Smoke exhaust pipe and manufacturing method thereof

By applying and heating the spiral wound structure of aluminum foil with a thermoplastic resin layer in the smoke exhaust pipe, the problems of low interface strength and thin aluminum foil are solved, and the tensile strength and sealing of the smoke exhaust pipe are improved, achieving high efficiency Energy-saving production and use effects.

CN118905093APending Publication Date: 2024-11-08梁立伟
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202411230006.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The interface strength of the existing smoke exhaust pipe is low, easy to break, and the aluminum foil is thin and easy to break, resulting in safety hazards and poor sealing during use.

Method used

The thermoplastic resin layer is coated with aluminum foil and wound spirally into a hollow spiral tube, and the thermoplastic resin layer is cured by heating to enhance the connection strength at the bite, while an annular joint and an inner ring are provided at the end to improve fixation and sealing.

Benefits of technology

It significantly improves the tensile strength and anti-pinning capability of the smoke exhaust pipe, improves sealing and durability, ensures that the interface is not easy to loosen, and achieves efficient and energy-saving production through the heating process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118905093A_ABST
    Figure CN118905093A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a smoke exhaust pipe, which comprises the following steps of: spirally winding aluminum foils coated with thermoplastic resin layers on the surfaces to form a hollow spiral pipe, overlapping the edges of the adjacent aluminum foils and meshing together to form a meshing part, adhering the thermoplastic resin layers on the two aluminum foils at the meshing part together, and heating the meshing part to form the hollow spiral pipe. And the thermoplastic resin layers which are attached together are subjected to hot melting and curing, and therefore the smoke exhaust pipe is manufactured. According to the smoke exhaust pipe manufactured through the manufacturing method of the smoke exhaust pipe, the connecting strength of the connector is high, and the smoke exhaust pipe is not prone to being snapped or punctured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a smoke exhaust pipe and a manufacturing method of the smoke exhaust pipe, belonging to the technical field of smoke exhaust pipes. Background Art

[0002] In daily life, smoke exhaust pipes are indispensable accessories for home appliances such as water heaters and range hoods. In the prior art, smoke exhaust pipes are mostly made of aluminum foil, stainless steel, and galvanized iron sheets. Among them, aluminum foil pipes are widely used because of their fast heat dissipation, good ductility, and low production cost. However, the aluminum foil pipes are spirally wound and interlocked together. Due to the low structural strength of the interlocking part, problems such as pulling or breaking may occur during use. In addition, the aluminum foil is very thin and easily punctured.

[0003] Chinese patent document CN202915428U discloses a novel range hood exhaust, comprising a spiral tube formed by wrapping aluminum foil on a spiral skeleton, with docking ports at both ends of the spiral tube, and a shaping ring on the inner wall of the docking port. The shaping ring in the patent is attached to the inner wall of the docking port by double-sided adhesive, and the spiral skeleton is formed by winding elastic steel wire.

[0004] Chinese patent document CN220582518U discloses a retractable range hood duct. The aluminum foil tube in the patent is formed by extruding aluminum foil and then spirally winding it. Adjacent aluminum foils are crimped and bitten together, and the strength of the connection structure at the biting part is poor.

[0005] Chinese patent document CN211591591U discloses an aluminum foil veneer for protecting the outer covering of a smoke exhaust pipe, including an aluminum foil fabric, several three-dimensional glass fiber meshes are arranged below the aluminum foil fabric, and a tensile layer formed by several longitudinally oblique bidirectionally spaced and staggered tensile reinforcements intersecting each other is arranged below the three-dimensional glass fiber mesh, and kraft paper is pasted and installed below the tensile layer, and PE adhesive or water-based adhesive is coated and formed below the tensile layer, and kraft paper is pasted and installed below the tensile layer through PE adhesive or water-based adhesive. The aluminum foil veneer structure in this patent is too complicated and the production cost is high.

