A method and system for laser powder bed fusion unsupported forming of complex parts, computer equipment, and computer-readable storage medium

By calculating the redundancy value and gain stress coefficient, using the pressurization device to form a transition layer of molten material, the problem of complex parts needing support structure in laser powder bed melting manufacturing is solved, and support is achieved without support structure, reducing costs and increasing parts Surface quality.

CN118848019BActive Publication Date: 2024-11-26GUANGDONG LASERADD TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411353202.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-09-26
Publication Date
2024-11-26
Estimated Expiration
2044-09-26

AI Technical Summary

Technical Problem

In laser powder bed melt manufacturing, complex parts, especially those containing suspended structures, need to add support structures to overcome gain stress and gravity during printing, but the addition of support structures increases time and material costs, and subsequent removal of support will Affects the surface quality of the parts.

Method used

By obtaining the processing characteristic information of the laser powder bed and the characteristic information of the melted material, calculating the redundancy value and gain stress coefficient, using the pressurization device to pressurize the molten material, forming a transition layer to provide support without support, ensuring that the parts are in the printing process. There is no collapse in the middle and avoids removing the impact of support on surface quality.

Benefits of technology

It realizes effective support of complex parts without increasing printing time and material costs, avoids the impact of support structure on surface quality, and ensures the firmness and mechanical properties of the parts.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118848019B_ABST
    Figure CN118848019B_ABST
Patent Text Reader

Abstract

The present invention relates to the field of laser powder bed melting technology, and specifically discloses a laser powder bed melting unsupported forming method and system for complex parts, computer equipment, and computer-readable storage medium. The present invention obtains the height of the complex part and the bottom area of ​​the complex part according to the characteristic information of the complex part, compares the height of the laser powder bed with the height of the complex part, obtains the redundancy value of the laser powder bed, then obtains the elastic modulus of the molten material and the linear thermal expansion coefficient of the molten material according to the characteristic information of the molten material, obtains the gain stress coefficient according to the bottom area of ​​the complex part, the elastic modulus and the linear thermal expansion coefficient of the molten material, then obtains the mass of the molten material, obtains the pressure value according to the mass of the molten material and the gain stress coefficient, and pressurizes the molten material according to the pressure value based on a pressurizing device to obtain a molten material transition layer and provide unsupported structural support for the complex part.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of laser powder bed melting technology, and in particular to a laser powder bed melting unsupported forming method and system for complex parts, computer equipment, and computer-readable storage medium. Background Art

[0002] Laser Powder Bed Fusion (LPBF, sometimes also called Selective Laser Melting, SLM) is an additive manufacturing (3D printing) technology that is primarily used for the production of metal parts. This technology is widely used in industries such as aerospace, medical, automotive, molds and jewelry because it can produce metal parts with complex geometries and high mechanical properties.

[0003] In L-PBF manufacturing, complex parts, especially those with suspended structures, usually require the addition of support structures to overcome the gain stress and gravity effects during the printing process. However, the addition of support structures not only increases printing time and material costs, but the subsequent removal of supports will also affect the surface quality of the parts. Therefore, a laser powder bed fusion support-free forming method and system for complex parts is needed to solve the problem that parts need to add support structures to overcome the gain stress and gravity effects during the printing process. Summary of the invention

[0004] The object of the present invention is to provide a method and system for laser powder bed melting unsupported forming of complex parts, a computer device, and a computer-readable storage medium to solve the technical problems raised in the above-mentioned background technology.

[0005] To achieve the above object, the present invention provides the following technical solutions:

[0006] A method for laser powder bed fusion without support for complex parts, comprising:

[0007] Acquire processing feature information of the laser powder bed, wherein the processing feature information includes feature information of complex parts and feature information of molten materials;

[0008] Acquire the height of the complex part and the bottom area of ​​the complex part according to the characteristic information of the complex part, compare the height of the laser powder bed with the height of the complex part, and obtain the redundancy value of the laser powder bed;

[0009] Acquire the elastic modulus and the linear thermal expansion coefficient of the molten material according to the characteristic information of the molten material, and acquire the gain stress coefficient according to the bottom area, elastic modulus and the linear thermal expansion coefficient of the molten material of the complex part;

[0010] Acquire a molten material filling density and a molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and acquire a molten material mass according to the molten material filling density and the molten material filling volume;

[0011] Obtaining a pressure value according to the mass of the molten material and the gain stress coefficient, and pressurizing the molten material corresponding to the redundant value according to the pressure value based on a pressurizing device to obtain a molten material transition layer, wherein the pressurizing device is installed on a laser powder bed;

[0012] The complex parts are supported by a support-free structure based on the molten material transition layer.

[0013] Preferably, the step of comparing the height of the laser powder bed with the height of the complex part to obtain the redundancy value of the laser powder bed comprises:

[0014] Acquire a stacking height of the molten material on the laser powder bed, and use the stacking height as a first processing end position;

[0015] Acquire the corresponding end position coordinates according to the first processing end position, and use the end position coordinates as the coordinate origin;

[0016] The processing starting coordinates of the molten material are obtained according to the coordinate origin and the height of the complex part, and the processing starting coordinates are used as the scale starting point to extend horizontally in two opposite directions to obtain an extended horizontal line, and the extended horizontal line is used as the starting scale of the molten material to obtain the bottom starting scale of the laser powder bed, and the distance between the starting scale of the molten material and the bottom starting scale of the laser powder bed is used as the redundancy value of the laser powder bed.

