Method for enhancing bipolar membrane electrodialysis process through temperature difference
By establishing a temperature difference on both sides of the bipolar membrane and using the temperature difference to act on the bipolar membrane, the efficiency of the bipolar membrane electrodialysis process and acid and alkali concentration are improved, and the energy consumption and efficiency in the existing concentrated seawater treatment technology are solved. Low problems achieve more efficient seawater desalination and high-salt wastewater treatment.
Patent Information
- Application Number
- CN202411190747.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-08-28
AI Technical Summary
Existing concentrated seawater treatment technologies such as evaporation crystallization and membrane distillation have high investment in equipment, high energy consumption and low efficiency, and bipolar membrane electrodialysis has limited efficiency under the influence of temperature, making it difficult to achieve large-scale industrial applications.
By establishing a temperature difference on both sides of the bipolar membrane, the ion migration speed is accelerated, and a bipolar membrane electrodialysis device with a three- compartment structure is adopted to control the acid-base solution to remain stable at different temperatures, and the temperature difference is used to act on the bipolar membrane to improve hydrolysis Removal rate and current density to reduce energy consumption.
It significantly improves acid production, alkali concentration and current efficiency, reduces energy consumption, improves the efficiency and economy of the bipolar membrane electrodialysis process, and provides new practical ideas for seawater desalination and high-salt wastewater treatment.
Smart Images

Figure CN118904082A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of bipolar membrane electrodialysis, and specifically relates to accelerating ion migration speed, increasing water dissociation rate in the bipolar membrane, increasing acid and alkali concentration, increasing current density, and reducing energy consumption by establishing a temperature difference on both sides of the bipolar membrane. Background Art
[0003] Evaporation and crystallization are often used to treat and concentrate concentrated seawater, but there are problems such as high equipment investment and energy consumption, and low efficiency. Membrane distillation is also based on heat-driven evaporation. The draw liquid required for forward osmosis usually comes from the hot regeneration liquid. Limited by thermodynamic limits, it has not yet been applied in large-scale industry. Bipolar Membrane ElectroDialysis (BMED) is based on electrodialysis ED. It electrolyzes water molecules through the bipolar membrane intermediate layer, and simultaneously achieves high-salt wastewater desalination and acid and alkali preparation, without the need to add chemical agents and almost no by-products.
[0004] Many domestic and foreign scholars have used BMED to study the treatment of seawater desalination brine and other types of high-salt wastewater. The results show that BMED has great potential for (near) zero emissions in actual production processes. In the bipolar membrane electrodialysis process, the influence of temperature is the most significant. This invention explores the mass transfer mechanism under the coupling of temperature field and electric field in the bipolar membrane process, better strengthens the bipolar membrane electrodialysis process, helps to reduce energy consumption, increase current density, and improve the quality of the produced acid and alkali. Summary of the invention
[0005] The present invention aims to explore the influence of temperature difference on the bipolar membrane electrodialysis process. By controlling the acid and alkali solutions to remain stable at different temperatures, the temperature difference is allowed to act on the bipolar membrane, and the changes in the bipolar membrane electrodialysis process under the condition of temperature difference are explored. The process is comprehensively evaluated by combining key indicators such as acid and alkali concentration, salt chamber conductivity change, current efficiency, and energy consumption. This can better strengthen the bipolar membrane electrodialysis technology, reduce energy consumption, increase current density, improve the quality of the produced acid and alkali, improve its efficiency and economy, and provide new practical ideas for research and application in related fields.
