Process for removing calcium and magnesium ions in wastewater and recycling water

Through the combination of modified biochar loaded nano-iron and starch-polysilicic acid flocculant, the problems of low calcium and magnesium ion removal efficiency and insufficient biochar stability in wastewater are solved, and efficient calcium and magnesium ion removal and environmentally friendly water treatment are achieved. , simplifies the recycling of biochar.

CN118878149APending Publication Date: 2024-11-01黄继林

Patent Information

Application Number
CN202411224231.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-03
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The prior art has low efficiency in removing calcium and magnesium ions in wastewater, and insufficient stability and recycling rate of biochar, and traditional flocculants have problems with non-degradable and secondary pollution.

Method used

Modified biochar-loaded nano-ferrous iron as adsorbent, combined with starch-polysilicic acid composite flocculant and polyaluminum chloride as complexing agent, and removed calcium and magnesium ions in wastewater through multiple steps, including aeration stirring and magnetic stirring. It separates the floating sludge slag and water from the nano-water purification integrated machine system, and utilizes the adsorption ability of modified biochar and the sedimentation effect of flocculant.

Benefits of technology

Effectively remove calcium and magnesium ions in wastewater, improve the water quality reuse standards, avoid the problem of dirt and calcium formation in equipment, realize green and environmentally friendly water treatment, and simplify the recycling and reuse of biochar.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118878149A_ABST
    Figure CN118878149A_ABST
Patent Text Reader

Abstract

According to the process for removing calcium and magnesium ions in wastewater and recycling water, the wastewater is subjected to metal removal and impurity adsorption through calcium and magnesium removal agent treatment, modified charcoal loaded nano-iron adsorbent treatment, modified starch as a composite flocculant treatment and polyaluminum chloride as a complexing agent, and the whole process is green and environmentally friendly; the ecological environment is protected, and the utilization rate of water resources is increased.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of wastewater treatment, and in particular relates to a process for removing calcium and magnesium ions from wastewater and reusing the wastewater. Background Art

[0002] Wastewater contains a variety of harmful substances, such as heavy metals, organic solvents, high-concentration COD (chemical oxygen demand), high-salt wastewater, etc., which need to undergo a series of professional deep treatments to meet recycling standards. Although wastewater recycling faces many technical and economic challenges, with the advancement of technology and the growth of market demand, the prospects for wastewater recycling are still very optimistic.

[0003] Heavy metal removal is one of the most important processes in wastewater treatment. Due to their non-degradable nature, heavy metals often persist in nature, causing serious environmental problems. At the same time, they seriously endanger human health. They enter the human body through various pathways. Once heavy metals enter the human body, they will coordinate with the internal tissues of the human body, destroy the normal physiological functions of the human body, and even destroy the nervous system, interfering with the normal function of the nerves, thus causing serious health problems. Therefore, it is necessary to find efficient and environmentally friendly methods to remove heavy metals from water. So far, methods for removing heavy metals from aqueous solutions have been widely studied, including various methods. Conventional methods include ion exchange, chemical precipitation, adsorption, membrane separation, electrodialysis, biological treatment, etc.

[0004] Biochar contains abundant functional groups, has a large specific surface area, a small and medium pore carbon skeleton, and good electrical conductivity. The rich active surface functional groups are crucial for the adsorption of heavy metals. It is generally believed that the chemical and physical interactions between heavy metals and the functional groups of the adsorbent improve the adsorption of heavy metals. Although biochar has excellent ability to adsorb heavy metal ions from metal-contaminated solutions, its adsorption capacity is relatively low compared with other adsorbents such as activated carbon. Therefore, although some scientific research has been conducted on the application of biochar in recent years, it has mainly focused on modifying biochar with good surface properties and novel structures to improve its environmental benefits and remediation effects. For example, efforts have been made to increase its porosity, surface area, and surface functional groups. There are four main methods for modifying biochar: chemical modification, physical modification, magnetic modification, and mineral oxide impregnation.

[0005] In order to overcome the shortcomings of biochar when in use, such as lack of stability, easy aggregation and oxidation, and improve the effective activity of biochar. In addition, after pollutants in the water body are adsorbed, powdered biochar is difficult to separate from the water quality, which reduces the utilization rate of water treated with biochar. The present invention chooses to modify it and load magnetic metals to improve the above problems.

[0006] Natural organic polymer modified flocculants can be divided into starch, cellulose, plant gum and polysaccharide according to their raw material sources. Starch modified flocculants are obtained by chemically modifying natural organic polymer substances in agricultural and sideline products. They are non-toxic and harmless to natural organisms and the environment during use, can be completely degraded naturally, have no secondary pollution, and meet the needs of green chemicals.

[0007] Inorganic-organic composite flocculants have a wide range of applications and significant effects, but improper selection of raw materials can easily lead to the same shortcomings as traditional inorganic flocculants and synthetic organic flocculants, such as non-degradability and secondary pollution. Natural organic matter such as starch and chitosan can overcome the above shortcomings. In recent years, the composite modified starch flocculants developed by research and development have increased functional groups through oxidation, etherification, graft copolymerization, cross-linking and other means, improved the performance of starch-based flocculants, and overcome the shortcomings of traditional flocculants.

[0008] The present invention is based on the development background of flocculants, and studies the environmentally friendly water treatment agent with high efficiency, low consumption, non-toxic, biodegradable and no secondary pollution - starch-polysilicate composite flocculant, which meets the characteristics of new high-efficiency and environmentally friendly flocculants, is the key research direction of countries around the world today, and is in line with the theme of the development of the times. Traditional inorganic flocculants have large dosage, large sludge production, residual metal and secondary pollution risks, while the marketization of synthetic organic polymer flocculants is mainly based on acrylamide and its derivatives, which are non-degradable and have the disadvantages of biological toxicity. This type of flocculant is no longer in line with the development concepts of the times such as green, healthy and environmental protection. This study uses natural starch and sodium silicate as the base material, which not only has simple raw materials and low prices, but also does not contain non-toxic and harmless substances. Compared with commercially available polyacrylamine flocculants, it has the advantage of being biodegradable. Compared with the flocculants used in combination with polysilicic acid and inorganic salts, it is simple to operate, and no metal ions remain after water treatment, which is in line with the theme of the times of green environmental protection and sustainable development.