[0017] Preferably, the step of obtaining the gain stress coefficient according to the bottom area of ​​the complex part, the elastic modulus and the linear thermal expansion coefficient of the molten material comprises:

[0018] Obtaining the starting temperature and ending temperature of the molten material during the melting process of the preset time;

[0019] The gain stress is obtained according to the starting temperature, the ending temperature, the bottom area of ​​the complex part, the elastic modulus and the linear thermal expansion coefficient of the molten material, wherein the calculation formula is:

[0020] ;

[0021] in, represents the gain stress, E(m) represents the elastic modulus, represents the linear thermal expansion coefficient of the molten material, represents the starting temperature, represents the end temperature, A(m) represents the bottom area of ​​the complex part;

[0022] The gain stress coefficient is calculated according to the gain stress, the starting temperature and the ending temperature, wherein the calculation formula is:

[0023] ;

[0024] in, represents the gain stress coefficient, represents the gain stress, represents the starting temperature, Indicates the end temperature.

[0025] Preferably, the step of obtaining the molten material filling density and the molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and obtaining the molten material quality according to the molten material filling density and the molten material filling volume comprises:

[0026] Obtaining surface image information filled with molten material, and extracting edges of the surface image information based on Canny edge detection to obtain edge wireframe information;

[0027] Acquiring the number of pixels in the corresponding edge wireframe according to the edge wireframe information, and mapping the number of pixels in the edge wireframe with a preset pixel number-density table to obtain the filling density of the molten material;

[0028] Acquire a first height of the corresponding molten material according to the redundant value;

[0029] The molten material filling volume is calculated based on the preset molten material filling bottom area and the first height of the molten material, wherein the shape of the molten material filling is cylindrical, and the calculation formula is:

[0030] ;

[0031] Wherein, V(t) represents the filling volume of the molten material, S(c) represents the preset bottom area of ​​the molten material filling, and H(g) represents the first height of the molten material;

[0032] The mass of the molten material is calculated according to the molten material filling density and the molten material filling volume, wherein the calculation formula is:

[0033]

[0034] Where R(m) represents the mass of molten material, represents the filling density of molten material, and V(t) represents the filling volume of molten material.

[0035] Preferably, the step of obtaining a pressure value according to the mass of the molten material and the gain stress coefficient, and pressurizing the molten material corresponding to the redundant value according to the pressure value by a pressurizing device to obtain a molten material transition layer includes:

[0036] Calculating the comprehensive gravity of the molten material corresponding to the redundant value according to the mass of the molten material, the gain stress coefficient and the preset gravity acceleration;

[0037] Acquire the radius of the bottom surface filled with the molten material based on the preset bottom area filled with the molten material, and calculate the side area filled with the molten material according to the radius of the bottom surface filled with the molten material and the first height, wherein the shape of the molten material filling is cylindrical;

[0038] Calculating a pressure value according to the side area filled by the molten material and the gravity of the molten material corresponding to the redundancy value;

[0039] Based on the pressure value, a pressurizing device pressurizes the molten material corresponding to the redundant value to obtain a pressurized molten material layer;

[0040] Obtaining the porosity corresponding to the pressurized layer of the molten material, and determining whether the porosity is equal to a preset porosity;

[0041] If the porosity is equal to the preset porosity, the pressurized layer of molten material having the preset porosity is used as the molten material transition layer;

[0042] If the porosity is not equal to the preset porosity, the molten material corresponding to the redundancy value continues to be pressurized until the porosity corresponding to the pressurized layer of the molten material is equal to the preset porosity.

[0043] Preferably, the step of providing a supporting structure-free support for a complex part based on the molten material transition layer comprises:

[0044] Acquire a corresponding first porosity according to the molten material transition layer, and acquire a bearing capacity of the molten material transition layer according to the first porosity;

[0045] Get the weight of complex parts;

[0046] Determining whether the bearing capacity of the transition layer of the molten material is greater than the weight of the complex part;

[0047] If the bearing capacity of the molten material transition layer is greater than the weight of the complex part, the weight of the complex part is supported by an unsupported structure according to the bearing capacity of the molten material transition layer.

[0048] The present application also provides a laser powder bed fusion support-free forming system for complex parts, comprising:

[0049] A first acquisition module is used to acquire processing feature information of the laser powder bed, wherein the processing feature information includes feature information of complex parts and feature information of molten materials;

[0050] A second acquisition module is used to acquire the height of the complex part and the bottom area of ​​the complex part according to the characteristic information of the complex part, compare the height of the laser powder bed with the height of the complex part, and obtain the redundancy value of the laser powder bed;

[0051] A third acquisition module is used to acquire the elastic modulus and the linear thermal expansion coefficient of the molten material according to the characteristic information of the molten material, and to acquire the gain stress coefficient according to the bottom area, elastic modulus and the linear thermal expansion coefficient of the molten material of the complex part;

[0052] A fourth acquisition module is used to acquire a molten material filling density and a molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and acquire a molten material mass according to the molten material filling density and the molten material filling volume;

[0053] a fifth acquisition module, configured to acquire a pressure value according to the mass of the molten material and the gain stress coefficient, and to pressurize the molten material corresponding to the redundant value according to the pressure value based on a pressurizing device to obtain a molten material transition layer, wherein the pressurizing device is installed on the laser powder bed;

[0054] The first support module is used to provide support structure-free support for complex parts based on the molten material transition layer.

