Surface treatment method of table body structure

By forming a protective film on the surface of the table body structure and attaching natural wood veneer, combined with paint treatment, the problems of foaming of the decorative surface layer and rusting of steel in the prior art are solved, and the appearance and reliability of the table body structure are improved.

CN118904691APending Publication Date: 2024-11-08GUANGZHOU ZHISHENG GUANMEI FURNITURE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410982184.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-22
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing table structure is prone to foaming of decorative surfaces and rusting of steel after long-term use, which affects the reliability of use.

Method used

A protective film is formed on the surface of the table body structure by hot melting, a viscose layer is sprayed, and natural wood veneer is attached to the viscose layer, and a solid wood decorative layer is formed by drying and painting.

Benefits of technology

It improves the appearance ornamentality of the table structure and packaging reliability, prevents the decorative layer from foaming and rusting of steel, and extends the service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118904691A_ABST
    Figure CN118904691A_ABST
Patent Text Reader

Abstract

The invention discloses a table body structure surface treatment method which comprises the steps that the surface of a table body structure is pretreated, and a protective film is formed on the surface of the table body structure based on a hot melting technology; coating the protective film on the surface of the table body structure based on spraying equipment to form an adhesive layer; a wood skin layer is attached to the adhesive layer, and a wood decoration layer is formed on the surface of the table body structure through airing for preset time; and paint treatment is conducted on the wood decoration layer, and packaging treatment is conducted on the wood decoration layer based on paint. The natural leather layer is attached to the surface of the table body structure of the steel structure, and paint treatment is matched, so that the table body structure has good appearance ornamental value, and meanwhile, the packaging reliability of the decorative layer attached to the surface of the table body structure is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of furniture technology, and in particular to a surface treatment method for a table structure. Background Art

[0002] At present, desks, dressing tables, office desks and other table structures are processed with steel materials to improve the structural rigidity of the table body. In order to improve the appearance of the table body structure, the existing table body structure improves the appearance of the table body structure by attaching a decorative layer on the surface.

[0003] The current decorative layer is attached by adhesive, which is prone to foaming of the decorative surface layer and rusting of the steel structure after long-term use, affecting the reliability of the table structure. Summary of the invention

[0004] The purpose of the present invention is to overcome the shortcomings of the prior art. The present invention provides a surface treatment method for a table structure. By attaching a natural leather layer to the surface of a table structure made of a steel structure and combining it with paint treatment, the table structure has a good appearance and the packaging reliability of the decorative layer attached to the surface of the table structure is improved.

[0005] The present invention provides a surface treatment method for a table structure, the treatment method comprising:

[0006] Pre-treating the surface of the table structure, and forming a protective film on the surface of the table structure based on a hot melt process;

[0007] Using a spraying device to coat the protective film on the surface of the table structure to form an adhesive layer;

[0008] Attaching the wood cortex layer to the adhesive layer, and drying it in the sun for a preset time to form a wood decorative layer on the surface of the table structure;

[0009] The wooden decorative layer is subjected to a paint treatment, and the wooden decorative layer is subjected to a packaging treatment based on the paint.

[0010] Furthermore, the pre-treatment of the surface of the table structure to form a protective film on the surface of the table structure based on a hot melt process includes:

[0011] The table structure is polished and cleaned, and the surface of the cleaned table structure is air-dried based on the air supply mechanism, so that the surface of the table structure remains dry.

[0012] Furthermore, the pre-treatment of the surface of the table structure and the formation of a protective film on the surface of the table structure based on a hot melt process further include:

[0013] The plastic powder is charged by an electrostatic generator, and the treated plastic powder is attached to the surface of the table structure;

[0014] The plastic powder is melted by baking equipment so that the plastic powder is completely melted on the surface of the table structure to form a protective film on the surface of the table structure.

[0015] Furthermore, the step of performing a melting process on the plastic powder based on the baking equipment so that the plastic powder is completely melted on the surface of the table structure and a protective film is formed on the surface of the table structure comprises:

[0016] Placing the table structure with plastic powder in a baking device, and continuously baking the table structure within a preset baking temperature;

[0017] Among them, the baking time range is set to 12min~18min, and the baking temperature range is set to 180℃~220℃.

[0018] Furthermore, the method of coating the protective film on the surface of the table structure with a spraying device to form an adhesive layer includes:

[0019] The table structure is placed in the working space of the spraying equipment, and the spraying operation of the spraying equipment is adjusted according to the posture state of the table structure.

