Testing method of thermoelectric device
Through finite element simulation calculation and precise control of test structure, the problem of temperature difference control error in thermoelectric device testing is solved, and the accuracy of thermoelectric device performance testing is improved.
Patent Information
- Application Number
- CN202410917469.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-10
- Publication Date
- 2024-11-01
AI Technical Summary
The existing thermoelectric device testing methods cannot accurately control the temperature difference between the upper and lower ends of the thermoelectric material layer, resulting in large performance testing errors.
Using finite element simulation calculation method, a three-dimensional structural model of thermoelectric devices is established, and the temperature difference between the two ends of the thermoelectric material layer is determined through heat transfer simulation, and the temperature of the upper and lower surfaces of the device is controlled by the test structure to ensure that the actual temperature difference reaches the simulation set value, thereby improving the test accuracy.
Through finite element simulation calculation and precise control of test structure, temperature difference control errors in the prior art are avoided and the accuracy of performance testing of thermoelectric devices is improved.
Smart Images

Figure CN118886255A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of thermoelectric device testing, and in particular to a method for testing a thermoelectric device. Background Art
[0002] By using the Seebeck effect or Peltier effect of thermoelectric materials, thermoelectric devices can realize the conversion of thermal energy and electrical energy. According to the different conversion directions, thermoelectric devices can be divided into thermoelectric power generation devices (when there is a temperature difference between the two ends of the device, thermal energy can be converted into electrical energy) and thermoelectric cooling devices (when the thermoelectric device is powered by current, one end of the device absorbs heat and the other end releases heat). Thermoelectric devices, especially thin-film thermoelectric devices, have the characteristics of small size, wide range of applications, and the ability to effectively utilize low-quality thermal energy. They have broad application prospects in the field of thermoelectric power generation. For this reason, it is necessary to accurately measure the performance of thermoelectric devices of thermoelectric power generation type to promote the development of thermoelectric devices.
[0003] For thermoelectric devices of the temperature difference power generation type, one end of the thermoelectric device is usually heated and the other end is cooled, so as to establish a stable temperature difference between the two ends of the device, and then measure the electrical characteristics of the thermoelectric device. However, in the existing test method, thermocouples are usually used to measure the upper and lower surfaces of the thermoelectric device, generally the substrate surface or even through the gasket, so as to control the temperature difference between the hot and cold ends of the device. Based on the multi-layer structure of the thermoelectric device (usually the structure is the lower substrate, the lower electrode layer, the thermoelectric material layer, the upper electrode layer, the packaging layer and the upper substrate), the temperature measured by the thermocouple is actually the temperature of the upper and lower surfaces of the thermoelectric device, rather than the actual temperature of the upper and lower ends of the thermoelectric material layer. There is still a big gap between the two, because the packaging layer and the upper and lower electrode layers of the thermoelectric device will cause additional temperature gradients. Therefore, the existing test method cannot guarantee the accurate control of the temperature difference between the hot and cold ends of the device (i.e., the temperature difference between the upper and lower ends of the thermoelectric material layer). The inability to accurately control the temperature difference between the upper and lower ends of the thermoelectric material layer will further lead to large errors in the performance test of the thermoelectric device.
