By forming a special-shaped structure and suede on the first glass incident surface of the photovoltaic module, and setting a raised structure on the reflective film, combining coating tempering and multi-objective optimization processes, the low power generation efficiency of the photovoltaic module under low light conditions is solved. The problem of low-light response performance is significantly improved.

CN118919588AInactive Publication Date: 2024-11-08JIANGSU HYPERION PHOTOVOLTAIC TECHNOLOGY CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202410922326.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-10
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The power generation efficiency of existing photovoltaic modules under low light conditions is low, mainly because the light transmittance and reflectance will decrease when the incident angle changes, resulting in a loss of radiation. The existing technology means are relatively single, making it difficult to effectively improve the weak light. response.

Method used

By forming a plurality of special-shaped structures and suede on the incident surface of the first glass and setting up a raised structure on the surface of the reflective film, combining coating tempering and multi-objective optimization processes, the light transmittance and reflectance are enhanced, and the photovoltaic module can be enhanced. Low light response.

Benefits of technology

The power generation efficiency of photovoltaic modules under low-light conditions is improved, the light transmittance and reflectivity are increased through suede, the light utilization and radiation amount are improved, and the weak light response performance is significantly improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919588A_ABST
    Figure CN118919588A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of photovoltaics, and discloses a high-weak light response photovoltaic module, which comprises first glass, a battery piece, a reflecting film and second glass which are arranged in sequence, a plurality of special-shaped structures are formed on the incident plane of the first glass, and suede surfaces are formed on the special-shaped structures; a plurality of protrusions are formed on the surface of the reflecting film, and the surfaces of the protrusions are cambered surfaces. The textured surface is formed on the special-shaped structure, the optical path can be increased through the textured surface, and the light transmittance of light penetrating through the first glass is improved; the textured surface is a rough surface formed by a plurality of small particles, and after light irradiates the small particles, the probability that the light penetrates through the first glass can be increased, so that the radiation quantity of the photovoltaic module is improved, the utilization rate of light can be improved under the condition of weak light, and then the weak light response of the photovoltaic module is improved; light rays are incident to the protrusions, an included angle is formed between the reflected light rays after primary reflection and the incident light rays, the reflected light rays are easily reflected to the surfaces of the battery pieces, and the reflectivity can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of photovoltaic technology, and more specifically to a photovoltaic component with high weak light response. Background Art

[0002] Photovoltaic modules are important components of photovoltaic power stations. The more fully the photovoltaic modules utilize light, the higher the power generation. Improving the utilization rate of light is an important means to increase the power generation of photovoltaic modules.

[0003] The weak light response of a photovoltaic module refers to its performance under weak light conditions, that is, the power generation efficiency of the photovoltaic module. There are many factors that affect the weak light response of a photovoltaic module, one of which is the structural design of the photovoltaic module. The structure of the photovoltaic module will affect its utilization of light; light enters the glass and EVA (transparent colloid) from the air and reaches the surface of the cell. In this process, the light enters the optically sparse medium into the optically dense medium. In this case, the transmittance and reflectivity of the light change with the change of the incident angle. When the incident angle is 0 (vertical incidence), the transmittance of the light is the largest and the reflectivity is the lowest. As the incident angle gradually increases, the transmittance of the light gradually decreases and the reflectivity gradually increases, resulting in radiation loss.

[0004] In the prior art, in order to improve the light transmittance of glass, the angle of the glass surface morphology is usually adjusted to improve the light transmittance, thereby improving the weak light response, and the means are relatively simple.

[0005] Therefore, it is necessary to provide a photovoltaic module with high weak light response to at least partially solve the problems existing in the prior art. Summary of the invention

[0006] A series of simplified concepts are introduced in the Summary of the Invention, which will be further described in detail in the Detailed Description of the Invention. The Summary of the Invention does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.

[0007] In order to at least partially solve the above-mentioned problems, the present invention provides a photovoltaic component with high weak light response, comprising: a first glass, a battery cell, a reflective film and a second glass arranged in sequence; the incident surface of the first glass is formed with a plurality of special-shaped structures, and a velvet surface is formed on the special-shaped structures; the surface of the reflective film is formed with a plurality of protrusions, and the surface of the protrusions is a curved surface.

[0008] Preferably, the incident surface of the first glass forms a plurality of special-shaped structures after a first etching, and forms a velvet surface on the special-shaped structures after a second etching.

[0009] Preferably, the first glass is subjected to secondary etching and then to coating and tempering to form a tempered film layer on the incident surface.

