Conductor element having insulating body that can be produced efficiently

By using uncrosslinked bismaleimide and epoxide powder coating formulations to form an insulating layer with high dielectric strength, the problems of stability and production complexity of the insulating system of rotary motors at high temperatures are solved, and the problem of insulating system stability and production complexity of rotary motors is achieved. Efficient and automated insulator production.

CN118901180APending Publication Date: 2024-11-05SIEMENS AG +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380029174.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-24
Filing Date
2023-03-16
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The insulation system of existing rotary motors is difficult to maintain stability under high temperature and high current conditions, resulting in heat loss and partial discharge. The production process of insulators is complex and costly, making it difficult to automate.

Method used

Thermoset powder coating formulations with uncrosslinked bismaleimide and epoxide as the main components are cured at high temperatures by electrostatic powder coating or fluidized bed sintering to form an insulating layer with high dielectric strength. , replaces traditional mica tape and resin insulator.

Benefits of technology

It realizes stable operation at temperatures above 155°C, reduces heat loss and local discharge, simplifies the production process of insulators, and improves the degree of automation and cost-effectiveness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005052417490000061
    Figure BDA0005052417490000061
  • Figure BDA0005052417490000062
    Figure BDA0005052417490000062
  • Figure BDA0005052417490000071
    Figure BDA0005052417490000071
Patent Text Reader

Abstract

The invention relates to a conductor element, for example a winding end and / or a copper flat wire, of a rotary electric machine, in particular an electric motor, a traction engine and / or a generator, having an insulating body that can be produced efficiently. The invention also relates to a method for producing an insulator for such a conductor element. By means of the powder coating of the insulator disclosed herein for producing conductor elements of rotating electrical machines having rated voltages greater than 700 volts, it is possible to omit expensive and complex VPI processes so far used for insulation of active components and winding ends. Thus, conventional mica tapes can be not required, and the active components and the winding ends can be insulated in an automated manner with an insulating material adapted in each case. In particular, the insulation of the winding ends can be achieved significantly faster and more cost-effective compared to the prior art. And the automation degree in the production of the rotating motor is obviously higher.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a conductor element, such as a winding head and / or a copper flat wire, of a rotating electrical machine, in particular an electric motor, a traction motor and / or a generator, having an insulation which can be produced efficiently. The invention also relates to a method for producing the insulation of such a conductor element.

[0002] Rotating electrical machines such as electric motors and generators in the medium and high voltage range are known. These machines are characterized by a wide variety of construction forms and fields of application. They are used in all areas of technology, industry, everyday life, transportation, medicine and other industries. The power range of electrical machines extends from the order of magnitude of less than 1 microwatt, for example in microsystem technology, to more than 1 gigawatt, i.e. a thousand times a million watt, for example in the field of power plants. In between are medium voltage applications with traction and drive engines in the vehicle field, the rail vehicle field, etc.

[0003] Common to all rotating electrical machines are conductor elements, such as winding ends, copper flat wires in hairpin technology and / or coils through which the current flows. In order to electrically insulate the conductor elements through which the current flows from one another and from the external environment, the electrical machine has an insulation system.

[0004] Rotating electrical machines with a rated voltage of more than 700 V, such as motors and generators, comprise a rotor surrounded by a stator. The stator has a laminated core in which grooves are present, into which electrical conductor elements are inserted in the form of coils or as individual rods that are fused or welded into coils. Two respective individual rods can be welded together to form a coil. The sub-electrical conductors in the coil are insulated from one another, the coil is additionally provided with a main insulation made of an insulating tape containing mica, and finally optionally also with a conductive corona protection device, in particular an external and / or end corona protection device, depending on the voltage level, so that the coil surface is at the same potential as the laminated core. This structure is also called an "ordered" winding, which is in contrast to a rotating electrical machine with wires of a "wild" winding, which generally relates to a rotating electrical machine with a rated voltage of less than 700 volts.

[0005] In rotating electrical machines in the high-voltage and / or medium-voltage range, there are coils made of sub-conductors insulated from one another, for example by windings and / or wire enamels. They are formed from blanks, such as coils, by drawing and twisting so that they can be inserted into recesses in the stator base body, i.e. into the laminated core of the electric motor. The coils are connected to one another via so-called winding ends and contacted via corresponding connecting pieces.

