Solar cell, manufacturing method thereof, photovoltaic module and photovoltaic system
The solar cell structure, with its full aluminum back surface coverage and perforated window design, solves the problem of missing aluminum back surface in the edge area, improves open-circuit voltage and conversion efficiency, and reduces costs.
Patent Information
- Application Number
- CN202411413077.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-11
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing solar cells lack an aluminum back field in the edge region, which weakens charge collection and affects open-circuit voltage and photoelectric conversion efficiency.
The design adopts an all-aluminum back surface field covering design, which covers the back surface of the battery except for the back electrode, and is connected to the back electrode through a hollow window. Combined with several independent sub-electrode pattern designs, the aluminum back surface field area is increased and the use of silver paste is reduced.
It improves the open-circuit voltage and photoelectric conversion efficiency of solar cells, reduces manufacturing costs, and avoids cell warping and deformation.
Smart Images

Figure CN118919580A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of photovoltaic technology, and in particular relates to a solar cell and a manufacturing method thereof, a photovoltaic module and a photovoltaic system. Background Art
[0002] Solar cells are mainly based on semiconductor materials. Their working principle is to use the photovoltaic effect after photoelectric materials absorb light energy. At present, the application of solar cells has long been extended from the military and aerospace fields to the industrial, commercial, agricultural, communication, household appliances and public utilities sectors. In particular, they can be used in remote areas, mountains, deserts, islands and rural areas to save expensive transmission lines. Therefore, photovoltaic systems have a very broad application prospect.
[0003] Depending on the materials used, solar cells can be divided into: 1. Crystalline silicon cells; 2. Cells made of inorganic salts such as gallium arsenide III-V compounds, cadmium sulfide, copper indium selenide and other multi-component compounds; 3. Solar cells made of functional polymer materials; 4. Nanocrystalline solar cells, etc.
[0004] Among the above types of solar cells, P-type crystalline silicon cells are the mainstream. In the manufacturing process of P-type crystalline silicon cells, screen printing technology is usually used to print aluminum paste on the back surface of the cell. After high-temperature sintering, an aluminum back field is formed in the silicon matrix. The aluminum back field structure is widely used in various battery structures. On the lower surface of the P-type crystalline silicon cell, a layer of P is formed due to heavy aluminum doping. + layer, thus forming a PP with the P-type substrate + The high-low junction has a built-in electric field that prevents photogenerated carriers from recombining on the back surface, which plays a passivation role, thereby increasing the open circuit voltage of the battery and improving the conversion efficiency of the battery.
[0005] Chinese patent CN102903765B discloses an all-aluminum back field crystalline silicon cell and a preparation method thereof, the all-aluminum back field crystalline silicon cell comprises a silicon wafer layer, a P+ passivation layer and an aluminum back conductive layer are sequentially laminated on the back of the silicon wafer layer, and a back electrode is provided on the aluminum back conductive layer. The method is to first print a layer of aluminum paste on all positions on the back of the solar cell except the edge, and then print the back electrode, and form a P+ passivation layer in the electrode area by sintering. The method uses a pattern slightly smaller than the size of the silicon wafer to print the aluminum paste, that is, a certain blank area is left at the edge of the battery without an aluminum back field. Due to the lack of aluminum back field in the edge area of the battery, the charge collection effect is weakened, and this area contributes very little to the output power of the battery, which is not conducive to improving the open circuit voltage of the solar cell.
[0006] Therefore, it is necessary to provide a solar cell and a manufacturing method thereof, a photovoltaic module and a photovoltaic system to solve the above problems. Summary of the invention
[0007] The present invention aims to solve the above technical problems to a certain extent. To this end, the present invention proposes a solar cell and a manufacturing method thereof, a photovoltaic module and a photovoltaic system, which can realize a cell structure with full aluminum back surface field coverage, improve the open circuit voltage of the solar cell, and further improve the photoelectric conversion efficiency of the solar cell.
[0008] To achieve the above object, the present invention provides the following solutions: A solar cell comprises a P-type substrate prepared from a P-type silicon wafer, wherein an N-type doping layer, an anti-reflection layer and a positive electrode are sequentially arranged on the upper surface of the P-type substrate, an aluminum back field and a back electrode are arranged on the back surface of the P-type substrate, the aluminum back field covers the entire back surface of the P-type substrate except the back electrode, the size of the hollow window of the aluminum back field at the back electrode is slightly smaller than that of the back electrode, and the outer boundary of the aluminum back field pattern coincides with the P-type substrate.