[0020] Further, adjusting the spraying operation of the spraying equipment according to the posture state of the table structure includes:

[0021] The spraying equipment is set to spray over a large area, and the spraying direction of the spraying equipment is set in combination with the placement position of the table structure, so that the nozzle of the spraying equipment sprays each surface of the table structure in turn;

[0022] Or the spraying equipment is set to spray in a small range, and the running path of the spraying equipment is set in combination with the shape and size of the table structure, and the spraying equipment is driven to spray the table structure along the running path.

[0023] Furthermore, the step of attaching the natural veneer to the adhesive layer and drying it for a preset time to form a wooden decorative layer on the surface of the table structure includes:

[0024] After spraying the adhesive layer on the surface of the table structure by the spraying equipment, attaching the natural veneer to the adhesive layer within a preset time interval;

[0025] The preset time interval is 40s to 60s.

[0026] Furthermore, the step of attaching the natural veneer to the adhesive layer and drying it for a preset time to form a wooden decorative layer on the surface of the table structure also includes:

[0027] The table structure is placed in a preset attachment operation space, and the environmental parameters of the table structure during natural veneer attachment are adjusted.

[0028] Furthermore, the environmental parameters are:

[0029] 15℃≤T≤35℃;

[0030] 50%≤H≤80%;

[0031] Wherein, T is the ambient temperature, and H is the ambient humidity.

[0032] Furthermore, the painting of the wooden decorative layer and the encapsulation of the wooden decorative layer based on the paint include:

[0033] The wooden decorative layer is subjected to an open paint treatment, or the wooden decorative layer is subjected to a semi-open paint treatment, or the wooden decorative layer is subjected to a closed paint treatment.

[0034] The present invention provides a surface treatment method for a table structure, by performing surface treatment on the table structure, natural veneer is attached to the surface of the table structure, so that the table structure has good appearance and ornamental properties. By setting paint sealing, the reliability of plastic sealing of the table structure is improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0036] Figure 1 is a flow chart of a surface treatment method of a table structure according to an embodiment of the present invention;

[0037] Figure 2 It is a flow chart of the table structure protective film processing method in an embodiment of the present invention. DETAILED DESCRIPTION

[0038] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0039] Figure 1A flow chart of a surface treatment method for a table structure in an embodiment of the present invention is shown, and the treatment method includes:

[0040] S11: Pre-treating the surface of the table structure and forming a protective film on the surface of the table structure based on a hot melt process.

[0041] Specifically, the table structure is a steel frame structure with good structural rigidity, which can meet the requirements of desk use. The pretreatment of the surface of the table structure includes:

[0042] The table structure is polished and cleaned, and the surface of the cleaned table structure is air-dried based on the air supply mechanism, so that the surface of the table structure remains dry. The burrs on the surface of the table structure are cleaned by polishing, so that the surface of the table structure can remain smooth for subsequent surface treatment processes.

[0043] Specifically, Figure 2 The flowchart of the table structure protective film processing method in the embodiment of the present invention is shown. The hot-melt process is used to form a protective film on the surface of the table structure, which includes:

[0044] S111: The plastic powder is charged by an electrostatic generator, and the treated plastic powder is attached to the surface of the table structure:.

[0045] The plastic powder is charged by an electrostatic generator, and the plastic powder is placed on a metal tray within the working range of the electrostatic generator. The plastic powder is discharged through the discharge needle of the electrostatic generator. Based on the metal tray, the charge released by the discharge needle of the electrostatic generator forms a closed loop with the high-voltage side of the electrostatic generator, so that the charge in the closed loop can adhere to the plastic powder, making the plastic powder charged.

[0046] Furthermore, the plastic powder is evenly covered on the metal tray, so that the plastic powder can completely cover the metal tray, so that the plastic powder can be blocked between the metal tray and the discharge needle, avoiding the discharge needle of the electrostatic generator to directly discharge high voltage toward the metal tray, so that the plastic powder can evenly attach charges, meeting the charging treatment requirements of the plastic powder.

[0047] S112: performing a melting process on the plastic powder using a baking device, so that the plastic powder is completely melted on the surface of the table structure, and a protective film is formed on the surface of the table structure.

[0048] Specifically, plastic powder with an electric charge is attached to the surface of the table structure so that the surface of the table structure can be evenly covered with the plastic powder. The table structure with the plastic powder is placed in a baking device, and the baking temperature is set between 180°C and 220°C. The table structure is continuously baked within the preset baking temperature, and the baking time is between 12 minutes and 18 minutes. In this embodiment, the baking time of the baking device is set to 15 minutes to meet the melting requirements of the plastic powder.

