Image visual reversal anti-counterfeiting preparation process for metal coin badge

Through ultra-fast laser micro-nano processing and micro-nano optical technology, combined with visual reversal design, the problem of insufficient aesthetics and stability of metal coin seal anti-counterfeiting technology is solved, and the visual light and dark reversal effect of metal coin seal is realized, and the anti-counterfeiting level is improved. and aesthetic effects, and reduce costs through batch processing.

CN118905437APending Publication Date: 2024-11-08CHINA BANKNOTE PRINTING & MINTING +1
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202310311125.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-03-28
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The anti-counterfeiting technology of existing metal coin seals is difficult to meet the aesthetic and stability requirements, and the anti-counterfeiting effect is poor under physical wear and chemical changes. It requires a simple and reliable process to improve the anti-counterfeiting level and aesthetic effect of metal coin seals.

Method used

Utilize ultrafast laser micro-nano processing and micro-nano optical technology, combined with visual inversion optical micro-nano pattern structure design and laser processing, realize micro-nano pattern structure processing on the surface of metal coin molds, and improve anti-counterfeiting through visual light and dark reversal effect level.

Benefits of technology

It significantly improves the aesthetics and anti-counterfeiting level of metal coin seals, ensures the stability and processing efficiency of micro-nano stripes, and realizes batch processing through mold imprinting, reducing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118905437A_ABST
    Figure CN118905437A_ABST
Patent Text Reader

Abstract

The invention discloses an image visual reversal anti-counterfeiting preparation process for a metal coin stamp. The image visual reversal anti-counterfeiting preparation process comprises the following steps: step 1, determining a visual light and shade reversal effect of a target pattern; 2, calculating gray values of different areas of the optimized target pattern by adopting a design method of a visual inversion optical micro-nano pattern structure, and determining the width, depth, filling spacing and filling direction of filling stripes in different areas of the target pattern according to the gray values; 3, the surface of the metal coin stamp mold to be machined is polished and cleaned, and it is guaranteed that the surface is smooth and free of foreign matter; 4, determining the laser power, the pulse width, the repetition frequency and the scanning speed of laser processing according to the to-be-processed target pattern and the visual light and shade inversion effect; and 5, the micro-nano pattern structure with the visual brightness reversal effect is machined on the surface of the metal coin stamp mold through a laser machining system. According to the invention, the aesthetic and anti-counterfeiting levels of the metal coin medal are improved; through the optical micro-nano stripe structure, a visual reversal effect is realized.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of coinage anti-counterfeiting, and in particular to an image visual reversal anti-counterfeiting preparation process for metal coins and stamps based on ultrafast laser micro-nano processing and micro-nano optics. Background Art Metal coins and seals are important circulating currencies that are indispensable in daily life. In the current commodity market, the proliferation of counterfeit coins has not only caused huge economic losses, but also seriously affected social stability and the image of the country. Therefore, improving the anti-counterfeiting technology of currency has become an urgent problem to be solved. The relevant technology of coin anti-counterfeiting in my country is still immature, and a relatively complete anti-counterfeiting standard for metal coins has not yet been formulated. At present, the anti-counterfeiting elements of coins mainly include the coin's size, weight, color, surface brightness, metal composition, and the pattern and text information on the coin surface. During the circulation process, coins are often affected by physical factors such as wear and scratches, and the chemical properties of metals are relatively active. It is inevitable that they will come into contact with air, moisture or acidic substances, and their surfaces are prone to chemical changes, resulting in discoloration and corrosion. These have caused great obstacles to the anti-counterfeiting technology of coins. In order to maintain social stability and reduce the waste of resources, it is necessary to further improve the anti-counterfeiting technology of metal coins. Therefore, developing new coin anti-counterfeiting technology that is "easy for the public to identify and difficult for counterfeiters to forge" is of great significance for improving my country's coin anti-counterfeiting standards, promoting the healthy development of the coin circulation market, and bringing my country's coin anti-counterfeiting technology in line with international standards.

[0003] At present, the popular coin anti-counterfeiting technologies in the world are mainly divided into mass anti-counterfeiting technologies, material anti-counterfeiting technologies and structural anti-counterfeiting technologies. Mass anti-counterfeiting technologies generally include side embossing or lettering technology, edge continuous bevel thread technology, secret mark and micro-text technology, fine pattern technology, etc. At present, many circulating coins still use material anti-counterfeiting technologies, such as bimetallic inlay, trimetallic inlay and partial inlay. It is to inlay two different metals or alloys together under a certain pressure. Bimetallic coins have good machine-readable performance due to their strong electromagnetic characteristics. In addition, there is also a type of structural anti-counterfeiting technology, such as two-color, polygonal, special-shaped, circular middle punching, etc., which is mainly convenient for identifying coins from the appearance. With the continuous development of science and technology and living standards, the above anti-counterfeiting technologies are gradually unable to meet the requirements of actual production and life for the anti-counterfeiting level, aesthetics, stability and other aspects of metal coins.

