Glass assembly having hydrophobic properties by gaseous release of hydrophobic compounds contained in emitter

By placing emitters around a transparent substrate to release hydrophobic compounds, the problems of short service life and complex maintenance of fluorinated silane coatings are solved, achieving the durability and predictability of continuous hydrophobic coatings, and reducing environmental risks and maintenance costs.

CN118922389APending Publication Date: 2024-11-08SAINT GOBAIN SULLY
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202380023942.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-02-28
Filing Date
2023-02-27
Publication Date
2024-11-08

Smart Images

  • Figure HDA0005012692790000011
    Figure HDA0005012692790000011
  • Figure HDA0005012692790000012
    Figure HDA0005012692790000012
  • Figure HDA0005012692790000013
    Figure HDA0005012692790000013
Patent Text Reader

Abstract

The invention relates to a glazing comprising a transparent substrate, characterized in that it comprises, at the periphery of the substrate, at least one emitter of a hydrophobic compound through a gaseous process; the at least one emitter is arranged to be capable of releasing the hydrophobic compound, and a portion of the released hydrophobic compound is capable of being deposited on a surface of the transparent substrate. The invention also relates to the use of such a glazing as described above as a rainproof glazing which can be used as a glazing for buildings, land vehicles, aircrafts or ships, or urban furniture, preferably as an aircraft cockpit glazing. The invention also relates to a method of hydrophobizing a glazing as described above.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to glazing, in particular glazing, comprising a transparent substrate, the outer surface of which is rendered hydrophobic by the gaseous release of a hydrophobic compound contained in an emitter located at the periphery of said substrate. The invention particularly relates to rainproof glazing for buildings, land vehicles, aircraft or ships, or urban furniture.

[0002] Hydrophobic properties are sought for windows and windshields in the transport sector, in particular for motor vehicles and aircraft, and for glazing in the building industry. For transport applications, rain protection properties are sought, since water collected on the glazing and upstream areas of the vehicle must flow easily in the form of droplets or trickles onto the glass wall in order to be transferred, for example, under the influence of air and wind while driving, in order to improve visibility and thus safety, or to facilitate cleaning, easy defrosting, etc.

[0003] For this purpose, it is sought that the contact angle of the water drop with the substrate is greater than 60° or 70° and preferably greater than 90°, so that the water drop does not crush or spread until a continuous film is formed. In fact, as long as this angle is greater than 60° for aviation and greater than 70° for motor vehicles, the glazing is said to be functional. In order to make the glass substrate hydrophobic, it is known to deposit a hydrophobic fluorinated silane type grafting compound on its outer surface, as described in patent application US 4,983,459. It is also known to cover the glass with an inorganic layer, which acts as a primer to graft the fluorinated silane molecules, the inorganic layer being a dense silicon dioxide layer, such as the layer described in patent EP 0545201, or a sol-gel silicon dioxide layer, such as described in patent EP 799873, or even a layer of activated silicon, such as the layer described in patent application WO 2005 / 084943. However, these hydrophobic coatings by grafting fluorinated silanes onto the outer surface of the glass substrate pose risks to health and the environment due to the fluorinated compounds; in addition, they are threatened by regulatory restrictions. In addition, these coatings tend to degrade over time due to the stresses that the glazing is constantly subjected to, such as: hydrolysis, photodegradation, sensitivity to the effects of atmospheric dust, sensitivity to electrostatic discharge, etc. As a result, these hydrophobic fluorinated silane coatings have a short service life, especially in flight, for example, about 6 months when applied to the windshield of a short-haul commercial aircraft. The thickness of the hydrophobic coating on the glazing surface can be increased to extend its service life. In addition, this strategy is adopted in the case of hydrophobic varnishes. However, these coatings are sensitive to scratches; this also limits their service life, and the overall optical quality of the glazing will also deteriorate. In addition, these visible scratches are generally not repairable and may require the replacement of the glazing. Thus, thick functionalized coatings (>100nm) should not be considered as a solution to the above-mentioned problems.

[0004] In addition, the performance loss of the coating of the compound grafted with the hydrophobic fluorinated silane type is very difficult to predict because, as mentioned above, it is highly dependent on the climate and atmospheric conditions (exposure to dust, electrostatic surface discharge events, salt water environment, etc.). In particular, the regeneration of the fluorinated silane-based solutions used in aviation glazing is very complicated. In fact, the maintenance of such glazing requires intervention to prevent rainwater from easily contacting the glazing, as well as good lighting to ensure good final optical quality, and a heating system to improve the fixation of the fluorinated silane. This also requires the occupation of the hangar and often leads to temporary interruptions in the commercial operation of the aircraft. In addition, the chemical products are used by specially trained operators, and the reagents prepared by these operators have a short service life, making the process sensitive to changes in deposition and to ambient temperature. In other words, poor control of deposition conditions can lead to a shortened service life of the hydrophobic functionalization of the regenerated fluorinated silane.