[0009] As a highly efficient flocculant and adsorbent, polyaluminium chloride (PAC) has the ability to remove pollutants such as suspended solids, colloids and heavy metal ions. However, in practical applications, there are also some problems and challenges. In the process of preparing polyaluminium chloride by acid leaching activation of fly ash, the obtained polyaluminium chloride product may contain a large amount of impurities. The present invention improves the comprehensive complexing performance of polyaluminium chloride by optimizing the roasting temperature, the activator ratio and the acid leaching conditions and compounding other complexing agents. Summary of the invention

[0010] The present invention discloses a process for removing calcium and magnesium ions from wastewater for water quality reuse, so as to solve the above and any potential problems in the prior art. In order to solve the above technical problems, the treatment method of the present invention is:

[0011] First, add 0.2-0.4% decalcifier to the raw water and aerate and stir it in the reaction tank. The aeration volume is 2.8L / min, and the stirring speed is 150-200r / min. After stirring for 20min, add 0.4-0.8% demagnesium agent and continue aeration and stirring for 20min. Then add 1-5% adsorbent. At room temperature, magnetic stirring is performed at 150-200r / min. The aeration power of the electromagnetic air pump is 90W, the aeration volume is 2.8L / min, and the aeration stirring time is 30 -60min, then add 0.1-0.3% flocculant and aerate and stir for 30-60min, and separate the floating mud and water through the nano water purifier system; then continue to add 3-8% complexing agent to the separated water, and magnetically stir at 150-200r / min, the electromagnetic air pump aeration power is 90W, the aeration volume is 2.8L / min, the aeration stirring time is 60-90min, and the floating mud and water are separated through the nano water purifier system, and the recovered water quality meets the reuse standard;

[0012] The main components of the calcium and magnesium ion removal agent are sodium carbonate and sodium hydroxide, and the removal principle is: Na2CO3+Ca2+→CaCO3↓+2Na+Ca2++2OH-→Ca(OH)2↓

[0013] The complexing agent is an activator: fly ash with a mass ratio of 1.2-1.5:1, heated in a water bath at 90°C until the mixture is dry, the obtained fly ash is ground into powder, put into a muffle furnace for roasting, the sintering temperature is 800°C, the roasting time is 1.5-2h, and after cooling, it is ground into powder, and twice the mass of sodium silicate solution is added, the reaction temperature is 50-60°C, the time is 2-3h, filtered and dried, and 10-20% of sodium polyphosphate is added to mix to obtain the complexing agent;

[0014] The activator is obtained by dissolving 5-10 parts of sodium n-hexane sulfonate in a sodium silicate solution with a mass fraction of 10-15%.

[0015] The main components of the complexing agent are polyaluminium chloride, sodium polyphosphate and sodium silicate. The removal principle is: Na3O10+Ca2+→Na3(CaP3O10)+2Na+Na2SiO3+CaCl2=CaSiO3↓+2NaCl. Polyaluminium chloride is used as a complexing agent to remove metals from wastewater. Polyaluminium chloride as a complexing agent can effectively complex flocs in water and increase alum flocs, thereby effectively removing calcium and magnesium ions from wastewater.

[0016] The adsorbent is biochar, and the biochar also includes a modification process: corn stalk powder and acidic oxygen-containing acid solution are mixed evenly according to a ratio of 1:0.8-1.2 and then ground, the obtained mixture is placed in a porcelain boat and placed in a tube furnace for pyrolysis, the temperature is increased to 700-800°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature is controlled for 2 hours to obtain a pyrolysis product, add a hydrochloric acid solution with a mass fraction of 0.35% for washing, filter with a vacuum filter, and then repeatedly wash with distilled water until the pH is neutral, and put it in an oven at 80°C for drying to obtain the modified biochar;

[0017] The acidic oxygen-containing acid is a phthalimide peroxycaproic acid solution with a mass fraction of 3-6%.

[0018] The modified biochar also includes the process of loading nano-iron: take 1.4-1.8 parts of the above modified biochar and add it to 100 parts of FeSO4 solution with a mass fraction of 3.8-4.5%, and under nitrogen protection and mechanical stirring at 150r / min, add an equal volume of NaBH4 solution with a mass fraction of 2.5% at a uniform rate, and the dropping speed is 3mL / min. After the addition is completed, continue to stir the reaction for 30 minutes, then use a magnet to separate the solid and liquid, wash the precipitate with ultrapure water and anhydrous ethanol twice each, and finally dry it in vacuum at 60°C for 12 hours and store it for later use.

[0019] The flocculant is based on soluble starch particles. 70-100 parts of starch raw materials that have passed through 40 meshes are placed in a 60°C oven for baking for 24 hours for activation. After being dissolved in water, the raw materials are sealed and placed in an oil bath at 60-80°C for heating and gelatinization for 30 minutes while being stirred with a magnetic force of 150 r / min. Then, 200 parts of a polysilicic acid solution with a mass fraction of 1.5-2% and 30-50 parts of a flocculant monomer are added. The mixture is stirred with a magnetic force of 150 r / min. Then, 0.02 -0.08 parts of 10% ammonium persulfate solution by mass to initiate monomer polymerization, maintain the polymerization temperature at 48-52°C, and continue for 4 hours under the protection of nitrogen inert gas, supplement 50 parts of 1.5-2% polysilicic acid solution by mass every 1 hour, and the reaction is completed to obtain a white viscous substance, which is naturally cooled to room temperature and then washed with anhydrous ethanol and precipitated with acetone. The extracted white solid is cut into pieces, dried in a vacuum oven or a freeze drying oven at 40°C for 48 hours, and then ground into granules.

[0020] The flocculant monomer is acetylhydrazine trimethylammonium chloride.

