Array substrate, preparation method of array substrate, steel mesh and preparation method of steel mesh

By designing the layout of overlapping and non-overlapping areas on the array substrate, combined with the openings and protrusions of the steel mesh, the problem of circuit short circuit during the solder paste printing process of the Mini-LED array substrate is solved, and the transfer yield is improved. and stability.

CN118866907APending Publication Date: 2024-10-29CHENGDU VISTAR OPTEOLECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310473275.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-04-27
Publication Date
2024-10-29

AI Technical Summary

Technical Problem

In the die-solid transfer process of Mini-LED, the array substrate is prone to circuit short circuit during the solder paste printing process, resulting in a reduction in the transfer yield of Mini-LED.

Method used

An array substrate is designed, which includes a stacked first circuit layer and a second circuit layer. The second conductor is vertically projected on the first circuit layer to form an overlapping area. The area outside the overlapping area is a non-overlapping area. Use To withstand the pressure of steel mesh and avoid short circuit. At the same time, a stencil preparation method is used, and multiple openings and protrusions are provided on the stencil to avoid overlapping areas and reduce pressure during the printing process.

Benefits of technology

It effectively avoids circuit short circuits, improves the transfer yield of Mini-LED, and ensures the stability and efficiency of the array substrate during the printing process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118866907A_ABST
    Figure CN118866907A_ABST
Patent Text Reader

Abstract

The invention discloses an array substrate and a preparation method thereof, and a steel mesh and a preparation method thereof. The array substrate is used for welding a light-emitting chip and comprises a first circuit layer, a first insulating layer and a second circuit layer which are arranged in a stacked mode. The first circuit layer comprises at least one first wire; the second circuit layer comprises at least one second wire; the vertical projection of the second wire on the first circuit layer is crossed with the first wire to form an overlapping area; and defining an area outside the overlapping area as a non-overlapping area, wherein the non-overlapping area is a stress area of the array substrate. According to the technical scheme of the embodiment of the invention, short circuit of two adjacent layers of wires can be avoided, and the transfer yield of the light-emitting chip is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present invention relate to the technical field of display panels, and in particular to an array substrate and a manufacturing method thereof, a steel mesh and a manufacturing method thereof. Background Art

[0002] With the development of display technology, display panels have undergone technological innovations from liquid crystal display technology to OLED display technology and then to Mini-LED display technology. As a new generation of display technology, Mini-LED with low temperature polysilicon (LTPS) array substrate has the advantages of high image quality, high reliability and low cost, and has become a research hotspot for the current new generation of display technology.

[0003] However, solder paste printing is required in the die-bonding transfer process of Mini-LED manufacturing, and the array substrate needs to withstand the pressure generated during printing. Different circuit layers of the existing array substrate are prone to short circuits after being subjected to pressure, resulting in a reduction in the transfer yield of Mini-LED. Summary of the invention

[0004] The present invention provides an array substrate and a preparation method thereof, a steel mesh and a preparation method thereof, so as to prevent short circuits between adjacent circuit layers and improve the transfer yield of Mini-LEDs.

[0005] According to one aspect of the present invention, an array substrate is provided for welding a light-emitting chip; the array substrate comprises: a first circuit layer, a first insulating layer, and a second circuit layer which are stacked;

[0006] The first circuit layer includes at least one first conductive line;

[0007] The second circuit layer includes at least one second conductive line;

[0008] A vertical projection of the second conductive line on the first circuit layer intersects with the first conductive line to form an overlapping area;

[0009] The area outside the overlapping area is a non-overlapping area, and the non-overlapping area is a force-bearing area of ​​the array substrate.

[0010] Optionally, a vertical projection of the at least one second conductive line on the first circuit layer forms an overlapping area with the at least one first conductive line in an array arrangement;

[0011] The area of ​​the overlapping region accounts for 40% to 60% of the area of ​​the array substrate.

[0012] Optionally, the first circuit layer and the second circuit layer are two circuit layers located on the top of the array substrate;

[0013] Preferably, the first conductive wire is a first power wire, and the second conductive wire is a second power wire.

[0014] Optionally, the array substrate further includes:

[0015] A second insulating layer is located on a side of the second circuit layer away from the first circuit layer;

[0016] At least one pad is located on a side of the second insulating layer away from the first circuit layer, and the pad is electrically connected to the light-emitting chip;

[0017] Preferably, an area outside the vertical projection of the pad on the first circuit layer at least partially overlaps with the non-overlapping area.

[0018] According to another aspect of the present invention, a system for preparing an array substrate is provided, comprising a steel mesh and the array substrate according to any one of claims 1 to 4, wherein the steel mesh is used for preparing the array substrate according to any one of the first aspect; the steel mesh comprises:

[0019] A steel mesh body, wherein a plurality of openings are arranged on the steel mesh body;

[0020] A plurality of raised portions are arranged on a side surface of the steel mesh body and avoid the opening; the raised portions are used to correspond to the non-overlapping areas of the array substrate.

