cross section over the entire area in the web width direction. In order to support the coating rod 1, the partition member 2' needs to be in contact from below, but since the coating rod 1 is cylindrical, in the commonly used partition member 2' having a V-shaped support portion 2a, the coating liquid accumulates in the gap 13 between the coating rod 1 and the support portion 2a provided on the partition member 2'. The coating liquid spreads in the width direction along the gap 13, and the coating liquid is not discharged, so as Figure 8 As shown, the coating liquid spreads to the outside of the side plate 5, and the coating rod 1 is wetted. That is, the coating liquid is also applied to the web outside the side plate 5, and no non-coated portion is formed.
[0065] [Third coating device]
[0066] See also Fig. 9 . Fig. 9It is a schematic three-dimensional diagram of the third coating device 100B of the present invention. The third coating device 100B has four holes 8 as a flow path for discharging the coating liquid, which penetrate the interior of the partition member 2B from the position vertically below the coating rod 1 and reach the side of the downstream side of the web conveying direction of the partition member 2B. At least one hole 8 is provided within the range of the web width of the partition member 2B and on the outside of the web width direction compared with the side plate 5, and it is preferably provided at both ends of the web width of the partition member 2B and on the outside of the web width direction compared with the side plate 5. The four holes 8 are provided in the third coating device 100B to cope with the change of the web width, and more than four holes 8 may also be provided. The hole 8 may also penetrate the interior of the partition member 2B and reach the side of the upstream side of the web conveying direction of the partition member 2. The cross-sectional shape of the hole 8 is not limited to a circle, an ellipse, a rectangle, etc., and its size is determined according to the flow rate of the coating liquid used. In the coating device 100B, the partition member 2B directly contacts and supports the coating rod 1 from below, and can support the coating rod 1 even in the range where the hole 8 is formed, so that the bending of the coating rod 1 will not be aggravated, and coating can be stably performed without reducing the coating quality even in the range of adjusting the coating width.
[0067] [Fourth coating device]
[0068] See also Fig.10 , 11 、12. Fig.10 It is a schematic perspective view of a fourth coating apparatus 100C of the present invention. Fig.11 It is a cross-sectional view of the XZ plane at a portion where the support body 14 of the fourth coating apparatus 100C exists. Fig.12 2C is a schematic perspective view of the partition member 2C at the portion where the support body 14 exists. Fig.10 As shown, the fourth coating device 100C is a coating device in which the support 14 supporting the coating rod 1 from below is arranged at intervals in the web width direction, and the partition member 2C extending in the web width direction is arranged vertically below the axial center of the coating rod 1. Fig.11 As shown, in the cross section where the support 14 exists, the partition member 2 extending in the web width direction also divides the coating rod 1 into an upstream side and a downstream side vertically below the axial center of the coating rod 1. Fig.10 and Fig.11In the figure, as a flow path for discharging the coating liquid, there are shown four holes 8 which penetrate the interior of the partition member 2 from the position vertically below the coating rod 1 and reach the side surface of the partition member 2 on the downstream side in the web conveying direction at the part where the support body 14 does not exist in the web width direction, and there is a form of an inclined surface 6C which is inclined vertically downward from the position vertically below the coating rod 1 toward the downstream side in the web conveying direction. It is sufficient to set at least one hole 8 within the web width range of the partition member 2C and on the outside of the side plate 5 in the web width direction, and it is preferably set at both ends within the web width range of the partition member 2C and on the outside of the side plate 5 in the web width direction. The four holes 8 are set in the fourth coating device 100C to cope with the change of the web width, and more than four holes 8 may be set. The inclined surface 6C may not be set in the flow path, and only grooves or holes are intermittently arranged. Fig.12 The support body 14 is a roller. The outer periphery of the roller of the support body 14 contacts the coating rod 1, and the shaft 22 installed on the partition member 2C is used as the rotation axis, and the roller rotates together with the coating rod 1, thereby reducing the wear of the coating rod 1 and the support body 14. Fig.10 , Fig.11 and Fig.12 , the support based on rollers is shown, but as long as a V-shaped support body, an arc-shaped support body, or a ball that supports the coating rod 1 while rotating, etc. can support the coating rod 1, its form is not limited. In addition, regarding the material of the support body 14, in order to reduce the wear of the coating rod 1, it is preferred to use a material with a lower hardness than the coating rod 1 on the surface layer of the support body.
