A method for comprehensive utilization of isopropylidene acetone byproducts

By using the thiolized strong acidic cationic resin WX-1 catalyst, a continuous reaction was carried out in a tubular reactor to convert the isopropylidene acetone byproduct 4-methyl-4-penten-2-one into isopropylidene acetone, solving the byproduct treatment problem, improving the reaction yield and selectivity, and simplifying the process.

CN118878403BActive Publication Date: 2026-11-17江苏宏邦化工科技有限公司
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202410776057.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-06-17
Publication Date
2026-11-17
Estimated Expiration
2044-06-17

AI Technical Summary

Technical Problem

The formation of 4-methyl-4-penten-2-one as a byproduct in the current isopropylidene acetone production process leads to a decrease in reaction yield and difficulty in purification.

Method used

Using thiolized strong acidic cationic resin WX-1 as a catalyst, a continuous reaction is carried out in a tubular reactor to convert low-grade isopropylidene acetone byproducts into isopropylidene acetone. By controlling the reaction temperature, pressure, and residence time, a highly selective conversion is achieved.

Benefits of technology

It improves the selectivity and yield of isopropylidene acetone, simplifies the process, avoids solvent use and wastewater generation, and has good prospects for industrial application.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

This invention belongs to the field of fragrance production technology, specifically disclosing a method for the comprehensive utilization of isopropylidene acetone byproducts, comprising the following steps: using low-grade isopropylidene acetone as raw material and thiolized strong acidic cationic resin WX-1 as catalyst, isopropylidene acetone is prepared by continuous reaction in a tubular reactor; the low-grade isopropylidene acetone is derived from the byproducts obtained in the preparation of isopropylidene acetone, wherein the GC content of isopropylidene acetone is 20-80%, and the GC content of 4-methyl-4-penten-2-one is 5-75%. The method of this invention is simple, does not use solvents, generates no wastewater, has good reactivity and high selectivity, and has good prospects for industrial application.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of fragrance production technology, and relates to the synthesis of isopropylidene acetone, and particularly to a method for the comprehensive utilization of by-products in the production process of isopropylidene acetone. Background Technology

[0002] Isopropylidene acetone, also known as 4-methyl-3-penten-2-one, is a colorless, transparent, oily, flammable liquid with a strong minty or honey-like odor. It is a strong medium-boiling-point solvent used as a solvent for nitrocellulose and various resins, especially vinyl resins, as well as for paints. In fragrance production, it is primarily used as an important intermediate for products such as isophorone.

[0003] The industrial production process of isopropylidene acetone is generally a two-step process. In the presence of an alkaline catalyst, acetone first undergoes Aldol reaction to produce diacetone alcohol, which is then dehydrated to produce isopropylidene acetone.

[0004]

[0005] Chinese patent CN103772175A discloses a method for simultaneously synthesizing isopropylidene acetone and sec-butanol. The method employs a fixed-bed reactor with a solid acid as a catalyst, where the two reactions occur simultaneously. First, two molecules of acetone undergo a condensation reaction to produce isopropylidene acetone and water. The byproduct water then undergoes an addition reaction with n-butene to yield sec-butanol. The selectivity for isopropylidene acetone is 97%. To ensure the conversion rate of acetone, the condensation reaction requires high pressure conditions of 3-10 MPa, placing high demands on the equipment.

[0006] US patents US5292980A, US patent US08697924B2, and US patent 2013 / 0185922A1 disclose the synthesis of diacetone alcohol and isopropylidene acetone from acetone using a multiphase aluminosilicate catalyst at high temperatures (>100°C).

[0007] However, the above-mentioned processes for synthesizing isopropylidene acetone all generate the byproduct 4-methyl-4-penten-2-one, which leads to a decrease in reaction yield and makes it difficult to purify the isopropylidene acetone product. Summary of the Invention

[0008] To address the shortcomings of existing technologies, the present invention aims to provide a comprehensive utilization method for isopropylidene acetone byproducts containing 4-methyl-4-penten-2-one, thereby achieving comprehensive utilization of isopropylidene acetone byproducts and having high industrial application value.

