Preparation process of weather-resistant PE modified material

By mixing and heating PE materials in the tank, combined with the air exchange and cooling technology of the drive components, weather-resistant PE modified materials are prepared, which solves the water absorption and aging problems of the profile and achieves improvements in anti-pollution and wear resistance.

CN118876261AActive Publication Date: 2024-11-01CHANGZHOU ATE NEW MATERIALS TECH CO LTD

Patent Information

Application Number
CN202410900800.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-05
Publication Date
2024-11-01
Estimated Expiration
2044-07-05

AI Technical Summary

Technical Problem

When used on the surface of the profile, the water absorption rate improvement effect is poor, and it cannot effectively improve the aging and pollution resistance of the profile.

Method used

Using a preparation process of weather-resistant PE modified materials, by mixing HDPE, propylene glycol butyl ether, wear-resistant agent, matting agent, antistatic agent and UV stabilizer in the tank, heating is performed using a high-speed stirring and granulator. Kneading, combined with the reciprocating motion of the drive assembly accelerates air exchange and cooling, a weather-resistant PE modified material is prepared.

Benefits of technology

Effectively reduce the water absorption rate of the profile, improve aging and anti-pollution properties, and the material is wear-resistant and not easy to fade, and improves the heat dissipation effect and avoids heat waste.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118876261A_ABST
    Figure CN118876261A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of PE material production, and discloses a preparation process of a weather-resistant PE modified material and a preparation device applied to the weather-resistant PE modified material.The preparation device comprises a tank body, a support is fixedly installed at the top of the tank body, and a motor is fixedly installed in the middle of the top wall of the support; a cylinder is fixedly mounted on an output shaft of the motor, and a stirring rod is fixedly connected to the bottom of the cylinder. The PE modified material is used as a surface layer material, so that the water absorption rate of the profile can be reduced, the purposes of improving aging and resisting pollution are achieved, the PE modified material is resistant to abrasion and not prone to fading, accelerated exchange and circulation between a tank body and outside air can be achieved in the preparation process, heat in the tank body is taken away, and in the preparation process, heat dissipation is accelerated, and the service life of the tank body is prolonged. And waste caused by the fact that materials move to the outside through the air outlet along with flowing of air can be avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of PE material production, and particularly relates to a preparation process of a weather-resistant PE modified material. Background Art

[0002] Polyethylene (PE for short) is a thermoplastic resin obtained by polymerization of ethylene. In industry, it also includes copolymers of ethylene and a small amount of α-olefins. Polyethylene is odorless, non-toxic, feels like wax, has excellent low temperature resistance (the lowest operating temperature can reach -100 to -70°C), good chemical stability, and can withstand the corrosion of most acids and alkalis (not resistant to acids with oxidizing properties). It is insoluble in general solvents at room temperature, has low water absorption, and has excellent electrical insulation. When the existing PE material is applied to the surface of the profile, it has a poor effect on improving the water absorption rate of the profile, and cannot improve the problem of profile aging, and has little help in the anti-pollution of the profile. Therefore, it is necessary to invent a preparation process for a weather-resistant PE modified material to solve the above problems. Summary of the invention

[0003] In view of the above problems, the present invention provides a preparation process of a weather-resistant PE modified material to solve the problems raised in the above background technology.

[0004] To achieve the above object, the present invention provides the following technical solutions:

[0005] A preparation process of a weather-resistant PE modified material, applied to a preparation device of a weather-resistant PE modified material, the preparation device comprising a tank body, a bracket fixedly installed on the top of the tank body, a motor fixedly installed on the middle of the top wall of the bracket, a cylinder fixedly installed on the output shaft of the motor, a stirring rod fixedly connected to the bottom of the cylinder, an opening opened on the top of the tank body, a pressing plate arranged in the opening, the pressing plate sleeved on the outside of the cylinder, the inner ring and the outer ring of the pressing plate are both provided with sealing rings, the sealing rings are in contact with the cylinder and the inner wall of the tank body, an air outlet is equidistantly arranged on the cylinder, an air inlet pipe communicating with the inside of the tank body is equidistantly fixedly installed on the outside of the tank body, a one-way valve is arranged inside the air inlet pipe and the air outlet, and a driving component for driving the pressing plate to reciprocate up and down is arranged on the outside of the pressing plate;

[0006] The preparation process of the weather-resistant PE modified material comprises the following steps:

