Solar cell, preparation method thereof and photovoltaic module
By forming a passivation structure on the emitter surface of the solar cell, including a first silicon oxide layer, a second silicon oxide layer doped with doped elements and a second doped element oxide layer, the low efficiency of the existing solar cell is solved by forming a passivation structure on the emitter surface of the solar cell, including a first silicon oxide layer, a second silicon oxide layer doped with doped elements, and a second doped element oxide layer, the low efficiency of the existing solar cell is solved. The problem of achieving higher battery efficiency and conversion efficiency.
Patent Information
- Application Number
- CN202411087794.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-12-03
AI Technical Summary
The battery efficiency of existing solar cells is low, making it difficult to effectively utilize optical energy, resulting in insufficient conversion efficiency.
The passivation structure is formed on the emitter surface of the solar cell, including a first silicon oxide layer, a second silicon oxide layer doped with doped elements and a second doped element oxide layer, through which chemical passivation is achieved and Field passivation reduces interface defects and composite current density, and improves battery efficiency.
Through the use of passivation structure, the hanging bond density of the emitter and the substrate is reduced, the composite current density is reduced, the open circuit voltage and conversion efficiency of the battery are improved, and the battery efficiency of the solar cell is significantly improved.
Smart Images

Figure CN119069548A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present application relate to the photovoltaic field, and in particular to a solar cell and a method for preparing the same, and a photovoltaic module. Background Art
[0002] At present, with the gradual depletion of fossil energy, solar cells are becoming more and more widely used as a new energy alternative. Solar cells are devices that convert sunlight into electrical energy. Solar cells use the photovoltaic principle to generate carriers, and then use electrodes to lead the carriers out, thereby facilitating the effective use of electrical energy.
[0003] The current solar cells mainly include IBC cells (Interdigitated Back Contact), TOPCON (Tunnel Oxide Passivated Contact), PERC cells (Passivated emitter and real cell) and heterojunction cells, etc. The photoelectric conversion efficiency of solar cells is improved by reducing optical losses and reducing the recombination of photogenerated carriers on the surface and in the body of the silicon substrate through different film layer settings and functional limitations.
[0004] However, the cell efficiency of current solar cells is still poor. Summary of the invention
[0005] The embodiments of the present application provide a solar cell and a method for preparing the same, and a photovoltaic module, which are at least beneficial to improving the cell efficiency of the solar cell.
[0006] According to some embodiments of the present application, on the one hand, an embodiment of the present application provides a solar cell, comprising: a substrate; an emitter, the emitter being located on the surface of the substrate; a doping element diffused in the emitter; a passivation structure, the passivation structure being located on the surface of the emitter, the passivation structure comprising: a first silicon oxide layer, the first silicon oxide layer being located on the surface of the emitter; a second silicon oxide layer, the second silicon oxide being located on the surface of the first silicon oxide layer, the second silicon oxide layer being doped with the doping element, and the doping mass ratio of the doping element being 1% to 50%; a first doped element oxide layer, the first doped element oxide layer being located on the surface of the second silicon oxide layer, the first doped element oxide layer being doped with silicon element, and the doping mass ratio of the silicon element being 1% to 50%; wherein the first doped element oxide layer is an oxide layer of the doped element; a second doped element oxide layer, the second doped element oxide layer being located on the surface of the first doped element oxide layer; a first electrode, the first electrode being located on the passivation structure and electrically connected to the emitter.
[0007] In some embodiments, the solar cell has a metal area and a non-metal area; the emitter is located on the substrate corresponding to the metal area; and also includes: a passivation layer, the passivation layer is located on the substrate surface corresponding to the non-metal area; at least one film layer of the passivation structure has one of a fixed positive charge or a fixed negative charge, and at least one film layer of the passivation layer has the other of a fixed positive charge or a fixed negative charge.
[0008] In some embodiments, the passivation layer is also located on the surface of the passivation structure, and the first electrode is located on the surface of the passivation layer and is electrically connected to the emitter.
[0009] In some embodiments, along a direction from the first silicon oxide layer to the first doped-element oxide layer, a doping mass ratio of the doping element in the second silicon oxide layer increases.
[0010] In some embodiments, along a direction from the second silicon oxide layer to the second doped element oxide layer, a doping ratio of the silicon element in the first doped element oxide layer decreases.
[0011] In some embodiments, the thickness of the second silicon oxide layer is 0.5 nm to 5 nm, and / or the thickness of the first doped element oxide layer is 0.5 nm to 5 nm.
[0012] According to some embodiments of the present application, on the other hand, the embodiments of the present application also provide a method for preparing a solar cell, comprising: providing a substrate; forming an emitter, the emitter being located on the surface of the substrate; a doping element being diffused in the emitter; forming a passivation structure, the passivation structure being located on the surface of the emitter, the passivation structure comprising: a first silicon oxide layer, the first silicon oxide layer being located on the surface of the emitter; a second silicon oxide layer, the second silicon oxide being located on the surface of the first silicon oxide layer, the second silicon oxide layer being doped with the doping element, and the doping mass ratio of the doping element being 1% to 50%; a first doped element oxide layer, the first doped element oxide layer being located on the surface of the second silicon oxide layer, the first doped element oxide layer being doped with silicon element, and the doping mass ratio of the silicon element being 1% to 50%; wherein the first doped element oxide layer is an oxide layer of the doped element; a second doped element oxide layer, the second doped element oxide layer being located on the surface of the first doped element oxide layer; forming a first electrode, the first electrode being located on the passivation structure and being electrically connected to the emitter.
