Preparation method and application of oat milk, oat milk emulsion and emulsion gel

By baking and heating the oat grains, combined with agar and sodium alginate, a high stability oat emulsion gel was prepared, which solved the environmental and safety issues of oat-based emulsion preparation in the prior art, and reduced food as a fat substitute Oxidation rate.

CN118901808APending Publication Date: 2024-11-08ANHUI AGRICULTURAL UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411329931.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-24
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing oat-based emulsion preparation methods have problems such as unfriendly environment, low food safety and cumbersome process, and the stability of the emulsion gel is poor, making it impossible to fully simulate the texture and taste of traditional fats.

Method used

Oat milk is prepared by mixing baked oat grains with water and beating, filtration, heat treatment, and backfill filter residue treatment. By combining with agar and sodium alginate, it is formed by high-speed shearing to form an oat emulsion gel, and calcium ions are added to regulate it. stability.

Benefits of technology

Oatmeal emulsion gel with high stability and good emulsification effect was obtained, which can be used as a fat substitute, reduce the oxidation rate of food products, and does not use chemical reagents.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118901808A_ABST
    Figure CN118901808A_ABST
Patent Text Reader

Abstract

The invention belongs to the field of food processing, and particularly relates to preparation methods and application of oat milk, oat milk emulsion and emulsion gel. Oats are subjected to baking treatment, heating treatment and filter residue backfilling treatment, so that the contents of protein and solid matters in the oat milk are increased, the hydrophobicity of the oat milk is enhanced, and the structure of the protein in the oat milk is changed. Oat milk is used as an emulsifying agent to prepare the emulsion, and the emulsifying effect and the stability of the oat milk emulsion are improved. Furthermore, the oat milk emulsion is prepared into oat milk emulsion gel, and the oat milk emulsion gel has relatively strong supporting property and thermal stability and is good in quality. By improving the preparation method of the oat milk, the performance of the oat milk is improved, and a foundation is laid for applying the oat milk and processed products thereof to the field of food processing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of food processing, and particularly relates to a preparation method and application of oat milk, oat milk emulsion and emulsion gel. Background Art

[0002] Oats are annual herbaceous plants belonging to the family Poaceae. Oats are one of the best complete nutritional cereal foods. Their nutritional components include starch, protein, unsaturated fatty acids, soluble and insoluble dietary fiber, minerals, etc., and they have certain health-care effects. In recent years, they have been widely used in food processing. At present, there have been many reports on the research on the use of oats to prepare emulsions, but current research is still limited to the use of the above-mentioned single oat component for stabilizing emulsions. However, the component separation operation is cumbersome, and the separation process involves the use of chemical reagents. In addition, there are also methods for chemically modifying the components to change their emulsifying ability, surface hydrophobicity and solubility, thereby improving their emulsifying effect, but the chemical modification of the components also involves the use of chemical reagents. Therefore, the preparation methods of the above oat-based emulsions have the disadvantages of being environmentally unfriendly, low food safety, and a relatively cumbersome process, which limits their development and utilization in the field of emulsions.

[0003] Emulsion gel is a gel-like material based on emulsion, in which emulsion droplets and gel network systems coexist. It has the advantages of stable structure, adjustable viscoelasticity and good encapsulation performance. Therefore, emulsion gel is very suitable as a fat substitute for the design and development of healthy fat-containing foods. However, there are still some shortcomings when emulsion gel is used as a fat substitute, such as: emulsion gel cannot completely simulate the texture and taste of traditional fat, emulsion gel has poor stability, and is easily affected by temperature changes and storage conditions, resulting in stratification or texture changes.

[0004] Therefore, how to obtain a preparation method of an emulsion gel that can achieve high stability and good physical and chemical properties without using chemical reagents and can be used as a fat substitute in foods containing fat raw materials has become an urgent problem to be solved in the field. Summary of the invention

[0005] The purpose of the present invention is to provide a preparation method and application of oat milk, oat milk emulsion and emulsion gel. The oat milk prepared by the preparation method provided by the present invention has good emulsification effect and good emulsion stability. The emulsion gel prepared by the preparation method can be used as a fat substitute. Compared with traditional solid oil fat pig back fat, the oat milk emulsion gel prepared by the present invention can also reduce the oxidation rate of food products.

[0006] In order to achieve the above object, the present invention provides the following technical solutions:

[0007] A method for preparing oat milk comprises the following steps:

[0008] The roasted oatmeal grains are mixed with water and then beaten to obtain a crude oatmeal liquid;

[0009] filtering the crude oatmeal liquid to obtain a filtrate and a filter residue;

[0010] The filtrate is centrifuged, and the supernatant and the colloid layer on the surface of the precipitate are taken respectively;

[0011] mixing the gelatin layer and the supernatant to obtain raw oat milk;

[0012] The raw oat milk is subjected to a heating treatment to obtain cooked oat milk;

[0013] The cooked oat milk is filtered to obtain the oat milk.

[0014] Furthermore, the method for obtaining the baked oat grains includes: placing the oat grains in a baking device and baking at 100-140° C. for 0.5-1.5 min; the material-liquid ratio of the baked oat grains to water is 1 g: 5-10 mL; and the beating time is 1-2 min.

[0015] Furthermore, the filtration is performed using a filtration device with a pore size of 100-300 meshes.

[0016] Furthermore, the step of mixing the colloid layer and the supernatant also includes the step of adding filter residue for mixing.

[0017] The present invention also provides oat milk, which is prepared by any of the above preparation methods.

[0018] The present invention also provides the use of the above oat milk in preparing oat milk emulsion or oat milk emulsion gel.

[0019] The present invention also provides an oat milk emulsion, which is obtained by the following preparation method:

[0020] The oat milk and the oil phase are mixed and sheared at a speed of 10000-25000 r / min for 1-2 min by a high-speed shearing device to obtain an oat milk emulsion; the oat milk is the oat milk described above.

[0021] Furthermore, the ratio of the oat milk to the oil phase is 3-7:3-7, and the oil phase is vegetable edible oil.

[0022] The present invention also provides an oat milk emulsion gel, which is obtained by the following preparation method:

[0023] Agar, sodium alginate and water are mixed in proportion and heated to obtain a polysaccharide solution; the mass concentration of agar in the polysaccharide solution is 2.0%, and the mass concentration of sodium alginate is 2.0%;

[0024] The polysaccharide solution and oat milk emulsion are mixed in a volume ratio of 1:2, and sheared at a speed of 10000-25000 r / min for 1-2 min using a high-speed shearing device to obtain an oat milk emulsion gel;

[0025] A calcium chloride solution is added or not added to the oat milk emulsion gel, so that the calcium ion concentration in the oat milk emulsion gel is 0-1.3%; the oat milk emulsion is the oat milk emulsion as described above.

[0026] The present invention also provides the use of the above-mentioned oat milk, oat milk emulsion or oat milk emulsion gel in the processing of food containing oil raw materials.

[0027] The beneficial effects of the technical solution of the present invention are as follows:

[0028] The present invention uses whole oat grains as raw materials, and changes the basic physical and chemical properties and emulsification characteristics of oat milk through baking, grinding, heating, and backfilling of filter residue. The emulsion and emulsion gel prepared with oat milk as an emulsifier have high stability. The oat milk emulsion and oat milk emulsion gel further prepared by the present invention using oat milk can be used as fat substitutes in the processing of fat-containing foods, and the fat oxidation rate of the foods prepared thereby is reduced. The preparation method of oat milk provided by the present invention provides theoretical guidance for the preparation and application of oat-based emulsions and emulsion gels. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required to be used in the embodiments are briefly introduced below.

[0030] Figure 1 The figure is a flow chart of the oat milk validation test operations (1) to (4);

[0031] Figure 2 Schematic diagram of the contact angle measurement results of the oat milk sample in Verification Example 2;

[0032] Figure 3 This is a schematic diagram of the particle size distribution measurement results of the oat milk sample in Verification Example 4;

[0033] Figure 4 Schematic diagram of the test results of the appearance and creaming index (a), particle size distribution (b) and microstructure (c) of the emulsion in Verification Example 5;

[0034] Figure 5 Schematic diagram of the test results to verify the effects of different oil phases on the appearance (a), microstructure (b), and particle size distribution (c) of the emulsion particle size in Example 8.

[0035] Figure 6Schematic diagram of the test results of the appearance (a), microstructure (b), stress scan (c), frequency scan (d) and temperature scan (e) of the emulsion gel with different dispersion methods in Example 9;

[0036] Figure 7 Schematic diagram of the test results of the appearance (a), microstructure (b), stress scan (c), frequency scan (d) and temperature scan (e) of the emulsion gels with different agar concentrations in Verification Example 10;

[0037] Figure 8 Schematic diagram of the test results of the appearance (a), microstructure (b), stress scan (c), frequency scan (d) and temperature scan (e) of the emulsion gels with different sodium alginate concentrations in Verification Example 11;

[0038] Fig. 9 Schematic diagram of the test results of the appearance (a), microstructure (b), stress scan (c), frequency scan (d) and temperature scan (e) of the emulsion gel with different oil phase volume fractions in Verification Example 12;

[0039] Fig.10 Schematic diagram of the test results of the appearance (a), stress scan (b), frequency scan (c) and temperature scan (d) of the emulsion gel with different calcium ion concentrations in Verification Example 13;

[0040] Fig.11 Schematic diagram of the apparent detection results of the emulsion gels with different polysaccharide concentrations after centrifugation (a) and freeze-thaw (b) treatment in Verification Example 14;

[0041] Fig.12 Schematic diagram of the apparent detection results of the emulsion gels with different calcium ion concentrations after centrifugation (a) and freeze-thaw (b) treatment in Verification Example 15;

[0042] Fig.13 This is a schematic diagram of the apparent detection results of the emulsified sausage in Example 4;

[0043] Fig.14 This is a schematic diagram of the volatile component detection results of the emulsified sausage in Example 4;

[0044] Among them: the substances detected by each sensor are: aromatic compounds (W1C), nitrogen oxides (W5S), ammonia aromatics (W3C), hydrides (W6S), short-chain alkanes (W5C), alkanes (W1S), inorganic sulfides (W1W), alcohols and aldehydes (W2S), organic sulfides (W2W), alkanes and fats (W3S). DETAILED DESCRIPTION

[0045] The present invention provides a method for preparing oat milk, comprising the following steps:

[0046] The roasted oatmeal grains are mixed with water and then pulped to obtain a crude oatmeal liquid; the crude oatmeal liquid is filtered to obtain a filtrate and a filter residue; the filtrate is centrifuged to respectively take the supernatant and the gelatinous layer on the surface of the precipitate; the gelatinous layer and the supernatant are mixed to obtain raw oatmeal milk; the raw oatmeal milk is heated to obtain cooked oatmeal milk; the cooked oatmeal milk is filtered to obtain the oatmeal milk.

[0047] The present invention preferably bakes the oat grains in a baking device to obtain baked oat grains. The baking device of the present invention is preferably an electric oven, the baking temperature is preferably 100-140°C, more preferably 120°C; the baking time is 0.5-1.5 minutes, more preferably 1 minute.

[0048] To obtain the baked oat grains, the present invention preferably mixes the baked oats with water at a solid-liquid ratio of 1 g: 5 to 10 mL, and beats to obtain a crude oat liquid. The solid-liquid ratio of the baked oats to water in the present invention is preferably 1 g: 5 mL; the water is preferably deionized water; the beating is preferably performed using a homogenizer, and the beating time is preferably 1 to 2 minutes, more preferably 1.5 minutes.

[0049] The crude oat liquid is obtained, and the present invention filters the crude oat liquid to obtain a filtrate and a filter residue. The present invention preferably uses a 200-mesh filter device to filter the crude oat liquid.

[0050] The filtrate is obtained, and the present invention centrifuges the filtrate, takes the supernatant and the gelatin layer, and discards the starch layer. The centrifugation condition is preferably 5000r / min for 10min.

[0051] After obtaining the supernatant and the gelatin layer, the present invention preferably mixes the gelatin layer and the supernatant to obtain raw oat milk; more preferably, the supernatant, the gelatin layer and the filter residue are mixed to obtain raw oat milk containing the filter residue. The present invention preferably adds the gelatin layer to the supernatant and mixes evenly using a stirrer, the stirrer is preferably an overhead stirrer, and the stirrer speed is preferably 500r / min.