[0005] Overall, these fluorinated silane solutions tend to degrade over time and result in maintenance costs, logistical complexity, and reduced commercial aircraft availability to airlines.

[0006] The inventors have therefore sought to develop glazings comprising a transparent substrate, preferably for glazings for aircraft such as airplanes, which have continuous hydrophobic properties and in which the regeneration of the hydrophobic properties of said substrate is easily achieved. Advantageously, the inventors have sought to provide glazings having improved hydrophobic properties, in particular in terms of their durability and predictability, while maintaining other properties, such as resistance to mechanical stresses (friction resistance, wear resistance and wiping resistance, etc.); resistance to climatic stresses (resistance to UVA and UVB, neutral salt spray, acid rain, etc.); and retention of optical properties, in particular when the glazing is a glass article. Even more preferably, the inventors have sought to use volatile hydrophobic compounds so that they can be applied continuously to the outer surface of the transparent substrate of the glazing, without the need for maintenance intervention, in other words, by continuous regeneration of the hydrophobic functions on the surface of said substrate.

[0007] The inventors have thus proposed that a hydrophobic compound is delivered by a gaseous process directly from an emitter located at the periphery of a transparent substrate of a glazing to the outer surface of said substrate. Thus, the object of the present invention is to provide a glazing (1) comprising a transparent substrate (S), said glazing comprising at least one emitter (2) of a hydrophobic compound by a gaseous process at the periphery of the substrate; said at least one emitter being arranged to release said hydrophobic compound and a portion of said released hydrophobic compound being able to be deposited on the surface of said transparent substrate.

[0008] In fact, the inventors have surprisingly found that the gaseous release of a hydrophobic compound contained in at least one emitter located at the periphery of a transparent substrate of a glazing makes it possible to render the outer surface of said substrate hydrophobic. It has further been observed that this hydrophobic property is maintained over time; as long as the flow balance between those hydrophobic compounds that arrive at the surface and come from the emitters or from the environment on the one hand and those that leave for the various reasons already mentioned (such as hydrolysis, evaporation, corrosion, etc.) on the other hand allows the retention of a sufficient amount of hydrophobic compound, which can be approximated as a fraction of a molecular monolayer of the hydrophobic compound. By generating a flow of hydrophobic compound emitted by the emitters and adding to the natural flow, and / or by a particularly strong affinity between the substrate surface and the hydrophobic compound, the maintenance of a sufficient amount of hydrophobic compound on the surface of the transparent substrate is thus improved according to the invention. By this mechanism, the emitters associated with the air flow on the surface of the transparent substrate ensure continuous regeneration of the surface with the hydrophobic compound and, therefore, ensure improved hydrophobic properties of the substrate. If necessary, it may be necessary to regenerate the emitters by replacing them or reloading them with hydrophobic compound.

[0009] The invention is illustrated using the following non-limiting drawings:

[0010] -Attached Figure 1 ( Figure 1 ) schematically shows a glazing (1) according to the present invention;

[0011] -Attached Figure 2 ( Figure 2 ) and 3( Figure 3 ) schematically show glazings (1) according to the invention, each glazing comprising an example of a substrate (S) and an emitter (2) which in both figures comprises at least one reservoir (20) in solid form serving as an emitting surface;

[0012] -Attached Figure 4 ( Figure 4 ) schematically shows a glazing ( 1 ) according to the invention, wherein the emitter ( 2 ) comprises a reservoir ( 20 ′) and an emitting surface ( 21 );

[0013] -Attached Figure 5a ( Figure 5a ) and 5b( Figure 5b ) schematically shows a glazing (1) comprising an emitter (2) comprising a reservoir (20') and an emitting surface (21) in the form of a film (210) or a plate (212) provided with at least one opening;

[0014] -Attached Figure 6 [ Figure 6 ] schematically shows an example of a glazing (1) according to the present invention;

[0015] -Attached Figure 7 ( Figure 7 ) and 8( Figure 8 ) schematically shows a glazing (1) according to the invention, comprising a frame (3) in which a transparent substrate (S) is mounted and at which an emitter (2) is arranged at the level of the frame (3).

[0016] The transparent substrate (S) of the glazing (1) according to the present invention may comprise:

[0017] - a sheet of material selected from glass, glass ceramics, polymers, such as Figure 2 as shown in, or

[0018] - a laminated assembly of at least two plies (S1, S2), said plies being made of the same or different materials, said materials being selected from glass, glass ceramics, polymers, such as Figure 3 as shown in .