[0006] Chinese patent document CN110899366A discloses a quantitative feeding spiral tube automatic processing equipment, including a support platform, a feeding mechanism, a molding mechanism, a cutting mechanism, a lifting and grinding mechanism and a moving mechanism, the feeding mechanism and the molding mechanism are arranged on the support platform, a work box is arranged on the side of the support platform, and a first bracket and a second bracket are arranged on the side of the work box away from the molding mechanism, the lifting and grinding mechanism includes two sets of lifting and grinding components, the feeding mechanism includes a guide component and a straightening component, the straightening component includes a plurality of rollers and a transmission component, and the plurality of rollers are arranged on the support platform, and the two ends of the rollers are respectively provided with bumps. The quantitative feeding spiral tube automatic processing equipment of the present invention can automatically feed, automatically process tinplate into spiral air ducts, and then perform cutting and grinding, thereby realizing automatic processing of spiral air ducts. The patent document discloses a production equipment for tinplate spiral exhaust pipes.

[0007] Chinese patent document CN1266387A discloses a method for producing a spiral exhaust pipe, providing a material having first and second edges spaced apart from each other and a mold having a groove. Exhaust holes are formed in the material. The material is rolled into a tube by the mold so that the exhaust holes extend outwardly away from the long axis of the tube. The exhaust holes pass through the groove of the mold when the material is rolled into the tube. Then the first and second edges of the material are connected to each other. The patent document discloses a production device for a spiral exhaust pipe. Summary of the invention

[0008] The technical problem to be solved by the present invention is to provide a manufacturing method for quickly and conveniently producing a smoke exhaust pipe with high interface strength and not easy to be broken, and a smoke exhaust pipe manufactured by the manufacturing method.

[0009] The technical solution provided by the present invention for solving the above technical problems is: a method for manufacturing a smoke exhaust pipe, wherein an aluminum foil coated with a thermoplastic resin layer on the surface is spirally wound into a hollow spiral tube, and the adjacent edges of the aluminum foils are overlapped and bitten together to form a bite portion, and the thermoplastic resin layers on the two aluminum foils at the bite portion are bonded together, and then the bite portion is heated to heat-melt and solidify the bonded thermoplastic resin layers, thereby manufacturing a smoke exhaust pipe.

[0010] A preferred technical solution is that the above-mentioned heating bite portion is to pass the hollow spiral tube that has formed the bite portion through the electromagnetic heating coil, so that the hollow spiral tube is heated under the action of electromagnetic induction.

[0011] A preferred technical solution is that the above-mentioned heating bite portion is to pass the hollow spiral tube that has formed the bite portion through an infrared radiation heating ring so that the hollow spiral tube is heated under the action of infrared radiation.

[0012] A preferred technical solution is that the above-mentioned heating bite portion is to pass the hollow spiral tube that has formed the bite portion through a hot air heater so that the hollow spiral tube is heated by the action of hot air.

[0013] A preferred technical solution is that the surface of the aluminum foil facing the outside of the smoke exhaust pipe is completely coated with a thermoplastic resin layer, and the thermoplastic resin layer is a polyethylene resin layer, and the mass ratio of the polyethylene resin layer to the aluminum foil is 1:6 to 1:3. The thermoplastic resin layer is coated on the outer layer of the aluminum foil, and the thermoplastic resin layer has good impact resistance, high hardness, and good anti-needle effect after curing. The thermoplastic resin layer can be any hot-melt adhesive material, such as polyethylene (PE), polypropylene (PP), polystyrene (PS), polyvinyl alcohol (PVA), the composite process of polyethylene and aluminum foil is relatively mature, and polyethylene has strong chemical stability and physical properties, so polyethylene (PE) is preferred, and low-density polyethylene (LDPE), high-density polyethylene (HDPE), linear low-density polyethylene (LLDPE) or ultra-high molecular weight polyethylene can be selected according to needs.