[0052] After obtaining the raw oat milk or raw oat milk containing filter residue, the present invention preferably heats the raw oat milk or raw oat milk containing filter residue to obtain cooked oat milk; the heating treatment preferably also includes a cooling step.

[0053] The heating treatment of the present invention is preferably water bath heating, the water bath heating temperature is preferably 90-100° C., more preferably 90° C., the heating time is preferably 20-30 min, more preferably 30° C. The cooling of the present invention is preferably carried out at ambient temperature, and the cooling time is preferably 10 min.

[0054] After obtaining the cooked oat milk, the present invention preferably filters the cooked oat milk using a 200-mesh filter device to obtain the oat milk.

[0055] The present invention also provides oat milk, which is obtained by the preparation method as described above.

[0056] The present invention also provides the use of the oat milk as described above in preparing oat milk emulsion or oat milk emulsion gel.

[0057] The present invention also provides an oat milk emulsion, which is prepared by the following preparation method: oat milk and an oil phase are mixed in proportion to obtain the oat milk emulsion; the oat milk is the oat milk described above. In the oat milk emulsion, the volume proportion of the oil phase is preferably 30-70%, more preferably 50%.

[0058] The oil phase of the present invention is preferably one or more edible plant oils, more preferably camellia oil.

[0059] The present invention preferably mixes the oat milk and the oil phase at high speed to obtain an oat milk emulsion, and the rotation speed of the high-speed mixing is preferably 10,000 to 25,000 r / min, more preferably 20,000 r / min; the time of the high-speed mixing is preferably 1 to 2 min, more preferably 1.5 min, and the high-speed mixing is achieved by a high-speed shearing device.

[0060] The present invention also provides a method for preparing an oat milk emulsion gel, which is prepared using the oat milk emulsion obtained by the above preparation method as a raw material, and specifically comprises the following steps:

[0061] Agar, sodium alginate and water are mixed in proportion and then heated to obtain a polysaccharide solution; oat milk and oil phase are mixed to obtain oat milk emulsion; the polysaccharide solution and the oat milk emulsion are mixed to obtain an oat milk emulsion gel.

[0062] The heating method of the present invention preferably includes: mixing agar, sodium alginate and water, heating in a water bath, and keeping warm for use.

[0063] The mass concentration of agar in the polysaccharide solution of the present invention is preferably 2.0%, and the mass concentration of sodium alginate is preferably 2.0%; the temperature of the water bath heating and insulation is preferably 90-100° C., more preferably 90° C.; the time of the water bath heating is preferably 30-50 min, more preferably 40 min.

[0064] Agar is a natural polysaccharide. During the cooling process of melted agar, its agarose molecular chains are cross-linked through hydrogen bonds to form a gel network structure. Sodium alginate is a natural polysaccharide extracted from marine brown algae. 2+ and Mg 2+The present invention uses both of them as gel matrix and adds them into the emulsion system, which can effectively adjust the emulsion properties, gel properties, rheological properties and thermal stability of the emulsion gel.

[0065] After obtaining the polysaccharide solution, the present invention mixes the polysaccharide solution with the oat milk emulsion to obtain an oat milk emulsion gel. The present invention preferably adds the polysaccharide solution to the oat milk emulsion to obtain a mixed solution; after the mixed solution is kept warm, it is evenly dispersed to obtain an emulsion gel, and then a calcium ion solution is added or not added to the emulsion gel, and after the calcium ions are evenly permeated, an oat milk emulsion gel containing or not containing calcium ions is obtained.

[0066] The volume ratio of the polysaccharide solution to the oat milk emulsion of the present invention is preferably 1:2.

[0067] The temperature of the heat preservation of the present invention is preferably 85-95°C, more preferably 90°C; the water bath heat preservation time is preferably 5-15min, more preferably 10min. The dispersion of the present invention is preferably uniformly dispersed by a high-speed shearing device, the speed of the uniform dispersion is preferably 20000r / min; the dispersion time is preferably 1.5min.

[0068] The present invention also provides the above-mentioned method for preparing oat milk, and application of the method for preparing oat milk and / or oat milk emulsion gel in food.

[0069] The application of the present invention is preferably: using the oat milk emulsion gel as a fat substitute in food, and the amount of fat replaced by the oat milk emulsion gel is preferably >0%, more preferably 50wt.%.

[0070] The food of the present invention is preferably a fat-containing food, and the fat-containing food is preferably a sausage.

[0071] In order to further illustrate the present invention, the preparation method and application of oat milk, oat milk emulsion and emulsion gel provided by the present invention are described in detail below in combination with the accompanying drawings and examples, but they should not be construed as limiting the scope of protection of the present invention.

[0072] Unless otherwise specified, the raw materials involved in this application are conventionally commercially available.

[0073] The main reagents involved in the present invention are shown in Table 1.

[0074] Table 1 List of main reagents

[0075] Reagent name Manufacturer Sodium hydroxide Sinopharm Chemical Reagent Co., Ltd. Concentrated sulfuric acid Sinopharm Chemical Reagent Co., Ltd. hydrochloric acid Sinopharm Chemical Reagent Co., Ltd. Boric acid Sinopharm Chemical Reagent Co., Ltd. Calcium chloride Xilong Scientific Co., Ltd. Trichloroacetic acid Shanghai Aladdin Biotechnology Co., Ltd. Thiobarbituric acid (TBA) Sinopharm Chemical Reagent Co., Ltd.

[0076] The instruments involved in the present invention are shown in Table 2.

[0077] Table 2 List of main instruments

[0078]

[0079]

[0080] In the present invention, the calculation formula of the emulsification index is as follows:

[0081] Creaming index (CI) = (creaming phase height / total oil-water mixture height) × 100%;

[0082] In the present invention, the water holding capacity (WHC) of the emulsion gel is calculated as follows: WHC (%) = (W 1 / W 2 )×100%, where W 1 is the weight of the gel sample, W 2 is the weight of the emulsion gel after centrifugation.

[0083] In the present invention, the calculation formula of the cooking loss rate is as follows: Cooking loss rate (%) = [(m 1 -m 2 ) / m1]×100%, where m 1 is the mass of emulsified sausage before cooking, m 2 The quality of emulsified sausage after cooking.

[0084] In the present invention, after the emulsion gel is added to the food, the water holding capacity of the food is measured = (M 2 / M 1 )×100%, where M 1 is the mass of emulsified sausage before centrifugation, M 2 is the mass of emulsified sausage after centrifugation.

[0085] Example 1 A method for preparing oat milk

[0086] Place the oat grains in an oven and bake at 120°C for 1.0 min. Take an appropriate amount of oat grains and add deionized water at a solid-liquid ratio of 1g:5mL. Use a homogenizer to beat for 90s, and then filter with a 200-mesh (75μm) filter cloth to obtain a filtrate and a filter residue. Centrifuge the filtrate at 5000r / min for 10min to collect the supernatant, and recover the colloid layer on the surface of the precipitate, discard the starch layer at the bottom, combine the filter residue, the colloid layer and the supernatant, and use a stirrer to fully dissolve the colloid layer and the filter residue in the supernatant to obtain raw oat milk. Put the raw oat milk into a container and heat it at 90°C for 30min. Take it out immediately after the heating is completed, cool it at ambient temperature for 10min, and then filter it through a 200-mesh filter cloth to obtain oat milk.

[0087] Example 2 A method for preparing oat milk emulsion

[0088] The oat milk and oil phase prepared according to the preparation method described in Example 1 were added into a container at a volume ratio of 1:1, dispersed at 20000 r / min using a high-speed shearing device for 1.5 min, and mixed evenly to obtain an oat milk emulsion.

[0089] Example 3 A method for preparing oat milk emulsion gel

[0090] Agar and sodium alginate were added to a container respectively, and then water was added so that the mass concentrations of agar and sodium alginate were both 2.0%, and the polysaccharide solution was obtained after heating at 90°C to fully dissolve them; the oat milk emulsion prepared according to the preparation method described in Example 2 was mixed with the above-mentioned polysaccharide mixed solution in a volume ratio of 2:1, and the mixture was kept warm at 90°C for 10 minutes, and then dispersed using a high-speed shear device at 20,000 r / min for 1.5 minutes to obtain an oat milk emulsion gel.

[0091] Oat milk validation test

[0092] (1) Heating treatment: Take an appropriate amount of oat grains and add water to a solid-liquid ratio of 1:5. Use a homogenizer to beat for 90 seconds, then filter with a 200-mesh (75μm) filter cloth. Centrifuge the filtrate at 5000r / min for 10min to collect the supernatant, and recover the gelatinous layer on the surface of the precipitate (discard the starch layer at the bottom) and combine it with the supernatant. Use an overhead stirrer to fully dissolve the gelatinous layer in the supernatant. At this time, the oat milk is recorded as raw oat milk. Take another portion of raw oat milk and put it into a 50mL round-bottom centrifuge tube, add glass beads, and cover the bottle cap tightly. Place it in a 90℃ shaking water bath and shake and heat at 150r / min for 30min. Take it out immediately after the heating is completed, cool it at ambient temperature for 10min, and record it as heated oat milk. Raw oat milk and heated oat milk are named ROM and HOM, respectively.

[0093] (2) Baking treatment: The oat grains were placed in an electric oven and baked at 120°C for 0.5, 1.0, 1.5 and 2.0 min, respectively, and then oat milk was prepared according to the preparation process of HOM. The oat milk samples with different baking conditions were named BOM-0.5min, BOM-1.0min, BOM-1.5min and BOM-2.0min.

[0094] (3) Backfill residue treatment: Oat kernels that had been baked for 1 min were used to prepare oat milk according to the preparation process of BOM-1min. The difference was that the residue obtained by pulping and filtering the oat kernels was collected and dissolved in the supernatant using an overhead stirrer to fully dissolve the gelatin layer in the supernatant. The evenly dispersed oat milk sample was then placed in a centrifuge tube and placed in a 90°C oscillating water bath, heated at 150 rpm for 30 min, taken out and cooled for 10 min, and then filtered through a 200-mesh filter cloth to obtain an oat milk sample treated with backfill residue, which was named BOM-FR.

[0095] (4) Preparation of dried oat milk samples: Each type of oat milk was spread in a 90 mm diameter dish and frozen at -18°C for 24 h, and then vacuum freeze-dried for 48 h to obtain a dried sample, named BOM-FR freeze-dried.

[0096] The process of the above operations (1) to (4) is as follows: Figure 1 shown.

[0097] The above method was used to prepare oat milk, and oat milks labeled ROM, HOM, BOM-0.5min, BOM-1.0min, BOM-1.5min, BOM-2.0min and BOM-FR were obtained respectively.

[0098] Verification Example 1

[0099] The protein content of the above oat milk was determined using a Kjeldahl nitrogen analyzer, and the solid content of the oat milk sample in the direct drying method according to GB5009.3-2016 "Determination of Water in Food" was referred to. The results are shown in Table 3.

[0100] Table 3 Protein and solid content of oat milk samples

[0101] sample protein(%) Solid content (%) Raw oatmeal <![CDATA[11.46±0.15 a ]]> -- ROM <![CDATA[26.02±0.34 e ]]> <![CDATA[6.57±0.16 a ]]> BOM-0.5min <![CDATA[26.24±0.14 e ]]> <![CDATA[6.59±0.09 a ]]> BOM-1.0min <![CDATA[25.90±0.17 de ]]> <![CDATA[6.60±0.12 a ]]> BOM-1.5min <![CDATA[25.07±0.37 c ]]> <![CDATA[6.47±0.16 a ]]> BOM-2.0min <![CDATA[25.21±0.01 cd ]]> <![CDATA[6.39±0.06 a ]]> BOM-FR <![CDATA[20.84±0.08 b ]]> <![CDATA[8.55±0.25 b ]]>

[0102] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0103] As shown in Table 3, the protein content of oat milk made from oat grains is significantly higher than that of raw oat grains, ranging from 20.8 to 26.24%, while the protein content of raw oat grains is 11.46%. Compared with freshly prepared oat milk ROM, the protein content of oat milk prepared by baking oat grains for 0.5 min and 1.0 min and then heating did not change significantly, but with the further extension of baking time, the protein content of oat milk prepared by baking oat grains for 1.5 min and 2.0 min was significantly reduced, which may be due to the increase in baking time, which intensified the degree of protein denaturation and formed more insoluble aggregates between protein and starch, which were removed together with the filter residue during the filtration process, thereby causing a decrease in the protein content in the sample. The protein content of oat milk treated with backfilled filter residue was 20.84%, which was significantly lower than that of the sample without backfilling filter residue, which may be due to the backfilling of filter residue into the sample with more starch and soluble dietary fiber, thus reducing the protein content relative to the total dry matter. This is consistent with the result that the solid content in oat milk was significantly increased after backfilling treatment.