[0007] S1. Weigh the following raw materials according to the component ratio: HDPE 1-98%, propylene glycol butyl ether 1-8%, anti-wear agent 1-60%, matting agent 0.1-15%, lubricant 0-10%, antistatic agent 1-15%, hexamethylenetetramine 1-14%, heat stabilizer 0.01-9%, UV stabilizer 0.01-9%; the UV stabilizer is a mixture of sodium acetate, chlorinated polyethylene and methyl hydroxybenzoate; the anti-wear agent is a mixture of hydroxy silicone oil, nano zinc oxide, titanium nitride powder and graphene oxide;

[0008] S2, the HDPE, wear resistance agent and heat stabilizer are mixed according to the formula ratio and added into the reactor, and propylene glycol butyl ether is added after being fully stirred at 100-110°C, and the stirring reaction is continued for 2-2.5 hours. After the reaction is completed, the material mixture A is obtained by drying; the matting agent, antistatic agent, hexamethylenetetramine and UV stabilizer are mixed according to the formula ratio, and the mixture is stirred at 60-70°C for 1-1.5 hours, and the material mixture B is obtained after drying and cooling;

[0009] S3, putting the mixture A and the mixture B obtained in step S2 into the tank body (1) and stirring at high speed, setting the baking temperature of the mixer to 150°C to 180°C, the mixing time to 2-3 hours, and discharging the materials after natural cooling to 40°C. During the cooling process, the pressing plate (6) is driven by the driving component to reciprocate, thereby accelerating the exchange of air in the tank body (1) with the outside, so that the temperature can be lowered faster;

[0010] S4. Add the raw materials obtained in step S3 into a granulator for heating, kneading and bonding. The aspect ratio of the granulator is 33:52, the granulation temperature is 180-250°C, the screw speed is 300-500r / min, and the PE modified material is obtained by water pelletizing.

[0011] Furthermore, the percentage content of each component of the wear-resistant agent is: 10-30% hydroxy silicone oil, 5-15% nano zinc oxide, 11-29% titanium nitride powder and 6-24% graphene oxide; the percentage content of each component of the UV stabilizer is: a mixture of 20-45% sodium acetate, 15-35% chlorinated polyethylene and 20-28% methyl hydroxybenzoate.

[0012] Furthermore, the preparation process of the wear-resistant agent is as follows: hydroxy silicone oil, titanium nitride powder and graphene oxide are added into a mixer in proportion, heated to 100-140° C. and stirred evenly, then nano zinc oxide and hydrazine hydrate solution are added, refluxed for 3-4.5 hours, and the wear-resistant agent is obtained by distillation, washing and drying.

[0013] Furthermore, the driving assembly includes a pressure rod symmetrically fixedly mounted on the pressure plate, the cross-sectional shape of the pressure rod is T-shaped, the pressure rod is slidably inserted into the bracket, a first spring is sleeved on the outside of the pressure rod and located above the bracket, a cross plate is fixedly mounted on the output shaft of the motor, a rotating shaft is rotatably mounted on the cross plate, a round rod is fixedly mounted outside the rotating shaft, a torsion spring is arranged outside the rotating shaft, two ends of the torsion spring are respectively fixedly connected to the rotating shaft and the cross plate, a baffle rod is fixedly mounted on the bottom of the cross plate, the baffle rod is fitted with the round rod, a pressure block is fixedly mounted equidistantly around the top of the pressure plate, and a curved surface is provided on one side of the pressure block.

[0014] Furthermore, the external fixed sleeve of the stirring rod is provided with a sleeve block, the outer side of the sleeve block is provided with an annular groove, an annular frame is slidably installed in the annular groove, a filter is fixedly installed inside the annular frame, the annular frame is fixedly connected to the cylinder by a pair of telescopic tubes, the air outlet is located between the pair of telescopic tubes, the annular frame and the top wall of the annular groove are fixedly connected by a plurality of second springs, a lifting rod is fixedly installed on the outside of the annular frame, and the inner wall of the tank body is provided with a lifting assembly for driving the lifting rod to rise.

[0015] Furthermore, the lifting assembly includes a top block, a first inclined surface is provided on a side of the top block close to the lifting rod, a second inclined surface is provided on a side of the top block away from the first inclined surface, a rectangular rod is fixedly installed on one side of the top block, a mounting frame is provided on the outer sleeve of the rectangular rod, the mounting frame is fixedly connected to the rectangular rod by a third spring, one end of the mounting frame is fixedly installed on the inner wall of the tank body, the number of the top blocks corresponds to the pressure blocks, and the top blocks are located between adjacent pressure blocks.

[0016] Furthermore, the inner wall of the tank body is provided with a cavity, and the cavity is provided with an electric heating network.

