EEPROM unit based on high-temperature SOI CMOS technology and manufacturing method
By using high-temperature SOI CMOS technology and all-dielectric isolation technology, the problems of process complexity and poor radiation resistance of EEPROM devices have been solved, and the high withstand voltage and low leakage current characteristics of the devices have been achieved in high-temperature and radiation-resistant environments.
Patent Information
- Application Number
- CN202410957861.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-11-01
AI Technical Summary
Existing EEPROM devices in SOI technology suffer from high process complexity, poor radiation resistance, and low withstand voltage, which limits their application in high-temperature and radiation-resistant fields.
Using high-temperature SOI CMOS technology, the two transistors are completely isolated through full dielectric isolation technology and source-drain injection technology. The P-type silicon film layer in the CG transistor region is modified into a deep N-type injection layer. Combined with the T-type floating gate design, the radiation resistance and voltage withstand value of the device are improved.
The process steps were simplified, the sensitive area and leakage current of the device were reduced, the performance of the device in high temperature and radiation environments was improved, and the withstand voltage capability of the device was enhanced.
Smart Images

Figure CN118890900A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor integrated circuit technology, and in particular to an EEPROM unit and a manufacturing method based on a high-temperature SOI CMOS process. Background Art
[0002] EEPROM can rewrite content at any time like RAM, and can store information for a long time like ROM. It also has the advantages of reversible programming, low power consumption, high stability, compatibility with standard CMOS process, and long data storage time. Therefore, it has been widely used in the fields of Internet of Things chips, automotive electronics, consumer electronics, etc. EEPROM can be divided into double-layer polysilicon floating gate structure and single-layer polycrystalline structure. The double-layer polycrystalline floating gate structure is widely used, such as Figure 1 As shown in the figure, the principle is to store electrons in the floating gate. This structure has disadvantages such as complex unit structure, many process steps, incompatibility with standard CMOS process, and high cost. The traditional single-layer polycrystalline structure EEPROM unit uses the common gate of two transistors as the floating gate. When performing programming and erasing operations, it is necessary to apply high voltage (~18V) between the WL of the control tube and the well area of the storage tube. This poses a great challenge to the withstand voltage of the source and drain N+ region and the P substrate in the control tube, resulting in high requirements for the process platform of this structure EEPROM and great limitations in practical application. In addition, EEPROM devices based on bulk silicon, whether it is a double-layer polycrystalline silicon floating gate structure or a single-layer polycrystalline structure, have problems with poor high temperature resistance and radiation resistance, which limits its further application in aerospace and other fields.
[0003] The features of small sensitive area, low leakage, low subthreshold swing and latch-up immunity provided by SOI technology make it one of the most competitive technologies in the field of high temperature and radiation resistance. The use of SOI CMOS process to prepare single-layer polycrystalline EEPROM is expected to reduce process complexity and improve the radiation resistance and high temperature resistance of the device. However, in order to reduce the leakage current of the device at high temperature, the wafer used in the SOI CMOS process must be a thin silicon film wafer. Due to the limitation of the thin top silicon film of SOI, the distance between the source and drain N+ region of the control tube and the substrate is very close, resulting in the voltage resistance value of EEPROM based on SOI process being lower than that based on traditional bulk silicon process. Therefore, in the single-layer polycrystalline EEPROM structure based on SOI technology, the voltage resistance design of the device is an urgent problem to be solved. Summary of the invention
[0004] The present application provides a single-layer polycrystalline EEPROM cell based on a high-temperature SOI CMOS process and a preparation method thereof, wherein two transistors are connected through polysilicon to form a single-layer polycrystalline EEPROM cell using a high-temperature SOI CMOS process, such as Figure 2Based on the STI full dielectric isolation technology in the SOI process, the control tube is prepared using the source-drain injection bottom process, which greatly improves the radiation resistance and withstand voltage of the EEPROM, in order to solve the current problems faced by EEPROM devices, such as high process complexity, poor radiation resistance, and low withstand voltage.
[0005] The present application provides a single-layer polycrystalline EEPROM cell based on a high-temperature SOI CMOS process, the single-layer polycrystalline EEPROM cell comprising:
[0006] P-type silicon substrate layer, buried oxide BOX layer, P-type silicon film layer, P-type body contact injection layer, N-type source injection layer, N-type drain injection layer, STI reinforcement injection layer, gate oxide layer, polycrystalline gate POLY layer, deep N-type injection layer, contact hole W1 layer, metal A1 layer;
[0007] Wherein, the gate oxide layer includes a FG gate oxide layer and a CG gate oxide layer;
[0008] The polycrystalline gate POLY layer includes FG polycrystalline floating gate, CG polycrystalline floating gate, and floating gate;
[0009] Furthermore, a buried oxide BOX layer and a P-type silicon film layer are sequentially disposed above the P-type silicon substrate layer.