[0055] Preferably, the second acquisition module includes:

[0056] A first acquisition unit is used to acquire a stacking height of the molten material on the laser powder bed, and use the stacking height as a first processing end position;

[0057] A second acquisition unit is used to acquire the corresponding end position coordinates according to the first processing end position, and use the end position coordinates as the coordinate origin;

[0058] The third acquisition unit is used to obtain the processing starting coordinates of the molten material according to the coordinate origin and the height of the complex part, and horizontally extend in two opposite directions with the processing starting coordinates as the scale starting point to obtain an extended horizontal line, and use the extended horizontal line as the starting scale of the molten material.

[0059] The present application also provides a computer device, including a memory and a processor, wherein the memory stores a computer program, and the processor implements the steps of the above method when executing the computer program.

[0060] The present application also provides a computer-readable storage medium on which a computer program is stored. When the computer program is executed by a processor, the steps of the above method are implemented.

[0061] The beneficial effects of the present application are as follows: the present invention first obtains processing characteristic information of the laser powder bed, wherein the processing characteristic information includes characteristic information of the complex part and characteristic information of the molten material, and obtains the height of the complex part and the bottom area of ​​the complex part according to the characteristic information of the complex part, compares the height of the laser powder bed with the height of the complex part, and obtains the redundant value of the laser powder bed, and then obtains the elastic modulus of the molten material and the linear thermal expansion coefficient of the molten material according to the characteristic information of the molten material, obtains the gain stress coefficient according to the bottom area of ​​the complex part, the elastic modulus and the linear thermal expansion coefficient of the molten material, and then obtains the molten material filling density and the molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and obtains the molten material filling density and the molten material filling volume according to the molten material filling density. The mass of the molten material is obtained according to the filling density and the filling volume of the molten material, a pressure value is obtained according to the mass of the molten material and the gain stress coefficient, and the molten material corresponding to the redundant value is pressurized according to the pressure value based on a pressurizing device to obtain a molten material transition layer, and complex parts are supported without a support structure based on the molten material transition layer. The pressurized molten material transition layer has a denser gap ratio, and therefore, the molten material with a denser gap ratio is more compact. Such a compact molten material transition layer is beneficial for supporting complex parts and will not collapse. At the same time, there is no need to add additional support structures to overcome the gain stress and gravity influence in the printing process, thereby saving printing time and material costs, and also avoiding the impact of removing the support on the surface quality of the part. BRIEF DESCRIPTION OF THE DRAWINGS

[0062] Figure 1 The figure is a schematic diagram of a method flow of an embodiment of the present application.

[0063] Figure 2 A schematic diagram of the system structure of an embodiment of the present application.

[0064] Figure 3 A schematic diagram of the internal structure of a computer device according to an embodiment of the present application.

[0065] Figure 4 This is a partial schematic diagram of a complex part and molten material according to an embodiment of the present application.

[0066] Figure 5 The figure is a schematic diagram showing the pixel number and density according to an embodiment of the present application.

[0067] The purpose, features and advantages of this application will be further described in conjunction with the embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0068] It should be understood that the specific embodiments described herein are only used to explain the present invention, and are not used to limit the present invention.

[0069] like Figure 1-3 As shown, the present application provides a laser powder bed melting unsupported forming method for complex parts, comprising:

[0070] S1. Acquire processing feature information of the laser powder bed, wherein the processing feature information includes feature information of complex parts and feature information of molten materials;

[0071] S2. Obtaining the height of the complex part and the bottom area of ​​the complex part according to the characteristic information of the complex part, comparing the height of the laser powder bed with the height of the complex part, and obtaining a redundancy value of the laser powder bed;

[0072] S3, obtaining the elastic modulus and the linear thermal expansion coefficient of the molten material according to the characteristic information of the molten material, and obtaining the gain stress coefficient according to the bottom area, elastic modulus and the linear thermal expansion coefficient of the molten material of the complex part;

[0073] S4, obtaining a molten material filling density and a molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and obtaining a molten material mass according to the molten material filling density and the molten material filling volume;

[0074] S5, obtaining a pressure value according to the mass of the molten material and the gain stress coefficient, and pressurizing the molten material corresponding to the redundant value according to the pressure value based on a pressurizing device to obtain a molten material transition layer, wherein the pressurizing device is installed on a laser powder bed;

[0075] S6. Supporting complex parts with an unsupported structure based on the molten material transition layer.

