Preparation method of cortex electrode, cortex electrode and electronic device

By integrating pressure sensors and temperature sensors on cortical electrodes, the problems of cranial brain damage and insufficient monitoring caused by traditional cortical electrode size are solved, real-time monitoring of the intracranial environment and neural signal recording are achieved.

CN118924301APending Publication Date: 2024-11-12SHANGHAI INST OF MICROSYSTEM & INFORMATION TECH CHINESE ACAD OF SCI
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202410990899.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

Traditional cortical electrodes cause brain damage due to size and lack real-time monitoring of mild intracranial pressure, making it impossible to fully evaluate and decode neural signals.

Method used

Using silicon-based mask plate and pre-stretched protein membrane, a pressure sensor and a temperature sensor are formed by evaporating metal, and the conductive structural area is integrated to achieve real-time monitoring of the intracranial environment.

Benefits of technology

It realizes real-time monitoring of mild intracranial pressure while recording cortical nerve electrical signals, ensuring the stability of the sensor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118924301A_ABST
    Figure CN118924301A_ABST
Patent Text Reader

Abstract

The invention relates to the field of biological material processing and brain function detection, in particular to a cortical electrode preparation method, a cortical electrode and an electronic device.The method comprises the steps that a silicon-based mask containing a first device pattern and a second device pattern opening area and a first protein film are obtained, and the first protein film and the silicon-based mask are temporarily fixed; the first protein film is a pre-stretched oriented curled film; evaporating metal on the surface of the first protein film by taking the silicon-based mask as a mask so as to form a device area on the first protein film; the device area comprises a pressure sensor and a temperature sensor; separating the first protein film from the silicon-based mask; according to the cortical electrode and the preparation method thereof, in-vivo recording of cortical electroneurographic signals is achieved, meanwhile, key data such as intracranial temperature and intracranial pressure are monitored in real time, in addition, by means of the good deformability of the first protein film, the detection accuracy is improved, and the detection accuracy is improved. And the device stability of the pressure sensor and the temperature sensor can be ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of biomaterial processing and brain function detection, and in particular to a method for preparing a cortical electrode, a cortical electrode and an electronic device. Background Art

[0002] Brain monitoring technology can collect EEG signals, which helps decode brain functions. With the development of brain monitoring technology, it has also promoted the development of a series of high-tech technologies based on it, such as brain-computer interfaces and neural regulation. Generally, methods for collecting neural signals mainly rely on brain cortical electrodes. Due to their size, traditional cortical electrodes usually have a large craniotomy area, which can easily cause craniocerebral damage to the implanted individual. In addition, they lack monitoring of key indicators of the cranial environment such as intracranial temperature and intracranial pressure during postoperative recovery and signal acquisition. Therefore, it is impossible to comprehensively evaluate and decode neural signals in combination with the real-time intracranial status of the implanted individual. Summary of the invention

[0003] In order to solve the above technical problems, the present invention provides a method for preparing a cortical electrode, comprising:

[0004] Obtain a silicon-based mask, wherein the silicon-based mask includes an opening area of ​​a first device pattern and a second device pattern; the first device pattern is used to define a pressure sensor area; and the second device pattern is used to define a temperature sensor area;

[0005] Obtaining a first protein film, and temporarily fixing the first protein film to a silicon-based mask; the first protein film is a pre-stretched directional curled film;

[0006] Using a silicon-based mask as a mask, evaporating metal on the surface of the first protein film to form a device area on the first protein film; the device area includes a pressure sensor and a temperature sensor;

[0007] separating the first protein film from the silicon-based mask;

[0008] A second protein film is obtained, and the encapsulation area of ​​the first protein film is encapsulated by the second protein film to obtain a target cortical electrode.

[0009] Furthermore, the silicon-based mask also includes an opening area of ​​a third device pattern;

[0010] The third device pattern is used to define the conductive structure area of ​​the target cortical electrode; the conductive structure area includes the electrode detection site and the back-end connection site.