[0009] Compared with the solar cell structure design in the prior art in which a certain blank area is left at the edge and the edge is not covered with aluminum back field, the above structure increases the passivation area of the aluminum back field, improves the open circuit voltage of the solar cell, and further improves the photoelectric conversion efficiency of the solar cell.
[0010] The size of the hollow window of the aluminum back field at the back electrode is slightly smaller than that of the back electrode, and it ensures that the printed back electrode can cover the hollow window. On the one hand, this pattern design ensures sufficient electrical connection between the aluminum back field and the back electrode, reducing the series resistance of the solar cell. On the other hand, it avoids the existence of gaps between the aluminum back field and the back electrode. The aluminum back field does not completely cover the back surface of the silicon wafer, which leads to a decrease in the open circuit voltage of the solar cell and further reduces the photoelectric conversion efficiency. The outer boundary of the aluminum back field pattern coincides with the P-type silicon wafer, ensuring that there is no blank area at the edge of the silicon wafer.
[0011] Preferably, the thickness of the aluminum back field is 20-40 microns. Since the thickness of crystalline silicon cells is relatively thin (currently 180-200 microns), the aluminum back field is prone to warping and deformation of the cell during the sintering process. Taking into account the passivation effect of the aluminum back field, manufacturing cost and product yield, when the thickness of the aluminum back field is 20-40 microns, the aluminum back field has a better passivation effect, and the produced solar cell is not prone to warping and deformation.
[0012] Preferably, the back electrode is composed of several independent sub-electrodes. The function of the back electrode is to collect the positive charge generated on the back surface of the solar cell, and electrically connect it to the welding strip by welding, and realize the series connection between the cells in the assembly through the welding strip. In order to increase the area of the aluminum back field as much as possible, the area of the back electrode should be as small as possible while ensuring that the back electrode and the welding strip are firmly connected. Compared with the continuous single back electrode design, the pattern design of a back electrode composed of several independent sub-electrodes can increase the area of the aluminum back field, enhance the passivation effect, and thus improve the open circuit voltage of the solar cell.
[0013] Preferably, the secondary electrode adopts a hollow pattern design, and the hollow position is covered with an aluminum back field, which further increases the area of the aluminum back field and enhances the passivation effect. In addition, the price of silver paste for printing the back electrode is much higher than that of aluminum paste. The hollow back electrode design can reduce the consumption of back electrode silver paste and reduce the manufacturing cost of solar cells.
[0014] A method for manufacturing a solar cell, used to manufacture any of the above-mentioned solar cells, the method comprising the following steps: Step 1: Texturing the P-type multi-crystalline or single-crystalline silicon wafer to remove the damaged layer of the silicon wafer while forming a surface texture structure to reduce the reflectivity of the silicon wafer surface and increase the number of absorbed photons; Step 2: Phosphorus is diffused into the surface textured P-type silicon wafer to form an N-type doped layer, which forms a PN junction with the P-type substrate to produce a photovoltaic effect; Step 3: wet-etch the diffused P-type silicon wafer to remove the phosphosilicate glass generated during the phosphorus diffusion process and the N-type doped layer that has expanded to the back surface of the silicon wafer; Step 4: Plasma enhanced chemical vapor deposition is performed on the N-type doped layer on the front surface of the P-type silicon wafer to form a silicon nitride anti-reflection film, which further reduces the reflectivity of the silicon wafer surface and passivates the front surface of the silicon wafer; Step 5: Printing positive electrode slurry on the anti-reflection film and drying; Step 6: Print aluminum paste and back electrode silver paste on the lower surface of the P-type silicon wafer in batches and dry them; Step 7: Sinter the silicon wafer after printing the slurry at high temperature to form a positive electrode, an aluminum back field and a back electrode, so as to achieve ohmic contact between the positive electrode, the aluminum back field and the back electrode and the silicon wafer; Step 8: Physically clean the side surface of the silicon wafer to complete the preparation of the solar cell. Since the outer boundary of the printed pattern coincides with the silicon wafer, it is very easy for the aluminum paste to stick to the side surface of the silicon wafer during printing, resulting in the connection between the N-type doped layer on the upper surface of the solar cell and the P-type substrate on the lower surface, causing the photogenerated carriers to flow from the upper surface of the solar cell along the aluminum on the side surface to the lower surface of the cell, forming a short circuit, causing the leakage current of the solar cell to increase and the conversion efficiency to decrease. Removing the aluminum on the side surface of the silicon wafer can ensure the insulation of the upper and lower surfaces of the silicon wafer.