[0009] This invention is achieved through the following technical solution: A method for the comprehensive utilization of isopropylidene acetone byproducts includes the following steps: Isopropylidene acetone is prepared by continuous reaction in a tubular reactor using low-grade isopropylidene acetone as raw material and thiolized strong acid cation exchange resin WX-1 as catalyst. The low-grade isopropylidene acetone is derived from a byproduct of isopropylidene acetone preparation, wherein the GC content of isopropylidene acetone is 20-80% and the GC content of 4-methyl-4-penten-2-one is 5-75%.

[0010] The reaction equation is shown below:

[0011] A further improvement to the present invention is as follows: The tubular reactor consists of a feed pump, a reaction section, and a cooling section. The residence time of the material in the tubular reactor is controlled by controlling the flow rate of the feed pump. The reaction section is made of a 4m long stainless steel tube with an inner diameter of 8mm, filled with a cationic resin catalyst (WX-1), and the reaction temperature is controlled by an oil bath. The cooling section is also made of a 4m long stainless steel tube with an inner diameter of 8mm. A back pressure valve at the tail end is used to control the reaction pressure. The liquid at the outlet of the back pressure valve is collected for analysis.

[0012] The amount of the mercapto-modified strong acidic cationic resin WX-1 is 55~75g.

[0013] The continuous reaction is carried out at a temperature of 50-100℃, with a residence time of 30-120 min in the reactor and a reaction pressure of 0.1-0.2 MPa.

[0014] The cationic resin catalyst WX-1 contains sulfonated styrene-divinylbenzene copolymer with an exchange capacity of 2.8-5.5 mg equivalences / g dry resin. 10-30% of its sulfonic acid groups are bonded to alkyl mercaptoamines with 1-7 carbon atoms via ammonium sulfonate ionic bonds. The structural diagram is shown below:

[0015] The beneficial effects of this invention are as follows: Using thiolized strong acidic cationic resin WX-1 as a catalyst and low-grade isopropylidene acetone byproducts from the synthesis of isopropylidene acetone as raw materials, the byproduct 4-methyl-4-penten-2-one is converted into the target product isopropylidene acetone with high selectivity. The method of this invention is simple, does not use solvents, generates no wastewater, has good reactivity and high selectivity, and has good prospects for industrial application. Detailed Implementation

[0016] The present invention will now be described in detail with reference to specific embodiments.

[0017] Example 1: Preparation of thiolized strong acid cation exchange resin WX-1 (1) Preparation of white balls: 880g of 1% polyvinyl alcohol aqueous solution was added to a 2L glass reactor as a dispersant, and a mixture of NY-200# solvent oil and refined paraffin (melting point 54~62℃) was added as a pore-forming agent. The weight ratio of paraffin to solvent oil was 3~6.1, and the amount added was 60g. 200g of styrene, 18g of divinylbenzene, and 2g of benzoyl peroxide were added. The suspension polymerization reaction was carried out at 82±2℃ for 6h under stirring, and then reacted at 90℃ for another 6h. The product was discharged, washed with water, and dried.

[0018] (2) Sulfonation: The white spheres were extracted with benzene in a Soxhlet extractor until no paraffin was found in the extract. 200g of white spheres, 100g of dichloroethane, and 1400g of 98% sulfuric acid were added to a 2L three-necked flask. The mixture was kept at 70°C with stirring for 2 hours, then heated to 80°C and kept at that temperature for another 6 hours. After the reaction was complete, the dichloroethane was distilled off at atmospheric pressure, and the mixture was allowed to continue reacting at 110-120°C for 2 hours. The residual acid was washed with distilled water and ethanol when the mixture was cooled to room temperature until the effluent was neutral. The sulfonated resin was then air-dried at room temperature for later use.