[0011] Furthermore, obtaining a silicon-based mask includes:

[0012] Obtaining a silicon wafer; a first oxide layer is formed on a first surface of the silicon wafer, and a second oxide layer is formed on a second surface of the silicon wafer;

[0013] Coating a photoresist on the first oxide layer and patterning it to form a patterned photoresist layer;

[0014] Based on the patterned photoresist layer, deep etching is performed from the oxide layer on the first surface to the second oxide layer to form opening areas of the first device pattern and the second device pattern;

[0015] The second oxide layer is removed to obtain a silicon-based mask.

[0016] Further, obtaining a second protein film, and encapsulating the encapsulation area of ​​the first protein film with the second protein film to obtain the target cortical electrode includes:

[0017] obtaining a second protein film, and performing plasma treatment on the surface of the second protein film;

[0018] Cutting the second protein film after the plasma treatment so that the size of the cut second protein film is adapted to the size of the encapsulation area;

[0019] The cut second protein film is covered on the encapsulation area of ​​the first protein film, and water cross-linked to obtain the target cortical electrode.

[0020] Furthermore, the metal material includes one or a combination of gold, magnesium, iron, and molybdenum.

[0021] On the other hand, the present invention provides a cortical electrode prepared by the cortical electrode preparation method as described above, the cortical electrode comprising a first protein film and a second protein film; the first protein film is formed with a pressure sensor and a temperature sensor; the second protein film is used to encapsulate the encapsulation area of ​​the first protein film.

[0022] Furthermore, the pressure sensor is a first curved serpentine resistor; the resistance of the pressure sensor increases as the pressure increases.

[0023] Further, the bending axis dimensions of the pressure sensor include 2219 μm*530 μm.

[0024] Furthermore, the temperature sensor is a second curved serpentine resistor; the resistance of the temperature sensor increases linearly with increasing temperature.

[0025] Further, the bending axis size of the temperature sensor includes 250 μm*1070 μm.

[0026] On the other hand, the present invention also provides an electronic device, which is formed by packaging the above-mentioned cortical electrode and the back-end circuit.

[0027] The technical solution provided by the embodiment of the present invention has the following technical effects:

[0028] The cortical electrode prepared by the present invention forms a pressure sensor and a temperature sensor by evaporating metal on a pre-stretched first protein film through a silicon-based mask plate, thereby realizing in vivo recording of cortical neural electrical signals while monitoring key data such as intracranial temperature and intracranial pressure in real time. In addition, the good deformability of the first protein film can ensure the device stability of the pressure sensor and the temperature sensor. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the technical solutions and advantages in the embodiments of the present invention or the prior art, the drawings required for use in the embodiments or the prior art descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0030] Figure 1 It is a schematic flow chart of a method for preparing a cortical electrode provided by an embodiment of the present invention;

[0031] Figure 2 It is a schematic diagram of a device region and a conductive structure region of a cortical electrode provided by an embodiment of the present invention;

[0032] Figure 3a-Figure 3i It is a schematic diagram of the structural change process of a method for preparing a cortical electrode provided in an embodiment of the present invention.

[0033] Figure numerals: 100 - silicon wafer; 101 - first oxide layer; 102 - second oxide layer; 110 - silicon-based mask; 200 - first protein film; 300 - metal; 400 - second protein film. DETAILED DESCRIPTION

[0034] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0035] It should be noted that the "one embodiment" or "embodiment" referred to in the description of the embodiment of the present invention refers to a specific feature, structure or characteristic that can be included in at least one implementation of the present invention. It should be understood that in the description and claims of the embodiment of the present invention and the above-mentioned drawings, the orientation or position relationship indicated by the terms "upper", "lower", "top", "bottom", etc. is based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. The terms "first" and "second" are used only for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. Moreover, the terms "first", "second", etc. are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, in the description of the present embodiment, unless otherwise specified, "plurality" means two or more. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system or product including a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0036] In order to make the purpose, technical solution and advantages disclosed in the embodiments of the present invention more clearly understood, the embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the embodiments of the present invention and are not used to limit the embodiments of the present invention.

