Horizontal sealing welding method and welding device for cylindrical battery

Through the cylindrical battery horizontal seal welding method and the slow-rise and lower power welding technology of multi-mode ring laser, combined with the dust removal device, the problems of slow welding speed and poor dust removal effect are solved, and efficient welding and optimized welding quality are achieved.

CN118926693APending Publication Date: 2024-11-12LUOYANG INST OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411037883.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing cylindrical battery sealing welding technology has problems such as slow welding speed, poor dust removal effect and welding tail defects.

Method used

The horizontal sealing welding method of cylindrical battery is adopted. By driving the battery to rotate and using a multi-mode ring laser for slow-rise and slow-down power welding, combined with the peripheral dust collecting cover structure and protective air pipe, the welding process and dust removal effect are optimized.

Benefits of technology

It improves welding efficiency, optimizes defects at the tail of welding receiving, improves dust removal effect, and enhances welding quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118926693A_ABST
    Figure CN118926693A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of new energy lithium battery manufacturing, and particularly relates to a horizontal sealing welding method and device for a cylindrical battery, and the welding device drives the cylindrical battery to rotate; after the cylindrical battery rotates at a constant speed, a laser is started, the welding power is gradually increased from zero to full power, and after the welding power of the laser is increased to full power, full welding is conducted on the cylindrical battery; and after the laser device conducts circumferential welding on the cylindrical battery by a circle, the laser device continues to weld the cylindrical battery, after the laser device conducts welding on the welding area corresponding to the laser device slow rising initial power, the laser device continues to weld the cylindrical battery, then the welding power of the laser device is gradually reduced to zero, finally the cylindrical battery stops rotating, and welding is completed. The welding device comprises a dust hood structure and a protective gas pipe. The defect of collapse at the welding ending position can be optimized, the sealing welding efficiency of the cylindrical battery is improved, and the dust removal effect is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of new energy lithium battery manufacturing, and specifically relates to a horizontal sealing welding method and a welding device for a cylindrical battery. Background Art

[0002] With the country's strong support for the development of new energy, large cylindrical batteries have emerged with their advantages of high capacity, high rate, good heat dissipation and low cost. The sealing welding of the cylinder is an important process in the assembly of the monomer.

[0003] There are two technical directions for the sealing welding process of cylindrical battery assembly, one is horizontal welding and the other is vertical welding. Both methods have their own advantages and disadvantages. The present invention improves horizontal welding. The cylindrical battery welding process is divided into single-pass and double-pass. The single-pass is to weld only the seal on one side of the cylindrical battery, and the double-pass is to weld the seals on both sides of the cylindrical battery.

[0004] In the current existing technology, cylindrical battery sealing welding has disadvantages such as slow welding speed, poor dust removal effect, and welding finishing defects. Summary of the invention

[0005] In order to solve the above technical problems, the present invention provides a cylindrical battery horizontal sealing welding method and welding device.

[0006] The object of the present invention is to achieve the following technical solution. According to the present invention, a cylindrical battery horizontal sealing welding method includes the following steps:

[0007] The welding device drives the cylindrical battery to rotate;

[0008] After the cylindrical battery rotates at a uniform speed, the laser is started to weld the cylindrical battery;

[0009] After the laser is started, the welding power gradually increases from zero to full power, at which time the cylindrical battery rotates through a certain angle;

[0010] After the laser welding power is increased to full power, the cylindrical battery is fully welded;

[0011] After the laser welds the cylindrical battery in a circle, the laser continues to weld the cylindrical battery so that the welding area at full power of the laser covers the welding area corresponding to the laser's slowly rising starting power;

[0012] After the laser welds the welding area corresponding to the laser's slowly rising starting power, the laser continues to weld the cylindrical battery. After the cylindrical battery continues to rotate through a certain angle, the laser's welding power gradually decreases to zero, and finally the cylindrical battery stops rotating, completing the welding.

[0013] Furthermore, when the welding power of the laser gradually decreases, the process of gradually decreasing the welding power includes two or more stages. In the same stage, the decreasing speed of the welding power of the laser is equal. During the whole process of decreasing the welding power, the decreasing speed of the welding power of the laser gradually decreases.

[0014] Furthermore, before using the welding device to weld the cylindrical battery, the outer shell and cover plate of the cylindrical battery are pre-welded.

[0015] Furthermore, the laser adopts a multi-mode ring laser, wherein the outer ring is responsible for expanding the keyhole opening, the inner ring is responsible for welding penetration, and the welding power of the inner ring is less than the welding power of the outer ring.

