Composition suitable for eyebrows
By using a specific ratio of silicone resin, silicone gel, volatile hydrocarbon oil, hydrophobic inorganic filler, and organic modified clay in eyebrow makeup products, the problems of stability and comfort in existing eyebrow makeup products are solved, providing a matte, durable, and low-tack cosmetic effect.
Patent Information
- Application Number
- CN202380030351.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-29
- Filing Date
- 2023-03-03
- Publication Date
- 2024-11-12
AI Technical Summary
Existing cosmetic compositions for the lips are inadequate in providing a matte finish, durability, and a comfortable texture, especially as they are unstable and highly viscous at high temperatures, making them unsuitable for eyebrow makeup.
An anhydrous liquid composition comprising silicone resin, silicone gel, volatile hydrocarbon oil, hydrophobic inorganic filler, and lipophilic gelling agent of organic modified clay is used to ensure the appropriate ratio of filler and gelling agent, providing stability and excellent cosmetic effects.
It achieves a stable matte finish at high temperatures, good abrasion resistance, and reduced makeup stickiness, providing a comfortable application texture and maintaining long-lasting beauty effects when in contact with sebum and water.
Smart Images

Figure BDA0005059492290000091 
Figure BDA0005059492290000181 
Figure BDA0005059492290000182
Abstract
Description
Technical Field
[0001] The present invention relates to compositions suitable for use on keratinous materials, preferably keratinous fibers, and more preferably eyebrows, and to methods involving the same. Background of the Invention
[0003] The combination of MQ resin and silicone gum has been used in anhydrous liquid cosmetic compositions with volatile carriers for color transfer resistance or wear resistance. U.S. Patents Nos. 6,074,654, 6,139,823, 6,340,466, 6,406,683, 6,071,503, 6,019,962, 6,464,964 and 7,160,550 relate to this technology. For example, U.S. Patents Nos. 6,074,654 and 6,340,466 disclose a composition for lips comprising MQ resin and silicone gum in isododecane (see Example 6).
[0004] Disclosure of the Invention
[0005] For some makeup products (especially eyebrow makeup products), both wear resistance and a natural makeup finish such as a matte finish are preferred. Compositions for lips (such as those disclosed in the above prior art documents) may not require a natural makeup finish. On the contrary, in many cases, compositions for lips require a higher gloss.
[0006] On the other hand, in general, a comfortable texture such as reduced makeup stickiness and smooth spreading during application is also preferred for makeup products. For liquid makeup products, it is particularly preferred to provide a non-tacky or non-sticky makeup film after drying.
[0007] Adding powder can create a matte finish or provide a non-sticky makeup film. However, adding too much powder ingredients for a matte finish or non-stickiness may deteriorate smoothness during application.
[0008] Furthermore, liquid makeup products are also preferably stable over extended periods of time, especially at elevated temperatures.
[0009] An object of the present invention is to provide an anhydrous liquid composition suitable for making up keratin substances, preferably keratin fibers, and more preferably eyebrows, which is stable and can provide excellent cosmetic effects, such as a matte finish, good wear resistance, and a comfortable texture such as reduced makeup stickiness and smooth spreading during application.
[0010] The above objects of the present invention can be achieved by an anhydrous liquid composition for keratin substances (preferably keratin fibers, and more preferably for eyebrows), the anhydrous liquid composition comprising:
[0011] (a) at least one silicone resin;
[0012] (b) at least one silicone adhesive;
[0013] (c) at least one volatile hydrocarbon oil;
[0014] (d) at least one filler; and
[0015] (e) at least one lipophilic gelling agent selected from organically modified clays, wherein
[0016] (d) The filler comprises
[0017] (d-1) at least one hydrophobic inorganic filler, which is preferably selected from hydrophobically modified metal oxides, and more preferably selected from hydrophobic silica,
[0018] and
[0019] in
[0020] The total amount of (d) filler and (e) lipophilic gelling agent in the composition is greater than 18.5% by weight relative to the total weight of the composition.
[0021] The amount of (e) lipophilic gelling agent in the composition is greater than 2.5 wt % and less than 10 wt %, relative to the total weight of the composition.
[0022] The amount of (d) filler in the composition is less than 21% by weight relative to the total weight of the composition, and
[0023] The amount of (d-1) the hydrophobic inorganic filler in the composition is less than 2 wt % relative to the total weight of the composition.
[0024] (a) The silicone resin may be selected from MQ resins.
[0025] The (a) silicone resin may be present in an amount of 1 to 30 wt %, preferably 5 to 25 wt %, and more preferably 10 to 20 wt %, relative to the total weight of the composition.
[0026] (b) The silicone adhesive may be selected from polydimethylsiloxane adhesive.
[0027] The dynamic viscosity of the (b) silicone gum at 25° C. may be 400,000 cSt or more, preferably 600,000 cSt or more, and more preferably 800,000 cSt or more.
[0028] The (b) silicone gum may be present in an amount of 1 to 25 wt %, preferably 3 to 20 wt %, and more preferably 5 to 15 wt %, relative to the total weight of the composition.
[0029] (c) The volatile hydrocarbon oil may be selected from isododecane, C 8-9 Isoparaffins and mixtures thereof.
[0030] (c) volatile hydrocarbon oil may be present in an amount of 10% to 60% by weight, preferably 15% to 55% by weight and more preferably 20% to 50% by weight relative to the total weight of the composition.
[0031] (d) filler may be present in an amount of 10 to 20 wt%, preferably 12 to 19 wt%, and more preferably 14 to 18 wt%, relative to the total weight of the composition.
[0032] (d) Filler may further comprise (d-2) at least one hydrophobic organic filler, which is preferably selected from hydrophobically modified starches, and more preferably selected from esterified starches.
[0033] The (d-1) hydrophobic inorganic filler may be present in an amount of 0.1 to less than 2 wt%, preferably 0.2 to 1.5 wt%, and more preferably 0.3 to 1 wt%, relative to the total weight of the composition.
[0034] (e) The lipophilic gelling agent may be selected from organically modified bentonite, organically modified hectorite, and mixtures thereof.
[0035] (e) The lipophilic gelling agent may be present in an amount of 3 to 9.5 wt%, preferably 4 to 9 wt%, and more preferably 5 to 8.5 wt%, relative to the total weight of the composition.
[0036] The total amount of (d) filler and (e) lipophilic gelling agent present may be 19 to 35 wt%, preferably 20 to 30 wt% and more preferably 21 to 25 wt% relative to the total weight of the composition.
[0037] The present invention may also relate to a cosmetic method for keratinous materials, preferably keratinous fibers, and more preferably eyebrows, comprising the following steps:
[0038] The composition according to the invention is applied to keratin substances. DETAILED DESCRIPTION OF THE INVENTION
[0040] After diligent research, the inventors have found that it is possible to provide an anhydrous liquid composition suitable for making up keratin substances, preferably keratin fibers, and more preferably eyebrows, which is stable and can provide excellent cosmetic effects such as a matte finish, good wear resistance, and a comfortable texture such as reduced makeup stickiness and smooth spreading during application.
[0041] The composition according to the invention is therefore an anhydrous liquid composition for keratinous materials, preferably keratinous fibres and more preferably eyebrows, comprising:
[0042] (a) at least one silicone resin;
[0043] (b) at least one silicone adhesive;
[0044] (c) at least one volatile hydrocarbon oil;
[0045] (d) at least one filler; and
[0046] (e) at least one lipophilic gelling agent selected from organically modified clays,
[0047] in
[0048] (d) The filler comprises
[0049] (d-1) at least one hydrophobic inorganic filler, which is preferably selected from hydrophobically modified metal oxides, and more preferably selected from hydrophobic silica,
[0050] and
[0051] in
[0052] The total amount of (d) filler and (e) lipophilic gelling agent in the composition is greater than 18.5% by weight relative to the total weight of the composition.
[0053] The amount of (e) lipophilic gelling agent in the composition is greater than 2.5 wt % and less than 10 wt %, relative to the total weight of the composition.
[0054] The amount of (d) filler in the composition is less than 21% by weight relative to the total weight of the composition, and
[0055] The amount of (d-1) the hydrophobic inorganic filler in the composition is less than 2 wt % relative to the total weight of the composition.
[0056] (d) The filler is different from (e) the lipophilic gelling agent.
[0057] The composition according to the present invention is stable and can provide excellent cosmetic effects such as a matte finish, good wear resistance, and a comfortable texture such as reduced makeup stickiness and smooth spreading during application.
[0058] The composition according to the invention is stable for a long period of time even at elevated temperatures. Thus, the composition according to the invention can be stored for a long period of time even under hot conditions.
[0059] The composition according to the present invention can provide a matte makeup surface or a makeup surface with low glossiness to keratin substances (preferably keratin fibers, and more preferably eyebrows). That is, the composition according to the present invention can provide a natural makeup makeup surface.
[0060] The composition according to the present invention can provide a comfortable texture, such as reduced makeup stickiness and smooth spreading during application. That is, the composition according to the present invention can slide or glide smoothly on keratin substances, preferably keratin fibers, and more preferably eyebrows.
[0061] The cosmetic effect provided by the composition according to the present invention may be long-lasting or may be maintained for a long period of time. The cosmetic effect provided by the composition according to the present invention may have good sebum resistance or water resistance. Therefore, even when exposed to, for example, sweat or rain, the makeup according to the composition according to the present invention may last for a long period of time. Therefore, the composition according to the present invention may also provide good wear resistance for keratin substances (preferably keratin fibers, and more preferably eyebrows).