[0019] According to the invention, “glass” is understood to mean inorganic glass, in particular of the soda-lime-silica, borosilicate or aluminosilicate type.

[0020] The polymer may be selected from polycarbonate (PC), poly(methyl methacrylate) (PMMA), polyurethane (PU) and polyethylene terephthalate (PET).

[0021] In the case of a laminated assembly, the plies (S1, S2) are laminated or assembled with the aid of an intermediate layer (S3). The intermediate layer (S3) may comprise one or more adhesive layers of a polymer material. The polymer material is preferably selected from thermoplastic polyurethane (TPU), polyvinyl butyral (PVB), poly(ethylene-vinyl acetate) (EVA), silicone and ionomer resins. Several different types of adhesive layers may be used on the same glazing between two consecutive or different pairs of plies and between the same consecutive pairs of plies.

[0022] In a preferred embodiment, the glazing (1) is a laminated glazing, the substrate (S) of which comprises at least two glass plies (S1, S2), which are bonded or assembled via an adhesive interlayer (S3) of the thermoplastic polyurethane, polyvinyl butyral or poly(ethylene vinyl acetate) type.

[0023] In another preferred embodiment, the glazing is a laminated glazing, the substrate of which comprises at least one ply of poly(methyl methacrylate) (PMMA), preferably at least two PMMA plies bonded or assembled via an adhesive interlayer as described above.

[0024] In yet another preferred embodiment, the glazing is a laminated glazing, the substrate of which comprises at least one ply of polycarbonate (PC), preferably at least two plies of PC bonded or assembled by an adhesive interlayer as described above.

[0025] However, other embodiments are also possible, such as glazing comprising at least one sheet layer of polyethylene terephthalate (PET) and an adhesive layer of thermoplastic polyurethane (TPU) or polyvinyl butyral (PVB).

[0026] In the present invention, Figure 1 and 2 As shown in, the glazing (1) includes a transparent substrate (S) and at least one emitter (2) of a hydrophobic compound through a gaseous process, which is located at the periphery of the transparent substrate. In the present application, "emitter" is understood to refer to a gas diffusion system. Therefore, the emitter is designed to generate / emit gases and supply them to the transparent substrate, and in particular to supply them to a layer capable of adsorbing hydrophobic compounds. In the present application, "periphery" is understood to refer to the area corresponding to the connection or interface between the transparent substrate and the structure on which the substrate is placed, on one side of the substrate or on one side of the structure, and preferably upstream of the air flow. It can also be away from this area (boundary), limited by the visible area on one side of the substrate, and extend even further upstream of the air flow on one side of the structure. However, positioning close to the transparent substrate, particularly in the lower part of the glazing, is preferred. When the structure is a structure of a vehicle, this positioning is particularly advantageous because it improves the efficiency of the use of the hydrophobic compound by utilizing the air flow on the surface of the substrate (usually caused by the speed of the vehicle) to sweep over the surface of the air loaded with the hydrophobic compound.

[0027] More specifically, in the case of glazing of aircraft, the emitters are located in the glazing-aircraft interface region, on the glazing side or on the aircraft side and upstream of the air flow sweeping over the glazing under flight conditions.

[0028] In a first configuration of the invention, the glazing comprises an emitter extending around the entire periphery of the substrate.

[0029] In a second configuration of the invention, the glazing comprises at least two emitters, which are arranged to extend around the entire periphery of the substrate.

[0030] In a third configuration of the invention, the glazing comprises one or at least two emitters at the periphery of the substrate, but which do not extend around the entire periphery of the substrate.

[0031] The emitters according to the invention may have a linear geometry, for example in the form of strips or slots, or consist of a plurality of point emission sites, for example in the form of holes. Furthermore, the emitters may be integrated into a transparent substrate or into a structure carrying a transparent substrate.

[0032] In a first embodiment, the emitter (2) according to the invention comprises at least one reservoir (20) in solid form serving as an emission surface, such as Figure 2 and Figure 3 shown.