[0019] (3) Thiolization: The thiolation agent solvent was prepared according to the weight ratio of dry resin: mercaptoethylamine hydrochloride: hydrochloric acid: water = 1:0.1:0.1:2. The resin was immersed in the above solution at room temperature and allowed to stand for 36 hours. Then it was washed with distilled water and ethanol in sequence until the effluent was neutral. After filtration, it was dried at 80°C for 6 hours and vacuum dried at 72°C for 12 hours to obtain catalyst WX-1.

[0020] Example 2: Comprehensive utilization of isopropylidene acetone byproducts The experiment was conducted in a stainless steel tube reactor with a length of 4 m and an inner diameter of 8 mm. The catalyst was a self-made strong acid cation exchange resin WX-1, with a loading of 64 g. The reaction temperature was 70 °C, and the residence time of low-grade isopropylidene acetone (isopropylidene acetone GC content of 20% and 4-methyl-4-penten-2-one GC content of 71%) in the reaction section was 90 min. The reaction pressure was 0.15 MPa. After the reaction, the products were qualitatively and quantitatively analyzed by gas chromatography. The analysis showed that the isopropylidene acetone GC content in the reaction liquid at the reactor outlet was 78.5%, and the 4-methyl-4-penten-2-one GC content was 12.1%. The selectivity and yield data are shown in Table 1.

[0021] Example 3: Comprehensive utilization of isopropylidene acetone byproducts The experiment was conducted in a 4m long stainless steel tube reactor with an inner diameter of 8mm. The catalyst was a self-made strong acid cation exchange resin WX-1, with a loading of 64g. The reaction temperature was 80℃, and the residence time of low-grade isopropylidene acetone (20% GC content of isopropylidene acetone and 71% GC content of 4-methyl-4-penten-2-one) in the reaction section was 90min. The reaction pressure was 0.15MPa. After the reaction, the products were qualitatively and quantitatively analyzed by gas chromatography. The analysis showed that the GC content of isopropylidene acetone in the reaction liquid at the reactor outlet was 87.5%, and the GC content of 4-methyl-4-penten-2-one was 3.4%. The selectivity and yield data are shown in Table 1.

[0022] Example 4: Comprehensive utilization of isopropylidene acetone byproducts The experiment was conducted in a 4m long stainless steel tube reactor with an inner diameter of 8mm. The catalyst was a self-made strong acid cation exchange resin WX-1, with a loading of 64g. The reaction temperature was 90℃, and the residence time of low-grade isopropylidene acetone (20% GC content of isopropylidene acetone and 71% GC content of 4-methyl-4-penten-2-one) in the reaction section was 90min. The reaction pressure was 0.15MPa. After the reaction, the products were qualitatively and quantitatively analyzed by gas chromatography. The analysis showed that the GC content of isopropylidene acetone in the reaction liquid at the reactor outlet was 88.6%, and the GC content of 4-methyl-4-penten-2-one was 2.3%. The selectivity and yield data are shown in Table 1.

[0023] Example 5: Comprehensive utilization of isopropylidene acetone byproducts The synthesis of isopropylidene acetone was carried out in a 4m long, 8mm inner diameter stainless steel tube reactor. The catalyst was a self-made strong acid cation exchange resin, WX-1, with a loading of 64g. The reaction temperature was 80℃. The residence time of the low-grade isopropylidene acetone (77% GC content of isopropylidene acetone and 16% GC content of 4-methyl-4-penten-2-one) in the reaction section was 60min, and the reaction pressure was 0.15MPa. After the reaction, the products were qualitatively and quantitatively analyzed by gas chromatography. The analysis showed that the GC content of isopropylidene acetone in the reactor outlet reaction liquid was 91.2%, and the GC content of 4-methyl-4-penten-2-one was 1.8%. Selectivity and yield data are shown in Table 1.