[0017] Furthermore, a feed port is provided at the upper outer portion of the tank body, a cover plate is threadedly connected to the feed port, a temperature monitor is provided on the outer side of the tank body, a discharge pipe is provided at the bottom of the tank body, and a solenoid valve is provided inside the discharge pipe.

[0018] Technical effects and advantages of the present invention:

[0019] 1. The PE modified material obtained by the present invention as the surface material can reduce the water absorption rate of the profile, achieve the purpose of improving aging and anti-pollution, and is wear-resistant and not easy to fade;

[0020] 2. The present invention can realize accelerated exchange and circulation between the tank body and the outside air during the preparation process, take away the heat in the tank body, accelerate cooling, and in the process of accelerating air flow, the stirring rod stirs the material to better dissipate the heat in the material, thereby improving the heat dissipation effect of the material;

[0021] 3. During the preparation process, the present invention accelerates heat dissipation and can avoid waste caused by the material moving to the outside through the air outlet along with the flow of air. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 A schematic structural diagram of a tank body according to an embodiment of the present invention is shown;

[0023] Figure 2 A schematic diagram showing a partial structure of an embodiment of the present invention Figure 1 ;

[0024] Figure 3 The embodiment of the present invention is shown Figure 2 The enlarged structural diagram at A in the middle;

[0025] Figure 4 A schematic cross-sectional view of a tank body according to an embodiment of the present invention is shown;

[0026] Figure 5 The embodiment of the present invention is shown Figure 4 The enlarged structural diagram at B in the middle;

[0027] Figure 6 A schematic diagram showing a partial structure of an embodiment of the present invention Figure 2 ;

[0028] Figure 7 The embodiment of the present invention is shown Figure 6 The enlarged structural diagram at C in the middle;

[0029] Figure 8 A schematic diagram showing a partial structure of an embodiment of the present invention Figure 3 ;

[0030] Fig. 9 The embodiment of the present invention is shown Figure 8 The enlarged structural diagram at D in the middle;

[0031] In the figure: 1, tank body; 2, bracket; 3, motor; 4, cylinder; 5, stirring rod; 6, pressure plate; 7, air outlet; 8, air inlet pipe; 9, one-way valve; 10, pressure rod; 11, first spring; 12, cross plate; 13, round rod; 14, torsion spring; 15, stop rod; 16, pressure block; 17, sleeve block; 18, ring frame; 19, filter screen; 20, telescopic tube; 21, second spring; 22, lifting rod; 23, top block; 24, first inclined plane; 25, second inclined plane; 26, rectangular rod; 27, mounting frame; 28, third spring; 29, electric heating network; 30, temperature monitor. DETAILED DESCRIPTION

[0032] In order to make the purpose, technical solution and advantages of the embodiments of the present invention more clear, the technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments.

[0033] The present invention provides a preparation process of a weather-resistant PE modified material, which is applied to a preparation device of a weather-resistant PE modified material, such as Figures 1 to 9 As shown, the preparation device includes a tank body 1, a bracket 2 is fixedly installed on the top of the tank body 1, a motor 3 is fixedly installed in the middle of the top wall of the bracket 2, a cylinder 4 is fixedly installed on the output shaft of the motor 3, a stirring rod 5 is fixedly connected to the bottom of the cylinder 4, an opening is opened on the top of the tank body 1, a pressing plate 6 is arranged in the opening, the pressing plate 6 is sleeved on the outside of the cylinder 4, the inner and outer rings of the pressing plate 6 are both provided with sealing rings, the sealing rings are in contact with the cylinder 4 and the inner wall of the tank body 1, an air outlet 7 is equidistantly arranged on the cylinder 4, an air inlet pipe 8 connected with the interior of the tank body 1 is fixedly installed equidistantly on the outer side of the tank body 1, a one-way valve 9 is arranged inside the air inlet pipe 8 and the air outlet 7, and a driving component for driving the pressing plate 6 to reciprocate up and down is arranged on the outside of the pressing plate 6;

[0034] When in use, start the motor 3 to make its output shaft rotate forward to drive the cylinder 4 and the stirring rod 5 to rotate, so that the raw materials in the tank body 1 are mixed. After completion, start the motor 3 to make its output shaft reverse, and cooperate with the driving component to drive the pressing plate 6 to reciprocate up and down. When the pressing plate 6 descends, the air in the tank body 1 is squeezed out. At this time, the one-way valve 9 located in the air outlet 7 is opened, and the one-way valve 9 located in the air inlet pipe 8 is closed. The air in the tank body 1 is discharged to the outside through the air outlet 7 with heat. When the pressing plate 6 rises, air is sucked into the tank body 1. At this time, the one-way valve 9 located in the air inlet pipe 8 is closed. The one-way valve 9 in the air outlet 7 is closed, and the one-way valve 9 in the air inlet pipe 8 is opened, and the outside air enters the tank body 1 through the air inlet pipe 8. As the pressing plate 6 reciprocates up and down, the outside air continuously enters the tank body 1 according to the above principle, and is then discharged through the air outlet 7, which accelerates the flow of internal air, allows the air to exchange with the outside air, takes away the heat in the tank body 1, accelerates cooling, and in the process of accelerating the air flow, the stirring rod 5 stirs the material to better dissipate the heat in the material, thereby improving the heat dissipation effect of the material.