[0076] As described in the above steps S1-S6, in L-PBF manufacturing, complex parts, especially parts containing suspended structures, usually need to add support structures to overcome the gain stress and gravity effects during the printing process. However, the addition of support structures not only increases the printing time and material costs, but also the subsequent removal of the support will also affect the surface quality of the parts. On this basis, the present invention first obtains the processing feature information of the laser powder bed, wherein the processing feature information includes the feature information of the complex parts and the feature information of the molten material, so that the imaging state of the complex parts can be judged by the design properties of the complex parts themselves and the properties of the materials. The complex parts can be complex structural components in aerospace, medical, automobiles and molds, such as: turbine blades in automobiles. This scheme does not specifically refer to it. Specifically, since laser powder bed melting is to produce parts by stacking and flattening the materials and then melting them in the process of making parts, after obtaining the height of the complex parts and the bottom area of ​​the complex parts according to the feature information of the complex parts, the height of the complex parts can reflect the melting state of the complex parts during the processing. The position in the molten material can also be determined, and the position of the complex parts after processing can be determined, which can provide a basis for designing the support position after the complex parts are processed, and the bottom area of ​​the complex parts can provide a basis for calculating the bottom stress. The height of the laser powder bed is compared with the height of the complex parts to obtain the redundant value of the laser powder bed. In this way, the starting scale can better provide an effective support position for the subsequent complex parts production. At the same time, the elastic modulus of the molten material and the linear thermal expansion coefficient of the molten material are obtained according to the characteristic information of the molten material, wherein the elastic modulus is a physical quantity that measures the material's ability to resist elastic deformation. It describes the relationship between stress and strain when the material is subjected to external force within the elastic range. The linear thermal expansion coefficient is a physical quantity that measures the length change of the material with temperature changes. It describes the degree of expansion or contraction of the material when the temperature changes. The elastic modulus of the molten material and the linear thermal expansion coefficient of the molten material are molten material design parameters, for example: Material: titanium alloy (such as Ti-6Al-4V), elastic modulus: about 110 GPa (gigapascal, equivalent to 110×10 9 Pa), linear thermal expansion coefficient: about 12 × 10 -6 / °C, therefore, the elastic modulus and linear thermal expansion coefficient of different materials depend on the properties of the preset material, and the gain stress coefficient is obtained according to the bottom area of ​​the complex part, the elastic modulus and the linear thermal expansion coefficient of the molten material, wherein the gain stress is the additional thermal stress generated in the process of material processing, and the gain stress coefficient is used to estimate the gain stress size that may be generated by the material when the temperature changes, so that the stress generated by the material when it is melted can be judged by the gain stress coefficient, and stress parameters can be provided for the subsequent support of complex parts, and then the molten material filling density and the molten material filling volume below the starting scale are obtained according to the starting scale and the characteristic information of the molten material, wherein the molten material filling density and the molten material filling volume below the starting scale are usually solved according to the starting position of the part to be manufactured, the carrying capacity of the processing platform and the total filling powder, and this scheme is obtained according to the actual measuring tools, such as: digital rangefinder, etc. The digital rangefinder is installed on the laser powder bed, and the filling density of the molten material and the filling volume of the molten material are obtained according to the filling density of the molten material and the The mass of the molten material is obtained by the filling volume of the molten material, so that the mass of the molten material can provide an important basis for determining the pressure value that the pressurizing device needs to apply in the subsequent steps, and then the pressure value is obtained according to the mass of the molten material and the gain stress coefficient. In this way, the pressure value can be obtained through the mass of the molten material and the additional gain stress coefficient generated in the melting process, and then the pressurizing layer can be set for the complex parts through the pressure value. On this basis, the molten material corresponding to the redundant value is pressurized according to the pressure value based on the pressurizing device to obtain a molten material transition layer, wherein the pressurizing device is installed on the laser powder bed, so that the gap rate of the pressurized molten material transition layer is denser, and therefore, the molten material with a denser gap rate is more compact, so that the compact molten material transition layer is conducive to supporting the complex parts and will not collapse, and there is no need to overcome the gain stress and gravity influence in the printing process by adding additional support structures, thereby saving printing time and material costs, and also avoiding the influence of removing the support on the surface quality of the parts.

[0077] In one embodiment, the step S2 of comparing the height of the laser powder bed with the height of the complex part to obtain the redundancy value of the laser powder bed includes:

[0078] S201, obtaining a stacking height of the molten material on the laser powder bed, and using the stacking height as a first processing end position;

[0079] S202, acquiring corresponding end position coordinates according to the first processing end position, and using the end position coordinates as the coordinate origin;

[0080] S203. Obtain the processing starting coordinates of the molten material according to the coordinate origin and the height of the complex part, and horizontally extend in two opposite directions with the processing starting coordinates as the scale starting point to obtain an extended horizontal line, and use the extended horizontal line as the starting scale of the molten material to obtain the bottom starting scale of the laser powder bed, and use the distance between the starting scale of the molten material and the bottom starting scale of the laser powder bed as the redundancy value of the laser powder bed.

[0081] As described in the above steps S201-S203, since the height of the complex part solves the end position of the complex part, obtaining the height of the complex part is conducive to setting the support for the complex part. On this basis, the stacking height of the molten material on the laser powder bed is first obtained, and the stacking height is used as the first processing end position, so that the preset complex part to be processed can be compared with the stacking height, and then the corresponding end position coordinates are obtained according to the first processing end position, and the end position coordinates are used as the coordinate origin, and then the processing start coordinates of the molten material are obtained according to the coordinate origin and the height of the complex part, and the processing start coordinates are horizontally extended in two opposite directions with the processing start coordinates as the scale starting point to obtain an extended horizontal line (such as Figure 4 As shown, Figure 4 Only a partial structure of the laser powder bed is provided, and components such as scrapers are not presented), and the extended horizontal line is used as the starting scale of the molten material, and then the starting scale of the bottom of the laser powder bed is obtained, and the distance between the starting scale of the molten material and the starting scale of the bottom of the laser powder bed is used as the redundancy value of the laser powder bed. After determining the redundancy value of the laser powder bed, it is helpful to provide important position information for the subsequent setting of the transition layer.