[0024] Example 6: Comprehensive utilization of isopropylidene acetone byproducts The synthesis of isopropylidene acetone was carried out in a 4m long, 8mm inner diameter stainless steel tube reactor. The catalyst was a self-made strong acid cation exchange resin, WX-1, with a loading of 66g. The reaction temperature was 80℃. The residence time of the low-grade isopropylidene acetone (44% GC content of isopropylidene acetone and 52% GC content of 4-methyl-4-penten-2-one) in the reaction section was 60 min, and the reaction pressure was 0.15 MPa. After the reaction, the products were qualitatively and quantitatively analyzed by gas chromatography. The analysis showed that the GC content of isopropylidene acetone in the reactor outlet reaction liquid was 92.5%, and the GC content of 4-methyl-4-penten-2-one was 3.4%. Selectivity and yield data are shown in Table 1.

[0025] To demonstrate the reaction characteristics of the catalyst provided by this invention in the isopropylideneacetone isomerization of low-grade isopropylideneacetone (isopropylideneacetone GC content of 44% and 4-methyl-4-penten-2-one GC content of 52%), three other commercially available sulfonic acid-based strong acid cation exchange resin catalysts (D072, NKC-9 and Amberlyst15) were measured in parallel under the same conditions.

[0026] Comparative Example 1 The synthesis of isopropylidene acetone was carried out in a 4m long, 8mm inner diameter stainless steel tube reactor. The catalyst was D072 type strong acidic cationic resin, with a loading of 66g. The reaction temperature was 80℃, and the residence time of the low-grade isopropylidene acetone (isopropylidene acetone GC content 44%, 4-methyl-4-penten-2-one GC content 52%) in the reaction section was 60min. The reaction pressure was 0.15MPa. After the reaction, the products were qualitatively and quantitatively analyzed by gas chromatography. The analysis showed that the isopropylidene acetone GC content in the reactor outlet reaction liquid was 79.5%, and the 4-methyl-4-penten-2-one GC content was 14.9%. Selectivity and yield data are shown in Table 1.

[0027] Comparative Example 2 The synthesis of isopropylidene acetone was carried out in a 4m long, 8mm inner diameter stainless steel tube reactor. The catalyst was NKC-9 type strong acidic cationic resin, with a loading of 70g. The reaction temperature was 80℃. The residence time of the low-grade isopropylidene acetone (44% GC content of isopropylidene acetone and 52% GC content of 4-methyl-4-penten-2-one) in the reaction section was 60min, and the reaction pressure was 0.15MPa. After the reaction, the products were qualitatively and quantitatively analyzed by gas chromatography. The analysis showed that the GC content of isopropylidene acetone in the reactor outlet reaction liquid was 84.3%, and the GC content of 4-methyl-4-penten-2-one was 11.0%. Selectivity and yield data are shown in Table 1.

[0028] Comparative Example 3 The synthesis of isopropylidene acetone was carried out in a 4m long, 8mm inner diameter stainless steel tube reactor. The catalyst was Amberlyst 15 strong acidic cationic resin, with a loading of 60g. The reaction temperature was 80℃. The residence time of the low-grade isopropylidene acetone (44% GC content of isopropylidene acetone and 52% GC content of 4-methyl-4-penten-2-one) in the reaction section was 60min, and the reaction pressure was 0.15MPa. After the reaction, the products were qualitatively and quantitatively analyzed by gas chromatography. The analysis showed that the GC content of isopropylidene acetone in the reactor outlet reaction liquid was 82.3%, and the GC content of 4-methyl-4-penten-2-one was 12.5%. Selectivity and yield data are shown in Table 1.

[0029] Table 1. Reaction results of Examples 2-6 and Comparative Examples 1-3 Reaction parameters Example 2 Example 3 Example 4 Example 5 Example 6 Comparative Example 1 Comparative Example 2 Comparative Example 3 Catalyst types WX-1 WX-1 WX-1 WX-1 WX-1 D072 NKC-9 Amberlyst15 Reaction temperature / ℃ 70 80 90 80 80 80 80 80 Dwell time / min 90 90 90 60 60 60 60 60 Reaction pressure / MPa 0.15 0.15 0.15 0.15 0.15 0.15 0.15 0.15 Yield / % 82.4 95.1 96.6 88.7 93.2 68.3 77.5 73.7 Selectivity / % 96.7 96.9 96.4 97.0 96.6 90.5 93.6 91.4 The above embodiments are only for illustrating the technical concept and features of the present invention, and are intended to enable those skilled in the art to understand the content of the present invention and implement it accordingly. They should not be construed as limiting the scope of protection of the present invention. All equivalent transformations or modifications made in accordance with the spirit and essence of the present invention should be covered within the scope of protection of the present invention.

