Manufacturing method of high-heat-dissipation aluminum-based multilayer rigid-flexible combined board

During the production process of aluminum-based multi-layer rigid-flex bonding plate, the aluminum-based copper clad plate is separated and pressed with the flexible circuit board layer, and combined with the browning and airbag structure, the bias and layering problems in the prior art are solved. The efficient production of aluminum-based multi-layer rigid-flex bonding plate is achieved, ensuring the stability of the outer circuit pattern and the accuracy of the through holes.

CN118900518AActive Publication Date: 2024-11-05深せん市実锐泰科技有限公司

Patent Information

Application Number
CN202410984337.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-05
Estimated Expiration
2044-07-22

AI Technical Summary

Technical Problem

The prior art is prone to problems such as bias, open or short circuit of outer circuit pattern, overflow of glue in holes and deep-controlled milling when making aluminum-based multi-layer rigid-flex bonding plates, resulting in unsolid compression and layering. .

Method used

By splitting the multi-layer flexible circuit board structure into the first copper layer and the multi-layer flexible board core board layer, firstly attach the copper layer to the aluminum substrate and press it to form an aluminum-based copper clad plate, and then gradually add the covering film layer and The overall pressing is carried out, combined with browning and pin matching, a reverse structure and airbag pressing mold is used to ensure positioning and flatness, and finally plating and back drilling are carried out to correct the through holes.

Benefits of technology

Effectively prevent the deviation and layering of aluminum substrate and multi-layer flexible circuit board when pressed, improve the stability of outer circuit pattern and the accuracy of through holes, avoid glue spills and deep-controlled milling in the holes. The difficulty of cutting improves the overall pressing quality and heat dissipation performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118900518A_ABST
    Figure CN118900518A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a high-heat-dissipation aluminum-based multi-layer rigid-flex board, which comprises the following steps of: splitting the structure of the multi-layer rigid-flex board into a first copper layer and a multi-layer flexible board core board layer, attaching the first copper layer to an aluminum substrate, manufacturing circuit patterns and through holes including pin holes, then windowing, and manufacturing other layers to form the core board layer, then manufacturing an adhesive layer, attaching a covering film layer, manufacturing a through hole including a pin hole, taking a second covering film layer including a covering film pin hole, stacking and pressing all layers, and then performing electroplating processing and back drilling processing to form the aluminum-based multilayer rigid-flexible combined board; according to the manufacturing method, the problems of deviation and displacement of lamination of the aluminum substrate and the multi-layer flexible plate, the problem of short circuit or open circuit caused by surface depression, the problem of large vibration of a depth-controlled milling plate, and the problems of multilayer flexible plate hole deflection, glue overflow in the hole and the like caused by lamination can be effectively prevented.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of manufacturing flexible circuit boards or rigid-flexible boards, and in particular to a method for manufacturing a high-heat dissipation aluminum-based multilayer rigid-flexible board. Background Art

[0002] For a type of rigid-flexible board used in smart connected cars and low-altitude aircraft, it is not only required to have flexible installation characteristics, but also needs to have the ability to carry multiple signal transmissions. Therefore, it is designed as a multi-layer flexible board structure. In addition, it is also required to have high heat dissipation performance. Therefore, an aluminum base layer is selected as the heat dissipation layer, and the overall structure forms an aluminum-based rigid-flexible board.

[0003] In the prior art, aluminum-based multi-layer rigid-flexible boards are generally made in a similar manner to ordinary rigid-flexible boards, that is, a multi-layer flexible board layer is made, a covering film is attached to the area that will subsequently form the flexing area of ​​the rigid-flexible board, an aluminum substrate is made, and a blind groove is made on the edge of the area where the aluminum substrate needs to be uncovered, the aluminum substrate and the multi-layer flexible board layer are pressed together, and then the outer layer circuit pattern is made and the surface covering film is attached, and then the cover is opened to form an aluminum-based rigid-flexible board.