[0104] Verification Example 2

[0105] Weigh 0.2g BOM-FR freeze-dried accurately, press it with a tablet press at 20MPa pressure for 2min, and press the sample into a flat round tablet. Use a high-precision syringe to gently drop 10μL of deionized water onto the tablet surface. Use a high-speed camera to start recording before the water drop falls, take images of the drop at a rate of 10 images per second, use the Laplace-Young equation to fit the contact angle data of the drop, and use a contact angle meter to measure the sample contact angle using the pendant drop method. The results are as follows: Figure 2 shown.

[0106] The hydrophilicity and hydrophobicity of the oat milk sample surface can be measured by its contact angle. A contact angle of >90° indicates that the sample is highly hydrophobic, and a contact angle of <90° indicates that the sample is highly hydrophilic. The closer the sample contact angle is to 90°, the stronger its adsorption capacity at the oil-water interface, and the more stable the spatial barrier formed to prevent droplet aggregation.

[0107] Depend on Figure 2It can be seen that the contact angle of the oat milk sample was measured by a contact angle meter. The contact angle of ROM is larger than that of HOM. This is because the starch particles in HOM are converted into amorphous starch after heating, and interact with oat protein to form aggregates, thereby covering the hydrophobic groups on the surface of the protein, resulting in a decrease in its hydrophobicity. After the oat grains were baked, except for the oat milk sample baked for 0.5 min, the contact angles of the samples baked for 1.0, 1.5 and 2.0 min were significantly larger than those of the raw oat milk ROM and the heated oat milk HOM. Among them, the oat milk BOM-1.0min treated with baking for 1.0 min had the largest contact angle of 57.26°, indicating that proper baking treatment can improve the hydrophobicity of oat milk. The improvement in its hydrophobicity is mainly related to the protein denaturation caused by baking, which exposes its hydrophobic groups. It is worth noting that when the baking time exceeds 1 min, the contact angle of the oat milk sample decreases instead, which is consistent with the above protein content determination results. In addition, the contact angle of oat milk BOM-FR treated with backfill residue was significantly reduced compared with that of oat milk BOM-1.0min not treated with backfill residue. This may be because the backfill residue treatment filled more starch and soluble dietary fiber into the sample, reduced the protein content, and increased the hydrophilicity of the sample.

[0108] Verification Example 3

[0109] Weigh 100 mg of potassium bromide and grind it into a uniform powder in an agate mortar. Then add 1 mg of freeze-dried oat milk sample and grind it evenly with potassium bromide. Then use a tablet press to press the mixture into a transparent sheet at a pressure of 20 MPa for 30 seconds. Use a Fourier transform infrared spectrometer to scan and collect spectra. The measurement band is 4000-500 cm -1 Wavenumber range. The protein amide I region spectrum was fitted and the peak was deconvoluted using PeakFit 4.12 software. The percentage of each secondary structure in the total amide I area was calculated based on the second-order derivative area corresponding to each structure. The oat milk FT-IR analysis was performed, and the results are shown in Table 4.

[0110] Table 4 Protein secondary structure content of oat milk samples

[0111] sample α-helix (%) β-fold (%) β-turn angle (%) Irregular curl (%) ROM <![CDATA[21.03±0.61 bc ]]> <![CDATA[19.45±0.92 a ]]> <![CDATA[40.27±0.21 a ]]> <![CDATA[19.24±0.78 c ]]> HOM <![CDATA[20.23±0.31 b ]]> <![CDATA[26.49±0.77 b ]]> <![CDATA[35.72±0.36 b ]]> <![CDATA[17.56±0.53 b ]]> BOM-0.5min <![CDATA[16.20±0.19 a ]]> <![CDATA[29.49±0.18 b ]]> <![CDATA[40.17±0.17 a ]]> <![CDATA[14.18±0.16 a ]]> BOM-1.0min <![CDATA[16.20±0.19 a ]]> <![CDATA[29.95±0.12 b ]]> <![CDATA[39.50±0.24 a ]]> <![CDATA[14.34±0.07 a ]]> BOM-1.5min <![CDATA[16.34±0.47 a ]]> <![CDATA[29.32±0.05 b ]]> <![CDATA[39.86±0.53 a ]]> <![CDATA[14.48±0.32 a ]]> BOM-2.0min <![CDATA[17.25±0.61 a ]]> <![CDATA[31.71±1.83 c ]]> <![CDATA[36.70±2.37 b ]]> <![CDATA[14.34±0.07 a ]]> BOM-FR <![CDATA[22.14±0.23 d ]]> <![CDATA[21.92±0.15 a ]]> <![CDATA[35.77±0.32 b ]]> <![CDATA[20.18±0.24 cd ]]>

[0112] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0113] As can be seen from Table 4, compared with raw oat milk ROM, the content of protein α-helix and random coil in the oat milk HOM treated with heat treatment is reduced, and the content of β-fold is increased. Compared with the oat milk treated with heat treatment, the content of protein α-helix and random coil in the oat milk treated with oat grains is further reduced, and the content of β-fold is further increased. This shows that both the heating treatment and the baking treatment of oat grains have changed the secondary structure of oat milk protein. Existing studies have shown that the β-fold structure of protein after heat treatment denaturation is no longer a simple regular β-fold structure (i.e., the intramolecular β-fold structure in natural protein), but has formed a structure called intermolecular β-fold. Therefore, the above phenomenon shows that the secondary structure of the protein in the oat milk sample has changed after heat treatment, from one ordered structure to another.

[0114] In addition, compared with oat milk BOM-1.0min that has not been treated with backfilling residue, the content of α-helix and random coil in oat milk BOM-FR protein treated with backfilling residue increased, and the content of β-fold decreased. This may be related to the fact that the backfilling residue treatment reduces the content of protein relative to the total dry matter in oat milk, and increases the content of substances such as starch and soluble dietary fiber. The sample system becomes more complicated, which affects the measurement results to a certain extent.

[0115] Verification Example 4

[0116] The oat milk samples were subjected to oat milk particle size and particle size distribution measurement, and the results are shown in Table 5 and Figure 3 As shown. The specific operation is as follows: After preparing the raw oat milk, use a rubber-tipped dropper to draw an appropriate amount of sample and add it to the sample pool of the Malvern laser particle size analyzer. When the shading degree reaches about 10%, measure the sample particle size. The experimental parameters of the instrument are set as follows: the speed of the stirrer is set to 2000r / min, and the refractive index of the sample and the continuous phase (deionized water) are set to 1.54 and 1.33 respectively. D(4,3) calculated by the software provided by the instrument is used as the average particle size value of the sample.

[0117] Table 5 Oat milk sample particle size

[0118] sample Particle size (μm) ROM <![CDATA[27.09±0.26 c ]]> HOM <![CDATA[16.65±0.05 a ]]> BOM-0.5min <![CDATA[16.81±0.09 a ]]> BOM-1.0min <![CDATA[17.01±0.49 a ]]> BOM-1.5min <![CDATA[17.50±0.36 a ]]> BOM-2.0min <![CDATA[18.82±0.55 b ]]> BOM-FR <![CDATA[19.39±0.58 b ]]>

[0119] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0120] From Table 5 and Figure 3It can be seen that the particle size of the oat milk sample treated with heating, oat grain baking and backfilling filter residue is significantly lower than that of the raw oat milk sample ROM, with a particle size range of 16.65-19.39μm, and the raw oat milk particle size is 27.09μm. This is because the starch granules in the oat milk are converted into amorphous starch after heating and gelatinization, and the average particle size decreases accordingly. Compared with the HOM particle size of the oat milk treated with heating (16.65μm), the particle size of the oat milk treated with oat grain baking did not change significantly. However, with the extension of baking time, the average particle size of the oat milk increased from 16.81μm to 18.82μm. This is because the extension of baking time intensifies the degree of protein denaturation, reduces protein solubility, and interacts with starch to form larger aggregates, thereby increasing the average particle size of the oat milk. In addition, compared with oat milk BOM-1.0min without backfilling treatment, the average particle size of oat milk BOM-FR in the backfilling residue treatment group increased significantly. This is because the backfilling residue treatment increased the content of substances such as starch, soluble dietary fiber and oat bran in the oat milk, thereby increasing the average particle size of the oat milk.

[0121] Oat milk lotion validation test

[0122] Preparation of oat milk emulsion

[0123] 6 mL of oat milk prepared as described in Example 1 and 6 mL of camellia oil were mixed in a glass sample bottle (27 mm in diameter and 57 mm in height), and dispersed at 20,000 r / min for 1.5 min using a high-speed disperser to prepare an emulsion. The emulsion sample was stored at ambient temperature for 24 h before subsequent determination.

[0124] Verification Example 5

[0125] Emulsion appearance observation and milking index determination: The prepared emulsion was placed at ambient temperature for 1 day, then its appearance was photographed and the height of the emulsified layer was measured, and the milking index of the emulsion was calculated. The results are as follows: Figure 4 (a)~(b) in Chinese.

[0126] Verification Example 6

[0127] Emulsion microstructure observation: The microstructure of the emulsion was observed using an inverted microscope. The specific operation was as follows: After the prepared emulsion was left to stand at ambient temperature for 1 day, a small amount of the emulsion was gently transferred onto a glass slide using a rubber-tipped dropper from the emulsified layer, and then the slide was gently scraped with a cover glass to obtain a sample suitable for observation. The glass slide was then immediately placed on the stage, and a photo of the sample was taken at 20 times magnification using the high-definition camera equipped with the instrument in bright field mode. The results are as follows: Figure 4 As shown in (c).

[0128] Verification Example 7

[0129] The particle size distribution of the emulsion was determined by the same method as in Verification Example 4. The results are shown in Table 6.

[0130] Table 6 Particle size of emulsion

[0131]

[0132]

[0133] Combined with the results of verification examples 5 to 7 Figure 4 As can be seen from (a) and (b) and Table 6, each group of emulsions showed a certain degree of creaming after being placed. Among them, the raw oat milk ROM stable emulsion had the highest creaming index value (37.50%), the most turbid creaming layer, and the largest particle size (100.99 μm), indicating that its emulsification effect was not good. The creaming of the emulsion stabilized by heat-treated oat milk HOM was significantly improved, the creaming value was reduced (24.04%), and the particle size was reduced (88.18 μm). This is because the starch particles in the raw oat milk ROM are difficult to be effectively adsorbed on the oil-water interface, and exist in large quantities in the continuous phase. They also compete with oat protein for adsorption on the surface of oil droplets, thereby reducing the emulsification effect of the oat milk. After the oat milk is heated, the starch particles are converted into amorphous starch, which plays a thickening role in the emulsion system and synergistically stabilizes the emulsion with oat protein, thereby enhancing its adsorption capacity at the oil-water interface. The amorphous starch that is not adsorbed on the oil-water interface fills the gaps between the oil droplets, preventing the aggregation and coalescence of the oil droplets through steric hindrance and self-gelation, thereby improving the emulsification effect of the oat milk and the stability of the emulsion.

[0134] Depend on Figure 4 As can be seen in (c), all emulsions formed spherical droplets of different sizes. The droplet size of each group of emulsions is consistent with the particle size results measured by the corresponding laser particle size analyzer.