Claims

1. A method for the comprehensive utilization of isopropylidene acetone byproducts, characterized in that, Includes the following steps: Isopropylidene acetone is prepared by a continuous reaction in a tubular reactor using low-grade isopropylidene acetone as raw material and WX-1 thiolized strong acidic cation exchange resin as catalyst. The low-grade isopropylidene acetone is derived from a byproduct of isopropylidene acetone preparation, wherein the isopropylidene acetone GC content is 20-80% and the 4-methyl-4-penten-2-one GC content is 5-75%. The preparation process of the mercapto-modified strong acid cationic resin WX-1 is as follows: (1) Preparation of white balls: 880g of 1% polyvinyl alcohol aqueous solution was added to a 2L glass reactor as a dispersant, and a mixture of NY-200# solvent oil and refined paraffin with a melting point of 54~62℃ was added as a pore-forming agent. The weight ratio of paraffin to solvent oil was 3~6.1, and the amount added was 60g. 200g of styrene, 18g of divinylbenzene, and 2g of benzoyl peroxide were added. The suspension polymerization reaction was carried out at 82±2℃ for 6h under stirring, and then reacted at 90℃ for another 6h. The product was discharged, washed with water, and dried. (2) Sulfonation: The white spheres were extracted with benzene in a Soxhlet extractor until no paraffin was found in the extract. 200g of white spheres, 100g of dichloroethane and 1400g of 98% sulfuric acid were added to a 2L three-necked flask. The mixture was kept at 70°C and stirred for 2 hours. The temperature was raised to 80°C and the mixture was kept at 80°C for 6 hours. After the reaction was completed, the dichloroethane was distilled off at atmospheric pressure and the mixture was kept at 110~120°C for 2 hours. When the temperature was lowered to room temperature, the residual acid was washed with distilled water and ethanol until the effluent was neutral. The sulfonated resin was dried at room temperature for later use. (3) Thiolization: The thiolation agent solvent was prepared according to the weight ratio of dry resin: mercaptoethylamine hydrochloride: hydrochloric acid: water = 1:0.1:0.1:

2. The resin was immersed in the above solution at room temperature and allowed to stand for 36 hours. Then it was washed with distilled water and ethanol in sequence until the effluent was neutral. After filtration, it was dried at 80°C for 6 hours and vacuum dried at 72°C for 12 hours to obtain catalyst WX-1.

2. The method for comprehensive utilization of isopropylidene acetone byproducts according to claim 1, characterized in that: The tubular reactor consists of a feed pump, a reaction section, and a cooling section. The reaction section is made of a stainless steel tube that is 4m long and has an inner diameter of 8mm.

3. The method for comprehensive utilization of isopropylidene acetone byproducts according to claim 1, characterized in that: The loading amount of the mercapto-modified strong acidic cationic resin WX-1 is 55~75g.

4. A method for comprehensive utilization of isopropylidene acetone byproducts according to claim 1, characterized in that: The continuous reaction is carried out at a temperature of 50-100℃, with a residence time of 30-120 min in the reactor and a reaction pressure of 0.1-0.2 MPa.

Citation Information

Patent Citations

  • Combined technique for synthesizing iso-propylidene acetone and sec-butyl alcohol

    CN103772175A

  • Electrosurgical Instrument And Method Of Manufacturing The Same

    US20130185922A1

  • Base-catalyzed reactions using zeolite catalysts

    US5292980A

  • Liquid fuel compositions

    US8697924B2

  • Ion exchange resin catalyzer for synthesising bisphenol and preparation thereof

    CN1121442A