[0006] The technical solution of the present invention is:
[0007] 1. A method for temperature-difference-enhanced bipolar membrane electrodialysis process, characterized in that a three-compartment structure bipolar membrane electrodialysis device is used, wherein the membrane stack of the bipolar membrane electrodialysis device is arranged in the order of cation exchange membrane-bipolar membrane-anion exchange membrane, and the adjacent membranes are separated by partitions to form an acid chamber, a salt chamber and an alkali chamber, and the bipolar membranes on both sides of the electrode plate and the membrane stack form two polar liquid chambers; each compartment is connected to a corresponding container through a pump; a temperature difference is established on both sides of the bipolar membrane to accelerate the ion migration speed, increase the water dissociation rate in the bipolar membrane, increase the acid and alkali concentrations, improve the current efficiency, and reduce energy consumption;
[0008] The steps of the temperature difference enhanced bipolar membrane electrodialysis process are as follows:
[0009] (1) introducing four liquid solutions, namely, acid solution, alkaline solution, saline solution and polar solution, into four chambers of a bipolar membrane electrodialysis device, and heating the alkaline chamber solution to establish a temperature difference on both sides of the bipolar membrane;
[0010] (2) turning on the peristaltic pump to set the flow rate value, turning on the DC power supply, setting the target voltage, and running the bipolar membrane electrodialysis device;
[0011] (3) During the process, the voltage of the membrane stack, the voltage and current of the power supply, and the temperatures of the acid, base, and salt are recorded, and samples are taken on time to perform acid-base titration or conductivity and pH measurements, and calculate current efficiency and energy consumption;
[0012] (4) When the current drops below 0.6 A under constant voltage operation conditions, stop the experiment and turn off the DC power supply.
[0013] The method for temperature difference enhancement of bipolar membrane electrodialysis process is characterized in that the NaCl solution in the salt chamber is 50g / L to 70g / L, and the initial acid and alkali concentrations are 0.05mol / L.
[0014] The method for temperature difference enhancement of bipolar membrane electrodialysis process is characterized in that the membrane surface flow rate is 4 to 8 cm / s.
[0015] The method for enhancing the bipolar membrane electrodialysis process by temperature difference is characterized in that the temperature difference is 0, 5, 10 and 15°C.
[0016] The method for temperature difference enhancement of bipolar membrane electrodialysis process is characterized in that the temperature difference on both sides of the membrane can also be obtained by heating the acid chamber solution.
[0017] Beneficial effects of the present invention:
[0018] The present invention controls the acid and alkali solutions to remain stable at different temperatures, allows the temperature difference to act on the bipolar membrane, accelerates the ion migration speed, increases the water dissociation rate in the bipolar membrane, increases the acid and alkali concentrations, improves the current efficiency, and reduces energy consumption, and has very good application prospects. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 Schematic diagram of temperature difference enhanced bipolar membrane electrodialysis;
[0020] Figure 2 The change of conductivity with time under temperature difference conditions at a salinity of 50 g / L;
[0021] Figure 3 The change of acid concentration in the acid chamber with salinity of 50g / L over time under temperature difference conditions;
[0022] Figure 4 Changes of alkali concentration in the alkali room with salinity of 50 g / L over time under temperature difference conditions;
[0023] Figure 5 The change of current efficiency with time under temperature difference conditions at a salinity of 50 g / L;
[0024] Figure 6 Energy consumption with salinity of 50 g / LL changes with time under temperature difference conditions;
[0025] Figure 7 The change of conductivity with time under temperature difference conditions at a salinity of 70 g / L;
[0026] Figure 8 Changes of acid concentration in the acid chamber with salinity of 70 g / L over time under temperature difference conditions;
[0027] Fig. 9 Changes of alkali concentration in the alkali room with salinity of 70 g / LL over time under temperature difference conditions;
[0028] Fig.10 The change of current efficiency with time under temperature difference conditions at salinity of 70g / LL;
[0029] Fig.11 Energy consumption at salinity of 70 g / L changes with time under temperature difference conditions;
[0030] Fig.12 Comparison of conductivity changes in alkaline and acid chambers with increasing temperature;
[0031] Fig.13 Comparison of changes in acid and alkali concentrations when the temperature in the alkali and acid chambers increases;
[0032] Fig.14 Comparison of the change in heating current efficiency between the alkaline chamber and the acid chamber;