[0135] In addition, compared with the oat milk treated with heat, as the baking time of oat grains increases, the creaming index of the emulsion made from the oat milk shows a trend of first decreasing and then increasing. Among them, the creaming index of the emulsion of the BOM-1min oat milk group is the lowest, with a creaming value of 20.19% and a smallest particle size (62.56μm), indicating that its emulsification properties and emulsion stability are the best. This is because after the oat grains are moderately baked, the oat protein undergoes moderate denaturation to expose more hydrophobic groups, thereby improving the emulsification properties of the oat milk. In addition, the results of the determination of the protein content of oat milk show that with the increase of baking time, the protein content gradually decreases, causing the emulsification ability of the oat milk to decrease accordingly. This part of the results is also consistent with the results of the contact angle measurement of the oat milk sample. As the baking time increases, the degree of denaturation of oat protein increases, its solubility and interfacial capacity decrease, and the emulsification effect becomes worse, which is clearly reflected in the BOM-2min oat milk. Compared with other emulsions, the emulsion stabilized by BOM-2min oat milk has a larger particle size and a darker apparent color. This is because large-sized emulsion droplets are not easy to form a relatively uniform dispersed phase, and increase light scattering, which reduces the transparency of the emulsion. As the droplet size in the emulsion decreases, the turbidity decreases and the optical transparency increases.

[0136] Compared with the stable emulsion of oat milk BOM-1min without backfilling residue treatment, the emulsion prepared from oat milk BOM-FR treated with backfilling residue did not undergo creaming, and the particle size was further reduced (50.06μm), indicating that its emulsification properties and emulsion stability were further improved. In addition, it was determined that the solid contents of oat milk BOM-FR and oat milk BOM-FR were 6.36% and 8.55%, respectively. This is because the backfilling residue treatment allows the residual protein, starch, β-glucan and other substances in the residue to be fully dissolved in the oat milk during the heating process, which increases the total solid content in the oat milk, thereby causing the emulsification ability and viscosity of the system to increase, thereby enhancing the emulsification ability of the oat milk. The above results are consistent with the determination results of the basic physical and chemical properties of oat milk.

[0137] Verification Example 8

[0138] Verify the effect of different oil phases on emulsion particle size

[0139] 6 mL of oat milk prepared as described in Example 1 was mixed with 6 mL of oil phase in a glass sample bottle (27 mm in diameter, 57 mm in height), and dispersed at 20000 r / min for 1.5 min using a high-speed disperser to obtain an emulsion. The emulsion sample was stored at ambient temperature for 24 h and then used for the subsequent determination of the emulsion particle size, using the same determination method as above.

[0140] The oil phase includes sunflower oil, corn oil, peanut oil and rapeseed oil in sequence, which can also be used to prepare oat milk emulsion. The appearance, microstructure, particle size distribution and particle size of the emulsion prepared from BOM-FR oat milk and these vegetable oils are shown in Figure 5 and Table 7.

[0141] Table 7 Effect of different oil phases on emulsion particle size

[0142] sample Particle size (μm) BOM-FR Sunflower Oil <![CDATA[61.5483±0.76 c ]]> BOM-FR Corn Oil <![CDATA[55.4303±0.63 b ]]> BOM-FR Peanut Oil <![CDATA[54.6107±0.52 b ]]> BOM-FR Rapeseed Oil <![CDATA[52.7047±0.37 a ]]>

[0143] from Figure 5 As can be seen from Table 7, the emulsions prepared with four vegetable oils, namely sunflower oil, corn oil, peanut oil and rapeseed oil, and camellia oil have similar appearance, microstructure and particle size distribution, and the particle size is between 50-62 μm. All indicators are close to those of the emulsion prepared with camellia oil. Therefore, different oil phases have no significant effect on the particle size of the oat milk emulsion. Based on this, those skilled in the art can use conventional oil phase to prepare oat milk emulsion.

[0144] Oat milk lotion gel validation test

[0145] Based on the results of the oat milk emulsion preparation conditions, oat milk emulsion prepared according to the optimal value was used to prepare oat milk emulsion gel

[0146] Preparation method of oat milk emulsion: oat milk BOM-FR and camellia oil are dispersed in a high-speed disperser at 20000r / min for 1.5min in a volume ratio of 1:1 to prepare an emulsion.

[0147] Preparation of polysaccharide mixed solution: Add a certain amount of agar and sodium alginate to a beaker at the same time, add water to dissolve so that the concentration of agar and sodium alginate in the solution is 2.0% (w / v), place the beaker in a 90°C heat-collecting water bath, stir magnetically and keep warm after fully dissolving for use.

[0148] Verification Example 9

[0149] The emulsion gel was prepared by a one-step dispersion method and a two-step dispersion method, respectively. The specific preparation methods are as follows:

[0150] One-step dispersion method was used to prepare emulsion gel: 4 mL of BOM-FR oat milk, 4 mL of oil phase and 4 mL of polysaccharide solution were added into the sample bottle at the same time, and dispersed at 20,000 r / min for 1.5 min using a high-speed disperser. The obtained emulsion gel (denoted as 1 step) was stored at ambient temperature for 24 h before subsequent determination.

[0151] Emulsion gel was prepared by two-step dispersion method: 4 mL of BOM-FR oat milk and 4 mL of oil phase were added to the sample bottle, and a high-speed disperser was used to disperse the mixture at a speed of 20,000 r / min for 1.5 min for the first dispersion. Then 4 mL of polysaccharide solution was added to the sample bottle, and the mixture was placed in a 90°C water bath for 10 min. The sample was then dispersed for the second time at a speed of 20,000 r / min for 1.5 min. The obtained emulsion gel (denoted as 2step) was stored at ambient temperature for 24 h for subsequent determination.

[0152] The oat milk emulsion gel prepared by the one-step dispersion method and the two-step dispersion method was observed for appearance, microstructure and particle size. Except for the particle size determination, the method was the same as that of Verification Examples 5 to 7. The rheological properties of the oat milk emulsion gel were determined as follows. The results are shown in Tables 8 and Figure 6 shown.

[0153] Particle size determination: Image J software was used to measure the average particle size of the droplets in the microscopic photographs of the emulsion gel. The results are shown in Tables 8-11.

[0154] Rheological property determination method: The rheological properties of the emulsion gel sample were tested using a rotational rheometer, with the trimming gap set to 1050 mm, the test gap set to 1000 mm, and the test temperature set to 25°C. The prepared sample was then loaded between a parallel plate with a diameter of 40 mm and a Peltier plate for the following test. When loading the sample, a weighing spoon was used to transfer the emulsion gel sample without calcium ions added. For the emulsion gel sample with calcium ions added, it was prepared in a beaker with a diameter greater than 40 mm in advance, and it was carefully cut into a thin layer of 1 mm thickness, and then transferred to the test platform of the rheometer for testing.

[0155] Stress amplitude sweep: the storage modulus (G') and loss modulus (G") of the emulsion gel sample as a function of stress are measured at a frequency of 1 Hz and a strain range of 0.01-50%, and the linear viscoelastic region of the sample is determined; frequency sweep: the frequency sweep is performed at a frequency range of 0.1-10 Hz and a strain of 0.5% (within the linear viscoelastic region); oscillation temperature sweep: before the test begins, silicone oil is sealed around the sample to prevent moisture loss during the test, and then, under the conditions of a fixed strain of 0.5% (within the linear viscoelastic range) and a frequency of 1 Hz, a temperature sweep test is performed from 20°C to 100°C at a rate of 5°C / min.

[0156] Table 8 Particle size of emulsion gel in different dispersion methods

[0157] sample Particle size (μm) 1step 42.38±2.53 2step 24.47±0.65

[0158] From Figure 6From the photo of the emulsion gel in (a), it can be seen that the emulsion gel prepared by the one-step dispersion method has a darker appearance. Figure 6 From Figure (b) and Table 8, compared with the particle size of the emulsion gel prepared by the two-step dispersion method (24.47 μm), the droplet size of the emulsion gel prepared by the one-step dispersion method is also larger (42.38 μm), indicating that its emulsification effect is relatively poor. This is because it is difficult for the one-step dispersion method to disperse the emulsion gel system evenly at one time, while the two-step dispersion method avoids this problem. First, the oat milk and polysaccharide solution are dispersed evenly in advance, and then the oil phase is added for the second dispersion, so that the two dispersions are more uniform, which improves the emulsification effect. Therefore, the emulsion gel prepared thereby has a whiter appearance and a smaller droplet size.

[0159] The linear viscoelastic region of the latex gel samples was tested by stress scanning, and the influence of two different dispersion methods on the modulus (G' and G') was investigated. Figure 6 As shown in (c), within the linear viscoelastic region, G' of the emulsion gel samples prepared under different dispersion conditions is always greater than G", indicating that both samples have a gel state dominated by elasticity. After the emulsion gel enters the nonlinear viscoelastic region, G' begins to drop sharply, and G" first rises and then decreases. This trend is called weak strain overshoot in rheology and is a typical characteristic of gel materials.

[0160] Figure 6 (d) shows the trend of the modulus of the latex gel sample changing with frequency. It can be seen that G' and G" of the two latex gel samples increase slightly with the increase of frequency, showing a weak frequency dependence. G' and G" do not intersect in the entire frequency range, resulting in solid-like rheological behavior, indicating that the latex gel sample has a relatively high stability. In addition, there is no significant difference in the modulus of the latex gels prepared by the two different dispersion methods. This is because the modulus of the latex gel is mainly affected by the content of the two polysaccharides, sodium alginate and agar. Therefore, when the content of the two polysaccharides is the same, their moduli are also equivalent.

[0161] Figure 6 (e) shows the trend of the modulus of the emulsion gel sample changing with temperature. In the temperature range of 20°C to 100°C, as the test temperature increases, the modulus of the emulsion gel sample shows a trend of first slowly decreasing, and then rapidly decreasing after the temperature reaches 70°C. This is because the emulsion gel prepared with agar as a gelling agent is a thermoreversible gel, which is gel-like at low temperatures and liquid-like at high temperatures. The temperature range for the transition from gel to sol is 70-85°C. At this time, the intermolecular hydrogen bond interaction of agar in the emulsion gel is weakened, and the molecules begin to move and lose their ordered arrangement, resulting in the destruction of the gel structure.

[0162] Verification Example 10

[0163] Verify the effect of agar concentration in polysaccharide solution on emulsion gelation

[0164] The emulsion gel was prepared by the two-step dispersion method as described in Verification Example 9, wherein the sodium alginate concentration in the polysaccharide solution was fixed at 2.0% (w / v), and the agar concentrations were set to 0, 1.0, 2.0, 3.0 and 4.0%, respectively. Five polysaccharide solutions were prepared and used to prepare emulsion gels. According to the concentration of agar in the aqueous phase of the prepared emulsion gels, the corresponding emulsion gel samples were named AG 0, AG 0.5, AG 1.0, AG 1.5 and AG 2.0%, respectively.

[0165] The oat milk emulsion gel prepared by the above method was subjected to appearance observation, microstructure observation, particle size measurement and rheological property measurement, respectively, the method was the same as that of Verification Example 8, and the results are shown in Tables 9 and Figure 7 shown.

[0166] Table 9 Particle size of emulsion gels with different agar concentrations

[0167]

[0168]

[0169] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0170] like Figure 7 As shown in (a). When agar is not added, a stable emulsion gel cannot be formed. Stable emulsion gel systems can be formed at other agar concentrations. In addition, when the agar concentration is 2.0%, the apparent color of the emulsion gel is relatively dark. Figure 7 The microstructure in (b) and the particle size distribution results in Table 9 show that the emulsion gel in this group has the largest particle size (50.29±0.05μm), indicating that the emulsification effect is not good at higher agar concentrations. As the agar concentration decreases, the particle size of the emulsion gel gradually decreases, and the particle size is the smallest when no agar is added (20.67±0.10μm), indicating that its emulsification ability gradually increases with the decrease of agar concentration. This is because when the viscosity of the system is within an appropriate viscosity range, the higher the viscosity, the stronger the emulsification effect and emulsification stability, and when the viscosity exceeds this appropriate viscosity range, the emulsifier will be difficult to be quickly dispersed to the oil-water interface.

[0171] The stress scanning results of the emulsion gel sample are as follows Figure 7As shown in (c), within the linear viscoelastic region, G' of the emulsion gel sample is always greater than G". In addition, in the nonlinear viscoelastic region, the gel fracture point (the intersection between G' and G") of the emulsion gel with an agar concentration in the range of 0.5 to 2.0% appears earlier as the agar concentration increases. The appearance of the gel fracture point indicates that the internal structure of the sample undergoes permanent deformation and loses its solid-like rheological properties. This indicates that the higher the agar concentration of the emulsion gel, the weaker its ability to resist strain, the worse its ductility, and the higher its brittleness.