[0069] When the spacing of the support body 14 arranged along the length direction of the coating rod 1 is too large, the deflection of the coating rod 1 becomes larger, so it is preferably narrower. As a benchmark, it is preferably arranged in a manner that the deflection of the coating rod 1 becomes less than 10μm. The deflection amount can be calculated as follows: the reaction force of the net 9 in the outward direction calculated according to the tension borne in the traveling direction of the net 9 is used as an equidistributed load applied to the coating rod 1, the support body 14 is used as a support point, and the second moment of section and Young's modulus of the coating rod 1 are used, and the formula of material mechanics is used to calculate. In this coating device, even within the range of adjusting the coating width, the coating rod 1 is contacted and supported by the support body 14 from below, so that the deflection of the coating rod 1 can be suppressed, and the coating can be stably performed without reducing the coating quality. It should be noted that in the aforementioned first coating device 100, the support body 14 can also be set within the range of the inclined surface 6 of the partition member 2. By providing the support body 14, even within the range of the inclined surface 6, that is, within the range of adjusting the coating width, it is possible to suppress the deflection of the coating rod 1, thereby stably performing coating without reducing the coating quality.
[0070] The material of the support 14 includes metals such as iron, stainless steel, aluminum, and copper, synthetic resins such as nylon, acrylic resin, vinyl chloride resin, and tetrafluoroethylene, or rubber, etc. The support 14 may be in a plate or block shape.
[0071] [Coating method]
[0072] A method for coating a web using the first to fourth coating devices 100, 100A, 100B and 100C is described. A coating liquid 12 is supplied from the coating liquid supply port 10 of the upstream container and the coating liquid supply port 11 of the downstream container to the upstream container 20 and the downstream container 21, respectively. The coating device is raised to press the coating rod 1 against the lower surface of the web 9 from below the web 9, thereby coating the transported web 9. The angle at which the web 9 wraps around the coating rod 1 is not particularly limited, and is preferably set to be above 0 degrees and below 20 degrees. As a coating liquid supply mechanism, a gear pump, a diaphragm pump, and a Mohno pump with quantitative and low pulsation are preferably used. In addition, the coating liquid 12 ejected from the pump can also be supplied to the container via a filter and a degassing mechanism. The coating liquid supplied from the coating liquid tank to the container via the pump and the supply port circulates to the coating liquid tank via the flow path of the coating devices 100, 100A, 100B and 100C. Preferably, before starting coating, the coating liquid supply flow rate is set to be large to deliver the liquid, thereby preliminarily performing defoaming in the supply flow path and the container of the coating device. At this time, it is preferred to remove the coating rod 1, allow the coating liquid 12 to continue to flow, and confirm that the bubbles disappear from the upstream container 20 and the downstream container 21.
[0073] See also Fig.13 , 14 . Fig.13 2 is a diagram showing a situation in which the coating liquid 12 supplied to the upstream container 20 is insufficient. Fig.14 The figures are cross-sectional views of the coating device taken along the XZ plane. Fig.13 As shown in FIG. 1 , the air accompanying the web 9 reaches the coating rod 1, causing poor wetting, and the air passes between the web 9 and the coating rod 1, thereby mixing bubbles 15 into the coating film. On the other hand, when the coating liquid 12 supplied to the downstream container 21 is small, as shown in FIG. Fig.14As shown, at the downstream side of the coating rod 1, the air accompanying the rotation of the coating rod 1 will pass through between the coating rod 1 and the partition member 2, and will be generated as bubbles 15 on the upstream side of the coating rod 1, and then pass through between the net 9 and the coating rod 1, so that the bubbles 15 will be mixed into the coating film. In this way, if the bubbles 15 are mixed into the coating film, it will become a defective point in the shape of a coating missing from the bubbles. Alternatively, if the bubbles 15 continue to remain between the net 9 and the coating rod 1, it will become a streak-shaped defective point. On the contrary, when the flow rate supplied is too much, there will be problems such as an increase in foreign matter and bubbles passing through the filter. Therefore, in order to prevent the mixing of such bubbles, it is preferred to adjust the balance between the flow rate of the coating liquid 12 supplied to the upstream container 20 and the flow rate of the coating liquid 12 supplied to the downstream container 21, and set the flow rate in a manner that minimizes the flow rate and does not generate bubbles. The coating liquid 12 supplied to the upstream container 20 and the downstream container 21 is preferably adjusted according to coating conditions such as the thickness of the coating film, the conveying speed of the web 9 , and the rotation speed of the coating rod 1 .