[0010] Preferably, the reflective film comprises: a diffuse reflective layer, a substrate layer and an adhesive layer which are arranged in sequence, the adhesive layer is connected to the second glass, and the diffuse reflective layer is formed by a plurality of evenly arranged protrusions.

[0011] Preferably, the first glass and the battery cell are connected via a first adhesive film, and an edge of the battery cell close to the second glass and an edge of the reflective film close to the first glass are both connected via a second adhesive film.

[0012] Preferably, the special-shaped structure is: a groove A with a triangular cross section, a plurality of grooves A are evenly arranged on the incident surface of the first glass, and the surface of the groove A forms a velvet surface.

[0013] Preferably, the special-shaped structure is an inverted pyramid-shaped groove B, a plurality of grooves B are evenly distributed on the incident surface of the first glass, and the surface of the grooves B forms a velvet surface.

[0014] Preferably, the first etching and the second etching of the first glass are performed by wet etching or dry etching.

[0015] Preferably, when both the first etching and the second etching of the first glass are wet etching, the first etching of the first glass uses a hydrofluoric acid etching solution with a volume fraction of 40%-50% at room temperature, and the etching time is 30s-60s; the second etching of the first glass uses a hydrofluoric acid etching solution with a volume fraction of 2%-4% at room temperature, and the etching time is 30s-60s.

[0016] Preferably, the velvet surface is formed on the surface of the special-shaped structure with a set particle density and a set etching depth; wherein the set particle density and the set etching depth of the velvet surface satisfy the condition that the light transmittance of the first glass is a maximum value.

[0017] Preferably, the setting of the grain density and the etching depth of the velvet surface comprises:

[0018] Acquire design data of the first glass, wherein the design data includes multiple sets of velvet structure parameter data and corresponding transmittance data, construct a velvet structure parameter variation space, establish a transmittance evaluation model, and train the transmittance evaluation model using the design data;

[0019] The velvet surface structural parameters include: velvet surface particle density and etching depth;

[0020] Based on the transmittance evaluation model, transmittance evaluation parameters and their optimization direction, a multi-objective optimization function is established:

[0021] R_MAX x∈Q f(x)=[f1(x),f2(x),f3(x)]

[0022] Among them, R_MAX x∈Q f(x) represents the solution set that maximizes the value of f(x) from the variable space formed by x, R is a vector, MAX is the maximum value, x is the structural parameter of the velvet, Q is the variation space of the velvet structural parameter, f(x) is the objective function to be optimized, f1(x), f2(x), f3(x) represent the first sub-objective function, the second sub-objective function and the third sub-objective function respectively;

[0023] Among them, the first sub-objective function is:

[0024] f1(x)=E n-1 (x)+α n σ m-1 (x)

[0025] Among them, E n-1 (x) and σ n-1 (x) are the expected value of the predicted transmittance and the standard deviation of the predicted transmittance corresponding to the structural parameter x of the velvet surface at the n-1th optimization iteration, respectively. n is the exploration coefficient of the nth optimization iteration;

[0026] The second sub-objective function is:

[0027]

[0028] Among them, f′ n-1 is the maximum expected value of the predicted transmittance in the design data at the n-1th optimization iteration, is the probability cumulative function of the standard Gaussian distribution, τ() is the probability density function of the standard Gaussian distribution;

[0029] The third sub-objective function is:

[0030]

[0031] Among them, E n-1 (x) and σ n-1 (x) are all obtained by inputting the structural parameters x of the suede into the trained transmittance evaluation model;

[0032] Setting a first setting range of the grain density of the suede surface and a second setting range of the etching depth as constraint conditions of the multi-objective optimization function;

[0033] A multi-objective genetic algorithm is used to solve the multi-objective optimization function and constraint conditions, and the optimal structural parameters of the suede are used as the set particle density and set etching depth of the suede.

[0034] Compared with the prior art, the present invention has at least the following beneficial effects:

[0035] The photovoltaic module with high weak light response described in the present invention forms a velvet surface on the special-shaped structure, which can increase the optical path and improve the transmittance of light passing through the first glass; the velvet surface is a rough surface formed by multiple small particles. After the light is irradiated on the small particles, it can increase the probability of the light passing through the first glass, thereby increasing the radiation amount of the photovoltaic module. In this way, under weak light conditions, the utilization rate of light can also be improved, thereby improving the weak light response of the photovoltaic module; when the light is incident on the protrusion, the reflected light after one reflection forms an angle with the incident light, and is more easily reflected to the surface of the battery cell, which can improve the reflectivity.