[0010] The thickness of the P-type silicon film layer is less than 500nm; the P-type silicon film layer is a SOI wafer;
[0011] One side of the P-type silicon film layer is the FG tube;
[0012] The FG tube includes a P-type body contact injection layer, an N-type source injection layer, an N-type drain injection layer in a P-type silicon film layer, and an FG gate oxide layer and an FG polycrystalline floating gate above the P-type silicon film layer;
[0013] The other side of the P-type silicon film layer is a CG tube; the CG tube includes a deep N-type injection layer, a CG gate oxide layer above the deep N-type injection layer, and a CG polycrystalline floating gate;
[0014] The FG polycrystalline floating gate and the CG polycrystalline floating gate are directly connected through the floating gate.
[0015] Furthermore, the STI full dielectric isolation technology is used between the FG transistor and the CG transistor, that is, the two transistors are completely separated by using an STI reinforced injection layer.
[0016] Furthermore, the CG tube adopts a source-drain-to-bottom approach to modify the P-type silicon film layer in the CG tube region into a deep N-type injection layer, thereby completely avoiding the breakdown between the source and body of the CG tube.
[0017] Furthermore, the P-type body contact injection layer of the CG tube is led out as the Word Line end through the contact hole W1 and the metal A1;
[0018] The N-type source injection layer, the N-type drain injection layer and the P-type body contact injection layer in the FG tube are respectively led out through the contact hole W1 and the metal A1 as the source, BitLine and body region Body ends.
[0019] Furthermore, the FG polycrystalline floating gate and the CG polycrystalline floating gate both adopt a T-type structure, and P-type body contact injection layers are provided on both sides of the T-type gate to enhance radiation resistance.
[0020] Furthermore, the FG tube is directly connected to the CG tube via a floating gate, and the floating gate, the FG polycrystalline floating gate and the CG polycrystalline floating gate are all single-layer polycrystalline silicon structures.
[0021] Furthermore, the FG capacitor formed by the FG gate oxide layer and the CG capacitor formed by the CG gate oxide layer are connected in series.
[0022] The coupling coefficient is the ratio of the FG capacitance to the CG capacitance, and the coupling coefficient can be changed by adjusting the width and thickness of the FG gate oxide layer and the CG gate oxide layer.
[0023] As a further preferred embodiment of the present invention, the lengths of the FG floating gate and the CG floating gate are both 0.13 μm, and the thicknesses of the FG gate oxide layer and the CG gate oxide layer are adjusted to control the coupling coefficient of the storage unit.
[0024] The present application also provides a method for preparing a single-layer polycrystalline EEPROM unit based on a high-temperature SOI CMOS process, the method is used to prepare the single-layer polycrystalline EEPROM unit provided in the present application, and the method comprises the following steps:
[0025] Step 1, providing SOI wafer and preparing for tape-out;
[0026] Step 2, using photolithography and etching technology to etch an STI groove on the top Si layer of the SOI wafer;
[0027] Step 3, performing STI deposition and radiation hardening treatment;
[0028] Step 4, define the FG tube active area by photolithography and perform well implantation;
[0029] Step 5, define the CG tube active area by photolithography and perform ion implantation;
[0030] Step 6, depositing an oxide layer and etching away the area outside the gate oxide layer;
[0031] Step 7, forming POLY by deposition and etching;
[0032] Step 8, define the source, drain, and body positions by photolithography and perform ion implantation;
[0033] Step 9, depositing an ILD dielectric layer, forming a through hole by etching, and depositing and CMPing to form a W plug;
[0034] Step 10, forming an IDM dielectric layer by deposition and CMP, and etching and depositing to form an Al aluminum metal layer.
[0035] Furthermore, in step 1, the silicon film of the SOI wafer is lightly doped with P type; the doping concentration is 1.5×10 15 cm -3 ; The silicon film of the SOI wafer is ≤500nm.
[0036] In step 2, full dielectric isolation technology is used, that is, the STI groove depth is equal to the thickness of the top Si film, and different transistors can be completely separated by STI.