[0013] In some embodiments, the surface of the substrate has a processed area and a non-processed area, and the emitter and the passivation structure are located in the processed area and the non-processed area: before forming the first electrode, it also includes: removing the emitter and the passivation structure located in the processed area to form a passivation layer, the passivation layer is located in the processed area, and the first electrode is located in the non-processed area.
[0014] In some embodiments, process parameters for forming the second doped element oxide layer include: a process temperature of 25° C. to 400° C., and a reaction time of 1 s to 500 s.
[0015] According to some embodiments of the present application, on the other hand, the embodiments of the present application further provide a photovoltaic assembly, including: a cell string, which is formed by connecting a plurality of solar cells as described in any one of the above embodiments or a solar cell prepared by the preparation method as described in any one of the above embodiments; a packaging film for covering the surface of the cell string; and a cover plate for covering the surface of the packaging film facing away from the cell string.
[0016] The technical solution provided by the embodiments of the present application has at least the following advantages:
[0017] The solar cell provided in the embodiment of the present application is provided with a passivation structure on the emitter of the solar cell, and the passivation structure includes a first silicon oxide layer, a second silicon oxide layer doped with a doping element, a second doping element oxide layer and a first doping element oxide layer doped with silicon element, wherein the first silicon oxide layer is directly in contact with the emitter film layer diffused with the doping element as the first passivation layer, and the fixed charge layer provided by the first silicon oxide layer can provide a strong chemical passivation effect, that is, a field passivation effect, that is, it is conducive to reducing interface defects, so that a good passivation effect can be produced on the emitter and the substrate. The second silicon oxide layer doped with the doping element and the first doping element oxide layer and the second doping element oxide layer can achieve the replacement of silicon element with part of the silicon element, and the doping element becomes an active impurity in the crystalline silicon atomic lattice structure, thereby generating a large number of positive ions or negative ions, forming a charge center, and the additional electrostatic field generated has a field passivation effect, passivating the dangling bond defects at the grain boundary, thereby reducing the composite current density and contact resistance, and improving the open circuit voltage and conversion efficiency of the battery. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] One or more embodiments are exemplarily illustrated by the figures in the corresponding drawings. These exemplified descriptions do not constitute a limitation on the embodiments. Unless otherwise specified, the figures in the drawings do not constitute a scale limitation. In order to more clearly illustrate the embodiments of the present application or the technical solutions in the traditional technology, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0019] Figure 1 A schematic diagram of the structure of a solar cell provided in one embodiment of the present application;
[0020] Figure 2 A schematic diagram of a passivation structure in a solar cell provided in one embodiment of the present application;
[0021] Figure 3 Another schematic diagram of the structure of a solar cell provided in one embodiment of the present application;
[0022] Figure 4 A schematic diagram of another structure of a solar cell provided in one embodiment of the present application;
[0023] Figures 5 to 8 A schematic diagram of the structure of a solar cell corresponding to each step in a method for preparing a solar cell provided in another embodiment of the present application;
[0024] Fig. 9 A schematic structural diagram of a laminated battery provided in yet another embodiment of the present application;
[0025] Fig.10 A schematic diagram of the structure of a photovoltaic module provided in yet another embodiment of the present application;
[0026] Fig.11 for Fig.10 Schematic diagram of the cross-sectional structure along the M1-M2 section. DETAILED DESCRIPTION
[0027] As known from the background art, the cell efficiency of current solar cells is poor.
[0028] The embodiments of the present application provide a solar cell and a method for preparing the same, and a photovoltaic module. A passivation structure is formed on the surface of the emitter of the solar cell. The emitter is passivated by the passivation structure, thereby reducing the density of dangling bonds in the emitter and the substrate, thereby reducing the composite current density and improving the cell efficiency.
[0029] In the description of the embodiments of the present application, the technical terms "first", "second", etc. are only used to distinguish different objects, and cannot be understood as indicating or implying relative importance or implicitly indicating the number, specific order or primary and secondary relationship of the indicated technical features. In the description of the embodiments of the present application, the meaning of "multiple" is more than two, unless otherwise clearly and specifically defined.
[0030] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0031] In the description of the embodiments of the present application, the term "and / or" is only a description of the association relationship of associated objects, indicating that three relationships may exist. For example, A and / or B can represent: A exists, A and B exist at the same time, and B exists. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.
[0032] In the description of the embodiments of the present application, the term "multiple" refers to more than two (including two). Similarly, "multiple groups" refers to more than two groups (including two groups), and "multiple pieces" refers to more than two pieces (including two pieces).
[0033] In the description of the embodiments of the present application, the technical terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, which are only for the convenience of describing the embodiments of the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the embodiments of the present application.
[0034] In the description of the embodiments of the present application, unless otherwise clearly specified and limited, technical terms such as "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, and it can be the internal connection of two elements or the interaction relationship between two elements. For those of ordinary skill in the art, the specific meanings of the above terms in the embodiments of the present application can be understood according to the specific circumstances.
[0035] In the drawings corresponding to the embodiments of the present application, the thickness and area of the layers are exaggerated for better understanding and ease of description. When describing a component (such as a layer, film, region or substrate) on another component or on the surface of another component, the component may be "directly" located on the surface of the other component, or a third component may be present between the two components. On the contrary, when describing a component on the surface of another component or when another component is formed or provided on the surface of a component, it means that there is no third component between the two components. In addition, when describing a component as being "substantially" formed on another component, it means that the component is not formed on the entire surface (or front surface) of the other component, nor is it formed on a partial edge of the entire surface.