[0033] Fig.15 Comparison of heating energy consumption changes between alkali chamber and acid chamber; DETAILED DESCRIPTION
[0034] The present invention will be further described below in conjunction with the accompanying drawings:
[0035] Example 1
[0036] The concentrations are: NaCl solution 50g / L, HCl solution 0.05mol / L in the acid chamber, NaOH solution 0.05mol / L in the alkali chamber, and Na 2 SO 4 The BMED experiment was carried out under constant current conditions, and the current density was set to 35 mA / cm 2 ,like Figure 1 As shown, the temperature of the salt chamber and the acid chamber is 20°C, the solution in the alkali chamber is increased to 20, 25, 30, and 35°C, the temperature difference acts on the bipolar membrane, and the conductivity of the salt chamber changes with time. Figure 2 As shown in the figure, the conductivity dropped from 62ms / cm at the initial moment to 8ms / cm. The lowest conductivity reached 4.4ms / cm at a temperature difference of 5℃, followed by 7.3ms / cm at a temperature difference of 10℃. The conductivity at the temperature difference of 5, 10, and 15℃ was lower than that at the isothermal condition at the same time. The conductivity dropped significantly at a temperature difference of 10℃, which was 6.84ms / cm lower than that at the isothermal condition, with an average reduction rate of about 18.84%.
[0037] like Figure 3 and Figure 4 As shown, the initial acid and alkali concentrations of the experiment were 0.05 mol / L, and the acid concentrations obtained under the temperature difference of 0, 5, 10, and 15 ° C were 0.64, 0.66, 0.65, and 0.69 mol / L, and the alkali concentrations obtained were 0.56, 0.57, 0.58, and 0.61 mol / L. The existence of the temperature difference slightly increased the final acid and alkali concentrations. The average acid concentration was 14% higher than that during isothermal operation, and the alkali concentration was about 4% higher than that during isothermal operation. Increasing the temperature of the alkali chamber is more conducive to increasing the acid production concentration. With the increase of feed salinity, the acid and alkali concentrations also increase accordingly. Due to the increase in the temperature of the alkali chamber, the leakage of OH- in the alkali chamber to the salt chamber is accelerated. Therefore, the final concentration of the alkali solution is lower than the acid solution concentration.
[0038] like Figure 5As shown in the figure, when the temperature difference is 5℃, the average current efficiency can be increased by 3.7% compared with the isothermal condition, and when the temperature difference is 15℃, it can also be increased by about 1.3%. The appropriate temperature difference can improve the current efficiency. The default current efficiency is 0 at time 0. Under the action of the external electric field, the ions in the solution migrate across the membrane in a directional manner. At the same time, a concentration gradient is formed on the membrane surface under the action of the electric field. The speed at which ions approach the membrane layer is significantly faster than the speed at which ions leave the membrane layer, and the current efficiency also increases accordingly. As the ions in the salt chamber migrate to both sides, the ion concentration in the salt chamber gradually decreases, and the current efficiency gradually decreases after reaching the maximum. On the one hand, the increase in salt chamber concentration increases the conductivity accordingly. Within a certain range, the current density is proportional to the electrical bandwidth (the potential difference between the two ends of the bipolar membrane). When the initial concentration of the salt chamber increases, the resistivity of the solution decreases, so the increase in current density is conducive to the improvement of current efficiency.
[0039] Energy consumption is calculated per kg of acid. Figure 6 At a medium salinity of 50 g / L, the energy consumption under the temperature difference of 10 and 15 °C was reduced by 9.5% and 4.8% respectively compared with the isothermal condition. Similar to the current efficiency, when the temperature of the alkali chamber is increased, the viscosity of the solution decreases, the ion transmission resistance is reduced, and the increase in the degree of ion thermal motion is conducive to promoting transmembrane migration, thereby reducing the process energy consumption. The energy consumption remains relatively stable from 40 to 120 minutes. This is because the membrane stack voltage also remains stable during this period, and the energy consumption is relatively stable under constant current conditions. The ion concentration in the salt chamber decreases, and the energy consumption gradually increases after 120 minutes. At 200 minutes, the conductivity of the salt chamber has dropped to 10ms / cm. If the energy consumption in this interval is ignored, the integral area under the energy consumption curve under the temperature difference of 15 °C from 0 to 160 minutes is 628.8, and the corresponding integral area during isothermal operation is 729.9, and the energy consumption is reduced by about 13.85%.