[0021] The advantages and beneficial effects of the present invention are:

[0022] 1. The present invention provides a process for removing calcium and magnesium ions from wastewater and recycling water quality. The process removes metal from wastewater by treating with calcium and magnesium agents, treating with modified biochar loaded with nano-iron adsorbents, treating with modified starch as a composite flocculant, and using polyaluminum chloride as a chelating agent. Polyaluminum chloride as a chelating agent can effectively chelate flocs in water and increase alum flocs, thereby effectively removing calcium and magnesium ions from wastewater, absorbing impurities, and avoiding the problem of calcium scale in equipment, reservoirs, and transportation pipelines. The whole process is green and environmentally friendly, which is beneficial to protecting the ecological environment and improving the utilization rate of water resources.

[0023] 2. The present invention uses magnetism and phthalimide peroxycaproic acid treatment to modify the adsorbent biochar. The process is simple and easy to operate, and a green and environmentally friendly activated carbon adsorption material is obtained. Phthalimide peroxycaproic acid can not only remove impurities on the surface of activated carbon, but also increase the specific surface area and acidic oxygen-containing functional groups. By increasing the π-π bonds of biochar, the introduction of magnetic substances increases the electrostatic effect, and the adsorption sites are greatly increased. Phthalimide peroxycaproic acid has strong oxidizing properties, and more acidic oxygen-containing groups are generated on the surface of biochar, thereby improving the hydrophilicity of biochar and increasing the cation exchange capacity of biochar, which is beneficial for the modified biochar to effectively adsorb metal ions such as calcium and magnesium in water bodies, and the loaded magnetic metal can enhance the adsorption and precipitation of metal ions on the surface of biochar, rather than simple electrostatic attraction, thereby achieving the purpose of purifying water quality.

[0024] 3. Through composite modification with magnetic materials, in the actual sewage treatment process, the solid-liquid separation of biochar materials and water can be achieved quickly by magnetic separation, so as to realize the rapid and easy recovery and reuse of biochar materials.

[0025] 4. Starch modified with etherifying agents such as acidic phenoxy groups is often used to prepare flocculants. The flocculants prepared by this method are prone to form hydrogen bond dimers due to the phenoxy groups. Therefore, it is necessary to destroy the dimers and eliminate protons to increase their selective adsorption performance.

[0026] 5. The flocs formed by the modified starch-polysilicate flocculant prepared by the invention are coarse and dense, and have a fast sedimentation rate, which is helpful to solve the problems of water pollution and water resources. The starch-polysilicate composite flocculant of the present invention is an improvement and combination of a natural modified starch flocculant and a traditional polysilicate inorganic flocculant. The combination of polysilicate and cationic modified starch can not only make up for the disadvantages of low molecular weight and short molecular chain of natural starch, but also better play the role of adsorption bridging and net capture and sweeping, and reduce the manufacturing cost. It can also overcome the disadvantages of polysilicate being anionic, having the same charge as sewage and wastewater, being mutually exclusive with suspended matter and maintaining stability, being difficult to settle, and having poor flocculation effect, thereby promoting the application of polysilicate.

[0027] 6. Activation: The starch molecular chains after heating and gelatinization are fully extended in the solution, exposing more active sites, which is convenient for subsequent grafting reaction with other monomers. The present invention uses acetylhydrazine trimethylammonium chloride and polysilicic acid as flocculant monomers. The structure of acetylhydrazine trimethylammonium chloride contains acylhydrazine units. The introduction of acylhydrazine units causes the helical structure in the starch molecules to be locally unfolded at the position of the substituent, making the starch macromolecular chains easier to extend and diffuse into the water.

[0028] 7. The steric hindrance of acetylhydrazine trimethylammonium chloride is small, the polymerization activity is high, and it is not easy to absorb free radicals in the system and cause self-inhibition. After a certain amount of acetylhydrazine trimethylammonium chloride cationic monomer is introduced, the starch surface has a multi-layer stacked structure, and holes of different pore sizes are distributed on the surface, which has a large surface area. The flocculant contains N and Cl elements, and the distribution on the surface is relatively uniform. It selectively adsorbs calcium and magnesium ions and forms micro-flocculations by bridging, which accelerates the sedimentation process, thereby improving the treatment efficiency of removing metal ions.

[0029] 8. Compared with polyacrylamide and other flocculants, acetylhydrazine trimethylammonium chloride modified starch flocculant has a wide distribution of pores, a more uniform pore size, and a better sense of wrinkle layering. The solid structure has a larger specific surface area, and can expose more adsorption sites in water after dissolution. Therefore, acetylhydrazine trimethylammonium chloride modified starch flocculant theoretically has better adsorption capacity, better play the role of adsorption charge neutralization, adsorption bridging and net capture and sweeping, and is conducive to flocculation.

[0030] 9. The present invention uses sodium n-hexane sulfonate as an activator. On the one hand, polyaluminium chloride as a complexing agent can effectively complex flocs in water and increase alum flocs, thereby effectively removing calcium and magnesium ions in wastewater, and plays a synergistic role with the flocculant in the previous step. On the other hand, during the acid leaching activation process of sodium n-hexane sulfonate, sodium ions have a good destructive effect on the network of fly ash glass, and the introduction of sulfonic acid will increase the solubility of aluminum salts. In order to further promote the rupture and reconstruction of Si-AI bonds in fly ash and transform the crystal form, the fly ash with the above activator added is respectively placed in a resistance furnace for roasting. The surface of the fly ash particles after roasting becomes rougher, the sponge-like peeling layer deepens, and many fine polyhedral broken particles appear. It is explained that after adding sodium n-hexane sulfonate and mixed calcination, some glass bodies break, which reduces the diffusion resistance of sodium n-hexane sulfonate, and the subsequent contact area with sodium polyphosphate, sodium silicate and other complexes becomes larger, which is easy to react; other glass bodies are spherical, with relatively small friction and difficult to break, but due to the collision of other irregular particles and grinding media, scratches and uneven undulating surfaces appear on the surface of the particles, forming surface defects and high-density dislocations, and the surface energy becomes larger, so that the potential energy of the polyaluminum chloride particles is improved, the surface activity is also enhanced, and the instability trend is increased, thereby increasing the thermal reaction activity of polyaluminum chloride, making it easier to cross the potential barrier, so that the activity of polyaluminum chloride is significantly enhanced, the complexing effect is increased, and it has a significant effect in removing calcium and magnesium ions. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 It is a process flow chart. DETAILED DESCRIPTION

[0032] The present invention is further described in detail below in conjunction with the examples. The fly ash used below is purchased from Shanghai Gaote Chemical Co., Ltd., and the particle size ranges from 80 μm to 150 μm.