[0036] The photovoltaic module with high weak light response described in the present invention, other advantages, objectives and features of the present invention will be reflected in part through the following description, and in part will be understood by technicians in this field through research and practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:

[0038] Figure 1 This is a schematic structural diagram of a photovoltaic module with high weak light response according to the present invention;

[0039] Figure 2 A process flow chart for manufacturing the first glass in the photovoltaic module with high weak light response according to the present invention;

[0040] Figure 3 It is a schematic diagram of the propagation path of light incident on the first glass surface in the photovoltaic module with high weak light response of the present invention;

[0041] Figure 4 A schematic diagram of the propagation path of light incident on the first glass surface in a photovoltaic module of the prior art;

[0042] Figure 5 It is a schematic diagram of the structure of the reflective film in the photovoltaic module with high weak light response according to the present invention;

[0043] Figure 6 It is a schematic diagram of the structure of a reflective film in a photovoltaic module in the prior art;

[0044] Figure 7 It is a schematic diagram of the propagation path of light rays incident on the first glass surface at different incident angles in the photovoltaic module with high weak light response of the present invention;

[0045] Figure 8 It is a schematic diagram comparing the relationship between the incident angle and the radiation amount of the photovoltaic module with high weak light response described in the present invention and the photovoltaic module with conventional structure. DETAILED DESCRIPTION

[0046] The present invention is further described in detail below in conjunction with the accompanying drawings and embodiments so that those skilled in the art can implement the invention with reference to the description.

[0047] It should be understood that the terms such as “having”, “including” and “comprising” used herein do not exclude the existence or addition of one or more other elements or combinations thereof.

[0048] like Figure 1 , Figure 2 and Figure 5 As shown, the present invention provides a photovoltaic module with high weak light response, comprising: a first glass 1, a battery cell 2, a reflective film 3 and a second glass 4 arranged in sequence; the incident surface of the first glass 1 is formed with a plurality of special-shaped structures 5, and a velvet surface 6 is formed on the special-shaped structures 5; the surface of the reflective film 3 is formed with a plurality of protrusions 311, and the surface of the protrusion 311 is a curved surface.

[0049] When sunlight shines on the first glass 1, it enters from the special-shaped structure 5 on the incident surface. Under the action of the velvet surface 6, the incident light forms a multi-directional reflection, and part of the reflected light can enter from the special-shaped structure 5 again, thereby increasing the light transmittance of the first glass 1, so that more light can shine on the battery cell 2, and reducing the probability of reflected light being reflected from the first glass 1; while in the conventional structure (such as Figure 4 As shown), after the light is incident on the special-shaped structure 5, a part of the light with a larger incident angle is easily reflected. The present invention is different from the conventional structure in that Figure 3 As shown, a velvet surface 6 is formed on the special-shaped structure 5, and the velvet surface 6 can increase the optical path and improve the transmittance of light passing through the first glass 1; the velvet surface 6 is a rough surface formed by a plurality of small particles, and after the light irradiates the small particles, the probability of the light passing through the first glass 1 can be increased, thereby increasing the radiation amount of the photovoltaic module. In this way, the utilization rate of light can also be improved under weak light conditions, thereby improving the weak light response of the photovoltaic module;

[0050] like Figure 7 As shown, the light reflection situation when sunlight is incident on the surface of the first glass 1 at different incident angles θ (θ=0°, θ=35.3°, θ=54.7°) is shown. It can be seen that under the action of the velvet surface 6, the light will be scattered, and a part of the scattered light will be reflected to the special-shaped structure 5 again, which can increase the reflection optical path of the light at the special-shaped structure 5, thereby improving the light transmittance of the first glass 1.

[0051] After the light transmitted through the first glass 1 is incident on the reflective film 3, it is reflected by the multiple protrusions 311 formed on the surface of the reflective film 3. Since the surface of the protrusion is a curved surface, the light can be reflected onto the battery cell 2 at one time to improve the reflectivity.

[0052] like Figure 6 As shown, in the conventional structure, the cross section of the protruding structure on the surface of the reflective film 3 is a triangle, and part of the light (such as the vertically incident light) is incident on the protruding structure, and after two reflections, it cannot irradiate the surface of the battery cell 2. The present invention is different from the conventional structure in that Figure 5 As shown, the light is incident on the protrusion 311, and after one reflection, the reflected light forms an angle with the incident light, and is more easily reflected to the surface of the battery cell 2, which can improve the reflectivity.