[0082] In one embodiment, the step S3 of obtaining the gain stress coefficient according to the bottom area of ​​the complex part, the elastic modulus and the linear thermal expansion coefficient of the molten material comprises:

[0083] S301, obtaining the starting temperature and the ending temperature of the molten material during the melting process of the preset time;

[0084] S302, obtaining gain stress according to the starting temperature, the ending temperature, the bottom area of ​​the complex part, the elastic modulus and the linear thermal expansion coefficient of the molten material, wherein the calculation formula is:

[0085] ;

[0086] in, represents the gain stress, E(m) represents the elastic modulus, represents the linear thermal expansion coefficient of the molten material, represents the starting temperature, represents the end temperature, A(m) represents the bottom area of ​​the complex part;

[0087] S303, calculating a gain stress coefficient according to the gain stress, the starting temperature, and the ending temperature, wherein the calculation formula is:

[0088] ;

[0089] in, represents the gain stress coefficient, represents the gain stress, represents the starting temperature, Indicates the end temperature.

[0090] As described in the above steps S301-S303, since complex parts will generate gain stress during the melting process, and the gain stress will affect the support of the complex parts, on this basis, the starting temperature and the ending temperature of the molten material during the melting process of the preset time are first obtained, and the gain stress is obtained according to the starting temperature, the ending temperature, the bottom area of ​​the complex part, the elastic modulus and the linear thermal expansion coefficient of the molten material. The specific calculation steps are: starting temperature = 20 °C, ending temperature = 1000 °C, elastic modulus = 110×10 9 Pa, linear thermal expansion coefficient of molten material = 12 × 10 -6 / °C, complex parts bottom area = 3cm 2 , gain stress Then, the gain stress coefficient is calculated according to the gain stress, the starting temperature and the ending temperature. The specific calculation steps are: gain stress coefficient In this way, after obtaining the gain stress coefficient, the influence of gain stress on the support of complex parts can be judged, thereby providing a basis for the design of the subsequent molten material transition layer.

[0091] In one embodiment, the step S4 of obtaining the molten material filling density and the molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and obtaining the molten material quality according to the molten material filling density and the molten material filling volume includes:

[0092] S401, the step of obtaining the molten material filling density and the molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and obtaining the molten material quality according to the molten material filling density and the molten material filling volume, comprises:

[0093] S402, obtaining surface image information filled with molten material, and performing edge extraction on the surface image information based on Canny edge detection to obtain edge wireframe information;

[0094] S403, acquiring the number of pixels in the corresponding edge wireframe according to the edge wireframe information, and mapping the number of pixels in the edge wireframe with a preset pixel number-density table to obtain the filling density of the molten material;

[0095] S404, obtaining a first height of the corresponding molten material according to the redundant value;

[0096] S405, calculating the molten material filling volume based on the preset molten material filling bottom area and the first height of the molten material, wherein the shape of the molten material filling is cylindrical, and the calculation formula is:

[0097] ;

[0098] Wherein, V(t) represents the filling volume of the molten material, S(c) represents the preset bottom area of ​​the molten material filling, and H(g) represents the first height of the molten material;

[0099] S406, calculating the mass of the molten material according to the molten material filling density and the molten material filling volume, wherein the calculation formula is:

[0100] ;

[0101] Where R(m) represents the mass of molten material, represents the filling density of molten material, and V(t) represents the filling volume of molten material.

[0102] As described in the above steps S401-S406, since the quality of the molten material is related to the bearing of complex parts, the molten material transition layer can be further designed after the quality of the molten material is calculated. On this basis, the surface image information filled with the molten material is first obtained, and the edge of the surface image information is extracted based on the Canny edge detection to obtain the edge wireframe information. In this way, the surface condition of the molten material filling can be determined through the edge wireframe information, and then the surface image information obtains the corresponding pixels in the edge wireframe according to the edge wireframe information, and then the pixels in the edge wireframe are compared with the preset pixel number-density table (such as Figure 5The molten material filling density is obtained by mapping, and then the first height of the corresponding molten material is obtained according to the redundant value, and then the molten material filling volume is calculated based on the preset molten material filling bottom area and the first height of the molten material, wherein the shape of the molten material filling is cylindrical, so the calculated molten material filling volume provides an important basis for the subsequent calculation of the molten material mass, and then the molten material mass is calculated according to the molten material filling density and the molten material filling volume, and the specific molten material gravity can be obtained through the molten material mass. Therefore, the pressure applied to the molten material can be designed through the molten material gravity, thereby facilitating the design of the molten material transition layer to support complex parts without support structures.