[0004] The disadvantages of the prior art are: The expansion and contraction rate of the multi-layer flexible board is much greater than that of the aluminum substrate, and the thickness of the aluminum substrate is generally thicker. If the pressing force is too large when the two are pressed together, it is easy to cause excessive expansion and contraction, deviation and displacement problems, or the thickness of the aluminum substrate is too thick, which may cause deviation and displacement problems during the pressing process. If the pressing force is too small, it is easy to cause problems of loose pressing and delamination.

[0005] A method of making blind grooves on an aluminum substrate and then pressing and then making outer circuits. After pressing, the outer circuit pattern is made. The multi-layer flexible board layer corresponding to the blind groove position is prone to depression, which is prone to short circuit or open circuit when making the outer circuit pattern.

[0006] Since the multi-layer flexible board layers are first manufactured and then pressed together, the holes of the multi-layer flexible board layers are electroplated to form via holes, which may easily cause problems such as skewed via holes and glue overflow in the holes during pressing together.

[0007] During the cover removal process, a depth-controlled milling plate is used. It is difficult to control the depth. If the depth is too large, the surface of the multi-layer flexible board layer may be easily damaged. If the depth is too small, the aluminum substrate will not be milled enough and it will be difficult to remove the cover. In addition, the depth-controlled milling plate requires the use of a milling cutter for transverse milling. The vibration generated during the process is large, which may easily cause problems such as delamination between the aluminum substrate and the multi-layer flexible board layer.

[0008] Based on the above background and problems, it is necessary to provide a method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board. Summary of the invention

[0009] The present invention aims to solve the problems of easy deviation, open circuit or short circuit of outer circuit pattern, glue overflow in hole, and easy damage of multi-layer flexible board by controlled depth milling when making aluminum-based multi-layer rigid-flexible board in the prior art, and proposes a method for making a high heat dissipation aluminum-based multi-layer rigid-flexible board, comprising the following steps: S10: splitting the structure of the multi-layer rigid-flexible board into a first copper layer and a multi-layer flexible board core layer, taking an aluminum substrate and a first adhesive layer, sequentially attaching the first adhesive layer and the first copper layer to the surface of the aluminum substrate, and pressing them together to form an aluminum-based copper-clad board.

[0010] S20: making a copper layer circuit pattern on the first copper layer of the aluminum-based copper-clad laminate, and making an aluminum substrate through hole, wherein the aluminum substrate through hole includes an aluminum substrate pin hole, and then making an aluminum substrate window area to form a window aluminum substrate.

[0011] S30: Produce a core board layer of a multi-layer flexible board according to an established process, and form a surface graphic layer of the core board layer; take a second adhesive layer, and attach the second adhesive layer to the core board layer; then take a first covering film, produce a first covering film pattern to form a first covering film layer, and attach the first covering film layer to the surface of the second adhesive layer, wherein the first covering film layer corresponds to the window area of ​​the aluminum substrate; form a covering film flexible board as a whole; make covering film flexible board through holes on the covering film flexible board, wherein the covering film flexible board through holes include flexible core board pin holes; and form a flexible adhesive board as a whole by processing.

[0012] S40: taking a second covering film, making a second covering film pattern to form a second covering film layer, wherein the second covering film pattern includes covering film pin holes; stacking the second covering film layer, the flexible adhesive plate, and the windowed aluminum substrate in sequence from bottom to top, placing them in a pressing device for whole-board pressing; and forming a pressed plate as a whole.

[0013] S50: performing electroplating processing on the laminated board and performing back drilling processing to form the aluminum-based multi-layer rigid-flexible board.

[0014] Furthermore, the whole plate lamination also includes: making a lamination mold, the surface of the lamination mold is provided with pins, and the lamination mold is set on the lower table surface of the lamination equipment; the stacking from bottom to top includes: the pin holes of the covering film, the pin holes of the flexible core board, and the pin holes of the aluminum substrate are correspondingly mounted on the pins from bottom to top.

[0015] Furthermore, the whole-board lamination further comprises: making an airbag, wherein the airbag is a structure inflated inside the sealed plastic layer, and the airbag is arranged on the upper surface of the lamination device.