[0033] Example 1

[0034] Biochar modification: corn straw powder and 5% phthalimide peroxycaproic acid solution were mixed in a ratio of 1:1 and then ground. The mixture was placed in a porcelain boat and placed in a tube furnace for pyrolysis. The temperature was raised to 750°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature was controlled for 2 hours to obtain the pyrolysis product. A 0.35% hydrochloric acid solution was added for washing, filtered with a vacuum filter, and repeatedly washed with distilled water until the pH was neutral. The modified biochar was dried in an oven at 80°C to obtain the modified biochar.

[0035] Biochar loaded with nano-iron: 1.6 parts of the modified biochar were added to 100 parts of 4.2% FeSO4 solution, and an equal volume of 2.5% NaBH4 solution was added at a uniform rate of 3 mL / min under nitrogen protection and mechanical stirring at 150 r / min. After the addition was completed, the stirring reaction was continued for 30 min, and then a magnet was used to separate the solid and liquid. The precipitate was washed twice with ultrapure water and anhydrous ethanol, and finally vacuum dried at 60 ° C for 12 h and stored for later use;

[0036] Flocculant: using soluble starch granules as the base material, 85 parts of starch raw materials that have passed through 40 meshes are placed in a 60°C oven for baking for 24 hours to activate, then dissolved in water and sealed and placed in a 70°C oil bath for heating and gelatinization for 30 minutes accompanied by magnetic stirring at 150 r / min, then 200 parts of 1.8% polysilicic acid solution and 40 parts of acetylhydrazine trimethylammonium chloride are added, followed by magnetic stirring at 150 r / min, and then 0.06 parts of 10% ammonium persulfate solution are added dropwise to initiate monomer polymerization, the polymerization temperature is maintained at 50°C, and the polymerization is continued for 4 hours under the protection of nitrogen inert gas, and 50 parts of 1.8% polysilicic acid solution are added every 1 hour. After the reaction is completed, a white viscous substance is obtained, which is naturally cooled to room temperature, washed with anhydrous ethanol, and precipitated with acetone, and the extracted white solid is cut into pieces, dried in a vacuum oven or a freeze drying oven at 40°C for 48 hours, and then ground and granulated;

[0037] First, 0.23% sodium carbonate decalcifier was added to the raw water for aeration and stirring in the reaction barrel. The aeration volume was 2.8L / min and the stirring speed was 180r / min. After stirring for 20 minutes, 0.6% sodium hydroxide demagnesium agent was added and aeration and stirring was continued for 20 minutes. Then 3% biochar adsorbent was added and magnetic stirring was performed at 180r / min at room temperature. The aeration power of the electromagnetic air pump was 90W, the aeration volume was 2.8L / min, and the aeration stirring time was 45 minutes. Finally, 0.2% flocculant was added and aerated and stirred for 45 minutes, and then the sludge and water were separated by air flotation through the nano water purification system.

[0038] Example 2

[0039] Biochar modification: corn straw powder and 3% phthalimide peroxycaproic acid solution were mixed at a ratio of 1:1.2 and then ground. The mixture was placed in a porcelain boat and put into a tube furnace for pyrolysis. The temperature was raised to 800°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature was controlled for 2 hours to obtain the pyrolysis product. A 0.35% hydrochloric acid solution was added for washing, filtered with a vacuum filter, and repeatedly washed with distilled water until the pH was neutral. The modified biochar was dried in an oven at 80°C to obtain the modified biochar.

[0040] Biochar loaded with nano-iron: 1.8 parts of the modified biochar were added to 100 parts of 3.8% FeSO4 solution, and an equal volume of 2.5% NaBH4 solution was added at a uniform rate of 3 mL / min under nitrogen protection and mechanical stirring at 150 r / min. After the addition was completed, the stirring reaction was continued for 30 min, and then a magnet was used to separate the solid and liquid. The precipitate was washed twice with ultrapure water and anhydrous ethanol, and finally vacuum dried at 60 ° C for 12 h and stored for later use;

[0041] Flocculant: Using soluble starch granules as the base material, 70 parts of starch raw materials that have passed through 40 meshes are placed in a 60°C oven for baking for 24 hours to activate, then dissolved in water and sealed and placed in an 80°C oil bath for heating and gelatinization for 30 minutes accompanied by magnetic stirring at 150r / min, then 200 parts of 2% polysilicic acid solution by mass, 50 parts of acetylhydrazine trimethylammonium chloride, and magnetic stirring at 150r / min are added, and then 0.02 parts of 10% ammonium persulfate solution by mass are continuously added to initiate monomer polymerization, and the polymerization temperature is maintained at 52°C. The polymerization is continued for 4 hours under the protection of nitrogen inert gas, and 50 parts of 2% polysilicic acid solution by mass are added every 1 hour. After the reaction is completed, a white viscous substance is obtained, which is naturally cooled to room temperature, washed with anhydrous ethanol, and precipitated with acetone. The extracted white solid is cut into pieces, dried in a vacuum oven or a freeze drying oven at 40°C for 48 hours, and then ground and granulated;

[0042] First, 0.2% sodium carbonate decalcifier was added to the raw water for aeration and stirring in the reaction barrel. The aeration volume was 2.8L / min and the stirring speed was 200r / min. After stirring for 20 minutes, 0.4% sodium hydroxide demagnesium agent was added and aeration and stirring was continued for 20 minutes. Then 1% biochar adsorbent was added and magnetic stirring was performed at 200r / min at room temperature. The aeration power of the electromagnetic air pump was 90W, the aeration volume was 2.8L / min, and the aeration stirring time was 30 minutes. Finally, 0.3% flocculant was added and aerated and stirred for 60 minutes, and then the sludge and water were separated by air flotation through the nano water purification system.

