Small oily coating integrated equipment for laboratory and application of small oily coating integrated equipment

By designing a small oil-based integrated equipment, the problems of unevenness and inefficiency in manual operation of oil-based coating diaphragms in laboratory are solved, and the uniformity and high efficiency of coating are achieved, reducing costs and energy consumption are suitable. Laboratory use and large-scale promotion.

CN118892961APending Publication Date: 2024-11-05DALIAN INSTITUTE OF CHEMICAL PHYSICS CHINESE ACADEMY OF SCIENCES
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411398831.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-09
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

Manual operation of traditional laboratory oil-coated diaphragms results in uneven coating and inefficient efficiency. Large-scale coating equipment is expensive and not suitable for early experiments, and there is a problem of slurry waste.

Method used

A small oil-based integrated equipment is designed, including an unwinding mechanism, a coating mechanism, a steam bath mechanism, a water washing mechanism and a drying mechanism, and uniformity is achieved through gravure rollers, steam bath guide rollers, a water washing guide rollers and a drying guide rollers. Coating and drying quickly, reducing errors and waste.

Benefits of technology

Improves the uniformity and efficiency of coating, reduces errors, saves energy and costs, is suitable for laboratory use, and achieves continuous production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118892961A_ABST
    Figure CN118892961A_ABST
Patent Text Reader

Abstract

The invention discloses small oily coating integrated equipment for a laboratory and application of the small oily coating integrated equipment, and belongs to the field of production and manufacturing of lithium battery diaphragms. The equipment comprises an unwinding mechanism, a coating mechanism, a steam bath mechanism, a water washing mechanism, a drying mechanism and a winding mechanism which are sequentially arranged in the belt conveying direction of the lithium ion battery diaphragm, the coating mechanism comprises a material box for storing oily slurry and a gravure roller for coating the surface of the lithium ion battery diaphragm with the oily slurry in the material box; a steam bath guide roller and a wet air circulating device which are horizontally and linearly arranged are arranged in the steam bath mechanism; the water washing mechanism comprises at least one water washing unit, and each water washing unit comprises a water washing tank and at least one water washing guide roller arranged in the water washing tank. The problem that continuous experiment of oily coating in a laboratory cannot be carried out is solved, meanwhile, the advantages of being uniform in coating thickness, good in film surface flattening, capable of continuously producing the oily coating diaphragm, small in occupied area, low in production cost and the like are achieved, and the device is suitable for large-scale popularization.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to a small-scale oily coating integrated equipment for laboratory use and its application, and belongs to the field of lithium battery diaphragm production and manufacturing. Background Art

[0002] Lithium batteries are gaining more and more attention due to their high energy storage, long battery life, and slow cycle decay. The core components of lithium batteries are positive electrodes, negative electrodes, separators, and electrolytes. The separators in the battery isolate the positive and negative electrodes from contact and prevent short circuits.

[0003] Traditional commercial diaphragms have poor heat resistance and no bonding effect with the positive and negative electrodes. At present, coated diaphragms are widely used. Ceramic or other materials are coated on the substrate through water-based or oil-based coating technology to improve the high temperature resistance or bonding performance of the diaphragm. Water-based coating is slurry coating with water as solvent, and oil-based coating is slurry coating with organic solvent as solvent. Since the bonding force between water-based coated diaphragms and the electrode pieces is much smaller than that between oil-based coated diaphragms and the wettability with the electrolyte is relatively poor, oil-based diaphragms are becoming more and more popular.

[0004] In the process of developing oily slurry, it is necessary to continuously coat the slurry on the substrate to evaluate the performance of the slurry or coated diaphragm. At present, the laboratory oily coating usually adopts manual single-piece coating, which is easy to cause uneven coating, low efficiency, and poor repeatability due to large manual errors. Large coating machines are expensive, and more slurry is used each time, which is easy to cause waste and is not suitable for initial experiments.