[0014] A preferred technical solution is that the aluminum foil is pressed into corrugations with equal spacing in the width direction of the aluminum foil by rollers arranged side by side before being spirally wound into a hollow spiral tube. After the hollow spiral tube is cut into sections, the baffles at both ends of the hollow spiral tube move toward each other to deform the corrugations and compress the hollow spiral tube. The aluminum foil of the smoke exhaust pipe adopts a full corrugation process, which makes ventilation smoother, less noisy, and will not shake when the internal wind speed is high.

[0015] A preferred technical solution is that the height of the corrugations on the aluminum foil is 2.5 to 5 mm, the width of the corrugations on the aluminum foil is 1 to 2 mm, the width of the aluminum foil is 10 to 20 mm, the thickness of the aluminum foil is 0.07 to 0.12 mm, the thickness of the thermoplastic resin layer is 0.01 to 0.04 mm, and the weight of the aluminum foil coated with the thermoplastic resin layer is 150 to 350 g / m 2 .

[0016] A preferred technical solution is that the above-mentioned bite portion is formed by folding the edges of two pieces of aluminum foil around each other at least once, the middle part of the bite portion is squeezed into a recessed portion, and the two sides of the recessed portion are gathered inwardly.

[0017] An annular joint is arranged outside the end of the smoke exhaust pipe, one end of the annular joint extends out of the aluminum foil, an inner ring is arranged inside the smoke exhaust pipe, the width of the inner ring is smaller than the width of the annular joint, and the aluminum foil at the end of the smoke exhaust pipe is clamped and fixed between the annular joint and the inner ring by squeezing the annular joint inwardly and the inner ring outwardly.

[0018] The technical solution provided by the present invention to solve the above technical problem is: a smoke exhaust pipe manufactured by adopting the above manufacturing method of the smoke exhaust pipe.

[0019] The present invention has positive effects: (1) The manufacturing method of the smoke exhaust pipe of the present invention comprises coating a thermoplastic resin layer on the outer surface of the aluminum foil, and curing the thermoplastic resin layer through a suitable process when the finished product is made, so that the two pieces of aluminum foil are firmly connected together and cannot be torn apart by hand, and the tensile strength of the bite portion is significantly improved. At the same time, the cured thermoplastic resin layer also increases the anti-needle puncture ability of the smoke exhaust pipe, making it not easy to be punctured, thereby improving the sealing and durability of the smoke exhaust pipe.

[0020] (2) The manufacturing method of the smoke exhaust pipe of the present invention adopts the method of passing the hollow spiral tube through the heater for heating. Since the hollow spiral tube itself needs to move forward at a uniform speed during the spiral winding, electromagnetic induction coil heating is the best technical solution and the most efficient and energy-saving. The hot melt curing of the thermoplastic resin layer does not require too high a temperature. For example, the polyethylene resin layer can be at about 150°C. If an electromagnetic heating coil is used, the power does not need to be too high, and a medium frequency can be used. The temperature of the hollow spiral tube can be accurately controlled by controlling the uniform forward speed of the hollow spiral tube and the power of the electromagnetic heating coil.

[0021] (3) The manufacturing method of the smoke exhaust pipe of the present invention can set a ring joint and an inner ring at one end or both ends of the smoke exhaust pipe. The ring joint is pressed inward and the inner ring is supported outward. The ring joint and the inner ring are interference fit to be fixed on the smoke exhaust pipe. The assembly process is convenient, the fixation is firm, and the sealing is good. The smoke exhaust pipe with a ring joint is more convenient to install.

[0022] (4) In the manufacturing method of the smoke exhaust pipe of the present invention, the bite portion of the smoke exhaust pipe adopts a double-button pressing technology, that is, the edges of the two pieces of aluminum foil are folded around each other and bite together, and then a depression is squeezed out in the middle of the bite portion by a pressing wheel, so that the aluminum foil of the bite portion is folded together in multiple layers, which effectively improves the connection strength of the bite portion, so that even if the aluminum foil of the smoke exhaust pipe is torn, the bite portion will not loosen.