[0062] The compositions according to the invention may also provide a make-up which is resistant to colour transfer or wear.
[0063] Hereinafter, the composition and method according to the present invention will be explained in a more detailed manner.
[0064] [Composition]
[0065] (Silicone resin)
[0066] The composition according to the invention comprises (a) at least one silicone resin. If two or more silicone resins are used, they may be identical or different.
[0067] The term "resin" refers to a compound whose structure is three-dimensional. "Silicone resin" is also called "silicone-based resin" or "silicone resin". For the purposes of the present invention, linear polydimethylsiloxanes are therefore not silicone resins.
[0068] The nomenclature of silicone resins (also called siloxane resins) is known by the name "MDTQ", the description of the resin varying with the various siloxane monomer units it comprises, wherein each of the letters "MDTQ" characterizes one type of unit.
[0069] The letter "M" stands for R 1 R 2 R 3 SiO 1 / 2 A monofunctional unit in which the silicon atom is bonded to only one oxygen atom in the polymer comprising the unit.
[0070] The letter "D" represents a difunctional unit R 1 R2 SiO 2 / 2 , in which a silicon atom is connected to two oxygen atoms.
[0071] The letter "T" stands for R l SiO 3 / 2 The trifunctional unit.
[0072] Such resins are described, for example, in "Encyclopedia of Polymer Science and Engineering" (Vol. 15, John Wiley & Sons, New York (1989), pp. 265-270) and USP 2,676,182, USP 3,627,851, USP 3,772,247 and USP 5,248,739 or USP 5,082,706, USP 5,319,040, USP 5,302,685 and USP 4,935,484.
[0073] In the previously defined M, D, and T units, R (i.e., R 1 , R 2 and R 3 ) represents a hydrocarbon-based group (especially an alkyl group) containing 1 to 10 carbon atoms, a phenyl group, a phenylalkyl group or a hydroxy group.
[0074] Finally, the letter "Q" represents the tetrafunctional unit SiO 4 / 2 , in which a silicon atom is linked to four oxygen atoms, which are themselves linked to the rest of the polymer.
[0075] From these different units it is possible to obtain a wide range of silicone resins having different properties, the properties of these polymers varying with the type of monomer (or unit), the nature and number of groups R, the length of the polymer chain, the degree of branching and the size of the side chains.
[0076] As the silicone resin that can be used in the composition according to the present invention, for example, an MQ type silicone resin, a T type silicone resin, or an MQT type silicone resin can be used.
[0077] MQ resin:
[0078] As examples of MQ type silicone resins, mention may be made of the formula [(R1) 3 SiO 1 / 2 ] x (SiO 4 / 2 ) y (MQ units) wherein x and y are integers ranging from 50 to 80 and such that the group R1 represents a group as previously defined and is preferably an alkyl group containing 1 to 8 carbon atoms, preferably a methyl group.
[0079] Mention may be made, as examples of MQ type solid silicone resins of the trimethylsiloxysilicate type, of those sold under the reference SR1000 by General Electric Co., TMS 803 by Wacker Chemie AG or KF-7312J by Shin-Etsu Chemical Co., Ltd. or DC749 or DC593 by Dow Corning Corporation.
[0080] Mention may also be made, as silicone resin comprising MQ siloxysilicate units, of phenylalkylsiloxysilicate resins, such as phenylpropyldimethylsiloxysilicate (Silshine 151 sold by the company General Electric). The preparation of such resins is described in particular in patent USP 5,817,302.
[0081] Resin T:
[0082] Examples of these T-type silicone resins that may be mentioned include those of the formula (RSiO 3 / 2 ) x (Unit T) a polysilsesquioxane wherein x is greater than 100 and such that the radical R is an alkyl radical containing from 1 to 10 carbon atoms, said polysilsesquioxane possibly also comprising Si-OH terminal groups.
[0083] Polymethylsilsesquioxane resins which may be preferably used are those in which R represents a methyl group, for example:
[0084] - those sold by the company Wacker under the reference ResinMK, for example Belsil PMS MK: containing CH 3 SiO 3 / 2 The polymer may further contain up to 1% by weight of (CH 3 ) 2 SiO 2 / 2 unit (unit D) and having an average molecular weight of about 10000 g / mol, or
[0085] - those sold by the company Shin-Etsu under the reference KR-220L, which are of the formula CH 3 SiO 3 / 2 Those sold under the designation KR-242A, which contain 98% of units T and 2% of dimethyl units D and have Si-OH end groups, or those sold under the designation KR-251, which contain 88% of units T and 12% of dimethyl units D and have Si-OH end groups.
[0086] MQT resin:
[0087] Especially known resins comprising MQT units are those mentioned in document USP 5,110,890.
[0088] A preferred form of MQT-type resin is MQT-propyl (also called MQTPr) resin.Resins of this type that can be used in the composition according to the invention are the resins described and prepared in patent application WO 2005 / 075542, the content of which is incorporated herein by reference.
[0089] The MQ-T-propyl resin preferably comprises the following units:
[0090] (i)(R1 3 SiO 1 / 2 ) a
[0091] (ii)(R2 2 SiO 2 / 2 ) b
[0092] (ii)(R3SiO 3 / 2 ) c and
[0093] (iv)(SiO 4 / 2 ) d
[0094] in
[0095] R1, R2 and R3 independently represent a hydrocarbon-based group (especially an alkyl group) containing 1 to 10 carbon atoms, a phenyl group, a phenylalkyl group or a hydroxyl group, and preferably an alkyl group containing 1 to 8 carbon atoms, or a phenyl group,
[0096] a is between 0.05 and 0.5,
[0097] b is between 0 and 0.3,
[0098] c is greater than 0,
[0099] d is between 0.05 and 0.6,
[0100] a+b+c+d=1, and a, b, c and d are mole fractions,
[0101] Provided that more than 40 mol % of the groups R3 of the siloxane resin are propyl groups.
[0102] Preferably, the siloxane resin comprises the following units:
[0103] (i)(R1 3 SiO 1 / 2 )a
[0104] (iii)(R3SiO 3 / 2 ) c and
[0105] (iv)(SiO 4 / 2 ) d
[0106] in
[0107] R1 and R3 independently represent an alkyl group containing 1 to 8 carbon atoms, R1 is preferably a methyl group, and R3 is preferably a propyl group,
[0108] a is between 0.05 and 0.5, and preferably between 0.15 and 0.4,
[0109] c is greater than 0 and preferably between 0.15 and 0.4,
[0110] d is between 0.05 and 0.6, preferably between 0.2 and 0.6 or between 0.2 and 0.55,
[0111] a+b+c+d=1, and a, b, c and d are mole fractions,
[0112] Provided that more than 40 mol % of the groups R3 of the siloxane resin are propyl groups.
[0113] The siloxane resins that can be used according to the invention can be obtained via a process comprising the reaction of:
[0114] A) contains at least 80 mol % of units (R1 3 SiO 1 / 2 ) and (SiO 4 / 2 ) d MQ resin
[0115] R1 represents an alkyl group, an aryl group, a carbinol group or an amino group containing 1 to 8 carbon atoms,
[0116] a and d are greater than 0,
[0117] The ratio a / d is between 0.5 and 1.5;
[0118] and
[0119] B) contains at least 80 mol% of units (R3SiO 3 / 2 ) c T-propyl resin,
[0120] R3 represents an alkyl group, an aryl group, a carbinol group or an amino group containing 1 to 8 carbon atoms,
[0121] c is greater than 0,
[0122] Provided that at least 40 mol % of the radicals R3 are propyl,
[0123] The mass ratio A / B is between 95 / 5 and 15 / 85, and the mass ratio A / B is preferably 30 / 70.
[0124] Advantageously, the mass ratio A / B is between 95 / 5 and 15 / 85. Preferably, the ratio A / B is less than or equal to 70 / 30. These preferred ratios have proven to produce a comfortable deposit, which is attributed to the absence of penetration of rigid MQ resin particles in the deposit.
[0125] Therefore, preferably, the silicone resin is selected from:
[0126] a) MQ type resins, in particular selected from (i) alkylsiloxysilicates, which may be of the formula [(R1) 3 SiO 1 / 2 ] x (SiO 4 / 2 ) y trimethylsiloxysilicate resins wherein x and y are integers ranging from 50 to 80 and such that the group R1 represents a hydrocarbon-based group containing 1 to 10 carbon atoms, a phenyl group, a phenylalkyl group or a hydroxyl group, and preferably an alkyl group containing 1 to 8 carbon atoms, preferably a methyl group, and (ii) a phenylalkylsiloxysilicate resin, for example phenylpropyldimethylsiloxysilicate, and / or
[0127] b) T-type resin, especially selected from the formula (RSiO 3 / 2 ) x wherein x is greater than 100, and the group R is an alkyl group containing 1 to 10 carbon atoms, such as a methyl group, and the polysilsesquioxane may also contain Si-OH end groups, and / or
[0128] c) MQT-type resins, especially MQT-propyl type resins, which may contain units (i) (R1 3 SiO 1 / 2 ) a (ii)(R2 2 SiO 2 / 2 ) b (iii)(R3SiO 3 / 2 ) c and (iv) (SiO 4 / 2 ) d ,
[0129] wherein R1, R2 and R3 independently represent a hydrocarbon-based group (especially an alkyl group) containing 1 to 10 carbon atoms, a phenyl group, a phenylalkyl group or a hydroxyl group, and preferably an alkyl group containing 1 to 8 carbon atoms, or a phenyl group,
[0130] a is between 0.05 and 0.5,
[0131] b is between 0 and 0.3,
[0132] c is greater than 0,
[0133] d is between 0.05 and 0.6,
[0134] a+b+c+d=1, and a, b, c and d are mole fractions,
[0135] Provided that more than 40 mol % of the groups R3 of the siloxane resin are propyl groups.