[0016] Furthermore, the forming of the laminated plate also includes: taking a third adhesive layer and making an adhesive layer window area, the adhesive layer window area corresponds to the first covering film layer, and making an adhesive layer through hole, the adhesive layer through hole includes an adhesive layer pin hole; forming a window adhesive layer as a whole; the stacking from bottom to top includes: correspondingly putting the covering film pin hole, the flexible core board pin hole, the adhesive layer pin hole, and the aluminum substrate pin hole on the pin in sequence from bottom to top.

[0017] Furthermore, after the window area of ​​the aluminum substrate is made, browning processing is performed.

[0018] Furthermore, before the electroplating process is performed on the laminated board, the laminated board needs to be drilled, and the drilling is performed according to the drilling pattern of the aluminum-based multi-layer rigid-flexible board.

[0019] Furthermore, after the drilling process, the pressed plate is sequentially subjected to laser ablation, plasma treatment, and alkaline washing treatment; the laser ablation is laser ablation of the stepped position of the window area of ​​the aluminum substrate and the first covering film layer.

[0020] Furthermore, the size of the window area of ​​the aluminum substrate is smaller than the size of the first covering film layer on one side.

[0021] Furthermore, the back drilling process is back drilling the through holes of the aluminum substrate.

[0022] Furthermore, the pressing equipment is a rigid plate press; the parameters for the whole plate pressing are a heating rate of 2°C / minute to 6°C / minute, a maximum temperature of 160°C to 180°C, a pressure of 15kg / cm2 to 25kg / cm2, and a cooling rate of 10°C / minute to 20°C / minute.

[0023] The technical solution of the present invention is to split the structure of the multi-layer flexible circuit board, first press the outer circuit layer on the aluminum substrate to form a reverse structure, and then press it with other prepared layers, combined with browning processing, pin matching pin hole processing method, effectively prevent the aluminum substrate and the multi-layer flexible circuit board from being easily offset and shifted during the pressing process due to the large difference in expansion and contraction rates. The windowed aluminum substrate is first made (a single aluminum substrate is formed), and then the outer circuit pattern and covering film layer of the flexible circuit board are made through the above-mentioned reverse structure, and the lower table is provided with a pressing mold, and the upper table is provided with an airbag pressing layout structure, and the lower table is formed during pressing. The effective positioning process of the table and the overall pressing process of the upper table during the molding process can effectively improve the problem of short circuit or open circuit of the circuit pattern caused by the depression on the surface of the flexible circuit board after pressing; and the use of the first-made window aluminum substrate (forming a single aluminum substrate) can effectively prevent the large vibration caused by the use of the controlled depth milling plate from causing the delamination problem between the aluminum substrate and the multi-layer flexible circuit board; by first making a through hole, repairing the hole after the overall pressing, and electroplating to form a via hole, and then back-drilling the hole of the aluminum substrate layer, the via hole of the multi-layer flexible circuit board is effectively made, which prevents the problems of hole skewness and glue overflow in the hole caused by pressing after the via holes of the multi-layer flexible circuit board are made first. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.

[0025] Figure 1 is a process flow chart of an embodiment of the present invention; Figure 2 A schematic diagram of the cross-sectional structure of an aluminum-based copper-clad laminate produced according to an embodiment of the present invention; Figure 3 A schematic diagram of the cross-sectional structure of an aluminum-based graphic plate produced according to an embodiment of the present invention; Figure 4 A schematic diagram of the planar structure of a separate aluminum substrate formed as a whole according to an embodiment of the present invention; Figure 5 It is a schematic diagram of the cross-sectional structure of the flexible adhesive sheet formed in the embodiment of the present invention; Figure 6 It is a schematic cross-sectional structure diagram of a pressed typesetting structure according to an embodiment of the present invention; Figure 7 A schematic diagram of the cross-sectional structure of a press plate formed in accordance with an embodiment of the present invention; Figure 8 The cross-sectional structure diagram of an aluminum-based multi-layer rigid-flexible board produced according to an embodiment of the present invention is shown.