[0016] Furthermore, the rotation speed of the cylindrical battery is v, tw is the time required for the cylindrical battery to weld a full circle, t0 is the time for the welding power set by the laser to gradually increase, t1 is the time for the full-power welding set by the laser, tw is included in the time period of t1, t2 is the time for the welding power set by the laser to gradually decrease from full power, t3 is the time for the welding power set by the laser to further decrease to zero, and the arc length corresponding to each welding area calculated by the above parameters is: the arc length corresponding to the starting power overlapping area L0 = t0*v, the arc length corresponding to the full-power overlapping area L1 = (t1-tw)*v, the low-power overlapping area L2 = t2*v, L3 = t3*v, and the non-overlapping area L4 = (2tw-t0-t1-t2-t3)*v.

[0017] Furthermore, before welding, the shielding gas blowing direction of the shielding gas pipe is adjusted so that the shielding gas blowing direction is opposite to the rotation tangent direction of the cylindrical battery welding part.

[0018] Furthermore, before welding, the position of the dust hood is adjusted so that it can absorb most of the welding slag and dust generated during welding.

[0019] A welding device in a horizontal sealing welding method for cylindrical batteries, the welding device comprises two clamping mechanisms arranged opposite to each other and a laser located above the clamping mechanisms, the clamping mechanism comprises a slide and a thrust cylinder for pushing the slide to move, a servo motor is arranged on the slide, the rotating shaft of the servo motor is connected to a clamping cylinder rotatably arranged on the slide, and a clamping claw for clamping the outer wall of the cylindrical battery is arranged on the clamping claw cylinder; a presser foot cylinder is also arranged on the slide, a presser foot is arranged at the end of the output shaft of the presser foot cylinder, and the presser foot cylinder can make the presser foot close to the cover plate at the end of the cylindrical battery; a dust cover structure and a protective air pipe are also arranged above the clamping mechanism, the dust cover structure comprises a dust cover and a connecting pipe which are connected and communicated with each other, and the dust cover is used to cover the outside of the weld of the cylindrical battery; a long hole for passing the protective air pipe is arranged on the side wall of the dust cover.

[0020] Furthermore, one end of the connecting pipe is provided with a flange for connecting to a negative pressure device, and the other end is provided with a magnet for adsorption and connection with a dust cover; the dust cover includes a first dust cover and a second dust cover of a split structure, and the first dust cover and the second dust cover are adsorbed and connected to form a special-shaped tube by magnet adsorption, and the cross-section of the end of the special-shaped tube close to the connecting pipe is circular matching the connecting pipe, and the cross-section of the end close to the weld is rectangular, and the dust cover is provided with a semicircular groove on the outside of the weld toward the end close to the weld of the cylindrical battery.

[0021] Furthermore, a spherical joint is provided at the end of the protective air pipe located outside the dust removal cover, and the spherical joint is used to connect to a nitrogen source.

[0022] The present invention is beneficial in that:

[0023] Through the above-mentioned horizontal sealing welding method for cylindrical batteries and the multi-layer slow-rise and slow-fall power setting, the collapse defect at the welding end can be optimized and the sealing welding efficiency of cylindrical batteries can be improved; through the above-mentioned peripheral dust removal device, the dust removal effect is improved.

[0024] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention, it can be implemented in accordance with the contents of the specification. In order to make the above and other purposes, features and advantages of the present invention more obvious and easy to understand, the following specifically cites a preferred embodiment and describes it in detail with the accompanying drawings as follows. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A schematic diagram of the welding area of ​​an embodiment of a cylindrical battery horizontal sealing welding method of the present invention;

[0026] Figure 2 A schematic diagram showing the change of laser welding power over time used in an embodiment of a cylindrical battery horizontal sealing welding method of the present invention;

[0027] Figure 3 It is a three-dimensional schematic diagram of a dust cover structure in an embodiment of a cylindrical battery horizontal sealing welding device of the present invention;

[0028] Figure 4 for Figure 3 A three-dimensional schematic diagram from another perspective;

[0029] Figure 5 for Figure 3 Front view of the diagram;

[0030] Figure 6 for Figure 3 An exploded schematic diagram of the dust cover structure shown in FIG.

[0031] Figure 7 It is a three-dimensional schematic diagram of an embodiment of a cylindrical battery horizontal sealing welding device of the present invention;

[0032] Figure 8 for Figure 7 Schematic diagram of the A-side components;

[0033] Fig. 9 for Figure 7 Schematic diagram of the b-side components.

[0034] [Reference Signs]

[0035] 1-A side component, 101-first servo motor, 102-first thrust cylinder, 103-first hydraulic buffer, 104-first clamping jaw cylinder, 105-first clamping jaw, 106-first presser foot cylinder, 107-first presser foot, 108-first base, 109-first slide.