[0004] The existing measurement methods have always been difficult to ensure the accurate temperature difference between the upper and lower ends of the thermoelectric material layer, and this has always been a major problem that has troubled researchers in this field. Therefore, there is an urgent need for a test method that can accurately ensure the actual temperature difference between the upper and lower ends of the thermoelectric material layer in a thermoelectric device, so as to improve the accuracy of the thermoelectric device performance test. Summary of the invention
[0005] In order to solve the above problems, the present invention introduces a finite element simulation calculation method to achieve accurate control of the temperature difference between the upper and lower ends of the thermoelectric material layer. The following provides a test method for a thermoelectric device, comprising the following steps:
[0006] S1. Acquire the structure and material parameters of a thermoelectric device, wherein the thermoelectric device is a multi-layer structure, establish a three-dimensional structure model according to the acquired multi-layer structure, set parameters for each layer in the three-dimensional structure model according to the acquired material parameters, and obtain a thermoelectric device model;
[0007] S2, setting the heating end temperature of the thermoelectric device model to A, setting the temperature difference between the two ends of the thermoelectric material layer to m, and setting the air convection heat transfer coefficient of the environment where the thermoelectric device model is located;
[0008] S3, establishing a finite element mesh and performing a heat transfer simulation to obtain the temperature distribution of each layer of the thermoelectric device model, wherein the heat transfer simulation is terminated when the temperature difference between the two ends of the thermoelectric material layer in the thermoelectric device model reaches a set value m, and the cooling end temperature B at this time is extracted;
[0009] S4. Install the thermoelectric device in the test structure, control the upper and lower surface temperatures of the thermoelectric device through the test structure to reach the heating end temperature A and the cooling end temperature B in the thermoelectric device model simulation process, stabilize the heating end temperature A and the cooling end temperature B, and test the electrical output performance of the thermoelectric device. This method uses finite element simulation calculation to obtain the actual temperature on the upper and lower surfaces of the thermoelectric device when the temperature difference at both ends of the thermoelectric material layer is a certain set value. In this way, by controlling the upper and lower surfaces of the thermoelectric device to reach the corresponding temperature obtained by the simulation, it is possible to ensure that the actual temperature difference at both ends of the thermoelectric material layer is the set value during the simulation. In this way, the error caused by the inability to directly test the temperature at both ends of the thermoelectric material layer in the prior art is avoided, and the test accuracy of the thermoelectric performance is improved.
[0010] In step S1, the multilayer structure includes at least a lower electrode layer, a thermoelectric material layer and an upper electrode layer from bottom to top. According to different thermoelectric devices to be tested, the modeling structure can be flexibly changed to make the simulation results more realistic.
[0011] The multilayer structure comprises, from bottom to top, a lower substrate, a lower electrode layer, a thermoelectric material layer, an upper electrode layer, a packaging layer and an upper substrate.
[0012] In step S1, the material parameters include the Seebeck coefficient, resistivity and thermal conductivity of the material. According to different thermoelectric devices to be tested, the material parameters can be flexibly changed to make the simulation results more realistic.
[0013] In step S2, the air convection heat transfer coefficient of the environment in which the thermoelectric device model is located is set to 5-50 W / m 2 .K.
[0014] In step S4, the test structure includes a heating component and a cooling component, the upper and lower surfaces of the thermoelectric device are in close contact with the heating component and the cooling component respectively, the heating component is a heating Cu block with a heat source, and the cooling component is a water-cooled Cu block. The use of the heating component and the cooling component can improve the uniform distribution and accuracy of the temperature and achieve the test conditions more quickly.
[0015] When the thermoelectric device is installed in the test structure, thermal conductive silicone grease is coated on the upper and lower surfaces of the thermoelectric device. During the test, the contact interface is filled with thermal conductive material to enhance the thermal conductivity between the interfaces, ensure accurate and uniform temperature control, and reach the test conditions more quickly.
[0016] The test structure is provided with at least two thermocouples, and through holes are provided at the center of the heating Cu block and the water-cooling Cu block. The thermocouples are respectively connected to the upper and lower surfaces of the thermoelectric device through the through holes to control the upper and lower surface temperatures of the thermoelectric device. The thermocouples directly contact the upper and lower surfaces of the thermoelectric device and are located at the center, which can ensure the accuracy of temperature measurement and further reduce temperature errors.
[0017] A cooling pipeline for cooling water to flow is reserved inside the water-cooled Cu block, and two ends of the cooling pipeline are respectively a water inlet and a water outlet.
[0018] In step S4, the test process is carried out in a closed environment without convection. Placing the test process in a closed environment without convection can reduce the impact of the external environment on the measured temperature.