[0172] from Figure 7 From the results of the frequency scan in (d), compared with the emulsion gel with added agar, the trend of the modulus of the emulsion gel without added agar increasing with the increase of frequency is the most prominent, indicating that its frequency dependence is relatively high and the stability of the emulsion gel is relatively poor. In addition, G' and G" of the emulsion gel show an increasing trend with the increase of agar concentration. This is because the gelation mechanism of agar is that the agarose chain dissolved in water presents a random coil conformation when it is above the gelation temperature, and part of the chain is transformed into a helical conformation when the temperature is lowered. This helical part tends to aggregate with each other through hydrogen bonds and cross-link to form a gel network. Therefore, when the agar concentration increases, the hydrogen bond interaction between the helical conformations of the agarose chain is enhanced, more cross-linking points are formed, and a denser gel network structure is formed, thereby increasing the strength and stability of the emulsion gel. In addition, compared with the increase in the modulus of the emulsion gel brought about by the increase of agar concentration from 0% to 0.5%, the increase in the modulus of the emulsion gel brought about by the increase of agar concentration from 0.5% to 1.0% is more significant. This is because the cross-linking points at lower agar concentrations are insufficient, and the gel network formed is not dense enough. When the agar concentration increases from 0.5% to 1.0%, the cross-linking points increase, the gel network structure formed is more compact, the droplets are difficult to aggregate, and the gel stability is enhanced, so the modulus of the emulsion gel increases significantly.

[0173] In addition, the results of the temperature scan are as follows Figure 7 As shown in (e), within the entire temperature range, the modulus of the emulsion gel without agar addition tends to decrease slowly with increasing temperature. When the agar concentration is 0.5, 1.0, 1.5 and 2.0%, in the temperature range of about 20°C to 70°C, the modulus of the emulsion gel decreases slowly with increasing temperature. When the temperature continues to rise, the modulus decreases rapidly, and the higher the agar concentration, the faster the rate of decrease of the emulsion gel modulus. When the temperature rises to 100°C, the modulus of each group of emulsion gels drops to the lowest and is basically the same. This is because the gel-sol transition temperature range of agar-based gel is 70-85°C. When the temperature is too high, the hydrogen bonds break and the gel structure is destroyed. At the same time, since the higher the agar concentration, the greater the initial modulus of the emulsion gel, the greater the modulus lost by the system during the transformation from gel to sol.

[0174] Verification Example 11

[0175] Verify the effect of different sodium alginate concentrations on emulsion gel

[0176] The emulsion gel was prepared by the two-step dispersion method described in Verification Example 9, wherein the concentration of agar in the polysaccharide mixed solution was fixed at 2.0% (w / v), and the concentration of sodium alginate was set to 0, 1.0, 2.0, 3.0 and 4.0%, respectively. Five polysaccharide mixed solutions were prepared and used for the preparation of emulsion gels, and the corresponding emulsion gel samples were named SA 0, SA 0.5, SA 1.0, SA 1.5 and SA2.0%, respectively, according to the concentration of sodium alginate in the aqueous phase of the prepared emulsion gels.

[0177] The oat milk emulsion gel prepared by the above method was subjected to appearance observation, microstructure observation, particle size measurement and rheological property measurement, respectively, the method was the same as that of Verification Example 8, and the results are shown in Tables 10 and Figure 8 shown.

[0178] Table 10 Particle size of emulsion gel at different sodium alginate concentrations

[0179] sample Particle size (μm) SA 0% <![CDATA[116.03±3.05 e ]]> SA 0.5% <![CDATA[32.01±0.87 b ]]> SA 1.0% <![CDATA[24.47±0.65 a ]]> SA 1.5% <![CDATA[42.19±0.80 c ]]> SA 2.0% <![CDATA[48.22±0.99 d ]]>

[0180] Note: Values ​​with different letters in the same column indicate significant differences (p < 0.05).

[0181] As shown in Table 10, Figure 8 As shown, Figure 8 In (a), it can be seen that the bottom of the emulsion gel when the sodium alginate concentration is 1.5% and the whole of the emulsion gel when the sodium alginate concentration is 2.0% both present a darker apparent color, indicating that the dispersion is uneven and the emulsification effect is poor. When the sodium alginate concentration is 0, 0.5, and 1.0%, the appearance of the emulsion gel is milky white, indicating that the emulsification effect is good. Figure 8 From the microstructure in (b) and the particle size results in Table 3-7, the droplet size decreases first and then increases with the increase of sodium alginate concentration. The particle size is the smallest (24.47μm) when the sodium alginate concentration is 1.0%, and the largest (116.03μm) when it is 0%. This is because as the sodium alginate concentration increases, the viscosity of the system is too high, and the emulsifier is difficult to be quickly dispersed to the oil-water interface, which reduces the emulsification effect.

[0182] The stress scanning results of the emulsion gel sample are as follows Figure 8 As shown in (c), within the linear viscoelastic region, G′ of the emulsion gel sample is always greater than G″. In addition, in the nonlinear viscoelastic region, as the concentration of sodium alginate increases, the gel fracture point of the emulsion gel appears later, indicating that the higher the sodium alginate concentration, the stronger the ability to resist strain, the higher the ductility, and the lower the brittleness.

[0183] The frequency scan results are as follows: Figure 8 As shown in (d), the modulus of each group of latex gels slightly increased with the increase of frequency, showing a weak frequency dependence, indicating that the latex gel is relatively stable. Compared with the large difference between the moduli of the latex gels with different agar concentrations, the difference between the moduli of the latex gels with different sodium alginate concentrations is significantly smaller. In addition, the linear viscoelastic region of the latex gel samples added with sodium alginate is relatively wider, indicating that the material has a higher elastic limit and better viscoelastic properties within a wider range of stress, and can maintain its original shape and properties to a greater extent, making the structure of the latex gel sample more stable. In addition, the modulus of the latex gel shows a decreasing trend with the increase of the amount of sodium alginate added. This is because sodium alginate, as a macromolecular substance, plays a spatial barrier role in the process of agarose chains forming a gel network through hydrogen bonding, hindering the aggregation and cross-linking of agar, reducing the density and strength of the gel network, and reducing the modulus of the latex gel.

[0184] The results of the temperature scan are as follows: Figure 8 As shown in (e), the change pattern of the modulus of the latex gel with different sodium alginate concentrations with temperature is basically the same. Except that the initial modulus is affected by different sodium alginate concentrations, it is shown that when the temperature rises from 20°C to about 70°C, the modulus of the latex gel slowly decreases with the increase of temperature. When the temperature continues to rise, the modulus decreases rapidly. It is worth noting that under high temperature conditions of about 85-100°C, the modulus of the latex gel when the sodium alginate concentration is 0.5, 1.0, 1.5 and 2.0% is higher than that when no sodium alginate is added. This is because sodium alginate plays a thickening role in the system.

[0185] Verification Example 12

[0186] Verify the effect of different oil phase volume fraction concentration on emulsion gel

[0187] The emulsion gel was prepared by the two-step dispersion method described in Verification Example 7, wherein the concentrations of agar and sodium alginate in the polysaccharide mixed solution were fixed at 2.0% (w / v), and the volume fractions of the oil phase in the emulsion gel were adjusted to 20.00, 26.67, 33.33, 40.00 and 46.67%, respectively. The corresponding emulsion gel samples were named Φ20.00, Φ26.67, Φ33.33, Φ40.00 and Φ46.67%, respectively.

[0188] The oat milk emulsion gel prepared by the above method was subjected to appearance observation, microstructure observation, particle size measurement and rheological property measurement, respectively, the method was the same as that of Verification Example 8, and the results are shown in Tables 11 and Fig. 9 shown.

[0189] Table 11 Particle size of emulsion gels with different oil phase volume fractions

[0190] sample Particle size (μm) Φ20.00% <![CDATA[14.82±0.25 a ]]> Φ26.67% <![CDATA[20.33±0.31 b ]]> Φ33.33% <![CDATA[24.47±0.65 c ]]> Φ40.00% <![CDATA[32.86±1.27 d ]]> Φ46.67% <![CDATA[46.91±1.08 e ]]>

[0191] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0192] like Fig. 9 As shown in (a). When Φ46.67%, the emulsion gel has a dull color, indicating that its emulsification effect is relatively poor. Fig. 9 From the results of the microstructure in (b) and the particle size in Table 11, as the volume fraction of the oil phase increases, the droplet size increases accordingly. The particle size is the smallest (14.82 μm) when Φ20.00%, and the particle size is the largest (46.91 μm) when Φ46.67%. This is because when the emulsifier content remains unchanged, the higher the oil phase volume fraction, the less emulsifier content per unit oil-water interface, and the droplets are more likely to coalesce, causing the droplet size to increase.

[0193] The stress scanning results of the emulsion gel sample are as follows Fig. 9 As shown in (c), within the linear viscoelastic region, G′ of the emulsion gel sample is always greater than G″. In addition, the gel fracture points of emulsion gels with different oil phase volume fractions are basically the same, indicating that different oil phase volume fractions have no obvious effect on the strain resistance, ductility and brittleness of the emulsion gel.

[0194] The frequency scanning results of the emulsion gel sample are as follows Fig. 9 As shown in (d), the modulus of each group of emulsion gels increases slightly with the increase of frequency, showing a weak frequency dependence, indicating that the emulsion gel is relatively stable. In addition, the modulus of the emulsion gel is relatively low when Φ20.00%. As the volume fraction of the oil phase increases, the modulus of the emulsion gel increases slowly. When the volume fraction of the oil phase is too high, the modulus decreases instead. This is because when the volume fraction of the oil phase is low, as the volume fraction of the oil phase increases, the interface area of ​​the droplets increases, the interaction force between the droplets is enhanced, the gel stability is improved, and the modulus increases. When the volume fraction of the oil phase is too high, the droplets are prone to aggregation, which increases the particle size, reduces the stability of the emulsion gel, and thus reduces the modulus. It is worth noting that the change in the volume fraction of the oil phase has a very limited effect on the modulus of the emulsion gel, which indicates that the modulus of the emulsion gel system is mainly affected by the type and content of substances in the water phase.

[0195] From the temperature scan Fig. 9 From the results in (e), the variation of the modulus of the emulsion gels with different oil phase volume fractions with temperature is basically the same as the variation of the modulus of the emulsion gels with different agar and sodium alginate concentrations mentioned above.

[0196] Verification Example 13

[0197] Verify the effect of different calcium ion concentrations on emulsion gel

[0198] The emulsion gel was prepared by the two-step dispersion method described in Verification Example 9, wherein the concentrations of agar and sodium alginate in the polysaccharide solution were fixed at 2.0% (w / v), the volume fraction of the oil phase was fixed at 33.33%, and a calcium chloride solution was added to the emulsion gel cooled to ambient temperature so that the mass concentration of calcium ions in the emulsion gel was 0, 0.1, 0.4, 0.7, 1.0 and 1.3%, respectively. The corresponding emulsion gel samples were named CaCl2, CaCl2 and CaCl2. 2+ 0. Ca 2+ 0.1, Ca 2+ 0.4, Ca 2+ 0.7, Ca 2+ 1.0 and Ca 2+ 1.3%.

[0199] The oat milk emulsion gel prepared by the above method was subjected to surface observation, microstructure observation, particle size measurement and rheological property measurement, respectively, using the same method as Example 8. The results are as follows: Fig.10 shown.

[0200] like Fig.10 As shown in (a). Compared with the latex gel with added calcium ions (concentrations of 0.1, 0.4, 0.7, 1.0 and 1.3%), the latex gel without added calcium ions has slightly weaker support and has a certain degree of spreadability, while the latex gel with added calcium ions has stronger support, is not easy to deform, and has a clear and smooth surface state and a flat and uniform cross-section state. There is no obvious difference in the appearance of the latex gel prepared at different calcium ion concentrations. In addition, due to the high strength of the latex gel system of the group with added calcium ions, microscopic structure observation was not carried out.

[0201] The stress scanning results of the emulsion gel sample are as follows Fig.10 As shown in (b), within the linear viscoelastic region, G′ of the latex gel sample is always greater than G″. In the nonlinear viscoelastic region, compared with the group without calcium ion addition, the modulus of the latex gel in the group with calcium ion addition shows a sharp downward trend, and as the calcium ion concentration increases, the gel fracture point of the latex gel appears earlier, indicating that the higher the calcium ion concentration, the weaker the ability of the latex gel to resist strain, the worse the ductility, and the higher the brittleness. This is because the gel network structure formed by ionic crosslinking of sodium alginate and calcium ions has a large gel strength, but this gel network structure is prone to break when subjected to external stress, so it usually exhibits a large gel strength and high brittleness.