[0074] The web to be coated by the present coating method is not particularly limited as long as it is in the form of a long sheet such as paper, film, or metal foil.
[0075] [Coating liquid]
[0076] The viscosity of the coating liquid 12 used in the coating device according to the present embodiment is preferably 0.1 Pa·s or less. When the viscosity of the coating liquid 12 is high, a ribbing phenomenon may occur, resulting in coating streaks.
[0077] The coating amount of the coating liquid 12 is preferably 100 g / m in a wet state immediately after coating. 2 Generally, in the bar coating method, the lower the coating amount, the better the coating quality, so the coating amount is more preferably 4 to 50 g / m 2 The coating amount can be adjusted by the size of the groove formed in the coating rod 1. The size of the groove can be changed by changing the wire diameter of the wound wire when the coating rod 1 is a winding rod, and can be changed by rolling with a mold having different groove depths and / or groove pitches when the coating rod 1 is a rolling rod.
[0078] Example
[0079] Next, the above-mentioned embodiment will be specifically described based on examples, but the above-mentioned embodiment is not necessarily limited to the following examples.
[0080] [Example 1]
[0081] Chips of polyethylene terephthalate (hereinafter referred to as PET) having a limiting viscosity (also called intrinsic viscosity) of 0.62 dl / g (measured in o-chlorophenol at 25°C according to JIS K7367-5 (2000 edition)) are thoroughly vacuum dried at 160°C. The vacuum-dried chips are supplied to an extruder and melted at 285°C. The molten polymer is extruded from a T-shaped die in the form of a sheet, and is wound on a mirror-finished casting drum having a surface temperature of 23°C using an electrostatic casting method, and is cooled and solidified to form an unstretched film. Next, in a longitudinal stretching machine, the unstretched film is heated with a roller group heated to 80°C, and then stretched 3.2 times in the length direction while being heated with an infrared heater, and cooled with a cooling roller adjusted to 50°C to form a uniaxially stretched resin film. The width of the resin film is 1700 mm. Next, a coating device is used. Figure 1 , 2 The first coating device 100 shown in the figure applies the coating liquid 12 on the lower surface of the resin film traveling at a speed of 200 m / min. Next, in the transverse stretching machine, the resin film coated with the coating liquid 12 is introduced into a 90°C oven for heating, and then the coating liquid 12 is dried in a 100°C oven, and the resin film is stretched 3.7 times in the width direction, and then, while performing a 5% relaxation treatment in the width direction in an oven at 220°C, the resin film is thermally fixed. In this way, a biaxially stretched film having a film formed by the coating liquid 12 on one side is obtained. The tension between the longitudinal stretching machine and the transverse stretching machine is controlled by an elastic adjustment roller so that the tension per unit width applied in the traveling direction of the resin film becomes 8000 N / m.
[0082] The coating liquid 12 is a mixed liquid obtained by adding 5 parts by mass of a melamine crosslinking agent (manufactured by Nippon Carbide Industries Co., Inc.: MW-390) and 1 part by mass of colloidal silica particles having an average particle size of 0.1 μm to 100 parts by mass of a polyester copolymer emulsion (containing components: 90 mol% of terephthalic acid, 10 mol% of sodium 5-sulfoisophthalate, and a solvent: 96 mol% of ethylene glycol, 3 mol% of neopentyl glycol, and 1 mol% of diethylene glycol). The viscosity of the coating liquid 12 is 2 mPa·s at a temperature of 25°C.