[0006] The current carrying coils are insulated from each other, from the laminated core and ultimately from the environment by an insulation system. The insulation system usually comprises a main insulation (which represents a pure insulation) and a corona protection system, which comprises an external corona protection device and / or an end corona protection device assembly, wherein the corona protection system also exhibits low electrical conductivity for better resistance to partial discharges.

[0007] The live coil is insulated from the grounded laminated core by a primary insulator made of a polymer-based material. In order for the machine to achieve maximum power, it is operated at the highest possible current density, which, however, also results in considerable losses in the form of heat.

[0008] For large electric motors, the highest conventional operating temperature is about 155° C. For such operating temperatures, it is known to use insulation systems made of mica tape and epoxy-based thermosetting plastics. The electric machine is designed so that the maximum heating (including the insulation) does not exceed 155° C. or only slightly.

[0009] In order to increase the power density of such machines, either the voltage or the current intensity must be increased. If the voltage is to be increased, the higher field strengths must be continuously reduced by the insulation system. The conventionally known epoxy-based insulation systems are not designed for this.

[0010] If the current intensity increases, the insulation system is subjected to greater thermal stresses, at least temporarily even to temperatures exceeding 200° C. For this purpose, insulation systems with materials based on m-aramid and polyetherimide are used.

[0011] Until now, all components of the insulation system, i.e. the main insulation and the corona protection, such as in particular the external corona protection AGS and the end corona protection EGS, have usually been wound around the sub-conductor in the form of a tape, but some of these components, such as the EGS, can also be applied by hand. Other components cannot be applied completely automatically either, because the number of workpieces does not make automation economical and / or the risk of air inclusions at the folds of the wound tape does not guarantee the required quality when winding. The wound tape usually has glued-on mica sheets, which serve in the insulator to extend the erosion path in the insulation system, i.e. the direct path from the voltage side, the conductor element to the grounded laminated core, thereby resulting in a significantly longer service life of the insulation system.

[0012] At present, in rotating electrical machines, in particular traction engines and industrial engines, the winding ends are insulated by the same insulating tape as used in the grooves of the active components. In the impregnation process conventional to date, the winding ends are therefore impregnated with the same winding tape and impregnation resin and then cured like the active components.

[0013] The winding of the winding head is time-consuming and therefore also cost-intensive. The impregnation process with impregnation resin required hitherto is also very time-consuming and cost-intensive.

[0014] The field strengths present in the winding heads during operation are a fraction of those in the active components and are less than 500 V / mm in the wound insulation itself. No partial discharges occur here during operation. However, according to the prior art, the winding heads are insulated like the active components, since it would be much more complicated to produce the insulation separately between the active components and the winding heads.

[0015] The winding end insulation ensures in particular a dielectric barrier and prevents phase flashovers and / or ground faults which may occur in the event of pollution. Therefore, the winding end insulation does not require an increased resistance to partial discharges, but essentially has a certain minimum dielectric strength. This applies in particular to traction machines in which the high temperature resistance of the insulation is above 200°C (which corresponds to thermal class 200).

[0016] The object of the present invention is therefore to produce a winding end insulation which firstly can be applied automatically and secondly is stable even at operating temperatures above 155° C., in particular up to 200° C. or 220° C., has the required dielectric strength and thus serves as a dielectric barrier on the winding end and prevents phase flashovers and / or ground faults in the event of contamination.

[0017] This object is achieved by the subject matter of the invention as disclosed in the description and the claims.

[0018] The subject matter of the present invention is therefore a conductor element of a rotating electrical machine with a rated voltage of more than 700 volts, for example a winding head and / or a copper flat wire, which has a powder coating, wherein the powder coating formulation for producing the powder-coated insulation contains at least two uncrosslinked plastic components which are solid under conventional conditions at room temperature RT, i.e. at about 20° C., namely at least one first uncrosslinked polyimide-containing, in particular bismaleimide-containing plastic component and a second uncrosslinked epoxide-containing plastic component, which are contained in the powder coating formulation in a mixing ratio of 99:1 to 1:99.