[0021] Optionally, the depth of the protrusion ranges from 8 to 12 μm;

[0022] And / or, the area of ​​the opening is 40% to 60% of the area of ​​the pad;

[0023] Preferably, the cross-sectional shape of the protrusion is trapezoidal.

[0024] Optionally, the method for preparing the steel mesh comprises:

[0025] providing a steel plate;

[0026] The steel plate is patterned to form a steel mesh body having a plurality of openings and a plurality of protrusions, wherein the plurality of protrusions are located on one side surface of the steel mesh body and avoid the openings, corresponding to the non-overlapping area of ​​the array substrate.

[0027] Optionally, the step of patterning the steel plate includes:

[0028] forming a plurality of openings penetrating the steel plate on the surface of the steel plate;

[0029] Thinning the surface of one side of the steel plate at a position corresponding to the opening to form a plurality of protrusions;

[0030] Preferably, the process of thinning the steel plate comprises at least one of laser engraving, chemical etching and dry etching.

[0031] According to another aspect of the present invention, there is also provided a method for preparing an array substrate, comprising:

[0032] forming a first circuit layer, wherein the first circuit layer includes at least one first conductive line;

[0033] forming a first insulating layer on the first wiring layer;

[0034] forming a second circuit layer on the first insulating layer, wherein the second circuit layer comprises at least one second conductive wire; wherein a vertical projection of the second conductive wire on the first circuit layer intersects with the first conductive wire to form an overlapping region; and defining a region outside the overlapping region as a non-overlapping region;

[0035] Placing a steel mesh on the surface of the array substrate and applying solder on the steel mesh;

[0036] The solder is scraped across the surface of the steel mesh at a constant speed by using a scraper to press the solder obliquely, so that the solder is applied to the surface of the pad through the opening. Optionally, after forming the second circuit layer, the method further includes:

[0037] forming a second insulating layer on the second circuit layer;

[0038] A plurality of pads arranged in an array are formed on the second insulating layer, and the pads are used for soldering the light-emitting chip; wherein the raised portion of the steel mesh avoids the position of the pads;

[0039] A steel mesh as described in any one of the second aspects is placed on the array substrate, and the pressure of the steel mesh acts on the non-overlapping area.

[0040] In the embodiment of the present invention, at least one first wire and at least one second wire are formed respectively by patterning the first wire and the second wire; wherein the overlapped portion of the second wire and the first wire forms an overlapped region. Since the overlapped region is dispersedly arranged on the array substrate, it is advantageous to set the pressure of the steel mesh to avoid the overlapped region during the solder printing process, so that the pressure on the overlapped region is greatly reduced compared to the non-overlapped region. Therefore, the first insulating layer between the first wire and the second wire in the overlapped region is not easily deformed by extrusion, which is advantageous to avoid a short circuit between the first wire and the second wire, thereby improving the transfer yield of the light-emitting chip.

[0041] It should be understood that the contents described in this section are not intended to identify the key or important features of the embodiments of the present invention, nor are they intended to limit the scope of the present invention. Other features of the present invention will become easily understood through the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0043] Figure 1 is a schematic diagram of a top view structure of an array substrate provided according to an embodiment of the present invention;

[0044] Figure 2 is a schematic diagram of a partial cross-sectional structure of an array substrate along the AA' direction provided according to an embodiment of the present invention;

[0045] Figure 3 is a schematic structural diagram of an array substrate during a printing process provided by an embodiment of the present invention;

[0046] Figure 4 is a schematic diagram of a partial cross-sectional structure of another array substrate provided according to an embodiment of the present invention;

[0047] Figure 5 is a schematic diagram of a cross-sectional structure of a steel mesh provided according to an embodiment of the present invention;

[0048] Figure 6 It is a structural schematic diagram corresponding to each step in a method for preparing a steel mesh provided in an embodiment of the present invention;

[0049] Figure 7 It is a structural schematic diagram corresponding to specific steps of step S102 in a method for preparing a steel mesh provided in an embodiment of the present invention;

[0050] Figure 8 is a schematic diagram of a cross-sectional structure of another steel mesh provided according to an embodiment of the present invention;

[0051] Fig. 9 is a schematic diagram of a top view of a steel mesh provided according to an embodiment of the present invention;

[0052] Fig.10 is a schematic diagram of a top view structure of another steel mesh provided according to an embodiment of the present invention;

[0053] Fig.11 is a schematic structural diagram corresponding to each step of a method for preparing an array substrate provided in an embodiment of the present invention;

[0054] Fig.12 It is a structural schematic diagram corresponding to each step of another array substrate preparation method provided according to an embodiment of the present invention. DETAILED DESCRIPTION

[0055] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.