[0136] Preferably, the (a) silicone resin is selected from MQ resins, and more preferably is trimethylsiloxysilicate.
[0137] The amount of (a) silicone resin in the composition according to the present invention may be 1 wt % or more, preferably 5 wt % or more, and more preferably 10 wt % or more, relative to the total weight of the composition.
[0138] The amount of (a) silicone resin in the composition according to the present invention may be 30 wt % or less, preferably 25 wt % or less, and more preferably 20 wt % or less, relative to the total weight of the composition.
[0139] Therefore, the amount of (a) silicone resin in the composition according to the present invention may be 1 to 30 wt%, preferably 5 to 25 wt%, and more preferably 10 to 20 wt%, relative to the total weight of the composition.
[0140] (Silicone glue)
[0141] The composition according to the invention comprises (b) at least one silicone gum. If two or more (b) silicone gums are used, they may be identical or different.
[0142] (b) The dynamic viscosity of the silicone gum at 25° C. may be 400,000 cSt or more, preferably 600,000 cSt or more, and more preferably 800,000 cSt or more.
[0143] (b) The dynamic viscosity of the silicone gum at 25° C. may be 10,000,000 cSt or less, preferably 5,000,000 cSt or less, and more preferably 3,000,000 cSt or less.
[0144] (b) The dynamic viscosity of the silicone gum at 25° C. may be 300,000 to 10,000,000 cSt, preferably 500,000 to 5,000,000 cSt or less, and more preferably 700,000 to 3,000,000 cSt.
[0145] (b) The dynamic viscosity of silicone gum can be measured according to standard ASTM D-445.
[0146] It is preferred that the (b) silicone gum has no functional groups such as amino groups.
[0147] (b) The silicone gel can be selected from silicones of the following formula:
[0148]
[0149] in:
[0150] R1, R2, R5 and R6 together or individually are alkyl groups containing 1 to 6 carbon atoms,
[0151] R3 and R4 together or individually are alkyl, vinyl, amino or hydroxyl groups containing 1 to 6 carbon atoms,
[0152] X is an alkyl group containing 1 to 6 carbon atoms, a hydroxyl group or an amine group, and
[0153] n and p are integers selected so that the compound has a dynamic viscosity at 25°C of 400,000 cSt or more, preferably 600,000 cSt or more, and more preferably 800,000 cSt or more.
[0154] As silicone gums that can be used according to the invention, mention may be made of the following:
[0155] - in which the substituents R1 to R6 represent methyl, the group X represents methoxy, and n and p are such that the polymer has a molecular weight of 600,000 g / mol, such as the product sold under the name Mirasil C-DPDM by the company Bluestar;
[0156] - in which the substituents R1 to R6 represent methyl, the group X represents a hydroxyl group and n and p are such that the polymer has a molecular weight of 600,000 g / mol, such as the product sold under the name SGM 36 by the company Dow Corning; and
[0157] - polydimethylsiloxanes of the (polydimethylsiloxane)(methylvinylsiloxane) type, for example SE63 sold by GE Bayer Silicones; poly(dimethylsiloxane)(diphenyl)(methylvinylsiloxane) copolymers; and mixtures thereof.
[0158] The molecular weight of the (b) silicone gum may be greater than 350,000 g / mol, between 350,000 and 800,000 g / mol, and preferably from 450,000 to 700,000 g / mol.
[0159] Preferably, (b) silicone gum is selected from polydimethylsiloxane gum.
[0160] The amount of (b) silicone gum in the composition according to the present invention is 1 wt% or more, and may be preferably 3 wt% or more, and more preferably 5 wt% or more, relative to the total weight of the composition.
[0161] The amount of (b) silicone gum in the composition according to the present invention is 25 wt% or less, and may preferably be 20 wt% or less, and more preferably 15 wt% or less, relative to the total weight of the composition.
[0162] Therefore, the amount of (b) silicone gum in the composition according to the invention is 1 to 25 wt%, preferably 3 to 20 wt%, and more preferably 5 to 15 wt%, relative to the total weight of the composition.
[0163] (Volatile hydrocarbon oil)
[0164] The composition according to the invention comprises (c) at least one volatile hydrocarbon oil. If two or more (c) volatile hydrocarbon oils are used, they may be identical or different.
[0165] "Oil" herein means a fatty compound or substance that is in the form of a liquid or paste (not solid) at room temperature (25°C) under atmospheric pressure (760 mmHg).
[0166] The term "volatile oil" is understood within the meaning of the present invention to mean an oil capable of evaporating in less than 1 hour on contact with the skin or keratin fibers at ambient temperature (20-25° C.) and atmospheric pressure. The volatile oils of the present invention are volatile cosmetic oils which are liquid at ambient temperature and have a non-zero vapor pressure at ambient temperature and atmospheric pressure, in particular ranging from 0.13 Pa to 40000 Pa (10 -3 mmHg to 300 mmHg), particularly in the range of 1.3 Pa to 13000 Pa (0.01 mmHg to 100 mmHg), and more particularly in the range of 1.3 Pa to 1300 Pa (0.01 mmHg to 10 mmHg).
[0167] As examples of volatile hydrocarbon oils that can be used in the present invention, mention may be made of volatile hydrocarbon oils chosen from hydrocarbon oils having 8 to 16 carbon atoms, in particular C 2-6 carbon atoms of petroleum origin. 8 -C 16Isoalkanes (also known as isoparaffins), such as isododecane (also known as 2,2,4,4,6-pentamethylheptane), isodecane and isohexadecane, such as the oils sold under the trade names Isopar or Permethyl; branched C 8 -C 16 Esters; isohexyl neopentanoate; and mixtures thereof. Other volatile hydrocarbon oils may also be used, such as petroleum fractions, in particular those sold by Shell under the name Shell Solt; volatile linear alkanes, such as those described in patent application DE102008012457 from Cognis.
[0168] Among the volatile hydrocarbon oils, C 8 -C 16 Isoalkanes, particularly isododecane.
[0169] Preferably, (c) the volatile hydrocarbon oil is selected from isododecane, C 8-9 Isoparaffins and mixtures thereof.
[0170] The amount of (c) volatile hydrocarbon oil in the composition according to the present invention may be 10% by weight or more, preferably 15% by weight or more, and more preferably 20% by weight or more, relative to the total weight of the composition.
[0171] The amount of (c) volatile hydrocarbon oil in the composition according to the invention may be 60% by weight or less, preferably 55% by weight or less and more preferably 50% by weight or less, relative to the total weight of the composition.
[0172] The amount of (c) volatile hydrocarbon oil in the composition according to the invention may range from 10% to 60% by weight, preferably from 15% to 55% by weight and more preferably from 20% to 50% by weight relative to the total weight of the composition.
[0173] (filler)
[0174] The composition according to the invention comprises (d) at least one filler. If two or more (d) fillers are used, they may be identical or different.
[0175] The term "filler" is understood to mean colourless or white inorganic or synthetic particles which are insoluble in possible liquid constituents of the composition according to the invention, whatever the temperature at which the composition is manufactured.
[0176] (d) Fillers may be inorganic or organic and may be spherical or ellipsoidal, regardless of the crystal form (e.g., lamellar, cubic, hexagonal, orthorhombic, etc.). Non-limiting examples include talc, mica, silica, silica silylate, kaolin, sericite, calcined talc, calcined mica, calcined sericite, synthetic mica, bismuth oxychloride, barium sulfate, boron nitride, calcium carbonate, magnesium carbonate, magnesium hydrogen carbonate and hydroxyapatite, polyamide Powders formed, powders formed of poly-β-alanine and polyethylene, powders formed of polyurethane, tetrafluoroethylene polymers powders, lauryl lysine, starch; polymer hollow microspheres, such as those of poly(vinylidene chloride) / acrylonitrile (e.g. (Nobel Industrie)) or acrylic copolymers; silicone resin microspheres (e.g. from Toshiba ), particles formed from polyorganosiloxane elastomers, precipitated calcium carbonate, magnesium carbonate, basic magnesium carbonate, hollow silica microspheres, glass or ceramic microcapsules; or metal soaps derived from organic carboxylic acids having 8 to 22 carbon atoms (e.g., 12 to 18 carbon atoms), such as zinc stearate, magnesium stearate, lithium stearate, zinc laurate or magnesium myristate.
[0177] For the purpose of the present invention, examples of (d) fillers include metal oxides, preferably silicon dioxide, titanium oxide, zinc oxide, and mixtures thereof.
[0178] Fillers suitable for use in the present invention may be, for example, fillers whose average particle size is less than 100 μm (and in particular between 1 μm and 50 μm, for example between 4 μm and 20 μm).
[0179] (d) The filler can be hydrophilic or hydrophobic.
[0180] The (d) filler may or may not be capable of absorbing (and / or adsorbing) oil or liquid fatty substances, such as sebum (from the skin). Preferably, the (d) filler is capable of absorbing (and / or adsorbing) oil or liquid fatty substances, such as sebum (from the skin).
[0181] The hydrophilic oil-absorbing powder or the hydrophobic oil-absorbing powder may comprise porous particles or hollow particles, in particular porous spherical particles or hollow spherical particles.
