Method for simulating reflow soldering temperature curve, PCB (printed circuit board) and IC (integrated circuit) board warping measurement method

By simulating the reflow soldering temperature curve, the heat deformation tester is used to adjust the parameters of the heater and exhaust port, and combined with the PID algorithm, the problem of inaccurate measurement of the warpage of PCB and IC boards in the existing technology is solved, and the reflow is achieved 焊温度曲线下的准确拟合和精确测量,提高了焊接质量。

CN118882579APending Publication Date: 2024-11-01SHANGHAI MEADVILLE SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411057743.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The prior art cannot accurately obtain the warpage values ​​of PCB boards and IC boards under the reflow temperature curve, resulting in poor solder joints and false solder joints.

Method used

By simulating the reflow soldering temperature curve, the temperature segment and system gain K value range are set using a thermal deformation tester, the heater power and exhaust air volume are adjusted, the system gain K is calculated in combination with the PID algorithm, and the temperature and warpage value are recorded in real time. , fit the functional relationship between temperature and warpage value to achieve accurate measurement of warpage.

Benefits of technology

It realizes accurate fitting of the welding temperature curve and precise measurement of warping under the reflow soldering temperature curve, improving welding accuracy, and being convenient, efficient and reusable.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118882579A_ABST
    Figure CN118882579A_ABST
Patent Text Reader

Abstract

The invention provides a method for simulating a reflow soldering temperature curve and a method for measuring warpage of a PCB (Printed Circuit Board) and an IC (Integrated Circuit) board. The method comprises the following steps of: placing a first sample and a second sample in a thermal deformation tester; presetting each temperature section of the thermal deformation tester and a system gain K value range according to the reflow soldering temperature curve; preheating the thermal deformation tester and adjusting the air volume of an air outlet of the thermal deformation tester; adjusting the air volume of an air outlet of the thermal deformation tester and the maximum power of a bottom heater at the heating section, the constant temperature section and the cooling section to enable the actual system gain K of the thermal deformation tester to be within a preset system gain K value range; and recording the real-time temperature of the first sample and the warping value of the second sample in the heating section, the constant-temperature section and the cooling section. Finally, the function relation between the temperature and the warping value under the reflow soldering temperature curve can be obtained, and under the function relation, the warping value of the PCB and the warping value of the IC board under the corresponding temperature can be accurately measured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electronic device welding, and in particular to a method for simulating a reflow soldering temperature curve, and a method for measuring the warpage of a PCB board and an IC board. Background Art

[0002] Printed Circuit Board, also known as PCB (Printed Circuit Board), is a carrier for the electrical connection between electronic components. Package substrate, also known as IC carrier, provides support, protection and heat dissipation for the chip, and at the same time, the package substrate provides electronic connection between the chip and PCB. In the production process of PCB and package substrate, reflow soldering is an indispensable procedure. Reflow soldering can be used to solder electronic components, PCB and package substrate. However, due to the influence of temperature, PCB and package substrate will warp during the soldering process, which will cause problems such as poor solder joints, cold solder joints, and overall deformation of the board surface.

[0003] In order to solve the warpage defect of reflow soldering, it is necessary to measure the warpage value of PCB and IC boards at different temperatures. The existing technology usually adopts the following two methods to solve it: board bending measurement technology such as bow and twist, and projection ripple technology. Among them, projection ripple technology can simulate the reflow soldering process and capture the historical warpage data of PCB and IC boards by using full-view optics. However, the board bending measurement technology such as bow and twist has the problem of too low accuracy, and the projection ripple technology has the problem of not being able to accurately obtain the reflow soldering temperature curve.

[0004] Therefore, how to design a method for accurately obtaining the warpage value of a PCB board and an IC board under a reflow soldering temperature curve has become one of the problems that technicians in this field need to solve urgently.

[0005] It should be noted that the above introduction to the technical background is only for the convenience of providing a clear and complete description of the technical solutions of the present invention and for the convenience of understanding by those skilled in the art. It cannot be considered that the above technical solutions are well known to those skilled in the art simply because these solutions are described in the background technology section of the present invention. Summary of the invention

[0006] In view of the shortcomings of the prior art described above, an object of the present invention is to provide a method for simulating a reflow soldering temperature curve and a method for measuring the warpage of a PCB board and an IC board, so as to solve the problem in the prior art that the warpage of a PCB board and an IC board cannot be accurately obtained under a reflow soldering temperature curve.