[0103] In one embodiment, the step S5 of obtaining a pressure value according to the mass of the molten material and the gain stress coefficient, and pressurizing the molten material corresponding to the redundant value according to the pressure value by a pressurizing device to obtain a molten material transition layer includes:

[0104] S501, calculating the comprehensive gravity of the molten material corresponding to the redundant value according to the mass of the molten material, the gain stress coefficient and the preset gravity acceleration, wherein the calculation formula is:

[0105] ;

[0106] Where, F(m) represents the comprehensive gravity, R(m) represents the mass of the molten material, and g represents the preset gravitational acceleration. represents the gain stress coefficient;

[0107] S502, based on the preset molten material filling bottom area, the radius of the molten material filling bottom surface is obtained, and the lateral area of ​​the molten material filling is calculated according to the radius of the molten material filling bottom surface and the first height, wherein the shape of the molten material filling is cylindrical, and the calculation formula is:

[0108] ;

[0109] in, represents the lateral area filled by the molten material, represents pi, r represents the radius of the bottom surface filled by the molten material, and H (g) represents the first height;

[0110] S503, calculating a pressure value according to the side area filled by the molten material and the gravity of the molten material corresponding to the redundancy value, wherein the calculation formula is:

[0111] ;

[0112] Among them, P represents the pressure value, F (m) represents the comprehensive gravity, It represents the lateral area filled by the molten material;

[0113] S504, pressurizing the molten material corresponding to the redundant value according to the pressure value by a pressurizing device to obtain a pressurized molten material layer;

[0114] S505, obtaining the porosity corresponding to the pressurized layer of the molten material, and determining whether the porosity is equal to a preset porosity;

[0115] If the porosity is equal to the preset porosity, the pressurized layer of molten material having the preset porosity is used as the molten material transition layer;

[0116] If the porosity is not equal to the preset porosity, the molten material corresponding to the redundancy value continues to be pressurized until the porosity corresponding to the pressurized layer of the molten material is equal to the preset porosity.

[0117] As described in the above steps S501-S505, the present invention calculates the comprehensive gravity of the molten material corresponding to the redundant value according to the mass of the molten material, the gain stress coefficient and the preset gravity acceleration, for example: the mass of the molten material = 1000kg, the preset gravity acceleration = 9.18m / s 2 , gain stress coefficient = 3.96×10 9 Pa / ℃, where 1Pa=1N / m 2 , comprehensive gravity , where the comprehensive gravity is the additional gravity affected by the molten material's own gravity plus the gain stress coefficient. The gain stress coefficient in this solution refers to the coefficient affected by the thermal stress generated by the melting process. Then, based on the preset molten material filling bottom area, the radius of the molten material filling bottom surface is obtained. The lateral area filled by the molten material is calculated according to the radius of the molten material filling bottom surface and the first height. For example, pi = 3.14, the radius of the molten material filling bottom surface = 0.5m, the first height = 0.1m, and the lateral area filled by the molten material = 2*3.14*0.5*0.1=0.314m 2 , and then calculate the pressure value according to the side area filled by the molten material and the gravity of the molten material corresponding to the redundancy value, for example: pressure value , then based on the pressurizing device, the molten material corresponding to the redundant value is pressurized according to the pressure value to obtain a pressurized layer of the molten material, and then the porosity corresponding to the pressurized layer of the molten material is obtained, and it is determined whether the porosity is equal to the preset porosity. If the porosity is equal to the preset porosity, the pressurized layer of the molten material with the preset porosity is used as the molten material transition layer. If the porosity is not equal to the preset porosity, the molten material corresponding to the redundant value continues to be pressurized until the porosity corresponding to the pressurized layer of the molten material is equal to the preset porosity. In this way, the porosity of the pressurized layer of the molten material is made smaller by pressurization, and then the pressurized layer of the molten material can support complex parts when the porosity is smaller. At the same time, the small porosity will make the transition layer of the molten material more compact, and the compact transition layer of the molten material is conducive to supporting complex parts without collapse. At the same time, there is no need to add additional support structures to overcome the gain stress and gravity influence during the printing process, thereby saving printing time and material costs, and avoiding the impact of removing the support on the surface quality of the part.

[0118] In one embodiment, the step S6 of providing support for the complex part without a support structure based on the molten material transition layer comprises:

[0119] S601, obtaining a corresponding first porosity according to the molten material transition layer, and obtaining a bearing capacity of the molten material transition layer according to the first porosity;

[0120] S602, obtaining the weight of the complex part;

[0121] S603, determining whether the bearing capacity of the transition layer of the molten material is greater than the weight of the complex part;

[0122] If the bearing capacity of the molten material transition layer is greater than the weight of the complex part, the weight of the complex part is supported by an unsupported structure according to the bearing capacity of the molten material transition layer.

[0123] As described in the above steps S601-S603, the present invention first obtains the corresponding first porosity according to the molten material transition layer, and obtains the bearing capacity of the molten material transition layer according to the first porosity, for example: the first porosity = 20%, the mass of the molten material = 1000kg, the weight of the complex part = 5kg, wherein the weight of the complex part is obtained based on an electronic scale, wherein the electronic scale is installed on the laser powder bed, and the density of the molten material is 4500kg / m 3 , the bearing capacity of the molten material transition layer = (1-first porosity) * weight of complex parts * density of molten material , 18000N=1832kg, therefore, 1832kg is greater than the weight of the complex part by 5kg, and then the weight of the complex part is supported without a support structure according to the bearing capacity of the molten material transition layer, and at the same time, there is no need to add additional support structures to overcome the gain stress and gravity influence during the printing process, thereby saving printing time and material costs, and also avoiding the impact of removing the support on the surface quality of the part.