[0019] The beneficial effects of the present invention are as follows: the present method introduces finite element simulation calculation, and obtains the actual temperature on the upper and lower surfaces of the thermoelectric device when the temperature difference at both ends of the thermoelectric material layer is a certain set value. The temperature difference control problem at both ends of the thermoelectric material layer is converted into the temperature control problem of the upper and lower surfaces of the thermoelectric device, thereby avoiding the temperature control error caused by the inability to directly test the temperature at both ends of the thermoelectric material layer in the prior art, thereby improving the test accuracy of the thermoelectric performance of the thermoelectric device. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the technical solutions in the specific embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0021] Figure 1 Schematic diagram of the testing principle of the temperature difference power generation type thermoelectric device provided by the present invention.
[0022] Figure 2 A two-dimensional diagram of the three-dimensional structural model of the thermoelectric device provided by the present invention.
[0023] Figure 3 The temperature distribution diagram inside the thermoelectric device obtained by simulating the Comsol solid heat transfer module provided by the present invention.
[0024] Figure 4 This is a schematic diagram of the measurement structure of the thermoelectric device provided by the present invention.
[0025] Figure 5 This is a graph showing the power generation performance test results of the thermoelectric device provided by the present invention. DETAILED DESCRIPTION
[0026] The above and other technical contents, features and effects of the present invention will be clearly presented in the following detailed description of a preferred embodiment with reference to the drawings. The directional terms mentioned in the following embodiments, such as up, down, left, right, front or back, etc., are only referenced to the directions of the attached drawings. Therefore, the directional terms used are used to illustrate and not to limit the present invention.
[0027] The following will describe the various embodiments of the present application in detail with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the various embodiments of the present application, many technical details are provided in order to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical solution claimed in the present application can be implemented.
[0028] The steps in the following embodiments do not correspond one to one with the summary of the invention.
[0029] Embodiment 1
[0030] In the present application, a test method for a thermoelectric device is provided for a thermoelectric device of a thermoelectric power generation type. The test principle diagram of a thermoelectric device of a thermoelectric power generation type is shown in FIG. Figure 1 As shown in Figure 2. For thermoelectric devices of temperature difference power generation, one end of the thermoelectric device is usually heated and the other end is cooled. Figure 1 As shown, the thermoelectric device 1 has a water cooling block 5 below and a heating plate 4 above. The upper and lower surfaces of the thermoelectric device are both temperature-controlled by a temperature control device. Figure 1 In order to prevent the accuracy of data during the measurement circuit test from being affected by electrical conduction between the heating plate 4 and the thermoelectric device 1 and between the water-cooling block 5 and the thermoelectric device 1, a first insulating ceramic sheet 2 and a second insulating ceramic sheet 3 are respectively arranged on the upper and lower surfaces of the thermoelectric device 1.
[0031] Since the thickness of thin film thermoelectric devices is usually within hundreds of microns, accurate reading of the temperature at both ends of the thermoelectric device 1 is the key point in the performance measurement of the thermoelectric device. In order to minimize the influence of contact thermal resistance, the following method can be used: Figure 1 The thermocouple placement shown is to place the first thermocouple 601 on the upper surface of the upper substrate of the thermoelectric device 1, and to place the second thermocouple 602 on the upper surface of the lower substrate of the thermoelectric device 1. Although the above measurement method can read the temperature of the hot and cold ends of the thermoelectric device 1 as accurately as possible, there is still a certain measurement error. This is because the thermoelectric device 1 is a multi-layer structure. Usually, the thermoelectric device 1 includes a lower substrate, a lower electrode layer, a thermoelectric material layer, an upper electrode layer, a packaging layer and an upper substrate 6-layer structure. In actual testing, the temperature measured by the thermocouple 6 is actually the temperature on the substrate of the thermoelectric device 1, and the temperature control is also based on the test temperature. The packaging layer and the upper and lower electrode layers in the thermoelectric device 1 will cause additional temperature gradients, resulting in a gap between the substrate temperature of the thermoelectric device 1 and the actual temperature at the upper and lower ends of the thermoelectric material layer. Therefore, the existing testing method cannot guarantee the accurate control of the temperature difference between the hot and cold ends of the thermoelectric device (i.e., the temperature difference between the upper and lower ends of the thermoelectric material layer).