[0182] Hydrophilic oil-absorbing powder:
[0183] For the purposes of the present invention, the term "hydrophilic" oil-absorbing powder means that the powder (or particles) can be dispersed individually in water in such a way that no aggregates are formed.
[0184] The hydrophilic oil-absorbing powder may have an oil absorption capacity of 100 ml / 100 g or more, preferably 150 ml / 100 g or more, and more preferably 200 ml / 100 g or more.
[0185] The amount of oil absorbed (and / or adsorbed) by a hydrophilic oil-absorbing powder can be characterized by measuring the wet point according to the method described below. The oil absorption capacity measured at the wet point (denoted as Wp) corresponds to the amount of oil that needs to be added to 100 grams of powder in order to obtain a homogeneous paste.
[0186] The amount of absorbed (and / or adsorbed) oil can be measured according to the method for determining the oil absorption of powders described in standard NF T 30-022. By measuring the wet point, it corresponds to the amount of oil absorbed / adsorbed onto the available surface of the powder.
[0187] An amount of powder m=2 grams is placed on a glass plate and then oil (for example ester oil and silicone oil) is added dropwise. After adding 4 to 5 drops of oil to the powder, mixing is carried out using a spatula and the addition of oil is continued until an aggregate of oil and powder is formed. At this point, the oil is added drop by drop and then the mixture is ground with a spatula. The addition of oil is stopped when a firm, smooth paste is obtained. This paste must be able to be spread on the glass plate without cracking or forming lumps. The volume of oil used Vs (expressed in milliliters) is then recorded. The oil absorption corresponds to the ratio Vs / m.
[0188] In addition, the oil absorption capacity can be measured in accordance with JIS-K6217-4.
[0189] The hydrophilic oil-absorbing powder may be of organic or inorganic nature.
[0190] The hydrophilic oil-absorbing powder may be selected from cellulose, silicon dioxide, silicates; perlite; magnesium carbonate; magnesium hydroxide; and derivatives thereof; and mixtures thereof.
[0191] According to one embodiment, the cellulose derivative may be selected from cellulose esters and cellulose ethers.
[0192] In the above and below, the term "cellulose ester" means a polymer consisting of an alpha (1-4) sequence of partially or completely esterified anhydroglucose rings, the esterification being obtained by reaction of all or only some of the free hydroxyl functions of said anhydroglucose rings with linear or branched carboxylic acids or carboxylic acid derivatives (acyl chlorides or anhydrides) containing from 1 to 4 carbon atoms. Preferably, the cellulose ester results from the reaction of some of the free hydroxyl functions of said rings with carboxylic acids containing from 1 to 4 carbon atoms. Advantageously, the cellulose ester is chosen from cellulose acetate, cellulose propionate, cellulose butyrate, cellulose isobutyrate, cellulose acetobutyrate and cellulose levulinate, and mixtures thereof.
[0193] The term "cellulose ether" means a polymer consisting of an alpha (1-4) sequence of partially etherified anhydroglucose rings, some of the free hydroxyl functions of which are substituted by a group -OR, R preferably being a linear or branched alkyl group containing 1 to 4 carbon atoms. Cellulose ethers are thus preferably chosen from cellulose alkyl ethers having an alkyl group containing 1 to 4 carbon atoms, such as cellulose methyl ether, cellulose propyl ether, cellulose isopropyl ether, cellulose butyl ether and cellulose isobutyl ether.
[0194] Cellulose and its derivatives that may be mentioned include, for example, the following spherical cellulose particles sold by Daito Kasei of Japan: Cellulobeads USF (oil absorption 250 ml / 100 g) with a particle size of 4 μm (porous cellulose).
[0195] Silica powders that may be mentioned include porous silica microspheres, especially those produced by the company Asahi Glass under the name H31 and H51 (oil absorption equal to 150 ml / 100 g); MSS-500-3H (sold by the company Kobo); amorphous hollow silica particles, in particular those sold under the name Silica Shells by the company Kobo (oil absorption equal to 550 ml / 100 g); porous silica microspheres sold under the name Sylysia 350 by the company Fuji Silysia Chemical (oil absorption equal to 310 ml / 100 g); and silica powder sold under the name Finesil X35 by the company Oriental Silycas (oil absorption equal to 380 ml / 100 g).
[0196] Silicates that may be mentioned in particular are aluminum silicates, which are marketed by the company Kyowa Chemical Industry under the name Sold at 700PEL (oil absorption equal to 195ml / 100g).
[0197] In particular, perlite powder is produced by the company World Minerals under the name 1430OR and Product sold at 2550OR (oil absorption equal to 240ml / 100g).
[0198] Magnesium carbonate powder which may be mentioned in particular is produced by the company Buschle & Lepper under the name Tipo Product sold (oil absorption equal to 214ml / 100g).
[0199] Magnesium carbonate / magnesium hydroxide powders that may be mentioned in particular are mMgCO 3-Mg(OH) 2 -nH 2 O product, which is sold under the name Mg Tube by the company Nittesu Mining (oil absorption equal to 250-310 ml / 100 g).
[0200] Preferably, the hydrophilic oil-absorbing powder comprises at least one selected from the group consisting of cellulose, silica, perlite and a mixture thereof.
[0201] Hydrophobic Oil-Absorbing Powder:
[0202] For the purposes of the present invention, the term "hydrophobic" oil-absorbing powder means that the powder (or particles) can be dispersed individually in oil in such a way that no aggregates are formed.
[0203] The hydrophobic oil-absorbing powder may have an oil absorption capacity of 100 ml / 100 g or more, preferably 150 ml / 100 g or more, and more preferably 200 ml / 100 g or more.
[0204] The amount of oil absorbed (and / or adsorbed) by the hydrophobic oil absorbing powder can be determined by the method described above.
[0205] The hydrophobic, oil-absorbing powders may be of organic or inorganic nature.
[0206] Organic hydrophobic oil absorbing powder:
[0207] The organic hydrophobic oil-absorbing powder may be selected from polyamide (especially nylon-6) powder; acrylic polymer powder, especially polymethyl methacrylate powder, polymethyl methacrylate / ethylene glycol dimethacrylate powder, polyallyl methacrylate / ethylene glycol dimethacrylate powder, or ethylene glycol dimethacrylate / lauryl methacrylate copolymer powder; and mixtures thereof. The above materials may be cross-linked.
[0208] It is preferred that the organic hydrophobic oil-absorbing powder is selected from powders of acrylic polymers, especially powders of ethylene glycol dimethacrylate / lauryl methacrylate copolymers.
[0209] Examples of the organic hydrophobic oil-absorbing powder include the fillers described below.
[0210] Acrylic polymer powders that may be mentioned include porous polymethyl methacrylate (INCI name Methyl Methacrylate Crosspolymer), for example the spheres sold under the name Covabead LH85 by the company Sensient; porous polymethyl methacrylate / ethylene glycol dimethacrylate spheres (oil absorption equal to 155 ml / 100 g) sold under the name Microsponge 5640 by the company Cardinal Health Technologies; ethylene glycol dimethacrylate / lauryl methacrylate crosslinked copolymer powders, especially sold under the name Lacrox® by the company Amcol Health & Beauty Solutions. those sold under the name Expancel 551DE40D42 by the company Akzo Novel (oil absorption equal to 1040 ml / 100 g).
[0211] Polyamide powders that may be mentioned include nylon-6 powders, especially the product sold under the name Pomp 610 by the company UBE Industries (oil absorption equal to 202 ml / 100 g).
[0212] Inorganic hydrophobic oil absorbing powder:
[0213] The inorganic hydrophobic oil-absorbing powder may have at least one inorganic core and at least one hydrophobic coating.
[0214] Preferably, the inorganic hydrophobic oil-absorbing powder is selected from the group consisting of hydrophobic silica powders, preferably hydrophobic silica aerogels, and more preferably hydrophobic aerogels of silylated silica, and mixtures thereof.
[0215] The term "hydrophobic silica" is understood to mean any silica whose surface has been treated to render it hydrophobic.
[0216] The hydrophobic silica (particularly silylated silica) may be based on silica aerogel, which is a porous material obtained by replacing (by drying) the liquid component of silica gel with air.
[0217] They are usually synthesized via a sol-gel process in a liquid medium and subsequently reacted with a supercritical fluid (the most common one being supercritical CO). 2) extraction to dry. This type of drying makes it possible to avoid shrinkage of pores and materials. The sol-gel process and various drying operations are described in detail in Brinker CJ. and Scherer GW, Sol-Gel Science (New York, Academic Press, 1990).
[0218] Aerogel is a material with high porosity. Herein, silica aerogel refers to solid silica with a porous structure, which is generally obtained by replacing the medium contained in wet silica gel with air by drying the wet silica gel while maintaining the solid network structure of silica. Porosity refers to the amount of air contained in the apparent volume of the material in volume percentage. The porosity of the hydrophobic silica aerogel of the present invention may be 60% or more, preferably 70% or more, and more preferably 80% or more.
[0219] Hydrophobic silica aerogel particles can exhibit
[0220] Range 500m 2 / g to 1,500m 2 / g, preferably 600m 2 / g to 1,200m 2 / g, and more preferably 600m 2 / g to 800m 2 / g of specific surface area per unit weight (SW), and / or
[0221] The size expressed as the volume mean diameter (D[0.5]) is 1 μm to 1,500 μm, preferably 1 μm to 1,000 μm, more preferably 1 μm to 100 μm, in particular 1 μm to 30 μm, more preferably 5 μm to 25 μm, more preferably 5 μm to 20 μm, and even more preferably 5 μm to 15 μm.
