Semiconductor device, manufacturing method thereof and electronic equipment

By forming a high-doped first and second regions in the semiconductor device and achieving low doping in the channel region, the problems of carrier utilization efficiency and contact resistance of traditional junction-free field effect transistors are solved, and the process flow is simplified , improve device performance and stability.

CN118919556APending Publication Date: 2024-11-08BEIJING SUPERSTRING ACAD OF MEMORY TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310506326.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-06
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Traditional junction-free field effect transistors are difficult to fully utilize carrier concentrations under high doping concentrations, and source-drain contacts with low doping concentrations show high contact resistance. The existing multiple ion implantation technology is complex and may lead to crystal structure damage. , affects device performance.

Method used

By forming a highly doped first and second regions on the semiconductor column and achieving low doping in the channel region, using doped layer annealing and etching techniques, a lossless and highly doped region structure is formed to reduce contact resistance.

Benefits of technology

It realizes a lossless and highly doped region structure, reduces contact resistance, improves device performance, simplifies process flow, and enhances device stability and controllability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919556A_ABST
    Figure CN118919556A_ABST
Patent Text Reader

Abstract

A semiconductor device and a manufacturing method thereof, and an electronic apparatus, the semiconductor device comprising: at least one transistor disposed on a substrate, the transistor comprising: a semiconductor column extending in a direction perpendicular to the substrate, the semiconductor column comprising a channel region, and a first region and a second region respectively disposed at two sides of the channel region, the surface of the first area and the surface of the second area are lossless, the doping concentration of the side wall of a channel area is smaller than that of the side wall of the first area and that of the side wall of the second area, the orthographic projection of the channel area on the substrate is located in the orthographic projection of the first area on the substrate, and the orthographic projection of the channel area on the substrate is smaller than that of the first area. And the first region is located in the orthographic projection of the second region on the substrate. According to the scheme provided by the embodiment of the invention, the lossless first region and the lossless second region are provided, high doping of the first region and the second region and low doping of the channel region are realized, the performance of the device is improved, and the stability of the device is enhanced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present disclosure relate to but are not limited to semiconductor technology, and in particular to a semiconductor device and a manufacturing method thereof, and an electronic device. Background Art

[0002] Junctionless Field Effect Transistor (JLT) has been proposed as an alternative to conventional Metal Oxide Semiconductor Field Effect Transistor (MOSFET) to alleviate the technical challenges faced by conventional transistors due to feature size scaling. Vertical integration of nanowires offers many advantages, such as the ease with which nanowires can be integrated into higher density arrays. Under uniform doping of the source, drain and channel of vertical junctionless transistors, highly doped JLTs provide large currents in their on state, but may not be able to fully deplete their large carrier concentrations. With lower doping concentrations, the source and drain contacts will show higher contact resistance. High doping of the source and drain and low doping of the channel can be achieved by using multiple ion implantation techniques. The steps are relatively complicated, and it is very difficult to achieve high doping concentrations at the bottom of the silicon pillar and less damage to the silicon crystal structure. The high lattice damage caused by the implanted ions may completely destroy the crystal structure and turn it into a disordered amorphous region. The damage cannot be eliminated during the annealing process, resulting in poor recrystallization, which causes a decrease in carrier concentration and reduced impurity activation, resulting in an increase in bottom contact resistance and reduced transistor performance. Summary of the invention

[0003] The following is a summary of the subject matter described in detail herein. This summary is not intended to limit the scope of the claims.

[0004] The embodiments of the present disclosure provide a semiconductor device and a manufacturing method thereof, and an electronic device, which simplify the process and improve the device performance.

[0005] An embodiment of the present disclosure provides a semiconductor device, comprising: at least one transistor arranged on a substrate, the transistor comprising: a semiconductor column extending in a direction perpendicular to the substrate, the semiconductor column comprising a channel region and a first region and a second region respectively arranged on both sides of the channel region, wherein the second region is arranged on the side of the first region facing the substrate, the surfaces of the first region and the second region are intact, the doping concentration of the sidewall of the channel region is less than the doping concentration of the sidewall of the first region, and less than the doping concentration of the sidewall of the second region, and the orthographic projection of the channel region on the substrate is located within the orthographic projection of the first region on the substrate, and is located within the orthographic projection of the second region on the substrate.

[0006] In some embodiments, the transistor further includes a gate electrode surrounding the channel region, and a gate insulation layer disposed between the gate electrode and the channel region, the gate insulation layer surrounding the channel region and the first region, and an isolation layer disposed between the gate insulation layer and the first region.

[0007] In some embodiments, the channel region, the first region, and the second region are an integrated structure.

[0008] In some embodiments, a doping concentration of a sidewall of the first region is the same as a doping concentration of a sidewall of the second region.

[0009] In some embodiments, in the semiconductor column, a change in doping concentration of the first region from the surface to the interior is consistent with a change in doping concentration of the second region from the surface to the interior.

[0010] An embodiment of the present disclosure provides an electronic device, comprising the semiconductor device described in any of the above embodiments.