[0007] To achieve the above object and other related objects, the present invention provides a method for simulating a reflow soldering temperature curve, which at least comprises the following steps:

[0008] S1: placing the first sample and the second sample in a thermal deformation tester;

[0009] S2: Presetting each temperature segment of the thermal deformation tester and a numerical range of a system gain K of the thermal deformation tester according to a reflow soldering temperature curve;

[0010] S3: setting the maximum power of the bottom heater of the thermal deformation tester and the air volume of the exhaust port of the thermal deformation tester to preheat the thermal deformation tester;

[0011] S4: After the preheating is completed, the temperature of the thermal deformation tester is continued to be increased so that the thermal deformation tester enters the heating stage, and the system gain K of the heating stage is calculated by using the PID algorithm, wherein the transfer function of the PID algorithm is a first-order mathematical model; the maximum power and the air volume at the exhaust port are adjusted so that the system gain K of the heating stage is within the range of the preset system gain K; the real-time temperature of the first sample and the real-time warpage value of the second sample are recorded;

[0012] S5: maintaining the temperature of the thermal deformation tester so that the thermal deformation tester enters a constant temperature section, adjusting the maximum power and the air volume of the exhaust port so that the cavity temperature of the thermal deformation tester remains constant; recording the real-time temperature of the first sample and the real-time warpage value of the second sample;

[0013] S6: lowering the temperature of the thermal deformation tester so that the thermal deformation tester enters a cooling stage, and using the PID algorithm to calculate the system gain K of the cooling stage; adjusting the maximum power and the air volume at the exhaust port so that the system gain K of the cooling stage is within a preset range of the system gain K; and recording the real-time temperature of the first sample and the real-time warpage value of the second sample;

[0014] Among them, the exhaust air volume of the temperature rising section is greater than the exhaust air volume of the constant temperature section, and the exhaust air volume of the constant temperature section is not greater than the exhaust air volume of the temperature dropping section; the maximum power of the temperature rising section is not less than the maximum power of the constant temperature section, and the maximum power of the constant temperature section is not less than the maximum power of the temperature dropping section.

[0015] Optionally, before preheating the thermal deformation tester, the temperature setting point of the top heater of the thermal deformation tester is matched with the temperature setting point of the system configuration of the thermal deformation tester.

[0016] Optionally, the loading platform of the thermal deformation tester is removed to improve the thermal conductivity efficiency of the thermal deformation tester to the first sample and the second sample.

[0017] Optionally, the first sample is placed at the center of the cavity of the thermal deformation tester, the first sample and the second sample are placed in the same plane, and the distance between the first sample and the second sample is set to 5mm-200mm.

[0018] Optionally, the calculation formula of the system gain K satisfies:

[0019]

[0020] Among them, y1 is the temperature when the thermal deformation tester reaches the starting end point of each temperature segment, y2 is the temperature when the thermal deformation tester reaches the ending end point of each temperature segment, x1 is the time when the thermal deformation tester reaches the starting end point of each temperature segment, x2 is the time when the thermal deformation tester reaches the ending end point of each temperature segment, τ is the system response time of each temperature segment of the thermal deformation tester, and b is the room temperature of the thermal deformation tester.

[0021] Optionally, in the preheating section, the air volume at the exhaust port is set to 1 / 10 to 1 / 3 of the full air volume.

[0022] Optionally, the temperature of the constant temperature section is preset to 98% to 102% of the maximum reflow temperature; in the constant temperature section, the maximum power is 30% to 90% of the full power; in the constant temperature section, the exhaust air volume is set to 1 / 20 to 1 / 10 of the full air volume.

[0023] Optionally, the temperature rising section is divided into a first temperature rising section and a second temperature rising section, and the temperature change slope of the first temperature rising section is greater than the temperature change slope of the second temperature rising section.

[0024] More optionally, the temperature of the starting end point of the first temperature rising section is preset to 10% to 15% of the maximum reflow temperature, the temperature of the junction end point of the first temperature rising section and the second temperature rising section is preset to 87% to 90% of the maximum reflow temperature, and the temperature of the junction end point of the second temperature rising section and the constant temperature section is preset to 98% to 102% of the maximum reflow temperature.

[0025] More optionally, in the first temperature rising section, the maximum power is 30% to 100% of the full power; in the second temperature rising section, the maximum power is 30% to 90% of the full power.

[0026] More optionally, in the first temperature rise section, the air volume at the exhaust outlet is set to 1 / 10 to 1 / 4 of the full air volume; in the second temperature rise section, the air volume at the exhaust outlet is set to 1 / 4 to 1 / 2 of the full air volume.

[0027] Optionally, the temperature reduction section is divided into a first temperature reduction section and a second temperature reduction section, and the temperature change slope of the first temperature reduction section is smaller than the temperature change slope of the second temperature reduction section.