[0056] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0057] An embodiment of the present invention provides an array substrate, which is suitable for bonding self-luminous light-emitting chips such as Mini-LED. Figure 1 is a schematic diagram of a top view of an array substrate provided by an embodiment of the present invention. Figure 2 A schematic diagram of a partial cross-sectional structure of an array substrate along the AA' direction provided by an embodiment of the present invention. Figure 1 and Figure 2 The array substrate includes: a first circuit layer 10, a first insulating layer 20 and a second circuit layer 30 which are stacked.

[0058] The first circuit layer 10 includes at least one first conductive line 11 , and the second circuit layer 30 includes at least one second conductive line 31 .

[0059] The vertical projection of the second wire 31 on the first circuit layer 10 intersects with the first wire 11 to form an overlapping area 40; the area outside the overlapping area 40 is defined as a non-overlapping area, which is a stress-bearing area of ​​the array substrate.

[0060] Among them, the first insulating layer 20 is used to insulate the first circuit layer 10 from the second circuit layer 30. In the related art, when the pressure of the steel mesh acts on the array substrate, the first insulating layer 20 will be squeezed and deformed, resulting in a short circuit problem in the circuits of the first circuit layer 10 and the second circuit layer 30. It should be noted that in the preparation process of the array substrate, the key process technology lies in the backplane array process and the solid crystal transfer process. Among them, the solid crystal transfer process includes plasma cleaning, solder printing, solder paste inspection (Solder Paste Inspection, SPI), light-emitting chip transfer and high-temperature thermal reflow. Among them, in the solder printing step, it is necessary to place the steel mesh on the array substrate, and apply pressure by a scraper to squeeze the solder on the surface of the steel mesh to the surface of the array substrate. Therefore, the array substrate needs to withstand a large pressure from the steel mesh.

[0061] The inventors further discovered that the reason for the short circuit problem on the array substrate is that the pressure of the steel mesh acts on the overlapping position of the wires in the first circuit layer 10 and the second circuit layer 30. If the pressure of the steel mesh is avoided from acting on the overlapping position of the wires, it will help to improve the occurrence of this problem.

[0062] Based on this, the wiring of the array substrate is redesigned in the embodiment of the present invention, so that at least one first wire 11 is provided in the first circuit layer 10, and at least one second wire 31 is provided in the second circuit layer 30. The second wire 31 is in the overlapping area 40 formed by the vertical projection of the first circuit layer 10 and the intersection of the second wire 31, that is, there is no large area of ​​conductor block in the first circuit layer 10 and the second circuit layer 30. For example, see Figure 1 , Figure 1 It is shown that the first circuit layer 10 includes multiple first wires 11, the second circuit layer 30 includes multiple second wires 31, and the overlapping area 40 formed between the first wires 11 and the second wires 31 is a dispersed small conductor block; accordingly, the area where the first wires 11 and the second wires 31 do not overlap (i.e., the non-overlapping area) is also dispersedly arranged.

[0063] For the first circuit layer 10, the first insulating layer 20 and the second circuit layer 30, the non-overlapping area includes an area with only the first wire 11, an area with only the second wire 31 and an area of ​​pure insulating material without a wire. In the non-overlapping area, since there is no overlap between the first wire 11 and the second wire 31, even if it is subjected to a large pressure, it will not cause a wire short circuit.

[0064] Figure 3 A schematic diagram of an array substrate during printing provided by an embodiment of the present invention. Figure 3, illustratively, the non-overlapping area of ​​the array substrate is used as a stress-bearing area to withstand the pressure of the steel mesh in the array substrate preparation process. Specifically, during the solder printing process, the steel mesh 70 is aligned with the array substrate so that the non-overlapping area of ​​the array substrate bears the pressure of the steel mesh 70. Exemplarily, a raised portion 72 is provided on the steel mesh 70, and the raised portion 72 corresponds to the non-overlapping area, so that the pressure of the steel mesh 70 acts on the non-overlapping area. Compared with the non-overlapping area, the pressure from the steel mesh 70 on the overlapping area 40 is very small. Therefore, the first insulating layer 20 in the overlapping area 40 is not easily deformed due to extrusion, which is beneficial to avoid a short circuit between the first wire 11 and the second wire 31, and improves the transfer yield of the light-emitting chip.

[0065] In the embodiment of the present invention, at least one first wire 11 and at least one second wire 31 are formed respectively by patterning the first wire 10 and the second wire 30; wherein the overlapped portion of the second wire 31 and the first wire 11 forms an overlapped region 40. Since the overlapped region 40 is dispersedly arranged on the array substrate, it is advantageous to set the pressure of the steel mesh 70 to avoid the overlapped region 40 during the solder printing process, so that the pressure on the overlapped region 40 is greatly reduced compared to the non-overlapped region. Therefore, the first insulating layer 20 between the first wire 11 and the second wire 31 in the overlapped region 40 is not easily deformed by extrusion, that is, it is advantageous to avoid a short circuit between the first wire 11 and the second wire 31, thereby improving the transfer yield of the light-emitting chip.