[0011] An embodiment of the present disclosure provides a method for manufacturing a semiconductor device, wherein the semiconductor device includes at least one transistor disposed on a substrate, wherein the transistor includes: a semiconductor column extending in a direction perpendicular to the substrate, wherein the semiconductor column includes a channel region and a first region and a second region disposed on both sides of the channel region, respectively, wherein the second region is disposed on a side of the first region facing the substrate, and the manufacturing method includes:

[0012] Forming at least one semiconductor column extending in a direction perpendicular to the substrate on a substrate, wherein the semiconductor column comprises a quasi-channel region, and a first region and a second region disposed on both sides of the quasi-channel region;

[0013] forming a doping layer covering the semiconductor column, performing thermal annealing so that dopants in the doping layer are doped into the semiconductor column, and removing the doping layer;

[0014] exposing the quasi-channel region;

[0015] The semiconductor column is thinned in the quasi-channel region along a direction parallel to the substrate to form the channel region, wherein the orthographic projection of the channel region on the substrate is located within the orthographic projection of the first region on the substrate, and is located within the orthographic projection of the second region on the substrate.

[0016] In some embodiments, after forming the doping layer covering the semiconductor pillar and before thermal annealing, the method further includes forming a protective layer covering the doping layer;

[0017] Before removing the doping layer, the method further includes removing the protective layer.

[0018] In some embodiments, thinning the semiconductor column in the quasi-channel region along a direction parallel to the substrate includes: thinning the semiconductor column in the quasi-channel region along a direction parallel to the substrate by dry etching; or, performing an oxidation process in the quasi-channel region to form a semiconductor oxide, and etching away the semiconductor oxide to thin the semiconductor column.

[0019] In some embodiments, forming a doping layer covering the semiconductor pillar includes: forming a doping layer covering the semiconductor pillar by atomic layer deposition.

[0020] The disclosed embodiments include a semiconductor device and a manufacturing method thereof, and an electronic device, wherein the semiconductor device includes: at least one transistor disposed on a substrate, the transistor includes: a semiconductor column extending in a direction perpendicular to the substrate, the semiconductor column including a channel region and a first region and a second region disposed on both sides of the channel region, respectively, wherein the second region is disposed on the side of the first region facing the substrate, the surfaces of the first region and the second region are lossless, the doping concentration of the sidewall of the channel region is less than the doping concentration of the first region, and less than the doping concentration of the sidewall of the second region, and the orthographic projection of the channel region on the substrate is located within the orthographic projection of the first region on the substrate, and is located within the orthographic projection of the second region on the substrate. The solution provided in this embodiment provides a lossless and highly doped first region, a second region, and a low-doped channel region, which can reduce contact resistance and improve device performance.

[0021] Other features and advantages of the present invention will be described in the following description, and partly become apparent from the description, or understood by practicing the present invention. The objects and advantages of the present invention can be realized and obtained by the structures particularly pointed out in the description and the drawings.

[0022] Other aspects will be apparent upon reading and understanding the drawings and detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The accompanying drawings are used to provide a further understanding of the technical solution of the present disclosure and constitute a part of the specification. Together with the embodiments of the present disclosure, they are used to explain the technical solution of the present disclosure and do not constitute a limitation on the technical solution.

[0024] Figure 1A A schematic cross-sectional view of a semiconductor device provided as an exemplary embodiment;

[0025] Figure 1B A schematic plan view of a semiconductor device provided for an exemplary embodiment;

[0026] Figure 2A cross-sectional view of a hard mask along a direction perpendicular to a substrate provided for an exemplary embodiment;

[0027] Figure 3 A cross-sectional view along a direction perpendicular to a substrate after forming a semiconductor pillar provided for an exemplary embodiment;

[0028] Figure 4 A cross-sectional view along a direction perpendicular to the substrate after forming a doping layer and a protective layer provided for an exemplary embodiment;

[0029] Figure 5A A cross-sectional view of a semiconductor column after doping along a direction perpendicular to a substrate provided by an exemplary embodiment;

[0030] Figure 5B A schematic diagram of semiconductor column doping distribution provided for an exemplary embodiment;

[0031] Figure 6 A cross-sectional view along a direction perpendicular to the substrate after forming a first insulating layer provided for an exemplary embodiment;

[0032] Figure 7 A cross-sectional view along a direction perpendicular to the substrate after exposing the first region provided for an exemplary embodiment;

[0033] Figure 8 A cross-sectional view along a direction perpendicular to the substrate after forming an isolation layer provided for an exemplary embodiment;

[0034] Fig. 9 A cross-sectional view along a direction perpendicular to the substrate after exposing the quasi-channel region provided for an exemplary embodiment;

[0035] Fig.10 A cross-sectional view along a direction perpendicular to the substrate after forming a channel region provided for an exemplary embodiment;

[0036] Fig.11 A cross-sectional view along a direction perpendicular to the substrate after a gate insulating layer is formed provided for an exemplary embodiment;

[0037] Fig.12 A cross-sectional view along a direction perpendicular to the substrate after a gate electrode is formed provided for an exemplary embodiment;

[0038] Fig.13 A flow chart of a method for manufacturing a semiconductor device is provided for an exemplary embodiment. DETAILED DESCRIPTION

[0039] The embodiments of the present disclosure will be described in detail below in conjunction with the accompanying drawings. In the absence of conflict, the embodiments of the present disclosure and the features in the embodiments can be combined with each other arbitrarily.