[0019] The subject of the invention is also a method for producing a conductor element, for example an insulation for a winding head and / or a copper flat wire, comprising the following method steps:

[0020] - providing a thermosetting powder coating formulation with at least two uncrosslinked plastic components, wherein the powder coating formulation comprises at least one first uncrosslinked polyimide-containing plastic component, in particular a bismaleimide plastic component, and at least one second uncrosslinked epoxide-containing plastic component, each of which is present in solid form at room temperature under conventional conditions, i.e. at about 20° C.,

[0021] - Single or multiple powder coating of the winding ends, and subsequent

[0022] - subjecting the powder coating thus obtained to curing and / or post-curing.

[0023] Finally, the subject of the invention is a rotating electrical machine with a rated voltage greater than 700 volts, in which the insulation of the active parts is of a different material than the insulation of the winding heads.

[0024] In particular, in the hairpin technology, which is a modern winding technology for stators in electric machines, new approaches are being tried to replace the mica tape insulation of active components. For example, instead of the winding technology in which the conductor elements are wound into grooves, here, in a molding-based assembly process, copper flat wires with a typical hairpin geometry are inserted into grooves of a laminated core. In this case, the coil side for the active component, which is part of the hairpin geometry, can be insulated by injection molding, for example, with a material that is resistant to partial discharges, in particular also containing silicones, and then the finished winding head inserted into the groove is provided with an insulation that has dielectric strength but is less resistant to partial discharges or not at all.

[0025] This is where the present invention comes in, since it achieves the object of producing an over-winding insulation that can be applied in an uncomplicated manner and exhibits the required dielectric strength, but without using expensive resins for partial discharge-resistant insulation of active components.

[0026] The general finding of the present invention is therefore that insulation of conductor elements, such as winding end insulation and / or insulation of copper flat wires, can be produced quickly and automatically, for example by means of corona and / or friction and / or fluidized bed processes, by powder coating with thermosetting powder coating formulations.

[0027] According to the invention, for example one or both winding ends of rotating electrical machines, engines and generators are insulated by powder coating using a thermosetting powder coating. This is applied automatically by means of a corona and / or friction and / or fluidized bed process, for example.

[0028] Here, in order to insulate the active components of a rotating electrical machine, the sub-conductors of the coils are first coated with a sub-conductor insulator. The sub-conductor insulator can be a wire enamel or a wound insulator. Now, the drawn coils, for example wound or hairpin geometry, or the undrawn coils are insulated in some way and type in the active component, for example by separate coil production and / or by injection molding of the active component and / or by powder coating. All coils are then inserted and glued into the grooves individually and connected to one another, for example using a sleeve or groove adhesive. Now, according to an advantageous embodiment of the method, the insulation is also produced on the winding ends including the circuit by powder coating.

[0029] The result is, for example, a rotating electrical machine in hairpin technology, wherein the active component insulator can be produced by injection molding and the winding end insulator can be produced according to one embodiment of the invention by powder coating.

[0030] The provision of uncrosslinked powder coating formulations can be done simply by weighing and mixing, wherein the powder coating is initially melted, degassed and / or initially crosslinked on the substrate, coil or coil section. After the powder is applied and a solid film is obtained, it is post-cured and fully cured at elevated temperature.

[0031] Here, powder coating is divided into two types, the first aspect is

[0032] - electrostatic powder coating, which operates by corona (charging by means of a generator) or by the so-called "tribo" method (friction charging), and secondly

[0033] - Fluidized bed sintering, which is also known in the automotive field as the "powder slurry" method.

[0034] In the electrostatic powder coating process, the powder coating formulation is sprayed onto the conductive workpiece. By means of a so-called spray element, such as a spray gun, the fluidized powder is formed into a specific spray jet and is simultaneously electrostatically charged, wherein different charging methods can be used for the method applicable here.

[0035] In a corona spray system, the powder particles of the powder coating formulation are charged by the accumulation of free air ions, which are generated in the spray element with the aid of one or more charged corona electrodes. Usually, a negative voltage is chosen, because the corona current is larger and more stable, and the back-spray effect on the workpiece surface occurs to a lesser extent. The voltage on the corona electrodes is up to 100 kV.

[0036] In a "tribo" spray system, the powder particles of the powder coating formulation are charged solely by triboelectric processes when flowing through the plastic channels in the spray element (e.g. in a spray gun), i.e. without a voltage generator. In this case, the powder particles are positively charged.

[0037] After spraying, curing and / or baking are carried out, wherein the powder coating can also contain all the ingredients of conventional wet coatings in addition to the solvent and thus, depending on the composition of the plastic component, forms a closed film at higher temperatures, for example above 100° C., in particular above 120° C., and then gels and cures.