[0032] In order to solve the above problems, the present invention introduces a finite element simulation calculation method, by simulating the thermoelectric device 1, by selecting the temperature difference between the upper and lower ends of the thermoelectric material layer as a fixed value, the corresponding temperatures of the upper and lower surfaces of the thermoelectric device 1 are obtained, and the temperature difference control problem at both ends of the thermoelectric material layer is converted into the temperature control problem of the upper and lower surfaces of the thermoelectric device, thereby avoiding the temperature control error caused by the inability to directly test the temperature at both ends of the thermoelectric material layer in the prior art, thereby achieving accurate control of the temperature difference at both ends of the thermoelectric material layer, and further providing a test method for the thermoelectric device, the test method comprising the following steps:
[0033] Step 1: Perform finite element simulation calculation to determine the set temperatures of the upper and lower surfaces of the thermoelectric device 1 .
[0034] S101: According to the structure of the thermoelectric device 1 to be tested and the material parameters of the materials constituting each layer, three-dimensional modeling is performed on the thermoelectric device 1 and corresponding material parameters are assigned to obtain a thermoelectric device model.
[0035] In this embodiment, Comsol simulation software is used to construct a model for finite element simulation calculation. First, different three-dimensional structural models are modeled according to the different structures of the thermoelectric device 1. In this embodiment, the thermoelectric device 1 includes a lower substrate, a lower electrode layer, a thermoelectric material layer, an upper electrode layer, a packaging layer and an upper substrate. The two-dimensional diagram of the three-dimensional structural model obtained according to the thermoelectric device 1 is as follows: Figure 2As shown, from bottom to top, they are a lower substrate 110, a lower electrode layer 120, a thermoelectric material layer 130, an upper electrode layer 140, a packaging layer 150 and an upper substrate 160, and the corresponding thickness of each layer is shown in Table 1 (the length and width of each layer are also modeled according to the actual thermoelectric device 1 to be tested, Figure 2 Only a two-dimensional diagram is shown in FIG. 1 ). In other embodiments, the number of layers and the size of each layer (ie, the length, width, and thickness of each layer) may be adjusted accordingly according to the structure of the thermoelectric device.
[0036] In order to make the simulation results consistent with the actual situation, it is necessary to assign the required material parameters to each layer in the three-dimensional structure model to obtain a thermoelectric device model. Material parameters include Seebeck coefficient (the Seebeck coefficient can describe the phenomenon that two different conductors or semiconductor materials generate electromotive force under temperature difference, reflecting the thermoelectric conversion ability of the material under temperature gradient), resistivity, thermal conductivity, etc. In this embodiment, the material parameters of each layer are shown in Table 1, where the upper and lower substrates are made of AlN material, and the thermoelectric material layer 130 is made of N-type thermoelectric material Bi 2 Te 3 and P-type thermoelectric material Sb 2 Te 3 Together, the encapsulation layer material is polydimethylsiloxane (PDMS).
[0037] Table 1 Material parameters of each layer
[0038]
[0039] S102, assigning temperature and determining the temperature difference between the two ends of the thermoelectric material layer 130, performing heat transfer simulation using Fourier's law of heat conduction, Newton's cooling law of heat convection, Stefan-Bolsmann's law of thermal radiation, etc., to obtain the corresponding set temperatures of the upper and lower surfaces of the thermoelectric device 1.
[0040] Since the thermoelectric device 1 will be heated at one end and cooled at the other end to provide a certain temperature difference when being tested, the temperature also needs to be assigned during the simulation. In the actual test process, the upper and lower surfaces of the thermoelectric device 1 (in this embodiment, the upper and lower substrate surfaces, in other embodiments, the upper and lower surfaces may also be different depending on the structure of the thermoelectric device to be tested) will be provided with a heat source and a cold source respectively through the heating component and the cooling component in the test structure, and due to the final heat conduction, the upper and lower surface temperatures of the thermoelectric device 1 will be maintained at a certain stable temperature.