[0040] Unless otherwise defined, technical or scientific terms used in the present disclosure should have the common meanings understood by one of ordinary skill in the art to which the present invention belongs.

[0041] The embodiments of the present disclosure are not necessarily limited to the dimensions shown in the drawings, and the shapes and sizes of the components in the drawings do not reflect the true proportions. In addition, the drawings schematically show ideal examples, and the embodiments of the present disclosure are not limited to the shapes or values ​​shown in the drawings.

[0042] The ordinal numbers such as “first”, “second” and “third” in the present disclosure are provided to avoid confusion among constituent elements and do not indicate any order, quantity or importance.

[0043] In the present disclosure, for the sake of convenience, the words and phrases indicating the orientation or positional relationship, such as "middle", "upper", "lower", "front", "back", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., are used to illustrate the positional relationship of the constituent elements with reference to the drawings. This is only for the convenience of describing the present specification and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operate in a specific orientation, and therefore cannot be understood as a limitation of the present disclosure. The positional relationship of the constituent elements is appropriately changed according to the direction in which each constituent element is described. Therefore, it is not limited to the words and phrases described in the disclosure and can be appropriately replaced according to the circumstances.

[0044] In the present disclosure, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate, or the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present disclosure can be understood according to specific circumstances.

[0045] In the present disclosure, a transistor refers to an element including at least three terminals: a gate electrode, a drain electrode, and a source electrode. A transistor has a channel region between a drain electrode (drain electrode terminal, drain region, or drain electrode) and a source electrode (source electrode terminal, source region, or source electrode), and current can flow through the drain electrode, the channel region, and the source electrode. In the present disclosure, a channel region refers to a region through which current flows.

[0046] In the present disclosure, "parallel" means approximately parallel or almost parallel, for example, the angle formed by two straight lines is greater than -10° and less than 10°, and therefore, the angle is greater than -5° and less than 5°. In addition, "perpendicular" means approximately perpendicular, for example, the angle formed by two straight lines is greater than 80° and less than 100°, and therefore, the angle is greater than 85° and less than 95°.

[0047] The phrase “the orthographic projection of B is within the range of the orthographic projection of A” in the present disclosure means that the boundary of the orthographic projection of B falls within the boundary of the orthographic projection of A.

[0048] In the embodiments of the present disclosure, "A and B are an integrated structure" may mean that there is no obvious boundary interface such as a fault or gap in the microstructure. Generally, a film layer patterned to form a connection is an integrated structure. For example, A and B use the same material to form a film layer and form a structure with a connection relationship at the same time through the same patterning process.

[0049] In the disclosed embodiments, lossless and conformal high doping of the source and drain regions is achieved by depositing a doping layer and annealing, and low doping of the channel region is achieved by removing the high doping region on the surface by etching.

[0050] Figure 1A FIG. 1 is a cross-sectional view of a semiconductor device provided by an exemplary embodiment along a direction perpendicular to the substrate. Figure 1A As shown, this embodiment provides a semiconductor device, which may include: at least one transistor disposed on a substrate 1, the transistor including: a semiconductor column 10 extending in a direction perpendicular to the substrate 1, the semiconductor column 10 including a channel region 11 and a first region 12 and a second region 13 disposed on both sides of the channel region 11, wherein the second region 13 is disposed on the side of the first region 11 facing the substrate 1, the surfaces of the first region 12 and the second region 13 are intact, the doping concentration of the sidewall of the channel region 11 is less than the doping concentration of the sidewall of the first region 12, and less than the doping concentration of the sidewall of the second region 13, and the orthographic projection of the channel region 11 on the substrate 1 is located within the orthographic projection of the first region 12 on the substrate 1, and is located within the orthographic projection of the second region 13 on the substrate 1. That is, the semiconductor column 10 forms a dumbbell-shaped structure with large ends and a small middle.

[0051] The semiconductor column 10 has a main surface, which is a side surface or a side wall of the semiconductor column, and the side surface may be perpendicular to the substrate 1. The surface of the first region 12 and the second region 13 is intact, which means that the side wall of the first region 12 is intact, and the side wall of the second region 13 is intact. The second region 13, the channel region 11 and the first region 12 are arranged in sequence along the extension direction of the semiconductor column 10. The channel region 11 can be roughly distinguished from the first region 12 and the second region 13 by the position of the gate electrode, or can be roughly distinguished by the different conductivity of the first region 12 and the second region 13 from the channel region 11.

[0052] The solution provided in this embodiment provides a lossless and highly doped first region, a second region, and a low-doped channel region, which can reduce contact resistance and improve device performance.

[0053] The term "damageless" in this embodiment means that there is no lattice damage caused by ion implantation or the like, and damage caused by conventional photolithography or the like may exist.

