Coating flash annealing equipment and operation method
By designing coating flash annealing equipment and combining vacuum and heat treatment technology, the problem of cumbersome transfer of substrates after coating in the existing technology has been solved, rapid cooling and continuous preparation of high-quality films have been achieved, and battery efficiency and product consistency have been improved. sex.
Patent Information
- Application Number
- CN202410992038.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-10-29
AI Technical Summary
The process of transferring the substrate to the flash evaporation and annealing equipment in existing coating equipment is cumbersome and time-consuming, which affects the film formation and crystallization of large-area films.
Design a coating flash annealing equipment that combines a vacuum device, a temperature control platform, a heating component and a cooling component. It realizes rapid flash evaporation and thermal annealing operations through a controller and temperature sensor, shortens the process time and improves film quality.
It realizes the continuous operation of the coating process and flash thermal annealing, reduces the time loss of the transfer process, improves the film formation quality and consistency, and improves the battery efficiency and product yield.
Smart Images

Figure CN118847460A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of battery manufacturing equipment, and in particular relates to a coating flash annealing equipment and an operating method. Background Art
[0002] Existing coating equipment (slit coating, wire rod coating or doctor blade coating) has cumbersome procedures and time-consuming process of transferring the substrate to the flash evaporation and annealing equipment after coating, and cannot cool quickly, which is not conducive to the film formation and crystallization of large-area thin films. Summary of the invention
[0003] The present invention provides a coating flash annealing device, aiming to solve at least one of the technical problems existing in the prior art.
[0004] The technical solution of the present invention is a coating flash annealing device, comprising: case; a cavity, the cavity being arranged in a space surrounded by the shell; A vacuum device, the vacuum device comprising a vacuum pump and a vacuum pipe connected in sequence, the vacuum pump being arranged outside the shell, one end of the vacuum pipe being connected to the vacuum pump, and the other end of the vacuum pipe passing through the shell to the inside of the cavity; A temperature control platform is arranged in the cavity.
[0005] Furthermore, a heating component and a cooling component are provided in the shell, the heating component is used to heat the temperature of the cavity, and the cooling component is used to reduce the temperature of the cavity.
[0006] Furthermore, a coating head is arranged on the temperature control platform.
[0007] Furthermore, it also includes a controller, which is arranged on the shell.
[0008] Furthermore, it also includes a temperature sensor and a vacuum gauge, and the temperature sensor and the vacuum gauge are arranged on the shell.
[0009] Furthermore, it also includes a flip-up cover, which is arranged on the shell and is used to add or remove materials from the cavity.
[0010] Furthermore, it also includes a visual window, which is arranged on the shell and is used to observe the cavity.
[0011] Furthermore, the present invention also provides a method for preparing a battery film layer, which is used to prepare a photovoltaic cell film layer based on the coating flash annealing equipment, and the method comprises the following steps: S1. Performing a coating operation under normal temperature and pressure, wherein the coating operation includes a combination of one or more of slit coating, wire rod coating and blade coating; S2, after the coating operation is completed, the chamber is placed in a quasi-vacuum state, and a flash evaporation operation is performed on the substrate that has undergone the coating operation; S3. After the flash evaporation operation is completed, the cavity is placed in a normal pressure state, and the temperature data in the cavity is obtained so that the temperature is 100-120 degrees Celsius. Under normal pressure, the substrate that has undergone the flash evaporation operation is annealed.
[0012] Furthermore, the present invention also provides an operating method of a coating flash annealing device, which is used to prepare a photovoltaic cell module by using the coating flash annealing device. The operating method of the coating flash annealing device comprises the following steps: S10, under normal temperature and pressure, the controller controls the coating head to perform a coating operation, wherein the coating operation includes a combination of one or more of slit coating, wire rod coating and blade coating; S20, after the coating operation is completed, the controller controls the vacuum device to work so that the cavity is in a vacuum state, and flash evaporation is performed on the substrate after the coating operation in a normal temperature vacuum environment, and the vacuum device reduces the air pressure of the cavity from the standard atmospheric pressure to below 10 Pascals within 10 seconds; S30. After the flash evaporation operation is completed, the controller controls the vacuum device to operate so that the cavity is at normal pressure. According to the temperature data in the cavity read by the temperature sensor, the controller controls the heating component or the cooling component to operate so that the temperature is 100-120 degrees Celsius. Under normal pressure, the substrate that has undergone the flash evaporation operation is annealed.