[0005] Therefore, it is urgent to develop a small-scale integrated oil coating equipment for laboratory use to improve the uniformity of coating and increase coating efficiency. Summary of the invention

[0006] In view of the shortcomings of the prior art, the purpose of this application is to overcome the problems of large errors, uneven coating, and low efficiency in manual coating of laboratory oil-coated diaphragms, while avoiding the waste of slurry caused by the use of large oil-coating machines, saving energy and reducing costs.

[0007] In one aspect of the present application, a small-scale oily coating integrated equipment for laboratory use is provided, comprising an unwinding mechanism, a coating mechanism, a steam bath mechanism, a water washing mechanism, a drying mechanism, and a winding mechanism sequentially arranged along the running direction of the lithium-ion battery separator; The coating mechanism includes a material box for storing oily slurry and a gravure roller for coating the oily slurry in the material box onto the surface of the lithium-ion battery separator; The steam bath mechanism is provided with steam bath guide rollers and a wet air circulation device arranged horizontally and linearly; The water washing mechanism comprises at least one water washing unit, wherein the water washing unit comprises a water washing tank and at least one water washing guide roller placed in the water washing tank; The drying mechanism is provided with at least one drying unit arranged in a horizontal straight line; The drying unit is provided with drying guide rollers and wind knives which are arranged horizontally and linearly.

[0008] Optionally, the steam bath guide roller and the wet air circulation device provided in the steam bath mechanism can meet the temperature and humidity requirements of different needs in the system.

[0009] Optionally, the drying mechanism can achieve rapid drying of the diaphragm and maintain sufficient flatness.

[0010] Optionally, the water washing mechanism comprises a first water washing tank, a second water washing tank and a third water washing tank which are sequentially arranged along the running direction of the lithium-ion battery diaphragm; The first washing tank is provided with a first washing guide roller for passing the pre-solidified lithium-ion battery separator in the washing liquid; The second water washing tank is provided with a second water washing guide roller for passing the lithium ion battery separator after passing through the first water washing tank in the water washing liquid; The third water washing tank is provided with a third water washing guide roller for allowing the lithium ion battery separator after passing through the second water washing tank to pass through the washing liquid.

[0011] Optionally, the first water washing guide roller, the second water washing guide roller and the third water washing guide roller are all located below the liquid surface of the washing liquid.

[0012] Optionally, discharge turning guide rollers are provided on the upper sides of the discharge ports of the first water washing tank, the second water washing tank and the third water washing tank.

[0013] Optionally, the drying mechanism includes a first drying unit and a second drying unit; The first drying unit includes a first oven and a drying guide roller and an air knife located in the first oven; The second drying unit includes a second oven and a drying guide roller and an air knife located in the second oven.

[0014] Optionally, the small-scale oily coating integrated equipment for laboratory use further comprises a frame, and the steam bath mechanism is located above the frame; The first water washing tank and the second water washing tank are located above the frame; The drying mechanism is located below the frame; The third washing tank is located below the frame.

[0015] Optionally, the small-scale oily coating integrated equipment for laboratory use has a length of 1.5-2.0 m and a height of 1.0-1.5 m.

[0016] Another aspect of the present application provides an application of the above-mentioned laboratory small oily coating integrated equipment in the preparation of lithium-ion battery separators, the application comprising: Step (S1): placing the lithium-ion battery separator to be coated on an unwinding mechanism, and clamping the inner wall of the tube core of the lithium-ion battery separator; Step (S2): placing the oily coating slurry in a material box, unwinding the lithium-ion battery separator through an unwinding mechanism, transferring the slurry in the material box to a gravure roller, and sequentially subjecting the lithium-ion battery separator to oily coating by the gravure roller, pre-solidification by a steam bath mechanism, washing by a water washing mechanism, and drying by a drying mechanism, and then receiving the membrane by a winding mechanism.