[0053] The comparison of the power generation gain results of the photovoltaic modules corresponding to the conventional structure and the photovoltaic modules corresponding to the present invention is shown in the following table:

[0054] The present invention conventional sunny 0.50% 0% cloudy day 1.20% 0% rain 2.30% 0%

[0055] It can be seen that on cloudy or rainy days under weak light conditions, the weak light response of the photovoltaic module of the present invention is higher, which can improve the power generation efficiency of the photovoltaic module under weak light conditions.

[0056] like Figure 8 As shown, the angle and radiation amount (i.e. Figure 8 From the comparison results of the IAM marked in the figure, it can be seen that when the incident angle is larger, the radiation amount of the photovoltaic module of the present invention is higher than that of the photovoltaic module of the conventional structure. In this way, it can ensure that the light transmittance of the glass is improved, so that more light can be irradiated onto the battery cell 2, thereby improving the power generation efficiency.

[0057] like Figure 5 As shown, further, the reflective film 3 includes: a diffuse reflective layer 310, a substrate layer 320 and an adhesive layer 330 arranged in sequence, the adhesive layer 330 is connected to the second glass 4, and the diffuse reflective layer 310 is formed by a plurality of evenly arranged protrusions 311.

[0058] Since there are multiple cells 2 arranged on the photovoltaic module, there is a gap distance between adjacent cells 2, and the reflective film 3 is arranged at the gap. When light is incident from the first glass 1 to the gap distance, it will be reflected by the reflective film 3;

[0059] The diffuse reflection layer 310 is used to reflect the light incident from the first glass 1, reflects the light onto the first glass 1, and then reflects the light onto the battery cell 2 through the first glass 1. The adhesive layer 330 is used to connect with the second glass 4. The diffuse reflection layer 310 is formed by a plurality of evenly arranged protrusions 311. The surface of the protrusion 311 is an arc-shaped surface, which can improve the reflectivity and increase the probability of light being reflected onto the battery cell 2.

[0060] like Figure 1 As shown, further, the first glass 1 and the battery cell 2 are connected via a first adhesive film 8, and the edge of the battery cell 2 close to the second glass 4 and the edge of the reflective film 3 close to the first glass 1 are connected via a second adhesive film 9.

[0061] The first adhesive film 8 connects the first glass 1 to the battery cell 2 and leaves a gap therebetween, so as to reflect the light reflected by the reflective film 3 onto the battery cell 2 . The second adhesive film 8 connects the reflective film 3 to the battery cell 2 to fix the battery cell 2 .

[0062] like Figure 2 As shown, in one embodiment, the incident surface of the first glass 1 is etched once to form a plurality of special-shaped structures 5, and a velvet surface 6 is formed on the special-shaped structures 5 after a second etching.

[0063] The first etching and the second etching of the first glass 1 are performed by wet etching or dry etching.

[0064] When wet etching is used, the first glass 1 is etched once at room temperature using a hydrofluoric acid etching solution with a volume fraction of 40%-50%, and the etching time is 30s-60s; the first glass 1 is etched twice at room temperature using a hydrofluoric acid etching solution with a volume fraction of 2%-4%, and the etching time is 30s-60s.

[0065] The manufacturing process of the first glass 1 is different from the conventional process in that Figure 2 As shown, the incident surface needs to be etched twice. After the first etching, a plurality of special-shaped structures 5 are formed on the surface of the original glass sheet of the first glass 1. After the second etching, a velvet surface 6 is formed on the surface of the special-shaped structure 5. The velvet surface 6 is a plurality of tiny particles formed on the surface of the special-shaped structure 5. The tiny particles can increase the light transmittance of the first glass 1 and improve the radiation amount, thereby improving the power generation efficiency of the photovoltaic module under weak light conditions.

[0066] The structure of the special-shaped structure 5 can be the following two:

[0067] In the first type, the special-shaped structure 5 is a groove A with a triangular cross section, a plurality of grooves A are evenly arranged on the incident surface of the first glass 1 , and a velvet surface 6 is formed on the surface of the groove A.

[0068] In the second type, the special-shaped structure 5 is an inverted pyramid-shaped groove B, a plurality of grooves B are evenly distributed on the incident surface of the first glass 1 , and the surface of the grooves B forms a velvet surface 6 .

[0069] Both of the above structures can ensure that the first glass 1 has good light transmittance.

[0070] In one embodiment, the first glass 1 is subjected to secondary etching and then to coating and tempering to form a tempered film layer 7 on the incident surface.