[0066] Optionally, based on the above embodiment, continue to refer to Figure 1 , the extension direction of each first wire 11 is the same, for example, they all extend along the first direction X; the extension direction of each second wire 31 is the same, for example, they all extend along the second direction Y, that is, the vertical projection of at least one second wire 31 on the first circuit layer 10 forms an overlapping area 40 arranged in an array with at least one first wire 11; the area of ​​the overlapping area 40 accounts for 40% to 60% of the area of ​​the array substrate. Among them, the area of ​​the overlapping area 40 is determined by the number and width of the first wires 11 and the number and width of the second wires 31. When the number and width of the two wires are large, the area of ​​the overlapping area 40 is large; when the number and width of the two wires are small, the area of ​​the overlapping area 40 is small. If the area ratio of the overlapping area 40 is set to be less than 40%, the number of wires is small or the wires are thin, which may cause the conductive performance to be reduced or the wires to break, and the reliability is low; if the area ratio of the overlapping area 40 is set to be greater than 60%, the area ratio of the non-overlapping area is less than 40%, and the area of ​​the array substrate that can be used to support the steel mesh 70 is small, and the steel mesh 70 may be unstable when subjected to the scraper pressure.

[0067] Optionally, based on the above embodiments, the shape of the overlapping area 40 formed by the vertical projection of the first wire 11 and the second wire 31 can be any shape according to the shapes of the first wire 11 and the second wire 31 and the angle between the two wires. Figure 1 , if the first wire 11 and the second wire 31 are both rectangular, the shape of the overlapping area 40 is a regular pattern. That is, when the cross-sectional shape of the first wire 11 and the second wire 31 is a rectangle, the overlapping area 40 formed by the two wires is a regular pattern. For example, when the angle between the extension direction of the first wire 11 and the second wire 31 is 90°, the overlapping area 40 is rectangular. In other embodiments, when the angle between the extension direction of at least one second wire 31 and at least one first wire 11 is not 90°, the overlapping area 40 is a parallelogram.

[0068] Optionally, based on the above embodiments, the plurality of first conductive lines 11 and the plurality of second conductive lines 31 are evenly arranged so that the overlapping areas 40 and the non-overlapping areas are evenly distributed on the entire surface of the array substrate, so that the entire surface of the array substrate has non-overlapping areas supporting the steel mesh 70. Therefore, the array substrate can evenly withstand the pressure of the steel mesh 70 during printing, effectively preventing the array substrate from being damaged due to uneven force.

[0069] Optionally, on the basis of the above embodiments, the array substrate includes other circuit layers in addition to the first circuit layer 10 and the second circuit layer 30, and the first circuit layer 10 and the second circuit layer 30 are two circuit layers located at the top of the array substrate. When the surface of the array substrate is subjected to pressure, the film layer located at the top of the array substrate is subjected to the greatest extrusion force, and the extrusion force of other signal transmission circuit layers gradually decreases. Therefore, the first insulating layer 20 between the second circuit layer 30 and the first circuit layer 10 is the position most likely to deform, and is also the position where the second wire 31 and the first wire 11 are most likely to short-circuit. In this embodiment, the first circuit layer 10 and the second circuit layer 30 are arranged at the position most likely to short-circuit, and the arrangement of the first circuit layer 10 and the second circuit layer 30 can effectively reduce the steel mesh pressure on the first wire 11 and the second wire 31 in the overlapping area 40, and avoid the deformation of the first insulating layer 20 between the first wire 11 and the second wire 31, resulting in a short circuit between the two wires. Therefore, the embodiment of the present invention is more conducive to preventing other film layer circuits in the array substrate from short-circuiting.

[0070] Preferably, the first wire 11 is a first power line, and the second wire 31 is a second power line. For example, the first wire 11 may be a cathode power line VSS, and the second wire 31 may be an anode power line VDD.

[0071] Optionally, based on the above embodiments, other circuit layers of the array substrate include: a first metal layer, a second metal layer, and a third metal layer, etc. Among them, the first metal layer is used to form a gate of a thin film transistor and one plate of a capacitor, the second metal layer is used to form another plate of the capacitor, and the third metal layer is used to form a source and a drain of the thin film transistor, etc.

[0072] Optionally, Figure 4 FIG. 1 is a schematic diagram of a partial cross-sectional structure of another array substrate provided by an embodiment of the present invention. Figure 3 and Figure 4 The array substrate further includes: a second insulating layer 50 and at least one pad 60. The second insulating layer 50 is located on a side of the second circuit layer 30 away from the first circuit layer 10, and the pad 60 is located on a side of the second insulating layer 50 away from the first circuit layer 10, and the pad 60 is used to electrically connect the light-emitting chip.