[0028] More optionally, the temperature of the junction end point of the constant temperature section and the first temperature reduction section is preset to 98% to 102% of the maximum reflow soldering temperature, the temperature of the junction end point of the first temperature reduction section and the second temperature reduction section is preset to 87% to 90% of the maximum reflow soldering temperature, and the temperature of the terminal end point of the second temperature reduction section is preset to 56% to 60% of the maximum reflow soldering temperature.

[0029] More optionally, in the first temperature reduction section, the maximum power is 20% to 90% of the full power; in the second temperature reduction section, the maximum power is 10% to 80% of the full power.

[0030] More optionally, in the first cooling section, the air volume at the exhaust outlet is set to 1 / 10 to 1 / 3 of the full air volume; in the second cooling section, the air volume at the exhaust outlet is set to 1 / 5 to the full air volume.

[0031] To achieve the above-mentioned object and other related objects, the present invention further provides a method for measuring the warpage of a PCB board and an IC board, and the method for measuring the warpage of a PCB board and an IC board at least comprises the following steps:

[0032] S1': using the method of simulating the reflow soldering temperature curve to obtain the real-time warpage value corresponding to the real-time temperature of each temperature section, and fitting the functional relationship between the temperature and the warpage value under the reflow soldering temperature curve;

[0033] S2': Under the reflow process, based on the functional relationship between temperature and warpage value, the warpage value of the PCB board and the IC board is obtained through the real-time temperature.

[0034] As described above, the method for simulating the reflow soldering temperature curve and the method for measuring the warpage of a PCB board and an IC board of the present invention have the following beneficial effects:

[0035] The present invention first sets each temperature segment of the thermal deformation tester and the system gain K value range of the thermal deformation tester according to the reflow soldering temperature curve; by adjusting the relevant parameters of the thermal deformation tester, the actual system gain K value of each temperature segment of the thermal deformation tester is within the preset system gain K value range, thereby achieving the purpose of accurately fitting the reflow soldering temperature curve and collecting the warpage value in real time. Therefore, the present invention achieves the goal of accurately fitting the reflow soldering temperature curve while accurately measuring the warpage, and the present invention has the advantages of convenience, high efficiency and high reusability.

[0036] Furthermore, based on the functional relationship between the temperature and the warpage value under the reflow soldering temperature curve, the present invention can accurately measure the warpage of the PCB board and the IC board. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1It is a schematic flow chart of the method for simulating the reflow soldering temperature curve of the present invention.

[0038] Figure 2 It is a schematic diagram showing the effect of the method for simulating the reflow soldering temperature curve of the present invention.

[0039] Figure 3 It is a schematic flow chart of the warpage measurement method of a PCB board and an IC board of the present invention. DETAILED DESCRIPTION

[0040] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0041] See also Figure 1-Figure 3 It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0042] The thermal deformation tester is an instrument for warping analysis of PCB boards and IC boards. Different temperature sections, heater power, exhaust air volume, etc. can be set to make the thermal deformation tester reach the set temperature. The pre-setting of different temperature sections is to optimize the temperature of the thermal deformation tester towards the target value. The heater power and exhaust air volume are the parameters that can directly affect the temperature rise and fall of the thermal deformation tester. The actual temperature reached by the thermal deformation tester is often different from the preset temperature section. The top heater and the bottom heater of the thermal deformation tester are respectively used to ensure that the upper and lower temperatures of the chamber are uniform. Since the bottom heater heats the sample more directly, the present invention is more concerned about the power of the bottom heater. The present invention uses the thermal deformation tester to accurately fit the reflow soldering temperature curve while accurately obtaining the warping value of the electronic device. Based on the functional relationship between the reflow soldering temperature curve and the warping value, the reflow soldering can better solder the electronic devices together during soldering.

[0043] The temperature control system of the thermal deformation tester generally adopts the PID algorithm. The control of the temperature change curve by the PID algorithm is usually complex and nonlinear. It is difficult to obtain a model with high accuracy in the prior art. The present invention approximates the transfer function of the PID algorithm to a first-order mathematical function, and approximates each variable of the transfer function to obtain the calculation formula of the system gain K value:

[0044]

[0045] Among them, y1 represents the temperature at which the temperature control system of the thermal deformation tester reaches the starting end point of each temperature segment, y2 represents the temperature at which the temperature control system of the thermal deformation tester reaches the ending end point of each temperature segment, x1 represents the time to reach the starting end point of each temperature segment, x2 represents the time to reach the ending end point of each temperature segment, τ represents the system response time of the temperature control system of the thermal deformation tester, and b represents the room temperature of the temperature control system of the thermal deformation tester. It should be noted that the temperature curve composed of the temperature segments of the thermal deformation tester is a continuous curve. For example, the boundary endpoint of the heating segment and the constant temperature segment is both the ending end point of the heating segment and the starting end point of the constant temperature segment, and the boundary endpoint of the constant temperature segment and the cooling segment is both the ending end point of the constant temperature segment and the starting end point of the cooling segment.