[0036] 2-B side component, 201-second servo motor, 202-second thrust cylinder, 203-second hydraulic buffer, 204-second clamping jaw cylinder, 205-second clamping jaw, 206-second presser foot cylinder, 207-second presser foot, 208-second base, 209-second slide.

[0037] S-welding starting point, E-welding ending point, L0, L1, L2, L3, L4-arc lengths corresponding to each welding area, C-dust cover structure, C1-dust cover, C11-first dust cover, C12-second dust cover, C13-long hole, C14-semicircular groove, C2-connecting pipe, C21-flange, D1-protective air pipe, D2-spherical joint, 3-cylindrical battery, 301-cover plate, 302-housing, 4-laser. DETAILED DESCRIPTION

[0038] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0039] An embodiment of a cylindrical battery horizontal sealing welding method of the present invention comprises the following steps:

[0040] 1. Fix the corresponding cover plate 301 at the end opening of the outer shell 302 of the cylindrical battery 3 by pre-welding.

[0041] 2. Place the pre-welded cylindrical battery 3 on a horizontal welding device.

[0042] 3. Determine welding process parameters according to welding depth / width requirements.

[0043] The welding process parameters include the matching slow-rise and slow-fall power, welding speed, angle and flow rate of the shielding gas (nitrogen), etc.

[0044] 4. According to the welding speed, the angle and flow rate of the shielding gas (nitrogen), determine the spattering direction of most welding slags, adjust the opening direction of the dust hood structure C, and ensure that the opening direction of the dust hood C1 is consistent with the spattering direction of most welding slags.

[0045] 5. Start the horizontal welding device, fully weld the cylindrical battery 3 according to the set parameters, and weld the circumferential weld between the end of the cylindrical battery 3 and the corresponding cover plate 301.

[0046] 6. After welding is completed, remove the cylindrical battery and complete the full welding of the end seal of the cylindrical battery 3.

[0047] If the cylindrical battery 3 is single-pass welded, the cylindrical battery 3 is welded after the above welding steps are completed; if the cylindrical battery 3 is double-pass welded, the other end of the cylindrical battery 3 is fully welded after the above welding steps are completed.

[0048] After the horizontal welding device fixes the cylindrical battery 3, during welding, the horizontal welding device first drives the cylindrical battery 3 to rotate, and the circumferential weld of the cylindrical battery 3 can pass through the fixed laser light extension line in sequence; starting the laser can achieve full welding of the cylindrical battery 3. The speed at which the horizontal welding device drives the cylindrical battery 3 to rotate is coordinated with the laser welding power to determine the welding speed of the cylindrical battery 3.

[0049] After the cylindrical battery 3 is fixed in the full welding position of the horizontal welding device, the horizontal welding device drives the cylindrical battery 3 to rotate, and the rotation speed of the cylindrical battery is accelerated from static to uniform speed, and then the laser is used to weld the cylindrical battery 3. When full welding is achieved, the laser is turned off, and the rotation speed of the cylindrical battery 3 is decelerated from uniform speed to static.

[0050] The laser performs circumferential welding on the weld of the cylindrical battery 3 to form a circumferential welding area. When setting the laser welding slow rise and slow fall power, the weld of the cylindrical battery 3 is divided into multiple circumferentially distributed welding areas according to the laser welding power of the cylindrical battery. The projection of each welding area on the end face of the cylindrical battery is an arc, and the arc length represents the welding area. Starting from the laser welding starting point S of the cylindrical battery, the arc length is L0, arc length L1, arc length L2, arc length L3, welding end point E, arc length L4, welding starting point S, etc. Figure 1 The inner circle and the outer arc line represent the welding area of ​​the cylindrical battery 3, wherein the outer arc line and the inner circle corresponding part are the same welding area of ​​the cylindrical battery 3, and in order to distinguish the repeated welding of the same welding area, it is divided into a circle and an arc line.