[0073] Among them, the pad 60 is a medium for realizing electrical connection between the array substrate and the light-emitting chip. Exemplarily, during the solder printing process, the steel mesh 70 is placed on the surface of the array substrate, and the raised portion of the steel mesh 70 corresponds to the non-overlapping area. By squeezing the solder on the surface of the steel mesh 70, the solder leaks down from the through openings set in the steel mesh 70 and is evenly applied to the surface of the pad 60. Therefore, when transferring the light-emitting chip, the light-emitting chip can be transferred to the corresponding pad 60 position, and the light-emitting chip and the pad 60 are soldered together by the solder, so that the light-emitting chip and the circuit in the array substrate connected to the pad 60 are electrically connected.

[0074] Preferably, the area other than the vertical projection of the pad 60 on the first circuit layer 10 at least partially overlaps with the non-overlapping area. Preferably, the vertical projection of the pad 60 on the first circuit layer 10 at least partially overlaps with the overlapping area 40. In this way, the pad 60 can be arranged to avoid the non-overlapping area, so that when the steel mesh 70 is placed on the array substrate, the pad 60 can avoid the protrusion of the steel mesh 70.

[0075] Based on the above embodiments, the shape and area of ​​the pad 60 can be set according to actual needs. For example, in the direction perpendicular to the thickness of the array substrate, the cross-sectional shape of the pad 60 can be rectangular or circular, without too much restriction.

[0076] Optionally, based on the above embodiments, the pad 60 is a multi-layer structure, including a stacked adhesive layer, a barrier layer and a wetting layer, the adhesive layer is used to firmly bond the pad 60 to the second insulating layer 50, the barrier layer is used to prevent the applied solder from penetrating into the pad 60, and the wetting layer is used to achieve uniform application of the solder on the surface of the pad 60, so as to firmly weld the light-emitting chip to the pad 60. The functional layers included in the pad 60 can be made of different metal materials. For example, the adhesive layer material can include chromium and titanium, the barrier layer material can include nickel, and the wetting layer material can include gold, copper, etc., which are not limited here.

[0077] The embodiment of the present invention further provides a system for preparing an array substrate, comprising a steel mesh and the array substrate described in any of the above embodiments. The steel mesh can be used in the preparation process of the array substrate in each of the above embodiments. Figure 5 FIG. 1 is a schematic diagram of a cross-sectional structure of a steel mesh provided by an embodiment of the present invention. Figure 5 As shown, the steel mesh 70 includes: a steel mesh body 71 and a plurality of protrusions 72 .

[0078] A plurality of openings 711 are provided on the steel mesh body 71; the openings 711 are used to limit the position of solder application; a plurality of protrusions 72 are provided on one side surface of the steel mesh body 71 and avoid the openings 711; the protrusions 72 are used to correspond to the non-overlapping area of ​​the array substrate to support the steel mesh 70.

[0079] Exemplarily, in the preparation process of the array substrate, the steel mesh 70 is aligned with the array substrate and placed on the array substrate, the raised portion 72 corresponds to the non-overlapping area on the array substrate, and the opening 711 corresponds to the pad 60 on the array substrate. The solder can be squeezed to the surface of the pad 60 through the opening 711 to achieve solder printing.

[0080] Among them, the raised portion 72 arranged at the lower part of the steel mesh 70 protrudes from the steel mesh main body 71, and the bottom of the raised portion 72 is in close contact with the surface of the array substrate and corresponds to the non-overlapping area, so that the non-overlapping area can withstand the greater pressure of the steel mesh main body 71 during the solder printing process, which greatly reduces the pressure on the overlapping area 40, which is beneficial to avoid short circuit between the first circuit layer 10 and the second circuit layer 30 in the overlapping area 40.

[0081] Optionally, based on the above embodiments, this embodiment provides a method for preparing a steel mesh, and the preparation method is applicable to the steel mesh provided by any embodiment of the present invention. Figure 6 Schematic diagram of the structure corresponding to each step in a method for preparing a steel mesh provided in an embodiment of the present invention. Figure 6 , the steel mesh preparation method comprises:

[0082] S101. Provide a steel plate 01.

[0083] Illustratively, the thickness of the steel plate may be 20 to 30 μm.

[0084] S102, patterning the steel plate 01 to form a steel mesh main body 71 having a plurality of openings 711 and a plurality of raised portions 72, wherein the openings 711 are used to limit the location of solder smearing; the plurality of raised portions 72 are located on one side surface of the steel mesh main body 71 and avoid the openings 711; the raised portions 72 are used to correspond to the non-overlapping area of ​​the array substrate to support the steel mesh 70.

[0085] The steel plate is subjected to a patterning process, such as laser engraving, chemical etching, dry etching, etc.