[0202] The results of the frequency sweep are as follows: Fig.10As shown in (c), compared with the G" of the emulsion gel when calcium ions are added, the G" of the emulsion gel when no calcium ions are added has a more prominent trend of increasing with increasing frequency, indicating that the emulsion gel when calcium ions are added has a relatively low frequency dependence and the gel system is more stable, which is related to the denser gel structure and greater gel strength formed by cross-linking of sodium alginate and calcium ions. In addition, compared with the modulus of the emulsion gel when no calcium ions are added, with the increase of calcium ion concentration, the modulus of the emulsion gel prepared therefrom increases significantly, and compared with the increasing trend of the emulsion gel modulus when the calcium ion concentration increases from 0.7% to 1.3%, the increasing trend of the emulsion gel modulus when the calcium ion concentration increases from 0% to 0.7% is more significant. This is because at low calcium ion concentrations, with the increase of calcium ion concentration, the cross-linking structure formed by calcium ions and carboxyl groups in sodium alginate increases, which increases the density of the gel network, thereby improving the strength and stability of the emulsion gel. However, when the calcium ion concentration continues to increase, the gel network has already approached the maximum cross-linking density, and adding more calcium ions will not significantly enhance the strength of the gel.

[0203] The results of the temperature scan are as follows: Fig.10 As shown in (d), the law of the change of the modulus of the latex gel with temperature when no calcium ions are added has been summarized in the previous article. In contrast, when the test temperature increases from 20°C to about 70°C, the modulus of the latex gel with the addition of calcium ions shows a slow downward trend, which is roughly the same as the law of the change of the modulus with temperature when no calcium ions are added. As the temperature rises to above 70°C, compared with the rapid decrease of G' and G" of the sample with the increase of temperature when no calcium ions are added, the G' of the latex gel with the addition of calcium ions decreases slightly, while G" increases to a certain extent, and the overall modulus does not change much. This is because the crosslinking of sodium alginate and calcium ions forms a thermally irreversible gel with strong thermal stability. When the temperature rises to above 70°C, the agar-based gel structure in the latex gel is gradually destroyed. Since the modulus of the system is mainly affected by the concentration of sodium alginate and calcium ions, G' only decreases slightly after the agar-based gel structure is destroyed.

[0204] Verification Example 14

[0205] Verification of the effect of different polysaccharide concentrations on emulsion gel:

[0206] The emulsion gel was prepared by the two-step dispersion method described in Verification Example 9, except that the volume fraction of the oil phase was fixed at 33.33%, the calcium ion concentration was 0%, and the five pairing combinations of agar concentration and sodium alginate concentration in the polysaccharide solution were as follows: 0.5% and 1.0%, 1.0% and 1.5%, 1.0% and 1.0%, 1.0% and 0.5%, and 1.5% and 1.0%, thereby preparing five emulsion gels for subsequent measurements.

[0207] The prepared emulsion gel was subjected to burst strength test, and the test method was as follows:

[0208] The gel burst strength of the emulsion gel was determined using a texture analyzer. The newly prepared emulsion gel sample was immediately poured into a cylindrical plastic cup with a diameter of 3 cm and a height of 2.5 cm and stored at ambient temperature for 24 h. The gel burst strength was determined using a texture analyzer at ambient temperature. The probe model was P / 0.5 and the test parameters were as follows: test rate 0.5 mm / s, post-test upward rate 1.0 mm / s, and downward pressure distance 15 mm.

[0209] The prepared emulsion gel was tested for water holding capacity, and the test method was as follows:

[0210] Prepare the emulsion gel in a 50 mL round-bottom centrifuge tube. After storing at ambient temperature for 1 day, record the weight W of the gel sample. 1 , centrifuge at 5000r / min for 30min at ambient temperature, remove the precipitated water, and record the remaining sample weight W 2 , and take photos to record the appearance of the emulsion after centrifugation. WHC is expressed as a percentage.

[0211] The prepared emulsion gel was subjected to freeze-thaw stability test, and the test method was as follows:

[0212] The prepared emulsion gel was placed at ambient temperature for 24 hours, then frozen at -18°C for 20 hours, and then thawed at 25°C for 4 hours. The above freeze-thaw cycle was repeated five times, and the appearance of the emulsion gel after each freeze-thaw treatment was photographed. The freeze-thaw stability of the emulsion was evaluated by comparing the oil-water separation state of the emulsion.

[0213] Test results such as Fig.11 As shown in Table 12.

[0214] Table 12 Gel rupture strength (a) and water holding capacity (b) of latex gels with different polysaccharide concentrations

[0215]

[0216]

[0217] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0218] As shown in Table 12, when the sodium alginate concentration is fixed at 1.0%, the gel rupture strength of the emulsion gel increases with the increase of agar concentration, which is because the gel network structure becomes denser with the increase of agar concentration. In addition, when the agar concentration is fixed at 1.0%, the gel rupture strength of the emulsion gel decreases with the increase of sodium alginate concentration, which is consistent with the results of the above rheological test.

[0219] The water holding capacity (WHC) results of the emulsion gel samples are as follows: Fig.11 As shown in (a), when the agar concentration is fixed at 1.0%, as the sodium alginate concentration increases, the oil-water separation phenomenon of the corresponding emulsion gel after centrifugation becomes more serious. When the sodium alginate concentration is 0.5%, the emulsion gel has a strong water holding capacity, with a WHC value of 26.01%, and when the sodium alginate concentration is 1.5%, the emulsion gel has a weak water holding capacity, with a WHC value of 15.51%, indicating that with the increase of sodium alginate concentration, the water holding capacity of the emulsion gel gradually decreases. This is because the increase in sodium alginate concentration reduces the gel rupture strength of the emulsion gel and reduces its stability. In addition, when the sodium alginate concentration is fixed at 1.0%, as the agar concentration increases, the oil-water separation phenomenon of the corresponding emulsion gel after centrifugation becomes milder. When the agar concentration is 0.5%, the water holding capacity of the emulsion gel is weak, with a WHC value of 15.37%, while when the agar concentration is 1.5%, the water holding capacity of the emulsion gel is strong, with a WHC value of 83.35%, indicating that with the increase of agar concentration, the water holding capacity of the emulsion gel gradually increases. This is because the increase in agar concentration makes the gel network structure more compact, the gel strength increases, and it can withstand stronger external stress and has stronger capillary force, so it can effectively retain the water in the gel network.

[0220] The freeze-thaw stability of emulsion gel mainly depends on its own composition and structure. Generally speaking, when the viscosity and gel strength of the emulsion gel are large, ice crystals can be effectively prevented from destroying the droplets in the sample during the freezing process, and the freeze-thaw stability is good. Fig.11 As shown in (b), the emulsion gel samples that have undergone freeze-thaw treatment all showed different degrees of oil-water separation, accompanied by the formation of a large number of pores. This is because a large number of ice crystals were generated inside the emulsion gel sample during the freezing process, which destroyed its stable gel network structure and droplet state, causing the droplets to coalesce during the melting process. As the number of freeze-thaw cycles increased, water and oil phases gradually escaped, causing oil-water separation, and forming a large number of pores, which reduced the stability of the emulsion gel sample. In addition, when the agar concentration was fixed at 1.0%, the degree of oil-water separation of the emulsion gel sample gradually decreased with the increase of sodium alginate concentration, and the best freeze-thaw stability was achieved when the sodium alginate concentration was 1.5%. This is because sodium alginate has a relatively stable hydration and thickening effect, which helps to maintain the stability of the system during the freeze-thaw process. When the sodium alginate concentration is fixed at 1.0%, the degree of oil-water separation of the emulsion gel sample gradually decreases with the increase of agar concentration. This is because the increase of agar concentration makes the gel structure denser and the gel strength increases, which can better resist the damage of ice crystals to the gel structure during freezing and thawing.

[0221] Verification Example 15

[0222] According to the preferred results of Verification Example 14, when the concentration ratio of agar: sodium alginate is 1.0%:1.0% and 1.5%:1.0%, the properties of the emulsion gel are relatively good, so these two polysaccharide ratios are selected to carry out the following experiments. Based on these two polysaccharide ratios, the calcium ion concentrations are set to 0.1% and 1.0% respectively to prepare four emulsion gels, and the bursting strength, water holding capacity and freeze-thaw stability are measured. The measurement method is the same as that of Verification Example 13. The results are shown in Tables 13 and 14. Fig.12 shown.

[0223] Table 13 Gel rupture strength (a) and water holding capacity (b) of emulsion gels with different calcium ion concentrations

[0224]

[0225]

[0226] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0227] The gel rupture strength results of the emulsion gel are shown in Table 13. Under two different polysaccharide ratios, the gel strength of the emulsion gel when the calcium ion concentration is 1.0% is significantly greater than the emulsion gel when the calcium ion concentration is 0.1%, indicating that as the calcium ion concentration increases, the gel strength increases. This is because as the calcium ion concentration increases, the cross-linked structure formed with sodium alginate increases, and the gel network becomes denser, which increases the gel strength, which is consistent with the results of the rheological test. In addition, under the same calcium ion concentration, compared with the emulsion gel when the agar: sodium alginate concentration ratio is 1.5%: 1.0%, the gel rupture strength of the emulsion gel with a concentration ratio of 1.0%: 1.0% is significantly greater. This is because as the agar concentration increases, the gel structure formed by agar becomes denser, which hinders the penetration of calcium ions in the emulsion gel system, affects the cross-linking effect of calcium ions and sodium alginate, and reduces the gel strength of the emulsion gel.

[0228] The water holding capacity (WHC) results of the emulsion gel samples are as follows: Fig.12As shown in (a), under two polysaccharide ratios, compared with the latex gel without calcium ion addition (WHC range of 20.68-83.35%), the water holding capacity of the latex gel at calcium ion concentrations of 0.1% and 1.0% is stronger, with a WHC range of 87.18-95.03%. This shows that the addition of calcium ions enhances the water holding capacity of the latex gel, because the cross-linking of calcium ions and sodium alginate further enhances the gel strength and stability of the latex gel, thereby enhancing the water holding capacity of the sample. In addition, under the condition of agar: sodium alginate concentration ratio of 1.0%:1.0%, compared with the latex gel at a calcium ion concentration of 1.0% (WHC value of 88.58%), the water holding capacity of the latex gel at a calcium ion concentration of 0.1% is higher, with a WHC value of 95.03%. Under the condition of agar: sodium alginate concentration ratio of 1.5%:1.0%, the water holding capacity of the emulsion gel at a calcium ion concentration of 0.1% was higher than that of the emulsion gel at a calcium ion concentration of 1.0% (WHC value of 87.18%), with a WHC value of 94.67%. This shows that under these two polysaccharide ratios, the water holding capacity of the emulsion gel at a calcium ion concentration of 0.1% is stronger. This is because when the calcium ion concentration is too high, the gel structure is too dense, thereby squeezing the space where the water inside the gel is located, causing the water to escape from the emulsion gel, resulting in a decrease in the water holding capacity of the gel. In addition, since the emulsion gel is more brittle when the calcium ion concentration is 1.0%, it is more likely to break when subjected to external forces, resulting in a decrease in water holding capacity. The results show that the gel strength of the fish paste gel increased after being treated with dense phase carbon dioxide, but the water holding capacity decreased significantly. It is worth noting that when the calcium ion concentration is fixed, the water holding capacity of the emulsion gel with an agar:sodium alginate concentration ratio of 1.5%:1.0% is slightly weaker than that of the emulsion gel with an agar:sodium alginate concentration of 1.0%:1.0%. This is because the higher agar concentration hinders the cross-linking effect of calcium ions and sodium alginate, which is consistent with the results of the gel rupture strength measurement.