[0038] Powder coating has some advantages over wet coating from a cost and / or environmental perspective:

[0039] -Solvent-free coating materials and minimal emissions,

[0040] -Powder coating can be recycled,

[0041] -Easy manual operation of the spray gun or other spraying elements and

[0042] -Suitable for automation.

[0043] Alternatively, powder coating can also be carried out using a fluidized bed sintering process. Here, a powder bath made of moving air (especially an air stream) and fluidized powder coating formulation is provided and the heated substrate is immersed in this powder bath - for example even for only a few seconds. When in contact with the hot substrate, the powder preliminarily sintered, melted and / or crosslinked, subsequently forming a smooth plastic layer. For example, when producing insulation systems, the final insulation of the winding head can be achieved by fluidized bed sintering at about 200°C.

[0044] According to an advantageous embodiment of the invention, one or more first polyimide-containing plastic components and one or more second epoxide-containing plastic components are present in the powder coating formulation.

[0045] "Polyimide" in solid, but not crosslinked powder coatings means a monomer or oligomer of a plastic having a "polyimide group". This usually means a compound having a unit as shown in structural formula I:

[0046]

[0047] I. Circle the polyimide group here.

[0048] R2 may be the same as or different from R3 and represents any organic molecular unit that is sterically possible on the C5 pentacyclic ring.

[0049] It has been found that bismaleimide polymers can be used particularly advantageously as the polyimide component because they

[0050] a) can be easily processed as a powder coating ingredient in combination with epoxy components, and

[0051] b) Bismaleimides, particularly species of this class of compounds as shown below, cure to form polyimides having the desired dielectric strength.

[0052] Preferred bismaleimides are those having the structural formula shown below:

[0053]

[0054] According to the invention, the uncrosslinked polyimide is also mixed with an uncrosslinked solid epoxide-containing plastic component, which is contained in the powder coating formulation in a mixing ratio of 99:1 to 1:99. The mixing with the solid epoxide-containing plastic component is also used, inter alia, to improve the mechanical properties and flow properties of the powder coating formulation during the coating process.

[0055] Various synthetic resins containing epoxy groups are referred to as "epoxy resins" or "epoxide-containing uncrosslinked plastic components".

[0056]

[0057] R can be any carbon-based molecular skeleton. R can also contain other epoxy groups suitable for crosslinking, especially terminal epoxy groups.

[0058] According to an advantageous embodiment of the invention, in addition to the two uncrosslinked polyimide-containing and epoxide-containing plastic components present in solid form, one or more further binders, thermoplastic binders, may also be present in the thermosetting powder coating formulation.

[0059] In the applied powder coating formulation, the two plastic components are initially melted by the use of temperature, for example in the form of convection and / or radiation energy, and then solidify in a crosslinking reaction.

[0060] According to an advantageous embodiment of the invention, the powder coating formulation is applied such that the resulting insulation and / or corona protection layer has a thickness of ≧100 μm. This layer can be formed by powder coating in one or more layers.

[0061] According to an advantageous embodiment, the formulation also comprises a filler, in particular a spherical and / or irregularly shaped filler. The filler may be in crystalline and / or amorphous form.

[0062] The fillers are preferably based on silicon dioxide, for example they comprise quartz frit, quartz powder and / or quartz glass.

[0063] It has been recognized that the dielectric strength of sprayable powder coating formulations can be increased by adding fillers, in particular mineral and / or synthetic fillers, such as quartz powder, quartz material, glass powder, in a mass proportion of, for example, 5% to 65% by weight, in particular 10% to 60% by weight, particularly advantageously 10% to 55% by weight.

[0064] It is thereby possible to dispense with the use of large mica sheets glued into tapes and to automate the application and production of the winding head insulation in the form of a powder coating formulation by spraying and / or dipping.

[0065] The powder coating proposed in this paper is very suitable for automated implementation and has high dielectric strength despite the absence of mica particles.

[0066] According to an advantageous embodiment of the invention, the powder coating formulation which is present as a solid powder at room temperature also comprises fillers, in particular in a plurality of fractions, and sintering aids and / or additives.

[0067] According to another advantageous embodiment of the present invention, one or more additives may be included in the powder coating formulation. For example, additives for improving processability may be included.