[0086] The steel mesh provided in the embodiment of the present invention has a protrusion on one side of the steel mesh body with openings, and the protrusion corresponds to the non-overlapping area to support the steel mesh. In addition, during the printing process, the pressure of the steel mesh can be applied to the non-overlapping area through the protrusion of the steel mesh to reduce the compression of the first insulating layer between the first wire and the second wire in the overlapping area, which is beneficial to avoid the short circuit between the first wire and the second wire, and improve the transfer yield of the light-emitting chip.

[0087] In the above embodiments, step S102 may be to form the opening first and then the protrusion, or to form the protrusion first and then the opening, which is not limited in the present invention.

[0088] Figure 7 1 is a structural schematic diagram corresponding to the specific steps of step S102 in a method for preparing a steel mesh provided in an embodiment of the present invention. Figure 7 In one implementation, optionally, step S102 specifically includes:

[0089] S1021. Form a plurality of openings 711 penetrating the steel plate 01 on the surface of the steel plate 01.

[0090] Exemplarily, a plurality of openings penetrating the steel plate are formed at specific positions of the steel plate by exposure and etching.

[0091] S1022, thinning the surface of one side of the steel plate 01 at a position corresponding to the opening 711 to form a plurality of protrusions 72.

[0092] It can be seen that the embodiment of the present invention first forms the opening and then forms the protrusion. The reason for this arrangement is that the process accuracy of forming the opening by patterning the steel plate is higher, while the process accuracy of forming the protrusion by thinning the steel plate is lower. If the protrusion is prepared first and then the opening is formed, the process accuracy of preparing the opening will be affected. Therefore, by first processing the steel plate to prepare the opening and then preparing the protrusion, the process accuracy of the obtained steel mesh can be higher and the solder printing effect can be better.

[0093] The technical solution provided in this embodiment is to open a plurality of openings 711 on the steel mesh body 71 of the steel mesh 70, and to set a plurality of protrusions 72 on the surface of one side of the steel mesh body 71, and the protrusions 72 are staggered with the openings 711. In the process of printing solder, the solder can be applied to the surface of the pad 60 on the array substrate through the openings 711. The pressure of the solder squeezed by the scraper is applied to the non-overlapping area of ​​the array substrate by the protrusions 72, which is conducive to preventing the first insulating layer 20 between the first circuit layer 10 and the second circuit layer 30 from being deformed due to the greater pressure on the overlapping area 40, improving the problem that the circuit on the top of the array substrate is prone to short circuit in the overlapping area 40, thereby improving the transfer yield of the light-emitting chip.

[0094] Optionally, based on the above embodiments, continue to refer to Figure 5 , the depth of the raised portion 72 ranges from 8 to 12 μm, for example, 8 μm, 9 μm, 10 μm, 11 μm or 12 μm, etc. Among them, the raised portion 72 and the steel mesh body 71 form an inwardly concave cavity, and the cavity is used to provide space for the pad 60 provided on the array substrate. If the depth of the raised portion 72 is less than 8 μm, the steel mesh body 71 may contact the pad 60, which is not conducive to solder printing. If the depth of the raised portion 72 is greater than 12 μm, the thickness of the steel mesh body 71 is too thin, and the steel mesh 70 is easily deformed under the pressure of the scraper, thereby affecting the accuracy of solder printing. Therefore, the embodiment of the present invention sets the depth range of the raised portion 72 to 8 to 12 μm, which is more conducive to solder printing.

[0095] Optionally, based on the above embodiments, the area of ​​the opening 711 is 40% to 60% of the area of ​​the pad 60. If the area of ​​the opening 711 is less than 40%, less solder is applied to the pad 60, which cannot meet the requirements of soldering the light-emitting chip to the pad 60, and may easily cause loose soldering. If the area of ​​the opening 711 is greater than 60%, more solder is applied to the pad 60, which may cause excessive solder to be squeezed out during the subsequent soldering of the light-emitting chip, thereby causing a short circuit with the adjacent pad 60. Therefore, the area of ​​the opening 711 is set to 40% to 60% of the area of ​​the pad 60, so that the solder applied to the pad 60 is moderate, which is conducive to the subsequent soldering of the light-emitting chip.

[0096] In the above-mentioned embodiments, there are many ways to dispose the protrusion 72, and several of them are described below, but they are not intended to limit the present invention.

[0097] In one embodiment, the cross-sectional shape of the protrusion 72 may be a rectangle (eg Figure 5 as shown) or trapezoidal (as Figure 8 The trapezoidal structure is more conducive to reducing the contact area between the protrusion 72 and the surface of the array substrate.

[0098] In another embodiment, the protrusions 72 may be arranged in an array on the entire steel mesh 70. For example, Fig. 9 Schematic diagram of a top view of a steel mesh provided by an embodiment of the present invention. Fig. 9 , each protrusion 72 is relatively small in size, and each protrusion 72 is arranged in an array of multiple rows and columns. Fig.10 Schematic diagram of a top view of another steel mesh provided by an embodiment of the present invention. Fig.10 Each protrusion 72 is in the shape of a long strip, and the protrusions 72 are arranged in a row.