[0036] In the description of the embodiments of the present application, when a component "includes" another component, unless otherwise specified, other components are not excluded, and other components may be further included. In addition, when a component such as a layer, a film, a region, or a plate is referred to as being "on / located on" another component, it may be "directly on" the other component (i.e., located on the surface of the other component with no other components between them), or another component may exist in between. In addition, when a component such as a layer, a film, a region, a plate, etc. is "directly located on" another component, or when a component such as a layer, a film, a region, a plate, etc. is located on the surface of another component, it means that no other components are located in between.
[0037] The terms used in the description of the various embodiments described herein are only used to describe specific embodiments and are not intended to be limiting. As used in the description of the various embodiments described and in the appended claims, "the part" is also intended to include the plural form unless the context clearly indicates otherwise. Among them, a component includes a layer, a film, a region, or a plate.
[0038] The following will describe the various embodiments of the present application in detail with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the various embodiments of the present application, many technical details are provided in order to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical solution claimed in the present application can be implemented.
[0039] Figure 1 A schematic diagram of the structure of a solar cell provided in one embodiment of the present application; Figure 2 A schematic diagram of a passivation structure in a solar cell provided in one embodiment of the present application.
[0040] refer to Figure 1 and Figure 2According to some embodiments of the present application, the embodiments of the present application provide a solar cell, including: a substrate 100; an emitter 112, the emitter 112 is located on the surface of the substrate 100; a doping element is diffused in the emitter 112; a passivation structure 120, the passivation structure 120 is located on the surface of the emitter 112, and the passivation structure 120 includes: a first silicon oxide layer 121, the first silicon oxide layer 121 is located on the surface of the emitter 112; a second silicon oxide layer 122, the second silicon oxide is located on the surface of the first silicon oxide layer 121, the second silicon oxide layer 122 is doped with a doping element, and the doping element The doping mass ratio is 1% to 50%; a first doped element oxide layer 123, the first doped element oxide layer 123 is located on the surface of the second silicon oxide layer 122, the first doped element oxide layer 123 is doped with silicon element, and the doping mass ratio of silicon element is 1% to 50%; wherein the first doped element oxide layer 123 is an oxide layer of doped element; a second doped element oxide layer 124, the second doped element oxide layer 124 is located on the surface of the first doped element oxide layer 123; a first electrode 106, the first electrode 106 is located on the passivation structure 120, and is electrically connected to the emitter 112.
[0041] In the embodiment of the present application, a passivation structure 120 is arranged on the emitter 112 of the solar cell, and the passivation structure 120 includes a first silicon oxide layer 121, a second silicon oxide layer 122 doped with an impurity element, a second impurity element oxide layer 124, and a first impurity element oxide layer 123 doped with silicon element, wherein the first silicon oxide layer 121 is directly in contact with the emitter film layer 112 diffused with the impurity element as the first passivation layer, and the fixed charge layer provided by the first silicon oxide layer 121 can provide a strong chemical passivation effect, that is, a field passivation effect, which is beneficial to reduce interface defects, thereby producing a good passivation effect on the emitter 112 and the substrate 100. The second silicon oxide layer 122 doped with the doped element and the first doped element oxide layer 123 and the second doped element oxide layer 124 can realize the replacement of part of the silicon element with the silicon element. The doped element becomes an active impurity in the atomic lattice structure of crystalline silicon, thereby generating a large number of positive ions or negative ions to form a charge center. The additional electrostatic field generated has the effect of field passivation, passivating the dangling bond defects at the grain boundaries, thereby reducing the composite current density and contact resistance, and improving the open circuit voltage and conversion efficiency of the battery.
[0042] In some embodiments, the material of the substrate 100 may be an elemental semiconductor material. Specifically, the elemental semiconductor material is composed of a single element, such as silicon or germanium. The elemental semiconductor material may be in a single crystalline state, a polycrystalline state, an amorphous state, or a microcrystalline state (a state having both a single crystalline state and an amorphous state is referred to as a microcrystalline state), for example, silicon may be at least one of single crystalline silicon, polycrystalline silicon, amorphous silicon, or microcrystalline silicon.
[0043] In some embodiments, the material of the substrate 100 may also be a compound semiconductor material. Common compound semiconductor materials include, but are not limited to, silicon germanium, silicon carbide, gallium arsenide, indium gallium, perovskite, cadmium telluride, copper indium selenide, and the like. The substrate 100 may also be a sapphire substrate 100, a silicon-on-insulator substrate 100, or a germanium-on-insulator substrate 100.
[0044] In some embodiments, the substrate 100 may be an N-type semiconductor substrate 100 or a P-type semiconductor substrate 100. The N-type semiconductor substrate 100 is doped with an N-type doping element, and the N-type doping element may be any one of the V-group elements such as phosphorus (P), bismuth (Bi), antimony (Sb), or arsenic (As). The P-type semiconductor substrate 100 is doped with a P-type element, and the P-type doping element may be any one of the III-group elements such as boron (B), aluminum (Al), gallium (Ga), or indium (In).
[0045] In some embodiments, the substrate 100 has a first surface and a second surface that are arranged opposite to each other. The solar cell is a single-sided cell, the first surface can be used as a light-receiving surface for receiving incident light, and the second surface is used as a backlight surface. Among them, the backlight surface can also receive incident light, but the efficiency of receiving the incident light is weaker than the efficiency of the light-receiving surface receiving the incident light. Among them, the embodiment of the present application takes the first surface covered by the emitter 112 as the front side, and the second surface that does not include the emitter 112 as the back side as an example.
[0046] In some embodiments, the conductivity type of the doping element doped in the emitter 112 is different from the conductivity type of the doping element in the substrate 100. For example, if the substrate 100 is an N-type substrate, the emitter 112 is doped with a P-type doping element; for another example, if the substrate 100 is a P-type substrate, the emitter 112 is doped with an N-type doping element.