[0040] Example 2
[0041] The concentrations are: NaCl solution 70g / L, HCl solution 0.05mol / L in the acid chamber, NaOH solution 0.05mol / L in the alkali chamber, and Na 2 SO 4 The BMED experiment was carried out under constant current conditions, and the current density was set to 35 mA / cm 2 The temperature of the salt chamber and the acid chamber is 20℃, the solution in the alkali chamber is increased to 20, 25, 30, and 35℃, the temperature difference is applied to the bipolar membrane, and the conductivity of the salt chamber is measured to change with time. Figure 7As shown in the figure, at a salinity of 70 g / L, it takes 340 min under isothermal conditions to reduce the conductivity of the salt chamber to below 10 ms / cm, while it takes 300 min under a temperature difference of 5°C and 10°C, and 320 min under a temperature difference of 15°C. Under the temperature difference conditions, the conductivity changes in the first 160 min are almost the same. After 160 min, the conductivity is slightly higher than the temperature difference of 5 and 10°C when the temperature difference is 15°C, but still lower than the conductivity of isothermal operation. The temperature difference is beneficial to the desalination effect of the bipolar membrane electrodialysis process. The increase in temperature can increase the diffusion rate of solutes in water, reduce the viscosity of water, and improve the desalination efficiency. However, the heat transfer at too high a temperature has an inhibitory effect on the migration of cations, especially when treating brine with higher concentrations.
[0042] Figure 8 and Fig. 9 It can be seen that when the salt concentration is 70g / L, the acid concentration increases most significantly under the temperature difference of 15℃, and the maximum concentration is about 13.1% higher than that under isothermal operation, and the alkali concentration is about 3.8% higher than that under isothermal operation. The initial acid and alkali concentrations of the experiment were 0.05mol / L. The acid concentrations were 0.84, 0.85, 0.86, and 0.95mol / L under the temperature difference of 0, 5, 10, and 15℃, respectively, and the alkali concentrations were 0.79, 0.8, 0.81, and 0.82mol / L, respectively. The existence of temperature difference increased the final acid and alkali concentrations of the process. Among them, the acid and alkali concentrations increased most significantly under the temperature difference of 15℃, with the highest acid concentration exceeding the isothermal by 13.1%, and the highest alkali concentration exceeding the isothermal by 3.8%. The effect of temperature difference on the increase of acid concentration is higher than that of alkali concentration.
[0043] The current efficiency curve measured at 70 g / L salinity is similar to that at 50 g / L salinity, e.g. Fig.10 As shown in the figure, the temperature difference of 15℃ has the most obvious effect on improving the current efficiency, with the maximum point increasing by 83.2% compared with the isothermal condition, followed by the temperature difference of 10℃, with the maximum point increasing by 48.3% compared with the isothermal condition, and the average current efficiency under the temperature difference of 5℃ is also slightly higher than that under the isothermal condition. During the experiment, the current efficiency was improved under the influence of the temperature difference. When the temperature difference was 15℃, the average efficiency was increased by about 17% compared with the isothermal condition, followed by the temperature difference of 10℃, with the average efficiency increased by 5.4%.
[0044] The energy consumption measured at 70g / L salinity changes with time as shown in Fig.11 As shown, from 0 to 350 minutes, compared with isothermal conditions, the average energy consumption of temperature differences of 5°C, 10°C, and 15°C decreased by approximately 6.1%, 14.6%, and 26.8%, respectively. The effect of temperature difference on energy consumption is related to the effect on current efficiency. As current efficiency increases, energy consumption decreases accordingly.