[0033] The reservoir (20) may then be flush and / or non-flush with the surface of the glazed transparent substrate and may include:

[0034] - According to a first alternative, at least one pure hydrophobic compound or several hydrophobic compounds in the form of a mixture, preferably in solid form. According to this alternative, the hydrophobic compound is emitted by sublimation at the outer surface of the substrate, that is: at the surface of the substrate exposed to the air, so that the emission can be amplified by air convection; or

[0035] -According to a second alternative, at least one hydrophobic compound dissolved and / or dispersed in a polymer matrix. The polymer matrix may comprise a polymer selected from polysulfides, epoxies, polyurethanes, silicones and rubbers. According to this alternative, the one or more hydrophobic compounds dissolved and / or dispersed in the polymer matrix are in the form of solid particles or droplets diffused into the matrix, whereupon the hydrophobic compound is desorbed and emitted in the gas phase onto the outer surface of the substrate. The polymer matrix helps to protect the hydrophobic compound, which, if not encapsulated by the matrix, can settle when in liquid state at high use temperatures, at least under certain conditions of use. The polymer matrix also protects the hydrophobic compound from dissolving in certain fluids (being eroded), rain or dust, or

[0036] -According to a third alternative, at least one hydrophobic compound is embedded in a porous matrix, in other words, one or more hydrophobic compounds fill the pores of the porous matrix. The porous matrix can be a metal, a ceramic or a sintered glass. Optionally, the porous matrix can be essentially composed of a polymer and, for example, in the form of a sponge or a seal. The porous matrix can be an open pore matrix. Advantageously, the pore size of the matrix is ​​1 μm to 0.1 mm to prevent rainwater from penetrating into the reservoir. This open pore porous matrix physically separates the reservoir from the outside air and allows the hydrophobic compound to diffuse through the open pores. This is followed by desorption, and the hydrophobic compound in the gas phase is then emitted toward the outer surface of the substrate. The hydrophobic compound filling the open pores of the matrix is ​​in liquid or solid form.

[0037] In a second embodiment, the emitter (2) according to the invention comprises a reservoir (20') and an emission surface (21), the reservoir (20') being a volume in communication with the emission surface (21), such as Figure 4 In other words, in this second embodiment, the reservoir (20') and the emitting surface (21) of the emitter (2) are separated. The volume of the reservoir may then contain at least one hydrophobic compound, which:

[0038] - in solid form, or

[0039] - in liquid form, or

[0040] - dissolved and / or dispersed in a polymer matrix, or

[0041] -Embedded in a porous matrix.

[0042] In the specific case of a reservoir (20') comprising at least one hydrophobic compound in liquid form, the reservoir may further comprise a compound that does not have hydrophobic properties, such as a solvent or a solid filler. If necessary, elements such as fibers, powders or porous particles may be added to the reservoir to prevent the liquid compound from flowing by capillary mechanisms. The reservoir (20') is thus designed to be able to deliver the hydrophobic compound in liquid form to the emitting surface (21) flush with the outer surface of the substrate by direct contact.

[0043] In the specific case where the reservoir (20') contains at least one hydrophobic compound in solid form, dissolved and / or dispersed in a polymer matrix, or embedded in a porous matrix, as described in the first embodiment, gas phase emission of the hydrophobic compound towards the outer surface of the substrate is carried out through the emission surface (21).

[0044] The emitting surface (21) according to the invention may comprise:

[0045] - at least one membrane (210), and / or

[0046] - at least one plate (212) having at least one opening.

[0047] According to a first alternative, the emitting surface (21) comprises at least one film (210) such as Figure 5aAs shown. The membrane according to the invention may consist essentially of at least one polymer selected from polysulfide, polyurethane, polyvinyl chloride and rubber. Advantageously, the membrane is solid; it is thus a permeable membrane. The use of the membrane as an emission surface enables the emission of hydrophobic compounds by absorption on one side of the reservoir, followed by diffusion into the membrane, subsequent desorption and emission of said hydrophobic compounds in the gas phase on the face of the substrate exposed to the external air (called the outside or external face of the substrate), with the advantage of better control or regulation of the gas phase release of the hydrophobic compound towards the external surface of the substrate.

[0048] According to a second alternative, the emission surface (21) comprises at least one plate (212) having at least one opening, such as Figure 5b or Figure 6 The plate may be a metal plate pierced by one or more slots or by a plurality of holes. These slots or these openings may all be identical, or there may be openings or slots of different sizes and shapes.

[0049] According to a third alternative, the emission surface (21) comprises at least one film (210) according to the first alternative and at least one plate (212) according to the second alternative.

[0050] Furthermore, the emitter (2) may comprise a protective layer for the emitting surface (21), said protective layer being made of a porous material. The porous material is a material selected from the group consisting of ceramics, metal foams, sintered glass and polymer foams.

[0051] In the particular case where the emitting surface (21) comprises at least one membrane (210) or a membrane (210) and a plate (212) having at least one opening, the porous material is placed above the membrane, the membrane itself covering the opening in the plate if necessary. The purpose of this protective layer is to protect the membrane from the abrasive external environment without hindering the gaseous transport of the hydrophobic compound.