[0047] In some embodiments, the emitter 112 and the substrate 100 are the same initial substrate, and after a diffusion process, part of the initial substrate serves as the emitter 112, and part of the initial substrate serves as the substrate 100, that is, there is no obvious boundary between the substrate 100 and the emitter 112, but the area formed by the PN junction serves as the distinction, that is, the substrate 100 is one of the P region or the N region, and the emitter 112 is the other of the P region or the N region.
[0048] In some embodiments, the emitter 112 is a film layer formed on the substrate 100 through a deposition process or an in-situ formation process, and then a diffusion layer is formed through in-situ doping or diffusion doping.
[0049] In some embodiments, the doping element is an N-type doping element, and the first silicon oxide layer 121 forms a fixed positive charge layer with the surface of the substrate 100, and the fixed positive charge can recombine the dangling bonds on the surface of the substrate 100 to avoid the recombination of electrons and holes, thereby improving the battery efficiency. In addition, the fixed positive charge formed by the first silicon oxide layer 121 is conducive to increasing the electric field between the N region and the P region formed by the emitter 112, thereby accelerating the migration rate of the carriers and improving the mobility of the carriers in the battery.
[0050] In some embodiments, the thickness of the first silicon oxide layer 121 is between 0.5 nm and 5 nm. Thus, the first silicon oxide layer 121 can serve not only as a field passivation layer but also as a tunneling layer. Carriers can tunnel through the first silicon oxide layer 121 to the next film layer and be collected by the first electrode 106 .
[0051] In some embodiments, the thickness of the first silicon oxide layer 121 may be 0.6 nm, 1 nm, 1.8 nm, 2.1 nm, 3.3 nm, 4.2 nm, or 4.9 nm.
[0052] In some embodiments, taking the doping element as the P element as an example, the doping element doped in the second silicon oxide layer 122 can serve as a carrier of the positive charge layer, thereby serving as a replacement for part of the silicon element and becoming an active impurity in the atomic lattice structure of crystalline silicon (Si), thereby generating a large number of P+ ions, forming a positive charge center, and the additional electrostatic field generated has a field passivation effect.
[0053] In some embodiments, the doping mass ratio of the doping element of the second silicon oxide layer 122 increases along the direction from the first silicon oxide layer 121 to the first doped element oxide layer 123. The increasing doping mass ratio of the doping element can prevent the emitter 112 surface from having more doping elements as recombination centers and dangling bonds to rob oxygen elements, thereby improving the passivation effect of the second silicon oxide layer 122, and the concentration of the doping element of the second silicon oxide layer 122 away from the substrate 100 is higher, and the area with a higher doping element concentration can be used as a transmission channel to promote the carriers to move toward the first electrode 106, thereby improving the carrier migration rate.
[0054] The doping mass ratio refers to the doping mass fraction of the doping element in the matrix material, and the doping mass fraction = the mass of the doping element / (the mass of the doping element + the mass of the matrix material).
[0055] In some embodiments, the doping mass ratio of the doping element may be 1%, 5%, 13%, 20%, 24%, 31%, 38%, 42%, 45% or 48%.
[0056] In some embodiments, the thickness of the second silicon oxide layer 122 is 0.5 nm to 5 nm.
[0057] In some embodiments, the thickness of the second silicon oxide layer 122 may be 0.6 nm, 1.1 nm, 1.7 nm, 2.2 nm, 3.3 nm, 4.2 nm, or 4.9 nm.
[0058] In some embodiments, silicon is doped in the first doped element oxide layer 123. The presence of silicon can improve the interface compatibility between the first doped element oxide layer 123 and the second silicon oxide layer 122, thereby improving the adhesion between the two. Second, silicon can cause silicon to destroy the PO bond, thereby allowing the P+ ion to be freed and serve as a positive charge center. In addition, silicon and doped elements can also passivate dangling bond defects at the grain boundary.
[0059] In some embodiments, along the direction from the second silicon oxide layer 122 to the second doped element oxide layer 124 , the doping ratio of the silicon element in the first doped element oxide layer 123 decreases.
[0060] In some embodiments, the thickness of the first doped element oxide layer 123 is 0.5 nm to 5 nm, or 0.6 nm, 1.1 nm, 1.7 nm, 2.2 nm, 3.3 nm, 4.2 nm, or 4.9 nm.
[0061] In some embodiments, the thickness of the second doping element oxide layer 124 is 0.5 nm to 5 nm, 0.6 nm, 1.1 nm, 1.7 nm, 2.2 nm, 3.3 nm, 4.2 nm or 4.9 nm.
[0062] In some embodiments, the solar cell further includes an anti-reflection layer 108 , which is located on the surface of the passivation structure 120 ; a back passivation layer 118 , which is located on the second surface of the substrate 100 ; and a second electrode 116 , which is electrically connected to the back side of the substrate 100 .
[0063] In some embodiments, the anti-reflection layer 108 may be a single-layer structure or a stacked-layer structure, and the material of the anti-reflection layer 108 may be one or more of silicon oxide, silicon nitride, silicon oxynitride, silicon carbonitride oxide, titanium oxide, hafnium oxide or aluminum oxide.
[0064] In some embodiments, the thickness of the anti-reflection layer 108 is 5 nm to 150 nm. The thickness of the anti-reflection layer 108 is 5 nm, 18 nm, 59 nm, 83 nm, 121 nm, 138 nm, or 149 nm.
[0065] In some embodiments, the back passivation layer 118 may be a single-layer structure or a stacked-layer structure, and the material of the back passivation layer 118 may be one or more of silicon oxide, silicon nitride, silicon oxynitride, silicon carbonitride oxide, titanium oxide, hafnium oxide or aluminum oxide.