[0051] When the cylindrical battery 3 rotates at a constant speed, the laser is turned on to start welding the cylindrical battery 3. At this time, the light emitted by the laser first contacts the welding starting point S of the cylindrical battery 3. As the cylindrical battery rotates, the welding power of the laser gradually increases (the gradually increasing welding power is the slowly rising starting power). The light emitted by the laser forms a welding area corresponding to the arc length L0 on the cylindrical battery 3. After passing through the welding area corresponding to the arc length L0, the welding power of the laser reaches full power. Then, as the cylindrical battery 3 rotates, the full-power light emitted by the laser passes through the welding areas corresponding to the arc lengths L1, L2, L3, L4, L0, and L1 in sequence, and the circumferential weld of the cylindrical battery 3 is fully welded. While welding at high rate, the full-power welding area is superimposed on the slowly rising starting power welding area corresponding to arc length L0 and the full-power welding area corresponding to arc length L1; after passing through the welding area corresponding to arc length L1, the power of the laser gradually decreases. At this time, the light emitted by the laser passes through the welding area corresponding to arc length L2, so that the low-power welding area is superimposed on the full-power welding area here; after passing through the welding area corresponding to arc length L2, the power of the laser gradually decreases again. At this time, the light emitted by the laser passes through the welding area corresponding to L3, until the power of the laser is reduced to zero. At this time, the laser is aimed at the welding end point E, so that the lower-power welding area is superimposed on the welding area corresponding to L3, and the welding is completed. The power of the laser in the welding area corresponding to L2 decreases faster than the power of the laser in the welding area corresponding to L3.

[0052] It can be seen that the welding areas corresponding to arc lengths L0, L1, L2, and L3 of cylindrical battery 3 are welding overlapping areas, and the welding area corresponding to L4 is a non-overlapping area. The welding area corresponding to arc length L0 has been welded twice by the laser with different powers, which are slowly rising starting power welding and full power welding, respectively. Therefore, this welding area is a starting power overlapping area. The welding area corresponding to arc length L1 has been welded twice at full power, so this welding area is a full power overlapping area. The welding areas corresponding to arc lengths L2 and L3 have been welded twice by the laser with different powers, which are full power welding and welding when the welding power is gradually reduced. Therefore, the welding areas corresponding to arc lengths L2 and L3 are low-power overlapping areas. Figure 1 shown.

[0053] The initial power overlap area corresponds to the power ramp-up phase of the laser and the full power welding phase in the second cycle. The purpose is to slowly transition the molten pool to the overlap area and reduce the risk of white explosion points caused by unstable molten pool. The full power overlap area is the transition area to the low power overlap area. The low power overlap area corresponds to the power ramp-down phase of the laser and is divided into several sections ( Figure 2 2 sections are shown), achieving a smooth transition and optimizing the concave at the welding end, which is beneficial to reducing the defect of the concave at the end point.

[0054] In this embodiment, the welding areas are divided into five. In other embodiments, by increasing the corresponding welding areas when the laser power is reduced, more low-power overlapping welding areas can be set to achieve the best welding effect.

[0055] In this embodiment, the laser adopts a multi-mode ring laser, whose outer ring is responsible for expanding the keyhole opening and the inner ring is responsible for welding penetration. The ring laser can suppress metal vapor splashing and reduce the requirements for dust removal during welding.

[0056] like Figure 2 The figure shows the change of laser welding power over time when welding cylindrical battery 3. The upper broken line is the change curve of laser outer ring power, and the lower broken line is the change curve of laser inner ring power. The rotation speed of cylindrical battery 3, that is, welding speed is v, t is the time required for welding cylindrical battery 3 in one circle, t0 is the time of gradually increasing welding power set by laser, t1 is the time of full power welding set by laser, t is included in the time period of t1, t2 is the time of gradually decreasing welding power set by laser, t3 is the time of further decreasing welding power set by laser to zero, Figure 2 It can be seen that the speed of welding power decrease in the t2 period is faster than that in the t3 period. The arc length corresponding to each welding area can be calculated from the above parameters: L0 = t0*v, L1 = (t1-tw)*v, L2 = t2*v, L3 = t3*v, L4 = (2tw-t0-t1-t2-t3)*v.

[0057] The angle and flow rate of the welding shielding gas need to cover the welding area to prevent the welding material from being oxidized during welding. According to the welding spatter direction of the cylindrical battery 3, the dust removal cover structure C is designed, such as Figures 3 to 6 As shown, the position covered by the dust cover structure C is kept in the direction relative to the cylindrical battery 3 and is consistent with the direction of most welding slag splashes, which can effectively absorb the welding slag and smoke generated during welding.

[0058] The dust cover structure C includes a dust cover C1 and a connecting pipe C2. A flange C21 is provided at one end of the connecting pipe C2 for connecting to a negative pressure device to absorb welding slag and smoke generated by laser welding. A magnet for adsorption and connection with the dust cover C1 is provided at the other end of the connecting pipe C2. The dust cover C1 is a split structure, including a first dust cover C11 and a second dust cover C12, which is convenient for disassembly and cleaning of welding slag. The first dust cover C11 and the second dust cover C12 can be docked by magnet adsorption to form a special-shaped tube. The cross-section of the end of the special-shaped tube close to the connecting pipe C2 is circular and matches the connecting pipe C2, and the cross-section of the end close to the weld is rectangular. The two ends of the special-shaped tube have a smooth transition. The connecting pipe C2 and the dust cover C1 are fixed by magnetic attraction, which is convenient for disassembly and timely cleaning of welding slag. The end of the dust cover C1 close to the cylindrical battery weld is provided with a semicircular groove C14 covering the outside of the weld to semi-enclose the weld of the cylindrical battery 3. When welding the cylindrical battery 3, the direction of the slag splashing cannot be accurately predicted. Only the direction with more welding spatter is considered. The part where the semicircular groove C14 wraps the cover of the cylindrical battery 3 is where most of the slag splashes, which improves the dust removal efficiency.