[0052] In another particular case, when the emitting surface (21) comprises at least one plate (212) provided with at least one opening, said porous material can cover said opening in the plate, acting as a "stopper" for filling with a hydrophobic compound. The filling can be carried out with a liquid hydrophobic compound by pouring it directly into the porous material (which can have the function of a tap). The stopper or stoppers can then be reached without removing the glazing.

[0053] In a preferred embodiment of the present invention, when the reservoir (20') comprises at least one hydrophobic compound in liquid form, the emitter (2) may further comprise at least one channel (22) connecting the emitting surface to the reservoir, such as Figure 8 This allows the emitter to include a larger reservoir so that a larger amount of liquid hydrophobic compound can be stored.

[0054] According to this embodiment, the emitter may also comprise diffusion means for supplying the entire emitting surface. The diffusion means may for example take the form of a cavity to which the entire emitting surface and the channel are connected.

[0055] According to a second embodiment, the emitting surface (21) can extend in particular over the entire periphery of the transparent substrate and more preferably over all or part of the length of the bottom support of the glazing (1) with a width of up to 3 cm. In the case of emission through several fine holes with a diameter of 0.05 mm to 2 mm, the emitting surface can also be partially up to one millionth of its surface.

[0056] According to the first and second specific embodiments described above, the reservoir (20) or (20') may be in the form of a profile or a sphere or a parallelepiped or any other shape. The reservoir may consist essentially of a material selected from elastomers such as rubber, thermoplastic polymers such as polyvinyl chloride, or metals such as steel or aluminum.

[0057] More particularly, the emitter according to the invention also provides the function of a peripheral seal for the glazing, generally known as a "bead". In fact, it is known that the bead provides the glazing with aerodynamic continuity between the glazing and the mounting structure (for example the aircraft structure), as well as good inertness towards process fluids (for example aviation fluids, cleaning products, degreasers, glycols for ground deicing, etc.); this bead can be made of polysulfide or equivalent.

[0058] According to the invention, the glazing (1) may further comprise at least one heating device. The heating device is preferably located in or around the emitter (2) so as to be able to heat by heat conduction: the reservoir (20) or (20'), the emitting surface (21) and, where applicable, any element allowing the transport of the hydrophobic compound from the reservoir to the emitting surface, such as a channel (22) or a duct. The heating can be achieved using a resistive wire or a resistive layer. The heating device can in particular be placed directly opposite the emitter. Alternatively, the heating device can be located in the transparent substrate (S) of the glazing (1). In the case of a laminated assembly, the heating device is placed inside the laminate, preferably in contact with the glass layer facing outwards. The heating device can take the form of a transparent conductive layer, typically based on ITO or a wire based on copper, nickel, an iron-nickel alloy or tungsten with a diameter of 20 μm to 40 μm.

[0059] In the case of glazing for aircraft, heating devices are very useful. In fact, convection and low pressure under flight conditions significantly accelerate the evaporation of hydrophobic compounds compared to ground conditions. On the other hand, the low temperatures encountered in flight significantly reduce the partial pressure of hydrophobic compounds and therefore significantly reduce the molecular flux through gaseous processes. For this reason, the heating device optimizes the preferential emission of hydrophobic compounds in the flight phase, which tends to bring the compounds to the glazing, compared to the emission of hydrophobic compounds when the aircraft is on the ground.

[0060] Furthermore, the heating device prevents the emitters from being clogged by frost.

[0061] According to the invention, the glazing (1) may further comprise a frame (3) in which the transparent substrate (S) is mounted. The frame (3) may be a metal profile or a polymer seal.

[0062] In the case of glazing for vehicles, the frame is either an integral part of the vehicle or, as previously mentioned, is the element in which the substrate is mounted and the assembly thus formed of frame and transparent substrate is subsequently installed in the vehicle.

[0063] In a preferred embodiment, the frame (3) is used to arrange the transmitter (2). In practice, the frame (3) can be arranged to carry the transmitter (2), such as Figure 7 and Figure 8 as shown, or arranged so that the emitter is placed at the interface between the substrate and the frame.