[0037] In step 3, ion implantation in the STI region can reduce the leakage current of the device under irradiation conditions and enhance the radiation resistance of the device.
[0038] In step 5, the source and drain are implanted to the bottom, and the thickness of the deep N-type implant layer is completely equal to the thickness of the silicon film. The doping concentration in the CG tube is 10 16 ~10 17 cm -3 .
[0039] Compared with the existing double-layer polycrystalline floating gate structure and single-layer polycrystalline structure EEPROM unit, the present invention is based on the full dielectric isolation technology and source-drain bottom technology in the high-temperature thin silicon film SOI process, uses the STI reinforcement injection layer to completely separate the two transistors, and at the same time completely modifies the P-type silicon film layer in the CG tube area into a deep N-type injection layer, which simplifies the device structure and process steps and completely avoids the breakdown problem between the CG tube source body. In summary, the single-layer polycrystalline structure EEPROM unit has the following advantages:
[0040] 1. The present invention uses a single-layer polycrystalline structure, the device structure is simple, the process steps are few, and it is compatible with the standard CMOS process;
[0041] 2. The present invention completely isolates the FG tube and the CG tube using STI, and at the same time completely modifies the P-type silicon film layer of the CG tube into a deep N-type injection layer, completely avoiding the breakdown problem between the CG tube source bodies;
[0042] 3. The present invention uses high-temperature SOI CMOS process technology. The device has the characteristics of small sensitive area, low leakage, low subthreshold swing and latch immunity, making it highly competitive in the field of high temperature and radiation resistance;
[0043] 4. The FG polycrystalline floating gate and the CG polycrystalline floating gate in the present invention both adopt a T-type structure, with P-type body contact injection layers on both sides of the T-type gate, and STI region ion implantation is added in the process steps, so the unit has strong radiation resistance. BRIEF DESCRIPTION OF THE DRAWINGS
[0044] Figure 1 This is a diagram of the structure of a traditional double-layer polycrystalline floating gate EEPROM storage cell.
[0045] Figure 2 A schematic diagram of an EEPROM unit based on a high temperature SOI CMOS process provided by the present invention.
[0046] Figure 3 The present invention provides a structural diagram of an EEPROM unit based on a high-temperature SOI CMOS process, including a side view, a top view and a front view; the front view and the side view are longitudinal cross-sectional views on the SOI wafer, and the top view is a plane view on the wafer (perpendicular to the normal direction of the wafer).
[0047] Figure 4 A circuit diagram of a single-layer polycrystalline EEPROM 1-bit structure based on a high-temperature SOI CMOS process provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0048] In order to make the objectives, technical solutions and advantages of the present application clearer, the implementation methods of the present application will be further described in detail below with reference to the accompanying drawings.
[0049] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0050] The present invention provides an EEPROM cell structure based on high temperature SOI CMOS process, and its structural schematic diagram is as follows: Figure 3 As shown, it includes a P-type silicon substrate layer (1), a buried oxide BOX layer (2), a P-type silicon film layer (3), a P-type body contact injection layer (4), an N-type source injection layer (5), an N-type drain injection layer (8), an STI reinforcement injection layer (9), an FG gate oxide layer (6), a CG gate oxide layer (10), an FG polycrystalline floating gate (7), a CG polycrystalline floating gate (11), a floating gate (15), a deep N-type injection layer (12), a contact hole W1 layer (13), and a metal A1 layer (14).
[0051] A method for preparing an EEPROM cell based on a high temperature SOI CMOS process in this embodiment at least comprises:
[0052] Step S1, providing an SOI wafer for tape-out.
[0053] Optionally, for the application of the device at high temperature and the subsequent STI etching and source-drain injection technology in full dielectric isolation, the silicon film thickness of the SOI wafer needs to be ≤500nm;
[0054] Optionally, the silicon film of the SOI wafer is lightly doped with P type, with a doping concentration of ∼1.5×1013-1015cm-3;
[0055] Step S2, using photolithography and etching technology to etch STI on the top Si layer of the SOI wafer, specifically: forming photoresist on the surface of the SOI wafer, exposing the photoresist layer through a photomask with a preset layout, then developing, patterning the photoresist, and etching the STI groove using the photoresist as a mask.
[0056] Step S3, performing radiation-resistant implantation on the STI groove region (conditions are based on the reference process) to increase the radiation-resistant performance of the device, and then depositing SiO2 to isolate the device.