[0045] The effect of the temperature rise of the acid chamber and the base chamber on the bipolar membrane electrodialysis process was investigated. Fig.12 , Fig.13 , Fig.14and Fig.15 As shown, when the temperature of the acid chamber or the base chamber is increased by 5°C, the change patterns of the salt chamber conductivity, acid-base concentration, current efficiency and energy consumption are almost the same. Therefore, there is no significant difference in the effect of maintaining the same temperature difference on the left or right side of the bipolar membrane.
[0046] The examples of the invention have been specifically described above, but the invention is not limited to the examples. Those skilled in the art may make various equivalent modifications or substitutions without violating the spirit of the invention, and these equivalent modifications or substitutions are all included in the scope defined by the claims of this application.
[0047] Matters not covered by the present invention are known technologies.
Claims
1. A method for temperature-difference-enhanced bipolar membrane electrodialysis process, characterized in that: A three-compartment structure bipolar membrane electrodialysis device is used, wherein the membrane stack of the bipolar membrane electrodialysis device is arranged in the order of cation exchange membrane-bipolar membrane-anion exchange membrane, and adjacent membranes are separated by partitions to form an acid chamber, a salt chamber and an alkali chamber, and the electrode plates and the bipolar membranes on both sides of the membrane stack form two polar liquid chambers; each compartment is connected to a corresponding container through a pump; a temperature difference is established on both sides of the bipolar membrane to accelerate the ion migration speed, increase the water dissociation rate in the bipolar membrane, increase the acid and alkali concentrations, improve the current efficiency, and reduce energy consumption; The steps of the temperature difference enhanced bipolar membrane electrodialysis process are as follows: (1) introducing four liquid solutions, namely, acid solution, alkaline solution, saline solution and polar solution, into four chambers of a bipolar membrane electrodialysis device, and heating the alkaline chamber solution to establish a temperature difference on both sides of the bipolar membrane; (2) turning on the peristaltic pump to set the flow rate value, turning on the DC power supply, setting the target voltage, and running the bipolar membrane electrodialysis device; (3) During the process, the voltage of the membrane stack, the voltage and current of the power supply, and the temperatures of the acid, base, and salt are recorded, and samples are taken on time to perform acid-base titration or conductivity and pH measurements, and calculate current efficiency and energy consumption; (4) When the current drops below 0.6 A under constant voltage operation conditions, stop the experiment and turn off the DC power supply.
2. The method for temperature-difference-enhanced bipolar membrane electrodialysis process according to claim 1, characterized in that: The NaCl solution in the salt chamber is 50 g / L to 70 g / L, and the initial acid and alkali concentrations are 0.05 mol / L.
3. The method for temperature-difference-enhanced bipolar membrane electrodialysis process according to claim 1, characterized in that: The flow rate on the membrane surface is 4 to 8 cm / s.
4. The method for temperature-difference-enhanced bipolar membrane electrodialysis process according to claim 1, characterized in that: The temperature differences were 0, 5, 10 and 15°C.
5. The method for temperature-difference-enhanced bipolar membrane electrodialysis process according to claim 1, characterized in that: The temperature difference between the two sides of the membrane can also be obtained by heating the acid chamber solution.
Citation Information
Patent Citations
Technique for preparing hypophosphorous acid through bipolar membrane electroosmosis method
CN105688676A
Bipolar membrane electrodialysis method for preparing hypophosphorous acid from sodium hypophosphite
CN108636123A
Bipolar membrane electrodialysis system, and method for preparing lithium hydroxide by using same
CN109772169A
Three-compartment bipolar membrane electrodialysis of salts of amino acids
CN112469494A
Ammonium adipate waste liquid recovery method and device based on high-temperature bipolar membrane electrodialysis
CN113274882A