[0046] The present invention first presets each temperature segment of the thermal deformation tester according to the reflow soldering temperature curve, and then sets the range of the system gain K of each temperature segment of the thermal deformation tester. The present invention adjusts the relevant parameters of the thermal deformation tester so that the actual system gain K of the thermal deformation tester is within the range of the preset system gain K, thereby making the temperature curve of the thermal deformation tester close to the reflow soldering temperature curve, thereby achieving the purpose of the present invention of accurately fitting the reflow soldering temperature curve.

[0047] Embodiment 1

[0048] This embodiment provides a method for simulating a reflow soldering temperature curve, by adjusting the parameters of a thermal deformation tester so that the thermal deformation tester fits the reflow soldering temperature curve. Figure 1 As shown:

[0049] First, step S1: placing the first sample and the second sample in a thermal deformation tester.

[0050] Specifically, in this embodiment, the first sample and the second sample have the same performance in terms of temperature, warpage, etc., that is, under the same external conditions, the first sample and the second sample have the same temperature and warpage. Further, in order to improve the thermal conductivity of the thermal deformation tester to the first sample and the second sample, the stage of the thermal deformation tester is removed so that the bottom heater of the thermal deformation tester directly works on the first sample and the second sample. In actual use, it is possible to choose whether to remove the stage of the thermal deformation tester as needed, which is not limited to this embodiment.

[0051] Specifically, in this embodiment, when the first sample is placed at the center of the thermal deformation tester cavity, the heat will be more uniform, and the collected temperature value will be more accurate. Furthermore, the first sample and the second sample are placed in the same plane, so that the thermal deformation tester adjusts the temperature of the first sample and the second sample to be consistent, and the distance between the second sample and the first sample is 5mm to 200mm, including but not limited to: 10mm, 50mm, 100mm, 150mm, which are not described here one by one. In actual use, the positions of the first sample and the second sample in the thermal deformation tester can be set as needed, not limited to this embodiment.

[0052] Specifically, in this embodiment, thermal conductive paste is applied on the upper and lower surfaces of the first sample, and thermocouples are fixed on the upper and lower surfaces of the first sample through the thermal conductive paste. The thermocouples record the real-time temperature of the first sample. In actual use, a temperature recording device for the first sample can be set as needed, which is not limited to this embodiment.

[0053] Next, step S2: preset the temperature sections of the thermal deformation tester and the numerical range of the system gain K of the thermal deformation tester according to the reflow temperature curve.

[0054] Specifically, in this embodiment, in view of the characteristics of the reflow soldering temperature curve, the thermal deformation tester is generally divided into a temperature rising section, a constant temperature section, and a temperature falling section. Furthermore, according to the specific characteristics of the reflow soldering temperature curve, the endpoint values ​​of each temperature section of the thermal deformation tester and the numerical range of the thermal deformation tester system gain K are set.

[0055] Specifically, in this embodiment, the method for presetting the numerical range of the system gain K can be: based on the reflow soldering temperature curve, each preset temperature segment is obtained, and the thermal deformation tester is used to simulate each preset temperature segment n times to obtain the time value when the thermal deformation tester reaches the end point of each temperature segment, and the system gain of the heating segment and the cooling segment is calculated based on the PID algorithm. As an example, the system gains of the first heating segment, the second heating segment, the first cooling end, and the second cooling segment are K1, K2, K3, and K4, respectively, where K1, K2, K3, and K4 represent a set of system gains K obtained in n measurements of each temperature segment; remove the noise data that obviously deviates from the expectation, and preset the extreme value of the system gain of each temperature segment as the range of the system gain K of each temperature segment. For example, after removing the noise data in K1, the extreme value of K1 is preset as the range end value of the system gain K of the first heating segment. It should be noted that n is a natural number greater than or equal to 2, and the larger the value of n is, the more accurate the range of the preset system gain K of each temperature segment is.

[0056] Specifically, in this embodiment, according to the calculation formula of the system gain K, the actual temperature and time when the thermal deformation tester reaches the end point of each temperature segment are substituted to calculate the actual system gain K of each temperature segment, and the relevant parameters of the thermal deformation tester are adjusted so that the actual system gain K of each temperature segment is within the range of the preset system gain K.