[0026] Description of Figure Numbers: Label name Label name 10 Aluminum-based copper clad laminate 30B First covering film layer 110 Aluminum substrate 310B Covering film pin hole 120 First glue layer 30C Second covering film layer 130 First copper layer 310C Glue layer window area 20 Window aluminum substrate 3110C Glue layer through hole 210 Aluminum substrate through hole 3111C Glue layer pin hole 2110 Aluminum base plate pin hole 410 Stacked structure 220 Aluminum substrate window area 420 Lower countertop 1310 Copper layer circuit pattern 430 Mold surface 1311 Brown surface 430A Pin 230 Single aluminum substrate 4310 First release film 2310 Aluminum substrate connecting wire 4320 Laminating film 30 Flexible adhesive sheet 4330 Second release film 30A Core layer 4340 The third release film 310 Cover Film Flexible Board Through Hole 440 Airbag 3110 Flexible core pin holes 450 On the stage 320 Surface Graphics Layer 50 Pressed board 330 Insulation dielectric layer 510 Trimming holes 340 Inner Graphics Layer 520 Glue overflow 350 Second adhesive layer 60 Aluminum-based multi-layer rigid-flex board 360 First covering film layer 610 Electroplated copper layer 40 Pressed layout structure 620 Back drilling The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION

[0027] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0028] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back, inside, outside...) are only used to explain the relative position relationship, movement status, etc. between the components in a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.

[0029] In addition, in the present invention, descriptions such as "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0030] In addition, the technical solutions between the various embodiments of the present invention can be combined with each other, but it must be based on the fact that ordinary technicians in the field can implement it. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.

[0031] See also Figure 1 , Figure 1 It is a process flow chart of the production method of the present invention.

[0032] The method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board according to an embodiment of the present invention includes: Figure 1 The key process flow shown in the figure has specific implementation steps as follows.

[0033] Step S10: The structure of the multi-layer rigid-flexible board is split into a first copper layer and a multi-layer flexible board core layer. The aluminum substrate 110 and the first adhesive layer 120 are taken, and the first adhesive layer 120 and the first copper layer 130 are sequentially attached to the surface of the aluminum substrate 110 and pressed together to form an aluminum-based copper clad laminate 10.

[0034] This embodiment splits the original multi-layer flexible circuit board structure according to the number of copper layer circuit layers, and independently manufactures one of the surface circuit layers on the aluminum substrate 110 to form an aluminum-based copper-clad laminate 10. The other layers are processed through a post-process to form a flexible adhesive sheet 30, so that the aluminum substrate 110 is first attached with a first adhesive layer 120 and a first copper layer 130, so as to facilitate the expansion and contraction matching of the aluminum-based copper-clad laminate 10 and the flexible adhesive sheet 30 formed by subsequent processing, and prevent the problem of displacement and displacement during pressing.

[0035] Step S20: A copper layer circuit pattern 1310 is made on the first copper layer 130 of the aluminum-based copper clad laminate 10, and an aluminum substrate through hole 210 is made, wherein the aluminum substrate through hole 210 includes an aluminum substrate pin hole 2110, and then an aluminum substrate window area 220 is made, followed by browning to form a browning surface 1311; the windowed aluminum substrate 20 is formed as a whole.

[0036] The first copper layer 130 is used to make the copper layer circuit pattern 1310, which is processed according to the outer layer circuit pattern in contact with the aluminum substrate 110 in accordance with the original design of the multi-layer flexible circuit board, that is, the outer layer circuit pattern of the multi-layer flexible circuit board is transferred to the aluminum substrate 110 for processing; the aluminum substrate window area 220 is the position of the flexure area of ​​the aluminum-based rigid-flexible composite board 60 that is finally formed; the role of browning is to make the copper surface form a more effective uniform rough surface, increase the friction and bonding force between the pressed layers, and form a better bonding force with other adhesive layers during subsequent pressing, and prevent the problem of lamination displacement and displacement; the aluminum substrate pin hole 2110 is used to match the pin 430A of the pressing mold 430 during subsequent pressing. It is worth noting that if there is a through hole with an aperture greater than or equal to 0.5 mm on the surface of the copper layer circuit pattern 1310, and the through hole needs to be connected to the through holes of other layers in the future, then the aluminum substrate pin hole 2110 can be made at the position of such through hole.