[0035] The preparation process of the weather-resistant PE modified material comprises the following steps:

[0036] S1. Weigh the following raw materials according to the component ratio: HDPE 1-98%, propylene glycol butyl ether 1-8%, anti-wear agent 1-60%, matting agent 0.1-15%, lubricant 0-10%, antistatic agent 1-15%, hexamethylenetetramine 1-14%, heat stabilizer 0.01-9%, UV stabilizer 0.01-9%; UV stabilizer is a mixture of sodium acetate, chlorinated polyethylene and methyl hydroxybenzoate; anti-wear agent is a mixture of hydroxy silicone oil, nano zinc oxide, titanium nitride powder and graphene oxide;

[0037] S2, HDPE, wear resistance agent and heat stabilizer are mixed according to the formula ratio and added into the reactor, propylene glycol butyl ether is added after being fully stirred at 100-110°C, and the reaction is continued by stirring for 2-2.5 hours. After the reaction is completed, the material mixture A is obtained by drying; the matting agent, antistatic agent, hexamethylenetetramine and UV stabilizer are mixed according to the formula ratio, the mixture is stirred at 60-70°C for 1-1.5 hours, and the material mixture B is obtained after drying and cooling;

[0038] S3, putting the mixture A and the mixture B obtained in step S2 into the tank body 1 for high-speed stirring, setting the baking temperature of the mixer to 150°C-180°C, the mixing time to 2-3 hours, and discharging the materials after natural cooling to 40°C. During the cooling process, the pressing plate 6 is driven by the driving assembly to reciprocate, thereby accelerating the exchange of air in the tank body 1 with the outside, so that the temperature can be lowered faster;

[0039] S4. Add the raw materials obtained in step S3 into a granulator for heating, kneading and bonding. The aspect ratio of the granulator is 33:52, the granulation temperature is 180-250°C, the screw speed is 300-500r / min, and the PE modified material is obtained by water pelletizing.

[0040] The percentage content of each component of the wear-resistant agent is: 10-30% of hydroxy silicone oil, 5-15% of nano zinc oxide, 11-29% of titanium nitride powder and 6-24% of graphene oxide; the percentage content of each component of the UV stabilizer is: a mixture of 20-45% of sodium acetate, 15-35% of chlorinated polyethylene and 20-28% of methyl hydroxybenzoate.

[0041] The added anti-wear agent and stabilizer make the material wear-resistant and corrosion-resistant, while the antistatic agent, lubricant, UV stabilizer and matting agent can make the co-extruded profile have a good gloss appearance and antistatic performance, and increase the texture of the profile. Among them, the raw material combination does not contain fillers, wood powder, and wood fiber, thereby improving the water absorption rate of the profile, thereby achieving the effect of improving aging and anti-pollution.

[0042] The PE modified material obtained by this process as the surface material can reduce the water absorption rate of the profile, achieve the purpose of improving aging and anti-pollution, and is wear-resistant and not easy to fade.

[0043] The preparation process of the wear-resistant agent is as follows: hydroxy silicone oil, titanium nitride powder and graphene oxide are added into a mixer in proportion, heated to 100-140°C and stirred evenly, then nano zinc oxide and hydrazine hydrate solution are added, refluxed for 3-4.5 hours, and the wear-resistant agent is obtained by distillation, washing and drying.

[0044] like Figures 1 to 3As shown, the driving assembly includes a pressure rod 10 symmetrically fixedly mounted on the pressure plate 6, the cross-sectional shape of the pressure rod 10 is T-shaped, the pressure rod 10 is slidably inserted into the bracket 2, and a first spring 11 is sleeved on the outside of the pressure rod 10 and located above the bracket 2, a cross plate 12 is fixedly mounted on the output shaft of the motor 3, a rotating shaft is rotatably mounted on the cross plate 12, a round rod 13 is fixedly mounted outside the rotating shaft, a torsion spring 14 is arranged outside the rotating shaft, and two ends of the torsion spring 14 are respectively fixedly connected to the rotating shaft and the cross plate 12, a baffle 15 is fixedly mounted on the bottom of the cross plate 12, and the baffle 15 is in contact with the round rod 13, a pressure block 16 is fixedly mounted equidistantly around the top of the pressure plate 6, and a curved surface is arranged on one side of the pressure block 16.