[0057] Next, step S3: setting the maximum power of the bottom heater of the thermal deformation tester and the air volume of the exhaust port of the thermal deformation tester to preheat the thermal deformation tester.

[0058] Specifically, in this embodiment, in order to calibrate the thermal deformation tester, the temperature setting point of the top heater of the thermal deformation tester is matched with the temperature setting point of the system configuration of the thermal deformation tester. As an example, the set point offset of the top heater of the thermal deformation tester can be set to zero for matching. In actual use, whether to calibrate the thermal deformation tester can be decided as needed, which is not limited to this embodiment.

[0059] Specifically, as an example, the total exhaust duct air valve of the thermal deformation tester is set to 90 degrees, and in subsequent steps, the setting of the total exhaust duct air valve is always maintained. In actual use, the total exhaust duct air valve can be set as needed, which is not limited to this embodiment.

[0060] Specifically, in this embodiment, in order to quickly preheat the thermal deformation tester, the air volume at the exhaust port is set to 1 / 10 to 1 / 3 of the full air volume, and further, the air volume at the exhaust port is set to 3 / 16 of the full air volume.

[0061] Again, step S4: after the preheating is completed, continue to increase the temperature of the thermal deformation tester so that the thermal deformation tester enters the heating section, and use the PID algorithm to calculate the system gain K of the heating section. The transfer function of the PID algorithm is a first-order mathematical model; adjust the maximum power and the exhaust air volume so that the system gain K of the heating section is within the preset system gain K range; record the real-time temperature of the first sample and the real-time warping value of the second sample.

[0062] Specifically, in this embodiment, in order to adapt to the characteristic changes of the reflow soldering heating section, the heating section can be divided into a first heating section and a second heating section, and the temperature change slope of the first heating section is greater than the temperature change slope of the second heating section. Specifically, in this embodiment, the temperature of the starting end point of the first heating section is preset to 10% to 15% of the highest reflow soldering temperature, the temperature of the junction end point of the first heating section and the second heating section is preset to 87% to 90% of the highest reflow soldering temperature, and the temperature of the junction end point of the second heating section and the constant temperature section is preset to 98% to 102% of the highest reflow soldering temperature; as an example, Figure 2As shown, when the maximum temperature of the reflow soldering is 260°C, the temperature of the starting endpoint of the first heating section is preset to 30°C, the temperature of the junction endpoint of the first heating section and the second heating section is preset to 230°C, and the temperature of the junction endpoint of the second heating section and the constant temperature section is preset to 260°C. Specifically, in this embodiment, in order to make the system gain K of the heating section within the range of the preset system gain K, the maximum power of the bottom heater of the first and second heating sections is not less than the maximum power of the bottom heater of the constant temperature section. Further, the maximum power of the bottom heater of the first heating section is 30% to 100% of the full power, and the maximum power of the bottom heater of the second heating section is 30% to 90% of the full power; as an example, the maximum power in the first heating section is 100% of the full power, and the maximum power in the second heating section is 90% of the full power. Specifically, in the present embodiment, in order to make the system gain K of the temperature rise section within the range of the preset system gain K, the exhaust air volume of the first and second temperature rise sections is greater than that of the constant temperature section. Furthermore, the exhaust air volume of the first temperature rise section is 1 / 10 to 1 / 4 of the full air volume, and the exhaust air volume of the second temperature rise section is 1 / 4 to 1 / 2 of the full air volume. As an example, the exhaust air volume in the first temperature rise section is 3 / 16 of the full air volume, and the exhaust air volume in the second temperature rise section is 1 / 4 of the full air volume. As an example, the preset system gain K value of the first temperature rise section ranges from 0.92 to 1.06, the preset system gain K value of the second temperature rise section ranges from 0.84 to 0.91, the actual system gain K value of the first temperature rise section is 0.96, and the actual system gain K value of the second temperature rise section is 0.84, wherein the system response time is the time for the thermal deformation tester to adjust into different temperature sections. Any preset K value range and actual calculated K value that can realize the simulated reflow soldering temperature curve of the present invention are applicable to the present invention, and are not limited to this embodiment.

[0063] Again, step S5: maintain the temperature of the thermal deformation tester so that the thermal deformation tester enters the constant temperature section, adjust the maximum power and the exhaust air volume to keep the cavity temperature of the thermal deformation tester constant; record the real-time temperature of the first sample and the real-time warping value of the second sample.