[0054] In an exemplary embodiment, the conductivity type of the first region 12 and the second region 13 may be n-type or p-type. The first region 12 may be a source region, and the second region 13 may be a drain region, or the first region 12 may be a drain region, and the second region 13 may be a source region.

[0055] In an exemplary embodiment, the cross-section of the channel region 11 in a direction parallel to the substrate 1 may be substantially the same in size and shape at different locations. It can be understood that the sidewall of the semiconductor column 10 is a curved surface with a continuous and smooth surface, and the cross-sections at different locations of the curved surface have similar shapes, but may differ in size. For example, in some embodiments, the cross-sectional area near the top of the semiconductor column 10 (the end surface away from the substrate 1) is smaller than the cross-sectional area away from the top.

[0056] In an exemplary embodiment, the size and shape of the cross section of the first region 12 in a direction parallel to the substrate 1 at different positions may be substantially the same.

[0057] In an exemplary embodiment, the size and shape of the cross section of the second region 13 in a direction parallel to the substrate 1 at different positions may be substantially the same.

[0058] In an exemplary embodiment, the first region 12, the second region 13, and the channel region 11 may be an integrated structure. That is, the semiconductor pillar 10 may be formed by a single patterning process.

[0059] In an exemplary embodiment, the transistor may further include a gate electrode 21 surrounding the channel region 11 , and a gate insulating layer 14 disposed between the gate electrode 21 and the channel region 11 , and the gate insulating layer 14 may surround the channel region 11 and the first region 12 .

[0060] In an exemplary embodiment, an isolation layer 45 may be disposed between the gate insulating layer 14 and the first region 12 .

[0061] In an exemplary embodiment, the doping concentration of the sidewall of the first region 12 and the doping concentration of the sidewall of the second region 13 may be the same. The first region 12 and the second region 13 may be doped by annealing after depositing the doping layer, so that the doping concentration of the sidewall of the first region 12 and the doping concentration of the sidewall of the second region 13 are the same. Here, the same may be substantially the same.

[0062] In an exemplary embodiment, in the semiconductor column 10, the change in the doping concentration of the first region 12 from the surface to the inside is consistent with the change in the doping concentration of the second region 13 from the surface to the inside. In this embodiment, doping can be achieved by annealing the doping layer, so that the change in the doping concentration of the first region 12 and the second region 13 is consistent, that is, the relationship between the depth from the surface and the doping concentration is consistent, and the doping concentration decreases as the depth from the surface increases, and the doping concentration is basically consistent at the same depth.

[0063] In an exemplary embodiment, the semiconductor device may include a plurality of transistors distributed in an array. The semiconductor device may include a plurality of vertical channel transistors distributed in an array along a first direction X and a second direction Y, a plurality of word lines 20 extending along the first direction X, and a plurality of bit lines 30 extending along the second direction Y. The gate electrodes 21 of transistors in the same row distributed along the first direction X are connected to form a word line 20, and the second regions 13 of transistors in the same column distributed along the second direction Y are connected to the same bit line 30. The first direction X and the second direction Y may intersect.

[0064] In an exemplary embodiment, the first direction X and the second direction Y may be perpendicular.

[0065] In an exemplary embodiment, the bit line 30 may be disposed between the substrate 1 and the transistor. The bit line 30 may be in contact with the second region 13.

[0066] In an exemplary embodiment, the first direction X may be parallel to the substrate 1 , and the second direction Y may be parallel to the substrate 1 .

[0067] In an exemplary embodiment, the plurality of word lines 20 may be distributed along the second direction Y at intervals, and the plurality of bit lines 30 may be distributed along the first direction X at intervals.

[0068] The above transistors can be connected to capacitors to form a 1T1C storage structure, etc., but are not limited to this, and can be connected to other transistors to form a 2T0C storage structure, etc.

[0069] The technical solution of this embodiment is further explained below through the preparation process of the semiconductor device of this embodiment. The "photolithography process" mentioned in this embodiment includes coating film layer, mask exposure and development, which is a mature preparation process in the relevant technology. Deposition can adopt known processes such as sputtering, evaporation, chemical vapor deposition, coating can adopt known coating processes, and etching can adopt known methods, which are not specifically limited here. In the description of this embodiment, it should be understood that "thin film" refers to a thin film made of a certain material on a substrate using a deposition or coating process. If the "thin film" does not require a composition process or a photolithography process during the entire production process, the "thin film" can also be called a "layer". If the "thin film" still requires a composition process or a photolithography process during the entire production process, it is called a "thin film" before the composition process and a "layer" after the composition process. The "layer" after the composition process or the photolithography process contains at least one "pattern".

[0070] In an exemplary embodiment, a process for manufacturing a semiconductor device may include:

[0071] 1) Providing a substrate, depositing a multi-layer hard mask on the substrate, such as Figure 2 As shown, Figure 2 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the hard mask is deposited.

[0072] The base plate may include a substrate 1 and a semiconductor layer 2 disposed on the substrate 1 .