[0059] A long hole C13 is provided on the side wall of the dust hood C1, and a protective air pipe D1 extends from the long hole C13 into the interior of the dust hood C1 to blow a protective gas, which is usually nitrogen, into the dust hood C1. The end of the protective air pipe D1 facing the welding area is a nitrogen blowing port, and the other end of the protective air pipe D1 is a spherical joint D2 located outside the dust hood C1, and the other side of the spherical joint D2 is connected to a nitrogen source. Through the spherical joint D2, it is convenient to adjust the angle of the protective air pipe D1, thereby changing the angle of the nitrogen blowing and adjusting the angle of the nitrogen flow direction. The nitrogen blowing port is aligned with the battery sealing welding area, and the angle between the blowing direction of the nitrogen and the light emitting direction of the laser 4 is between 30-60°, which is the optimal angle. Figure 5 As shown, the long hole C13 leaves space for adjusting the angle of the protective air tube D1, so as to facilitate the adjustment of the angle and position of the protective air tube D1.

[0060] During the rotation of the cylindrical battery 3, the rotation tangent direction of the part of the outer circumference close to the nitrogen blowing port is opposite to the blowing direction of the nitrogen, which can make the molten pool form better. Figure 5As shown. The light outlet and nitrogen blowing outlet of the laser 4 are both located on one side of the radial line of the vertical direction of the cylindrical battery 3. The laser 4 is located above the cylindrical battery and its light outlet is vertically downward, blowing the welding slag and dust to the other side of the radial line, increasing the contact area between the semicircular groove and the welding slag and dust, and improving the dust removal efficiency. During welding, most of the welding slag or dust splashes in the same direction as the rotation tangent direction of the cylindrical battery without blowing nitrogen; in the case of blowing nitrogen, most of the welding slag or dust is affected by the nitrogen flow, which is opposite to the rotation tangent direction. Therefore, when blowing nitrogen, the welding slag or dust can be prevented from affecting subsequent welding. By blowing nitrogen, the welding material (aluminum) can be prevented from being oxidized, which has a positive effect on weld formation, reducing pores, and dust removal. Nitrogen can blow away the plasma generated during welding and improve the quality of the weld.

[0061] The dust cover structure C, the laser 4, and the spherical joint D2 are all arranged on the welding device.

[0062] Through the above-mentioned horizontal sealing welding method for cylindrical batteries and the multi-layer slow-rise and slow-fall power setting, the collapse defect at the welding end can be optimized and the sealing welding efficiency of cylindrical batteries can be improved; through the above-mentioned peripheral dust removal device, the dust removal effect is improved.

[0063] An embodiment of a cylindrical battery horizontal sealing welding device of the present invention is as follows Figures 7 to 9 As shown, this embodiment takes the double-pass welding of a cylindrical battery as an example for explanation. The cylindrical battery 3 includes a cylindrical shell 302 with openings at both ends of the shell, and the cover plate 301 is welded to the openings at both ends of the shell to seal the cylindrical battery 3. Before welding using the welding device of the present invention, the two ends of the cylindrical battery 3 are pre-welded (spot welding or line welding + swinging, the pre-welding between the shell 302 and the cover plate 201 is usually divided into several sections) with the cover plate, and the cover plate is fixed to the end of the cylindrical battery 3. A weld is formed between the cover plate 301 and the edge of the end of the shell 302, and the weld is fully welded by the welding device. The cover plate, shell and other structures on the cylindrical battery 3 are all prior art and will not be repeated here.

[0064] The welding device of the present invention includes two symmetrically arranged clamping mechanisms for clamping cylindrical batteries 2, and a laser 4 for welding cylindrical batteries. For ease of description, the two symmetrical clamping mechanisms are A-side component 1 and B-side component 2, which are symmetrically arranged and act together on cylindrical batteries 3. The A-side component 1 is used as an example for description. The laser 4 is located above the A-side component 1 and the B-side component 2, and is used for welding cylindrical batteries 3.