[0037] It is worth mentioning that after the windows are opened on the aluminum substrate, individual independent aluminum substrates 230 to be pressed together may be formed. At the same time, the flexible circuit board is processed in a panelizing manner during the processing. There is a "tool graphic area" on the panel structure surface, which is the invalid area that needs to be removed in the end. The position distribution of the tool graphic area corresponding to the aluminum substrate and the position graphic of the individual aluminum substrate 230 to be bonded can be used to set aluminum substrate connecting lines 2310 between the individual aluminum substrates 230, so that the individual aluminum substrates 230 form a whole, which is convenient for subsequent bonding and pressing processing.

[0038] Step S30: The core layer 30A of the multi-layer flexible board is manufactured according to the established process, and the surface pattern layer 320 of the core layer 30A is formed. The core layer 30A is the other layers of the originally designed multi-layer flexible circuit board except the first copper layer 130 transferred to the aluminum substrate 110, for example Figure 5 As shown in , a double-sided flexible copper-clad laminate including an insulating dielectric layer 330 is taken to make double-sided patterns, namely a surface pattern layer 320 and an inner pattern layer 340 .

[0039] Take the second adhesive layer 350 and attach the second adhesive layer 350 to the core board layer 30A; since the core board layer 30A needs to be pressed with the window aluminum substrate 10 later, the second adhesive layer 350 plays the role of bonding and interlayer insulation. The second adhesive layer 350 is equivalent to the insulating medium layer under the copper layer circuit pattern 1310 of the original multi-layer flexible circuit board structure.

[0040] Then, the first covering film is taken, and a first covering film pattern is made to form a first covering film layer 360 , and the first covering film layer 30B is attached to the surface of the second adhesive layer 340 , and the first covering film layer 360 corresponds to the aluminum substrate window area 220 , and the size of the aluminum substrate window area 220 is smaller than the size of the first covering film layer 360 on one side.

[0041] The first covering film layer 360 is the covering film layer of the flexing area of ​​the aluminum-based rigid-flexible composite board that is finally formed. Therefore, the first covering film layer 360 is set corresponding to the aluminum substrate window area 220. At the same time, the first covering film layer 360 needs to be pressed under the window aluminum substrate 10. Therefore, the size of the aluminum substrate window area 220 needs to be smaller than the size of the first covering film layer 360 on one side. Generally, the size of one side is 10μm to 50μm smaller. The overall processing forms a covering film flexible board.

[0042] A covering film flexible board through hole 310 is made on the covering film flexible board, and the covering film flexible board through hole 310 includes a flexible core board pin hole 3110; the flexible board pin hole 3110 is made, which is also used to match the pin 430A of the pressing mold during subsequent pressing; the whole is processed to form a flexible adhesive board 30.

[0043] Step S40: Take the second covering film, make a second covering film pattern to form a second covering film layer 30B, the second covering film pattern includes a covering film pin hole 310B; the covering film pin hole 310B is also used for matching the pin of the pressing mold 4310 during subsequent pressing.

[0044] In one embodiment, a third adhesive layer is taken and an adhesive layer window area 310C is made, the adhesive layer window area 310C corresponds to the first covering film layer 360, and an adhesive layer through hole 3110C is made, the adhesive layer through hole 3110C includes an adhesive layer pin hole 3111C; a window adhesive layer 30C is formed as a whole.

[0045] Since the second adhesive layer 350 already exists, the window adhesive layer 30C is an optional adhesive layer. However, in order to prevent the flexible adhesive plate and the window aluminum substrate from being directly pressed together during subsequent pressing, which may easily cause deviation and displacement, the window adhesive layer 30C is provided to better improve the interlayer bonding effect and the glue filling effect during pressing.

[0046] A pressing mold 430 is manufactured, and a pin 430A is disposed on the surface of the pressing mold 430 . The pressing mold 430 is disposed on the surface of the lower table 420 of the pressing device.