[0017] Optionally, when the oily coating adopts a pre-coagulation method of a multi-stage coagulation bath, in step (S2): the steam bath mechanism is turned off, and the first water washing tank, the second water washing tank and the third water washing tank in the water washing mechanism are respectively filled with liquids required for the coagulation bath; Or, when the oily coating adopts the pre-solidification method of the steam bath, in step (S2): the lithium ion battery separator is pre-solidified by the steam bath mechanism, and then sequentially washed by the first water washing tank, the second water washing tank and the third water washing tank; Alternatively, when the oily coating adopts a mixed pre-coagulation method of a steam bath and a coagulation bath, in step (S2): the lithium-ion battery diaphragm is pre-coagulated by a steam bath mechanism, pre-coagulated by a first water washing tank coagulation bath, and then washed by a second water washing tank and a third water washing tank in sequence, wherein the first water washing tank is filled with liquid required for the coagulation bath; or the lithium-ion battery diaphragm is pre-coagulated by a steam bath mechanism, pre-coagulated by a first water washing tank and a second water washing tank in sequence, and then washed by a third water washing tank, wherein the first water washing tank and the second water washing tank are respectively filled with liquids required for the coagulation bath.

[0018] Optionally, in the application, the coating thickness error of the lithium-ion battery separator is within ±0.2µm; The effective width of coating is 20~40cm; The coating efficiency is 5~20m / h.

[0019] As a specific implementation method, the technical solution of the present application includes a small laboratory oily coating integrated equipment and a method of use, including an unwinding system, a coating system, a steam bath system, a water washing system, a drying system and a winding system arranged in sequence along the diaphragm belt direction.

[0020] The membrane substrate is sequentially unwound by the unwinding system, coated by the coating system, pre-solidified by the steam bath system, solidified and washed by the water washing system, dried by the drying system, and stored by the winding system.

[0021] The specific method of use includes the following steps: 1) Uncoated lithium-ion battery separators of different specifications are placed on an unwinding roller, and the inner wall of the battery separator tube core is clamped; 2) The battery separator is coated by a gravure roller, pre-solidified by a steam bath system, washed by a water washing system, dried by a drying system, and finally collected by a winding system.

[0022] The beneficial effects of this application include: 1) Suitable size for laboratory use.

[0023] 2) The coating thickness is uniform, with an error within ±0.2µm, which improves coating efficiency and coating quality.

[0024] 3) It solves the problem that laboratory oily coating cannot be continuously tested, and at the same time achieves the advantages of uniform coating thickness, good membrane flatness, continuous production of oily coated diaphragms, small footprint, and low production cost, which is suitable for large-scale promotion. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 This is a schematic diagram of a small-scale integrated oily coating equipment for laboratory use.

[0026] List of parts and reference numerals: 1. Unwinding mechanism; 2. Lithium-ion battery separator; 3. Over-roller; 4. Gravure roller; 5. Material box; 6. Steam bath mechanism; 7. Steam bath guide roller; 8. First water washing tank; 9. Second water washing tank; 10. Third water washing tank; 11. First water washing guide roller; 12. Second water washing guide roller; 13. Third water washing guide roller; 14. Discharging turning guide roller; 15. First drying oven; 16. Second drying oven; 17. Drying guide roller; 18. Air knife; 19. Winding mechanism. DETAILED DESCRIPTION

[0027] The present application is described in detail below with reference to embodiments, but the present application is not limited to these embodiments.