[0064] Specifically, in this embodiment, the temperature of the constant temperature section is preset to 98% to 102% of the highest reflow temperature; as an example, Figure 2 As shown, when the maximum reflow temperature is 260°C, the constant temperature section is set to 260°C.

[0065] Specifically, in this embodiment, in order to keep the temperature of the thermal deformation tester unchanged in the constant temperature section, the maximum power of the bottom heater in the constant temperature section is not less than the maximum power of the bottom heater in the cooling section, and the exhaust air volume in the constant temperature section is not greater than the exhaust air volume in the cooling section. Furthermore, the maximum power of the bottom heater is 30% to 90% of the full power, and the exhaust air volume is 1 / 20 to 1 / 10 of the full air volume; as an example, the maximum power of the bottom heater is 60% of the full power, and the exhaust air volume is 1 / 10 of the full air volume.

[0066] Finally, step S6: lower the temperature of the thermal deformation tester so that the thermal deformation tester enters the cooling section, and use the PID algorithm to calculate the system gain K of the cooling section; adjust the maximum power and exhaust air volume so that the system gain K of the cooling section is within the preset system gain K range; record the real-time temperature of the first sample and the real-time warping value of the second sample.

[0067] Specifically, in this embodiment, in order to adapt to the characteristic changes of the reflow soldering cooling section, the cooling section can be divided into a first cooling section and a second cooling section, and the temperature change slope of the first cooling section is smaller than the temperature change slope of the second cooling section. Specifically, in this embodiment, the temperature of the junction point between the constant temperature section and the first cooling section is preset to 98% to 102% of the highest reflow soldering temperature, the temperature of the junction point between the first cooling section and the second cooling section is preset to 87% to 90% of the highest reflow soldering temperature, and the temperature of the terminal end of the second cooling section is preset to 56% to 60% of the highest reflow soldering temperature; as an example, Figure 2As shown, when the highest temperature of the reflow soldering is 260°C, the temperature of the junction point between the constant temperature end and the first cooling section is preset to 260°C, the temperature of the junction point between the first cooling section and the second cooling section is preset to 230°C, and the temperature of the terminal point of the second cooling section is preset to 150°C. Specifically, in this embodiment, in order to make the system gain K of the temperature rise section within the range of the preset system gain K, the maximum power of the bottom heater of the first cooling section is 20% to 90% of the full power, and the maximum power of the bottom heater of the second cooling section is 10% to 80% of the full power; as an example, the maximum power of the bottom heater in the first cooling section is 60% of the full power, and the maximum power of the bottom heater in the second cooling section is 50% of the full power. Specifically, in the present embodiment, in order to make the system gain K of the temperature rise section within the range of the preset system gain K, the air volume at the exhaust port of the first temperature drop section is 1 / 10 to 1 / 3 of the full air volume, and the air volume at the exhaust port of the second temperature drop section is 1 / 5 to the full air volume; as an example, the air volume at the exhaust port in the first temperature drop section is 1 / 8 of the full air volume, and the air volume at the exhaust port in the second temperature drop section is 1 / 4 of the full air volume. As an example, in the present embodiment, the preset system gain K value of the first temperature drop section ranges from -0.71 to -0.41, and the preset system gain K value of the second temperature drop section ranges from -3.08 to -0.99. The actual system gain K value of the first temperature drop section is -0.68, and the actual system gain K value of the second temperature drop section is -0.99. Any preset K value range and actual calculated K value that can realize the simulated reflow soldering temperature curve of the present invention are applicable to the present invention, and are not limited to the present embodiment.

[0068] Specifically, as an example, Figure 2 As shown, the temperature curve obtained by the thermal deformation tester in this embodiment is within the system gain range of the preset reflow soldering temperature curve, and is consistent with the changing law of the preset reflow soldering temperature curve as a whole. The reflow soldering temperature curve simulated according to this example can obtain accurate PCB board and IC board warping in the reflow soldering process.

[0069] It should be noted that, in the present embodiment, when the temperature drops below 150°C, the reflow soldering process is generally nearing its end, the warping of the PCB board and the IC board tends to stabilize, and the cooling section below 150°C will not affect the system gain of other temperature sections. Therefore, the present invention does not care about the system gain of the thermal deformation tester cooling section below 150°C. After the temperature drops to 150°C, it is only necessary to quickly cool down the thermal deformation tester. Therefore, in the present embodiment, the terminal temperature of the second cooling section is set to 150°C. In actual use, the terminal temperature of the second cooling section can be set as needed, which is not limited to the present embodiment.

[0070] Embodiment 2

[0071] like Figure 3As shown, this embodiment provides a method for measuring the warpage of a PCB board and an IC board.