[0066] In some embodiments, the first electrode 106 may be formed by sintering a burn-through paste. The method for forming the first electrode 106 includes: printing a metal paste on a surface of a portion of the anti-reflection layer using a screen printing process. The metal paste may include at least one of silver, aluminum, copper, tin, gold, lead or nickel. Then, the metal paste is subjected to a sintering process, and the metal paste contains a material with a highly corrosive component such as glass powder. In this way, during the sintering process, the corrosive component will corrode the anti-reflection layer and the passivation structure 120, so that the metal paste penetrates into the anti-reflection layer 108 and the passivation structure 120 and makes electrical contact with the emitter 112.
[0067] In some embodiments, the first electrode 106 may be formed by sintering LECO (Laser-enhanced contact optimization) slurry, and part of the LECO slurry corrodes the anti-reflection layer 108 and penetrates into the passivation structure 120 and contacts the emitter 112 or forms an electrical connection with the emitter 112 through a crystal.
[0068] In some embodiments, the second electrode 116 can be formed by sintering a burn-through paste. The method for forming the second electrode 116 includes: printing a metal paste on a portion of the back passivation layer surface using a screen printing process. The metal paste may include at least one of silver, aluminum, copper, tin, gold, lead or nickel. Then, the metal paste is subjected to a sintering process, and the metal paste contains a material with a highly corrosive component such as glass powder. In this way, during the sintering process, the corrosive component will corrode the back passivation layer, so that the metal paste penetrates into the back passivation layer 118 and makes electrical contact with the substrate 100.
[0069] In some embodiments, the second electrode 116 may be formed by sintering LECO slurry, and a portion of the LECO slurry corrodes the back electrode and contacts the substrate 100 or forms an electrical connection with the substrate 100 through crystals.
[0070] In some embodiments, the back side of the substrate 100 may be covered with a tunnel dielectric layer and a doped conductive layer, and the second electrode 116 is in contact with the doped conductive layer.
[0071] Figure 3 Another schematic diagram of the structure of a solar cell provided in one embodiment of the present application; Figure 4 A schematic diagram of another structure of a solar cell provided in an embodiment of the present application.
[0072] Accordingly, an embodiment of the present application further provides a solar cell having a local emitter structure. Figure 1 The difference of the solar cell provided is that the emitter of the solar cell described above is located on the surface of the entire substrate, while Figure 3 A local emitter is formed in the solar cell shown, that is, the emitter is located on the substrate corresponding to the metal area, and other features are the same as or corresponding to the above embodiments, which will not be described in detail here.
[0073] refer to Figure 3 In some embodiments, the solar cell has a metal region 11 and a non-metal region 12 ; the emitter 112 is located on the substrate 100 corresponding to the metal region 11 .
[0074] In some embodiments, the metal region 11 refers to the region where the orthographic projection of the first electrode 106 on the substrate 100 is located, and the non-metal region 12 refers to the region other than the orthographic projection of the first electrode 106 on the substrate 100. In order to ensure that the film layer contacted by the first electrode 106 has a large doping concentration or the region contacted by the first electrode 106 is a high-concentration emitter 112, the area of the metal region 11 is generally set to be greater than or equal to the area of the orthographic projection of the first electrode 106 on the substrate 100.
[0075] In some embodiments, the solar cell further includes: a passivation layer 113, the passivation layer 113 is located on the surface of the substrate 100 corresponding to the non-metallic region 12; at least one film layer of the passivation structure 120 has one of a fixed positive charge or a fixed negative charge, and at least one film layer of the passivation layer 113 has the other of a fixed positive charge or a fixed negative charge. In other words, the passivation layer 113 forms a field passivation effect on the surface of the substrate 100, and the passivation structure 120 exerts a field passivation effect on the emitter 112.
[0076] In some embodiments, the passivation layer 113 may be a single-layer structure or a stacked-layer structure, and the material of the passivation layer 113 may be one or more of silicon oxide, silicon nitride, silicon oxynitride, silicon carbonitride oxide, titanium oxide, hafnium oxide, or aluminum oxide.
[0077] In some embodiments, the thickness of the passivation layer 113 is 5 nm to 150 nm. The thickness of the passivation layer 113 is 5 nm, 18 nm, 59 nm, 83 nm, 121 nm, 138 nm, or 149 nm.
[0078] The passivation layer with fixed positive charge can be any one of a silicon nitride layer, a hydrogenated amorphous silicon layer or a phosphorus oxide layer, or a stack of multiple layers. The passivation layer with fixed negative charge can be any one or more of an aluminum oxide layer, a gallium oxide layer, a stack of aluminum oxide and silicon oxide, and a stack of gallium oxide and silicon nitride.
[0079] In some embodiments, there may be a silicon dioxide layer between the passivation layer 113 and the substrate 100. Since the passivation layer contains a certain amount of hydrogen, for example, the hydrogen content of the aluminum oxide layer is about 2% to 4%, when the passivation of the passivation layer is activated during the annealing process, the crystallinity of the silicon surface changes from a microcrystalline amorphous mixture to a polycrystalline. At the same time, the hydrogen ions in the passivation layer will diffuse to the interface. The silicon dioxide layer can effectively prevent excessive hydrogen ions from penetrating into the semiconductor silicon substrate, thereby avoiding the more serious light elevated temperature induced degradation (LeTID) effect.
[0080] In some embodiments, reference Figure 3 The passivation layer 113 is also located on the surface of the passivation structure 120 , and the first electrode 116 is located on the surface of the passivation layer 113 and is electrically connected to the emitter 112 .