[0043] Example 3

[0044] Biochar modification: corn straw powder and 6% phthalimide peroxycaproic acid solution were mixed evenly at a ratio of 1:1.2 and then ground. The mixture was placed in a porcelain boat and placed in a tube furnace for pyrolysis. The temperature was raised to 700°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature was controlled for 2 hours to obtain the pyrolysis product. A 0.35% hydrochloric acid solution was added for washing, filtered with a vacuum filter, and repeatedly washed with distilled water until the pH was neutral. The modified biochar was dried in an oven at 80°C to obtain the modified biochar.

[0045] Biochar loaded with nano-iron: 1.4 parts of the modified biochar were added to 100 parts of a 4.5% FeSO4 solution, and an equal volume of a 2.5% NaBH4 solution was added at a uniform rate of 3 mL / min under nitrogen protection and mechanical stirring at 150 r / min. After the addition was completed, the stirring reaction was continued for 30 min, and then a magnet was used to separate the solid and liquid. The precipitate was washed twice with ultrapure water and anhydrous ethanol, and finally dried under vacuum at 60 ° C for 12 h and stored for later use;

[0046] Flocculant: using soluble starch granules as the base material, 100 parts of starch raw materials that have passed through 40 meshes are placed in a 60°C oven for baking for 24 hours to activate, then dissolved in water and sealed and placed in a 60°C oil bath for heating and gelatinization for 30 minutes accompanied by magnetic stirring at 150r / min, then 200 parts of 1.5% polysilicic acid solution by mass, 30 parts of acetylhydrazine trimethylammonium chloride, and magnetic stirring at 150r / min are added, and then 0.08 parts of 10% ammonium persulfate solution by mass are continuously added to initiate monomer polymerization, and the polymerization temperature is maintained at 48°C, and the polymerization is continued for 4 hours under the protection of nitrogen inert gas, and 50 parts of 1.5% polysilicic acid solution by mass are added every 1 hour. After the reaction is completed, a white viscous substance is obtained, which is naturally cooled to room temperature, washed with anhydrous ethanol, and precipitated with acetone, and the extracted white solid is cut into pieces, dried in a vacuum oven or a freeze drying oven at 40°C for 48 hours, and then ground and granulated;

[0047] First, 0.4% sodium carbonate decalcifier was added to the raw water for aeration and stirring in the reaction barrel. The aeration volume was 2.8L / min and the stirring speed was 150r / min. After stirring for 20 minutes, 0.8% sodium hydroxide demagnesium agent was added and aeration and stirring was continued for 20 minutes. Then, 5% biochar adsorbent was added and magnetic stirring was performed at 150r / min at room temperature. The aeration power of the electromagnetic air pump was 90W, the aeration volume was 2.8L / min, and the aeration stirring time was 60 minutes. Finally, 0.1% flocculant was added for aeration and stirring for 30 minutes, and then the sludge and water were separated by air flotation through the nano water purification system.

[0048] Comparative Example 1

[0049] The difference between this comparative example and Example 1 is that the biochar in this comparative example is not modified. The specific biochar preparation process is as follows: the corn stalk powder is evenly ground and placed in a porcelain boat and placed in a tubular furnace for pyrolysis, and the temperature is raised to 750°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature is controlled for 2 hours to obtain a pyrolysis product, add a hydrochloric acid solution with a mass fraction of 0.35% to wash, filter with a vacuum filter, and then repeatedly wash with distilled water until the pH is neutral, and dry in an oven at 80°C.

[0050] Biochar loaded with nano-iron: 1.6 parts of the above biochar were added to 100 parts of 4.2% FeSO4 solution by mass, and an equal volume of 2.5% NaBH4 solution was uniformly added at a rate of 3 mL / min under nitrogen protection and mechanical stirring at 150 r / min. After the addition was completed, the stirring reaction was continued for 30 min, and then a magnet was used to separate the solid and liquid. The precipitate was washed twice with ultrapure water and anhydrous ethanol, and finally vacuum dried at 60°C for 12 h and stored for later use. The rest was the same as in Example 1.

[0051] Comparative Example 2

[0052] The difference between this comparative example and Example 1 is that in this comparative example, nano-iron is not loaded on the biochar. The specific biochar preparation process is as follows: Biochar modification: corn straw powder and 5% by mass phthalimide peroxyhexanoic acid solution are mixed in a ratio of 1:1 and then ground. The resulting mixture is placed in a porcelain boat and placed in a tubular furnace for pyrolysis. The temperature is raised to 750°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature is controlled for 2 hours to obtain a pyrolysis product. A 0.35% by mass hydrochloric acid solution is added for washing, filtered with a vacuum filter, and then repeatedly washed with distilled water until the pH is neutral, and dried in an oven at 80°C to obtain the modified biochar; the rest is the same as Example 1.

[0053] Comparative Example 3

[0054] The difference between this method and Example 1 is that the biochar is not modified and loaded with nano-iron. The specific process is: the corn straw powder is evenly ground and placed in a porcelain boat and placed in a tubular furnace for pyrolysis. The temperature is raised to 750°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature is controlled for 2 hours to obtain the pyrolysis product, add a hydrochloric acid solution with a mass fraction of 0.35% to wash, filter with a vacuum filter, and then repeatedly wash with distilled water until the pH is neutral, and put it in an 80°C oven for drying; the rest is the same as Example 1.

[0055] Comparative Example 4

[0056] The difference between this comparative example and Example 1 is that the phthalimide peroxycaproic acid solution is hydrochloric acid, and the rest is the same as Example 1.

[0057] Comparative Example 5

[0058] The difference between this comparative example and Example 1 lies in the addition amount of phthalimide peroxycaproic acid solution. The specific process is as follows: corn straw powder and 10% phthalimide peroxycaproic acid solution are mixed in a ratio of 1:1 and then ground. The obtained mixture is placed in a porcelain boat and put into a tubular furnace for pyrolysis. The temperature is increased to 750°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature is controlled for 2h to obtain a pyrolysis product. A 0.35% hydrochloric acid solution is added for washing, filtered with a vacuum filter, and then repeatedly washed with distilled water until the pH is neutral. The modified biochar is dried in an oven at 80°C to obtain the modified biochar. The rest is the same as Example 1.