[0071] In order to improve the protective performance of the first glass 1, after secondary etching, a coating liquid is coated on the surface of the first glass 1, and then high-temperature tempering is performed at a temperature of 500 degrees Celsius to 600 degrees Celsius to form a tempered film layer 7 to protect the incident surface.

[0072] In one embodiment, the velvet surface 6 is formed on the surface of the special-shaped structure 5 with a set particle density and a set etching depth; wherein the set particle density and the set etching depth of the velvet surface 6 satisfy the condition that the transmittance of the first glass 1 is a maximum value.

[0073] The particle density of velvet 6 refers to the ratio of the area occupied by the multiple particles forming velvet 6 to the total area of ​​velvet 6, and the etching depth of velvet 6 refers to the depth of the grooves formed between adjacent particles. The larger the particle density of velvet 6, the greater the probability of light being incident on the particles, thereby increasing the optical path. The light reflected from the particles is preferably reflected into the grooves formed between adjacent particles, thereby reducing the probability of light being reflected to the outside of the first glass 1. However, when the particle density increases to a certain extent, the probability of reflection into the grooves decreases. The greater the depth of the grooves, the longer the optical path of light reflected on the first glass 1. However, when the groove depth increases to a certain extent, the optical path will not change. Therefore, the particle density and etching depth of velvet 6 need to be set to ensure that the light transmittance of the first glass 1 is maximized.

[0074] Furthermore, the present invention also provides a method for determining a set particle density and a set etching depth of the velvet surface 6, comprising:

[0075] Acquire design data of the first glass 1, wherein the design data includes multiple sets of velvet structure parameter data and corresponding transmittance data, construct a velvet structure parameter variation space, establish a transmittance evaluation model, and train the transmittance evaluation model using the design data;

[0076] The structural parameters of the velvet surface 6 include: the particle density and etching depth of the velvet surface 6;

[0077] Based on the transmittance evaluation model, transmittance evaluation parameters and their optimization direction, a multi-objective optimization function is established:

[0078] R-MAX x∈Qf(x)=[f1(x),f2(x),f3(x)]

[0079] Among them, R-MAX x∈Q f(x) represents the solution set that maximizes the value of f(x) from the variable space formed by x, R is a vector, MAX is the maximum value, x is the structural parameter of velvet 6, Q is the variation space of velvet structural parameters, f(x) is the objective function to be optimized, f1(x), f2(x), f3(x) represent the first sub-objective function, the second sub-objective function and the third sub-objective function respectively;

[0080] Among them, the first sub-objective function is:

[0081] f1(x)=E n-1 (x)+α n σ m-1 (x)

[0082] Among them, E n-1 (x) and σ n-1 (x) are the expected value of the predicted transmittance and the standard deviation of the predicted transmittance corresponding to the structural parameter x of the velvet surface 6 at the n-1th optimization iteration, respectively. n is the exploration coefficient of the nth optimization iteration;

[0083] The second sub-objective function is:

[0084]

[0085] Among them, f′ n-1 is the maximum expected value of the predicted transmittance in the design data at the n-1th optimization iteration, is the probability cumulative function of the standard Gaussian distribution, τ() is the probability density function of the standard Gaussian distribution;

[0086] The third sub-objective function is:

[0087]

[0088] Among them, E n-1 (x) and σ n-1 (x) are all obtained by inputting the structural parameters x of the velvet surface 6 into the trained transmittance evaluation model;

[0089] Setting a first setting range of the particle density of the suede surface 6 and a second setting range of the etching depth as constraint conditions of the multi-objective optimization function;

[0090] A multi-objective genetic algorithm is used to solve the multi-objective optimization function and the constraint conditions, and the optimal structural parameters of the suede 6 are obtained as the set particle density and the set etching depth of the suede 6.

[0091] Among them, the transmittance evaluation model is established using Gaussian process regression.

[0092] Multiple groups of textured surface structural parameter data of the first glass 1 can be obtained through the established three-dimensional model of the first glass 1, and the corresponding transmittance data can be obtained by performing optical simulation on the three-dimensional model of the first glass 1 corresponding to each group of textured surface structural parameter data, and the established transmittance evaluation model is trained using the above design data to obtain a trained transmittance evaluation model;

[0093] Then, a multi-objective optimization function is established based on the transmittance evaluation model, transmittance evaluation parameters and their optimization direction. The transmittance evaluation parameters include transmittance, and the corresponding optimization direction is to improve the transmittance. The constraint conditions are that the particle density is within the first set range, and the etching depth is within the second set range.