[0037] Due to their size, traditional cortical electrodes usually have a large craniotomy area, which can easily cause craniocerebral damage to the implanted individual, and lack monitoring of key indicators of the cranial environment such as intracranial temperature and intracranial pressure during postoperative recovery and signal acquisition. Therefore, it is impossible to comprehensively evaluate and decode neural signals in combination with the real-time intracranial status of the implanted individual. Therefore, the present invention provides a cortical electrode that integrates an intracranial temperature sensor and a pressure sensor to make up for the lack of intracranial environment monitoring by the cortical electrode during postoperative recovery and neural EEG signal recording stages. Next, the preparation method of the cortical electrode of the present invention is specifically introduced.

[0038] See also Figure 1 , which is a schematic diagram of a method for preparing a cortical electrode provided by an embodiment of the present invention, such as Figure 1As shown in the figure, the preparation method includes S101-S105:

[0039] S101: Obtain a silicon-based mask, wherein the silicon-based mask includes an opening area of ​​a first device pattern and a second device pattern; the first device pattern is used to define a pressure sensor area; and the second device pattern is used to define a temperature sensor area.

[0040] Specifically, the present invention integrates a pressure sensor and a temperature sensor on a cortical electrode for detecting intracranial pressure and intracranial temperature. The target cortical electrode is made of a protein film. The pressure sensor and the temperature sensor are prepared on the protein film, and metal is evaporated through a mask. A silicon-based mask is used, and the silicon-based mask has an opening area of ​​a first device pattern and a second device pattern to form a mask pattern, wherein the first device pattern is used to define the pressure sensor area; the second device pattern is used to define the temperature sensor area. The opening area of ​​the first device pattern and the second device pattern can be determined on the silicon-based mask based on the shape, size and arrangement position of the pressure sensor and the temperature sensor.

[0041] In a possible implementation, the silicon-based mask further includes an opening area of ​​a third device pattern; the third device pattern is used to define a conductive structure area of ​​a target cortical electrode; the conductive structure area includes an electrode detection site and a back-end connection site.

[0042] Specifically, the silicon-based mask also includes an opening area of ​​the third device pattern, which is used to define the conductive structure area of ​​the target cortical electrode. The conductive structure area includes electrode detection sites and rear-end connection sites for recording electrical signals and obtaining physiological signals. The opening area of ​​the third device pattern can be determined on the silicon-based mask based on the shape, size and position of the conductive structure area. The third device pattern includes but is not limited to one or a combination of regular shapes such as rectangles, diamonds, circles, polygons, etc., and can also be an irregular shape opening, which is specifically determined according to the conductive structure area. Exemplarily, the conductive structure area is provided with a four-channel detection site, the site diameter is set to 150μm, and the distance between two adjacent detection sites is 500μm.

[0043] In a possible implementation, for obtaining a silicon-based mask, step S101 may include the following steps:

[0044] (1) obtaining a silicon wafer; a first oxide layer is formed on a first surface of the silicon wafer, and a second oxide layer is formed on a second surface of the silicon wafer;

[0045] (2) coating a photoresist on the first oxide layer and patterning the layer to form a patterned photoresist layer;

[0046] (3) based on the patterned photoresist layer, etching deeply from the oxide layer on the first surface to the second oxide layer to form an opening area of ​​the first device pattern and the second device pattern;

[0047] (4) Remove the second oxide layer to obtain a silicon-based mask.

[0048] Specifically, a silicon wafer of suitable thickness is selected. Exemplarily, the thickness of the silicon wafer is selected to be 200μm. In other possible embodiments, the silicon wafer substrate can be adjusted according to actual needs, all within the scope of protection of the present invention. The silicon wafer has a first surface and a second surface relative to each other, and there is no specific order between the first surface and the second surface. The first surface and the second surface are thermally oxidized respectively to form a first oxide layer on the first surface and a second oxide layer on the second surface of the silicon wafer. Exemplarily, the thermal oxidation treatment can be a wet thermal oxidation method, the temperature of the thermal oxidation treatment is 1000℃-1150℃, and the time is 0-24 hours. In other embodiments, the method of forming the first silicon oxide layer and the second silicon oxide layer may also include a vapor deposition method. The first oxide layer and the second oxide layer are silicon oxide. Exemplarily, the thickness of the first oxide layer and the second oxide layer is 2μm.

[0049] Next, a photolithography step is performed to coat photoresist on the first oxide layer, and a region for photoresist patterning is determined according to the first device pattern, the second device pattern and the third device pattern, and the photoresist is patterned to form a patterned photoresist layer.

