Method for reducing unmelted particles on inner surface of quartz crucible
By using a high-temperature and durable adsorption device to remove impurities from unmelted particles during the quartz crucible manufacturing process, the problem of unmelted particles embedded on the inner surface of the quartz crucible is solved, and the crystallization rate and product quality are improved.
Patent Information
- Application Number
- CN202310467340.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-04-27
- Publication Date
- 2024-10-29
AI Technical Summary
During the quartz crucible manufacturing process, the upper edge temperature of the quartz crucible is relatively low, resulting in unmelted quartz microparticles embedded in the inner surface, increasing the risk of heterogeneous nucleation of single crystals and affecting the crystallization rate.
During the second melting process and cooling process, a high-temperature and durable adsorption device is used to remove impurities from the unmelted particles on the inner surface of the quartz crucible. The adsorption device set above the mold is combined with a vacuum pump for adsorption to ensure effective collection of unmelted particles in a high-temperature environment. melt particles.
It significantly reduces the risk of embedded particles on the inner surface of the quartz crucible, reduces the risk of heterogeneous nucleation of single crystals, and improves the crystallization rate and quality.
Smart Images

Figure CN118851547A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of quartz crucible manufacturing, and in particular relates to a method for reducing unmelted particles on the inner surface of a quartz crucible. Background Art
[0002] In the manufacturing process of the existing quartz crucible for crystal pulling, the quartz crucible is formed into a finished product style at one time, leaving only a margin in height. After melting, the reserved height above is cut to meet the requirements of the specified height. Since the height of the quartz crucible mold is higher than the height of the finished product, the quartz raw sand can be normally formed at the above reserved place, but the position of the electrode column is relatively fixed. During the manufacturing process of the quartz crucible, the demand for heat in the middle and lower parts is higher than that in the upper part, and the highest temperature area of the electrode column cannot rise to the upper edge of the crucible, otherwise it will cause a lot of heat energy waste and affect the melting effect of the bottom of the crucible. Therefore, during the melting process of the crucible, the temperature of the upper edge of the quartz crucible is lower than that of the middle and lower parts, and there are a large number of unmelted quartz microparticles. During the melting process of the crucible, there is a risk that the unmelted quartz microparticles will fall on the inner surface of the crucible, resulting in the quartz microparticles being embedded in the inner wall surface of the quartz crucible. During the process of pulling single crystals, the microparticles embedded on the inner surface are at risk of falling off, which increases the risk of heterogeneous nucleation of silicon single crystals, resulting in single crystal breakage and affecting the crystallization rate. Summary of the invention
[0003] To solve the above technical problems, the present invention provides a method for reducing unmelted particles on the inner surface of a quartz crucible, which effectively solves the problem of heterogeneous nucleation of single crystals caused by the falling of unmelted particles on the inner surface of the quartz crucible, and overcomes the shortcomings of the prior art.
[0004] The technical solution adopted by the present invention is: a method for reducing unmelted particles on the inner surface of a quartz crucible, comprising: a first melting process, a second melting process, a cooling process and a demolding process, in which a process of removing impurities from the unmelted particles on the inner surface of the quartz crucible is performed during the second melting process and the cooling process.
[0005] Furthermore, the impurity removal process includes using an adsorption device to adsorb the unmelted particles.
[0006] Furthermore, the adsorption device is continuously arranged above the mold of the quartz crucible.
[0007] Furthermore, the adsorption device is intermittently arranged above the mold of the quartz crucible.
[0008] Furthermore, the adsorption device is connected to a vacuum pump.
[0009] Furthermore, the operating temperature of the adsorption device is above 1700°C.
[0010] Furthermore, the temperature of the inner surface of the quartz crucible during the second melting process is higher than the temperature of the inner surface of the quartz crucible during the first melting process, and the temperature of the inner surface of the quartz crucible during the demolding process is lower than the temperature of the inner surface of the quartz crucible during the cooling process.
[0011] Furthermore, during the first melting process and the second melting process, the electrode column is turned on.
[0012] Furthermore, during the cooling process and the demoulding process, the electrode column is closed.
[0013] Furthermore, the time consumption ratio of the first melting process, the second melting process, the cooling process and the demoulding process is 7-10:1-3:2-3:2-4.