[0229] The freeze-thaw stability results of the emulsion gel samples are as follows Fig.12As shown in (b), when the polysaccharide concentration is fixed, the emulsion gel in the group with a calcium ion concentration of 0.1% is more likely to undergo oil-water separation during the freeze-thaw process than the emulsion gel in the group with a calcium ion concentration of 1.0%, indicating that as the calcium ion concentration increases, the freeze-thaw stability of the emulsion gel becomes stronger. This is because the gel structure formed by the cross-linking of a higher calcium ion concentration and sodium alginate is tighter and the gel strength is higher. In addition, when the calcium ion concentration is fixed, the degree of oil-water separation of the emulsion gels with two different polysaccharide concentrations during the freeze-thaw process is basically the same, indicating that the two different agar concentrations of 1.0% and 1.5% have no significant effect on the freeze-thaw stability of the emulsion gel. This is because the gel strength of the emulsion gel system with added calcium ions is mainly determined by the cross-linking degree of sodium alginate and calcium ions. Therefore, when the sodium alginate and calcium ion concentrations are the same, the two different agar concentrations of 1.0% and 1.5% will not significantly affect the gel strength and freeze-thaw stability of the emulsion gel. The above results are consistent with the results of the determination of the gel rupture strength.

[0230] Example 4

[0231] Preparation method of emulsified sausage: the lean meat mass fraction is 80%, the back fat mass fraction is 20%, 1% salt and 0.2% sodium tripolyphosphate (water retaining agent) are added, mixed and then beaten evenly with a meat grinder (beating 3 times, each time for 15 seconds); the obtained meat filling is stuffed into the collagen casing, and then the emulsified sausage is placed in a water bath and steamed at 85°C for 30 minutes, taken out, washed, dried and naturally cooled to ambient temperature, and refrigerated at 4°C for testing.

[0232] Emulsified sausages were prepared by replacing pig back fat with emulsion gel. The specific operation was as follows: first, the emulsion gel was prepared by a two-step dispersion method, so that the concentrations of agar and sodium alginate in the aqueous phase of the prepared emulsion gel were both 1.0%, and the volume fraction of the oil phase was 33.33%. On this basis, the calcium ion concentrations in the emulsion gel were set to 0, 0.1 and 1.0%, respectively, to prepare three emulsion gels. Subsequently, on the basis of keeping the mass fraction of lean pork unchanged, the above three emulsion gels were used to prepare emulsified sausages at 50% and 100% pig back fat replacement levels, respectively. According to different replacement rates and different calcium ion concentrations in the emulsion gel, the prepared emulsified sausages were named 50%-0%, 50%-0.1%, 50%-1.0%, 100%-0%, 100%-0.1% and 100%-1.0%, respectively. The prepared sausages were subjected to appearance observation and cooking loss rate determination, water holding capacity, color value, pH value, volatile components, TBA value, and texture characteristics determination. The determination methods and results are shown below.

[0233] Apparent observation and cooking loss rate determination method:

[0234] Determine the mass of the emulsified sausage before cooking, denoted as m 1After steaming and cooling to ambient temperature, use absorbent paper to absorb the surface moisture of the emulsified sausage and measure its mass after steaming, which is recorded as m 2 , the cooking loss rate of the emulsified sausage was calculated using the formula, and photos were taken to record the appearance of the surface and cross section of the emulsified sausage after cooking. The results are as follows Fig.13 As shown in Table 14.

[0235] Water holding capacity determination method:

[0236] First, cut the emulsified sausage into small pieces of uniform size, weigh about 3g of chopped emulsified sausage, record it as m 1 , wrap it completely with filter paper, put it into a 50mL centrifuge tube with a small piece of absorbent cotton in advance, and centrifuge it at 5000r / min for 15min. Weigh the mass of the emulsified sausage after centrifugation and record it as m 2 The water holding capacity of the emulsified sausage was calculated using the formula and the results are shown in Table 14.

[0237] Table 14 Cooking loss and water holding capacity of emulsified sausage

[0238] sample Cooking loss (%) Water holding capacity (%) Control group <![CDATA[3.13±0.19 ab ]]> <![CDATA[68.91±1.26 cd ]]> 50%-0% <![CDATA[3.42±0.13 abcd ]]> <![CDATA[67.42±0.61 c ]]> 50%-0.1% <![CDATA[2.99±0.17 a ]]> <![CDATA[71.39±0.36 de ]]> 50%-1.0% <![CDATA[3.28±0.23 abc ]]> <![CDATA[72.61±0.49 e ]]> 100%-0% <![CDATA[4.17±0.18 d ]]> <![CDATA[59.75±0.40 a ]]> 100%-0.1% <![CDATA[3.76±0.26 bcd ]]> <![CDATA[60.91±0.08 a ]]> 100%-1.0% <![CDATA[3.94±0.28 cd ]]> <![CDATA[63.75±1.22 b ]]>

[0239] Note: Values ​​with different letters in the same column indicate significant differences (p < 0.05).

[0240] like Fig.13 As shown. Each group of emulsified sausages has a full and firm appearance, and as the fat replacement rate increases, the appearance of the emulsified sausages becomes whiter. As shown in Table 14, compared with the cooking loss rate of the control group sausage (3.13%), there was no significant difference in the cooking loss rate of the emulsified sausages in each group at a 50% replacement rate, ranging from 2.99 to 3.42%, while the cooking loss rate of the emulsified sausages in each group at a 100% fat replacement rate was significantly higher than that of the control group sausage, ranging from 3.76 to 4.17%. This is because the emulsified sausages are prone to water loss during the cooking process, and the water content in the emulsion gel is high. Therefore, as the fat replacement rate increases, the more water is lost, the greater the cooking loss rate. At the same time, the animal fat particles in the meat mixture help to lose water in a stable and controlled manner, thereby improving the texture of the emulsified sausage. It is worth noting that compared with the emulsified sausages without added calcium ions, the cooking loss rate of the emulsified sausages at concentrations of 0.1% and 1.0% is lower. This is because the gel formed by cross-linking of sodium alginate and calcium ions is stronger and has a stronger water holding capacity, so the water loss during the cooking process is less.

[0241] As shown in Table 14, at a 50% replacement rate, the water holding capacity of the emulsified sausages prepared by the emulsion gel without adding calcium ions and at a calcium ion concentration of 0.1% was not significantly different from that of the control group, and the water holding capacity of the corresponding sausages at a calcium ion concentration of 1.0% was significantly higher than that of the control group. At a 100% replacement rate, the water holding capacity of the sausages prepared by the three calcium ion concentrations was significantly lower than that of the control group. At the same calcium ion concentration, the water holding capacity of the emulsified sausages at a 100% replacement rate was significantly lower than that of the emulsified sausages at a 50% replacement rate. This is because the emulsion gel has a higher strength and stronger water holding capacity when the calcium ion concentration of the 50% replacement group is 1.0%, so the corresponding sausage has a stronger water holding capacity. In addition, the moisture content in the sausage at a 100% replacement rate is higher, so more water is lost under the action of external force. The above results are consistent with the results of cooking loss. In addition, at the same fat replacement rate, the higher the calcium ion concentration, the stronger the water holding capacity of the corresponding emulsified sausage. This is because as the calcium ion concentration increases, the strength of the emulsion gel produced increases and the water holding capacity of the gel is enhanced.

[0242] Chromaticity value determination method:

[0243] The emulsified sausage samples were cut into 20 mm lengths, and the colorimeter was used to measure the chromaticity of the cross-section of the emulsified sausage. The chromaticity value has three indicators: L*, a*, and b*. L* represents the brightness value, a* represents the redness value, and b* represents the yellowness value. Before the color measurement, the instrument was calibrated using a color calibration plate, and then the emulsified sausage cut into sections was tested on the machine. The results are shown in Table 15.

[0244] Table 15 Chromaticity values ​​of emulsified sausage

[0245] sample L* Brightness a*Redness b* yellowness Control group <![CDATA[71.69±0.16 a ]]> <![CDATA[3.53±0.12 a ]]> <![CDATA[13.19±0.19 abc ]]> 50%-0% <![CDATA[73.13±0.01 b ]]> <![CDATA[2.85±0.03 c ]]> <![CDATA[13.09±0.07 ab ]]> 50%-0.1% <![CDATA[74.24±0.04 c ]]> <![CDATA[2.93±0.06 c ]]> <![CDATA[13.23±0.20 abc ]]> 50%-1.0% <![CDATA[75.57±0.11 d ]]> <![CDATA[2.81±0.05 c ]]> <![CDATA[12.96±0.14 a ]]> 100%-0% <![CDATA[76.83±0.01 e ]]> <![CDATA[2.42±0.07 b ]]> <![CDATA[13.33±0.05 abc ]]> 100%-0.1% <![CDATA[77.01±0.03 f ]]> <![CDATA[2.34±0.02 b ]]> <![CDATA[13.50±0.09 bc ]]> 100%-1.0% <![CDATA[76.14±0.07 f ]]> <![CDATA[2.38±0.04 b ]]> <![CDATA[13.57±0.10 c ]]>

[0246] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0247] As shown in Table 15. Emulsified sausage of the control group L * The value was the lowest, which was 71.69. Compared with the control group, with the increase of fat replacement rate, the L * The value is getting higher and higher, indicating that its color is getting whiter and whiter, which may be related to the light reflection produced by the vegetable oil in the emulsion gel, or it may be related to the color difference between the fat and the emulsion gel itself. * Compared with the value of a in the emulsified sausage samples of the fat replacement group * The values ​​of a and b decreased significantly, and with the increase of fat replacement rate, the a of emulsified sausage * The values ​​were reduced. In addition, the b *This is because the fat content in the emulsified sausage of the control group is the highest, and fat oxidation will cause myoglobin in the emulsified sausage to be oxidized into metmyoglobin, causing browning, making the color of the emulsified sausage sample darker, a * As the fat replacement rate increases, the fat content in the emulsified sausage decreases, and the degree of fat oxidation and browning decreases, making the color relatively lighter. * The value decreases.

[0248] pH value determination method:

[0249] The emulsified sausages before and after cooking were cut into small pieces of uniform size, 10 g of the chopped emulsified sausages were weighed and put into a beaker filled with 90 mL of distilled water, and the mixture was blended evenly using a homogenizer. The pH value was then immediately measured. The results are shown in Table 16.

[0250] Table 16 pH value of emulsified sausage

[0251] sample pH value before cooking pH after cooking Control group <![CDATA[6.33±0.02 a ]]> <![CDATA[6.48±0.04 a ]]> 50%-0% <![CDATA[6.28±0.01 a ]]> <![CDATA[6.44±0.02 a ]]> 50%-0.1% <![CDATA[6.30±0.03 a ]]> <![CDATA[6.45±0.03 a ]]> 50%-1.0% <![CDATA[6.30±0.02 a ]]> <![CDATA[6.45±0.03 a ]]> 100%-0% <![CDATA[6.29±0.01 a ]]> <![CDATA[6.43±0.04 a ]]> 100%-0.1% <![CDATA[6.30±0.03 a ]]> <![CDATA[6.45±0.02 a ]]> 100%-1.0% <![CDATA[6.31±0.02 a ]]> <![CDATA[6.44±0.02 a ]]>

[0252] Note: Values ​​with different letters in the same column indicate significant differences (p < 0.05).

[0253] As shown in Table 16, there was no significant difference in the pH of each group of sausages before cooking, and there was no significant difference in the pH of the sausages in the reserve group after cooking, indicating that the use of the emulsion gel as a fat substitute to prepare emulsified sausages would not affect the pH value of the sausages. In addition, the pH value of the emulsified sausages before cooking ranged from 6.28 to 6.33, and the pH value of the emulsified sausages after cooking ranged from 6.43 to 6.48, indicating that the pH value of the emulsified sausages increased slightly after cooking, and the increase in pH caused by cooking was mainly due to protein denaturation and changes in protein charge.

[0254] Determination method of volatile components:

[0255] Weigh 3g of chopped emulsified sausage into a glass bottle, cover the bottle cap, place it in a 45℃ water bath and heat for 10 minutes before testing. The parameters of the electronic nose are set as follows: cleaning time 100s, zeroing time 5s, preparation time 5s, measurement time 120s, air flow 400mL / min. The sensors are: aromatic compounds (W1C), nitrogen oxides (W5S), ammonia aromatics (W3C), hydrides (W6S), short-chain alkanes (W5C), alkanes (W1S), inorganic sulfides (W1W), alcohols and aldehydes (W2S), organic sulfides (W2W), alkanes and fats (W3S). The results are as follows: Fig.14 shown.