[0083] The coating liquid was pumped from Figure 1The coating liquid supply port 10 of the upstream container and the coating liquid supply port 11 of the first coating device 100 are respectively supplied to the upstream container 20 and the downstream container 21. The coating rod 1 is a coating rod (manufactured by Kano Shoji Co., Ltd.) obtained by winding a wire with a wire diameter of 0.1 mm on a stainless steel round rod material with a diameter of 12.7 mm and a length of 2000 mm. The side plate 5 is configured in a manner that the side plate interval L2 becomes 1600 mm (L3: 1000 mm).
[0084] The first coating device 100 is used to apply coating while pressing the coating rod 1 against the web 9 being conveyed and causing it to rotate. It should be noted that the coating rod 1 is supported by the V-shaped support portion 2a of the partition member 2. Figure 1 and Figure 2 As shown, in the coating adjustment width (300mm on one side), the partition member 2 is provided with an inclined surface 6 obtained by cutting off the downstream side of the V-shape. The coating results are shown in Table 1. Relative to the side plate interval L2 (1600mm), the width coated on the web is L2+8mm, and it is confirmed that the film can be formed without problems. In addition, in order to defoam the supply flow path and the container of the coating device, the coating rod 1 is disassembled once, and the coating liquid is allowed to flow continuously for 3 minutes at a supply rate of 50L / min, and then the coating rod 1 is installed again and coated, and the non-coated part can be formed without problems. The supply amount of the coating liquid without bubble bite from both the upstream and downstream sides is 10L / min on the upstream side and 27L / min on the downstream side.
[0085] [Example 2]
[0086] Use the second coating device 100A, such as Figure 5 The V-shaped support portion 2a of the partition member 2A shown supports the coating rod 1 over the entire width. In the coating adjustment width of the partition member 2A, a structure in which the V-shaped support portion 2a is intermittently dug out the shape of a groove 7 along the web width direction is applied. The width of the groove 7 is set to 10mm, the depth is set to 20mm, and the center distance between the grooves in the web width direction is set to 140mm. Except for this, the coating is carried out in the same manner as in Example 1. The results of the coating are shown in Table 1. Relative to the width L2 (1600mm) between the side plates limited by the side plates 5, the width coated on the web is L2+10mm, and it is confirmed that the film can be formed without problems. In addition, as in Example 1, after the coating liquid is allowed to flow continuously for 3 minutes at a supply rate of 50L / min, the non-coated part can still be formed by coating again. The supply rate of the coating liquid without bubble bite from both the upstream and downstream sides is 10L / min on the upstream side and 25L / min on the downstream side.
[0087] [Example 3]
[0088] Using the third coating device 100B, such as Fig. 9 The V-shaped support portion 2a of the partition member 2B shown supports the coating rod 1 over the entire width. In the coating adjustment width of the partition member 2B, a structure in which holes 8 are intermittently arranged in the V-shaped support portion 2a along the web width direction is applied. The diameter of the hole 8 is set to 8mm so that it is connected to the outside of the partition member 2B at a position 10mm downward along the Z direction. The center distance between the holes in the web width direction is set to 142mm. Except for this, the coating is carried out in the same manner as in Example 1. The results of the coating are shown in Table 1. Relative to the width L2 (1600mm) between the side plates limited by the side plates 5, the width coated on the web is L2+11mm, and it is confirmed that the film can be formed without problems. In addition, as in Example 1, after the coating liquid is allowed to flow continuously for 3 minutes at a supply amount of 50L / min, the non-coated part can still be formed by coating again. The supply amount of the coating liquid without bubble bite from both the upstream and downstream sides is 10L / min on the upstream side and 25L / min on the downstream side.