[0015] Preferably, in the above-mentioned solar cell manufacturing method, the physical cleaning uses a grinding wheel to grind the side surfaces of the overlapping cells and remove the aluminum on the side surfaces of the silicon wafers. During grinding, the cells are stacked and fixed with a clamp, and then the four side surfaces of each stack of cells are grinded in sequence with a grinding wheel. This grinding method can grind hundreds of cells at the same time, with high production efficiency.
[0016] Preferably, in the above-mentioned solar cell manufacturing method, the physical cleaning uses laser etching, using a high-intensity focused laser beam emitted by a laser to vaporize the aluminum on the side surface of the cell. This process can be directly integrated into the conveyor belt of the solar cell production line, and the edges of the silicon wafers are sequentially etched by a laser etcher. This polishing method is well matched with the solar cell production line, is convenient for production operation, and has non-contact processing, high flexibility, and noise-free processing performance.
[0017] A photovoltaic module comprises a front plate, a rear plate and a battery cell encapsulated between the front plate and the rear plate, wherein the battery cell is any one of the solar cells described above.
[0018] A photovoltaic system comprises a photovoltaic module, a photovoltaic inverter, a control cabinet and a cable for connecting the photovoltaic module, the photovoltaic inverter and the control cabinet. The photovoltaic module uses any one of the solar cells described above.
[0019] The present invention discloses the following technical effects: The solar cell design adopted by the present invention has an aluminum back field that fully covers the lower surface of the battery except for the back electrode. Without adding additional production equipment, the existing production equipment is used to improve the passivation effect of the lower surface of the solar cell, increase the open circuit voltage of the battery, and thus improve the battery conversion efficiency. The aluminum back field design thickness of the present invention ensures the passivation effect while taking into account the product yield, and the battery is not easy to warp and deform. The back electrode of the present invention adopts a design of several sections of hollowed-out secondary electrode patterns, which not only increases the area of the aluminum back field and improves the passivation effect, but also reduces the manufacturing cost of the solar cell. The present invention uses a physical cleaning method to remove the aluminum on the side surface of the silicon wafer to avoid short circuits between the upper and lower surfaces of the battery. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0021] Figure 1 A schematic diagram of the structure of a solar cell according to an embodiment of the present invention; Figure 2 It is a schematic diagram of the structure of a conventional P-type crystalline silicon solar cell; Figure 3 is a schematic diagram of the structure of the back electrode in an embodiment of the present invention; Figure 4 A flow chart of a method for manufacturing a solar cell according to the present invention; In the figure: 1. P-type substrate; 2. N-type doped layer; 3. Aluminum back surface field; 4. Anti-reflection layer; 5. Positive electrode; 6. Back electrode; 7. Auxiliary electrode. DETAILED DESCRIPTION
[0022] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0023] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.
[0024] In the manufacturing process of conventional P-type crystalline silicon cells, screen printing technology is usually used to print aluminum paste on the lower surface of the cell, and after high-temperature sintering, an aluminum back surface field 3 is formed in the silicon matrix. However, in order to prevent the aluminum paste from reaching the side surface of the silicon wafer and forming a short circuit between the positive and negative electrodes of the cell during screen printing, the aluminum paste is generally printed in a pattern slightly smaller than the size of the silicon wafer, that is, a certain blank area is left at the edge of the cell without an aluminum back surface field 3. The structure diagram of conventional P-type crystalline silicon cells is shown in Figure 1. Figure 2 shown.
[0025] Embodiment 1: Reference Figure 1 As shown, embodiment 1 of the present invention provides a solar cell, comprising a P-type substrate 1, wherein an N-type doping layer 2, an anti-reflection layer 4, and a positive electrode 5 are sequentially prepared on the upper surface of the P-type substrate 1, and an aluminum back surface field 3 and a back electrode 6 are sequentially prepared on the lower surface, wherein the aluminum back surface field 3 reaches the edge of the cell and covers the entire back surface of the cell except the back electrode 6, with reference to Figure 1The fully covered aluminum back surface field 3 increases the passivation area, increases the open circuit voltage, and further increases the photoelectric conversion efficiency of the solar cell.