[0049] Furthermore, the plastic powder is melted based on the baking equipment, so that the plastic powder is completely melted on the surface of the table structure, thereby forming a protective film on the surface of the table structure.

[0050] Specifically, the plastic powder may be epoxy resin powder or polyurethane powder, which has good chemical corrosion resistance and wear resistance, and can meet the requirements of plastic sealing protection of the surface of the table structure. The plastic powder may also be polyester powder, which has good weather resistance and light resistance, and can reduce the wear of the surface of the table structure by the external environment. The plastic powder may also be polypropylene powder, which has good electrical insulation performance and low-temperature toughness, and can insulate and protect the table structure, reducing the impact of electrochemical corrosion on the table structure.

[0051] Furthermore, the plastic powder may be polyolefin powder or acrylic powder, which has good corrosion resistance and weather resistance to meet the plastic sealing protection requirements of the table structure.

[0052] S12: Using a spraying device to apply a coating on the protective film on the surface of the table structure to form an adhesive layer.

[0053] The table structure is placed in the working space of the spraying equipment, and the spraying operation of the spraying equipment is adjusted according to the posture state of the table structure.

[0054] Glue is sprayed onto the protective film on the surface of the table structure by a spraying device, and the spraying device is provided with an arc-shaped nozzle. Based on the arc-shaped nozzle, a large range of spraying can be performed on the table structure, so that the spraying device can spray and cover multiple parts of the surface of the table structure at the same time, thereby improving the spraying efficiency.

[0055] Specifically, the table structure is placed in the working area of ​​the spraying equipment, and the spraying direction of the spraying equipment is set according to the spraying range of the spraying equipment and the placement position of the table structure, so that the nozzle of the spraying equipment can spray each surface of the table structure in turn, thereby meeting the spraying processing requirements of the surface of the table structure.

[0056] Furthermore, a plurality of spraying directions are set based on the spraying range of the spraying equipment to reduce the intersection between the spraying directions, so that the spraying equipment can evenly spray the table structure, so that the surface of the table structure can be evenly covered with glue, thereby forming an adhesive layer on the surface of the table structure.

[0057] Specifically, the spraying equipment can be set to spray in a small range. Based on the spraying range of the spraying equipment and the shape and size of the table structure, the operation path of the spraying equipment is set, so that the spraying equipment can spray the table structure along the operation path, so that the spraying equipment can evenly spray the surface of the table structure to meet the uniform coating of the surface of the table structure.

[0058] Furthermore, by controlling the spray range of the spray equipment, the spray range of the spray equipment can cover the surface of the table structure to evenly coat the glue. Based on a preset running path, the nozzle of the spray equipment is driven to move on the surface of the table structure, thereby achieving a uniform spraying operation on the surface of the table structure.

[0059] Furthermore, the spraying equipment is set to apply 100g / m 2 ~150g / m 2 , so that the thickness of the adhesive layer on the surface of the table structure can meet the bonding processing requirements.

[0060] S13: attaching natural veneer to the adhesive layer, and drying it in the sun for a preset time to form a wooden decorative layer on the surface of the table structure.

[0061] Specifically, after the adhesive layer is sprayed on the surface of the table structure by the spraying equipment, the natural veneer is attached to the adhesive layer within a preset time interval, and the preset time interval is 40s to 60s. After the spraying equipment completes the spraying, it is ensured that the adhesive layer has sufficient viscosity to meet the attachment requirements of the natural veneer.

[0062] Furthermore, the natural veneer may be made of willow veneer, elm veneer, fir veneer or other tree wood materials. Suitable natural veneer may be selected according to the actual use requirements of the table structure to meet the decoration requirements of the table structure.

[0063] Furthermore, the table structure is placed in a preset attachment operation space, and the environmental parameters of the table structure during natural veneer attachment are adjusted, and the environmental parameters are set as follows:

[0064] 15℃≤T≤35℃;

[0065] 50%≤H≤80%;

[0066] Wherein, T is the ambient temperature, and H is the ambient humidity.

[0067] Specifically, within the preset environmental parameters, the adhesive layer on the surface of the table structure can maintain sufficient viscosity, that is, the curing rate of the adhesive layer is slowed down, so that the natural veneer can be attached to the table structure.