[0089] [Example 4]
[0090] Using the fourth coating device 100C, such as Fig.10 As shown, the coating rod 1 is supported by rollers (support bodies 14) intermittently arranged in the web width direction. In the coating adjustment width of the partition member 2, the following structure is applied: in the part where the support body 14 does not exist, the partition member 2 has the shape of holes 8 intermittently arranged along the web width direction, and in the part where the support body 14 exists, it has the shape of an inclined surface 6C that is inclined at 5° vertically downward from the vertically downward position of the coating rod 1 toward the downstream side of the web conveying direction. The diameter of the hole 8 is set to 8mm so that it is connected to the outside of the partition member 2B at a position 10mm downward along the Z direction. The center distance between the holes in the web width direction is set to 192mm. Except for this, the coating is carried out in the same manner as in Example 1. The results of the coating are shown in Table 1. With respect to the width L2 (1600mm) between the side plates limited by the side plates 5, the width coated on the web is L2+8mm, and it is confirmed that the film can be made without problems. In addition, similarly to Example 1, the coating liquid was allowed to flow continuously for 3 minutes at a supply rate of 50 L / min, and then the non-coating width was formed by coating again. The supply rate of the coating liquid without bubble bite from both the upstream and downstream sides was 10 L / min on the upstream side and 28 L / min on the downstream side.
[0091] [Comparative Example 1]
[0092] A partition plate with a V-shaped support portion 2a formed over the entire width was used, and a V-shaped block (without flow path) of the same cross section was also formed on the outside of the side plate. Except for this, the coating was carried out under the same conditions using the same coating device as in Example 1. The coating results are shown in Table 1. Relative to the width L2 (1600mm) between the side plates limited by the side plates, the width coated on the net exceeded L2+30mm, and the coating was applied over the entire width of the net. Then, in the transverse stretching process, the two ends of the net in the width direction were gripped with a clamp, but since there was a coating liquid between the clamp and the net, the clamp slid and fell off, and stretching could not be performed. In addition, as in Example 1, the coating liquid was allowed to flow continuously for 3 minutes at a supply rate of 50L / min, and then it was coated again, but a non-coated part could not be formed. The supply rate of the coating liquid without bubble bite from both the upstream and downstream sides was 11L / min on the upstream side and 25L / min on the downstream side.
[0093] [Comparative Example 2]
[0094] See also Fig.15 . Fig.15 The coating device described in Patent Document 4 is shown in a state where the coating rod is removed. The container 17 is formed by arranging a side plate 18 at the end of the coating device in the web width direction. A structure having a V-shaped support portion is applied to the partition member 16. The length of the partition member 16 in the web width direction is set to 1250 mm. When the coating width is adjusted to be greater than 1250 mm by sliding the side plate 18 to the outside in the web width direction, the side plate 18 at the end of the web width direction is separated from the partition member 16, and the container on the upstream side and the downstream side are connected. The coating width is adjusted to be wider using the coating device, so that the partition member 16 and the side plate 18 are separated. Except for this, the coating is carried out in the same manner as in Example 1. The coating results are shown in Table 1. With respect to the width L2 (1600 mm) between the side plates limited by the side plate 18, the width coated on the web is L2+11 mm, and it is confirmed that the film can be formed without problems. In addition, similarly to Example 1, after the coating liquid was continuously flowed at a supply rate of 50 L / min for 3 minutes, the non-coated portion was still formed by coating again. The supply rate of the coating liquid without bubble bite from both the upstream and downstream sides was 20 L / min on the upstream side and 32 L / min on the downstream side. Due to the rotation of the coating rod, the coating liquid freely moves back and forth in the container 17 connected to a large amount of coating liquid, so the supply rate of the coating liquid on the downstream and upstream sides cannot be controlled, resulting in a large amount of coating liquid being required.
[0095] The coating results in each of the examples and comparative examples were evaluated based on the following criteria.
[0096] [Controllability of coating width]
[0097] The expansion of the coating width compared to the side plate interval L2 is small, and it is better to form a non-coated part when coating is restarted. Therefore, the preferred benchmark for the expansion of the coating width is judged based on the actual coating situation of the applicant of this application in the past, and the controllability of the coating width is evaluated according to the following benchmarks.
[0098] ○ (good): The spread width of the coating liquid relative to the side plate interval L2 is +30 mm or less, and a non-coated portion can be formed when coating is resumed.
[0099] × (bad): The spread width of the coating liquid relative to the side plate interval L2 exceeds +30 mm, or a non-coated portion cannot be formed when coating is resumed.