[0124] The present application also provides a laser powder bed fusion support-free forming system for complex parts, comprising:

[0125] The first acquisition module 1 is used to acquire processing feature information of the laser powder bed, wherein the processing feature information includes feature information of complex parts and feature information of molten materials;

[0126] The second acquisition module 2 is used to obtain the height of the complex part and the bottom area of ​​the complex part according to the characteristic information of the complex part, compare the height of the laser powder bed with the height of the complex part, and obtain the redundancy value of the laser powder bed;

[0127] The third acquisition module 3 is used to acquire the elastic modulus and the linear thermal expansion coefficient of the molten material according to the characteristic information of the molten material, and acquire the gain stress coefficient according to the bottom area, elastic modulus and the linear thermal expansion coefficient of the molten material of the complex part;

[0128] A fourth acquisition module 4 is used to acquire a molten material filling density and a molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and acquire a molten material mass according to the molten material filling density and the molten material filling volume;

[0129] A fifth acquisition module 5 is used to obtain a pressure value according to the mass of the molten material and the gain stress coefficient, and to pressurize the molten material corresponding to the redundant value according to the pressure value based on a pressurizing device to obtain a molten material transition layer, wherein the pressurizing device is installed on the laser powder bed;

[0130] The first support module 6 is used to provide support for the complex parts without supporting structure based on the molten material transition layer.

[0131] In one embodiment, the second acquisition module includes:

[0132] A first acquisition unit is used to acquire a stacking height of the molten material on the laser powder bed, and use the stacking height as a first processing end position;

[0133] A second acquisition unit is used to acquire the corresponding end position coordinates according to the first processing end position, and use the end position coordinates as the coordinate origin;

[0134] The third acquisition unit is used to obtain the processing starting coordinates of the molten material according to the coordinate origin and the height of the complex part, and horizontally extend in two opposite directions with the processing starting coordinates as the scale starting point to obtain an extended horizontal line, and use the extended horizontal line as the starting scale of the molten material.

[0135] The present invention also provides a computer-readable storage medium having a computer program stored thereon, and when the computer program is executed by a processor, the steps of the above-mentioned laser powder bed fusion unsupported forming method for complex parts are implemented.

[0136] Those of ordinary skill in the art can understand that all or part of the processes in the above-mentioned embodiment methods can be completed by instructing the relevant hardware through a computer program, and the computer program can be stored in a non-volatile computer-readable storage medium. When the computer program is executed, it can include the processes of the embodiments of the above-mentioned methods. Among them, any reference to memory, storage, database or other media provided in this application and used in the embodiments may include non-volatile and / or volatile memory. Non-volatile memory may include read-only memory (ROM), programmable ROM (PROM), electrically programmable ROM (EPROM), electrically erasable programmable ROM (EEPROM) or flash memory. Volatile memory may include random access memory (RAM) or external cache memory. By way of illustration and not limitation, RAM is available in many forms, such as static RAM (SRAM), dynamic RAM (DRAM), synchronous DRAM (SDRAM), double data rate SDRAM (SSRSDRAM), enhanced SDRAM (ESDRAM), synchronous link (Synchlink) DRAM (SLDRAM), memory bus (Rambus) direct RAM (RDRAM), direct memory bus dynamic RAM (DRDRAM), and memory bus dynamic RAM (RDRAM), etc.

[0137] It should be noted that, in this article, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, device, article or method including a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, device, article or method. In the absence of further restrictions, an element defined by the sentence "includes a ..." does not exclude the presence of other identical elements in the process, device, article or method including the element.

[0138] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made by using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the protection scope of this application.