[0065] The A-side component 1 includes a first servo motor 101 , a first thrust cylinder 102 , a first hydraulic buffer 103 , a first clamping jaw cylinder 104 , a first clamping jaw 105 , a first presser foot cylinder 106 , and a first presser foot 107 .

[0066] The first thrust cylinder 102 is fixedly arranged on the first base 108 , and the first slide 109 is horizontally slidably arranged on the first base 108 . The output shaft end of the first thrust cylinder 102 is connected to the first slide 109 . Under the thrust of the first thrust cylinder 102 , the first slide 109 slides on the first base 108 .

[0067] The first servo motor 101 is fixedly mounted on the first slide 109, and the first gripper cylinder 104 is rotatably mounted on the first slide 109. The rotating shaft of the first servo motor 101 coincides with the central axis of the first gripper cylinder 104. The first gripper cylinder 104 is a prior art and will not be described in detail herein. The output shaft end of the first servo motor 101 is fixed on the first gripper cylinder 104, and the rotation of the first servo motor 101 can drive the first gripper cylinder 104 to rotate.

[0068] The first clamping jaw 105 is arranged on the first clamping jaw cylinder 104, and the central axis of the first clamping jaw cylinder 104 coincides with the central axis of the first clamping jaw 105. The first clamping jaw cylinder 104 can drive the first clamping jaw 105 to open and close to loosen or clamp an object. This is the prior art and will not be described in detail here.

[0069] A plurality of clamp fingers are circumferentially distributed on the first clamp 105. In the present embodiment, a total of three clamp fingers are provided. When the first clamp 105 is used to clamp the cylindrical battery, the concentricity of the cylindrical battery is ensured. Under the action of the first clamp cylinder 104, the three clamp fingers can move toward or away from the central axis of the three first clamps 5, thereby clamping or loosening the cylindrical battery. When the clamp clamps the cylindrical battery, the central axis of the clamp coincides with the central axis of the cylindrical battery. The extension direction of the clamp fingers is parallel to the central axis of the first clamp 105 and faces the B side component 2. The rotating shaft of the first servo motor 101 coincides with the central axis of the first clamp cylinder 104 and the central axis of the first clamp 105. After the first clamp 105 clamps the cylindrical battery 3, the rotating shaft of the first servo motor 101 drives the cylindrical battery 3 to rotate.

[0070] The first presser foot cylinder 106 is fixedly arranged at the center position of the first clamping jaw 105, and the output shaft of the first presser foot cylinder 106 coincides with the center axis of the first clamping jaw 105. The output shaft of the first presser foot cylinder 106 extends toward the B side component 2, and the first presser foot 107 is arranged at its end, and the first presser foot 107 is in the shape of a round cover or a disc. Under the action of the first presser foot cylinder 106, the first presser foot 107 approaches or moves away from the B side component 2. Under the action of the first presser foot cylinder 106, the first presser foot 107 approaches the cover plate of the cylindrical battery, and during welding, the pole, explosion-proof valve, QR code, and liquid injection port on the cover plate are protected to prevent impurities such as welding slag from falling into the liquid injection port or sticking to the pole, and to prevent the pole, explosion-proof valve, and QR code from being damaged. The specific structure of the cylindrical battery is prior art and will not be repeated here.

[0071] A first hydraulic buffer 103 is disposed on the first slide 109 to position the first slide 109 as a whole and absorb vibration. This is a prior art and will not be described in detail herein.

[0072] In this embodiment, both the positive and negative electrodes of the cylindrical battery are provided with poles, which are bipolar poles (positive pole and negative pole respectively), and double-pass welding is adopted. The device can also be used for single-pass welding of cylindrical batteries. The QR code on the cover plate can be set as needed.

[0073] The second servo motor 201, the second thrust cylinder 202, the second hydraulic buffer 203, the second clamping cylinder 204, the second clamping jaw 205, the second presser foot cylinder 206, the second presser foot 207, the second base 208 and the second slide 209 on the B-side component 2 are symmetrically positioned with the corresponding components on the A-side component. For easy distinction, the components in the A-side component 1 are prefixed with "first" and the corresponding components in the B-side component 2 are prefixed with "second", but the corresponding components on both sides are essentially the same and will not be repeated here.