[0014] The advantages and positive effects of the present invention are as follows: due to the adoption of the above technical scheme, unmelted particles are prevented from being embedded in the inner surface of the quartz crucible during the melting process of the quartz crucible, the risk of single crystal heterogeneous nucleation caused by the falling off of unmelted particles during the use of the quartz crucible is reduced, the crystal quality is improved, and the crystal rate is increased. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 The present invention is a schematic diagram of a method for reducing unmelted particles on the inner surface of a quartz crucible according to an embodiment of the present invention.
[0016] In the figure:
[0017] 1. Quartz crucible 2. Mold 3. Adsorption device DETAILED DESCRIPTION
[0018] An embodiment of the present invention provides a method for reducing unmelted particles on the inner surface of a quartz crucible. The embodiment of the present invention is described below with reference to the accompanying drawings.
[0019] In the description of the embodiments of the present invention, it should be understood that the orientation or positional relationship indicated by the terms "top", "bottom", etc. is based on the orientation or positional relationship shown in the accompanying drawings, and is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "set" and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected, or indirectly connected through an intermediate medium, or it can be a connection between the two elements. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood through specific circumstances.
[0020] like Figure 1As shown, a method for reducing unmelted particles on the inner surface of a quartz crucible according to an embodiment of the present invention includes: a first melting process, a second melting process, a cooling process, and a demolding process. In the second melting process and the cooling process, in order to prevent unmelted quartz particles on the upper edge of the quartz crucible 1 from entering the inner surface of the quartz crucible 1 and affecting the subsequent single crystal pulling, a de-impurity process is performed on the unmelted particles on the inner surface of the quartz crucible 1. Since the temperature in the middle and late stages of melting, i.e., the second melting process, is relatively high, some of the unmelted particles that enter the inner surface of the quartz crucible 1 in the early and middle stages of melting the quartz crucible 1, i.e., the first melting process, will be directly melted in the second melting process. Therefore, there is no need to perform a de-impurity process in the first melting process. In the demolding process, the temperature of the inner surface of the quartz crucible 1 is relatively low. Even if unmelted quartz particles enter the inner surface of the quartz crucible 1, they cannot be embedded in the inner surface of the quartz crucible 1. They can be removed in the subsequent cleaning process. Therefore, there is no need to perform a de-impurity process in the demolding process.
[0021] Specifically, the impurity removal process includes adsorbing the unmelted particles using an adsorption device 3. The adsorption device 3 is arranged above the quartz crucible 1. The adsorption device 3 can be arranged continuously along the upper edge of the mold 2, or can be arranged discontinuously and distributedly along the upper edge of the mold 2. In order to ensure the adsorption effect, the discontinuous and distributed arrangement should be evenly distributed.
[0022] The adsorption device 3 is connected to a vacuum pump and connected through a pipeline to collect unmelted particles to avoid environmental pollution. Since the quartz crucible 1 is in a high temperature environment during the manufacturing process, the adsorption device 3 needs to be resistant to high temperatures. The operating temperature of the adsorption device 3 needs to be above 1700°C, and the material of the adsorption device 3 needs to be resistant to high temperatures, and ceramic material can be used.
[0023] The surface temperature t of the quartz crucible 1 is 100°C < t < 1000°C in the first melting process, 1000°C ≤ t ≤ 1700°C in the second melting process, 1700°C < t ≤ 1400°C in the cooling process, and 1400°C < t < 800°C in the demoulding process. The temperature of the inner surface of the quartz crucible 1 in the second melting process is higher than the temperature of the inner surface of the quartz crucible 1 in the first melting process, and the temperature of the inner surface of the quartz crucible 1 in the demoulding process is lower than the temperature of the inner surface of the quartz crucible 1 in the cooling process.
[0024] In the first melting process and the second melting process, the electrode column is opened to melt the quartz particles. After the quartz crucible 1 is melted and formed, the electrode column is closed during the cooling process and the demoulding process.
[0025] The time consumption ratio of the first melting process, the second melting process, the cooling process and the demoulding process is 7-10:1-3:2-3:2-4.