[0073] The multi-layer hard mask may include a first hard mask layer 41 , a second hard mask layer 42 , and a third hard mask layer 43 which are sequentially stacked on the semiconductor layer 2 .

[0074] In an exemplary embodiment, the substrate 1 may be a low-K dielectric layer, i.e., a dielectric layer with a dielectric constant K<3.9, such as any one or more of silicon nitride (SiNx), silicon oxide (SiOx), silicon oxynitride (SiON), and silicon carbide (SiC).

[0075] In an exemplary embodiment, the first hard mask layer 41 may be silicon nitride (SiN), the second hard mask layer 42 and the third hard mask layer 43 may be titanium nitride (TiN), SiN, silicon dioxide (SiO 2 )wait.

[0076] In an exemplary embodiment, the semiconductor layer 2 may include, for example, silicon (Si). However, this is only an example, and the semiconductor 2 may include, for example, a Group IV semiconductor material (such as germanium (Ge), silicon germanium (SiGe) or silicon carbide (SiC)), a Group III-V semiconductor material (such as gallium arsenide (GaAs), indium arsenide (InAs) or indium phosphide (InP)), an oxide semiconductor, a nitride semiconductor or a nitride oxide semiconductor, etc.

[0077] 2) forming a semiconductor column 10;

[0078] The forming of the semiconductor pillars 10 may include: using a self-aligned double-layer mask (double pattern) lithography technique to etch out a plurality of semiconductor pillars 10 extending in a direction perpendicular to the substrate 1, such as Figure 3 As shown, Figure 3 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the semiconductor pillar 10 is formed. A sacrificial layer 44 formed by a first hard mask layer 41 is disposed on the side of the semiconductor pillar 10 away from the substrate 1 .

[0079] The embodiments of the present disclosure are not limited thereto, and other etching techniques may be used to form the semiconductor pillar 10 .

[0080] At this time, along the extension direction of the semiconductor column 10, the semiconductor column 10 may include a first region 12, a quasi-channel region 11' and a second region 13. The quasi-channel region 11' is located between the first region 12 and the second region 13, and the second region 13 is arranged on the side of the quasi-channel region 11' facing the substrate 1.

[0081] 3) forming a doping layer 31 and a protective layer 32;

[0082] The forming of the doping layer 31 and the protective layer 32 may include: depositing a doping layer thin film and a protective layer thin film on the substrate 1 having the aforementioned structure in sequence to form the doping layer 31 and the protective layer 32, such as Figure 4 As shown, Figure 4 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the doping layer 31 and the protection layer 32 are formed. The doping layer 31 may completely cover the semiconductor pillar 10 and the sacrificial layer 44 , and the protection layer 32 may completely cover the doping layer 31 .

[0083] In an exemplary embodiment, the doping layer film and the protection layer film may be deposited by an atomic layer deposition (ALD) method.

[0084] In an exemplary embodiment, the doping layer film may be an oxide film containing a dopant, such as boron oxide (boron trioxide (B 2 O 3) etc.), phosphorus oxides (phosphorus pentoxide (P 2 O 5 ) etc.), but not limited thereto, and may be other substances according to doping requirements.

[0085] In an exemplary embodiment, the doping layer thin film may include a mixture of an oxide film containing a dopant and silicon oxide, such as B 2 O 3 and silicon dioxide (SiO 2 ), or, P 2 O 5 and SiO 2 Compared with using only an oxide film containing a dopant to generate the doping layer 31, the growth process of the doping layer 31 generated by using the mixture is more stable.

[0086] In an exemplary embodiment, the thickness of the doping layer 31 is, for example, 3 nm to 15 nm, but is not limited thereto and can be other thicknesses and can be changed according to the requirements of the doping concentration. The thickness of the doping layer 31 is the thickness of the deposited doping film.

[0087] In an exemplary embodiment, the protective layer film may be silicon oxide, silicon nitride, antimony oxide, etc., such as SiO 2 , SiN, antimony pentoxide (Sb 2 O 5 )wait.

[0088] The protective layer 32 can prevent the doping layer 31 from absorbing moisture and reduce the evaporation of the doping layer 31 during the subsequent annealing process. However, the embodiment of the present disclosure is not limited thereto, and in another exemplary embodiment, the protective layer 32 may not be formed.

[0089] 4) doping the semiconductor column 10;

[0090] The step of doping the semiconductor column 10 may include:

[0091] Performing thermal annealing to diffuse the dopant in the doping layer 31 into the semiconductor pillar 10;

[0092] Remove the protective layer 32 and the remaining doping layer 31, such as Figure 5A As shown, Figure 5A It is a cross-sectional view along a direction perpendicular to the substrate 1 after the semiconductor column 10 is doped.

[0093] In an exemplary embodiment, the thermal annealing may be rapid thermal annealing (RTA), flash lamp annealing (FLA), microwave annealing, etc.

[0094] In an exemplary embodiment, when performing RTA annealing, the annealing temperature may be 850° C. to 1050° C. The annealing time may be less than or equal to 20 seconds. When using FLA annealing, the energy density may be 120 J / cm3. 2 ) to 150J / cm 2 , the annealing time is less than or equal to 20 milliseconds (ms).