[0045] The output shaft of the motor 3 rotates forwardly, driving the horizontal plate 12, the rotating shaft, and the round rod 13 to move accordingly. After the round rod 13 contacts the pressure block 16, the round rod 13 drives the rotating shaft to rotate, causing the torsion spring 14 to torsionally deform the round rod 13 to generate a force, causing the round rod 13 to avoid the pressure block 16. After the round rod 13 leaves the pressure block 16, the torsion spring 14 drives the rotating shaft and the round rod 13 to reset, thereby ensuring the normal rotation of the output shaft of the motor 3. When the output shaft of the motor 3 is reversed, after the round rod 13 contacts the arc surface of the pressure block 16, At this time, due to the existence of the blocking rod 15, the round rod 13 cannot be deflected. As a result, the movement of the round rod 13 causes the arc surface to press the pressure block 16, causing it to move down with the pressure plate 6 and the pressure rod 10, thereby compressing the first spring 11 and deforming it to generate a force. When the round rod 13 leaves the pressure block 16, the first spring 11 releases its force and moves the pressure rod 10, the pressure plate 6, and the pressure block 16 up and back to their original position. As the round rod 13 continuously contacts and separates from the pressure block 16, the pressure plate 6 can achieve an up and down reciprocating motion.

[0046] like Figures 4 to 8 As shown, the outside of the stirring rod 5 is fixedly sleeved with a sleeve block 17, the outside of the sleeve block 17 is provided with an annular groove, an annular frame 18 is slidably installed in the annular groove, a filter screen 19 is fixedly installed inside the annular frame 18, the annular frame 18 is fixedly connected to the cylinder 4 by a pair of telescopic tubes 20, the air outlet 7 is located between the pair of telescopic tubes 20, the annular frame 18 is fixedly connected to the top wall of the annular groove by a plurality of second springs 21, a lifting rod 22 is fixedly installed on the outside of the annular frame 18, and the inner wall of the tank body 1 is provided with a lifting assembly for driving the lifting rod 22 to rise.

[0047] The output shaft of the motor 3 is reversed, driving the cylinder 4, the stirring rod 5, the sleeve block 17, the second spring 21, the annular frame 18, and the lifting rod 22 to rotate accordingly. When the round rod 13 does not conflict with the pressing block 16, the lifting assembly drives the lifting rod 22 to make it rise with the annular frame 18 and the filter screen 19, compressing the second spring 21 to deform it and generate a force. Then the lifting assembly cancels the drive to the lifting rod 22, and the second spring 21 releases the force to drive the annular frame 18 and the filter screen 19 down. The annular frame 18 hits the bottom wall of the annular groove to generate vibration, which is transmitted to the filter screen 19. Then the round rod 13 and the pressing block The arc surface of 16 conflicts with the pressure plate 6, driving the pressure plate 6 to descend and discharge the air in the tank body 1 to the outside. At this time, the air in the tank body 1 passes through the filter screen 19 to filter out the floating materials and then is discharged to the outside. The materials remain on the filter screen 19. When the round rod 13 is separated from the pressure block 16, the pressure plate 6 rises and resets. At this time, air is replenished in the tank body 1. At this time, the lifting component drives the lifting rod 22 again. The vibration of the filter screen 19 can be achieved as above, so that the materials on the filter screen 19 can be shaken off. The subsequent principle is the same as above. During the whole process, it can be avoided that the materials move to the outside through the air outlet 7 with the flow of air to cause waste.

[0048] like Figures 4 to 8 As shown, the lifting assembly includes a top block 23, a first inclined surface 24 is provided on the side of the top block 23 close to the lifting rod 22, a second inclined surface 25 is provided on the side of the top block 23 away from the first inclined surface 24, a rectangular rod 26 is fixedly installed on one side of the top block 23, a mounting frame 27 is provided on the outer sleeve of the rectangular rod 26, the mounting frame 27 is fixedly connected to the rectangular rod 26 by a third spring 28, one end of the mounting frame 27 is fixedly installed on the inner wall of the tank body 1, the number of the top blocks 23 corresponds to the pressing blocks 16, the top blocks 23 are located between adjacent pressing blocks 16, and the second inclined surface 25 is arranged toward the annular frame 18.