[0059] Comparative Example 6

[0060] The difference between this comparative example and Example 1 lies in the addition amount of phthalimide peroxycaproic acid solution. The specific process is as follows: corn straw powder and 1% phthalimide peroxycaproic acid solution are mixed in a ratio of 1:1 and then ground. The obtained mixture is placed in a porcelain boat and placed in a tubular furnace for pyrolysis. The temperature is raised to 750°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature is controlled for 2h to obtain a pyrolysis product. A 0.35% hydrochloric acid solution is added for washing, filtered with a vacuum filter, and then repeatedly washed with distilled water until the pH is neutral. The modified biochar is dried in an oven at 80°C to obtain the modified biochar. The rest is the same as Example 1.

[0061] Comparative Example 7

[0062] The difference between this comparative example and Example 1 is that the flocculant is sodium alginate, and the specific process is as follows: Biochar modification: corn straw powder and 5% by mass phthalimide peroxycaproic acid solution are mixed in a ratio of 1:1 and then ground, the obtained mixture is placed in a porcelain boat and placed in a tube furnace for pyrolysis, and the temperature is raised to 750°C at a heating rate of 10°C / min under a nitrogen environment, and the temperature is controlled for 2h to obtain a pyrolysis product, add a hydrochloric acid solution with a mass fraction of 0.35% to wash, filter with a vacuum filter, and then repeatedly wash with distilled water until the pH is neutral, and dry in an oven at 80°C to obtain the modified biochar;

[0063] Biochar loaded with nano-iron: Take 1.6 parts of the modified biochar mentioned above and add them to 100 parts of 4.2% FeSO4 solution by mass. Under nitrogen protection and mechanical stirring at 150r / min, add an equal volume of 2.5% NaBH4 solution at a uniform rate of 3mL / min. After the addition is completed, continue to stir the reaction for 30min, then use a magnet to separate the solid and liquid, wash the precipitate twice with ultrapure water and anhydrous ethanol respectively, and finally dry it in vacuum at 60℃ for 12h and store it for later use.

[0064] First, 3% biochar was added to the wastewater, and magnetic stirring was performed at 180r / min at room temperature. The aeration power of the electromagnetic air pump was 90W, the aeration volume was 2.8L / min, and the aeration stirring time was 45min. Then, 0.2% sodium alginate was added and aerated and stirred for 45min, and then the sludge and water were separated by air flotation through the nano water purification system.

[0065] Comparative Example 8

[0066] The difference between this comparative example and Example 1 is that the acetylhydrazine trimethylammonium chloride in the flocculant is ammonium bicarbonate; the rest is the same as Example 1.

[0067] Comparative Example 9

[0068] The difference between this comparative example and Example 1 is that the amount of acetylhydrazine trimethylammonium chloride added in the flocculant is different. The specific flocculant process is as follows: using soluble starch granules as the base material, 85 parts of starch raw materials that have passed through 40 meshes are placed in a 60°C oven for 24 hours for activation, then dissolved in water and sealed and placed in a 70°C oil bath for heating and gelatinization for 30 minutes accompanied by magnetic stirring at 150 r / min, 200 parts of a polysilicic acid solution with a mass fraction of 1.8%, 80 parts of acetylhydrazine trimethylammonium chloride, 150 r / min are added, and the mixture is stirred for 30 minutes. n magnetic stirring, then continue to drop 0.06 parts of 10% ammonium persulfate solution to initiate monomer polymerization, maintain the polymerization temperature at 50 ° C, and continue for 4 hours under the protection of nitrogen inert gas, supplement 50 parts of 1.8% polysilicic acid solution every 1 hour, the reaction is completed, and a white viscous substance is obtained, which is naturally cooled to room temperature, washed with anhydrous ethanol, and precipitated with acetone. The extracted white solid is cut into pieces, dried in a vacuum oven or a freeze drying oven at 40 ° C for 48 hours, and then ground and granulated; the rest is the same as Example 1.

[0069] Comparative Example 10

[0070] The difference between this comparative example and Example 1 is that the amount of acetylhydrazine trimethylammonium chloride added in the flocculant is different. The specific flocculant process is as follows: using soluble starch granules as the base material, 85 parts of starch raw materials that have passed through 40 meshes are placed in a 60°C oven for baking for 24 hours for activation, then dissolved in water and sealed and placed in a 70°C oil bath for heating and gelatinization for 30 minutes accompanied by magnetic stirring at 150 r / min, and then 200 parts of a polysilicic acid solution with a mass fraction of 1.8%, 10 parts of acetylhydrazine trimethylammonium chloride, and 150 r / min are added. n magnetic stirring, then continue to drop 0.06 parts of 10% ammonium persulfate solution to initiate monomer polymerization, maintain the polymerization temperature at 50 ° C, and continue for 4 hours under the protection of nitrogen inert gas, supplement 50 parts of 1.8% polysilicic acid solution every 1 hour, the reaction is completed, and a white viscous substance is obtained, which is naturally cooled to room temperature, washed with anhydrous ethanol, and precipitated with acetone. The extracted white solid is cut into pieces, dried in a vacuum oven or a freeze drying oven at 40 ° C for 48 hours, and then ground and granulated; the rest is the same as Example 1.

[0071] Test 1:

[0072] The results of various indicators in the water before and after the wastewater is tested are shown in Table 1 below.

[0073] Table 1 Removal rate results

[0074]

[0075]

[0076] The following examples are all carried out based on the following steps in Example 1.

[0077] Example 4

[0078] Preparation of complexing agent: The mass ratio of activator to fly ash is 1.4:1. The activator is obtained by dissolving 8 parts of sodium n-hexane sulfonate in a sodium silicate solution with a mass fraction of 12%. The mixed fly ash mixture is heated in a water bath at 90°C until the mixture is dry. The obtained fly ash is ground into powder and calcined in a muffle furnace at a sintering temperature of 800°C and a calcination time of 1.8h. After cooling, it is ground into powder and twice the mass of sodium silicate solution is added. The reaction temperature is 55°C and the reaction time is 2.5h. Filter and dry, add 15% of sodium polyphosphate and mix to obtain the complexing agent.