[0013] Furthermore, the present invention also provides a battery preparation method. Based on the battery film preparation method, the battery preparation method comprises the following steps: S100, placing a substrate and materials into the cavity through the removable cover, and closing the removable cover; S200, performing steps S1 to S3 in sequence, coating an electron transport layer or a hole transport layer on a conductive substrate; S300, a coating flash annealing device repeatedly performs steps S1 to S3 in sequence to prepare a perovskite active layer or an organic active layer of an organic solar cell; S400, the coating flash annealing equipment repeatedly performs steps S1 to S3 in sequence to prepare a passivation layer on the perovskite active layer or the organic active layer of the organic solar cell; S500, the coating flash annealing equipment repeatedly performs steps S1 to S3 in sequence to prepare a hole transport layer or an electron transport layer; S600, preparing electrodes by coating or evaporation to complete the preparation of photovoltaic cell modules; S700, annealing is completed, the temperature of the cavity is cooled to room temperature within 10 seconds, and the photovoltaic cell module is taken out through the removable cover.
[0014] Furthermore, if the electrode is prepared by coating, the coating flash annealing equipment repeatedly performs steps S1 to S3 in sequence to prepare a carbon electrode or a silver electrode; If the electrode is prepared by evaporation, a metal electrode is evaporated on the photovoltaic cell module, and the material of the metal electrode includes gold, silver and copper.
[0015] The beneficial effects of the present invention are as follows: In the present application, the coating flash annealing equipment effectively combines the coating process with the flash thermal annealing process, solves the cumbersome process and time consumption of transferring the substrate after coating, and realizes rapid cooling and crystallization. After the solution is coated, vacuum is quickly drawn, and then the thermal annealing and crystallization process is completed continuously at one time, which shortens the cumbersome process and time consumption of transferring the substrate after solution coating, continuously performs the flash evaporation and thermal annealing processes, reduces the harmful effects of the transfer process on the quality of large-area thin films, and can continuously prepare large-area high-quality thin films, effectively improving the film quality and consistency of thin-film batteries, thereby improving battery efficiency and product yield. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a schematic structural diagram of the coating flash annealing equipment according to the present invention.
[0017] Figure 2 It is a schematic diagram of the process of preparing the battery membrane layer according to the present invention.
[0018] Figure 3 It is a schematic diagram of a process of preparing a battery according to the present invention.
[0019] In the above figure, 100, shell; 110, heating component; 120, cooling component; 130, retractable cover; 140, visual window; 200, cavity; 300, vacuum device; 310, vacuum pump; 320, vacuum pipe; 400, temperature control platform; 410, coating head; 500, controller; 600, temperature sensor; 700, vacuum gauge. DETAILED DESCRIPTION
[0020] The following will be combined with the embodiments and drawings to clearly and completely describe the concept, specific structure and technical effects of the present invention, so as to fully understand the purpose, scheme and effect of the present invention. It should be noted that the embodiments and features in the embodiments of this application can be combined with each other without conflict.
[0021] It should be noted that, unless otherwise specified, when a feature is referred to as being "fixed" or "connected" to another feature, it may be directly fixed or connected to the other feature, or it may be indirectly fixed or connected to the other feature. In addition, the descriptions of up, down, left, right, top, bottom, etc. used in the present invention are only relative to the relative positional relationship of the components of the present invention in the drawings.
[0022] In addition, unless otherwise defined, all technical and scientific terms used herein have the same meaning as those generally understood by those skilled in the art. The terms used in this specification are only for describing specific embodiments, not for limiting the present invention. The term "and / or" used herein includes any combination of one or more related listed items.