[0064] As previously mentioned, the glazing (1) according to the invention comprises a transparent substrate (S) and at least one emitter (2) of a hydrophobic compound by a gaseous process positioned at the periphery of the substrate; said at least one emitter is arranged to be able to release said hydrophobic compound and a portion of said released hydrophobic compound is able to be deposited on the surface of said transparent substrate. In the present application, "by a gaseous process" is understood to mean that the hydrophobic compound is transported between the emitter and the glazing in the form of gaseous molecules, affected by the phenomenon of being carried by the air flow and diffusing in the gaseous medium. As mentioned above, the emitter can contain pure hydrophobic compounds, or diluted hydrophobic compounds in the case where these hydrophobic compounds are dissolved and / or dispersed in a polymer matrix or embedded in a porous matrix. Subsequently, said hydrophobic compound is either: directly exposed to the air (when the emitter comprises a reservoir in solid form acting as an emission surface), or transported to an emission surface, such as a film or a plate provided with openings (when the emitter comprises a reservoir and an emission surface). Thus, geometrically, the emission surface of the hydrophobic compound can take a variety of forms. In the case of continuous emission or multiple emission areas along a support for glazing, the emission surface can be compared to an equivalent strip characterized by an equivalent slot width that produces the same contaminant flow. The emission surface thus produces a flow of hydrophobic compounds that is less than or equal to the flow emitted by the same surface consisting essentially of pure compounds. For example, an emission surface comprising 20 mm openings associated with a product diluted at 10% is equivalent to an emission surface with 2 mm openings for pure compounds. A person skilled in the art thus knows that the flow of hydrophobic compounds is weighted relative to the emission surface, the dilution ratio, etc.

[0065] Additionally, the emitting surface may be a strip placed around the perimeter of the transparent substrate of the glazing, or one or more sections (or one or more pieces) placed around the perimeter of the substrate, which also changes the vapor pressure of the hydrophobic compound of the emitter. One skilled in the art will take this variable into account and make adjustments in each case to obtain the correct vapor partial pressure for the release of the hydrophobic compound.

[0066] Therefore, according to the invention, the hydrophobic compound of the emitter preferably has a hydrophobicity of 10 mm to 30 mm for emitters with large emitting surfaces. -8 Pa to 1 Pa, more preferably 10 -8 Pa to 10 -6 Pa vapor pressure, and advantageously 10 for emitters with small emitting surfaces of 10 μm to 3 mm. -2 Pa to 1 Pa. These partial pressures are determined at a temperature ranging from 20° C. to 30° C., more preferably at a temperature equal to 25° C. Such a low vapor pressure, suitable for the emitting surface, allows the hydrophobic compound to evaporate in a sufficiently high amount to be able to functionalize the transparent substrate, while being limited so as to minimize the consumption of the hydrophobic compound.

[0067] Once the hydrophobic compound is emitted by the emitter through a gaseous process, it becomes part of an air flow running parallel to the transparent substrate of the glazing. In this air flow, the hydrophobic compound can diffuse, and in particular diffuse in the direction normal to the surface of the glazing, so that a portion of the compound moves away from the glazing and is lost, while a portion of the compound is redirected to the outer surface of the transparent substrate, where they can be adsorbed. Thus, some or a portion of the hydrophobic compound released by the emitter condenses on the surface of the glazing, giving it hydrophobic properties.

[0068] The hydrophobic compound of the emitter according to the invention is preferably selected from:

[0069] (a) Carboxylic acid of formula (I): R-COOH

[0070] Where R represents a linear, branched or cyclic, saturated or unsaturated C4-C 22 Alkyl, preferably R is an alkyl of formula (A): C n H 2n+1 , where n is 6 to 20, or

[0071] (b) Phosphate of formula (II): RO-PO(OH)2

[0072] Where R represents a linear, branched or cyclic, saturated or unsaturated C4-C 22 Alkyl, preferably R is an alkyl of formula (A): C n H 2n+1 , where n is 6 to 20, or

[0073] (c) Phosphonic acid of formula (iii): R-PO(OR')(OR")

[0074] Where R, R' and R" represent hydrogen atoms, C4-C 22 Alkyl or aryl, preferably R, R' and R" are alkyl of formula (A): C n H 2n+1 , where n is 6 to 20, or

[0075] (d) silicone,

[0076] (e) kerosene, or

[0077] (f) mixtures thereof.

[0078] More preferably, the hydrophobic compound is selected from carboxylic acids of formula (IA): n H 2n+1-COOH, where n is between 7 and 19. In the specific case of large emitting surfaces, the preferred carboxylic acid is stearic acid (n equal to 17), since this hydrophobic compound has the advantage of being inexpensive, of not being a risk to health or the environment, and of being sufficiently volatile. And in the specific case of small emitting surfaces, obtained, for example, by puncturing openings in a plate with openings of 0.1 mm in diameter, spaced a few millimeters from each other and aligned parallel to the edge of the glass, the preferred carboxylic acid is decanoic acid (n equal to 9), since this hydrophobic compound has the advantage of being a liquid, which allows the reservoir to be refilled easily, while still being a safe and inexpensive compound.

[0079] In fact, the inventors have selected hydrophobic compounds which:

[0080] -is volatile enough to evaporate, vaporize or sublime readily,

[0081] - chemically stable to avoid polymerization, and

[0082] -Resistant to weather or atmospheric conditions such as oxidation, UV rays, neutral salt spray, etc.