[0072] First, step S1': a method of simulating the reflow soldering temperature curve is used to obtain the real-time warpage value corresponding to the real-time temperature of each temperature segment, and a functional relationship between the temperature and the warpage value under the reflow soldering temperature curve is fitted.

[0073] Specifically, in this embodiment, a method of simulating the reflow soldering temperature curve using a thermal deformation tester can collect the temperature value of the first sample and the warpage value of the second sample in each temperature segment. This embodiment can obtain a set of discrete mathematical relationships between temperature values ​​and warpage values. Furthermore, through numerical analysis methods such as least squares fitting method and polynomial fitting method, this embodiment can obtain the functional relationship between temperature and warpage value under the reflow soldering temperature curve.

[0074] Secondly, step S2': under the reflow process, based on the functional relationship between the temperature and the warpage value under the reflow temperature curve, the warpage values ​​of the PCB board and the IC board are obtained through the real-time temperature.

[0075] Specifically, in this embodiment, based on the functional relationship between temperature and warpage value under the reflow soldering temperature curve, the warpage value of the PCB board and the IC board under the reflow soldering process can be accurately measured. Furthermore, by accurately knowing the warpage of the PCB board and the IC board under the reflow soldering process in advance, the reflow soldering process can be optimized and verified.

[0076] In summary, the present invention first presets the temperature sections and system gain range of the thermal deformation tester according to the reflow soldering temperature curve. Secondly, the present invention adjusts the system gain and other parameters of the thermal deformation tester by controlling the exhaust air volume of the thermal deformation tester, the maximum power of the bottom heater and other parameters so that the thermal deformation tester can fit the reflow soldering temperature curve. At the same time, the thermal deformation tester collects the warpage value of the sample in real time. Therefore, the present invention can achieve the purpose of accurately measuring the warpage of the PCB board and the IC board while accurately fitting the reflow soldering temperature curve. The present invention has the advantages of convenience, high efficiency and high reusability. Furthermore, through the functional relationship between the temperature and the warpage value under the reflow soldering temperature curve, the present invention can accurately measure the warpage value of the PCB board and the IC board under the reflow soldering process, and then the reflow soldering process can be optimized and verified. Therefore, the present invention effectively overcomes the various shortcomings in the prior art and has a high industrial utilization value.

[0077] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for simulating a reflow soldering temperature curve, characterized in that: The method for simulating a reflow soldering temperature curve comprises at least the following steps: S1: placing the first sample and the second sample in a thermal deformation tester; S2: Presetting each temperature segment of the thermal deformation tester and a numerical range of a system gain K of the thermal deformation tester according to a reflow soldering temperature curve; S3: setting the maximum power of the bottom heater of the thermal deformation tester and the air volume of the exhaust port of the thermal deformation tester to preheat the thermal deformation tester; S4: After the preheating is completed, the temperature of the thermal deformation tester is continued to be increased so that the thermal deformation tester enters the heating stage, and the system gain K of the heating stage is calculated by using the PID algorithm, wherein the transfer function of the PID algorithm is a first-order mathematical model; the maximum power and the air volume at the exhaust port are adjusted so that the system gain K of the heating stage is within the range of the preset system gain K; the real-time temperature of the first sample and the real-time warpage value of the second sample are recorded; S5: maintaining the temperature of the thermal deformation tester so that the thermal deformation tester enters a constant temperature section, adjusting the maximum power and the air volume of the exhaust port so that the cavity temperature of the thermal deformation tester remains constant; recording the real-time temperature of the first sample and the real-time warpage value of the second sample; S6: lowering the temperature of the thermal deformation tester so that the thermal deformation tester enters a cooling stage, and using the PID algorithm to calculate the system gain K of the cooling stage; adjusting the maximum power and the air volume at the exhaust port so that the system gain K of the cooling stage is within a preset range of the system gain K; and recording the real-time temperature of the first sample and the real-time warpage value of the second sample; Among them, the exhaust air volume of the temperature rising section is greater than the exhaust air volume of the constant temperature section, and the exhaust air volume of the constant temperature section is not greater than the exhaust air volume of the temperature dropping section; the maximum power of the temperature rising section is not less than the maximum power of the constant temperature section, and the maximum power of the constant temperature section is not less than the maximum power of the temperature dropping section.

2. The method for simulating a reflow soldering temperature curve according to claim 1, wherein: Before preheating the heat deformation tester, the temperature setting point of the top heater of the heat deformation tester is matched with the temperature setting point of the system configuration of the heat deformation tester.