[0023] It should be understood that, although the terms first, second, third, etc. may be used to describe various elements in the present disclosure, these elements should not be limited to these terms. These terms are only used to distinguish elements of the same type from each other. For example, without departing from the scope of the present disclosure, the first element may also be referred to as the second element, and similarly, the second element may also be referred to as the first element.
[0024] Reference Figures 1 to 3 In some embodiments, according to a coating flash annealing device of the present invention, refer to Figure 1 ,include: Housing 100; A cavity 200, wherein the cavity 200 is disposed in a space surrounded by the housing 100; A vacuum device 300, the vacuum device 300 comprises a vacuum pump 310 and a vacuum pipe 320 connected in sequence, the vacuum pump 310 is arranged outside the housing 100, one end of the vacuum pipe 320 is connected to the vacuum pump 310, and the other end of the vacuum pipe 320 passes through the housing 100 to the inside of the cavity 200; The temperature control platform 400 is disposed in the cavity 200 .
[0025] The beneficial effects of the present invention are as follows: In the present application, the coating flash annealing equipment effectively combines the coating process with the flash thermal annealing process, solving the cumbersome process and time consumption of transferring the substrate after coating. After the solution is coated, vacuum is quickly evacuated, and then the thermal annealing crystallization process is completed continuously at one time, shortening the cumbersome process and time consumption of transferring the substrate after solution coating, continuously performing the flash evaporation and thermal annealing processes, reducing the harmful effects of the transfer process on the quality of large-area thin films, and continuously preparing large-area high-quality thin films, effectively improving the film quality and consistency of thin-film batteries, thereby improving battery efficiency and product yield.
[0026] The coating flash annealing equipment is used for preparing perovskite solar cells, organic solar cells and lithium ion batteries.
[0027] Further, refer to Figure 1 A heating component 110 and a cooling component 120 are disposed in the shell 100 . The heating component 110 is used to heat the temperature of the cavity 200 , and the cooling component 120 is used to reduce the temperature of the cavity 200 .
[0028] Specifically, the controller 500 obtains the real-time temperature in the cavity 200 through the temperature sensor 600. If the real-time temperature deviates from a preset temperature range, the controller 500 controls the heating component 110 or the cooling component 120 to heat or cool the temperature of the cavity 200.
[0029] Further, refer to Figure 1 The temperature control platform 400 is provided with a coating head 410 .
[0030] Specifically, the coating pattern is at least used for coating the substrate, and the coating at least includes a combination of one or more of slit coating, wire rod coating or blade coating.
[0031] Further, refer to Figure 1 , further comprising a controller 500 , wherein the controller 500 is disposed on the housing 100 .
[0032] Specifically, the controller 500 is used to control the coating flash evaporation and annealing operations according to a preset program.
[0033] Further, refer to Figure 1 , further comprising a temperature sensor 600 and a vacuum gauge 700 , wherein the temperature sensor 600 and the vacuum gauge 700 are disposed on the housing 100 .
[0034] Specifically, the temperature sensor 600 is used to detect the real-time temperature in the cavity 200, and the vacuum gauge 700 is used to detect the real-time pressure in the cavity 200. The temperature sensor 600 and the vacuum gauge 700 are connected to the control device respectively.
[0035] Further, refer to Figure 1 , and also includes a removable cover plate 130, which is arranged on the shell 100, and the removable cover plate 130 is used to add or remove materials into or out of the cavity 200.
[0036] Further, refer to Figure 1 , further comprising a visible window 140 , wherein the visible window 140 is disposed on the housing 100 , and the visible window 140 is used to observe the cavity 200 .
[0037] Specifically, the visible window 140 is made of transparent material.