[0083] The transparent substrate (S) of the glazing (1) may further comprise on its outer surface at least one layer capable of adsorbing hydrophobic compounds. For the purposes of the present invention, the outer (or "exterior") face corresponds to the face of the transparent substrate facing the exterior of the building or vehicle.

[0084] The layer capable of adsorbing hydrophobic compounds may comprise:

[0085] - at least one oxide or nitride of a lanthanide element or an alloy of at least two lanthanides, the lanthanide element being selected from lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), promethium (Pm), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb), lutetium (Lu), or

[0086] - at least one oxide or nitride of a metal or an alloy of at least two metals, the metal being selected from scandium (Sc), yttrium (Y), titanium (Ti), zirconium (Zr), hafnium (Hf), or

[0087] - at least one oxide or nitride of an alloy comprising a lanthanide element and a metal selected from the above list.

[0088] Advantageously, the layer capable of adsorbing hydrophobic compounds consists essentially of a material selected from cerium oxide (CeO x ), gadolinium oxide (Gd), yttrium oxide (YO x ), titanium oxide (TiO x ), zirconium oxide (ZrO x) or hafnium oxide (HfO x )’s material composition.

[0089] Also, examples of the alloy include the following mixed oxides such as TiYO x ,Hf x 、HfZrO x ,ZrYO x or GdYO x .

[0090] Furthermore, it should be noted that the layer capable of adsorbing a hydrophobic compound according to the invention is deposited on the outer surface of the transparent substrate by a physical vapor deposition (PVD) or chemical vapor deposition (CVD) method, such as sputtering, or by evaporation or by atomic layer deposition (ALD) or alternatively by a liquid sol-gel type process.

[0091] The layer capable of adsorbing the compound may have a thickness of 5 to 1000 nm, preferably 6 to 200 nm, and more preferably 7 to 30 nm.

[0092] The present inventors have found that at least one layer capable of adsorbing a hydrophobic compound placed on the outer surface of a substrate makes it possible to promote the adsorption of the hydrophobic compound after the hydrophobic compound is diffused and transported due to air flow.

[0093] The transparent substrate may further comprise at least one additional layer on its outer surface which does not have the function of adsorbing volatile hydrophobic compounds. For example, the additional layer may have electrically dissipative properties. The additional layer may be placed above or below the at least one layer capable of adsorbing hydrophobic compounds. The additional layer preferably consists essentially of a material selected from tin oxide or indium tin oxide.

[0094] The glazing (1) according to the invention is advantageously used as rain protection glazing and even more advantageously as glazing for buildings, land vehicles, aircraft or ships, or urban furniture, preferably as aircraft cockpit glazing.

[0095] The present invention also relates to a method for hydrophobizing a glazing (1) as described above, comprising the following steps:

[0096] - In 2×10 4 Pa to 10 5 The hydrophobic compound is released from the emitter (2) in a gaseous state at a pressure of Pa,

[0097] - depositing a portion of said released hydrophobic compound on the transparent substrate using a stream or flow of air running parallel to said transparent substrate and at a speed of at least 70 m / s.

[0098] During the method, part of the hydrophobic compound released by the emitter condenses on the surface of the glazing, giving it hydrophobic properties. It can be understood from this that, by means of the emitter, the glazing according to the invention can be hydrophobized and this hydrophobization can be renewed over time. In fact, the emitter associated with the air flow on the surface of the transparent substrate ensures a continuous regeneration of the surface with the hydrophobic compound and therefore ensures improved hydrophobic properties of the substrate.

Claims

1. A glazing (1) comprising a transparent substrate (S), characterized in that It comprises at the periphery of the substrate at least one emitter (2) of a hydrophobic compound by a gaseous process; The at least one emitter is arranged to release the hydrophobic compound, and A portion of the released hydrophobic compound can be deposited on the surface of the transparent substrate.

2. The glazing according to claim 1, characterized in that The transparent substrate (S) comprises: - a sheet of material selected from glass, glass ceramic, polymer, or - A laminated assembly of at least two plies (S1, S2), said plies being made of the same or different materials, said materials being chosen from glass, glass ceramics, polymers.

3. The glazing according to claim 1 or 2, characterized in that The transparent substrate (S) further comprises, on its outer surface, at least one layer capable of adsorbing a hydrophobic compound.