[0222] The specific surface area per unit weight can be determined by a nitrogen adsorption method called the BET (Brunauer-Emmett-Teller) method described in the Journal of the American Chemical Society (Volume 60, page 309, February 1938) in accordance with the international standard ISO 5794 / 1 (Appendix D). The BET specific surface area corresponds to the total specific surface area of the particles under consideration.
[0223] The size of the hydrophobic silica aerogel particles can be measured by static light scattering using a commercial particle size analyzer of the MasterSizer 2000 type from Malvern. The data are processed based on the Mie scattering theory. This theory, which is exact for isotropic particles, makes it possible to determine the "effective" particle size in the case of non-spherical particles. The theory is described in particular in the publication "Light Scattering by Small Particles" by Van de Hulst, HC (Chapters 9 and 10, Wiley, New York, 1957).
[0224] The hydrophobic silica aerogel particles may advantageously exhibit a range of 0.04 g / cm 3 Up to 0.10g / cm 3 , and preferably 0.05g / cm 3 Up to 0.08g / cm 3 The packing density (r).
[0225] In the context of the present invention, this density, called packing density, can be evaluated according to the following procedure:
[0226] Pour 40 g of powder into a graduated cylinder;
[0227] The cylinder was then placed on a Stav 2003 device from StampfVolumeter;
[0228] The cylinder is then subjected to a series of 2500 filling operations (this operation is repeated until the volume difference between 2 consecutive tests is less than 2%); and
[0229] The final volume Vf of the filled powder is then measured directly on the graduated cylinder. The final volume Vf is calculated by the ratio w / Vf (in this case 40 / Vf) (Vf is in cm 3 The packing density is determined by .
[0230] Regarding the preparation of hydrophobic silica aerogel particles modified at the surface by silylation, reference may be made to document US Pat. No. 7,470,725.
[0231] Use will in particular be made of hydrophobic silica aerogel particles modified at the surface with trimethylsilyl groups.
[0232] Inorganic hydrophobic oil-absorbing powders that may be mentioned include amorphous silica microspheres coated with polydimethylsiloxane, in particular those known under the name H33 and H53 (oil absorption equal to 400 ml / 100 g); precipitated silica powders surface-treated with mineral waxes, for example precipitated silicas treated with polyethylene wax, and in particular those sold under the name Acematt OR 412 by the company Evonik-Degussa (oil absorption equal to 398 ml / 100 g); and silylated silicas sold under the name VM-2270 by the company Dow (oil absorption equal to 1,040 ml / 100 g).
[0233] As inorganic hydrophobic oil-absorbing powder, preferably use is made of silylated silica sold under the name VM-2270 by the company Dow, the particles of which exhibit an average size ranging from 5 to 15 μm and a particle size of 600 μm. 2 / g to 800m 2 / g of specific surface area per unit weight.
[0234] The hydrophobic silica aerogel particles can be characterized by a spherical shape of each particle. Due to the spherical shape, the hydrophobic silica aerogel particles can provide good smoothness to the cosmetic composition. The sphericity of the hydrophobic silica aerogel can be determined by the average circularity.
[0235] The average circularity of the spherical hydrophobic silica aerogel particles may be 0.8 or more, and preferably 0.82 or more. The average circularity of the spherical hydrophobic silica aerogel may be less than 1, preferably 0.99 or less, more preferably 0.98 or less, even more preferably 0.97 or less, still even more preferably 0.96 or less, and most preferably 0.95 or less.
[0236] The “average circularity” may be determined by an image analysis method. Specifically, the “average circularity” may be the arithmetic mean of circularities obtained by image analysis of a scanning electron microscope (SEM) image of not less than 2,000 aerogel particles observed at 1,000 magnifications by secondary electron detection using a scanning electron microscope (SEM).
[0237] The "roundness" of each aerogel particle is a value determined by the following formula:
[0238] C=4πS / L 2
[0239] Where C represents circularity, S represents the area of the aerogel particles in the image (projected area), and L represents the outer circumference (perimeter) of the aerogel particles in the image. When the average circularity approaches 1, the shape of each particle becomes more spherical.
[0240] The hydrophobic silica aerogel particles that can be used according to the present invention are preferably of a silylated silica type (INCI name: Silica Silylate). Preferably, the hydrophobic silica aerogel particles may be those described in JP-A-2014-088307, JP-A-2014-218433 or JP-A-2018-177620.
[0241] As the inorganic hydrophobic oil-absorbing powder, hydrophobic aerogel of silylated silica is preferably used.
[0242] The hydrophobicity of the hydrophobic aerogel of silylated silica can be obtained by reacting a hydrophobizing agent with silanol groups represented by the following formula present on the surface of silica:
[0243] ≡Si-OH
[0244] The symbol “≡” represents the remaining three valences of the Si atom.
[0245] The silanol group is thereby converted into a group represented by the formula:
[0246] (≡Si-O-) (4-n) S i n
[0247] wherein n is an integer from 1 to 3; each R is independently a hydrocarbon group; and when n is 2 or greater, two or more Rs may be the same as or different from each other.
[0248] The hydrophobizing agent may be a silylating agent. Therefore, according to a preferred embodiment, in the hydrophobic aerogel of silylated silica, the silica particles may be modified at the surface by silylation. As examples of silylating agents, a treating agent having one of the following formulae (1) to (3) may be mentioned.
[0249] Formula (1):
[0250] R n SiX (4-n)
[0251] wherein n represents an integer from 1 to 3; R represents a hydrocarbon group; X represents a group that can leave the molecule by breaking the bond with the Si atom in a reaction with a compound having a hydroxyl group (i.e., a leaving group); when n is 2 or greater, each R may be different; and when n is 2 or less, each X may be different.
[0252] Formula (2):
[0253]
[0254] Where R 1 represents an alkylene group; R2 and R 3 independently represent a hydrocarbon group; and R 4 and R 5 independently represent a hydrogen atom or a hydrocarbon group.
[0255] Formula (3):
[0256]
[0257] Where R 6 and R 7 independently represent a hydrocarbon group; m represents an integer from 3 to 6; when there are two or more R 6 When each R 6 can be different; and when there are two or more R 7 When each R 7 Can be different.
[0258] In the above formula (1), R is a hydrocarbon group, preferably a hydrocarbon group having a carbon number of 1 to 10, more preferably a hydrocarbon group having a carbon number of 1 to 4, and particularly preferably a methyl group.
[0259] As examples of the leaving group represented by X, there can be mentioned a halogen atom such as chlorine and bromine; an alkoxy group such as methoxy and ethoxy; a leaving group represented by -NH-SiR 3 (wherein R has the same meaning as R in formula (1)) represented by a group.
[0260] Specific examples of the hydrophobizing agent represented by the above formula (1) include chlorotrimethylsilane, dichlorodimethylsilane, trichloromethylsilane, monomethyltrimethoxysilane, monomethyltriethoxysilane and hexamethyldisilazane.
[0261] From the viewpoint of favorable reactivity, chlorotrimethylsilane, dichlorodimethylsilane, trichloromethylsilane and / or hexamethyldisilazane can most preferably be used.
[0262] The number of bonds between Si atoms and silanol groups on the silica backbone varies depending on the number (4-n) of leaving groups X. For example, if n is 2, the following bonds will occur:
[0263] (≡Si-O-) 2 S i 2 ,
[0264] If n is 3, the following bonding will occur:
[0265] ≡Si-O-SiR 3 .
[0266] In this way, the silanol groups can be silylated and thus made hydrophobic.
[0267] In the above formula (2), R 1 It may be an alkylene group, preferably an alkylene group having 2 to 8 carbon atoms, and particularly preferably an alkylene group having 2 to 3 carbon atoms.
[0268] In the above formula (2), R 2 and R 3 R is independently a hydrocarbon group, and the same preferred groups as those of R in formula (1) can be mentioned. 4 represents a hydrogen atom or a hydrocarbon group, and when it is a hydrocarbon group, there can be mentioned preferred groups the same as those of R in formula (1). When a gel of silica is treated with a compound represented by formula (2) (cyclic silazane), cleavage of Si-N bonds occurs by reaction with silanol groups, and thus the following bonding will occur on the surface of the silica skeleton in the gel:
[0269] (≡Si-O-) 2 S i 2 R 3 .
[0270] In this manner, the silanol groups can also be silylated with the cyclic silazane of the above formula (2), and can thereby be hydrophobized.
[0271] Specific examples of the cyclic silazane represented by the above formula (3) include hexamethylcyclotrisilazane and octamethylcyclotetrasilazane.
[0272] In the above formula (3), R 6 and R 7 R is independently a hydrocarbon group, and the same preferred groups as those of R in formula (2) can be mentioned. m represents an integer of 3 to 6. When a gel of silica is treated with a compound represented by formula (3) (cyclic siloxane), the following bonding will occur on the surface of the silica skeleton in the gel:
[0273] (≡Si-O-) 2 S i 6 R 7 .
[0274] In this manner, the silanol groups can also be silylated with the cyclic siloxane of the above formula (3), and can thereby be hydrophobized.
[0275] Specific examples of the cyclic siloxane represented by the above formula (3) include hexamethylcyclotrisiloxane, octamethylcyclotetrasiloxane and decamethylcyclopentasiloxane.
[0276] A hydrophobic aerogel of silylated silica can be prepared by preparing a silica sol, converting the sol into a gel, aging the gel, washing the aged gel, replacing water in the washed gel with a solvent, treating the gel with a hydrophobizing agent, and drying the hydrophobized silica.