[0099] It should be noted that the position and shape of the raised portion 72 only need to correspond to the non-overlapping area and can play the role of supporting the steel mesh 70. The combination of the above embodiments or other settings of the raised portion 72 are all within the protection scope of the present invention.

[0100] An embodiment of the present invention also provides a method for preparing an array substrate. Fig.11 Schematic diagram of the structure corresponding to each step of a method for preparing an array substrate provided by an embodiment of the present invention. Fig.11 , the preparation method of the array substrate comprises:

[0101] S110 , forming a first circuit layer 10 , wherein the first circuit layer 10 includes at least one first conductive line 11 .

[0102] Exemplarily, the first circuit layer 10 is made of metal material, and is obtained by evaporating a metal film layer and performing patterning processes such as exposure and development on the surface of the metal film layer to form at least one first conductive line.

[0103] S120 , forming a first insulating layer 20 on the first circuit layer 10 .

[0104] Exemplarily, the material of the first insulating layer is silicon nitride and / or silicon oxide. The insulating layer is formed on the first circuit layer by a deposition process, so that the insulating layer covers the surface of the first circuit layer and fills the area between two adjacent first wires in the first circuit layer to keep the first wires in the first circuit layer insulated.

[0105] S130, forming a second circuit layer 30 on the first insulating layer 20, the second circuit layer 30 including at least one second conductive wire 31; wherein a vertical projection of the second conductive wire 31 on the first circuit layer 10 intersects with the first conductive wire 11 to form an overlapping region 40; and defining an area outside the overlapping region 40 as a non-overlapping area.

[0106] Exemplarily, the second circuit layer is also made of metal material. By evaporating a metal film layer and performing patterning processes such as exposure and development on the metal film layer, at least one second wire is formed, and the vertical projection of the second wire on the first circuit layer is arranged to intersect with the first wire to form an overlapping area.

[0107] S140 , placing the steel mesh 70 on the surface of the array substrate, and applying solder on the steel mesh 70 .

[0108] S150 , use a scraper to press the solder obliquely and scrape it across the surface of the steel mesh 70 at a uniform speed, so that the solder passes through the opening 711 and is smeared on the surface of the pad 60 .

[0109] Exemplarily, the scraper squeezes the solder at a certain tilt angle and scrapes it at a uniform speed on the surface of the steel mesh. The tilt angle of the scraper can be 55° to 75°, and the pressure of the scraper can be 15 to 45N. In addition, the length of the scraper needs to be greater than the length of the printing area on the array substrate. Exemplarily, the part where the length of the scraper is greater than the length of the printing area can be 5 to 10 cm. If the scraper is too short, it is impossible to obliquely press a sufficient amount of solder to scrape across the steel mesh at a uniform speed, resulting in insufficient solder leaking from the printing area, affecting the welding effect of the light-emitting chip.

[0110] The array substrate preparation method provided by the embodiment of the present invention forms at least one first wire and a second wire by patterning the first wire layer and the second wire layer; and the extension direction of the first wire intersects with the extension direction of the second wire to form an overlapping area, and the area outside the overlapping area is a non-overlapping area. Since the overlapping areas are dispersedly arranged on the surface of the array substrate, the steel mesh can be aligned and fixed on the array substrate when solder printing is performed, so that the non-overlapping area of ​​the array substrate is subjected to a greater pressure of the steel mesh during printing, and the pressure borne by the overlapping area is reduced, thereby protecting the first insulating layer between the first wire and the second wire in the overlapping area from being easily deformed, which is conducive to avoiding a short circuit between the first wire and the second wire, and effectively improving the transfer yield of the light-emitting chip.

[0111] Optionally, Fig.12 FIG. 1 is a schematic diagram of the structure corresponding to each step of another method for preparing an array substrate provided by an embodiment of the present invention. Fig.12 , after forming the second circuit layer, further comprising:

[0112] S160 , forming a second insulating layer 50 on the second circuit layer 30 .

[0113] Exemplarily, the material of the second insulating layer is silicon oxide and / or silicon nitride, and the second insulating layer is formed on the second circuit layer by a deposition process, so that the second insulating layer covers the second circuit layer and fills the area between two adjacent wires in the second circuit layer, so as to achieve insulation between the second wires in the second circuit layer.

[0114] S170 , forming a plurality of pads 60 arranged in an array on the second insulating layer 50 , the pads 60 being used for soldering the light-emitting chip; wherein the raised portions 72 of the steel mesh 70 avoid the positions of the pads 60 .

[0115] S180, placing the steel mesh 70 provided by any embodiment of the present invention on the array substrate, wherein the raised portion of the steel mesh 70 corresponds to the non-overlapping area of ​​the array substrate.