[0074] For the double-pass welding of cylindrical batteries, the specific operation process of the device is as follows:

[0075] 1. Fix the corresponding cover plates 301 at both ends of the cylindrical battery 3 by pre-welding;

[0076] 2. The first thrust cylinder 102 of the A-side component 1 pushes the first slide 109 to the welding position. At this time, the A-side component 1 is the non-welding side, and the B-side component is the welding side (B welding side);

[0077] 3. The first clamping jaw 105 of the A-side component 1 is closed to clamp the outer wall of the cylindrical battery 3, and the cylindrical battery 3 is exposed toward the end of the B-side component 2. At this time, the end of the cylindrical battery 3 close to the A-side component 1 is the non-welding side, and the end close to the B-side component 2 is the welding side (B welding side);

[0078] 4. The output shaft of the second presser foot cylinder 206 of the B-side component 2 is extended, so that the distance between the presser foot end face of the second presser foot 207 and the cover plate of the welding side of the cylindrical battery B is 0.1-0.3mm, so that the presser foot end face does not contact the cover plate, preventing friction and damage to the battery cover plate, while protecting the cover plate;

[0079] 5. The laser 4 reaches the top of the weld on the welding side of the cylindrical battery B and sets the power of the laser 4. The position of the dust cover structure C and the angle of the protective air pipe D1 are adjusted. The first servo motor 101 drives the first clamping cylinder 104 to rotate, thereby driving the cylindrical battery 3 to rotate. When the rotation of the cylindrical battery 3 is accelerated to a uniform speed state, light welding is performed to ensure that the welding of the weld of the cylindrical battery 3 is performed in a uniform speed section.

[0080] 6. After the welding of the weld seam on the welding side of the cylindrical battery 3B is completed, the switch is performed. After the switch, the A-side component 1 is the welding side (A welding side), the B-side component 2 is the non-welding side, the end of the cylindrical battery 3 close to the A-side component is the welding side (A welding side), and the end close to the B-side component is the non-welding side;

[0081] 7. The second presser cylinder 206 of the B-side component 2 contracts, the second thrust cylinder 202 pushes the second slide 209 to the welding position, and the second clamping jaw 205 closes and clamps the cylindrical battery 3;

[0082] 8. The first clamping jaw 105 of the A-side component 1 is opened, the output shaft of the first thrust cylinder 102 contracts and drives the first slide 109 to retreat, and the output shaft of the first presser foot cylinder 106 extends, so that the first presser foot 107 is close to the cover plate on the welding side of the cylindrical battery A, so that the distance between the end face of the first presser foot 107 and the cover plate on the welding side of the cylindrical battery 3A is 0.1-0.3mm, the laser 4 reaches the battery weld on the welding side of the cylindrical battery A and sets the power of the laser 4, adjusts the position of the dust cover structure C and the angle of the protective air pipe D1, and the second servo motor 101 of the B-side component 2 drives the second clamping jaw cylinder 204 to rotate, thereby driving the cylindrical battery 3 to rotate, and completes the welding of the A welding side during the uniform rotation stage of the cylindrical battery 3;

[0083] 9. The first presser cylinder 106 contracts, the second clamping jaw 205 is released, the cylindrical battery 3 is taken out, and the A-side component 1 and the B-side component 2 are restored to the initial state, waiting for the next cycle.

[0084] The present invention provides a novel horizontal welding device, which uses a clamping jaw (a first clamping jaw 105 or a second clamping jaw 205) to clamp a cylindrical battery 3, and a presser foot (a first presser foot 107 or a second presser foot 207) close to but not in contact with a cover plate, does not use an adhesive layer to clamp the cylindrical battery 3, and does not provide friction, thereby preventing the presser foot from being subjected to high temperature and friction, thereby preventing the adhesive layer from being reduced in thickness and damaged, thereby causing poor welding, and maintaining the weld position unchanged, thereby improving the sealing yield of the cylindrical battery 3 and reducing the consumption of the presser foot (if the presser foot is in contact with the cover plate and fixed by static friction, the adhesive layer of the presser foot is worn under the action of high temperature and friction). Faster, and at the same time, the presser foot is needed to keep the cylindrical battery 3 clamped, which will change the weld position, causing the weld position to change in the height direction of the cylindrical battery 3, so that the position of the laser changes relative to the weld position, and the laser has high requirements on the weld position accuracy, and the deviation is generally ±0.1mm. After the welding deviation occurs, poor welding is likely to occur, reducing the welding yield), thereby reducing costs; the presser foot does not contact the cover plate, will not scratch the surface of the battery cover plate, and the presser foot is close to the cover plate, avoiding dust and welding slag during welding from entering the liquid filling port, and can protect the cover plate and the pole, explosion-proof valve, QR code, etc. on the cover plate.

[0085] In other embodiments of the cylindrical battery horizontal sealing welding device of the present invention, the existing welding device can also be used, and the dust cover structure C, the protective air pipe D1 and the ball joint D2 are arranged on the welding device.

[0086] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the invention, and that the scope of the invention is defined by the appended claims and their equivalents.