[0049] When the output shaft of the motor 3 is reversed, the lifting rod 22 moves to contact the first inclined surface 24 of the top block 23. As the lifting rod 22 moves, it rises along the first inclined surface 24, thereby bringing the annular frame 18 and the filter screen 19 up and compressing the second spring 21 to deform and generate a force. When the lifting rod 22 leaves the top block 23, the second spring 21 releases its force and brings the annular frame 18 and the filter screen 19 down. The annular frame 18 hits the bottom wall of the annular groove to generate vibration, and the vibration is transmitted to the filter screen 19. Subsequently, as the lifting rod 22 continues to move, the filter screen 19 can be continuously vibrated. When the output shaft of the motor 3 rotates forward, the lifting rod 22 moves accordingly. The lifting rod 22 conflicts with the second inclined surface 25, so that the second inclined surface 25 squeezes the rectangular rod 26 to make it contract and compresses the third spring 28 to deform and generate a force, so that the top block 23 avoids the lifting rod 22 to ensure the rotation of the output shaft of the motor 3. When the lifting rod 22 is separated from the top block 23, the third spring 28 releases its force and resets the rectangular rod 26 and the top block 23.

[0050] like Figure 4As shown, the inner wall of the tank body 1 is provided with a cavity, and the cavity is provided with an electric heating network 29.

[0051] The tank body 1 can be heated by starting the electric heating network 29 .

[0052] like Figure 4 As shown, a feed port is provided at the upper outer portion of the tank body 1, a cover plate is threadedly connected to the feed port, a temperature monitor 30 is provided at the outer side of the tank body 1, a discharge pipe is provided at the bottom of the tank body 1, and a solenoid valve is provided in the discharge pipe.

[0053] Raw materials can be poured into the tank body 1 through the feed port, and the cover plate can be rotated to combine with the feed port. The temperature monitor 30 can monitor the temperature inside the tank body 1 to facilitate understanding whether the heating temperature meets the requirements. When discharging, the solenoid valve is opened and the internal material is discharged through the discharge pipe.

[0054] Working principle: When in use, start the motor 3 to make its output shaft rotate forward to drive the cylinder 4 and the stirring rod 5 to rotate, so that the raw materials in the tank body 1 are mixed. The output shaft of the motor 3 rotates forward to drive the horizontal plate 12, the rotating shaft, and the round rod 13 to move accordingly. After the round rod 13 contacts the pressing block 16, the round rod 13 drives the rotating shaft to rotate, so that the torsion spring 14 torsional deformation generates a force, so that the round rod 13 avoids the pressing block 16. When the round rod 13 leaves the pressing block 16, the torsion spring 14 drives the rotating shaft and the round rod 13 to reset, so that To ensure the normal rotation of the output shaft of the motor 3, after completion, start the motor 3 to reverse its output shaft. When the output shaft of the motor 3 reverses, the round rod 13 contacts the arc surface of the pressure block 16. At this time, due to the existence of the blocking rod 15, the round rod 13 cannot deflect. As a result, the movement of the round rod 13 makes the arc surface press the pressure block 16 to make it move with the pressure plate 6 and the pressure rod 10 to descend, compressing the first spring 11 to deform it and generate a force. When the round rod 13 leaves the pressure block 16, the first spring 11 releases its force and brings When the pressure plate 6 is lowered, the air in the tank body 1 is squeezed outwards, and the one-way valve 9 in the air outlet 7 is opened, and the one-way valve 9 in the air inlet pipe 8 is closed. The air in the tank body 1 is discharged to the outside through the air outlet 7 with heat. When the pressure plate 6 rises, air is extracted into the tank body 1. At this time, the one-way valve 9 in the air outlet 7 is closed, and the one-way valve 9 in the air inlet pipe 8 is opened. The outside air enters the tank body 1 through the air inlet pipe 8. With the up and down reciprocating motion of the pressure plate 6, the same principle is used, so that the outside air continuously enters the tank body 1 and is discharged through the air outlet 7, which accelerates the flow of internal air, so that the air is exchanged with the outside air, takes away the heat in the tank body 1, and accelerates the cooling. In the process of accelerating the air flow, the stirring rod 5 stirs the material to better dissipate the heat in the material, thereby improving the heat dissipation effect of the material.The output shaft of the motor 3 is reversed, driving the cylinder 4, the stirring rod 5, the sleeve block 17, the second spring 21, the annular frame 18, and the lifting rod 22 to rotate accordingly. When the round rod 13 does not conflict with the pressure block 16, the lifting rod 22 moves to conflict with the first inclined surface 24 of the top block 23. As the lifting rod 22 moves, it rises along the first inclined surface 24, thereby driving the annular frame 18 and the filter screen 19 to rise and compress the second spring 21 to deform and generate a force. When the lifting rod 22 leaves the top block 23, the second spring 21 releases the force and drives the annular frame 18 and the filter screen 19 to descend. The annular frame 18 hits the bottom wall of the annular groove to generate vibration, and the vibration is transmitted to the filter screen 19. Subsequently, the round rod 13 conflicts with the arc surface of the pressure block 16, driving the pressure plate 6 to descend and discharge the air in the tank body 1 to the outside. At this time, the air in the tank body 1 passes through the filter screen 19 to filter out the floating materials and is discharged to the outside, and the materials remain on the filter screen 19 , when the round rod 13 is separated from the pressing block 16, the same principle applies. At this time, the pressing plate 6 rises and resets. At this time, air is added to the tank body 1. The lifting rod 22 continues to contact and separate from the top block 23. Subsequently, with the continuous movement of the lifting rod 22, the filter screen 19 can be continuously vibrated to avoid the blockage of the filter screen 19 and shake the material into the material below. Subsequently, the same principle applies. During the whole process, the material can be prevented from moving to the outside through the air outlet 7 with the flow of air and causing waste. When the output shaft of the motor 3 rotates forward, the lifting rod 22 moves accordingly. The lifting rod 22 contacts the second inclined surface 25, so that the second inclined surface 25 squeezes the rectangular rod 26 to make it contract and compresses the third spring 28 to deform it to generate a force, so that the top block 23 avoids the lifting rod 22, ensuring the rotation of the output shaft of the motor 3. When the lifting rod 22 is separated from the top block 23, the third spring 28 releases the force to reset the rectangular rod 26 and the top block 23. ;