3. The method for simulating a reflow soldering temperature curve according to claim 1, wherein: The stage of the thermal deformation tester is removed to improve the heat conduction efficiency of the thermal deformation tester to the first sample and the second sample.

4. The method for simulating a reflow soldering temperature curve according to claim 1, wherein: The first sample is placed at the center of the cavity of the thermal deformation tester, the first sample and the second sample are placed in the same plane, and the distance between the first sample and the second sample is set to 5mm-200mm.

5. The method for simulating a reflow soldering temperature curve according to claim 1, wherein: The calculation formula of the system gain K satisfies: Among them, y1 is the temperature when the thermal deformation tester reaches the starting end point of each temperature segment, y2 is the temperature when the thermal deformation tester reaches the ending end point of each temperature segment, x1 is the time when the thermal deformation tester reaches the starting end point of each temperature segment, x2 is the time when the thermal deformation tester reaches the ending end point of each temperature segment, τ is the system response time of each temperature segment of the thermal deformation tester, and b is the room temperature of the thermal deformation tester.

6. The method for simulating a reflow soldering temperature curve according to claim 1, wherein: In the preheating stage, the air volume at the exhaust port is set to 1 / 10 to 1 / 3 of the full air volume.

7. The method for simulating a reflow soldering temperature curve according to claim 1, wherein: The temperature of the constant temperature section is preset to 98% to 102% of the highest reflow temperature; In the constant temperature section, the maximum power is 30% to 90% of the full power; In the constant temperature section, the air volume at the exhaust port is set to 1 / 20 to 1 / 10 of the full air volume.

8. The method for simulating a reflow soldering temperature curve according to any one of claims 1 to 7, characterized in that: The temperature rising section is divided into a first temperature rising section and a second temperature rising section, and the temperature change slope of the first temperature rising section is greater than the temperature change slope of the second temperature rising section.

9. The method for simulating a reflow soldering temperature curve according to claim 8, characterized in that: The temperature of the starting end point of the first heating section is preset to 10% to 15% of the maximum reflow temperature, the temperature of the junction end point of the first heating section and the second heating section is preset to 87% to 90% of the maximum reflow temperature, and the temperature of the junction end point of the second heating section and the constant temperature section is preset to 98% to 102% of the maximum reflow temperature.

10. The method for simulating a reflow soldering temperature curve according to claim 8, wherein: In the first temperature rise stage, the maximum power is 30% to 100% of the full power; In the second temperature rising stage, the maximum power is 30% to 90% of the full power.

11. The method for simulating a reflow soldering temperature curve according to claim 8, wherein: In the first temperature rise stage, the air volume at the exhaust port is set to 1 / 10 to 1 / 4 of the full air volume; In the second temperature rise stage, the air volume at the exhaust port is set to 1 / 4 to 1 / 2 of the full air volume.

12. The method for simulating a reflow soldering temperature curve according to any one of claims 1 to 7, characterized in that: The temperature reduction section is divided into a first temperature reduction section and a second temperature reduction section, and the temperature change slope of the first temperature reduction section is smaller than the temperature change slope of the second temperature reduction section.

13. The method for simulating a reflow soldering temperature curve according to claim 12, characterized in that: The temperature of the junction point between the constant temperature section and the first temperature reduction section is preset to 98% to 102% of the highest reflow temperature, the temperature of the junction point between the first temperature reduction section and the second temperature reduction section is preset to 87% to 90% of the highest reflow temperature, and the temperature of the terminal point of the second temperature reduction section is preset to 56% to 60% of the highest reflow temperature.

14. The method for simulating a reflow soldering temperature curve according to claim 12, wherein: In the first cooling stage, the maximum power is 20% to 90% of the full power; In the second temperature reduction stage, the maximum power is 10% to 80% of the full power.

15. The method for simulating a reflow soldering temperature curve according to claim 12, wherein: In the first cooling stage, the air volume at the exhaust port is set to 1 / 10 to 1 / 3 of the full air volume; In the second cooling stage, the air volume at the exhaust port is set to be 1 / 5 of the full air volume to the full air volume.

16. A method for measuring the warpage of a PCB board and an IC board, characterized in that: The warpage measurement method of the PCB board and the IC board comprises at least the following steps: S1': using the method for simulating the reflow soldering temperature curve according to any one of claims 1 to 15 to obtain the real-time warpage value corresponding to the real-time temperature of each temperature segment, and fitting the functional relationship between the temperature and the warpage value under the reflow soldering temperature curve; S2': Under the reflow process, based on the functional relationship between temperature and warpage value, the warpage value of the PCB board and the IC board is obtained through the real-time temperature.