[0050] Then, based on the patterned photoresist layer, the first oxide layer is first etched to form etching areas of the first device pattern, the second device pattern and the third device pattern in the first oxide layer. Exemplarily, the method for etching the first silicon oxide layer can be to use reactive ion etching technology in dry etching, use chemically reactive gases to generate chemically active groups and ions, and bombard the first oxide layer with high-energy ions accelerated by an electric field for etching. Chemically reactive gases may include but are not limited to hydrogen fluoride, tetrafluoromethane or hydrogen. In other possible embodiments, ion beam etching of the first oxide layer can be used. Ion beam etching is a physical etching process, and the general gas source is an inert gas such as argon, which bombards the sample surface with inert ions. The ion beam can act more accurately on the patterned photoresist layer for etching, and the etching of the first oxide layer is achieved by the relative movement of the ion beam and the silicon wafer substrate.

[0051] Based on the etching area, the silicon wafer is subjected to deep silicon etching, and the etching depth is to etch to the second oxide layer. The deep silicon etching can also adopt the reactive ion etching technology in dry etching, or the inductively coupled plasma (ICP) etching technology, to form the first oxide layer on the silicon wafer to form the opening area of ​​the first device pattern, the second device pattern and the third device pattern. Wet etching can also be adopted to gradually etch and dissolve the silicon wafer and the chemical etching solution through chemical reaction. There are many reagents for wet etching, such as acidic etching agents, alkaline etching agents and organic etching agents. By controlling factors such as the dosage of the etching agent and the etching time, the etching thickness can reach the thickness of the entire silicon wafer substrate, so the etching depth reaches the second oxide layer, and the first oxide layer is formed on the silicon wafer to form the opening area of ​​the first device pattern, the second device pattern and the third device pattern.

[0052] Finally, the second oxide layer and the remaining first oxide layer are removed to obtain a silicon-based mask. The first oxide layer and the second oxide layer can be removed by wet etching with BOE (Buffered Oxide Etch), that is, the first oxide layer and the second oxide layer are etched with a mixture of hydrofluoric acid and nitric acid, and then stripped.

[0053] S102: Obtain a first protein film, and temporarily fix the first protein film to a silicon-based mask; the first protein film is a pre-stretched directional curled film.

[0054] Specifically, the first protein film is the main material for forming the target cortical electrode. The first protein film can be prepared by standing and volatilizing a prefabricated protein solution. The protein solution is coated on a hard surface, such as a flat silicon wafer, at a certain spin coating speed, and is left to stand for a period of time until the protein solution evaporates and forms a film to obtain a protein film. The first protein film can also be water-crosslinked to change its molecular structure, improve the thermal stability and mechanical strength of the protein film, and then pre-stretched. The water-crosslinked protein film can be stretched according to the winding direction of the cortical electrode on the target object, such as the cranial nerves of experimental animals, and the target directional crystallization direction, and then fixed on a preset fixture and left to stand to obtain a stretched directional curled film, i.e., the first protein film.

[0055] S103: using the silicon-based mask plate as a mask, evaporating metal on the surface of the first protein film to form a device area on the first protein film; the device area includes a pressure sensor and a temperature sensor.

[0056] Specifically, when the first protein film and the silicon-based mask are in a dry state, the first protein film is temporarily fixed to the silicon substrate. Exemplarily, the temporary fixing method can be to align the first protein film and the silicon-based mask and then stick them together with tape. Using the silicon-based mask as a mask, metal is evaporated on the surface of the first protein film based on the opening areas of the first device pattern, the second device pattern, and the third device pattern. Electron beam evaporation can be selected to evaporate a metal with better conductivity on the surface of the first protein film under vacuum conditions to form a device area and a conductive structure area on the first protein film. The device area includes a pressure sensor and a temperature sensor, and the conductive structure area includes a conductive structure area. For details, please refer to Figure 2 shown.

[0057] In a possible implementation, the metal material includes one or a combination of gold, magnesium, iron, and molybdenum. For example, the pressure sensor and the temperature sensor may be made of gold with excellent ductility and conductivity to avoid device breakage, and the conductive structure area may be made of safe metals such as magnesium, iron, and molybdenum.