[0081] In some embodiments, reference Figure 4 , the passivation layer 113 is not located on the surface of the passivation structure 120 , and the anti-reflection layer 108 covers the passivation layer 113 and the surface of the passivation structure 120 .
[0082] In some embodiments, the non-metallic region 12 has no emitter 112, and the emitter 112 is set in the metal region 11, so as to ensure that the area corresponding to the electrode is a heavily doped area, thereby reducing the contact resistance. Not setting the emitter 112 in the non-metallic region 12 can reduce the carrier recombination rate on the surface of the substrate 100 of the non-metallic region 12, thereby improving the battery efficiency.
[0083] In some embodiments, the doping concentration of the emitter 112 may be 1×10 18 atom / cm 3 ~1×10 21 atom / cm 3 .
[0084] Among them, the doping mentioned above refers to chemical doping, that is, there is a chemical change between the doping element and the molecules in the corresponding film layer, and a chemical bond is formed. For example, a Si-O bond is formed in the second silicon oxide layer 122, and the phosphorus doping element is located in the chemical structure formed by the Si-O bond, and part of the oxygen element forms a PO bond with the phosphorus doping element.
[0085] The solar cell provided in the embodiment of the present application has a passivation structure 120 arranged on the emitter 112 of the solar cell, and the passivation structure 120 includes a first silicon oxide layer 121, a second silicon oxide layer 122 doped with an doping element, a second doped element oxide layer 124 and a first doped element oxide layer 123 doped with silicon element, wherein the first silicon oxide layer 121 is directly in contact with the emitter 112 film layer of the diffused doped element as the first passivation layer, and the fixed charge layer provided by the first silicon oxide layer 121 can provide a strong chemical passivation effect, that is, a field passivation effect, which is beneficial to reduce interface defects, thereby producing a good passivation effect on the emitter 112 and the substrate 100. The second silicon oxide layer 122 doped with the doped element and the first doped element oxide layer 123 and the second doped element oxide layer 124 can realize the replacement of part of the silicon element with the silicon element, that is, the doped element becomes an active impurity in the atomic lattice structure of crystalline silicon, thereby generating a large number of positive ions or negative ions to form a charge center. The additional electrostatic field generated has the effect of field passivation, passivating the dangling bond defects at the grain boundaries, thereby reducing the composite current density and contact resistance, and improving the open circuit voltage and conversion efficiency of the battery.
[0086] Accordingly, according to some embodiments of the present application, the embodiments of the present application also provide a method for preparing a solar cell, which is used to provide the solar cell described in the above embodiments. The technical features that are the same or corresponding to the above embodiments are not described in detail here. Figure 3 The method of manufacturing the formed solar cell is taken as an example.
[0087] Figures 5 to 8 A schematic diagram of the structure of a solar cell corresponding to each step in a method for preparing a solar cell provided in another embodiment of the present application.
[0088] refer to Figure 3 , Figure 5 as well as Figure 8According to some embodiments of the present application, the embodiments of the present application also provide a method for preparing a solar cell, including: providing a substrate 100; forming an emitter 112, the emitter 112 is located on the surface of the substrate 100; a doping element is diffused in the emitter 112; forming a passivation structure 120, the passivation structure 120 is located on the surface of the emitter 112, and the passivation structure 120 includes: a first silicon oxide layer 121, the first silicon oxide layer 121 is located on the surface of the emitter 112; a second silicon oxide layer 122, the second silicon oxide is located on the surface of the first silicon oxide layer 121, and the second silicon oxide layer 122 is doped with a doping element , and the doping mass ratio of the doped element is 1% to 50%; a first doped element oxide layer 123, the first doped element oxide layer 123 is located on the surface of the second silicon oxide layer 122, the first doped element oxide layer 123 is doped with silicon element, and the doping mass ratio of the silicon element is 1% to 50%; wherein the first doped element oxide layer 123 is an oxide layer of the doped element; a second doped element oxide layer 124, the second doped element oxide layer 124 is located on the surface of the first doped element oxide layer 123; a first electrode 106 is formed, the first electrode 106 is located on the passivation structure 120, and is electrically connected to the emitter 112.
[0089] refer to Figure 5 , providing an initial substrate 107.
[0090] refer to Figure 6 , a texturing process is performed on one side of the initial substrate 107 so that one side of the initial substrate 107 has a suede structure 111 . The suede structure 111 includes a plurality of first protruding structures 101 .
[0091] In some embodiments, the texturing process includes: chemical etching, for example, a mixed solution of potassium hydroxide and hydrogen peroxide solution can be used to clean the initial substrate 107, and the suede structure with the expected morphology can be formed by controlling the concentration ratio of potassium hydroxide and hydrogen peroxide solution. In some embodiments, the suede structure can also be formed by laser etching, mechanical method or plasma etching. In laser etching, the suede structure with the expected morphology is obtained by controlling the laser process parameters.
[0092] refer to Figure 7 The diffusion layer 102 is formed by high temperature diffusion or ion implantation. A partial thickness of the initial substrate 100 is diffused to form a diffusion layer.
[0093] Continue to refer Figure 7 and Figure 2 , a first silicon oxide layer 121, a second silicon oxide layer 122, a first doped element oxide layer 123 and a second doped element oxide layer 124 are prepared by an atomic layer deposition (ALD) method.
[0094] In some embodiments, the process steps for forming the first silicon oxide layer 121 include: introducing an oxygen-containing gas (CO2, O3 or N2O, water vapor, etc.) into the ALD equipment, controlling its process temperature to 25°C to 400°C, and the process time to 1s to 500s to form the first silicon oxide layer 121 on the surface of the diffusion layer 102.