[0095] In an exemplary embodiment, the annealing atmosphere may be 5 mbar to 5 bar oxygen (O 2 ) or nitrogen (N 2 ). However, the embodiments of the present disclosure are not limited thereto, and other annealing atmospheres may be used.

[0096] After annealing, the dopant concentration distribution in the semiconductor pillar 10 is gradually reduced from the surface to the middle. 2 O 5 and SiO 2 As an example, in this embodiment, the dopant is P 2 O 5 and SiO 2 When the annealing method is RTP (Rapid Thermal Processing, also known as RTA), the annealing temperature is 950°C and the annealing time is 5s. Figure 5B As shown in FIG. 1 , the concentration of phosphorus (P) decreases as the depth from the surface increases. In this embodiment, under the same doping conditions, the concentration of phosphorus (P) decreases with the depth from the surface. 2 O 5 As the protective layer 32, at the same depth, the concentration of P without the protective layer may be greater than the concentration of P with the protective layer 32. However, it is not limited thereto. In other embodiments, at the same depth, when there is no protective layer, the concentration of the dopant after doping may be less than the concentration of the dopant with the protective layer 32. Figure 5B Also shown in FIG. 1 is the doping concentration of antimony (Sb), which decreases with increasing depth from the surface.

[0097] 5) forming a first insulating layer 3;

[0098] The forming of the first insulating layer 3 may include: depositing a first insulating film on the substrate 1 having the aforementioned structure, and grinding the film to form the first insulating layer 3, such as Figure 6 As shown, Figure 6 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the first insulating layer 3 is formed.

[0099] In an exemplary embodiment, the first insulating film may be any one or more of silicon nitride (SiNx), silicon oxide (SiOx), silicon oxynitride (SiON), and silicon carbide (SiC). 2 .

[0100] In an exemplary embodiment, the first insulating layer 3 can be smoothed by chemical mechanical polishing (CMP). After smoothing, the first insulating layer 3 is flush with the sacrificial layer 44, that is, the distance between the surface of the first insulating layer 3 away from the substrate 1 and the substrate 1 is the same as the distance between the surface of the sacrificial layer 44 away from the substrate 1 and the substrate 1.

[0101] 6) exposing the first region 12;

[0102] Exposing the first region 12 may include: etching the first insulating layer 3 to expose the first region 12 of the semiconductor column 10. Figure 7 As shown, Figure 7 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the first region 12 is exposed.

[0103] In an exemplary embodiment, etching the first insulating layer 3 may include: etching the first insulating layer 3 by a wet method.

[0104] 7) forming an isolation layer 45;

[0105] The forming of the isolation layer 45 may include: depositing an isolation film on the substrate 1 forming the aforementioned structure, etching and removing the isolation film covering the first insulating layer 3, and forming the isolation layer 45. Figure 8 As shown, Figure 8 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the isolation layer 45 is formed. The isolation layer 45 covers the sidewall of the second region 12 and protects the second region 12 together with the sacrificial layer 44 in the subsequent preparation process.

[0106] In an exemplary embodiment, the isolation film is, for example, SiN.

[0107] 8) exposing the sidewalls of the quasi-channel region 11';

[0108] Exposing the sidewall of the quasi-channel region 11' may include: etching the first insulating layer 3 to expose the sidewall of the quasi-channel region 11'. Fig. 9 As shown, Fig. 9 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the sidewall of the quasi-channel region 11 ′ is exposed.

[0109] In an exemplary embodiment, the etching of the first insulating layer 3 may be performed by wet etching of the first insulating layer 3 .

[0110] 9) removing a preset thickness from the surface of the semiconductor pillar 10 along the quasi-channel region 11' to form a channel region 11;

[0111] The dopant concentration distribution in the semiconductor column 10 is gradually reduced from the surface to the middle. By removing a certain thickness of the surface of the semiconductor column 10 and using the newly exposed surface as the sidewall of the channel region 11, a channel region 11 with a lower doping concentration can be achieved.

[0112] The removing of a predetermined thickness from the surface of the semiconductor pillar 10 along the quasi-channel region 11' to form the channel region 11 may include:

[0113] A) using a dry etching method to etch the semiconductor column 10 in the quasi-channel region 11', etching away the surface layer of the semiconductor column 10 with a high doping concentration by a preset thickness to form the channel region 11;

[0114] B) using thermal oxidation growth, consuming the semiconductor material in the quasi-channel region 11' of the semiconductor column 10 by oxidation growth to generate semiconductor oxide, removing the generated semiconductor oxide, achieving the effect of thinning the semiconductor column 10, and forming the channel region 11, such as Fig.10 As shown, Fig.10 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the channel region 11 is formed.

[0115] For example, when the semiconductor pillar comprises Si, by thermally oxidizing SiO 2 Growth, SiO 2 The Si in the quasi-channel region 11' is consumed during the growth process, and the grown SiO is subsequently removed. 2 , by controlling SiO 2 The thickness of Si is consumed during the growth, thereby controlling the doping concentration of the channel region 11 .