[0068] Specifically, the natural veneer is adsorbed by a robot with a suction cup assembly and driven to adhere to the adhesive layer of the table structure. The natural veneer is blown by the blowing assembly on the robot so that the natural veneer can be adsorbed on the surface of the table structure.

[0069] Furthermore, by using a robot to attach the natural veneer to the surface of the table structure, the efficiency of the attachment operation on the table structure can be improved.

[0070] Specifically, in another feasible embodiment, the natural veneer can be attached manually by an operator. Based on the manual attachment by the operator, the reliability of the attachment between the natural veneer and the turning position of the table structure can be improved, and the reliability of the attachment between the natural veneer and the table structure can be improved.

[0071] Specifically, the step of attaching the natural veneer to the adhesive layer and drying it in the sun for a preset time to form a wooden decorative layer on the surface of the table structure includes:

[0072] The natural veneer is attached to the adhesive layer of the table structure, and the table structure is aired for a preset time so that the natural veneer can be closely attached to the surface of the table structure.

[0073] Furthermore, the preset time is set to 5 minutes to 10 minutes, and the adhesive layer can be solidified by drying the table structure, thereby achieving fixation of the adhesive layer and the natural veneer.

[0074] Specifically, the table structure can be dried in the sun by placing it outdoors and allowing it to stand and solidify in the sun, thereby improving the convenience of drying and solidifying the table structure.

[0075] Specifically, the drying treatment of the table structure can be achieved by using a baking device to dry and fix the table structure. The heating lamp of the baking device is used to illuminate and dry the table structure. The table structure is baked based on the heat emitted by the heating lamp, thereby increasing the curing rate of the adhesive layer of the table structure, so that the natural veneer can fit tightly to the table structure.

[0076] S14: performing a paint treatment on the wooden decorative layer, and performing a packaging treatment on the wooden decorative layer using paint.

[0077] The wooden decorative layer is painted, and the paint treatment process can be open paint treatment, semi-open paint treatment or closed paint treatment. The paint treatment process is adjusted according to the packaging treatment requirements of the natural veneer to ensure that the natural veneer has a good decorative effect.

[0078] Specifically, the wooden decorative layer is subjected to an open paint treatment. The open paint is a nitrocellulose lacquer formed by a low-concentration polyurethane ratio. The nitrocellulose lacquer is applied on the surface of the wooden decorative layer so that the wood pores on the surface of the wooden decorative layer can be completely exposed, thereby improving the wood texture effect on the surface of the wooden decorative layer, that is, retaining the natural wood grain texture on the surface of the wooden decorative layer, and improving the decorative effect of the wooden decorative layer on the surface of the table structure.

[0079] Furthermore, the open paint can also be wood wax oil. By penetrating the wood wax oil into the wooden decorative layer, the wooden decorative layer can be protected while retaining the natural texture of the wooden decorative layer. Based on the fully open paint processing process, the natural texture decorative effect of the wooden decorative layer can be met.

[0080] Furthermore, the wood wax oil is a natural environmentally friendly paint. The wood decorative layer is plastic-sealed and protected based on the wood wax oil, which is harmless to the human body and improves the safety of the table structure.

[0081] Furthermore, based on the fully open paint treatment, the wooden decorative layer can be repaired a second time to improve the reliability of the table structure.

[0082] Specifically, the wooden decorative layer is subjected to a semi-open paint treatment, and the semi-open paint treatment reduces the amount of paint used, and the wooden decorative layer is coated and sealed, thereby completing the plastic sealing protection of the wooden decorative layer while retaining part of the texture of the wooden decorative layer.

[0083] Furthermore, the use of paint can be reduced based on the semi-open paint process, which can reduce the cost of paint processing and reduce environmental pollution.

[0084] Specifically, the wooden decorative layer is treated with a fully sealed paint. After a layer of paint is applied to the wooden decorative layer of the table body structure, the formed paint is polished to make the surface of the paint layer smooth. After multiple layers of coating and polishing, the paint can completely seal the wooden decorative layer, so that the holes on the surface of the wooden decorative layer are sealed, thereby improving the plastic sealing protection effect of the paint on the wooden decorative layer, making the surface of the table body structure smooth and flat, with a certain gloss, and improving the decorative effect of the wooden decorative layer.

[0085] The embodiment of the present invention provides a surface treatment method for a table structure, by performing surface treatment on the table structure, natural veneer is attached to the surface of the table structure, so that the table structure has a good appearance. By setting a paint seal, the reliability of the plastic sealing of the table structure is improved.