[0041] Therefore, when we simulate, the thermoelectric device 1 will also be heated at one end and cooled at the other end. The heated end is recorded as the heating end, and the cooled end is recorded as the cooling end. In this embodiment, first, the temperature of the upper surface of the upper substrate 160 (i.e., the upper surface of the thermoelectric device 1) is fixed to a certain fixed temperature, and the upper surface of the upper substrate 160 is set to 350K. In other embodiments, different upper surface temperatures of the upper substrate 160 (i.e., the heating end temperature is set to A) can be set according to the heating effect of the test device and the test needs, such as 340K, 360K or 365K, etc., and there is no limitation to this; then, the air convection heat transfer coefficient of the environment in which the thermoelectric device model is located is set to 10W / m 2 .K. Then, a cooling condition is set for the lower surface of the lower substrate 110 (i.e., the lower surface of the thermoelectric device 1). The thermoelectric device model is meshed by finite element, and a solid heat transfer simulation is performed. The termination condition of the heat transfer simulation is that the temperature difference between the upper and lower ends of the thermoelectric material layer 130 reaches a set value m. At this time, the temperature of the lower surface of the lower substrate 110, i.e., the cooling end temperature B, can be obtained. In this embodiment, the set value m of the temperature difference between the upper and lower ends of the thermoelectric material layer 130 is 10K. In other embodiments, the set value m of the temperature difference can be determined according to the test requirements, such as 20K, 30K or 35K, etc., and there is no limitation to this.
[0042] like Figure 3 As shown, in this embodiment, when the temperature of the upper surface of the upper substrate 160 is 350K and the temperature difference between the upper and lower ends of the thermoelectric material 130 reaches 10K, the temperature of the lower surface of the lower substrate 110 obtained by simulation is 320K (that is, the cooling end temperature B is 320K). According to such simulation results, it is helpful to guide the actual performance test of the thermoelectric device of the temperature difference battery type, that is, when we control the upper and lower surface temperatures of the thermoelectric device 1 to be 350K and 320K respectively, it can be ensured that the temperature difference between the upper and lower ends of the thermoelectric material layer 130 is 10K at this time. Then, subsequent calculations can be performed based on the temperature difference, avoiding the problem of test performance deviation caused by the inability to accurately obtain the temperature difference between the two ends of the thermoelectric material layer in the prior art.
[0043] Step 2: Conduct an electrical output performance test based on the obtained set temperatures of the upper and lower surfaces of the thermoelectric device 1 .
[0044] The performance test method is as follows:
[0045] S201 , applying heat-conducting material on the upper and lower surfaces of the thermoelectric device 1 and placing it in a test structure.
[0046] In this embodiment, in order to reduce the contact thermal resistance, a layer of thermal conductive silicone grease is coated on the lower surface of the lower substrate 110 and the upper surface of the upper substrate 160 as a thermal conductive material; in other embodiments, other thermal conductive materials may also be used, or thermal conductive material may not be coated.
[0047] Afterwards, the thermoelectric device 1 is installed in a test structure so that the upper surface of the upper substrate 160 of the thermoelectric device 1 is in close contact with the heating component of the test structure, and the lower surface of the lower substrate 110 of the thermoelectric device 1 is in close contact with the cooling component of the test structure.
[0048] S202 , starting the heating component and the cooling component to make the upper and lower surfaces of the thermoelectric device 1 reach corresponding set temperatures.