Claims

1. A method for laser powder bed melting of complex parts without support, characterized in that: include: Acquire processing feature information of the laser powder bed, wherein the processing feature information includes feature information of complex parts and feature information of molten materials; Acquire the height of the complex part and the bottom area of ​​the complex part according to the characteristic information of the complex part; Obtaining the height of the laser powder bed, and comparing the height of the laser powder bed with the height of the complex part to obtain a redundancy value of the laser powder bed, wherein the height of the laser powder bed is greater than the height of the complex part; Acquire a stacking height of the molten material on the laser powder bed, and use the stacking height as a first processing end position; Acquire the corresponding end position coordinates according to the first processing end position, and use the end position coordinates as the coordinate origin; The processing starting coordinates of the molten material are obtained according to the coordinate origin and the height of the complex part, and the processing starting coordinates are used as the scale starting point to horizontally extend in two opposite directions to obtain an extended horizontal line, and the extended horizontal line is used as the starting scale of the molten material to obtain the bottom starting scale of the laser powder bed, and the distance between the starting scale of the molten material and the bottom starting scale of the laser powder bed is used as the redundancy value of the laser powder bed; Acquire the elastic modulus and the linear thermal expansion coefficient of the molten material according to the characteristic information of the molten material, and acquire the gain stress coefficient according to the bottom area, elastic modulus and the linear thermal expansion coefficient of the molten material of the complex part; Obtaining the starting temperature and ending temperature of the molten material during the melting process of the preset time; The gain stress is obtained according to the starting temperature, the ending temperature, the bottom area of ​​the complex part, the elastic modulus and the linear thermal expansion coefficient of the molten material, wherein the calculation formula is: ; Wherein, σ(r) represents the gain stress, E(m) represents the elastic modulus, α(p) represents the linear thermal expansion coefficient of the molten material, ΔT1 represents the starting temperature, ΔT2 represents the ending temperature, and A(m) represents the bottom area of ​​the complex part; The gain stress coefficient is calculated according to the gain stress, the starting temperature and the ending temperature, wherein the calculation formula is: ; Among them, K thermal represents the gain stress coefficient, σ(r) represents the gain stress, ΔT1 represents the starting temperature, and ΔT2 represents the ending temperature; Acquire a molten material filling density and a molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and acquire a molten material mass according to the molten material filling density and the molten material filling volume; Obtaining the surface image information filled with molten material, and extracting the edge of the surface image information based on Canny edge detection to obtain edge wireframe information; Acquiring the number of pixels in the corresponding edge wireframe according to the edge wireframe information, and mapping the number of pixels in the edge wireframe with a preset pixel number-density table to obtain the filling density of the molten material; Acquire a first height of the corresponding molten material according to the redundant value; Calculating a molten material filling volume based on a preset molten material filling bottom area and a first height of the molten material, wherein the molten material filling has a cylindrical shape; Calculating the mass of the molten material according to the molten material filling density and the molten material filling volume; Obtaining a pressure value according to the mass of the molten material and the gain stress coefficient, and pressurizing the molten material corresponding to the redundant value according to the pressure value based on a pressurizing device to obtain a molten material transition layer, wherein the pressurizing device is installed on a laser powder bed; Calculating the comprehensive gravity of the molten material corresponding to the redundant value according to the mass of the molten material, the gain stress coefficient and the preset gravity acceleration; Acquire the radius of the bottom surface filled with the molten material based on the preset bottom area filled with the molten material, and calculate the side area filled with the molten material according to the radius of the bottom surface filled with the molten material and the first height, wherein the shape of the molten material filling is cylindrical; Calculating a pressure value according to the side area filled by the molten material and the gravity of the molten material corresponding to the redundancy value; Based on the pressure value, a pressurizing device pressurizes the molten material corresponding to the redundant value to obtain a pressurized molten material layer; Obtaining the porosity corresponding to the pressurized layer of the molten material, and determining whether the porosity is equal to a preset porosity; If the porosity is equal to the preset porosity, the pressurized layer of molten material having the preset porosity is used as the molten material transition layer; If the porosity is not equal to the preset porosity, the molten material corresponding to the redundancy value continues to be pressurized until the porosity corresponding to the pressurized layer of the molten material is equal to the preset porosity; The complex parts are supported by a support-free structure based on the molten material transition layer.

2. The method for laser powder bed melting of complex parts without support according to claim 1 is characterized in that: The step of providing a complex part with a support-free structure based on the molten material transition layer comprises: Acquire a corresponding first porosity according to the molten material transition layer, and acquire a bearing capacity of the molten material transition layer according to the first porosity; Get the weight of complex parts; Determining whether the bearing capacity of the molten material transition layer is greater than the weight of the complex part; If the bearing capacity of the molten material transition layer is greater than the weight of the complex part, the weight of the complex part is supported by an unsupported structure according to the bearing capacity of the molten material transition layer.

3. A laser powder bed fusion unsupported forming system for complex parts, used to perform the laser powder bed fusion unsupported forming method for complex parts as described in any one of claims 1-2, characterized in that: include: A first acquisition module is used to acquire processing feature information of the laser powder bed, wherein the processing feature information includes feature information of complex parts and feature information of molten materials; A second acquisition module is used to acquire the height of the complex part and the bottom area of ​​the complex part according to the characteristic information of the complex part, compare the height of the laser powder bed with the height of the complex part, and obtain the redundancy value of the laser powder bed; A third acquisition module is used to acquire the elastic modulus and the linear thermal expansion coefficient of the molten material according to the characteristic information of the molten material, and to acquire the gain stress coefficient according to the bottom area, elastic modulus and the linear thermal expansion coefficient of the molten material of the complex part; A fourth acquisition module is used to acquire a molten material filling density and a molten material filling volume corresponding to the redundant value according to the redundant value and the molten material characteristic information, and acquire a molten material mass according to the molten material filling density and the molten material filling volume; a fifth acquisition module, configured to acquire a pressure value according to the mass of the molten material and the gain stress coefficient, and to pressurize the molten material corresponding to the redundant value according to the pressure value based on a pressurizing device to obtain a molten material transition layer, wherein the pressurizing device is installed on the laser powder bed; The first support module is used to provide support structure-free support for complex parts based on the molten material transition layer.

4. The laser powder bed fusion unsupported forming system for complex parts according to claim 3 is characterized in that: The second acquisition module includes: A first acquisition unit is used to acquire a stacking height of the molten material on the laser powder bed, and use the stacking height as a first processing end position; A second acquisition unit is used to acquire the corresponding end position coordinates according to the first processing end position, and use the end position coordinates as the coordinate origin; The third acquisition unit is used to obtain the processing starting coordinates of the molten material according to the coordinate origin and the height of the complex part, and horizontally extend in two opposite directions with the processing starting coordinates as the scale starting point to obtain an extended horizontal line, and use the extended horizontal line as the starting scale of the molten material to obtain the bottom starting scale of the laser powder bed, and use the distance between the starting scale of the molten material and the bottom starting scale of the laser powder bed as the redundant value of the laser powder bed.

5. A computer device comprising a memory and a processor, wherein the memory stores a computer program, wherein: When the processor executes the computer program, the steps of the method according to any one of claims 1 to 2 are implemented.

6. A computer-readable storage medium having a computer program stored thereon, characterized in that: When the computer program is executed by a processor, the steps of the method according to any one of claims 1 to 2 are implemented.