[0086] A person skilled in the art may understand that all or part of the steps in the various methods of the above embodiments may be completed by instructing related hardware through a program, and the program may be stored in a computer-readable storage medium, and the storage medium may include: a read-only memory (ROM), a random access memory (RAM), a disk or an optical disk, etc.

[0087] In addition, the surface treatment method of a table structure provided by an embodiment of the present invention is introduced in detail above. Specific examples are used herein to illustrate the principle and implementation mode of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea. At the same time, for those skilled in the art, according to the idea of ​​the present invention, there will be changes in the specific implementation mode and application scope. In summary, the content of this specification should not be understood as a limitation on the present invention.

Claims

1. A surface treatment method for a table structure, characterized in that: The processing method comprises: Pre-treating the surface of the table structure, and forming a protective film on the surface of the table structure based on a hot melt process; Using a spraying device to coat the protective film on the surface of the table structure to form an adhesive layer; Attaching the wood cortex layer to the adhesive layer, and drying it in the sun for a preset time to form a wood decorative layer on the surface of the table structure; The wooden decorative layer is subjected to a paint treatment, and the wooden decorative layer is subjected to a packaging treatment based on the paint.

2. The surface treatment method of the table structure according to claim 1, characterized in that: The pre-treatment of the surface of the table structure to form a protective film on the surface of the table structure based on a hot melt process includes: The table structure is polished and cleaned, and the surface of the cleaned table structure is air-dried based on the air supply mechanism, so that the surface of the table structure remains dry.

3. The surface treatment method of the table structure according to claim 2, characterized in that: The pre-treatment of the surface of the table structure to form a protective film on the surface of the table structure based on a hot melt process also includes: The plastic powder is charged by an electrostatic generator, and the treated plastic powder is attached to the surface of the table structure; The plastic powder is melted by baking equipment so that the plastic powder is completely melted on the surface of the table structure to form a protective film on the surface of the table structure.

4. The surface treatment method of the table structure according to claim 3, characterized in that: The step of melting the plastic powder using a baking device so that the plastic powder is completely melted on the surface of the table structure and a protective film is formed on the surface of the table structure comprises: Placing the table structure with plastic powder in a baking device, and continuously baking the table structure within a preset baking temperature; Among them, the baking time range is set to 12min~18min, and the baking temperature range is set to 180℃~220℃.

5. The surface treatment method of a table structure according to claim 1, characterized in that: The method of coating the protective film on the surface of the table structure with a spraying device to form an adhesive layer comprises: The table structure is placed in the working space of the spraying equipment, and the spraying operation of the spraying equipment is adjusted according to the posture state of the table structure.

6. The surface treatment method of a table structure according to claim 5, characterized in that: The step of adjusting the spraying operation of the spraying equipment according to the posture state of the table structure comprises: The spraying equipment is set to spray over a large area, and the spraying direction of the spraying equipment is set in combination with the placement position of the table structure, so that the nozzle of the spraying equipment sprays each surface of the table structure in turn; Or the spraying equipment is set to spray in a small range, and the running path of the spraying equipment is set in combination with the shape and size of the table structure, and the spraying equipment is driven to spray the table structure along the running path.

7. The surface treatment method of a table structure according to claim 1, characterized in that: The step of attaching the wood cortex layer to the adhesive layer and drying it for a preset time to form a wood decorative layer on the surface of the table structure comprises: After spraying the adhesive layer on the surface of the table structure by the spraying equipment, the wood cortex layer is attached to the adhesive layer within a preset time interval; The preset time interval is 40s to 60s.

8. The surface treatment method of a table structure according to claim 7, characterized in that: The step of attaching the wood cortex layer to the adhesive layer and drying the wood cortex layer for a preset time to form a wood decorative layer on the surface of the table structure also includes: The table structure is placed in a preset attachment operation space, and the environmental parameters of the table structure during the attachment of the wood cortex are adjusted.

9. The surface treatment method of a table structure according to claim 8, characterized in that: The environmental parameters are: 15℃≤T≤35℃; 50%≤H≤80%; Wherein, T is the ambient temperature, and H is the ambient humidity.

10. The surface treatment method of a table structure according to claim 1, characterized in that: The painting of the wooden decorative layer and the encapsulation of the wooden decorative layer based on the paint include: The wooden decorative layer is subjected to an open paint treatment, or the wooden decorative layer is subjected to a semi-open paint treatment, or the wooden decorative layer is subjected to a closed paint treatment.