[0055] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit them.

Claims

1. A preparation process of a weather-resistant PE modified material, characterized in that: A preparation device for a weather-resistant PE modified material, the preparation device comprising a tank body (1), a bracket (2) fixedly mounted on the top of the tank body (1), a motor (3) fixedly mounted in the middle of the top wall of the bracket (2), a cylinder (4) fixedly mounted on the output shaft of the motor (3), a stirring rod (5) fixedly connected to the bottom of the cylinder (4), an opening formed on the top of the tank body (1), a pressing plate (6) disposed in the opening, and the pressing plate (6) sleeved on the cylinder The outer part of the column (4), the inner ring and the outer ring of the pressure plate (6) are both provided with sealing rings, the sealing rings are in contact with the inner wall of the cylinder (4) and the tank body (1), the cylinder (4) is provided with air outlets (7) at equal intervals, the outer side of the tank body (1) is fixedly provided with air inlet pipes (8) connected with the interior thereof at equal intervals, the inside of the air inlet pipes (8) and the air outlets (7) are both provided with one-way valves (9), and the outer side of the pressure plate (6) is provided with a driving component for driving the pressure plate (6) to reciprocate up and down; The preparation process of the weather-resistant PE modified material comprises the following steps: S1. Weigh the following raw materials according to the component ratio: HDPE 1-98%, propylene glycol butyl ether 1-8%, anti-wear agent 1-60%, matting agent 0.1-15%, lubricant 0-10%, antistatic agent 1-15%, hexamethylenetetramine 1-14%, heat stabilizer 0.01-9%, UV stabilizer 0.01-9%; the UV stabilizer is a mixture of sodium acetate, chlorinated polyethylene and methyl hydroxybenzoate; the anti-wear agent is a mixture of hydroxy silicone oil, nano zinc oxide, titanium nitride powder and graphene oxide; S2, the HDPE, wear resistance agent and heat stabilizer are mixed according to the formula ratio and added into the reactor, and propylene glycol butyl ether is added after being fully stirred at 100-110°C, and the stirring reaction is continued for 2-2.5 hours. After the reaction is completed, the material mixture A is obtained by drying; the matting agent, antistatic agent, hexamethylenetetramine and UV stabilizer are mixed according to the formula ratio, and the mixture is stirred at 60-70°C for 1-1.5 hours, and the material mixture B is obtained after drying and cooling; S3, putting the mixture A and the mixture B obtained in step S2 into the tank body (1) and stirring at high speed, setting the baking temperature of the mixer to 150°C to 180°C, the mixing time to 2-3 hours, and discharging the materials after natural cooling to 40°C. During the cooling process, the pressing plate (6) is driven by the driving component to reciprocate, thereby accelerating the exchange of air in the tank body (1) with the outside, so that the temperature can be lowered faster; S4. Add the raw materials obtained in step S3 into a granulator for heating, kneading and bonding. The aspect ratio of the granulator is 33:52, the granulation temperature is 180-250°C, the screw speed is 300-500r / min, and the PE modified material is obtained by water pelletizing.