[0026] In the above embodiment, the size of the hollow window of the aluminum back field 3 at the back electrode 6 is slightly smaller than the back electrode 6, ensuring that the printed back electrode 6 can cover the hollow window. On the one hand, it ensures that there is sufficient electrical connection between the aluminum back field 3 and the back electrode 6, reducing the series resistance of the solar cell. On the other hand, it avoids the existence of a gap between the aluminum back field 3 and the back electrode 6, and the aluminum back field 3 does not completely cover the lower surface of the silicon wafer, resulting in a decrease in the open circuit voltage of the solar cell.
[0027] Further optimization scheme, the thickness of aluminum back field 3 is 20-40 microns. The thickness of aluminum back field 3 has a significant effect on the passivation effect and the warping deformation of the battery. A thinner aluminum back field 3 can reduce the manufacturing cost of solar cells, and the battery is not easy to deform, but an overly thin aluminum back field 3 has a poor passivation effect, causing the open circuit voltage of the solar cell to decrease, thereby reducing the photoelectric conversion efficiency of the battery. A thicker aluminum back field 3 has a good passivation effect, but it will increase the slurry cost. At the same time, the silicon wafer is easy to warp and deform during the sintering process, resulting in bent wafers and reducing the yield of the product. Therefore, when designing the solar cell of this embodiment, the passivation effect of aluminum back field 3, the manufacturing cost and the product yield should be comprehensively considered, and a balance should be made between the photoelectric conversion efficiency, cost and yield. Experiments show that when the thickness of aluminum back field 3 is 20-40 microns, aluminum back field 3 has a good passivation effect, and the produced solar cell is not easy to deform.
[0028] Further optimization scheme, the battery back electrode 6 is a discontinuous pattern, and each back electrode 6 is composed of several independent sub-electrodes 7. The function of the back electrode 6 is to collect the positive charge generated on the lower surface of the solar cell, and electrically connect it to the welding belt by welding, and realize the series connection of the battery through the welding belt. In order to increase the area of the aluminum back field 3 as much as possible, under the premise of ensuring that the back electrode 6 is firmly connected to the welding belt, the area of the back electrode 6 should be as small as possible. Compared with the design of a continuous back electrode 6, the design of several independent sub-electrodes 7 patterns can increase the area of the aluminum back field 3 and improve the open circuit voltage of the solar cell.
[0029] Further optimizing the scheme, the secondary electrode 7 adopts a hollow pattern design, and the hollow position is covered with an aluminum back field 3, which further increases the area of the aluminum back field 3 and enhances the passivation effect. In addition, the price of silver paste for printing the back electrode 6 is much higher than that of aluminum paste. The hollow secondary electrode 7 design can reduce the manufacturing cost of solar cells.
[0030] Embodiment 2: Reference Figure 4 As shown, Embodiment 2 of the present invention provides a method for manufacturing a solar cell, comprising the following steps: Step 1: Texturing the P-type silicon wafer: Optionally, the silicon wafer provided in this embodiment is a P-type single crystal silicon wafer, and an alkali solution (such as KOH or NaOH) is used as a reaction liquid to form a 2-5 micron micro-pyramid structure on the surface of the silicon wafer. In other embodiments, the silicon wafer is a P-type multicrystalline silicon wafer, and an acid solution (such as HNO 3 The mixture of HF and MgO is used as the reaction agent to form 3-10 micron worm-like corrosion pits on the surface of the silicon wafer. Both the micro-pyramid structure and the worm-like corrosion pits texture the surface of the silicon wafer, which can effectively reduce the reflectivity of the silicon wafer surface.
[0031] Step 2: Phosphorus diffusion on surface textured P-type silicon wafer: using POCl 3 , O 2 It reacts chemically with silicon at high temperature to form an N-type doped layer 2 on the surface of the silicon wafer. The thickness of the N-type doped layer 2 is 200-500 nanometers, and the sheet resistance is 90-120 ohms / square. The N-type doped layer 2 and the P-type substrate 1 form a PN junction, which produces a photovoltaic effect.