[0277] The hydrophobic aerogel of silylated silica may have the following specific surface area determined by the BET method: 200 m 2 / g or more, preferably 400m 2 / g or more, and more preferably 500m 2 / g or more, and may have the following specific surface area measured by the BET method: 1,200 m 2 / g or less, preferably 1,000m 2 / g or less, and more preferably 800m 2 / g or less.
[0278] The hydrophobic aerogel of silylated silica may have a pore volume of 1 ml / g or more, preferably 2 ml / g or more, and more preferably 3 ml / g or more, as measured by the BJH method, and may have a pore volume of 10 ml / g or less, preferably 8 ml / g or less, and more preferably 7 ml / g or less, as measured by the BJH method. The hydrophobic aerogel of silylated silica may have a peak pore radius of 5 nm or more, preferably 10 nm or more, and more preferably 12 nm or more, as measured by the BJH method, and may have a peak pore radius of 50 nm or less, preferably 40 nm or less, and more preferably 30 nm or less, as measured by the BJH method.
[0279] The "pore volume determined by the BJH method" refers to the pore volume obtained by analyzing the adsorption isotherm on the nitrogen adsorption side obtained in the same manner as explained in the "specific surface area determined by the BET method" above by the BJH method (Barrett, EP; Joyner, LG; Halenda, PP, J. Am. Chem. Soc. 73, 373 (1951)) for pores having a pore radius of 1 nm to 100 nm. The "peak pore radius determined by the BJT method" refers to the pore radius value giving a peak in a pore distribution curve (volume distribution curve) plotted by taking the logarithm of the pore radius obtained by analyzing the adsorption isotherm on the nitrogen adsorption side obtained in the same manner as above by the BJH method on the vertical axis and taking the pore radius on the horizontal axis.
[0280] The hydrophobic aerogel of silylated silica may have an average particle size of 0.5 μm or more, preferably 1 μm or more, and more preferably 2 μm or more, and may have an average particle size obtained by an image analysis method of 30 μm or less, preferably 20 μm or less, and more preferably 15 μm or less.
[0281] The "average particle size" herein can be measured by an image analysis method. Specifically, the value of the "average particle size" is the arithmetic mean of the equivalent circular diameter, which can be obtained by image analysis of a scanning electron microscope (SEM) image of, for example, not less than 2,000 aerogel particles observed at 1,000 magnifications by secondary electron detection using a scanning electron microscope (SEM). The "equivalent circular diameter" of each aerogel particle is the diameter of a circle having an area equal to the area (projected area) of the aerogel particle in the image.
[0282] Preferably, the hydrophobic aerogel of silylated silica may have the following oil absorption capacity, measurable at the wet point as explained above: 2 ml / g or more, preferably 3 ml / g or more, more preferably 4 ml / g or more, and most preferably 5 ml / g or more, and may have the following oil absorption capacity, measured at the wet point: 12 ml / g or less, preferably 10 ml / g or less, more preferably 8 ml / g or less, and most preferably 7 ml / g or less.
[0283] (d) The filler comprises (d-1) at least one hydrophobic inorganic filler. The term "hydrophobic" means that the inorganic filler can be dispersed individually in oil in such a manner that aggregates are not formed.
[0284] It is preferred that (d-1) the hydrophobic inorganic filler is selected from hydrophobically modified metal oxides, and more preferably from hydrophobic silica. The term "hydrophobically modified" means that at least the surface of the metal oxide has been treated to have hydrophobicity. In particular, silylated silica is most preferred.
[0285] The amount of (d-1) the hydrophobic inorganic filler in the composition according to the present invention may be 0.1 wt % or more, preferably 0.2 wt % or more, and more preferably 0.3 wt % or more, relative to the total weight of the composition.
[0286] The amount of (d-1) hydrophobic inorganic filler in the composition according to the present invention is less than 2 wt % relative to the total weight of the composition, and may be 1.5 wt % or less, and preferably 1 wt % or less.
[0287] The amount of the (d-1) hydrophobic inorganic filler may be 0.1 wt% to less than 2 wt%, preferably 0.2 wt% to 1.5 wt%, and more preferably 0.3 wt% to 1 wt%, relative to the total weight of the composition according to the present invention.
[0288] (d) The filler may include (d-2) at least one hydrophobic organic filler. The term "hydrophobic" means that the organic filler can be dispersed individually in oil in such a manner that aggregates are not formed.
[0289] It may be preferred that (d-2) the hydrophobic organic filler is selected from hydrophobically modified starch, more preferably esterified starch. The term "hydrophobically modified" means that at least the surface of the starch has been treated to have hydrophobicity.
[0290] The esterified starch preferably used in the present invention can be chosen from phosphorylated starch, starch acetate, oxidized starch acetate, starch laurate, sodium starch phosphate, alkyl- or alkenyl-succinate starch, for example calcium starch octenylsuccinate, sodium starch octenylsuccinate; aluminum starch octenylsuccinate, which is a starch esterified with octenylsuccinic anhydride and its salts, for example, sold under the name "Dry Flo Plus" by AKZO NOVEL; carboxymethyl-esterified potato starch sold under the name "Supramyl P 60" by Amylum; hydroxypropyl-esterified corn starch sold under the name "Merigel EF6" by Amylum; corn starch esterified with dodecenylsuccinic anhydride (INCI name: modified corn starch); and potato starch esterified with halomethylaminodipropionic acid (INCI name: modified potato starch).
[0291] The amount of (d-2) the hydrophobic organic filler in the composition according to the present invention may be 1 wt % or more, preferably 5 wt % or more, and more preferably 10 wt % or more, relative to the total weight of the composition.
[0292] The amount of (d-2) the hydrophobic organic filler in the composition according to the present invention may be 20 wt% or less, preferably 19 wt% or less, and more preferably 18 wt% or less, relative to the total weight of the composition.
[0293] The amount of (d-2) hydrophobic organic filler in the composition according to the invention may be 1 to 20 wt %, preferably 5 to 19 wt %, and more preferably 10 to 18 wt %, relative to the total weight of the composition.
[0294] (d) The filler may include (d-3) at least one hydrophilic filler, preferably at least one hydrophilic inorganic filler. The term "hydrophilic" means that the filler can be dispersed in water alone in such a manner that aggregates are not formed.
[0295] It is preferred that the (d-3) hydrophilic filler is selected from metal oxides, and more preferably selected from silicon dioxide, titanium oxide, zinc oxide and mixtures thereof. In particular, silicon dioxide is most preferred.
[0296] The amount of (d-3) the hydrophilic filler in the composition according to the present invention may be 1 wt % or more, preferably 5 wt % or more, and more preferably 10 wt % or more, relative to the total weight of the composition.
[0297] The amount of (d-3) hydrophilic filler in the composition according to the present invention may be 20 wt% or less, preferably 19 wt% or less, and more preferably 18 wt% or less, relative to the total weight of the composition.
[0298] The amount of (d-3) hydrophilic filler in the composition according to the invention may range from 1% to 20% by weight, preferably from 5% to 19% by weight and more preferably from 10% to 18% by weight relative to the total weight of the composition.
[0299] The amount of (d) filler in the composition according to the present invention may be 10 wt% or more, preferably 12 wt% or more, and more preferably 14 wt% or more, relative to the total weight of the composition.
[0300] The amount of (d) filler in the composition according to the invention is less than 21 wt % and may be 20 wt % or less, preferably 19 wt % or less and more preferably 18 wt % or less, relative to the total weight of the composition.
[0301] The amount of (d) filler in the composition according to the invention may range from 10% to 20% by weight, preferably from 12% to 19% by weight and more preferably from 14% to 18% by weight relative to the total weight of the composition.
[0302] (lipophilic gelling agent)
[0303] The composition according to the invention comprises (e) at least one lipophilic gelling agent chosen from organically modified clays. If two or more (e) lipophilic gelling agents are used, they may be identical or different.
[0304] The term "lipophilic gelling agent" means an agent in particulate or non-particulate form capable of gelling the oil in the composition according to the invention.
[0305] The term "particulate" lipophilic gelling agent means a lipophilic gelling agent in the form of particles or crystals (granules or crystals).
[0306] The composition according to the invention comprises at least one lipophilic gelling agent, which is preferably in the form of particles.
[0307] According to the present invention, (e) the lipophilic gelling agent is selected from organomodified clays.
[0308] Clays are understood to mean materials based on hydrated silicates and / or aluminosilicates having a layered structure.
[0309] The clays may be natural or synthetic and are rendered lipophilic by treatment with alkylammonium salts, such as C10 to C22 ammonium chlorides, especially stearalkonium chloride or distearyldimethylammonium chloride.
[0310] They may be chosen from bentonites, in particular bentonites, hectorites and montmorillonites, beidellites, saponites, nontronites, sepiolites, biotites, attapulgiites, vermiculites and zeolites.
[0311] The organomodified clay may be a clay treated with a compound chosen in particular from quaternary and tertiary amines. Mention may be made of organomodified bentonites, such as the product sold under the name Bentone 34 by the company Rheox, and organomodified hectorites, such as the products sold under the names Bentone 27 and Bentone 38 by the company Rheox. Mention may be made in particular of modified clays, such as modified magnesium silicates (Bentone gel VS38 from Rheox), modified hectorites, such as hectorites modified with ammonium chlorides of C10 to C22 fatty acids, such as hectorites modified with distearyldimethylammonium chloride, such as the product sold under the name Bentone 38VCG by the company Elementis, or the product sold under the name Bentone 38CE by the company Rheox, or the product sold under the name Bentone Gel V55V by the company Elementis.