[0047] The second covering film layer 30B, the flexible adhesive plate 30, and the windowed aluminum substrate 20 are stacked in sequence from bottom to top to form a stacked structure 410, and placed in a pressing device for whole-plate pressing; further, the covering film pin holes, the flexible core plate pin holes, and the aluminum substrate pin holes are correspondingly sleeved on the pins in sequence from bottom to top; further, if a windowed adhesive layer 30C is provided, the windowed adhesive layer 30C is provided between the flexible adhesive plate 30 and the windowed aluminum substrate 20, and the adhesive layer pin holes are provided corresponding to the flexible core plate pin holes.

[0048] In the prior art, the aluminum substrate and the multi-layer flexible circuit board are directly pressed together, the thickness of the aluminum substrate is thicker than that of the multi-layer flexible circuit board, and the difference in expansion and contraction between the two is too large. Therefore, in this embodiment, a pressing mold 430 with pins is set on the lower table of the pressing equipment, and corresponding pin holes are set on the pressed stacked structure 410. During pressing, the edges of each layer of the board are first fixed by traditional hot melt or riveting methods, and then the pin holes of each layer of the structure are correspondingly inserted into the pins 430A. During the pressing process, the pin holes are matched with the pins to further fix the layers of the board, forming a stable pressing process and preventing the problems of deviation and displacement during the pressing process.

[0049] It is worth noting that the height of the pin 430A protruding from the surface of the pressing mold 430 is 5 μm to 35 μm smaller than the thickness of the pressing plate 50 formed after pressing, and preferably 10 μm or 15 μm smaller.

[0050] In one embodiment, because the release layer and the coating layer need to be provided on the upper and lower surfaces of the stacked structure during the lamination process, it cannot be completely ensured that the pin 430A will not hit the release layer and the coating layer during the lamination process, nor can it be completely ensured that the pin 430A can be flush with the thickness of the lamination plate 50. Therefore, a pre-lamination device can be used for pre-lamination, and the lamination mold 430 is set on the pre-lamination device. The pre-lamination generally adopts a lower temperature, shorter time, and smaller pressure than the formal lamination, so that each layer is in a pre-lamination state, and then placed in the lamination device for formal lamination. For example, the pre-lamination adopts a temperature of 130°C to 150°C and a pressure of 10kg / cm 2 Up to 20kg / cm 2 The pressure is 1500 g / cm2 and the pre-pressing time is 60 to 90 seconds. The formal pressing temperature is 160 to 180 degrees Celsius and the pressure is 15 kg / cm2. 2 Up to 25kg / cm 2 The pressure is increased and the time is from 7 to 15 minutes, using the fast pressing equipment used for flexible circuit boards for fast pressing.

[0051] For the upper table 440 of the laminating device, an airbag 450 is manufactured. The airbag 450 is a structure in which the sealed plastic layer is inflated. The airbag 450 is arranged on the upper table 440 of the laminating device.

[0052] The airbag 450 provided in this embodiment is a flat structure with a thickness of 1.0mm to 5.0mm. The material of the airbag 450 can be optionally PP, PE, PET, PTFE, preferably PTFE. The internal inflation is in an unsaturated state and can be fixed to the upper table 440 of the pressing equipment by gluing or edge nailing. Since the pressed stacking structure 40 is provided with an aluminum substrate window area 220 and is arranged upward, it is necessary to use a layout structure with good coating performance on the upper surface for coating. The use of the airbag 450 structure can effectively play a buffering coating role and improve the flatness of the aluminum-based multi-layer rigid-flexible composite board lamination.

[0053] It is worth mentioning that a first release layer 4310, a covering layer 4320, and a second release layer 4330 are sequentially laid on the lamination mold 430, and the positions corresponding to the pins 430A are sleeved on the pins 430A to play a covering and releasing role. A third release layer 4340 is laid on the surface of the airbag 450 to play a releasing role.

[0054] After the above layout, a pressed layout structure 40 is formed.

[0055] In one embodiment, the lamination equipment is a rigid plate press; the parameters of the whole plate lamination are: a heating rate of 2°C / min to 6°C / min, a maximum temperature of 160°C to 180°C, and a pressure of 15kg / cm 2Up to 25kg / cm 2 The cooling rate is 10℃ / min to 20℃ / min; if better interlayer bonding effect and better lamination stability effect are required, a rigid plate press can be used for lamination.

[0056] After lamination, a lamination plate 50 is formed as a whole.