[0116] Among them, when fixing the steel mesh on the array substrate, accurate alignment is required. It can be seen from the aforementioned embodiments that the openings on the steel mesh correspond to the positions of the pads on the array substrate, and the raised portions on the steel mesh correspond to the non-overlapping areas on the array substrate, so that when printing solder, the pressure of the steel mesh can act on the non-overlapping areas through the raised portions of the steel mesh, while the overlapping areas are not squeezed, thereby protecting the first insulating layer between the first circuit layer and the second circuit layer in the overlapping area from being squeezed and deformed, causing a short circuit between the first wire and the second wire.

[0117] The above specific implementations do not constitute a limitation on the protection scope of the present invention. It should be understood by those skilled in the art that various modifications, combinations, sub-combinations and substitutions can be made according to design requirements and other factors. Any modification, equivalent substitution and improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. An array substrate, characterized in that: The array substrate comprises: a first circuit layer, a first insulating layer and a second circuit layer which are stacked; The first circuit layer includes at least one first conductive line; The second circuit layer includes at least one second conductive line; A vertical projection of the second conductive line on the first circuit layer intersects with the first conductive line to form an overlapping area; The area outside the overlapping area is a non-overlapping area, and the non-overlapping area is a force-bearing area of ​​the array substrate.

2. The array substrate according to claim 1, characterized in that: The vertical projection of the at least one second conductive line on the first circuit layer and the at least one first conductive line form the overlapping area arranged in an array; The area of ​​the overlapping region accounts for 40% to 60% of the area of ​​the array substrate.

3. The array substrate according to claim 1, characterized in that: The first circuit layer and the second circuit layer are two circuit layers located on the top of the array substrate; Preferably, the first conductive wire is a first power wire, and the second conductive wire is a second power wire.

4. The array substrate according to claim 1, characterized in that: Also includes: A second insulating layer is located on a side of the second circuit layer away from the first circuit layer; At least one pad is located on a side of the second insulating layer away from the first circuit layer, and the pad is electrically connected to the light-emitting chip; Preferably, an area outside the vertical projection of the pad on the first circuit layer at least partially overlaps with the non-overlapping area.

5. A system for preparing an array substrate, characterized in that: The invention comprises a steel mesh and an array substrate according to any one of claims 1 to 4, wherein the steel mesh is used for preparing the array substrate according to any one of claims 1 to 4; the steel mesh comprises: A steel mesh body, wherein a plurality of openings are arranged on the steel mesh body; A plurality of raised portions are arranged on a side surface of the steel mesh body and avoid the opening; the raised portions correspond to the non-overlapping areas of the array substrate.

6. The array substrate preparation system according to claim 5, characterized in that: The depth of the protrusion ranges from 8 to 12 μm; And / or, the area of ​​the opening is 40% to 60% of the area of ​​the pad; Preferably, the cross-sectional shape of the protrusion is trapezoidal.

7. The array substrate preparation system according to claim 5, characterized in that: The method for preparing the steel mesh comprises: providing a steel plate; The steel plate is patterned to form a steel mesh body having a plurality of openings and a plurality of protrusions, wherein the plurality of protrusions are located on one side surface of the steel mesh body and avoid the openings, corresponding to the non-overlapping area of ​​the array substrate.

8. The array substrate preparation system according to claim 7, characterized in that: The step of patterning the steel plate comprises: forming a plurality of openings penetrating the steel plate on the surface of the steel plate; Thinning the surface of one side of the steel plate at a position corresponding to the opening to form a plurality of protrusions; Preferably, the process of thinning the steel plate comprises at least one of laser engraving, chemical etching and dry etching.

9. A method for preparing an array substrate, characterized in that: include: forming a first circuit layer, wherein the first circuit layer includes at least one first conductive line; forming a first insulating layer on the first wiring layer; forming a second circuit layer on the first insulating layer, wherein the second circuit layer comprises at least one second conductive wire; wherein a vertical projection of the second conductive wire on the first circuit layer intersects with the first conductive wire to form an overlapping region; and defining a region outside the overlapping region as a non-overlapping region; Placing a steel mesh on the surface of the array substrate and applying solder on the steel mesh; The solder is scraped across the surface of the steel mesh at a uniform speed by oblique pressure using a scraper, so that the solder is smeared onto the surface of the pad through the openings.

10. The method for preparing an array substrate according to claim 9, characterized in that: After forming the second circuit layer, the method further includes: forming a second insulating layer on the second circuit layer; A plurality of pads arranged in an array are formed on the second insulating layer, and the pads are used for soldering the light-emitting chip; wherein the raised portion of the steel mesh avoids the position of the pads; A steel mesh as described in any one of claims 5 to 8 is placed on the array substrate, and the pressure of the steel mesh acts on the non-overlapping area.