[0312] Preferably, (e) the lipophilic gelling agent is selected from the group consisting of organically modified bentonite, organically modified hectorite and mixtures thereof.
[0313] More preferably, the (e) lipophilic gelling agent is disteardimonium hectorite.
[0314] The amount of (e) lipophilic gelling agent in the composition according to the invention is greater than 2.5 wt % and may be 3 wt % or more, preferably 4 wt % or more and more preferably 5 wt % or more relative to the total weight of the composition.
[0315] The amount of (e) lipophilic gelling agent in the composition according to the invention is less than 10 wt % and may be 9.5 wt % or less, preferably 9 wt % or less and more preferably 8.5 wt % or less, relative to the total weight of the composition.
[0316] Relative to the total weight of the composition according to the present invention, the amount of (e) lipophilic gelling agent in the composition is greater than 2.5% by weight and less than 10% by weight, and can be from 3% by weight to 9.5% by weight, preferably from 4% by weight to 9% by weight, and more preferably from 5% by weight to 8.5% by weight.
[0317] (Total quantity required)
[0318] The total amount of (d) filler and (e) lipophilic gelling agent in the composition according to the present invention is greater than 18.5% by weight, relative to the total weight of the composition, and may be 19% by weight or more, preferably 20% by weight or more, and more preferably 21% by weight or more.
[0319] The total amount of (d) filler and (e) lipophilic gelling agent in the composition according to the invention may be 35 wt% or less, preferably 30 wt% or less and more preferably 25 wt% or less relative to the total weight of the composition.
[0320] The total amount of (d) filler and (e) lipophilic gelling agent in the composition according to the invention may range from 19% to 35% by weight, preferably from 20% to 30% by weight and more preferably from 21% to 25% by weight relative to the total weight of the composition.
[0321] (Optional Ingredients)
[0322] The composition according to the invention may further comprise at least one optional ingredient commonly used in the cosmetic field, selected, for example, from film-forming polymers, solvents, dyes, pigments, UV filters, antioxidants, preservatives, pH regulators, cosmetic active agents (e.g. vitamins), moisturizers, emollients or collagen protectants, and mixtures thereof.
[0323] The composition according to the invention may include one or more cosmetically acceptable organic solvents, which may be alcohols, in particular monohydric alcohols, such as ethanol, isopropanol, benzyl alcohol and phenylethyl alcohol; dihydric alcohols, such as ethylene glycol, caprylyl glycol, propylene glycol and butylene glycol; other polyols, such as glycerol, sugars and sugar alcohols; and ethers, such as ethylene glycol monomethyl ether, ethylene glycol monoethyl ether and ethylene glycol monobutyl ether, propylene glycol monomethyl ether, propylene glycol monoethyl ether and propylene glycol monobutyl ether, and butylene glycol monomethyl ether, butylene glycol monoethyl ether and butylene glycol monobutyl ether.
[0324] The organic solvent may be present in a concentration of 0.01% to 30% by weight, preferably 0.1% to 20% by weight, and more preferably 1% to 15% by weight relative to the total weight of the composition.
[0325] It is a routine matter for a person skilled in the art to adjust the nature and amount of the abovementioned optional additives that may be present in the compositions according to the invention such that the desired cosmetic properties are not thereby affected.
[0326] (Cosmetic products)
[0327] The composition according to the invention may be a cosmetic composition, preferably a cosmetic composition for keratin substances, more preferably a cosmetic composition for keratin fibers, and even more preferably a cosmetic composition for eyebrows.
[0328] The composition according to the present invention may be a color makeup cosmetic composition (particularly an eye makeup cosmetic composition), and more preferably an eyebrow makeup composition.
[0329] The composition according to the invention can be used for the cosmetic treatment, preferably the make-up treatment, of keratin substances, preferably keratin fibers, and more preferably eyebrows.
[0330] The composition according to the invention may be in the form of an anhydrous liquid.
[0331] The term "anhydrous" means here that the composition according to the invention may contain only very small amounts of water and preferably contains no water. Thus, the amount of water in the composition according to the invention may be 3% by weight or less, preferably 1% by weight or less, and more preferably 0.1% by weight or less, relative to the total weight of the composition according to the invention. It is particularly preferred that the composition according to the invention does not contain water as a deliberately added distinct ingredient. On the other hand, small amounts or traces of water may be present in the ingredients themselves to be contained in the composition according to the invention.
[0332] The term "liquid" here means that the composition is flowable at room temperature (25° C.) at atmospheric pressure (760 mmHg) and has a measurable viscosity. Thus, a composition in powder form does not correspond to a composition according to the invention.
[0333] [preparation]
[0334] The composition according to the present invention can be prepared by mixing the essential ingredients and optional ingredients described above.
[0335] For example, the composition according to the present invention can be prepared by a method comprising the following steps:
[0336] Components (a) to (e) of the composition and optional other components are mixed with or without heating, preferably at 70° C. or higher. Preferably, they are further mixed with any of the optional components described above.
[0337] [Methods and Uses]
[0338] The composition according to the invention can be used to coat keratin substances, preferably keratin fibers, and more preferably the eyebrows.
[0339] For example, the composition according to the invention can be used by a method for coating keratin fibers comprising the following steps:
[0340] applying a composition according to the invention to keratin fibers so as to form at least one coating on the keratin fibers, and
[0341] The coating is dried.
[0342] Therefore, the present invention also relates to a cosmetic method for keratin materials, preferably keratin fibers, and more preferably eyebrows, comprising the following steps:
[0343] The composition according to the invention is applied to keratin substances.
[0344] The cosmetic method according to the invention can be used, for example, to make up keratin substances, preferably keratin fibers, and more preferably eyebrows.
[0345] The present invention may also relate to
[0346] (d) at least one filler comprising (d-1) at least one hydrophobic inorganic filler, and
[0347] (e) at least one lipophilic gelling agent selected from organically modified clays,
[0348] Use in an anhydrous liquid composition for keratinous materials, preferably keratinous fibers, and more preferably eyebrows, the anhydrous liquid composition comprising:
[0349] (a) at least one silicone resin;
[0350] (b) at least one silicone gel; and
[0351] (c) at least one volatile hydrocarbon oil,
[0352] in
[0353] The amount of (d) filler and (e) lipophilic gelling agent in the composition is greater than 18.5% by weight, relative to the total weight of the composition.
[0354] The amount of (e) lipophilic gelling agent in the composition is greater than 2.5 wt % and less than 10 wt %, relative to the total weight of the composition.
[0355] The amount of (d) filler in the composition is less than 21% by weight relative to the total weight of the composition, and
[0356] The amount of the hydrophobic inorganic filler (d-1) in the composition is less than 2% by weight relative to the total weight of the composition.
[0357] In order to stabilize the composition and provide excellent cosmetic effects, such as a matte finish, good wear resistance, and a comfortable texture such as reduced makeup stickiness and smooth spreading during application. Example
[0358] The present invention will be described in more detail by way of examples. However, these examples should not be interpreted as limiting the scope of the present invention. The following examples are presented as non-limiting illustrations in the field of the present invention.
[0359] Example 1 and Comparative Examples 1-19
[0360] The cosmetic compositions for making up eyebrows according to Example 1 and Comparative Examples 1 to 19 shown in Tables 1 and 2 were prepared by mixing the components shown in Tables 1 and 2. The numerical values of the amounts of the components shown in Tables 1 and 2 are all based on "weight %" of the raw materials.
[0361] Symbols "a", "b", "c", "d", "d-1", and "e" in Tables 1 and 2 correspond to those in the claims.
[0362]
[0363]
[0364]
[0365]
[0366] [Evaluate]
[0367] (Smoothness)
[0368] The cosmetic composition of each of Example 1 and Comparative Examples 1 to 19 was filled into a dip-type applicator package, and evaluated in terms of smoothness during application on the arm according to the following criteria.
[0369] Good: Feels light to moderately smooth glide
[0370] Acceptable: Slightly less smooth sliding, but acceptable
[0371] Poor: Unacceptable draggy texture
[0372] The results are shown in Tables 1 and 2.
[0373] (matte finish after drying)
[0374] By applying the cosmetic composition of each of Example 1 and Comparative Examples 1-19, a film having a thickness of 100 μm was prepared on a comparison card (white and black). The film was dried at room temperature for 30 minutes. Subsequently, the matte effect on the film was evaluated by a panelist according to the following criteria.
[0375] Very good: completely matte, no shine
[0376] Good: Very slight gloss
[0377] Poor: Glossy
[0378] The results are shown in Tables 1 and 2.
[0379] (Gloss after drying)
[0380] By applying the cosmetic composition of each of Example 1 and Comparative Examples 1-19, a film having a thickness of 100 μm was prepared on a contrast card (white and black). The film was dried at room temperature for 30 minutes. Subsequently, the gloss of the film (reflected light on the card) was measured by a polarization camera. The average gloss on the white and black (back) backgrounds was used as the gloss value.
[0381] The results are shown in Tables 1 and 2.
[0382] A smaller gloss value means a better matte effect. Preferably, the gloss value is less than 6.0, and more preferably less than 1.0.
[0383] (stickiness after drying)
[0384] A film having a thickness of 100 μm was prepared on a comparison card (white and black) by applying each of the cosmetic compositions of Example 1 and Comparative Examples 1 to 19. The film was dried at room temperature for 30 minutes.