[0057] Step S50: Optionally, the laminated plate 50 is firstly drilled to form trimming holes 510, and the drilling is performed according to the drilling pattern of the aluminum-based multi-layer rigid-flexible board.

[0058] The drilling here is for trimming drilling. Since problems such as uneven inner wall of the hole may occur after pressing, the hole shape is trimmed to make it regular, which is convenient for subsequent electroplating hole copper processing.

[0059] After the drilling process, laser ablation, plasma treatment, and alkaline washing treatment are performed in sequence; the laser ablation is to perform laser ablation on the stepped position of the aluminum substrate window area 220 and the first covering film layer 360 .

[0060] Since overflow glue 520 may be generated at the stepped position of the first covering film layer 360 after lamination, the overflowed glue is burned off by laser ablation. Carbon black impurities will appear after laser ablation, and impurities such as drill contamination will exist after trimming the drill holes. Therefore, carbon black impurities and drill contamination impurities can be effectively removed by plasma treatment and alkaline washing treatment.

[0061] Afterwards, the laminated plate 50 is electroplated to form an electroplated copper layer 610, and is back-drilled to form a back-drilled hole 620. The back-drilling process is to back-drill the aluminum substrate through hole 210. Optionally, the depth of the back-drilled hole 620 is pre-enlarged by 5μm to 50μm from the depth of the aluminum substrate through hole 210 to form the aluminum-based multi-layer rigid-flexible composite board 60.

[0062] Since the flexible adhesive sheet 30 first produces the surface graphic layer 320 and then attaches the second covering film layer 30B through lamination to form a multi-layer flexible circuit layer structure, but the layers need to be connected through vias, and therefore electroplating is also required. In this embodiment, the electroplating is placed after the surface graphic layer 320 and the second covering film layer 30B are processed, which effectively prevents the original processing technology of first laminating the multiple layers, then drilling and electroplating the via holes, and then producing the outer layer circuit graphics, which is prone to outer surface depression, thereby causing the circuit graphics to short-circuit or open-circuit.

[0063] After electroplating, the inner wall of the aluminum substrate through hole 210 of the aluminum substrate 110 is also electroplated with copper. Through the back drilling process, the copper on the inner wall of the aluminum substrate through hole 210 is effectively removed to prevent short circuit problems.

[0064] It is worth noting that due to the fact that the flexible circuit board in the actual design and processing process is relatively precise, the actual structure diagram and the thickness of each layer, line width and other dimensions are all in the micron level. For example, the thickness of each layer is generally 5μm to 50μm, and the aluminum substrate is generally 0.1mm to 3.0mm. If the drawings in the specification are made according to the actual proportion, there will be a problem of unclear drawings. Therefore, in order to more clearly show the implementation process of the manufacturing method, the drawings of this embodiment are all schematic diagrams that enlarge the technical features, which do not represent the size of the actual structure diagram, nor do they represent enlarged views of the actual structure diagram in proportion.

[0065] The above are only preferred embodiments of the present invention, and are not intended to limit the patent scope of the present invention. All equivalent structural changes made using the contents of the present invention's specification and drawings, or directly / indirectly applied in other related technical fields, are included in the patent protection scope of the present invention.

Claims

1. A method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board, It is characterized in that The production method comprises the following steps: S10: splitting the structure of the multi-layer rigid-flex board into a first copper layer and a multi-layer flexible board core layer, taking an aluminum substrate and a first adhesive layer, sequentially attaching the first adhesive layer and the first copper layer to the surface of the aluminum substrate, and pressing them together to form an aluminum-based copper-clad board; S20: forming a copper layer circuit pattern on the first copper layer of the aluminum-based copper-clad laminate, and forming an aluminum substrate through hole, wherein the aluminum substrate through hole includes an aluminum substrate pin hole, and then forming an aluminum substrate window area to form a window aluminum substrate; S30: manufacturing a core board layer of a multi-layer flexible board according to a predetermined process, and forming a surface graphic layer of the core board layer; Taking a second adhesive layer, and attaching the second adhesive layer to the core plate layer; Then, take the first covering film, make a first covering film pattern to form a first covering film layer, and attach the first covering film layer to the surface of the second adhesive layer, wherein the first covering film layer corresponds to the window area of ​​the aluminum substrate; The whole is formed into a flexible sheet of covering film; Making a cover film flexible board through hole on the cover film flexible board, wherein the cover film flexible board through hole includes a flexible core board pin hole; The whole is processed to form a flexible adhesive plate; S40: taking a second covering film and making a second covering film pattern to form a second covering film layer, wherein the second covering film pattern includes a covering film pin hole; The second covering film layer, the flexible adhesive sheet, and the windowed aluminum substrate are stacked in sequence from bottom to top, and placed in a pressing device for whole-plate pressing; The whole is formed into a pressed board; S50: performing electroplating processing on the laminated board and performing back drilling processing to form the aluminum-based multi-layer rigid-flexible board.