[0095] In some embodiments, the process steps for forming the second silicon oxide layer 122 include: introducing a doping element source gas, a silicon source, and an oxygen-containing gas into an ALD device, controlling the flow ratio of the doping element source gas and the silicon source to be 1:50 to 1:1, the process temperature to be 25°C to 400°C, and the process time to be 1s to 500s, so as to form the second silicon oxide layer 122 on the surface of the first silicon oxide layer 121, and the doping element is in-situ generated in the second silicon oxide layer 122. Taking phosphorus as an example, the doping element source gas can be trimethyl phosphate (TMP, (CH3)3PO4) gas.
[0096] In some embodiments, the process steps for forming the first doped element oxide layer 123 include: introducing doped element source gas, silicon source and oxygen-containing gas into the ALD equipment, controlling the flow ratio of the silicon source and the doped element source gas to be 1:50 to 1:1, the process temperature to be 25°C to 400°C, and the process time to be 1s to 500s, so as to form the first doped element oxide layer 123 on the surface of the second silicon oxide layer 122, and the silicon element is in-situ generated in the first doped element oxide layer 123.
[0097] The process parameters for forming the second doped element oxide layer 124 include: a process temperature of 25°C to 400°C and a reaction time of 1s to 500s. Compared with the conventional preparation process of the oxide layer, the process temperature for forming the second doped element oxide layer 124 in this solution is lower, thereby reducing the effects of heat treatment on the emitter, the first silicon oxide layer, the second silicon oxide layer and the first doped element oxide layer in the cell, that is, the doped element in each film layer exists and is within a preset range.
[0098] In some embodiments, reference Figure 8 The surface of the substrate 100 has a processed area and a non-processed area, and the emitter 112 and the passivation structure 120 are located in the processed area and the non-processed area: before forming the first electrode 106, it also includes: removing the emitter 112 and the passivation structure 120 located in the processed area to form a passivation layer 113, the passivation layer is located in the processed area, and the first electrode 106 is located in the non-processed area.
[0099] In some embodiments, reference Figure 3 The preparation method includes: forming a passivation layer 113, an anti-reflection layer 108, and a back passivation layer 118 and a second electrode 116 located on the back side.
[0100] Accordingly, according to some embodiments of the present application, reference Fig. 9 On the other hand, the embodiments of the present application further provide a stacked battery, including: a bottom battery, which is a solar cell as in any one of the above embodiments or a solar cell prepared by the preparation method as in any one of the above embodiments; and a top battery, which is located on the side of the substrate in the bottom battery away from the electrode.
[0101] Fig. 9 A schematic structural diagram of a stacked battery provided in yet another embodiment of the present application.
[0102] In some embodiments, the stacked battery has a first gridline 186 of a first polarity and a second gridline of a second polarity, wherein the first gridline 186 is in electrical contact with the top battery 180 and the second gridline is in electrical contact with the bottom battery 150. The second gridline is the first electrode 106 of the bottom battery.
[0103] In some embodiments, there is an interface layer 181 between the top cell and the bottom cell, and the interface layer 181 also covers the passivation contact structure.
[0104] It is worth noting that the stacked cell in the embodiment of the present application only illustrates two layers of solar cells, and those skilled in the art can set three layers of solar cells or more than three layers of stacked solar cells according to actual needs.
[0105] In some embodiments, the top cell 180 may be a perovskite solar cell, which includes: a stacked first transmission layer 182, a perovskite substrate 183, a second transmission layer 184, a transparent conductive layer 185, and an anti-reflection layer (not shown), wherein the first transmission layer is opposite to the bottom cell.
[0106] In some embodiments, the first transport layer may be one of an electron transport layer and a hole transport layer, and the second transport layer may be the other of the electron transport layer and the hole transport layer.
[0107] Accordingly, according to some embodiments of the present application, the embodiments of the present application further provide a photovoltaic module, including the solar cell provided in the above embodiments, and the technical features that are the same as or corresponding to the above embodiments are not described in detail here.
[0108] Fig.10 A schematic diagram of the structure of a photovoltaic module provided in yet another embodiment of the present application; Fig.11 for Fig.10 Schematic diagram of the cross-sectional structure along the M1-M2 section.
[0109] refer to Fig.10 and Fig.11, a photovoltaic module includes: a battery string, which is electrically connected by a plurality of solar cells as in any of the above embodiments, a solar cell prepared by the preparation method as in any of the above embodiments, or a laminated battery as described in the above embodiments; a connecting component 218, the connecting component 218 is used to electrically connect two adjacent solar cells 20; a packaging film 21, which is used to cover the surface of the battery string; a cover plate 22, which is used to cover the surface of the packaging film 21 away from the battery string.
[0110] Specifically, in some embodiments, multiple cells can be electrically connected through a connecting member 218, and the connecting member 218 is welded to a main grid on the cell. The main grid includes a main electrode electrically connected to the first electrode 106 and a main electrode electrically connected to the second electrode 116.
[0111] In some embodiments, no intervals are set between the battery cells, that is, the battery cells overlap each other.
[0112] In some embodiments, the connection component 218 is welded to the secondary grid 208 on the solar cell, and the secondary grid 208 includes the first electrode 106 and the second electrode 116 .
[0113] In some embodiments, the encapsulation film 21 includes a first encapsulation layer and a second encapsulation layer, the first encapsulation layer covers one of the front side or the back side of the solar cell, and the second encapsulation layer covers the other of the front side or the back side of the solar cell. Specifically, at least one of the first encapsulation layer or the second encapsulation layer can be an organic encapsulation film such as a polyvinyl butyral (PVB) film, an ethylene-vinyl acetate copolymer (EVA) film, a polyethylene octene co-elastomer (POE) film or a polyethylene terephthalate (PET) film.