[0058] S104: Separating the first protein film from the silicon-based mask.

[0059] Specifically, the first protein film and the silicon-based mask plate can be separated by directly removing the tape to separate the first protein film and the silicon-based mask plate.

[0060] S105: Obtain a second protein film, and encapsulate the encapsulation area of ​​the first protein film with the second protein film to obtain a target cortical electrode.

[0061] Specifically, the second protein film is a protein film that does not deform when exposed to water. The second protein film is covered on the packaging area of ​​the first protein film, and the packaging area is the device area of ​​the first protein film. The pressure sensor and the temperature sensor are adhered to the first protein film, and the electrode detection site and the rear-end connection site are exposed. The target positions of the electrode detection site and the rear-end connection site are determined, and deionized water is used to dissolve and absorb the second protein film at the target position.

[0062] In a possible implementation, step S105 may include:

[0063] obtaining a second protein film, and performing plasma treatment on the surface of the second protein film;

[0064] Cutting the second protein film after the plasma treatment so that the size of the cut second protein film is adapted to the size of the encapsulation area;

[0065] The cut second protein film is covered on the encapsulation area of ​​the first protein film, and water cross-linked to obtain the target cortical electrode.

[0066] Specifically, the surface of the second protein film can be treated with plasma to change the chemical composition and structure of the surface of the second protein film, to excite hydroxyl groups on the surface of the second protein film, and to improve its adhesion. The atmosphere conditions for the plasma treatment can be nitrogen, oxygen, ammonia, etc. The plasma-treated second protein film is cut according to the packaging area of ​​the first protein film, and the cut second protein film is covered on the packaging area of ​​the first protein film, and is placed in a container filled with water vapor for a period of time to perform water cross-linking treatment to obtain the target cortical electrode.

[0067] On the other hand, the present invention provides a cortical electrode prepared by the cortical electrode preparation method as described above, the cortical electrode comprising a first protein film and a second protein film; the first protein film is formed with a pressure sensor and a temperature sensor; the second protein film is used to encapsulate the encapsulation area of ​​the first protein film.

[0068] In a possible implementation, the pressure sensor is a first curved serpentine resistor; the resistance of the pressure sensor increases as the pressure increases. Further, the bending axis size of the pressure sensor includes 2219 μm*530 μm.

[0069] Specifically, the pressure sensor is a first curved serpentine resistor, and the curved line can increase the actual straight length of the resistor. The size of each curved axis of the pressure sensor includes 2219μm*530μm. In other embodiments, the size of the pressure sensor can be determined according to the target object of the target cortical electrode, which is not limited here. In the embodiment of the present invention, the sensing principle of the pressure sensor is that when the target cortical electrode is deformed under pressure, since the first protein film substrate is a pre-stretched directional curled film, it has good deformability, which will drive the pressure sensor to extend together. The curved line of the pressure sensor is compressed and straightened, the cross-sectional area is reduced, the length is increased, and the resistance value is increased. When the temperature is constant, the resistance of the pressure sensor increases with the increase of the pressure, and the formula is as follows: R=ρL / S, where R is the resistance of the pressure sensor, ρ is the metal conductivity, L is the line length of the pressure sensor, and S is the cross-sectional area perpendicular to the current direction.

[0070] In a possible implementation, the temperature sensor is a second curved serpentine resistor; the resistance of the temperature sensor increases linearly with increasing temperature. Further, the bending axis size of the temperature sensor includes 250 μm*1070 μm.

[0071] Specifically, the temperature sensor is a second curved serpentine resistor, whose line width can be 50μm, and the size of each curved axis includes 250μm*1070μm. In other embodiments, the size of the temperature sensor can be determined according to the target object of the target cortical electrode, which is not limited here. The sensing principle of the temperature sensor utilizes the metal thermoelectric effect. When the temperature rises, the metal resistance increases. The temperature sensor can be designed in the center area of ​​the device to minimize the impact of the deformation of the target cortical electrode on the resistance of the temperature sensor. When other conditions are constant, the resistance of the temperature sensor increases linearly with the increase of temperature. The formula is as follows: R=R o (1+αT), where T is temperature in °C, R is the resistance of the temperature sensor at temperature T, Ro is the resistance of the temperature sensor at 0 °C, and α is the temperature coefficient of the metal, which can be determined based on the specific metal material used. For most metals, α≈0.4%.