[0038] Further, refer to Figure 2 The present invention also provides a method for preparing a battery film layer, which is used to prepare a photovoltaic cell film layer based on the coating flash annealing equipment, and the method comprises the following steps: S1. Performing a coating operation under normal temperature and pressure, wherein the coating operation includes a combination of one or more of slit coating, wire rod coating and blade coating; S2, after the coating operation is completed, the chamber 200 is placed in a quasi-vacuum state, and a flash evaporation operation is performed on the substrate that has undergone the coating operation; S3. After the flash evaporation operation is completed, the chamber 200 is placed in a normal pressure state, and the temperature data in the chamber 200 is obtained so that the temperature is 100-120 degrees Celsius. Under normal pressure, the substrate that has undergone the flash evaporation operation is annealed.
[0039] Specifically, in step S2, the quasi-vacuum state is below 10 Pascals.
[0040] Furthermore, the present invention also provides an operating method of a coating flash annealing device, which is used to prepare a photovoltaic cell module by using the coating flash annealing device. The operating method of the coating flash annealing device comprises the following steps: S10, under normal temperature and pressure, the controller controls the coating head to perform a coating operation, wherein the coating operation includes a combination of one or more of slit coating, wire rod coating and blade coating; S20, after the coating operation is completed, the controller controls the vacuum device to work so that the cavity is in a vacuum state, and flash evaporation is performed on the substrate after the coating operation in a normal temperature vacuum environment, and the vacuum device reduces the air pressure of the cavity from the standard atmospheric pressure to below 10 Pascals within 10 seconds; S30. After the flash evaporation operation is completed, the controller controls the vacuum device to operate so that the cavity is at normal pressure. According to the temperature data in the cavity read by the temperature sensor, the controller controls the heating component or the cooling component to operate so that the temperature is 100-120 degrees Celsius. Under normal pressure, the substrate that has undergone the flash evaporation operation is annealed.
[0041] Further, refer to Figure 3 The present invention also proposes a battery preparation method. Based on the battery film preparation method, the battery preparation method comprises the following steps: S100, placing a substrate and materials into the cavity through the removable cover, and closing the removable cover; S200, performing steps S1 to S3 in sequence, coating an electron transport layer or a hole transport layer on a conductive substrate; S300, a coating flash annealing device repeatedly performs steps S1 to S3 in sequence to prepare a perovskite active layer or an organic active layer of an organic solar cell; S400, the coating flash annealing equipment repeatedly performs steps S1 to S3 in sequence to prepare a passivation layer on the perovskite active layer or the organic active layer of the organic solar cell; S500, the coating flash annealing equipment repeatedly performs steps S1 to S3 in sequence to prepare a hole transport layer or an electron transport layer; S600, preparing electrodes by coating or evaporation to complete the preparation of photovoltaic cell modules; S700, annealing is completed, the temperature of the cavity is cooled to room temperature within 10 seconds, and the photovoltaic cell module is taken out through the removable cover.
[0042] In some specific embodiments, in step S200, the conductive substrate is a rigid conductive substrate or a flexible conductive substrate.
[0043] In some specific embodiments, in step S700, the temperature of the cavity 200 is cooled to about 25 degrees Celsius within 10 seconds.
[0044] Further, refer to Figure 3 , the step S600 comprises: If the electrode is prepared by coating, the coating flash annealing equipment repeatedly performs steps S1 to S3 in sequence to prepare a carbon electrode or a silver electrode; If the electrode is prepared by evaporation, a metal electrode is evaporated on the photovoltaic cell module, and the material of the metal electrode includes gold, silver and copper.
[0045] The above is only a preferred embodiment of the present invention. The present invention is not limited to the above implementation. As long as the technical effect of the present invention is achieved by the same means, any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present disclosure shall be included in the scope of protection of the present disclosure. All should belong to the protection scope of the present invention. Within the protection scope of the present invention, its technical scheme and / or implementation method can have various modifications and changes.