[0385] The tack of the dried films was evaluated by the panelists according to the following criteria:
[0386] Non-sticky: When you touch the surface of the film with your fingers, you will not feel any stickiness at all
[0387] Very Slightly Tacky (Acceptable): Very slightly sticky, but no noticeable feeling is felt when touching the film with a finger Slightly (Tacky): A clear sticky feeling is felt when touching the film with a finger
[0388] The results are shown in Tables 1 and 2.
[0389] (Stability at 25°C or 45°C)
[0390] The cosmetic composition of each of Example 1 and Comparative Examples 1 to 19 was filled into a 50 ml glass jar and kept at 25° C. or 45° C. for 8 weeks.
[0391] Subsequently, the presence or absence of separated oil on the top surface of each composition was checked. If separated oil was present, the phase separation rate was calculated by the following equation:
[0392] Separation rate (%) = A / B × 100
[0393] A: Height of oil separated on the top (mm),
[0394] B: Height of the total bulk composition including separated oil (mm)
[0395] The stability of each cosmetic composition was evaluated according to the following criteria:
[0396] Very good: no oil separation or very slight oil separation (not measurable)
[0397] Good: Slight oil separation with a separation rate of less than 5%
[0398] Acceptable: Oil separation with a separation rate of 5% or more and less than 6%
[0399] Poor: Great oil separation with a separation rate of 6% or more
[0400] Very bad: Completely separated
[0401] The results are shown in Tables 1 and 2.
[0402] (Sebum resistance)
[0403] Each of the cosmetic compositions of Example 1 and Comparative Examples 1-19 was filled into a dip-type applicator package with a flocking applicator, applied to a white Bio Skin sheet of Beaulax, and dried at room temperature for 30 minutes to form a dry film. Subsequently, artificial sebum* was dropped on the film and rubbed with fingers 30 times (1 time / second) at room temperature. The stain level was evaluated according to the following criteria:
[0404] Very good: Almost no smudges
[0405] Good: Very lightly soiled
[0406] Slightly dirty (acceptable)
[0407] Poor: Heavily soiled and partially or completely faded
[0408] * Composition of artificial sebum:
[0409] 28.7 wt% triisostearin, 28 wt% oleic acid, 22.9 wt% oleyl erucate, 13.7 wt% hydrogenated polyisobutene and 6.7 wt% octyldodecanol
[0410] The results are shown in Tables 1 and 2.
[0411] (Water resistance)
[0412] The cosmetic composition of each of Example 1 and Comparative Examples 1-19 was filled into a dip-type applicator package with a flocking applicator, applied to a white Bio Skin sheet of Beaulax, and dried at room temperature for 30 minutes to form a dry film. Subsequently, water was dropped on the film and rubbed with fingers 30 times (1 time / second) at room temperature. The stain level was evaluated according to the following criteria:
[0413] Very good: Almost no smudges
[0414] Good: Very lightly soiled
[0415] Poor: wrinkled or faded
[0416] The results are shown in Tables 1 and 2.
[0417] (Summarize)
[0418] As shown in Tables 1 and 2, the cosmetic composition according to Example 1 corresponding to the present invention is stable, and can provide matte and sebum / water-resistant cosmetic effects, and comfortable texture such as smoothness upon application and no stickiness after drying.
[0419] On the other hand, the cosmetic compositions according to Comparative Examples 1 to 19 that do not satisfy any of the following quantitative requirements are unstable or fail to provide a matte or sebum / water-resistant cosmetic effect, or an excellent feeling of use such as smoothness during application and no stickiness after drying:
[0420] (d) filler and (e) lipophilic gelling agent in an amount greater than 18.5% by weight,
[0421] (e) the amount of lipophilic gelling agent is greater than 2.5 wt % and less than 10 wt %,
[0422] (d) the amount of filler is less than 21% by weight, and
[0423] (d-1) The amount of the hydrophobic inorganic filler is less than 2% by weight.
[0424] Examples 2 and 3, and Comparative Example 20
[0425] The cosmetic compositions for making up eyebrows according to Examples 2 and 3 and Comparative Example 20 shown in Table 3 were prepared by mixing the components shown in Table 3. The numerical values of the amounts of the components shown in Table 3 are all based on "weight %" of the raw materials.
[0426] Symbols "a", "b", "c", "d", "d-1", and "e" in Table 3 correspond to those in the claims.
[0427] Table 3
[0428]
[0429] NA: Not Available
[0430] [Evaluate]
[0431] "Smoothness", "Gloss after drying", "Tackiness after drying", "Stability at 25°C", "Stability at 45°C", "Sebum resistance" and "Water resistance" were evaluated according to the same procedures as used for evaluating Example 1 and Comparative Examples 1-19.
[0432] The results are shown in Table 3.
[0433] As shown in Table 3, the cosmetic compositions according to Examples 2 and 3 corresponding to the present invention are stable and can provide matte and sebum / water-resistant cosmetic effects as well as comfortable textures such as smoothness upon application and no stickiness after drying.
[0434] The composition according to Example 2 and the composition according to Example 3 are similar. However, they differ in that for Example 3, the polydimethylsiloxane with a dynamic viscosity of 1,000,000 cSt is diluted with isododecane, while for Example 2, the polydimethylsiloxane with a dynamic viscosity of 1,000,000 cSt is not diluted. The production of the composition according to Example 3 is easier than the production of the composition according to Example 2 because the handling of the polydimethylsiloxane is improved in Example 3.
[0435] On the other hand, the cosmetic composition according to Comparative Example 20 not including any silicone gum could not provide sebum / water-resistant cosmetic effects or comfortable texture such as no stickiness after drying.
Claims
1. An anhydrous liquid composition for keratin substances, preferably for keratin fibers, and more preferably for eyebrows, comprising: (a) at least one silicone resin; (b) at least one silicone adhesive; (c) at least one volatile hydrocarbon oil; (d) at least one filler; and (e) at least one lipophilic gelling agent selected from organically modified clays, in (d) The filler comprises (d-1) at least one hydrophobic inorganic filler, which is preferably selected from hydrophobically modified metal oxides, and more preferably selected from hydrophobic silica, and in The total amount of (d) filler and (e) lipophilic gelling agent in the composition is greater than 18.5% by weight relative to the total weight of the composition. Relative to the total weight of the composition, the amount of (e) lipophilic gelling agent in the composition is greater than 2.5 wt % and less than 10 wt %, The amount of (d) filler in the composition is less than 21% by weight relative to the total weight of the composition, and The amount of (d-1) the hydrophobic inorganic filler in the composition is less than 2 wt % relative to the total weight of the composition.
2. The composition according to claim 1, wherein the (a) silicone resin is selected from MQ resins.
3. The composition according to claim 1 or 2, wherein the (a) silicone resin is present in an amount of 1 to 30 wt %, preferably 5 to 25 wt %, and more preferably 10 to 20 wt %, relative to the total weight of the composition.
4. The composition according to any one of claims 1 to 3, wherein the (b) silicone gum is selected from polydimethylsiloxane gum.
5. The composition according to any one of claims 1 to 4, wherein the (b) silicone gum has a dynamic viscosity at 25°C of 400,000 cSt or more, preferably 600,000 cSt or more, and more preferably 800,000 cSt or more.
6. The composition according to any one of claims 1 to 5, wherein the amount of (b) silicone gum present is 1% to 25% by weight, preferably 3% to 20% by weight, and more preferably 5% to 15% by weight, relative to the total weight of the composition.
7. The composition according to any one of claims 1 to 6, wherein the (c) volatile hydrocarbon oil is selected from isododecane, C8-9 Isoparaffins and mixtures thereof.
8. The composition according to any one of claims 1 to 7, wherein the (c) volatile hydrocarbon oil is present in an amount of 10% to 60% by weight, preferably 15% to 55% by weight, and more preferably 20% to 50% by weight relative to the total weight of the composition.
9. The composition according to any one of claims 1 to 8, wherein the (d) filler is present in an amount of 10 to 20 wt. %, preferably 12 to 19 wt. %, and more preferably 14 to 18 wt. %, relative to the total weight of the composition.
10. The composition according to any one of claims 1 to 9, wherein the (d) filler further comprises (d-2) at least one hydrophobic organic filler, which is preferably selected from hydrophobically modified starches, and more preferably selected from esterified starches.
11. The composition according to any one of claims 1 to 10, wherein the (d-1) hydrophobic inorganic filler is present in an amount of 0.1 wt % to less than 2 wt %, preferably 0.2 wt % to 1.5 wt %, and more preferably 0.3 wt % to 1 wt %, relative to the total weight of the composition.
12. The composition according to any one of claims 1 to 11, wherein the (e) lipophilic gelling agent is selected from the group consisting of organically modified bentonites, organically modified hectorites and mixtures thereof.
13. The composition according to any one of claims 1 to 12, wherein the (e) lipophilic gelling agent is present in an amount of 3% to 9.5% by weight, preferably 4% to 9% by weight, and more preferably 5% to 8.5% by weight, relative to the total weight of the composition.
14. The composition according to any one of claims 1 to 13, wherein the total amount of the filler (d) and the lipophilic gelling agent (e) present is from 19% to 35% by weight, preferably from 20% to 30% by weight, and more preferably from 21% to 25% by weight, relative to the total weight of the composition.
15. A cosmetic method for keratinous materials, preferably keratinous fibers, and more preferably eyebrows, comprising the following steps: A composition according to any one of claims 1 to 14 is applied to the keratinous material.