[0026] Embodiment: A method for reducing unmelted particles on the inner surface of a quartz crucible, wherein quartz particles are placed in a stone mold 2 for melting, including a first melting process, a second melting process, a cooling process, and a demolding process, with a time ratio of 9:1:2:3. In the first melting process, i.e., the early and middle stages of melting, the electrode column is powered on and turned on, the temperature of the inner surface of the crucible is 100°C < t < 1000°C, and the first melting process takes 900s. In the second melting process, i.e., the late stage of melting, the electrode column is continuously powered on and turned on, the temperature of the inner surface of the crucible is 1000°C ≤ t ≤ 1700°C, a de-impurity process is performed, the adsorption device 3 is turned on, and the unmelted particles are adsorbed, and the second melting process takes 100s. In the cooling process, the electrode column is powered off and turned off, the temperature of the inner surface of the crucible is 1700°C < t ≤ 1400°C, the de-impurity process is continuously performed, the adsorption device 3 is continuously turned on, and the unmelted particles are continuously adsorbed, and the cooling process takes 200s. During the demoulding process, the electrode column is powered off and closed, the adsorption device 3 is closed, the inner surface temperature of the crucible is 1400°C<t<800°C, and the demoulding process takes 300s. In this embodiment, the upper edge of the quartz crucible 1 is circular. To ensure the adsorption effect, the adsorption device 3 is continuously arranged along the upper edge of the mold 2 in an annular shape and is made of a ceramic material with a high temperature resistance of more than 1700°C.
[0027] The opening status of the adsorption device during the melting process of the quartz crucible is shown in the following table:
[0028] Time / s process Electrode column status Crucible inner surface temperature / t Adsorption device opening status 0-900 First Melting Power on 100℃<t<1000℃ closure 900-1000 Second Melting Power on 1000℃≤t≤1700℃ Open 1000-1200 cool down Power off 1700℃<t≤1400℃ Open 1200-1500 Demolding Power off 1400℃<t<800℃ closure
[0029] The advantages and positive effects of the present invention are:
[0030] By adopting the above technical scheme, 65%-75% of the unmelted particles on the inner surface of the quartz crucible can be reduced, the cleanliness of the inner surface of the quartz crucible is greatly improved, and the unmelted particles are avoided from being embedded in the inner surface of the quartz crucible during the melting process of the quartz crucible. The risk of single crystal heterogeneous nucleation caused by the falling off of unmelted particles during the use of the quartz crucible is reduced, the crystal quality is improved, and the crystallization rate is increased.
[0031] The embodiments of the present invention are described in detail above, but the contents are only preferred embodiments of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made according to the scope of application of the present invention should still fall within the scope of the patent coverage of the present invention.
Claims
1. A method for reducing unmelted particles on the inner surface of a quartz crucible, It is characterized in that include: The first melting process, the second melting process, the cooling process and the demoulding process are performed. In the second melting process and the cooling process, the unmelted particles on the inner surface of the quartz crucible are removed.
2. A method for reducing unmelted particles on the inner surface of a quartz crucible according to claim 1, Features: The impurity removal process includes using an adsorption device to adsorb the unmelted particles.
3. A method for reducing unmelted particles on the inner surface of a quartz crucible according to claim 2, Features: The adsorption device is continuously arranged above the mold of the quartz crucible.
4. A method for reducing unmelted particles on the inner surface of a quartz crucible according to claim 2, Features: The adsorption device is intermittently arranged above the mold of the quartz crucible.
5. A method for reducing unmelted particles on the inner surface of a quartz crucible according to claim 2, Features: The adsorption device is connected with a vacuum pump.
6. A method for reducing unmelted particles on the inner surface of a quartz crucible according to any one of claims 2 to 5, Features: The operating temperature of the adsorption device is above 1700°C.
7. A method for reducing unmelted particles on the inner surface of a quartz crucible according to claim 1, Features: The temperature of the inner surface of the quartz crucible during the second melting process is higher than the temperature of the inner surface of the quartz crucible during the first melting process, and the temperature of the inner surface of the quartz crucible during the demolding process is lower than the temperature of the inner surface of the quartz crucible during the cooling process.
8. A method for reducing unmelted particles on the inner surface of a quartz crucible according to any one of claims 1 to 5 and 7, Features: During the first melting process and the second melting process, the electrode column is turned on.
9. A method for reducing unmelted particles on the inner surface of a quartz crucible according to claim 8, Features: During the cooling process and demoulding process, the electrode column is closed.
10. A method for reducing unmelted particles on the inner surface of a quartz crucible according to any one of claims 1 to 5, 7 and 9, Features: The time consumption ratio of the first melting process, the second melting process, the cooling process and the demoulding process is 7-10:1-3:2-3:2-4.