[0072] On the other hand, the present invention also provides an electronic device, which is packaged by the cortical electrode and the back-end circuit as described above. Exemplarily, the back-end connection site of the target cortical electrode is effectively connected to the back-end circuit using ACF (Anisotropic Conductive Film) hot pressing welding to obtain a usable electronic device.

[0073] Based on the above introduction to a method for preparing a cortical electrode, a cortical electrode, and an electronic device, the above preparation method will be further described below in conjunction with the device structure diagram to facilitate understanding of the various structural changes in a method for preparing a cortical electrode. It should be understood that the following figures are only an exemplary description, and based on the above description, those skilled in the art can also obtain other figures without creative work. In addition, the structural changes shown in the following figures are only a feasibility example of a method for preparing a device, and do not mean that the method for preparing the device described in the embodiment of the present invention is limited to the following example.

[0074] The following is based on Figures 3a to 3i The device structure change process in a method for preparing a silk protein cortical electrode and a silk protein electrode device provided by an embodiment of the present invention is introduced in sequence.

[0075] refer to Figure 3a As shown, a silicon wafer 100 is obtained; a first oxide layer 101 is formed on the first surface of the silicon wafer 100, and a second oxide layer 102 is formed on the second surface of the silicon wafer 100.

[0076] refer to Figure 3b As shown, a photoresist is coated on the first oxide layer 101 and patterned to form a patterned photoresist layer.

[0077] refer to Figure 3cAs shown, the first oxide layer 101 is first etched based on the patterned photoresist layer to form etching regions of the first device pattern, the second device pattern and the third device pattern in the first oxide layer 101 .

[0078] refer to Figure 3d As shown, based on the etching area, the silicon wafer 100 is deep etched to the second oxide layer 102, and the first oxide layer 101 is formed on the silicon wafer 100 to form opening areas of the first device pattern, the second device pattern and the third device pattern.

[0079] refer to Figure 3e As shown, the second oxide layer 102 and the remaining first oxide layer 101 are removed to obtain a silicon-based mask 110 .

[0080] refer to Figure 3f As shown, a first protein film 200 is obtained, and the first protein film 200 is temporarily fixed to a silicon-based mask plate 110; the first protein film 200 is a pre-stretched directional curled film.

[0081] refer to Figure 3g As shown, using a silicon-based mask plate 110 as a mask, metal 300 is evaporated on the surface of the first protein film 200 to form a device area and a conductive structure area on the first protein film 200; the device area includes a pressure sensor and a temperature sensor; the conductive structure area includes an electrode detection site and a back-end connection site.

[0082] refer to Figure 3h As shown, the first protein film 200 is separated from the silicon-based mask 110 .

[0083] refer to Figure 3i As shown, a second protein film 400 is obtained, and the encapsulation area of ​​the first protein film 200 is encapsulated by the second protein film 400 to obtain a target cortical electrode.

[0084] Above Figures 3a to 3i The specific exemplary process of the implemented steps can be referred to the description above and will not be repeated here.

[0085] The present invention uses the cortical electrodes prepared by the above-mentioned embodiments to form a pressure sensor and a temperature sensor by evaporating metal on a pre-stretched first protein film through a silicon-based mask plate, and further forms a conductive structure area on the surface of the first protein film. The second protein film encapsulates the pressure sensor and the temperature sensor, exposing the electrode detection site and the back-end connection site to obtain a usable cortical electrode. Through an effective back-end connection, it is possible to record cortical neural electrical signals in vivo while monitoring key data such as intracranial temperature and intracranial pressure in real time. In addition, the good deformability of the first protein film can ensure the device stability of the pressure sensor and the temperature sensor.

[0086] It should be noted that the sequence of the embodiments of the present invention described above is for description only and does not represent the advantages and disadvantages of the embodiments. The above describes specific embodiments of this specification. Other embodiments are within the scope of the appended claims. In some cases, the actions or steps recorded in the claims can be performed in an order different from that in the embodiments and still achieve the desired results. In addition, the processes depicted in the drawings do not necessarily require the specific order or continuous order shown to achieve the desired results. In some embodiments, multitasking and parallel processing are also possible or may be advantageous.