[0028] like Figure 1As shown, a small laboratory oily coating integrated equipment includes an unwinding mechanism 1, a coating mechanism, a steam bath mechanism 6, a water washing mechanism, a drying mechanism and a winding mechanism 19 arranged in sequence along the running direction of the diaphragm. The total length of the fuselage is 1.5m and the total height is 1.2m. The coating mechanism includes a material box 5 for storing oily slurry and a gravure roller 4 for coating the oily slurry in the material box 5 onto the surface of the diaphragm, and a roller 3 is provided between the unwinding mechanism 1 and the coating mechanism. The steam bath mechanism 6 is provided with a steam bath guide roller 7 and a wet air circulation device arranged horizontally and linearly, which can meet the temperature and humidity requirements of different requirements in the system. The water washing mechanism is provided with a first water washing tank 8, a second water washing tank 9 and a third water washing tank 10 arranged in sequence along the running direction of the lithium-ion battery diaphragm 2. The drying mechanism is provided with a first oven 15 and a second oven 16 arranged in sequence along the running direction of the lithium-ion battery diaphragm 2. The first washing tank 8 is provided with a first washing guide roller 11 for passing the pre-solidified diaphragm in the washing liquid, the second washing tank 9 is provided with a second washing guide roller 12 for passing the diaphragm after passing the first washing tank 8 in the washing liquid, the third washing tank 10 is provided with a third washing guide roller 13 for passing the diaphragm after passing the second washing tank 9 in the washing liquid, and a discharge turning guide roller 14 is provided between the first washing tank 8 and the second washing tank 9, between the second washing tank 9 and the third washing tank 10, and between the third washing tank 10 and the first drying oven 15, and the first washing guide roller 11, the second washing guide roller 12 and the third washing guide roller 13 are all located below the liquid surface of the washing liquid. The first drying oven 15 and the second drying oven 16 are both provided with drying guide rollers 17 and wind knives 18 arranged horizontally and linearly, which can achieve rapid drying of the diaphragm and maintain sufficient flatness. It should be noted that the water washing tank will change the type of liquid in the water washing tank according to the experimental requirements, and the steam bath mechanism 6 can also be used according to the experimental requirements. If the oily coating adopts a multi-stage coagulation bath instead of a steam bath pre-coagulation method, the steam bath can be removed, and the three water washing tanks are placed with the liquid required for the coagulation bath according to the requirements. If the oily coating adopts a steam bath pre-coagulation method, the coated diaphragm will be pre-coagulated in the steam bath in turn, then washed in the water washing tank, and finally dried and rolled. If the oily coating adopts a steam bath + coagulation bath pre-coagulation method, the coated diaphragm will be pre-coagulated in the steam bath in turn, and then the first water washing tank 8 or the first water washing tank 8 and the second water washing tank 9 will be changed to a coagulation bath as needed, and then washed in the third water washing tank 10, and finally dried and rolled.

[0029] Example 1 Using the above equipment, the prepared aramid oily coating slurry is placed in the material box 5, and the lithium-ion battery separator 2 is unwound by the unwinding mechanism 1, wherein the unwinding rate is 7 meters / hour, and the slurry in the material box 5 is transferred to the gravure roller 4, and then transferred to the lithium-ion battery separator 2 for coating. After the coating is completed, uncured slurry adheres to the lithium-ion battery separator 2; then the lithium-ion battery separator 2 enters the steam bath mechanism 6, and under the action of water vapor, the slurry is pre-solidified, and then enters the first water washing tank 8, the second water washing tank 9, and the third water washing tank 10 in turn, and is washed with water under the traction of the first water washing guide roller 11, the second water washing guide roller 12 and the third water washing guide roller 13 to remove residual solvents and other water-soluble substances; then it enters the first oven 15 and the second oven 16 simultaneously, and is dried by the drying guide roller 17 and the wind knife 18 to ensure the drying of the separator; finally, it is wound by the winding mechanism 19. According to the measurement, the effective coating width is 20cm and the coating layer thickness is between 1.2±0.05µm.

[0030] Example 2 Using the above equipment, the prepared aramid oily coating slurry is placed in the material box 5, a mixed solution of 75wt% NMP (N-methylpyrrolidone) + 25wt% H2O is placed in the first water washing tank 8, a mixed solution of 55wt% NMP + 45wt% H2O is placed in the second water washing tank 9, and 100wt% H2O is placed in the third water washing tank 10. The lithium-ion battery separator 2 is unwound by the unwinding mechanism 1, wherein the unwinding rate is 20 m / h, the slurry in the material box 5 is transferred to the gravure roller 4, and then transferred to the lithium-ion battery separator 2 for coating. After the coating is completed, the lithium-ion battery separator 2 is adhered with uncured slurry; the steam bath mechanism 6 is turned off, and then the lithium-ion battery separator 2 enters the first water washing tank 8, the second water washing tank 9, and the third water washing tank 10 through the steam bath mechanism 6 for pre-solidification, and pre-solidifies under the traction of the first water washing guide roller 11, the second water washing guide roller 12 and the third water washing guide roller 13; then it enters the first oven 15 and the second oven 16 synchronously, and is dried by the drying guide roller 17 and the wind knife 18 to ensure the drying of the separator; finally, the winding is realized by the winding mechanism 19. According to measurement, the effective coating width is 20 cm, and the coating layer thickness is between 1.0±0.05µm.