[0079] Then continue to add 5% of the complexing agent to the separated water, perform magnetic stirring at 180r / min, the aeration power of the electromagnetic air pump is 90W, the aeration volume is 2.8L / min, the aeration stirring time is 75min, and the floating sludge and water are separated by the nano water purification system, and the recovered water quality is tested.

[0080] Example 5

[0081] Preparation of complexing agent: The mass ratio of activator to fly ash is 1.2:1. The activator is obtained by dissolving 10 parts of sodium n-hexane sulfonate in a sodium silicate solution with a mass fraction of 15%. The mixed fly ash mixture is heated in a water bath at 90°C until the mixture is dry. The obtained fly ash is ground into powder and calcined in a muffle furnace at a sintering temperature of 800°C and a calcination time of 2h. After cooling, it is ground into powder, and twice the mass of sodium silicate solution is added. The reaction temperature is 60°C and the time is 3h. Filter and dry, add 10% of sodium polyphosphate and mix to obtain the complexing agent.

[0082] Then continue to add 3% of the complexing agent to the separated water, perform magnetic stirring at 200r / min, the aeration power of the electromagnetic air pump is 90W, the aeration volume is 2.8L / min, the aeration stirring time is 90min, and the floating sludge and water are separated by the nano water purification system, and the recovered water quality is tested.

[0083] Example 6

[0084] Preparation of complexing agent: The mass ratio of activator to fly ash is 1.5:1. The activator is obtained by dissolving 5 parts of sodium n-hexane sulfonate in a sodium silicate solution with a mass fraction of 10%. The mixed fly ash mixture is heated in a water bath at 90°C until the mixture is dry. The obtained fly ash is ground into powder and calcined in a muffle furnace at a sintering temperature of 800°C and a calcination time of 1.5h. After cooling, it is ground into powder, and twice the mass of sodium silicate solution is added. The reaction temperature is 50°C and the time is 2h. Filter and dry, add 20% of sodium polyphosphate and mix to obtain the complexing agent.

[0085] Then continue to add 8% of the complexing agent to the separated water, perform magnetic stirring at 150r / min, the aeration power of the electromagnetic air pump is 90W, the aeration volume is 2.8L / min, the aeration stirring time is 60min, and the floating sludge and water are separated by the nano water purification system, and the recovered water quality is tested.

[0086] Comparative Example 11

[0087] The difference between this comparative example and Example 4 is that the activator in this comparative example is a hydrochloric acid solution with a mass fraction of 12%, and the rest is the same as Example 4.

[0088] Comparative Example 12

[0089] The difference between this comparative example and Example 4 is that no activation treatment is performed in this comparative example. The specific process is: the fly ash is ground evenly, put into a muffle furnace for roasting, the sintering temperature is 800°C, the roasting time is 1.8h, and after cooling, it is ground into powder, and twice the mass of sodium silicate solution is added. The reaction temperature is 55°C and the time is 2.5h. The complexing agent is obtained by filtering and drying, and 15% of sodium polyphosphate is added and mixed. The rest is the same as Example 4.

[0090] Comparative Example 13

[0091] The difference between this comparative example and Example 4 is that the amount of sodium n-hexane sulfonate added in this comparative example is different, specifically: complexing agent preparation: activator: fly ash, the mass ratio is 1.4:1, the activator is obtained by dissolving 20 parts of sodium n-hexane sulfonate in a sodium silicate solution with a mass fraction of 12%, the mixed fly ash mixture is heated in a water bath at 90°C until the mixture is dry, the obtained fly ash is ground into powder, put into a muffle furnace and roasted at a sintering temperature of 800°C and a roasting time of 1.8h, and then ground into powder after cooling, and twice the mass of sodium silicate solution is added, the reaction temperature is 55°C, the time is 2.5h, filtered and dried, and 15% of sodium polyphosphate is added to obtain the complexing agent; the rest is the same as Example 4.

[0092] Comparative Example 14

[0093] The difference between this comparative example and Example 4 is that the amount of sodium n-hexane sulfonate added in this comparative example is different, specifically: complexing agent preparation: activator: fly ash, the mass ratio is 1.4:1, the activator is obtained by dissolving 2 parts of sodium n-hexane sulfonate in a sodium silicate solution with a mass fraction of 12%, the mixed fly ash mixture is heated in a water bath at 90°C until the mixture is dry, the obtained fly ash is ground into powder, put into a muffle furnace and roasted at a sintering temperature of 800°C and a roasting time of 1.8h, and then ground into powder after cooling, and twice the mass of sodium silicate solution is added, the reaction temperature is 55°C, the time is 2.5h, filtered and dried, and 15% of sodium polyphosphate is added to obtain the complexing agent; the rest is the same as Example 4.

[0094] Test 2: Ion removal rate

[0095] Ion removal rate refers to the percentage of ion concentration removed after treatment to the ion concentration in the original solution before treatment. Its size reflects the precipitation effect of the precipitant and the treatment effect under the best experimental conditions. Its definition is:

[0096] Where: R-ion removal rate, %;

[0097] Co and C- are the mass concentrations of a certain ion in the solution before and after treatment, mg / L

[0098] Determination of Ca in the supernatant of wastewater before and after treatment with complexing agent 2+ ,Mg 2+ The concentrations before and after in wastewater are shown in Table 2.