[0100] [Controllability of coating liquid supply amount]
[0101] In order to prevent bubbles from being inserted during coating, the sum of the coating liquid supply amount on the upstream side and the coating liquid supply amount on the downstream side should be as large as possible, but this will cause the problem of increasing the capacity of the coating liquid supply pump and the problem of increasing foreign matter passing through the filter. While preventing bubbles from being inserted during coating, the sum of the coating liquid supply amount should be as small as possible. Therefore, based on the actual coating situation of the applicant of this application in the past, the controllability of the coating liquid supply amount was evaluated according to the following criteria.
[0102] ○ (good): The total supply amount of the coating liquid is 50 L / min or less.
[0103] × (bad): The total supply amount of the coating liquid exceeded 50 L / min.
[0104] [Comprehensive evaluation]
[0105] The comprehensive evaluation was conducted based on the following criteria.
[0106] ○ (good): Both the controllability of the coating width and the controllability of the coating liquid supply amount were evaluated as ○ (good).
[0107] × (poor): The controllability of the coating width and the controllability of the coating liquid supply amount were evaluated as × (poor).
[0108] [Table 1]
[0109]
[0110] Industrial Applicability
[0111] The coating device of the present invention can be used when coating a coating liquid onto a web such as a film, paper, or metal foil.
[0112] Description of Reference Numerals
[0113] 1 coating rod
[0114] 2Separator components
[0115] 2a Supporting part
[0116] 3Upstream side main board
[0117] 4 Downstream side main board
[0118] 5 side panels
[0119] 6.6C inclined surface
[0120] 7 slots
[0121] 8 holes
[0122] 9net
[0123] 10 Upstream container coating liquid supply port
[0124] 11 Downstream container coating liquid supply port
[0125] 12 coating liquid
[0126] 13 Gap between coating rod and partition member
[0127] 14 Support
[0128] 15 bubbles
[0129] 16 Supporting member
[0130] 17Coating liquid supply tank
[0131] 18 Movable side panels
[0132] 19 Supply port
[0133] 20 Upstream container
[0134] 21 Downstream container
[0135] 22 Axis
[0136] L1 network width
[0137] L2 width between side panels
[0138] L3 support width
[0139] 100, 100A, 100B, 100C, 100' coating device
Claims
1. A coating device for applying a coating liquid to a moving web, wherein: The coating device comprises: A coating rod extending in the width direction of the web; A partition member, which is arranged vertically below the axial center of the coating rod and extends in the web width direction; and an upstream container and a downstream container for storing the coating liquid, wherein the upstream container and the downstream container have side plates arranged on the inner side of the web width direction relative to both ends of the partition member in the web width direction, and are arranged on the upstream side and the downstream side in the web conveying direction respectively with the partition member interposed therebetween, The partition member is a member that partitions the upstream container from the downstream container, and forms a flow path for discharging the coating liquid from a position within the web width and outside the side plate in the web width direction.
2. The coating device according to claim 1, wherein: The flow path for discharging the coating liquid is a plane that is inclined vertically downward from a position vertically below the coating rod toward the upstream side or the downstream side in the web conveying direction.
3. The coating device according to claim 1, wherein: The flow channel for discharging the coating liquid is one or more grooves whose bottom surface is inclined vertically downward from a position vertically below the coating rod toward the upstream side or the downstream side in the web conveying direction.
4. The coating device according to claim 1, wherein: The flow path for discharging the coating liquid is one or more holes that penetrate the interior of the partition member from a position vertically below the coating rod and reach the side surface of the partition member on the upstream side or the downstream side in the web conveying direction.
5. The coating device according to any one of claims 1 to 4, wherein The side plates are slidable in the width direction of the web.
6. The coating device according to any one of claims 1 to 5, wherein The partition member supports the coating rod from below.
7. The coating device according to any one of claims 1 to 5, wherein Support bodies that support the coating rod from below are arranged at intervals in the web width direction.
8. A method for producing a coated web, wherein: The coating device according to any one of claims 1 to 7 applies the coating liquid to the web by pressing the coating rod against the web being transported from the upstream side to the downstream side at a predetermined speed while supplying the coating liquid to the upstream container and the downstream container.