[0031] Example 3 By using the above equipment, the prepared aramid oily coating slurry is placed in the material box 5, and the lithium-ion battery separator 2 is unwound by the unwinding mechanism 1, wherein the unwinding rate is 5 m / h, and the slurry in the material box 5 is transferred to the gravure roller 4, and then transferred to the lithium-ion battery separator 2 for coating. After the coating is completed, uncured slurry adheres to the lithium-ion battery separator 2; then the lithium-ion battery separator 2 is placed in the steam bath mechanism 6, and the slurry is pre-solidified under the action of water vapor, and then enters the first water washing tank 8 (the first water washing tank 8 is placed in the first water washing tank 8). 55wt%NMP+45wt%H2O), pre-solidified in a coagulation bath under the traction of the first water washing guide roller 11, then sequentially enter the second water washing tank 9 and the third water washing tank 10, and wash under the traction of the second water washing guide roller 12 and the third water washing guide roller 13 to remove residual solvents and other water-soluble substances; then enter the first oven 15 and the second oven 16 simultaneously, dry through the drying guide roller 17 and the wind knife 18 to ensure the drying of the diaphragm; finally, rewind through the rewinding mechanism 19. According to measurement, the effective width of the coating is 40cm, and the thickness of the coating layer is between 1.1±0.05µm.

[0032] As mentioned above, gravure coating can ensure the uniformity of coating, ensure the coating effect of lithium-ion battery separators, and ensure continuous and stable operation, which well solves the problem of uneven manual coating and difficulty in repeatability. At the same time, the equipment is simple and efficient, and can be operated by one person, and the production cost is low, which is suitable for laboratory use.

[0033] The above are only a few embodiments of the present application and do not constitute any form of limitation to the present application. Although the present application is disclosed as above with preferred embodiments, it is not intended to limit the present application. Any technician familiar with the profession, without departing from the scope of the technical solution of the present application, using the technical content disclosed above to make slight changes or modifications are equivalent to equivalent implementation cases and fall within the scope of the technical solution.

Claims

1. A small oily coating integrated equipment for laboratory use, It is characterized in that It comprises an unwinding mechanism (1), a coating mechanism, a steam bath mechanism (6), a washing mechanism, a drying mechanism and a winding mechanism (19) which are arranged in sequence along the running direction of the lithium-ion battery separator (2); The coating mechanism comprises a material box (5) for storing oily slurry and a gravure roller (4) for coating the oily slurry in the material box (5) onto the surface of the lithium-ion battery separator (2); The steam bath mechanism (6) is provided with steam bath guide rollers (7) and a wet air circulation device arranged horizontally and linearly; The water washing mechanism comprises at least one water washing unit, wherein the water washing unit comprises a water washing tank and at least one water washing guide roller placed in the water washing tank; The drying mechanism is provided with at least one drying unit arranged in a horizontal straight line; The drying unit is provided with drying guide rollers (17) and air knives (18) arranged in a horizontal straight line.

2. The small-sized oily coating integrated equipment for laboratory use according to claim 1, It is characterized in that The water washing mechanism comprises a first water washing tank (8), a second water washing tank (9) and a third water washing tank (10) which are arranged in sequence along the running direction of the lithium-ion battery separator (2); The first washing tank (8) is provided with a first washing guide roller (11) for allowing the pre-solidified lithium-ion battery separator (2) to pass through the washing liquid; The second water washing tank (9) is provided with a second water washing guide roller (12) for allowing the lithium ion battery separator (2) that has passed through the first water washing tank (8) to pass through the washing liquid; The third water washing tank (10) is provided with a third water washing guide roller (13) for allowing the lithium ion battery separator (2) that has passed through the second water washing tank (9) to pass through the washing liquid.

3. The small-sized oily coating integrated equipment for laboratory use according to claim 2, It is characterized in that The first water washing guide roller (11), the second water washing guide roller (12) and the third water washing guide roller (13) are all located below the liquid surface of the washing liquid.