[0004] Nano holographic fantasy is a structural color based on micro-nano optics. It uses high-density micro-nano structure gratings to produce certain visual colors. This technology can be applied to anti-counterfeiting labels, tobacco packaging, card security and other fields. White light irradiates different grating structures, which will produce different diffraction fields. This requires designers to design and control from the perspective of aesthetics and art, and effectively manage these diffracted rainbow lights so that they can achieve the required process effects. However, this anti-counterfeiting technology requires complex structural design and special processing technology, which is very difficult. At present, the design and production of such nano gratings mainly include surface array interference, dot matrix interference, imaging projection lithography and laser direct writing. Among them, laser direct writing uses high-energy laser beams to etch high-precision lines on the surface of the mold, so that the surface of the commemorative coin presents a multi-level color effect. "Fantasy" is technically called "visual variable light design", and its English name is "OVD", which is the abbreviation of Optical Variable Device. "Fantasy" can be achieved through two different processes. One is to use high-resolution point-to-moment holographic technology to carve fine lines on the mold, and the fantasy process can be formed in one go. The other is to use a special pad or metal plate as a mold to emboss fine wrinkles on the surface of the material. These wrinkles can diffract all the light irradiated on the coin and decompose into component colors according to the spacing of the wrinkles at different positions on the coin. There are two main problems in using laser direct writing to process micro-nano structures with special visual effects. One is the design of micro-nano structures with different patterns and different visual effects, and the other is high-quality and efficient processing of micro-nano structures.

[0005] In view of this, there is an urgent need for a mature, simple and reliable process method to achieve the design and processing of micro-nano pattern structures that can produce certain visual effects, and to improve the anti-counterfeiting level and aesthetic effect of metal coins and stamps. In view of the above phenomenon, the present invention proposes an image visual reversal anti-counterfeiting preparation process for metal coins and stamps, which is applied to the fields of coinage and anti-counterfeiting, aiming to solve the above-mentioned problems, and is committed to the development of coinage, anti-counterfeiting and other industries, and to protect the legitimate rights and interests of the country and citizens.

[0006] The information disclosed in this background technology section is only intended to deepen the understanding of the overall background technology of the present invention, and should not be regarded as acknowledging or suggesting in any form that the information constitutes the prior art already known to those skilled in the art. Summary of the invention

[0007] In order to meet the above needs, the present invention provides a laser processing method for metal coin stamp molds with visual light and dark reversal effects. The purpose is to propose a process method that combines the image visual reversal technology in the field of micro-nano optics with laser processing technology, and applies it to the surface of metal coin stamp molds to achieve the design and processing of micro-nano pattern structures with special visual light and dark reversal effects, thereby improving the anti-counterfeiting level of metal coins and stamps. By designing the selected pattern into a certain micro-nano pattern structure, laser processing is used to realize the processing of the micro-nano pattern structure on the surface of the metal mold to achieve the visual effect of light and dark reversal of the pattern when the observation angle is changed. The technical solution is as follows: An image visual reversal anti-counterfeiting preparation process for metal coins and stamps, comprising the following steps: Step 1: Determine the visual light-dark reversal effect of the target pattern; Step 2: Use the design method of visual inversion optical micro-nano pattern structure to calculate and optimize the grayscale values ​​of different areas of the target pattern, and determine the width, depth, filling spacing, and filling direction of the filling stripes in different areas of the target pattern according to the grayscale values; Step 3: Polish the surface of the metal coin mold to be processed and clean it to ensure that the surface is smooth and free of foreign matter; Step 4: Determine the laser power, pulse width, repetition frequency, and scanning speed of laser processing according to the target pattern to be processed and the visual light and dark reversal effect; Step 5: Use a laser processing system to process the above-mentioned micro-nano pattern structure with visual light and dark reversal effect on the surface of the metal coin mold.

[0008] The filling stripes described in step 2 are linear arrays. According to the different visual effects of the light and dark reversal of the target pattern, the width, depth, filling spacing, and filling direction of the straight lines in different areas are different.

[0009] Furthermore, the width of the straight line ranges from 15 to 50 μm, the depth ranges from 2 to 10 μm, the filling spacing ranges from 15 to 50 μm, and the filling direction ranges from 0 to 180°.

[0010] Furthermore, the angle between the adjacent area filling lines is 90°.