[0094] Through the first sub-objective function, the maximum confidence upper limit value of the transmittance evaluation target variable (transmittance) can be improved, through the second sub-objective function, the expectation maximization of the transmittance evaluation parameter (transmittance) can be maximized, and through the third sub-objective function, the probability of the transmittance evaluation parameter (transmittance) can be maximized.

[0095] Through the above method, the transmittance can be maximized, the optimal particle density and etching depth of the velvet surface 6 can be obtained, and the secondary etching process can be determined using the optimal particle density and etching depth, thereby increasing the radiation of the photovoltaic module and further improving the power generation efficiency of the photovoltaic module under weak light conditions.

[0096] In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0097] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection, an electrical connection, or communication with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0098] Although the embodiments of the present invention have been disclosed as above, they are not limited to the applications listed in the specification and the implementation methods. They can be fully applied to various fields suitable for the present invention. For those familiar with the art, additional modifications can be easily implemented. Therefore, without departing from the general concept defined by the claims and the scope of equivalents, the present invention is not limited to the specific details and the illustrations shown and described herein.

Claims

1. A photovoltaic module with high weak light response, characterized in that: include: A first glass (1), a battery cell (2), a reflective film (3), and a second glass (4) are arranged in sequence; a plurality of special-shaped structures (5) are formed on the incident surface of the first glass (1), and a velvet surface (6) is formed on the special-shaped structures (5); a plurality of protrusions (311) are formed on the surface of the reflective film (3), and the surface of the protrusions (311) is a curved surface.

2. The photovoltaic module with high weak light response according to claim 1, characterized in that: The incident surface of the first glass (1) is etched once to form a plurality of special-shaped structures (5), and velvet surfaces (6) are formed on the special-shaped structures (5) after secondary etching.

3. The photovoltaic module with high weak light response according to claim 2, characterized in that: After the first glass (1) is etched twice, it is coated and tempered to form a tempered film layer (7) on the incident surface.

4. The photovoltaic module with high weak light response according to claim 1, characterized in that: The reflective film (3) comprises: a diffuse reflective layer (310), a substrate layer (320) and an adhesive layer (330) which are arranged in sequence, the adhesive layer (330) being connected to the second glass (4), and the diffuse reflective layer (310) being formed by a plurality of evenly arranged protrusions (311).

5. The photovoltaic module with high weak light response according to claim 1, characterized in that: The first glass (1) and the cell sheet (2) are connected via a first adhesive film (8), and the edge of the cell sheet (2) close to the second glass (4) and the edge of the reflective film (3) close to the first glass (1) are both connected via a second adhesive film (9).

6. The photovoltaic module with high weak light response according to claim 1, characterized in that: The special-shaped structure (5) is: a groove A with a triangular cross section, a plurality of grooves A are evenly arranged on the incident surface of the first glass (1), and the surface of the groove A forms a velvet surface (6).

7. The photovoltaic module with high weak light response according to claim 1, characterized in that: The special-shaped structure (5) is an inverted pyramid-shaped groove B, a plurality of grooves B are evenly distributed on the incident surface of the first glass (1), and the surface of the grooves B forms a velvet surface (6).

8. The photovoltaic module with high weak light response according to claim 2, characterized in that: The first etching and the second etching of the first glass (1) are performed by one or more of wet etching and dry etching.

9. The photovoltaic module with high weak light response according to claim 8, characterized in that: When both the first etching and the second etching of the first glass (1) are wet etching, the first etching of the first glass (1) uses a hydrofluoric acid etching solution with a volume fraction of 40%-50% at room temperature, and the etching time is 30s-60s; the second etching of the first glass (1) uses a hydrofluoric acid etching solution with a volume fraction of 2%-4% at room temperature, and the etching time is 30s-60s.

10. The photovoltaic module with high weak light response according to claim 1, characterized in that: The velvet surface (6) is formed on the surface of the special-shaped structure (5) with a set particle density and a set etching depth; wherein the set particle density and the set etching depth of the velvet surface (6) satisfy the condition that the light transmittance of the first glass (1) is the maximum value.

Citation Information

Patent Citations

  • Cover plate glass of solar photovoltaic cell

    CN101950766A

  • Photovoltaic reflecting thin-film

    CN102751344A

  • Concentrating glass plate with micro-nano composite suede, and production process and application thereof

    CN112103369A

  • Solar cell module

    JP2010074053A

  • A prism glass structure for enhancing the performance of sollar cell module

    KR100934358B1