[0116] At this time, the semiconductor pillar 10 forms a dumbbell-shaped structure with large ends and a small middle. That is, the orthographic projection of the channel region 11 falls within the orthographic projection of the first region 12 on the substrate 1 , and falls within the orthographic projection of the second region 13 on the substrate 1 .

[0117] 10) forming a gate insulating layer 14;

[0118] The forming of the gate insulating layer 14 may include: depositing a gate insulating film on the substrate 1 forming the aforementioned structure, forming a gate insulating layer 14 surrounding the sidewalls of the channel region 11 and the sidewalls of the first region 12, and providing an isolation layer 45 between the gate insulating layer 14 and the first region 12. Fig.11 As shown, Fig.11 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the gate insulating layer 14 is formed.

[0119] In an exemplary embodiment, the gate insulating layer 14 may include a High-K dielectric material, including but not limited to at least one of the following: a single-layer structure or a multi-layer structure of at least one of silicon oxide, aluminum oxide, silicon nitride, hafnium oxide, and silicon oxynitride.

[0120] 11) forming a gate electrode 21;

[0121] The forming of the gate electrode 21 may include:

[0122] A gate electrode film is deposited on the substrate 1 forming the above structure, and the gate electrode film surrounding the first region 12 is etched away to form a gate electrode 21 surrounding the channel region 11 ; the gate electrodes 21 of transistors in the same row can be connected to form a word line 20 .

[0123] The sacrificial layer 44 is removed by etching to expose the top of the semiconductor pillar 10. Fig.12 As shown, Fig.12 It is a cross-sectional view along a direction perpendicular to the substrate 1 after the gate electrode 21 is formed.

[0124] In an exemplary embodiment, the gate electrode film surrounding the first region 12 may be removed by wet etching.

[0125] The solution provided in this embodiment is to achieve high doping in the first region and the second region by annealing the deposited doping layer, and to obtain a low-doped channel region by etching the semiconductor column located between the first region and the second region. No additional graphic process is added, and high source and drain doping and low channel region doping can be achieved without damaging the first region and the second region, thereby achieving conformal and undamaged first and second regions, improving device performance and enhancing device stability. In addition, the doping concentration of the channel can be conveniently controlled by controlling the etching degree of the semiconductor column, and the process is simple. In addition, the highly doped first and second regions can reduce contact resistance, thereby reducing power consumption, and are easier to turn off and turn on transistors than transistors with consistent doping concentrations in the first, second and channel regions, thereby enhancing device controllability.

[0126] The present disclosure also provides an electronic device, including the semiconductor device of the above embodiment. The electronic device may be a storage device, a smart phone, a computer, a tablet computer, an artificial intelligence device, a wearable device, or a mobile power supply. The storage device may include a memory in a computer, etc., which is not limited here.

[0127] Fig.13 The flowchart of the method for manufacturing a semiconductor device provided by the embodiment of the present disclosure is as follows. Fig.13As shown, an embodiment of the present disclosure provides a method for manufacturing a semiconductor device, wherein the semiconductor device includes at least one transistor disposed on a substrate, wherein the transistor includes: a semiconductor column extending in a direction perpendicular to the substrate, wherein the semiconductor column includes a channel region and a first region and a second region disposed on both sides of the channel region, respectively, wherein the second region is disposed on a side of the first region facing the substrate, and the manufacturing method may include:

[0128] Step 1301, forming at least one semiconductor column extending in a direction perpendicular to the substrate on a substrate, wherein the semiconductor column comprises a quasi-channel region, and the first region and the second region respectively disposed on both sides of the quasi-channel region;

[0129] Step 1302, forming a doping layer covering the semiconductor pillar, performing thermal annealing so that dopants in the doping layer are doped into the semiconductor pillar, and removing the doping layer;

[0130] Step 1303, exposing the quasi-channel region, thinning the semiconductor column in the quasi-channel region along a direction parallel to the substrate to form the channel region, wherein the orthographic projection of the channel region on the substrate is located within the orthographic projection of the first region on the substrate, and the orthographic projection of the second region on the substrate is located within.

[0131] The manufacturing method of the semiconductor device provided in this embodiment realizes lossless high doping of the first region and the second region by forming a doping layer and annealing, and forms a low-doped channel region by etching away the high-doping region on the surface of the semiconductor column, without adding an additional patterning process, improving device performance and enhancing device stability. In addition, the doping concentration of the channel can be conveniently controlled by controlling the etching degree of the semiconductor column, and the process is simple. In addition, the highly doped first region and the second region can reduce the contact resistance, thereby reducing power consumption, and compared with the transistor with the same doping concentration in the first region, the second region and the channel region, it is easier to turn off and turn on the transistor, thereby increasing the controllability of the device.

[0132] In an exemplary embodiment, after forming the doping layer covering the semiconductor pillar and before thermal annealing, the method further includes forming a protective layer covering the doping layer;

[0133] Before removing the doping layer, the protective layer is also removed. The solution provided in this embodiment can prevent the doping layer from absorbing moisture and reduce the evaporation of the doping layer in the subsequent annealing process by providing the protective layer.