[0023] (5) In the manufacturing method of the smoke exhaust pipe of the present invention, the aluminum foil of the smoke exhaust pipe adopts a full corrugated process, which makes the ventilation smoother, the noise is lower, and there is no shaking when the internal wind speed is high. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The manufacturing method of the smoke exhaust pipe of the present invention is further described below in conjunction with the accompanying drawings.

[0025] Figure 1 is a schematic diagram of the three-dimensional structure of the smoke exhaust pipe of Example 1; Figure 2 It is a cross-sectional schematic diagram of the annular joint and the inner ring of the smoke exhaust pipe of Example 1; Figure 3 for Figure 2 Schematic diagram of the cross section of the bite portion of the middle exhaust pipe.

[0026] The above-mentioned reference numerals are as follows: Aluminum foil 1, bite portion 11, recessed portion 12, annular joint 2, inner ring 3. DETAILED DESCRIPTION

[0027] Example 1, see Figures 1 to 3 The manufacturing method of the smoke exhaust pipe of this embodiment is that a roll of aluminum foil 1 is conveyed forward under the action of a guide component and a straightening component, and after being soaked in a processing liquid tank, corrugations arranged at equal intervals are pressed out on the aluminum foil 1 by rollers arranged side by side, and then the aluminum foil 1 coated with a thermoplastic resin layer on the surface is spirally wound into a hollow spiral tube, and the edges of adjacent aluminum foils 1 are overlapped and bite together under the action of a bite component to form a bite portion 11, and the thermoplastic resin layers on the two aluminum foils 1 at the bite portion 11 are bonded together, and then the hollow spiral tube with the bite portion 11 formed is passed through an electromagnetic heating coil, so that the hollow spiral tube is heated under the action of electromagnetic induction, and the hollow spiral tube is controlled to be 150°C, and the thermoplastic resin layers bonded together are hot-melt solidified, and are cut off by a cutting device after reaching a certain length, and the baffles at both ends of the hollow spiral tube move toward each other, and the smoke exhaust pipe is compressed along its length direction by the deformation of the corrugations, thereby manufacturing the smoke exhaust pipe.

[0028] The surface of the aluminum foil 1 facing the outside of the smoke exhaust pipe is entirely coated with a thermoplastic resin layer, which is a polyethylene resin layer, and the mass ratio of the polyethylene resin layer to the aluminum foil 1 is 1:3.

[0029] The height of the corrugation on the aluminum foil 1 is 3 mm, the width of the corrugation on the aluminum foil 1 is 2 mm, the width of the aluminum foil 1 is 15 mm, the total thickness of the aluminum foil 1 and the thermoplastic resin layer is 0.1 mm, and the gram weight of the aluminum foil 1 coated with the thermoplastic resin layer is 250 g / m 2 .

[0030] The bite portion 11 is formed by folding the edges of the two aluminum foils 1 around each other at least once, and the middle of the bite portion 11 is squeezed into a recessed portion 12, and the two sides of the recessed portion 12 are gathered inwardly.

[0031] The equipment used in this embodiment, except for the electromagnetic heating coil, can refer to patent documents CN1266387A and CN110899366B.

[0032] The exhaust pipe of this embodiment has been tested by tensile test. The tensile strength of the bite part can reach the tensile strength of the aluminum foil 50.2N / mm 2 .

[0033] The aluminum foil of this embodiment adopts the alloy grade of cigarette tube aluminum foil 8011, and the measured aluminum content is 98.5%.

[0034] Embodiment 2, the manufacturing method of the smoke exhaust pipe of this embodiment is that a roll of aluminum foil 1 is conveyed forward under the action of a guiding component and a straightening component, and after being soaked in a processing liquid tank, corrugations arranged at equal intervals are pressed out on the aluminum foil 1 by rollers arranged side by side, and then the aluminum foil 1 coated with a thermoplastic resin layer on the surface is spirally wound into a hollow spiral tube, and the edges of adjacent aluminum foils 1 are overlapped and bite together under the action of a bite component to form a bite portion 11, and the thermoplastic resin layers on the two aluminum foils 1 at the bite portion 11 are bonded together, and then the hollow spiral tube with the bite portion 11 formed is passed through an infrared radiation heating ring, so that the hollow spiral tube is heated under the action of infrared radiation, and the hollow spiral tube is controlled to be 130°C, and the thermoplastic resin layers bonded together are hot-melt solidified, and are cut off by a cutting device after reaching a certain length, and the baffles at both ends of the hollow spiral tube move toward each other, and the smoke exhaust pipe is compressed along its length direction by the deformation of the corrugations, thereby obtaining the smoke exhaust pipe.