Claims
1. A coating flash annealing device, characterized in that: include: Housing (100); a cavity (200), the cavity (200) being arranged in a space surrounded by the shell (100); A vacuum device (300), the vacuum device (300) comprising a vacuum pump (310) and a vacuum pipe (320) connected in sequence, the vacuum pump (310) being arranged outside the housing (100), one end of the vacuum pipe (320) being connected to the vacuum pump (310), and the other end of the vacuum pipe (320) passing through the housing (100) to the interior of the cavity (200); A temperature control platform (400), wherein the temperature control platform (400) is arranged in the cavity (200).
2. The coating flash annealing equipment according to claim 1, characterized in that: A heating component (110) and a cooling component (120) are arranged in the housing (100); the heating component (110) is used to heat the temperature of the cavity (200), and the cooling component (120) is used to reduce the temperature of the cavity (200).
3. The coating flash annealing equipment according to claim 1, characterized in that: The temperature control platform (400) is provided with a coating head (410).
4. The coating flash annealing equipment according to claim 1, characterized in that: It also includes a controller (500), wherein the controller (500) is arranged on the housing (100).
5. The coating flash annealing equipment according to claim 1, characterized in that: It also includes a temperature sensor (600) and a vacuum gauge (700), wherein the temperature sensor (600) and the vacuum gauge (700) are arranged on the housing (100).
6. The coating flash annealing equipment according to claim 1, characterized in that: It also comprises a removable cover plate (130), wherein the removable cover plate (130) is arranged on the shell (100), and the removable cover plate (130) is used to add or remove materials into or from the cavity (200).
7. The coating flash annealing equipment according to claim 1, characterized in that: It also includes a visible window (140), wherein the visible window (140) is arranged on the housing (100), and the visible window (140) is used to observe the cavity (200).
8. A method for preparing a battery film layer, for preparing a photovoltaic cell film layer based on the coating flash annealing equipment according to any one of claims 1 to 7, characterized in that: The method comprises the following steps: S1. Performing a coating operation under normal temperature and pressure, wherein the coating operation includes a combination of one or more of slit coating, wire rod coating and blade coating; S2, after the coating operation is completed, the chamber (200) is placed in a quasi-vacuum state, and a flash evaporation operation is performed on the substrate that has undergone the coating operation; S3. After the flash evaporation operation is completed, the cavity (200) is placed in a normal pressure state, and the temperature data in the cavity (200) is obtained so that the temperature is 100-120 degrees Celsius. In a normal pressure environment, an annealing operation is performed on the substrate that has undergone the flash evaporation operation.
9. A method for preparing a battery, characterized in that: Based on the method for preparing a battery film layer according to claim 8, the battery preparation method comprises the following steps: S100, placing a substrate and a material into the cavity (200) through the removable cover plate (130), and closing the removable cover plate (130); S200, performing steps S1 to S3 in sequence, coating an electron transport layer or a hole transport layer on a conductive substrate; S300, a coating flash annealing device repeatedly performs steps S1 to S3 in sequence to prepare a perovskite active layer or an organic active layer of an organic solar cell; S400, the coating flash annealing equipment repeatedly performs steps S1 to S3 in sequence to prepare a passivation layer on the perovskite active layer or the organic active layer of the organic solar cell; S500, the coating flash annealing equipment repeatedly performs steps S1 to S3 in sequence to prepare a hole transport layer or an electron transport layer; S600, preparing electrodes by coating or evaporation to complete the preparation of photovoltaic cell modules; S700, annealing is completed, the temperature of the cavity (200) is cooled to room temperature within 10 seconds, and the photovoltaic cell module is taken out through the removable cover plate (130).
10. The battery preparation method according to claim 9, characterized in that: The step S600 includes: If the electrode is prepared by coating, the coating flash annealing equipment repeatedly performs steps S1 to S3 in sequence to prepare a carbon electrode or a silver electrode; If the electrode is prepared by evaporation, a metal electrode is evaporated on the photovoltaic cell module, and the material of the metal electrode includes gold, silver and copper.
Citation Information
Cited By
A segmented vacuum thermal annealing process and its application in organic photovoltaic thin films
CN122766230A