[0011] Furthermore, the laser power adjustment range of step 4 is 20 to 60 W, the pulse width adjustment range is 1 to 9 ns, the repetition frequency adjustment range is 500 to 5000 kHz, and the scanning speed range is 1000 to 3000 mm / s.

[0012] Furthermore, the repetition frequency, scanning speed and pulse width need to match each other so that the laser spot overlap ratio is greater than 1 to avoid the appearance of optical diffraction stripes and surface pitting.

[0013] Furthermore, the laser processing system described in step 5 uses a femtosecond laser with a wavelength of 1035 nm, a single pulse energy of >80 μJ, and an adjustable pulse width.

[0014] Furthermore, the micro-nano pattern structure with visual light and dark reversal effect processed on the surface of the metal coin mold as described in step 5 is copied to the surface of the metal coin through embossing technology, so that the metal coin presents a visual light and dark reversal effect.

[0015] Compared with the existing technology, its advantages and effects are: based on the relevant theories of micro-nano optics and laser processing, a design method for visually reversed optical micro-nano pattern structures is established and developed, the grayscale values ​​of different areas of the target pattern are calculated and optimized, and the structural parameters of the micro-nano patterns such as the stripe filling density and filling direction in different areas of the target pattern are determined according to the grayscale value calculation, thereby realizing the design of optical micro-nano pattern structures with different visual light and dark reversal effects for different patterns, which significantly improves the aesthetics and anti-counterfeiting level of metal coins and stamps; by utilizing the fine processing technology of laser processing, a visual reversal effect is achieved through an optical micro-nano stripe structure on the metal coin and stamp mold, thereby ensuring the stability, processing efficiency and processing quality of the micro-nano stripe structure; batch processing is achieved through mold imprinting technology, which improves processing efficiency and reduces processing costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0017] Figure 1 is a flow chart of the present invention; Figure 2 Schematic diagram of the micro-nano structure designed for the present invention; Figure 3 A schematic diagram of a laser processing system used in the present invention; Figure 4 The micro-nano pattern structure diagram processed by the present invention; Figure 5 It is the actual processing effect diagram of the present invention; In the figure, 1. laser, 2. laser beam, 3. reflector A, 4. reflector B, 5. galvanometer, 6. focusing field lens, 7. metal coin mold. Implementation

[0018] In order to make the purpose, technical solution and advantages of the embodiments of the present disclosure clearer, the technical solution of the embodiments of the present disclosure will be clearly and completely described below in conjunction with the drawings of the embodiments of the present disclosure. Obviously, the described embodiments are part of the embodiments of the present disclosure, not all of the embodiments. Based on the described embodiments of the present disclosure, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present disclosure.

[0019] The following will describe in detail an image visual reversal anti-counterfeiting preparation process for metal coins and stamps according to the present invention in conjunction with the accompanying drawings. Example

[0020] like Figure 1 As shown, a specific processing flow of an image visual reversal anti-counterfeiting preparation process for metal coins and stamps is as follows: Step 1: Determine the visual light-dark reversal effect of the target pattern; Step 2: Use the design method of visual inversion optical micro-nano pattern structure to calculate and optimize the grayscale values ​​of different areas of the target pattern, and determine the width, depth, filling spacing, and filling direction of the filling stripes in different areas of the target pattern according to the grayscale values; Step 3: Polish the surface of the metal coin mold to be processed and clean it to ensure that the surface is smooth and free of foreign matter; Step 4: Determine the laser power, pulse width, repetition frequency, and scanning speed of laser processing according to the target pattern to be processed and the visual light and dark reversal effect; Step 5: Use a femtosecond laser processing system to process the above-mentioned micro-nano pattern structure with visual light and dark reversal effect on the surface of the metal coin mold. Example

[0021] like Figure 2 As shown in the figure, the design algorithm of optical micro-nano pattern structure with visual inversion is used to calculate the filling method, stripe filling spacing and stripe filling direction of the micro-nano pattern structure according to the target pattern and the color rendering effect. The light and dark inversion effect is best when the stripe filling directions of adjacent patterns are 90° vertical. Therefore, in order to pursue the best light and dark inversion color rendering effect, the pattern design should be carried out as much as possible according to the 90° vertical stripe filling direction. Example

[0022] like Figure 3As shown, the micro-nano pattern structure is processed by ultrafast laser, and the laser beam 2 emitted by the laser 1 is guided to the galvanometer 5 through the reflector A3 and the reflector B4, and then focused to the surface of the metal coin mold 7 to be processed through the focusing field lens 6 to process the micro-nano pattern structure. Among them, the movement of the laser beam 2 on the surface of the metal coin mold 7 to be processed is controlled by the galvanometer 5, so as to realize the processing of the micro-nano pattern structure in different areas on the surface of the metal coin mold 7. Example