[0256] like Fig.14As shown. Only the content of volatile components represented by the W5S (nitrogen oxide) sensor is relatively high, among which the W5S content of the control group sample is the highest, and the W5S content of the sample with a calcium ion concentration of 0% at a 50% replacement rate is second. In comparison, the W5S content of the sample with a calcium ion concentration of 0% at a 100% replacement rate is lower. This is because W5S is mainly produced by fat oxidation. The deeper the oxidation degree, the higher the W5S content. The fat content in the emulsified sausage of the control group is the highest, so its oxidation product W5S content is the highest. The emulsion gel strength of the group without calcium ion addition is low and its stability is poor, so the camellia oil in the emulsion gel is prone to oxidation. Because its fat replacement rate is 50%, there is still 50% unreplaced pig back fat in the emulsified sausage, which makes the total fat content in the sausage sample higher, so its fat oxidation products are more, and the W5S content is relatively higher. In addition, when the calcium ion concentration is 0.1% and 1.0%, the W5S content of each group of emulsified sausages under the two replacement rates is extremely low and almost the same. This is because when the calcium ion concentration is 0.1% and 1.0%, the emulsion gel has strong gel strength and stability, strong water and oil holding capacity, slowing down the oxidation of fat. Because of its strong emulsion gel stability, it has a better emulsification effect when preparing sausage mince, reducing the chance of direct contact between fat in sausage and air, further reducing the oxidation rate. The stronger the emulsion gel, the stronger the oxidation stability of the oil phase.

[0257] TBA value determination method:

[0258] First, a TBA test solution was prepared so that the concentrations of TBA, trichloroacetic acid and hydrochloric acid were 0.375% (w / v), 15% (w / v) and 0.25 mol / L, respectively. Take 25 mL of the test solution, add 5 g of chopped emulsified sausage and mix evenly, then place it in a 100°C heat-collecting water bath for incubation for 10 minutes. After the reaction is completed, cool it to ambient temperature and collect the supernatant by centrifugation at 5000 r / min for 25 minutes. The absorbance of the supernatant was measured at a wavelength of 532 nm using an enzyme marker. The results are expressed as the mass (mg) of malondialdehyde contained in 100 g of emulsified sausage in terms of TBA value, calculated by multiplying the absorbance by 2.77. Each emulsified sausage sample was sampled and tested on the 1st, 3rd, 5th, 7th and 9th days under refrigeration at 4°C, and the results are shown in Table 17.

[0259] Table 17 TBA value of emulsified sausage

[0260]

[0261] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0262] The TBA value represents the content of malondialdehyde, a fat oxidation product. The higher the TBA value, the deeper the fat oxidation degree. The changes in the TBA value of the emulsified sausage during storage are shown in Table 17. Under different storage days, the TBA value of the emulsified sausage in the control group was the highest, indicating that the emulsified sausage in the control group had the highest oxidation degree. This is because the fat content in the emulsified sausage in the control group was the highest, so the oxidation products were the most and the TBA value was the highest. In addition, under the same calcium ion concentration, compared with the emulsified sausage with a 100% replacement rate, the TBA value of the emulsified sausage at a 50% replacement rate was significantly higher, indicating that increasing the fat replacement rate can reduce the degree of fat oxidation in the emulsified sausage. This is because increasing the fat replacement rate reduces the fat content in the sausage sample, so the fat oxidation products are reduced. In addition, during the storage period, as the storage time increases, the TBA values ​​of the emulsified sausages in each group increase accordingly. This is because as the storage time increases, the degree of fat oxidation continues to intensify and the oxidation products continue to increase. In addition, when the calcium ion concentration was 0.1% and 1.0%, there was no significant difference in the TBA value of the emulsified sausages made therefrom. In contrast, the TBA value of the emulsified sausages without calcium ion addition was significantly higher. Moreover, during the entire storage period, the increase in the TBA value of the emulsified sausages in the control group and the group without calcium ion addition was significantly greater than the increase in the TBA value of the emulsified sausages when the calcium ion concentration was 0.1% and 1.0%, indicating that the fat oxidation in these two groups of emulsified sausages was deeper. This is because the total fat content in the control group was the highest, so there were more fat oxidation products, and the emulsion gel in the group without calcium ion addition had lower gel strength and stability, and relatively weak water and oil holding capacity, so the fat in the emulsified sausages made therefrom was more easily oxidized, resulting in an increase in the TBA value. In addition, when the calcium ion concentration was 0.1% and 1.0%, the emulsion gel had stronger gel strength and stability, so the fat in the corresponding emulsified sausages was not easily oxidized. This is consistent with the determination results of volatile substances.

[0263] Method for determination of texture characteristics:

[0264] In the texture test, a double compression cycle was used to simulate the biting and chewing process, and the texture characteristics of the emulsified sausage were determined by a texture analyzer, including changes in hardness, elasticity, cohesion, chewiness and resilience. The emulsified sausage was cut into 10mm high cylinders for test determination. The P / 36R probe and TPA measurement mode were selected. The parameters were set as follows: pre-test downward speed 2.00mm / s, test speed 1.00mm / s, post-test upward speed 1.00mm / s, downward distance 5.00mm, compression times 2 times, interval time 5s, trigger force 5.00g, and the results are shown in Table 18.

[0265] Table 18 Texture characteristics of emulsified sausage

[0266]

[0267] Note: Values ​​with different letters in the same column indicate significant differences (p<0.05).

[0268] As shown in Table 18. There was no significant difference in elasticity, cohesion and recovery among the emulsified sausages of each group. In addition, the hardness and chewiness of the control group sausages were the highest among the emulsified sausages of each group, and the hardness and chewiness of the emulsified sausages of the group without calcium ion addition at a replacement rate of 100% were the lowest. Compared with the control group sausages, at a replacement rate of 50%, the hardness and chewiness of the emulsified sausages were not significantly different when the calcium ion concentration was 1.0%, and the hardness and chewiness of the emulsified sausages were slightly lower than those of the control group when the calcium ion concentration was 0.1%, indicating that the two groups of emulsified sausages had similar texture characteristics to those of the control group sausages. In addition, at the same calcium ion concentration, as the fat replacement rate increased, the hardness and chewiness of the emulsified sausages decreased. This is because the water content in the emulsion gel is high. Therefore, as the fat replacement rate increased, the water content in the emulsified sausage increased, which produced a dilution effect on the minced meat system, resulting in a decrease in the hardness and chewiness of the emulsified sausages. In addition, under the same fat replacement rate conditions, with the increase of calcium ion concentration, the hardness and chewiness of the emulsified sausage increased. This is because with the increase of calcium ion concentration, the corresponding emulsion gel has stronger gel strength, water retention and stability, and reduces the dilution effect of water on the minced meat system.

[0269] In summary, in the present invention, after the raw oat milk is heated (heated in a water bath at 90°C for 30 minutes), the hydrophobicity is reduced, the starch granules are transformed into amorphous starch, the particle size is significantly reduced, and the content of the α-helical structure of the oat protein is reduced, and the β-folding content is increased. Compared with the unbaked group, the oat milk prepared from the oat grains after baking (120°C, baking for 0.5min, 1.0min, 1.5min and 2.0min) has a trend of first increasing and then decreasing with the increase of baking time, which is basically consistent with the trend of its protein content first increasing and then decreasing, and the particle size increases accordingly, and the α-helical content of the oat protein is further reduced, and the β-folding content is further increased. On the basis of the heating treatment and baking treatment, after the oat milk is backfilled with filter residue, compared with the group without the filter residue backfilling treatment, its solid content increases, the hydrophobicity decreases slightly, the protein purity decreases slightly, and the oat milk particle size increases.

[0270] The emulsion of the oat milk group treated with heating showed significant improvements in terms of creaming, particle size and stability. In addition, the oat milk obtained by baking the oat seeds further improved its emulsification effect and the quality of the emulsion. With the increase of baking time, the creaming index first decreased and then increased. Among them, the emulsification effect of the oat milk was the best when the baking time was 1.0 min. In addition, the emulsion prepared by the oat milk in the backfill residue treatment group did not cream, and the droplet size was the smallest, with the best emulsification effect.

[0271] Compared with the one-step dispersion method, the two-step dispersion method has a better emulsification effect, but there is no significant difference in rheological properties. As the agar concentration increases, the droplet size gradually increases, and the modulus of the emulsion gel also increases. Among them, a stable emulsion gel structure cannot be formed when agar is not added. As the sodium alginate concentration increases, the droplet size shows a trend of first decreasing and then increasing, and the modulus of the emulsion gel decreases accordingly. In addition, as the volume fraction of the oil phase increases, the droplet size gradually increases, and the rheological properties do not change significantly. After adding calcium ions, the modulus of the emulsion gel increases significantly, and it has strong support. As the calcium ion concentration increases, the modulus increases accordingly. The appearance of the emulsion gel does not change significantly, and when the temperature reaches above 70°C, the modulus does not change much, indicating that the emulsion gel has good thermal stability. When the temperature of the emulsion gel without adding calcium ions rises to 70°C~85°C, the hydrogen bonds between the agarose chains break, the gel system is destroyed, and the modulus decreases rapidly.

[0272] When the emulsion gel was used as a fat substitute in emulsified sausage, at a 50% replacement rate, the emulsion gel with a calcium ion concentration of 0.1% and 1.0% had a better replacement effect. When the fat replacement rate was further increased, the quality of the emulsified sausage decreased. In addition, compared with the control group, the emulsified sausage prepared by replacing pig back fat with the emulsion gel reduced the fat oxidation rate of the product.

[0273] Although the above embodiment describes the present invention in detail, it is only a part of the embodiments of the present invention, not all of the embodiments. People can also obtain other embodiments based on this embodiment without creativity, and these embodiments all fall within the protection scope of the present invention.

Claims

1. A method for preparing oat milk, characterized in that: The steps include: The roasted oatmeal grains are mixed with water and then beaten to obtain a crude oatmeal liquid; filtering the crude oatmeal liquid to obtain a filtrate and a filter residue; The filtrate is centrifuged, and the supernatant and the colloid layer on the surface of the precipitate are taken respectively; mixing the gelatin layer and the supernatant to obtain raw oat milk; The raw oat milk is subjected to a heating treatment to obtain cooked oat milk; The cooked oat milk is filtered to obtain the oat milk.

2. The preparation method according to claim 1, characterized in that The method for obtaining the baked oat grains comprises: placing the oat grains in a baking device and baking them at 100-140° C. for 0.5-1.5 min; the material-liquid ratio of the baked oat grains to water is 1 g: 5-10 mL; and the beating time is 1-2 min.

3. The preparation method according to claim 1, characterized in that: The filtration is performed using a filter device with a pore size of 100-300 meshes.

4. The preparation method according to claim 1, characterized in that: The step of mixing the gelatinous layer and the supernatant also includes the step of mixing the gelatinous layer, the supernatant and the filter residue to obtain raw oat milk.

5. An oat milk, characterized in that: The method is prepared by the method according to any one of claims 1 to 4.

6. Use of the oat milk according to claim 5 in the preparation of oat milk emulsion or oat milk emulsion gel.

7. An oatmeal emulsion, characterized in that: The following preparation method is used to obtain: The oat milk and the oil phase are mixed and sheared at a speed of 10,000 to 25,000 r / min for 1 to 2 minutes using a high-speed shearing device to obtain an oat milk emulsion; the oat milk is the oat milk according to claim 5.

8. The oat milk emulsion according to claim 7, characterized in that The volume ratio of the oat milk to the oil phase is 3-7:3-7, and the oil phase is vegetable edible oil.

9. An oatmeal milk emulsion gel, characterized in that: The following preparation method is used to obtain: Agar, sodium alginate and water are mixed in proportion and heated to obtain a polysaccharide solution; the mass concentration of agar in the polysaccharide solution is 2.0%, and the mass concentration of sodium alginate is 2.0%; The polysaccharide solution and oat milk emulsion are mixed in a volume ratio of 1:2, and sheared at a speed of 10000-25000 r / min for 1-2 min using a high-speed shearing device to obtain an oat milk emulsion gel; adding or not adding a calcium chloride solution to the oat milk emulsion gel so that the calcium ion concentration in the oat milk emulsion gel is 0 to 1.3%; The oat milk emulsion is the oat milk emulsion according to claim 7 or 8.

10. Use of the oat milk according to claim 5, the oat milk emulsion according to claim 7 or the oat milk emulsion gel according to claim 9 in food processing containing oil raw materials.