[0032] Step 3: Wet-etch the diffused P-type silicon wafer: Optionally, this embodiment uses an acid solution (such as H 2 SO 4 , HNO 3 and HF mixture) as a reaction solution to remove the phosphosilicate glass generated on the surface of the silicon wafer during the phosphorus diffusion process and the N-type doped layer 2 that diffuses to the lower surface of the silicon wafer.
[0033] Step 4: Plasma enhanced chemical vapor deposition is performed on the N-type doped layer 2 of the P-type silicon wafer: Optionally, this embodiment uses NH 3 and SiH 4 As a reaction gas, a silicon nitride anti-reflection film is generated on the N-type doped layer 2. The thickness of the silicon nitride anti-reflection film is 70-90 nanometers and the refractive index is 2.0-2.1. The anti-reflection film can effectively reduce the reflectivity of the silicon wafer surface. At the same time, the hydrogen in the anti-reflection film can saturate the dangling bonds on the silicon wafer surface to achieve a passivation effect.
[0034] Step 5: Print the positive electrode 5 slurry on the anti-reflection film and dry it: In this embodiment, the front electrode adopts a comb-like pattern, including a sub-grid for collecting photogenerated carriers and a main grid for collecting the sub-grid current and electrically connecting the welding strip by welding, and finally connected in series with other batteries on the component through the welding strip.
[0035] Step 6: Print aluminum paste and silver paste for the back electrode 6 on the P-type layer in batches and dry them: Optionally, in this embodiment, the back electrode 6 is composed of a number of independent sub-electrodes 7, and a hollow pattern is adopted inside the sub-electrode 7. The hollow position is covered with an aluminum back field 3. The hollow window size of the aluminum back field 3 at the back electrode 6 is slightly smaller than the back electrode 6, covering the entire back surface of the battery except the back electrode 6.
[0036] Step 7: sinter the silicon wafer after printing the slurry at high temperature: Optionally, the sintering temperature of this embodiment is 700-980 degrees Celsius, so that the organic solvent in the slurry is completely volatilized, and the electrode and the silicon wafer form a good ohmic contact. The aluminum paste is sintered at high temperature to form an aluminum-silicon alloy, forming an aluminum back field 3, which can reduce the minority carrier recombination at the junction of the metal and silicon, thereby increasing the open circuit voltage of the solar cell and further improving the photoelectric conversion efficiency.
[0037] Step 8: Physical cleaning: Optionally, every 100 cells are overlapped and stacked into a stack, and fixed with a clamp, and the four sides of each stack of cells are polished in sequence with a grinding wheel during polishing. In other embodiments, laser etching is used for physical cleaning, and the aluminum on the side surface of the cell is vaporized using a high-intensity focused laser beam emitted by a laser. Optionally, the laser wavelength is 532 nanometers, the energy is 120mJ, and the spot diameter is 0.2 mm. This process can be directly integrated into the conveyor belt of the solar cell production line, and the edges of the cells are etched in sequence with a laser etcher. This polishing method is well matched with the solar cell production line, and has non-contact processing, high flexibility, and noise-free processing performance.
[0038] It should be understood that, in practical applications, the P-type crystalline silicon cell structure may also be a PERC cell, a MWT cell, etc., which is not specifically limited in this embodiment.
[0039] Embodiment 3: Embodiment 3 of the present invention provides a photovoltaic module, comprising a front plate, a rear plate, and a cell packaged between the front plate and the rear plate, wherein the cell is the solar cell described in any one of Embodiment 1.
[0040] Embodiment 4: Embodiment 4 of the present invention provides a photovoltaic system, including a photovoltaic module, a photovoltaic inverter, a control cabinet and a cable for connecting the photovoltaic module, the photovoltaic inverter and the control cabinet, wherein the photovoltaic module is the photovoltaic module described in any one of Embodiment 3.
[0041] Compared with the prior art, the solar cell and the manufacturing method thereof, the photovoltaic module and the photovoltaic system of the embodiments of the present invention disclose at least the following beneficial effects: 1. Improve battery conversion efficiency: The solar cell design adopted by the present invention, except for the back electrode 6, the aluminum back field 3 fully covers the lower surface of the battery, improves the passivation effect of the lower surface of the solar cell, increases the open circuit voltage of the battery, and thus improves the battery conversion efficiency.