[0057] Step S4, define the FG tube active area by photolithography, and perform well implantation using photoresist as a mask (conditions are based on high temperature reference process). In this embodiment, well implantation is divided into three steps, namely boron implantation, boron implantation and boron fluoride implantation.
[0058] Step S5, using photolithography to define the CG tube active area and perform ion implantation. In this embodiment, three implantations are performed, namely phosphorus implantation, phosphorus implantation and arsenic implantation. The CG tube active area is N-type doped by implantation.
[0059] Step S6, depositing an oxide layer. In this embodiment, the oxide layer thickness is 3 nm, and a photolithography process is used to define the FG gate oxide layer and the CG gate oxide layer, and a photoresist is used as a mask to etch away the oxide layer in the remaining area.
[0060] Step S7, depositing polysilicon. Using photolithography to define the FG polycrystalline floating gate and the CG polycrystalline floating gate, using photoresist as a mask and etching away the polysilicon in the remaining area.
[0061] Step S8, defining the positions of source, drain and body by photolithography, and using photoresist as a mask to perform N-type doping on the source and drain, and perform P-type doping on the body.
[0062] Step S9, depositing an ILD dielectric layer, using photolithography to define the position of the through hole, forming the through hole by etching, and depositing and CMPing to form a W plug.
[0063] Step S10, forming an IDM dielectric layer by deposition and CMP, depositing aluminum metal on the surface of the IDM dielectric, defining the position of the metal line by photolithography, and etching the aluminum metal using photoresist as a mask to form A1.
[0064] The EEPROM cell based on the radiation-resistant SOI CMOS process proposed in the present invention has three operation modes, namely, programming mode, erasing mode and reading mode. Specifically:
[0065] In programming mode, the programming voltage VP is applied to the WL terminal of the CG tube, the drain terminal BL of the FG tube is applied with a low voltage, and the source terminal CS and the body terminal Body of the FG tube are grounded. The CG gate oxide layer capacitor C1 of the CG tube and the FG gate oxide layer capacitor C2 of the FG tube are connected in series to divide the voltage, thereby achieving the effect of injecting hot electrons in the FG channel into the FG polycrystalline floating gate.
[0066] In the erase mode, the erase voltage VE is applied to the WL terminal of the CG tube, the drain terminal BL of the FG tube is floating, and a low voltage is applied to the source terminal CS and the body terminal Body of the FG tube. The electrons in the polysilicon are erased by utilizing the FN tunneling effect under the high electric field strength formed on the CG gate oxide layer.
[0067] In the read mode, the operating voltage VDD is applied to the drain terminal BL of the FG tube, the CS terminal is grounded, and the read voltage VR is applied to the WL terminal of the CG tube. VE is changed from small to large and the FG tube channel current is recorded. Since the number of electrons on the floating gate will affect the threshold voltage and current of the FG tube, the state of the storage unit can be determined by the magnitude of the current.
[0068] The circuit diagram of the single-layer polycrystalline EEPROM 1bit structure based on high temperature SOI CMOS process in the preferred embodiment of the present invention is as follows: Figure 4 As shown, after testing and evaluation, the structure can be programmed and erased at a high voltage of 18V, and there is no breakdown problem of the CG tube during this process.
[0069] It will be easily understood by those skilled in the art that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A single-layer polycrystalline EEPROM cell based on high-temperature SOI CMOS technology, It is characterized in that The single-layer polycrystalline EEPROM cell comprises: P-type silicon substrate layer (1), buried oxide BOX layer (2), P-type silicon film layer (3), P-type body contact injection layer (4), N-type source injection layer (5), N-type drain injection layer (8), STI reinforcement injection layer (9), gate oxide layer, polycrystalline gate POLY layer, deep N-type injection layer (12), contact hole W1 layer (13), metal A1 layer (14); Wherein, the gate oxide layer comprises an FG gate oxide layer (6) and a CG gate oxide layer (10); The polycrystalline gate POLY layer comprises a FG polycrystalline floating gate (7), a CG polycrystalline floating gate (11) and a floating gate (15).