[0087] The same or similar parts between the various embodiments in this specification can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the device embodiment, since it is basically similar to the method embodiment, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiment.

[0088] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for preparing a cortical electrode, characterized in that: include: Obtaining a silicon-based mask, wherein the silicon-based mask comprises an opening area of ​​a first device pattern and a second device pattern; the first device pattern is used to define a pressure sensor area; The second device pattern is used to define a temperature sensor area; Obtaining a first protein film, and temporarily fixing the first protein film and the silicon-based mask; The first protein film is a pre-stretched oriented curled film; Using the silicon-based mask as a mask, evaporating metal on the surface of the first protein film to form a device area on the first protein film; The device region includes the pressure sensor and the temperature sensor; separating the first protein film from the silicon-based mask; A second protein film is obtained, and the encapsulation area of ​​the first protein film is encapsulated by the second protein film to obtain a target cortical electrode.

2. The method for preparing a cortical electrode according to claim 1, characterized in that: The silicon-based mask also includes an opening area of ​​a third device pattern; The third device pattern is used to define the conductive structure area of ​​the target cortical electrode; the conductive structure area includes an electrode detection site and a rear-end connection site.

3. The method for preparing a cortical electrode according to claim 2, characterized in that: The obtaining of a silicon-based mask comprises: Obtaining a silicon wafer; a first surface of the silicon wafer is formed with a first oxide layer, and a second surface of the silicon wafer is formed with a second oxide layer; Coating a photoresist on the first oxide layer and patterning the layer to form a patterned photoresist layer; Based on the patterned photoresist layer, deeply etching from the oxide layer on the first surface to the second oxide layer to form opening areas of the first device pattern and the second device pattern; The second oxide layer is removed to obtain the silicon-based mask.

4. The method for preparing a cortical electrode according to claim 3, characterized in that: The step of obtaining a second protein film and encapsulating the encapsulation area of ​​the first protein film with the second protein film to obtain a target cortical electrode comprises: obtaining a second protein film, and performing plasma treatment on a surface of the second protein film; Cutting the second protein film after the plasma treatment so that the size of the cut second protein film is adapted to the size of the packaging area; The cut second protein film is covered on the packaging area of ​​the first protein film, and subjected to water cross-linking treatment to obtain the target cortical electrode.

5. The method for preparing a cortical electrode according to claim 1, characterized in that: The metal material includes one or a combination of gold, magnesium, iron and molybdenum.

6. A cortical electrode, characterized in that: The cortical electrode is prepared by the cortical electrode preparation method described in any one of claims 1-5, and the cortical electrode includes a first protein film and a second protein film; the first protein film is formed with a pressure sensor and a temperature sensor; the second protein film is used to encapsulate the encapsulation area of ​​the first protein film.

7. The cortical electrode according to claim 6, characterized in that: The pressure sensor is a first curved serpentine resistor; the resistance of the pressure sensor increases as the pressure increases.

8. The cortical electrode according to claim 7, characterized in that: The bending axis dimensions of the pressure sensor include 2219 μm*530 μm.

9. The cortical electrode according to claim 6, characterized in that: The temperature sensor is a second curved serpentine resistor; the resistance of the temperature sensor increases linearly with increasing temperature.

10. The cortical electrode according to claim 9, characterized in that: The bending axis dimensions of the temperature sensor include 250 μm*1070 μm.

11. An electronic device, characterized in that: The cortical electrode according to claim 6 is packaged with a back-end circuit.

Citation Information

Patent Citations

  • Intracerebral signal acquisition device, preparation method thereof and brain-computer interface

    CN111938632A

  • Preparation method of composite protein membrane electrode, composite protein membrane electrode and electronic device

    CN117462842A

  • Fibroin cortex electrode, fibroin electrode device and preparation method

    CN117814804A

  • Sign monitoring scarf

    CN213188271U

  • Artificial retina nerve electrode, encapsulation structure and preparation method therefor

    WO2024082398A1