[0042] 2. Reduce the manufacturing cost of solar cells: The back electrode 6 adopts a design of several hollowed-out sub-electrodes 7, which not only increases the area of the aluminum back surface field 3 and improves the passivation effect, but also reduces the consumption of silver paste of the back electrode 6 and reduces material costs.
[0043] The details not described in detail in the present invention are all conventional technical means well known to those skilled in the art.
[0044] In the description of the present invention, it should be understood that the terms "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0045] The embodiments described above are only descriptions of the preferred modes of the present invention, and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.
Claims
1. A solar cell, characterized in that: The invention comprises a P-type substrate (1) prepared from a P-type silicon wafer, wherein an N-type doping layer (2), an anti-reflection layer (4) and a positive electrode (5) are sequentially arranged on the upper surface of the P-type substrate (1), and an aluminum back field (3) and a back electrode (6) are arranged on the back surface of the P-type substrate (1), wherein the aluminum back field (3) covers the entire back surface of the P-type substrate (1) except the back electrode (6), the size of the hollow window of the aluminum back field (3) at the back electrode (6) is slightly smaller than that of the back electrode (6), and the outer boundary of the aluminum back field (3) pattern coincides with the P-type substrate (1).
2. The solar cell according to claim 1, characterized in that The thickness of the aluminum back surface field (3) is 20-40 microns.
3. The solar cell according to claim 2, characterized in that: The back electrode (6) comprises a plurality of independent sub-electrodes (7).
4. The solar cell according to claim 3, characterized in that: The secondary electrode (7) adopts a hollow pattern design, and the hollow position is covered with an aluminum back surface field (3).
5. A method for manufacturing a solar cell, used for manufacturing the solar cell according to any one of claims 1 to 4, characterized in that: The following steps are involved: S1: performing texturing treatment on the P-type silicon wafer to form a surface textured structure; S2: Phosphorus diffusion is performed on the surface textured P-type silicon wafer to form a PN junction; S3: wet-etching the diffused P-type silicon wafer to remove the phosphosilicate glass generated during the phosphorus diffusion process and the N-type doping layer (2) on the back surface; S4: performing plasma enhanced chemical vapor deposition on the N-type doping layer (2) of the P-type silicon wafer to form a silicon nitride anti-reflection film; S5: printing a positive electrode (5) slurry on the anti-reflection film and drying it; S6: printing aluminum paste and back electrode (6) silver paste on the P-type layer in batches and drying; S7: sintering the silicon wafer after printing the slurry at a high temperature to form a positive electrode (5), an aluminum back field (3) and a back electrode (6); S8: Physically clean the four sides of the silicon wafer to ensure insulation of the front and back sides of the silicon wafer, and complete the preparation of the solar cell.
6. The method for manufacturing a solar cell according to claim 5, characterized in that: The physical cleaning includes removing aluminum on the side surface of the silicon wafer by side grinding.
7. The method for manufacturing a solar cell according to claim 5, characterized in that: The physical cleaning includes insulating the aluminum and aluminum back surface field (3) on the side surface of the silicon wafer by laser etching.
8. The method for manufacturing a solar cell according to claim 5, characterized in that: In step S4, a silicon nitride anti-reflection film is formed on the N-type doped layer (2). The thickness of the silicon nitride anti-reflection film is 70-90 nanometers, and the refractive index is 2.0-2.
1.
9. A photovoltaic module, comprising a front plate, a rear plate and a battery cell encapsulated between the front plate and the rear plate, characterized in that: The cell is the solar cell according to any one of claims 1 to 4.
10. A photovoltaic system, comprising a photovoltaic module, a photovoltaic inverter, a control cabinet and a cable for connecting the photovoltaic module, the photovoltaic inverter and the control cabinet, characterized in that: The photovoltaic module is the photovoltaic module according to claim 9.
Citation Information
Patent Citations
Novel aluminum emitter junction N type single crystal silicon solar battery
CN101150148A
Back electrode structure of crystalline silicon solar cell with passivated back and screen printing plate used by crystalline silicon solar cell
CN103280468A
Solar cell unit, solar cell module and production method thereof
CN104638044A
Manufacturing method of N type all-aluminum back emitter solar cell and solar cell prepared by the same
CN104868011A
Full-back-field diffusion N-type silicon-based battery and preparation method thereof
CN105655424A
Cited By
Photovoltaic cell and preparation method thereof, laminated cell and photovoltaic module