[0035] The edges of both sides of the surface of the aluminum foil 1 facing the outside of the smoke exhaust pipe are coated with a thermoplastic resin layer, which is a low-density polyethylene resin layer. The mass ratio of the polyethylene resin layer to the aluminum foil 1 is 1:4.

[0036] The height of the corrugation on the aluminum foil 1 is 3.5 mm, the width of the corrugation on the aluminum foil 1 is 1.8 mm, the width of the aluminum foil 1 is 20 mm, the total thickness of the aluminum foil 1 and the thermoplastic resin layer is 0.12 mm, and the gram weight of the aluminum foil 1 coated with the thermoplastic resin layer is 300 g / m 2 .

[0037] The seam portion 11 is formed by folding the edges of two aluminum foils 1 around each other.

[0038] Embodiment 3, the manufacturing method of the smoke exhaust pipe of this embodiment is that a roll of aluminum foil 1 is conveyed forward under the action of a guiding component and a straightening component, and after being soaked in a processing liquid tank, corrugations arranged at equal intervals are pressed out on the aluminum foil 1 by rollers arranged side by side, and then the aluminum foil 1 coated with a thermoplastic resin layer on the surface is spirally wound into a hollow spiral tube, and the edges of adjacent aluminum foils 1 are overlapped and bite together under the action of a bite component to form a bite portion 11, and the thermoplastic resin layers on the two aluminum foils 1 at the bite portion 11 are bonded together, and then the hollow spiral tube with the bite portion 11 formed is passed through a hot air oven, so that the hollow spiral tube is heated under the action of hot air, and the hollow spiral tube is controlled to be 160°C, and the thermoplastic resin layers bonded together are hot-melt solidified, and are cut off by a cutting device after reaching a certain length, and the baffles at both ends of the hollow spiral tube move toward each other, and the smoke exhaust pipe is compressed by the deformation of the corrugations along its length direction, thereby obtaining the smoke exhaust pipe.

[0039] The edges of both sides of the surface of the aluminum foil 1 facing the outside of the smoke exhaust pipe are coated with a thermoplastic resin layer, which is a high-density polyethylene resin layer. The mass ratio of the polyethylene resin layer to the aluminum foil 1 is 1:5.

[0040] The height of the corrugation on the aluminum foil 1 is 2.5 mm, the width of the corrugation on the aluminum foil 1 is 1 mm, the width of the aluminum foil 1 is 10 mm, the total thickness of the aluminum foil 1 and the thermoplastic resin layer is 0.08 mm, and the gram weight of the aluminum foil 1 coated with the thermoplastic resin layer is 200 g / m 2 .

[0041] The bite portion 11 is formed by folding the edges of the two aluminum foils 1 around each other at least once, and the middle of the bite portion 11 is squeezed into a recessed portion 12, and the two sides of the recessed portion 12 are gathered inwardly.

[0042] Obviously, the above embodiments are merely examples for clearly illustrating the embodiments of the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the embodiments here. However, these obvious changes or modifications derived from the spirit of the present invention are still within the scope of protection of the present invention.

Claims

1. A method for manufacturing a smoke exhaust pipe, characterized in that: An aluminum foil (1) coated with a thermoplastic resin layer on its surface is spirally wound into a hollow spiral tube, and the edges of adjacent aluminum foils (1) are overlapped and bitten together to form a bite portion (11). The thermoplastic resin layers on the two aluminum foils (1) at the bite portion (11) are bonded together, and then the bite portion (11) is heated to heat-melt and solidify the bonded thermoplastic resin layers, thereby manufacturing a smoke exhaust pipe.