2. A method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board as claimed in claim 1, It is characterized in that The whole board pressing also includes: Making a pressing mold, the surface of which is provided with pins, and setting the pressing mold on the lower table surface of the pressing device; The stacking from bottom to top includes: The pin holes of the covering film, the pin holes of the flexible core board, and the pin holes of the aluminum substrate are sequentially placed on the pins from bottom to top.

3. The method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board according to claim 1, It is characterized in that The whole board pressing also includes: An airbag is manufactured, wherein the airbag is a structure in which air is inflated inside a sealed plastic layer, and the airbag is arranged on the upper table surface of the laminating device.

4. A method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board as claimed in claim 2, It is characterized in that The forming of the pressed plate further comprises: Take the third adhesive layer, and make an adhesive layer window area, the adhesive layer window area corresponds to the first covering film layer, and make an adhesive layer through hole, the adhesive layer through hole includes an adhesive layer pin hole; The whole window glue layer is formed; The stacking from bottom to top includes: The pin holes of the covering film, the pin holes of the flexible core board, the pin holes of the adhesive layer, and the pin holes of the aluminum substrate are sequentially mounted on the pins from bottom to top.

5. The method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board according to claim 1, It is characterized in that After the window area of ​​the aluminum substrate is produced, browning processing is performed.

6. The method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board according to claim 1, It is characterized in that Before the press plate is electroplated, the press plate needs to be drilled, and the drilling is performed according to the drilling pattern of the aluminum-based multi-layer rigid-flexible board.

7. A method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board as claimed in claim 6, It is characterized in that After the drilling process, the pressed plate is sequentially subjected to laser ablation, plasma treatment, and alkali washing treatment; The laser ablation is to perform laser ablation on the stepped position of the window area of ​​the aluminum substrate and the first covering film layer.

8. The method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board according to claim 1, It is characterized in that The size of the window area of ​​the aluminum substrate is smaller than the size of the first covering film layer on one side.

9. The method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board according to claim 1, It is characterized in that The back drilling process is to perform back drilling on the through holes of the aluminum substrate.

10. The method for manufacturing a high heat dissipation aluminum-based multi-layer rigid-flexible board according to claim 1, It is characterized in that The pressing equipment is a rigid plate press; The parameters of the whole plate pressing are: heating rate of 2°C / min to 6°C / min, maximum temperature of 160°C to 180°C, pressure of 15kg / cm 2 Up to 25kg / cm 2 , the cooling rate is 10℃ / min to 20℃ / min.

Citation Information

Patent Citations

  • Aluminum-based flexible circuit board manufacturing method

    CN105530757A

  • Manufacturing method of circuit board embedded with special-shaped copper block

    CN118234137A

  • Rigid -flex circuit board with heat dissipation function

    CN207491294U

  • Printed circuit board structure, signal processing device and electronic equipment

    CN219555242U

  • Manufacturing of stacks of multilayer plastic laminates for printed circuits

    US20140020245A1

Cited By

  • Large-bending-angle semi-flexible rigid-flex printed circuit board manufacturing method

    CN119767576A

  • Manufacturing method of semi-flexural rigid-flexual combined board with large bending angle

    CN119767576B

  • Method for manufacturing rigid-flex printed circuit board with surface flexible layer

    CN120456463A