[0099] Table 2 Ion removal rate

[0100] Group Calcium ion removal rate (%) Magnesium ion removal rate (%) Example 4 99.5 98.8 Example 5 99.4 98.5 Example 6 99.2 98.2 Comparative Example 11 60.8 65.2 Comparative Example 12 85.4 86.9 Comparative Example 13 95.2 94.5 Comparative Example 14 90.7 89.6

[0101] Test 3: Water recovery standards

[0102] The water quality of Examples 1-3 was measured to see if it met the requirements of the "Water Quality for Industrial Water Use in Urban Wastewater Reclamation"

[0103] (GB / T19923-2005) standard, the results are shown in Table 3:

[0104]

[0105]

Claims

1. A process for removing calcium and magnesium ions from wastewater for water quality reuse, characterized in that: The processing method specifically comprises the following steps: First, add 0.2-0.4% of decalcifier to the raw water, perform aeration and stirring in the reaction barrel, the aeration volume is 2.8L / min, the stirring speed is 150-200r / min, add 0.4-0.8% of magnesium remover after stirring for 20min, continue aeration and stirring for 20min, then add 0.1-0.3% of flocculant, perform aeration and stirring for 30-60min, and separate the floating mud and water through the nano water purification system; then continue to add 3-8% of complexing agent to the separated water, perform magnetic stirring at 150-200r / min, the aeration power of the electromagnetic air pump is 90W, the aeration volume is 2.8L / min, the aeration stirring time is 60-90min, the floating mud and water are separated through the nano water purification system, and the recovered water quality meets the reuse standard; The complexing agent is an activator: fly ash with a mass ratio of 1.2-1.5:

1. The mixture is heated in a water bath at 90°C until it is dry. The obtained fly ash is ground into powder, put into a muffle furnace for roasting, the sintering temperature is 800°C, the roasting time is 1.5-2h, and after cooling, it is ground into powder. Two times the mass of sodium silicate solution is added. The reaction temperature is 50-60°C, the time is 2-3h, and the complexing agent is obtained by filtering and drying, and 10-20% of sodium polyphosphate is added and mixed.

2. A process for removing calcium and magnesium ions from wastewater for water quality reuse according to claim 1, characterized in that: The activator is obtained by dissolving 5-10 parts of sodium n-hexane sulfonate in a sodium silicate solution with a mass fraction of 10-15%.

3. A process for removing calcium and magnesium ions from wastewater for water quality reuse according to claim 1, characterized in that: After adding the magnesium removal agent for aeration and stirring, 1-5% of the adsorbent is also added. At room temperature, magnetic stirring is performed at 150-200r / min, the aeration power of the electromagnetic air pump is 90W, the aeration volume is 2.8L / min, and the aeration stirring time is 30-60min. Thereafter, flocculant is added for treatment and the sludge and water are separated by air flotation through the nano water purification integrated machine system.

4. A process for removing calcium and magnesium ions from wastewater for water quality reuse according to claim 3, characterized in that: The adsorbent is biochar, and the biochar also includes a modification process: corn stalk powder and acidic oxygen-containing acid solution are mixed evenly according to a ratio of 1:0.8-1.2 and then ground, the obtained mixture is placed in a porcelain boat and placed in a tube furnace for pyrolysis, the temperature is increased to 700-800°C at a heating rate of 10°C / min in a nitrogen environment, and the temperature is controlled for 2 hours to obtain a pyrolysis product, add a hydrochloric acid solution with a mass fraction of 0.35% for washing, filter with a vacuum filter, and then repeatedly wash with distilled water until the pH is neutral, and put it in an oven at 80°C for drying to obtain the modified biochar; The acidic oxygen-containing acid is a phthalimide peroxycaproic acid solution with a mass fraction of 3-6%.

5. A process for removing calcium and magnesium ions from wastewater for water quality reuse according to claim 4, characterized in that: The modified biochar also includes the process of loading nano-iron: take 1.4-1.8 parts of the above modified biochar and add it to 100 parts of FeSO4 solution with a mass fraction of 3.8-4.5%, and under nitrogen protection and mechanical stirring at 150r / min, add an equal volume of NaBH4 solution with a mass fraction of 2.5% at a uniform rate, and the dropping speed is 3mL / min. After the addition is completed, continue to stir the reaction for 30 minutes, then use a magnet to separate the solid and liquid, wash the precipitate with ultrapure water and anhydrous ethanol twice each, and finally dry it in vacuum at 60°C for 12 hours and store it for later use.

6. A process for removing calcium and magnesium ions from wastewater for water quality reuse according to claim 1, characterized in that: The flocculant is based on soluble starch particles. 70-100 parts of starch raw materials that have passed through 40 meshes are placed in a 60°C oven for baking for 24 hours for activation. After being dissolved in water, the raw materials are sealed and placed in an oil bath at 60-80°C for heating and gelatinization for 30 minutes while being stirred with a magnetic force of 150 r / min. Then, 200 parts of a polysilicic acid solution with a mass fraction of 1.5-2% and 30-50 parts of a flocculant monomer are added. The mixture is stirred with a magnetic force of 150 r / min. Then, 0.02 -0.08 parts of 10% ammonium persulfate solution by mass to initiate monomer polymerization, maintain the polymerization temperature at 48-52°C, and continue for 4 hours under the protection of nitrogen inert gas, supplement 50 parts of 1.5-2% polysilicic acid solution by mass every 1 hour, and the reaction is completed to obtain a white viscous substance, which is naturally cooled to room temperature and then washed with anhydrous ethanol and precipitated with acetone. The extracted white solid is cut into pieces, dried in a vacuum oven or a freeze drying oven at 40°C for 48 hours, and then ground into granules.

7. A process for removing calcium and magnesium ions from wastewater for water reuse according to claim 6, characterized in that: The flocculant monomer is acetylhydrazine trimethylammonium chloride.

Citation Information

Patent Citations

  • Method for preparing solid-state efficient flocculant by using coal ash as raw material

    CN104724737A

  • Method for preparing polyaluminum ferric silicate composite coagulant from coal ash

    CN108609711A

  • Biochar / polyaluminum chloride composite adsorbent

    CN117861621A

  • Dosing unit for washing or cleaning agents

    WO2006066721A1

  • Enhanced coagulation method for removing micro-plastics in water

    WO2022236964A1

Cited By

  • Aluminosilicate solid waste heavy metal adsorbent as well as preparation method and application thereof

    CN120132801A

  • Treatment method of ammonia-nitrogen-containing wastewater

    CN120698642A

  • Composite flocculant for adsorbing, flocculating and settling Ca < 2 + > in water body and method for removing high-concentration Ca < 2 + > in wastewater by using composite flocculant

    CN121005444A

  • Adsorption, flocculation and sedimentation of Ca in water bodies 2+ Composite flocculants and their application in removing high concentrations of Ca from wastewater 2+ Method

    CN121005444B