2. The single-layer polycrystalline EEPROM cell based on high temperature SOI CMOS process as claimed in claim 1, It is characterized in that Above the P-type silicon substrate layer are a buried oxide BOX layer (2) and a P-type silicon film layer (3); The thickness of the P-type silicon film layer (3) is less than 500 nm; the P-type silicon film layer (3) is an SOI wafer; One side of the P-type silicon film layer (3) is a FG tube; The FG tube comprises a P-type body contact injection layer (4), an N-type source injection layer (5), an N-type drain injection layer (8) in a P-type silicon film layer, and an FG gate oxide layer (6) and an FG polycrystalline floating gate (7) above the P-type silicon film layer; The other side of the P-type silicon film layer (3) is a CG tube; the CG tube comprises a deep N-type injection layer (12), a CG gate oxide layer (10) above the deep N-type injection layer (12), and a CG polycrystalline floating gate (11); The FG polycrystalline floating gate (7) and the CG polycrystalline floating gate (11) are directly connected via a floating gate (15).
3. The single-layer polycrystalline EEPROM cell based on high temperature SOI CMOS process as claimed in claim 2, It is characterized in that The STI full dielectric isolation technology is used between the FG transistor and the CG transistor, that is, the two transistors are completely separated by using the STI reinforcement injection layer (9).
4. The single-layer polycrystalline EEPROM cell based on high temperature SOI CMOS process as claimed in claim 2, It is characterized in that The CG tube adopts a source-drain-to-bottom method to modify the P-type silicon film layer (3) in the CG tube area into a deep N-type injection layer (12).
5. The single-layer polycrystalline EEPROM cell based on high temperature SOI CMOS process as claimed in claim 2, It is characterized in that The P-type body contact injection layer (4) of the CG tube is led out as the Word Line end through the contact hole W1 (13) and the metal A1 (14); The N-type source injection layer (5), the N-type drain injection layer (8) and the P-type body contact injection layer (4) in the FG tube are respectively used as the source, the Bit Line and the body region Body end and are led out through the contact hole W1 and the metal A1.
6. The single-layer polycrystalline EEPROM cell based on high temperature SOI CMOS process as claimed in claim 2, It is characterized in that The FG polycrystalline floating gate (7) and the CG polycrystalline floating gate (11) both adopt a T-type structure, and P-type body contact injection layers (4) are provided on both sides of the T-type gate.
7. The single-layer polycrystalline EEPROM cell based on high temperature SOI CMOS process as claimed in claim 2, It is characterized in that The FG tube and the CG tube are directly connected via a floating gate (15); the floating gate (15), the FG polycrystalline floating gate (7) and the CG polycrystalline floating gate (11) are all single-layer polycrystalline silicon structures.
8. The single-layer polycrystalline EEPROM cell based on high temperature SOI CMOS process as claimed in claim 2, It is characterized in that The FG capacitor formed by the FG gate oxide layer (6) and the CG capacitor formed by the CG gate oxide layer (10) are connected in series; The coupling coefficient is the ratio of the FG capacitance to the CG capacitance, and the coupling coefficient can be changed by adjusting the width and thickness of the FG gate oxide layer and the CG gate oxide layer.
9. A method for preparing a single-layer polycrystalline EEPROM cell based on a high-temperature SOI CMOS process, the method being used for preparing the single-layer polycrystalline EEPROM cell as claimed in any one of claims 1 to 8, It is characterized in that The method comprises the following steps: Step 1, providing SOI wafer and preparing for tape-out; Step 2, using photolithography and etching technology to etch an STI groove on the top Si layer of the SOI wafer; Step 3, performing STI deposition and radiation hardening treatment; Step 4, define the FG tube active area by photolithography and perform well implantation; Step 5, define the CG tube active area by photolithography and perform ion implantation; Step 6, depositing an oxide layer and etching away the area outside the gate oxide layer; Step 7, forming POLY by deposition and etching; Step 8, define the source, drain, and body positions by photolithography and perform ion implantation; Step 9, depositing an ILD dielectric layer, forming a through hole by etching, and depositing and CMPing to form a W plug; Step 10, forming an IDM dielectric layer by deposition and CMP, and etching and depositing to form an Al aluminum metal layer (14).
10. The preparation method according to claim 9, Features: In step 1, the silicon film of the SOI wafer is lightly doped with P type; the doping concentration is 1.5×10 15 cm -3 ; The silicon film of the SOI wafer is ≤500nm; In step 2, full dielectric isolation technology is used, that is, the depth of the STI trench is equal to the thickness of the top Si film; In step 5, the source and drain are implanted to the bottom, the thickness of the deep N-type implant layer (12) is completely equal to the thickness of the silicon film, and the doping concentration in the CG tube is 10 16 ~10 17 cm -3 .