[0068] Alternatively or in addition, additives may be included to increase the stability of the insulation system. For example, one or more metal oxides may be present, such as TiO2 and / or those having one of the following general chemical formulas: Na8Al6Si6O 24 S4 and / or Na6Al6Si6O 24 S2. Other additives may be Fe2O3 and / or MnFe2O4 and / or non-conductive carbon-based fillers, such as carbon black. If desired, the additive particles may be provided with a SiO2 coating partially or completely, on the entire surface or on part of the surface.

[0069] These additives are particularly oxidation-inhibiting and can therefore further increase the thermal resistance class or temperature index of the powder coatings produced therefrom.

[0070] For example, additives are mixed in during the production of powder coating formulations. Other additives, flow aids, color pigments, quartz particles, etc. can be mixed into powder coating formulations.

[0071] The proportion of the additive in the powder coating material is, for example, 0.05 to 10% by weight, in particular 0.05 to 2% by weight, particularly preferably 0.1 to 1% by weight.

[0072] By means of the powder coating disclosed here for producing insulation of conductor elements of rotating electrical machines with rated voltages greater than 700 volts, the expensive and complex VPI process, which has hitherto been used mainly for the insulation of active components and winding heads, can be dispensed with. Thus, conventional mica tapes can be dispensed with and active components and winding heads can be insulated in an automated manner with insulating materials adapted in each case. Insulating winding heads in particular can be achieved significantly faster and more cost-effectively than in the prior art. Furthermore, the degree of automation in the production of rotating electrical machines is also significantly higher.

Claims

1. Conductor elements of rotating electrical machines with a rated voltage of more than 700 V, which have a powder coating as insulation, wherein a powder coating formulation is used, which contains at least two uncrosslinked plastic components which are solid under normal conditions at room temperature RT, i.e. at about 20° C., namely at least one first uncrosslinked polyimide-containing plastic component and a second uncrosslinked epoxide-containing plastic component, which are contained in the powder coating formulation in a mixing ratio of 99:1 to 1:

99. 2 . The conductor element according to claim 1 , wherein the first uncrosslinked polyimide-containing component of the powder coating formulation comprises a bismaleimide polymer. 3 . The conductor element according to claim 1 , wherein the first uncrosslinked polyimide-containing plastic component of the powder coating formulation comprises a mixture, a copolymer and / or a blend comprising a plurality of polyimide-containing plastic components. 4 . The conductor element according to claim 1 , wherein the second uncrosslinked epoxide-containing plastic component of the powder coating formulation comprises one or more solid epoxy resins. 5 . The conductor element according to claim 1 , wherein the second uncrosslinked epoxide-containing plastic component of the powder coating formulation contains a mixture, copolymer and / or blend comprising a plurality of epoxide-containing plastic components. 6 . The conductor element according to claim 1 , wherein the two uncrosslinked plastic components are present in the powder coating formulation as a mixture, blend or copolymer.

7. Conductor element according to any of the preceding claims, wherein the powder coating formulation contains fillers.

8. Conductor element according to any one of the preceding claims, wherein the powder coating formulation comprises additives.

9. A method for producing an insulator for a conductor element, comprising the following method steps: o providing a thermosetting powder coating formulation having at least two uncrosslinked plastic components, wherein the powder coating formulation comprises at least one first uncrosslinked polyimide-containing plastic component and at least one second uncrosslinked epoxide-containing plastic component, each of which is present in solid form at room temperature under conventional conditions, i.e. at about 20° C., o Single or multiple powder coating of conductor components, and subsequent o subjecting the powder coating thus obtained to curing and / or post-curing.

10. The method of claim 9, which is performed automatically.

11. A method according to claim 9 or 10, wherein the conductor element is a winding head.

12. The method according to claim 9 or 10, wherein the conductor element is a copper flat wire.

13. Rotating electrical machines of rated voltage greater than 700 V, in which the insulation of active parts is of a different material from the insulation of winding ends.

14. The rotating electric machine according to claim 13, wherein the material of the active component insulator contains siloxane, whereas the material of the winding head insulator does not contain siloxane.

15. A rotating electric machine according to claim 13 or 14, wherein the insulation of the winding heads is mica tape-free.

16. Rotating electric machine with hairpin technology, wherein the active part insulator is producible by injection molding and the winding head insulator is producible by powder coating according to any one of claims 9 to 11.