Claims

1. A cylindrical battery horizontal sealing welding method, characterized in that: The following steps are involved: The welding device drives the cylindrical battery to rotate; After the cylindrical battery rotates at a uniform speed, the laser is started to weld the cylindrical battery; After the laser is started, the welding power gradually increases from zero to full power, at which time the cylindrical battery rotates through a certain angle; After the laser welding power is increased to full power, the cylindrical battery is fully welded; After the laser welds the cylindrical battery in a circle, the laser continues to weld the cylindrical battery so that the welding area at full power of the laser covers the welding area corresponding to the laser's slowly rising starting power; After the laser welds the welding area corresponding to the laser's slowly rising starting power, the laser continues to weld the cylindrical battery. After the cylindrical battery continues to rotate through a certain angle, the laser's welding power gradually decreases to zero, and finally the cylindrical battery stops rotating, completing the welding.

2. A cylindrical battery horizontal sealing welding method according to claim 1, characterized in that: When the welding power of the laser gradually decreases, the process of gradually decreasing the welding power includes two or more stages. In the same stage, the decreasing speed of the welding power of the laser is equal. During the whole process of decreasing the welding power, the decreasing speed of the welding power of the laser gradually decreases.

3. A cylindrical battery horizontal sealing welding method according to claim 1, characterized in that: Before using a welding device to weld the cylindrical battery, the outer shell and cover plate of the cylindrical battery are pre-welded.

4. A cylindrical battery horizontal sealing welding method according to claim 1, characterized in that: The laser adopts a multi-mode ring laser, the outer ring of which is responsible for expanding the keyhole opening, the inner ring is responsible for welding penetration, and the welding power of the inner ring is less than the welding power of the outer ring.

5. A cylindrical battery horizontal sealing welding method according to claim 1, characterized in that: The rotation speed of the cylindrical battery is v, tw is the time required for the cylindrical battery to weld a full circle, t0 is the time for the welding power set by the laser to gradually increase, t1 is the time for the full-power welding set by the laser, tw is included in the time period of t1, t2 is the time for the welding power set by the laser to gradually decrease from full power, t3 is the time for the welding power set by the laser to further decrease to zero, and the arc lengths corresponding to each welding area calculated by the above parameters are: the arc length corresponding to the starting power overlapping area L0=t0*v, the arc length corresponding to the full-power overlapping area L1=(t1-tw)*v, the low-power overlapping area L2=t2*v, L3=t3*v, and the non-overlapping area L4=(2tw-t0-t1-t2-t3)*v.

6. A cylindrical battery horizontal sealing welding method according to claim 1, characterized in that: Before welding, adjust the shielding gas blowing direction of the shielding gas pipe so that the shielding gas blowing direction is opposite to the rotation tangent direction of the cylindrical battery welding part.

7. A cylindrical battery horizontal sealing welding method according to claim 1, characterized in that: Before welding, adjust the position of the dust hood so that it can absorb most of the welding slag and dust generated during welding.

8. A welding device in a cylindrical battery horizontal sealing welding method according to any one of claims 1 to 7, characterized in that: The welding device includes two clamping mechanisms arranged opposite to each other and a laser located above the clamping mechanisms. The clamping mechanism includes a slide and a thrust cylinder for pushing the slide to move. A servo motor is arranged on the slide. The rotating shaft of the servo motor is connected to a clamping cylinder rotatably arranged on the slide. The clamping cylinder is provided with a clamping claw for clamping the outer wall of the cylindrical battery. A presser foot cylinder is also arranged on the slide. A presser foot is arranged at the end of the output shaft of the presser foot cylinder. The presser foot cylinder can make the presser foot close to the cover plate at the end of the cylindrical battery. A dust cover structure and a protective air pipe are also arranged above the clamping mechanism. The dust cover structure includes a dust cover and a connecting pipe which are connected and communicated with each other. The dust cover is used to cover the outside of the weld of the cylindrical battery. A long hole for passing the protective air pipe is arranged on the side wall of the dust cover.

9. A welding device according to claim 8, characterized in that: One end of the connecting tube is provided with a flange for connecting to a negative pressure device, and the other end is provided with a magnet for adsorption and connection with a dust cover; the dust cover includes a first dust cover and a second dust cover of a split structure, and the first dust cover and the second dust cover are adsorbed and connected to form a special-shaped tube by magnet adsorption. The cross-section of the end of the special-shaped tube close to the connecting tube is circular matching the connecting tube, and the cross-section of the end close to the weld is rectangular. The dust cover is provided with a semicircular groove on the outside of the weld facing the end close to the cylindrical battery weld.

10. A welding device according to claim 8, characterized in that: A spherical joint is arranged at the end of the protective air pipe located outside the dust removal cover, and the spherical joint is used to connect to a nitrogen source.