[0049] like Figure 4 As shown, the cooling component of the test structure is a water-cooled Cu block, which is composed of a block structure and an internal cooling pipeline. The block structure is a solid Cu block, and a cooling pipeline for cooling water 8 is left inside. The two ends of the cooling pipeline are respectively a water inlet and a water outlet, which are used to connect to a water source and circulate cooling water 8. The circulating flow of cooling water 8 in the water-cooled Cu block removes the heat of the thermoelectric device 1 on its surface; the heating component of the test structure is a heating Cu block with a heat source (in order to show the thermoelectric device 1, Figure 4 The heating Cu block is in contact with the upper surface of the upper substrate 160 of the thermoelectric device 1 and conducts heat to the thermoelectric device 1. A through hole (not shown in the figure) is reserved at the center of the heating Cu block and the water-cooling Cu block for placing the thermocouple 6. Figure 4 As shown, the thermocouple 602 is connected to the center of the lower surface of the lower substrate 110 through the through hole of the water-cooled Cu block, and is used to collect the temperature of the lower surface of the lower substrate 110. Similarly, the thermocouple 601 is connected to the center of the upper surface of the upper substrate 160 through the through hole of the heated Cu block, and is used to collect the temperature of the upper surface of the upper substrate 160. When the heating component and the cooling component start to work, the temperatures of the upper and lower substrates can be determined and the heating component and the cooling component can be controlled by the thermocouple 601 and the thermocouple 602 until the actual measured temperatures of the upper and lower surfaces of the thermoelectric device 1 reach the corresponding set temperature and remain stable, and then the subsequent steps can be carried out.
[0050] In this embodiment, the heating component and the cooling component provided above can ensure accurate, stable and uniform distribution of the temperature of the upper and lower surfaces of the thermoelectric device 1. In this embodiment, when the test temperature of the upper substrate of the thermoelectric device 1 reaches its set temperature of 350K and is stable, when the test temperature of the lower substrate of the thermoelectric device 1 also reaches its set temperature of 320K and is stable, subsequent tests can be performed.
[0051] S203, connecting the thermoelectric device to a test circuit and performing an electrical output performance test.
[0052] like Figure 4As shown, the thermoelectric device 1 is connected to a test circuit for testing via a first test lead 701 and a second test lead 702 . The first test lead 701 and the second test lead 702 can be connected to different electrode pins of the lower electrode of the thermoelectric device 1 .
[0053] Based on the characteristics of the thermoelectric device of the temperature difference battery type, when there is a temperature difference at both ends of the thermoelectric device 1, heat will be converted into current, so that the relevant electrical parameters can be measured. The output current, output voltage and output power of the thermoelectric device 1 can be measured by the test circuit. According to the temperature difference between the upper and lower ends of the thermoelectric device 1 (the temperature difference is the temperature difference m between the two ends of the thermoelectric material layer set in step S102, in this embodiment, the temperature difference m is 10K), the heat discharged from the cold end of the thermoelectric device 1 and the thermoelectric conversion efficiency of the thermoelectric device 1 can be calculated to achieve the test of the electrical output performance of the thermoelectric device 1. The setting of the test circuit and the analysis and processing of the measurement results are both existing technologies, which are not the focus of this application and will not be repeated here.
[0054] In order to reduce the influence of the external environment on the measured temperature, the measurement process can also be placed in a closed non-convection environment. Repeated tests have proved that this test method has good test stability. Some test results in this embodiment are as follows Figure 5 As shown, the density of the two arrays is 578 pairs / cm 2 The power generation performance of the micro thermoelectric device was tested. The temperature of the hot end (i.e., the upper substrate surface) of the test equipment was controlled at 350K, and the temperature of the cold end (i.e., the lower substrate surface) was controlled at 320K. After taking into account the pin contact resistance and lead resistance, the device output power was above 0.14mW.
[0055] It should be noted that in this embodiment, the upper substrate of the thermoelectric device 1 is in contact with the heating component, and the lower substrate of the thermoelectric device 1 is in contact with the cooling component, so that the hot end of the thermoelectric device 1 is the side of the thermoelectric material layer 130 close to the upper substrate, and the cold end of the thermoelectric device 1 is the side of the thermoelectric material layer 130 close to the lower substrate. However, this method is not limited to this, that is, the thermoelectric device 1 can also be reversed, in which case the upper substrate of the thermoelectric device 1 is in contact with the cooling component, and the lower substrate of the thermoelectric device 1 is in contact with the heating component, so that the hot end of the thermoelectric device 1 is the side of the thermoelectric material layer 130 close to the lower substrate, and the cold end of the thermoelectric device 1 is the side of the thermoelectric material layer 130 close to the upper substrate.