[0023] like Figure 4 As shown in (a), a Huari 65W1035nm femtosecond laser is used, with a single pulse energy of >80μJ and a Scanlab three-dimensional motion galvanometer. Stainless steel is selected as the processing material, the laser power is 90%, the laser frequency is 4000kHz, the laser pulse width is 2ns, the scanning speed is 3000m / s, and the micro-nano pattern structure is a straight stripe with a spacing of 46.09μm, a line width of 19.64μm, a depth of 4.50μm, and the stripe filling direction of adjacent patterns is 90°. The above process method has an excellent visual light and dark reversal effect, and the visual light and dark are reversed when the observation angle is changed. Example

[0024] like Figure 4 As shown in (b), a Huari 65W1035nm femtosecond laser is used, with a single pulse energy of >80μJ and a Scanlab three-dimensional motion galvanometer. Stainless steel is selected as the processing material, the laser power is 45%, the laser frequency is 1500kHz, the laser pulse width is 9ns, the scanning speed is 1500m / s, and the micro-nano pattern structure is a straight stripe with a spacing of 45.45μm, a line width of 28.95μm, a depth of 6.50μm, and the stripe filling direction of adjacent patterns is 90°. The above process method has an excellent visual light and dark reversal effect, and the visual light and dark are reversed when the observation angle is changed.

Claims

1. A process for preparing metal coins and stamps with visual reversal for anti-counterfeiting. It is characterized in that The steps include: Step 1: Determine the visual light-dark reversal effect of the target pattern; Step 2: Use the design method of visual inversion optical micro-nano pattern structure to calculate and optimize the grayscale values ​​of different areas of the target pattern, and determine the width, depth, filling spacing, and filling direction of the filling stripes in different areas of the target pattern according to the grayscale values; Step 3: Polish the surface of the metal coin mold to be processed and clean it to ensure that the surface is smooth and free of foreign matter; Step 4: Determine the laser power, pulse width, repetition frequency, and scanning speed of laser processing according to the target pattern to be processed and the visual light and dark reversal effect; Step 5: Use a laser processing system to process the above-mentioned micro-nano pattern structure with visual light and dark reversal effect on the surface of the metal coin mold.

2. According to claim 1, a method for producing metal coins and stamps with visual reversal anti-counterfeiting properties, It is characterized in that The filling stripes described in step 2 are linear arrays. According to the different visual effects of the light and dark reversal of the target pattern, the width, depth, filling spacing, and filling direction of the straight lines in different areas are different.

3. According to claim 2, a method for preparing metal coins and stamps with visual reversal for anti-counterfeiting, It is characterized in that The width of the straight line ranges from 15 to 50 μm, the depth ranges from 2 to 10 μm, the filling spacing ranges from 15 to 50 μm, and the filling direction ranges from 0 to 180°.

4. The image visual reversal anti-counterfeiting preparation process for metal coins and stamps according to claim 2, It is characterized in that The angle between the adjacent area filling straight lines is 90°.

5. According to claim 1, a method for producing metal coins and stamps with visual reversal anti-counterfeiting properties, It is characterized in that The laser power adjustment range described in step 4 is 20 to 60 W, the pulse width adjustment range is 1 to 9 ns, the repetition frequency adjustment range is 500 to 5000 kHz, and the scanning speed range is 1000 to 3000 mm / s.

6. The image visual reversal anti-counterfeiting preparation process for metal coins and stamps according to claim 5, It is characterized in that The repetition frequency, scanning speed and pulse width need to match each other so that the laser spot overlap rate is greater than 1 to avoid the occurrence of optical diffraction stripes and surface pitting.

7. The image visual reversal anti-counterfeiting preparation process for metal coins and stamps according to claim 1, It is characterized in that The laser processing system described in step 5 uses a femtosecond laser with a wavelength of 1035nm, a single pulse energy of >80μJ, and an adjustable pulse width.

8. The image visual reversal anti-counterfeiting preparation process for metal coins and stamps according to claim 1, It is characterized in that Processing the above-mentioned micro-nano pattern structure with visual light and dark reversal effect on the surface of the metal coin mold as described in step 5 is copied to the surface of the metal coin through embossing technology, so that the metal coin presents a visual light and dark reversal effect.

Citation Information

Patent Citations

  • Metal coin or stamp with DOE (Diffraction Optical Element) anti-counterfeit pattern and manufacturing method thereof

    CN106054294A

  • Laser sand blasting methods applied to precious metal commemorative coin

    CN109848570A

  • Metal surface coloring and frosting machining method

    CN111531279A

  • Multi-strip movable white light column anti-counterfeit label and printing method thereof

    CN115416412A

  • Method and apparatus for processing chip based on deep learning

    US20220152742A1