4. The glazing according to claim 3, wherein the layer capable of adsorbing hydrophobic compounds comprises: - at least one oxide or nitride of a lanthanide element or an alloy of at least two lanthanides, the lanthanide element being chosen from lanthanum, cerium, praseodymium, neodymium, promethium, samarium, europium, gadolinium, terbium, dysprosium, holmium, erbium, thulium, ytterbium, lutetium, or - at least one oxide or nitride of a metal or an alloy of at least two metals selected from scandium, yttrium, titanium, zirconium, hafnium, or - at least one oxide or nitride of an alloy comprising a lanthanide element and a metal selected from the above list. 5 . The glazing according to claim 3 , wherein the layer capable of adsorbing hydrophobic compounds has a thickness of 5 to 1000 nm, preferably 6 to 200 nm, and more preferably 7 to 30 nm.

6. Glazing according to any one of the preceding claims, characterized in that The emitter comprises at least one reservoir (20) in solid form acting as an emission surface, the reservoir (20) comprising: - at least one hydrophobic compound in pure form or in the form of a mixture of several hydrophobic compounds, or - at least one hydrophobic compound dissolved and / or dispersed in the polymer matrix, or - At least one hydrophobic compound embedded in the porous matrix.

7. The glazing according to any one of claims 1 to 5, characterized in that The emitter comprises a reservoir (20') and an emission surface (21), the reservoir being a volume in communication with the emission surface.

8. The glazing according to claim 7, characterized in that The volume of the reservoir (20') comprises at least one hydrophobic compound, said hydrophobic compound: - in solid form, or - in liquid form, or - dissolved and / or dispersed in a polymer matrix, or -Embedded in a porous matrix.

9. The glazing according to any one of claims 7 or 8, characterized in that The emitting surface (21) comprises: - at least one membrane (210), and / or - at least one plate (212) having at least one opening.

10. The glazing according to any one of claims 7 to 9, characterized in that The emitter (2) comprises a protective layer for the emitting surface (21), the protective layer being made of a porous material.

11. The glazing according to any one of claims 8 to 10, characterized in that When the reservoir (20') contains at least one hydrophobic compound in liquid form, the emitter (2) further comprises at least one channel (22) connecting the emission surface (21) to the reservoir (20').

12. The glazing according to claim 11, characterized in that The emitter (2) further comprises a diffusion device.

13. Glazing according to any one of the preceding claims, characterised in that It further comprises at least one means for heating said emitter.

14. Glazing according to any one of the preceding claims, characterized in that It further comprises a frame (3) in which the transparent substrate (S) is mounted.

15. The glazing according to claim 14, characterized in that The frame (3) is arranged to also carry the transmitter (2).

16. Glazing according to any one of the preceding claims, characterised in that The hydrophobic compound of the emitter (2) has a hydrophobicity of 10 at a temperature of 20°C to 30°C. -8 Pa to 1Pa vapor pressure.

17. Glazing according to any one of the preceding claims, characterized in that The hydrophobic compound of the emitter (2) is selected from: (a) Carboxylic acid of formula (I): R-COOH Where R represents a linear, branched or cyclic, saturated or unsaturated C4-C 22 Alkyl, preferably R is an alkyl of formula (A): C n H 2n+1 , where n is 6 to 20, or (b) Phosphate of formula (II): RO-PO(OH)2 Where R represents a linear, branched or cyclic, saturated or unsaturated C4-C 22 Alkyl, preferably R is an alkyl of formula (A): C n H 2n+1 , where n is 6 to 20, or (c) Phosphonic acid of formula (III): R-PO(OR')(OR") Where R, R' and R" represent hydrogen atoms, C4-C 22 Alkyl or aryl, preferably R, R' and R" are alkyl of formula (A): C n H 2n+1 , where n is 6 to 20, or (d) silicone, (e) kerosene, or (f) mixtures thereof.

18. Use of the glazing (1) according to any one of the preceding claims as rain protection glazing.

19. Use of the rainproof glazing according to claim 18 as glazing for buildings, land vehicles, aircraft or ships, or urban furniture, preferably as glazing for aircraft cockpits.

20. Method for hydrophobizing a glazing (1) according to any one of claims 1 to 17, comprising the following steps: - In 2×10 4 Pa to 10 5 The hydrophobic compound is released from the emitter (2) in a gaseous state at a pressure of Pa, - depositing a portion of said released hydrophobic compound on the transparent substrate using a stream or flow of air running parallel to said transparent substrate and at a speed of at least 70 m / s.

Citation Information

Patent Citations

  • Textured hydrophobic / hydrophilic substrate able to be used in a glazing unit has relief formed of a collection of identical or different objects perpendicular to the plane of the substrate

    FR2792628A1

  • Method of rendering materials water repellent

    US2306222A

  • Rain repellent compositions, method of application and base coated therewith

    US2962390A

  • Rain repellent application system for an aircraft windshield

    US3231196A

  • Lidar detection device provided with a releasable protective layer

    WO2020127335A1