[0056] In order to facilitate the description, some common English nouns or letters used in the present invention are only used for exemplary reference rather than restrictive interpretation or specific usage, and the protection scope of the present invention should not be limited by their possible Chinese translations or specific letters.
[0057] It should also be noted that, in this document, relational terms such as "first" and "second" are merely used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any actual relationship or order between these entities or operations.
Claims
1. A method for testing a thermoelectric device, It is characterized in that The steps include: S1. Acquire the structure and material parameters of a thermoelectric device, wherein the thermoelectric device is a multi-layer structure, establish a three-dimensional structure model according to the acquired multi-layer structure, set parameters for each layer in the three-dimensional structure model according to the acquired material parameters, and obtain a thermoelectric device model; S2, setting the heating end temperature of the thermoelectric device model to A, setting the temperature difference between the two ends of the thermoelectric material layer to m, and setting the air convection heat transfer coefficient of the environment where the thermoelectric device model is located; S3, establishing a finite element mesh and performing a heat transfer simulation to obtain the temperature distribution of each layer of the thermoelectric device model, wherein the heat transfer simulation is terminated when the temperature difference between the two ends of the thermoelectric material layer in the thermoelectric device model reaches a set value m, and the cooling end temperature B at this time is extracted; S4. Install the thermoelectric device in a test structure, control the upper and lower surface temperatures of the thermoelectric device through the test structure to respectively reach the heating end temperature A and the cooling end temperature B in the thermoelectric device model simulation process, stabilize the heating end temperature A and the cooling end temperature B, and test the electrical output performance of the thermoelectric device.
2. A method for testing a thermoelectric device according to claim 1, It is characterized in that In step S1 , the multilayer structure includes at least a lower electrode layer, a thermoelectric material layer and an upper electrode layer from bottom to top.
3. A method for testing a thermoelectric device according to claim 2, It is characterized in that The multilayer structure comprises, from bottom to top, a lower substrate, a lower electrode layer, a thermoelectric material layer, an upper electrode layer, a packaging layer and an upper substrate.
4. A method for testing a thermoelectric device according to claim 1, It is characterized in that In step S1 , the material parameters include the Seebeck coefficient, resistivity and thermal conductivity of the material.
5. A method for testing a thermoelectric device according to claim 1, It is characterized in that In step S2, the air convection heat transfer coefficient of the environment in which the thermoelectric device model is located is set to 5-50 W / m 2 .K.
6. A method for testing a thermoelectric device according to claim 1, It is characterized in that In step S4, the test structure includes a heating component and a cooling component, and the upper and lower surfaces of the thermoelectric device are in close contact with the heating component and the cooling component respectively. The heating component is a heated Cu block with a heat source, and the cooling component is a water-cooled Cu block.
7. A method for testing a thermoelectric device according to claim 6, It is characterized in that When the thermoelectric device is installed in a test structure, thermal conductive silicone grease is coated on the upper and lower surfaces of the thermoelectric device.
8. A method for testing a thermoelectric device according to claim 7, It is characterized in that The test structure is provided with at least two thermocouples, and through holes are provided at the center positions of the heating Cu block and the water-cooling Cu block. The thermocouples are respectively connected to the upper and lower surfaces of the thermoelectric device through the through holes to control the upper and lower surface temperatures of the thermoelectric device.
9. A method for testing a thermoelectric device according to claim 6, It is characterized in that A cooling pipeline for cooling water to flow is reserved inside the water-cooled Cu block, and two ends of the cooling pipeline are respectively a water inlet and a water outlet.
10. A method for testing a thermoelectric device according to claim 1, It is characterized in that In step S4, the testing process is performed in a closed convection-free environment.