4. The small-sized oily coating integrated equipment for laboratory use according to claim 2, It is characterized in that Discharge turning guide rollers (14) are provided on the upper sides of the discharge ports of the first water washing tank (8), the second water washing tank (9) and the third water washing tank (10).

5. The small-sized oily coating integrated equipment for laboratory use according to claim 1, It is characterized in that The drying mechanism comprises a first drying unit and a second drying unit; The first drying unit comprises a first drying oven (15) and a drying guide roller (17) and an air knife (18) located in the first drying oven (15); The second drying unit comprises a second drying oven (16) and a drying guide roller (17) and an air knife (18) located in the second drying oven (16).

6. The small-sized oily coating integrated equipment for laboratory use according to claim 2, It is characterized in that The small-scale oily coating integrated equipment for laboratory use also includes a frame, and the steam bath mechanism (6) is located above the frame; The first water washing tank (8) and the second water washing tank (9) are located above the frame; The drying mechanism is located below the frame; The third water washing tank (10) is located below the frame.

7. The small-sized oily coating integrated equipment for laboratory use according to claim 1, It is characterized in that The small-scale oily coating integrated equipment for laboratory use has a length of 1.5-2.0 m and a height of 1.0-1.5 m.

8. Use of the small-scale oily coating integrated equipment for laboratory use according to any one of claims 1 to 7 in the preparation of lithium-ion battery separators, It is characterized in that The applications include: Step (S1): placing the lithium-ion battery separator (2) to be coated on the unwinding mechanism (1), and clamping the inner wall of the tube core of the lithium-ion battery separator (2); Step (S2): placing the oily coating slurry in a material box (5), unwinding the lithium-ion battery separator (2) through an unwinding mechanism (1), transferring the slurry in the material box (5) to a gravure roller (4), and sequentially subjecting the lithium-ion battery separator (2) to oily coating by the gravure roller (4), pre-solidification by a steam bath mechanism (6), washing by a water washing mechanism, and drying by a drying mechanism before being received by a rewinding mechanism (19).

9. The use according to claim 8, It is characterized in that When the oily coating adopts a pre-coagulation method of a multi-stage coagulation bath, in step (S2): the steam bath mechanism (6) is turned off, and the first water washing tank (8), the second water washing tank (9) and the third water washing tank (10) in the water washing mechanism are respectively filled with liquids required for the coagulation bath; Alternatively, when the oily coating is pre-solidified by a steam bath, in step (S2): the lithium-ion battery separator (2) is pre-solidified by a steam bath mechanism (6), and then sequentially washed by a first water washing tank (8), a second water washing tank (9), and a third water washing tank (10); Alternatively, when the oily coating adopts a mixed pre-coagulation method of a steam bath and a coagulation bath, in step (S2): the lithium-ion battery diaphragm (2) is pre-coagulated by a steam bath mechanism (6), pre-coagulated by a first water washing tank (8) and then washed by a second water washing tank (9) and a third water washing tank (10), wherein the first water washing tank (8) contains a liquid required for the coagulation bath; or the lithium-ion battery diaphragm (2) is pre-coagulated by a steam bath mechanism (6), pre-coagulated by a first water washing tank (8) and a second water washing tank (9) and then washed by a third water washing tank (10), wherein the first water washing tank (8) and the second water washing tank (9) contain liquids required for the coagulation bath, respectively.

10. The use according to claim 8, It is characterized in that In the application, the coating thickness error of the lithium-ion battery separator (2) is within ±0.2 µm; The effective width of coating is 20~40cm; The coating efficiency is 5~20m / h.

Citation Information

Patent Citations

  • High-temperature-resistant para-aramid coated lithium ion battery diaphragm and preparation method thereof

    CN112531285A

  • Preparation method of aramid fiber / garnet type solid electrolyte coated diaphragm

    CN115863909A

  • Preparation method of diaphragm, diaphragm and alkaline electrolysis device

    CN118007185A

  • Efficient coating system for oily diaphragm

    CN215695308U

  • Display panel and manufactuinf method for the same

    KR1020240126901A