[0114] It is worth noting that there is a boundary line between the first encapsulation layer and the second encapsulation layer before lamination. After lamination, the photovoltaic module is no longer a first encapsulation layer and a second encapsulation layer, that is, the first encapsulation layer and the second encapsulation layer have formed an integral encapsulation film 21.
[0115] In some embodiments, the cover plate 22 may be a glass cover plate, a plastic cover plate or the like with a light-transmitting function. Specifically, the surface of the cover plate 22 facing the encapsulation film 21 may be a concave-convex surface, thereby increasing the utilization rate of the incident light. The cover plate 22 includes a first cover plate and a second cover plate, the first cover plate is opposite to the first encapsulation layer, and the second cover plate is opposite to the second encapsulation layer; or the first cover plate is opposite to one side of the solar cell, and the second cover plate is opposite to the other side of the solar cell.
[0116] Those skilled in the art will appreciate that the above-mentioned embodiments are specific examples for implementing the present application, and in practical applications, various changes may be made to the embodiments in form and detail without departing from the spirit and scope of the present application. Any person skilled in the art may make various changes and modifications without departing from the spirit and scope of the present application, and therefore the scope of protection of the present application shall be subject to the scope defined in the claims.
Claims
1. A solar cell, It is characterized in that include: substrate; An emitter, the emitter being located on a surface of the substrate; The emitter is diffused with doping elements; A passivation structure, the passivation structure is located on the emitter surface, and the passivation structure includes: A first silicon oxide layer, wherein the first silicon oxide layer is located on the surface of the emitter; a second silicon oxide layer, wherein the second silicon oxide is located on the surface of the first silicon oxide layer, the second silicon oxide layer is doped with the doping element, and the doping mass ratio of the doping element is 1% to 50%; A first doped element oxide layer, the first doped element oxide layer is located on the surface of the second silicon oxide layer, the first doped element oxide layer is doped with silicon element, and the doping mass ratio of the silicon element is 1% to 50%; wherein the first doped element oxide layer is the doped element oxide layer; a second doped element oxide layer, the second doped element oxide layer being located on a surface of the first doped element oxide layer; A first electrode is located on the passivation structure and is electrically connected to the emitter.
2. The solar cell according to claim 1, It is characterized in that The solar cell has a metal area and a non-metal area; the emitter is located on the substrate corresponding to the metal area; and also includes: a passivation layer, the passivation layer is located on the surface of the substrate corresponding to the non-metal area; at least one film layer of the passivation structure has one of a fixed positive charge or a fixed negative charge, and at least one film layer of the passivation layer has the other of a fixed positive charge or a fixed negative charge.
3. The solar cell according to claim 2, It is characterized in that The passivation layer is also located on the surface of the passivation structure, and the first electrode is located on the surface of the passivation layer and is electrically connected to the emitter.
4. The solar cell according to claim 1 or 2, It is characterized in that Along the direction from the first silicon oxide layer to the first doped element oxide layer, the doping mass ratio of the doping element in the second silicon oxide layer increases gradually.
5. The solar cell according to claim 1 or 2, It is characterized in that Along the direction from the second silicon oxide layer to the second element-doped oxide layer, the doping ratio of the silicon element in the first element-doped oxide layer decreases gradually.
6. The solar cell according to claim 1 or 2, It is characterized in that The thickness of the second silicon oxide layer is 0.5 nm to 5 nm, and / or the thickness of the first element-doped oxide layer is 0.5 nm to 5 nm.
7. A method for preparing a solar cell, It is characterized in that include: providing a substrate; forming an emitter, wherein the emitter is located on a surface of the substrate; The emitter is diffused with doping elements; A passivation structure is formed, wherein the passivation structure is located on the emitter surface, and the passivation structure comprises: A first silicon oxide layer, wherein the first silicon oxide layer is located on the surface of the emitter; a second silicon oxide layer, wherein the second silicon oxide is located on the surface of the first silicon oxide layer, the second silicon oxide layer is doped with the doping element, and the doping mass ratio of the doping element is 1% to 50%; A first doped element oxide layer, the first doped element oxide layer is located on the surface of the second silicon oxide layer, the first doped element oxide layer is doped with silicon element, and the doping mass ratio of the silicon element is 1% to 50%; wherein the first doped element oxide layer is the doped element oxide layer; a second doped element oxide layer, the second doped element oxide layer being located on a surface of the first doped element oxide layer; A first electrode is formed, wherein the first electrode is located on the passivation structure and is electrically connected to the emitter.
8. The method for preparing a solar cell according to claim 7, It is characterized in that The surface of the substrate has a processed area and a non-processed area, and the emitter and the passivation structure are located in the processed area and the non-processed area: before forming the first electrode, it also includes: removing the emitter and the passivation structure located in the processed area to form a passivation layer, the passivation layer is located in the processed area, and the first electrode is located in the non-processed area.
9. The method for preparing a solar cell according to claim 7, It is characterized in that The process parameters for forming the second doped element oxide layer include: a process temperature of 25° C. to 400° C., and a reaction time of 1 s to 500 s.
10. A photovoltaic module, It is characterized in that include: A battery string, formed by connecting a plurality of solar cells according to any one of claims 1 to 6 or a plurality of solar cells prepared by the preparation method according to any one of claims 7 to 9; A packaging film, used to cover the surface of the battery string; The cover plate is used to cover the surface of the packaging film facing away from the battery string.
Citation Information
Cited By
Solar cell and manufacturing method thereof, laminated cell and photovoltaic module
CN120417496A
Solar cell and method of manufacturing the same, stacked cell, and photovoltaic module
CN120417496B