2. The preparation process of the weather-resistant PE modified material according to claim 1, characterized in that: The percentage content of each component of the wear-resistant agent is: 10-30% of hydroxy silicone oil, 5-15% of nano zinc oxide, 11-29% of titanium nitride powder and 6-24% of graphene oxide; the percentage content of each component of the UV stabilizer is: a mixture of 20-45% of sodium acetate, 15-35% of chlorinated polyethylene and 20-28% of methyl hydroxybenzoate.

3. The preparation process of the weather-resistant PE modified material according to claim 2, characterized in that: The preparation process of the wear-resistant agent is as follows: hydroxy silicone oil, titanium nitride powder and graphene oxide are added into a mixer according to a proportion, heated to 100-140° C. and stirred evenly, then nano zinc oxide and hydrazine hydrate solution are added, refluxed for 3-4.5 hours, and the wear-resistant agent is obtained by distillation, washing and drying.

4. The preparation process of the weather-resistant PE modified material according to claim 3, characterized in that: The driving assembly comprises a pressure rod (10) symmetrically fixedly mounted on a pressure plate (6), the cross-sectional shape of the pressure rod (10) being T-shaped, the pressure rod (10) being slidably inserted into a bracket (2), a first spring (11) being sleeved on the outside of the pressure rod (10) and located above the bracket (2), a transverse plate (12) being fixedly mounted on the output shaft of the motor (3), a rotating shaft being rotatably mounted on the transverse plate (12), a round rod (13) being fixedly mounted outside the rotating shaft, a torsion spring (14) being sleeved on the rotating shaft, two ends of the torsion spring (14) being fixedly connected to the rotating shaft and the transverse plate (12) respectively, a baffle rod (15) being fixedly mounted on the bottom of the transverse plate (12), the baffle rod (15) being in contact with the round rod (13), a pressure block (16) being fixedly mounted equidistantly around the top of the pressure plate (6), and a curved surface being provided on one side of the pressure block (16).

5. The preparation process of the weather-resistant PE modified material according to claim 4, characterized in that: The outer sleeve of the stirring rod (5) is provided with a sleeve block (17), the outer side of the sleeve block (17) is provided with an annular groove, an annular frame (18) is slidably installed in the annular groove, a filter screen (19) is fixedly installed inside the annular frame (18), the annular frame (18) and the cylinder (4) are fixedly connected via a pair of telescopic tubes (20), the air outlet (7) is located between the pair of telescopic tubes (20), the annular frame (18) and the top wall of the annular groove are fixedly connected via a plurality of second springs (21), a lifting rod (22) is fixedly installed outside the annular frame (18), and the inner wall of the tank body (1) is provided with a lifting assembly for driving the lifting rod (22) to rise.

6. The preparation process of the weather-resistant PE modified material according to claim 5, characterized in that: The lifting assembly comprises a top block (23), a first inclined surface (24) is provided on a side of the top block (23) close to the lifting rod (22), a second inclined surface (25) is provided on a side of the top block (23) away from the first inclined surface (24), a rectangular rod (26) is fixedly mounted on one side of the top block (23), a mounting frame (27) is sleeved on the outside of the rectangular rod (26), the mounting frame (27) is fixedly connected to the rectangular rod (26) via a third spring (28), one end of the mounting frame (27) is fixedly mounted on the inner wall of the tank body (1), the number of the top blocks (23) corresponds to the pressure blocks (16), and the top blocks (23) are located between adjacent pressure blocks (16).

7. The preparation process of the weather-resistant PE modified material according to claim 6, characterized in that: The inner wall of the tank body (1) is provided with a cavity, and the cavity is provided with an electric heating network (29).

8. The preparation process of the weather-resistant PE modified material according to claim 7, characterized in that: A feed port is provided at the upper outer portion of the tank body (1), a cover plate is threadedly connected to the feed port, a temperature monitor (30) is provided at the outer side of the tank body (1), a discharge pipe is provided at the bottom of the tank body (1), and a solenoid valve is provided inside the discharge pipe.

Citation Information

Patent Citations

  • Manufacturing process for weather-resistant PE modified material and profile co-extrusion device

    CN112693093A

  • Multi-station building template machining equipment

    CN114734329A

  • Rapid bag breaking, mixing and limited discharging device for two ton bag fertilizer raw materials

    CN117753291A

  • Preparation method and preparation equipment of liquid crystal emulsifier for preventing sebum of human body

    CN118058981A

Cited By

  • Wastewater treatment device for cosmetic processing and treatment method thereof

    CN119349763A