[0134] In an exemplary embodiment, thinning the semiconductor column in the quasi-channel region along a direction parallel to the substrate includes: thinning the semiconductor column in the quasi-channel region along a direction parallel to the substrate by dry etching; or, performing an oxidation process in the quasi-channel region to form a semiconductor oxide, and etching away the semiconductor oxide to thin the semiconductor column.

[0135] In an exemplary embodiment, forming a doping layer covering the semiconductor pillar includes: forming the doping layer covering the semiconductor pillar by atomic layer deposition.

[0136] In an exemplary embodiment, RTA, FLA or microwave annealing can be used, wherein when RTA is used for annealing, the annealing temperature can be 850°C to 1050°C, and the annealing time can be less than or equal to 20 seconds. When FLA is used for annealing, the energy density can be 120 J / cm 2 Up to 150J / cm 2 , annealing time is less than or equal to 20ms.

[0137] In an exemplary embodiment, when the annealing is performed, the annealing atmosphere may be 5 mbar to 5 bar of oxygen or nitrogen.

[0138] Although the embodiments disclosed in the present invention are as above, the contents described are only embodiments adopted to facilitate understanding of the present invention and are not intended to limit the present invention. Any technician in the field to which the present invention belongs can make any modifications and changes in the form and details of implementation without departing from the spirit and scope disclosed in the present invention, but the patent protection scope of the present invention shall still be subject to the scope defined in the attached claims.

Claims

1. A semiconductor device, It is characterized in that include: At least one transistor is arranged on a substrate, the transistor comprising: a semiconductor column extending in a direction perpendicular to the substrate, the semiconductor column comprising a channel region and a first region and a second region respectively arranged on both sides of the channel region, wherein the second region is arranged on the side of the first region facing the substrate, the surfaces of the first region and the second region are intact, the doping concentration of the sidewall of the channel region is less than the doping concentration of the sidewall of the first region, and less than the doping concentration of the sidewall of the second region, and the orthographic projection of the channel region on the substrate is located within the orthographic projection of the first region on the substrate, and is located within the orthographic projection of the second region on the substrate.

2. The semiconductor device according to claim 1, It is characterized in that The transistor further includes a gate electrode surrounding the channel region, and a gate insulating layer disposed between the gate electrode and the channel region, the gate insulating layer surrounding the channel region and the first region, and an isolation layer disposed between the gate insulating layer and the first region.

3. The semiconductor device according to claim 1, It is characterized in that The channel region, the first region, and the second region are an integrated structure.

4. The semiconductor device according to any one of claims 1 to 3, It is characterized in that The doping concentration of the sidewall of the first region is the same as the doping concentration of the sidewall of the second region.

5. The semiconductor device according to any one of claims 1 to 3, It is characterized in that In the semiconductor column, a change in doping concentration of the first region from the surface to the inside is consistent with a change in doping concentration of the second region from the surface to the inside.

6. An electronic device, It is characterized in that Comprising the semiconductor device according to any one of claims 1 to 5.

7. A method for manufacturing a semiconductor device, It is characterized in that The semiconductor device comprises at least one transistor disposed on a substrate, the transistor comprising: a semiconductor column extending in a direction perpendicular to the substrate, the semiconductor column comprising a channel region and a first region and a second region respectively disposed on both sides of the channel region, wherein the second region is disposed on a side of the first region facing the substrate, and the manufacturing method comprises: Forming at least one semiconductor column extending in a direction perpendicular to the substrate on a substrate, wherein the semiconductor column comprises a quasi-channel region, and the first region and the second region respectively disposed on both sides of the quasi-channel region; forming a doping layer covering the semiconductor column, performing thermal annealing so that dopants in the doping layer are doped into the semiconductor column, and removing the doping layer; exposing the quasi-channel region; The semiconductor column is thinned in the quasi-channel region along a direction parallel to the substrate to form the channel region, wherein the orthographic projection of the channel region on the substrate is located within the orthographic projection of the first region on the substrate, and is located within the orthographic projection of the second region on the substrate.

8. The method for manufacturing a semiconductor device according to claim 7, It is characterized in that After forming the doping layer covering the semiconductor column and before thermal annealing, the method further includes forming a protective layer covering the doping layer; Before removing the doping layer, the method further includes removing the protective layer.

9. The method for manufacturing a semiconductor device according to claim 7, It is characterized in that Thinning the semiconductor column in the quasi-channel region along a direction parallel to the substrate includes: thinning the semiconductor column in the quasi-channel region along a direction parallel to the substrate by dry etching; or, performing an oxidation process in the quasi-channel region to form a semiconductor oxide, and etching away the semiconductor oxide to thin the semiconductor column.

10. The method for manufacturing a semiconductor device according to any one of claims 7 to 9, It is characterized in that The forming of the doping layer covering the semiconductor column comprises: forming the doping layer covering the semiconductor column by atomic layer deposition.