2. The method for manufacturing a smoke exhaust pipe according to claim 1, characterized in that: The heating bite portion (11) is achieved by passing the hollow spiral tube that has formed the bite portion (11) through an electromagnetic heating coil, so that the hollow spiral tube is heated under the action of electromagnetic induction.

3. The method for manufacturing a smoke exhaust pipe according to claim 1, characterized in that: The heating of the bite portion (11) is performed by passing the hollow spiral tube that has formed the bite portion (11) through an infrared radiation heating ring, so that the hollow spiral tube is heated under the action of infrared radiation.

4. The method for manufacturing a smoke exhaust pipe according to claim 1, characterized in that: The heating of the bite portion (11) is performed by passing the hollow spiral tube that has formed the bite portion (11) through a hot air heater, so that the hollow spiral tube is heated under the action of hot air.

5. The method for manufacturing a smoke exhaust pipe according to any one of claims 1 to 4, characterized in that: The surface of the aluminum foil (1) facing the outside of the smoke exhaust pipe is entirely coated with a thermoplastic resin layer, wherein the thermoplastic resin layer is a polyethylene resin layer, and the mass ratio of the polyethylene resin layer to the aluminum foil 1 is 1:6 to 1:

3.

6. The method for manufacturing a smoke exhaust pipe according to any one of claims 1 to 4, characterized in that: Before the aluminum foil (1) is spirally wound into a hollow spiral tube, rollers arranged side by side are used to press out corrugations arranged at equal intervals in the width direction of the aluminum foil (1); after the hollow spiral tube is cut into sections, baffles at both ends of the hollow spiral tube are moved toward each other so that the corrugations are deformed and the hollow spiral tube is compressed.

7. The method for manufacturing a smoke exhaust pipe according to any one of claims 1 to 4, characterized in that: The height of the corrugations on the aluminum foil (1) is 2.5 to 5 mm, the width of the corrugations on the aluminum foil (1) is 1 to 2 mm, the width of the aluminum foil (1) is 10 to 20 mm, the thickness of the aluminum foil (1) is 0.07 to 0.12 mm, the thickness of the thermoplastic resin layer is 0.01 to 0.04 mm, and the gram weight of the aluminum foil (1) coated with the thermoplastic resin layer is 150 to 350 g / m 2 .

8. A method for manufacturing a smoke exhaust pipe according to any one of claims 1 to 4, characterized in that: The bite portion (11) is formed by folding the edges of two pieces of aluminum foil (1) around each other at least once, the middle of the bite portion (11) is squeezed into a recessed portion (12), and the two sides of the recessed portion (12) are gathered inwardly.

9. The method for manufacturing a smoke exhaust pipe according to any one of claims 1 to 4, characterized in that: An annular joint (2) is disposed on the outer surface of the end of the smoke exhaust pipe, one end of the annular joint (2) extends out of the aluminum foil (1), an inner ring (3) is disposed in the smoke exhaust pipe, the width of the inner ring (3) is smaller than the width of the annular joint (2), and the aluminum foil (1) at the end of the smoke exhaust pipe is clamped and fixed between the annular joint (2) and the inner ring (3) by pressing the annular joint (2) inwards and the inner ring (3) outwards.

10. A smoke exhaust pipe manufactured by the method for manufacturing a smoke exhaust pipe according to claim 1.

Citation Information

Patent Citations

  • Quantitative feeding spiral pipe automatic machining equipment

    CN110899366A

  • An automatic processing equipment for quantitative feeding of spiral tubes

    CN110899366B

  • Spiral-formed exhaust tube

    CN1266387A

  • Novel smoke exhaust pipe for range hood

    CN202915428U

  • Aluminum foil veneer for coating and protecting smoke exhaust pipeline

    CN211591591U