Monolithic complementary field effect transistor with carbon-doped release layer

By using a vertically stacked superlattice structure and a carbon-doped release layer in the CFET, the performance problems caused by high Ge concentration in the intermediate sacrificial layer are solved, and the effects of high strain and low etching rate are achieved, which improves the performance of the transistor.

CN118946971APending Publication Date: 2024-11-12APPLIED MATERIALS INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380029643.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-07
Filing Date
2023-04-03
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

In existing complementary field effect transistors (CFETs), due to the high Ge concentration in the intermediate sacrificial layer, the superlattice relaxation, strain and mobility decrease, affecting transistor performance.

Method used

Using a vertically stacked superlattice structure, wherein the first and second horizontal wraparound gate structures include a nanosheet channel layer and a doped silicon germanium release layer, the sacrificial layer containing SiGe of 0% to 50% germanium content, by The carbon-doped release layer reduces the etching rate and increases strain.

Benefits of technology

A defect-free or substantially defect-free channel layer and a low selective removal rate release layer are achieved, which improves the drive current and mobility of the transistor and improves the performance of the CFET.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118946971A_ABST
    Figure CN118946971A_ABST
Patent Text Reader

Abstract

Embodiments of the present disclosure advantageously provide semiconductor devices, CFETs, and methods of making such devices having fully strained superlattice structures with substantially defect-free channel layers and with release layers with reduced selective removal rates. In one embodiment, a CFET described herein includes a vertically stacked superlattice structure on a substrate, the vertically stacked superlattice structure comprising: a first hGAA structure on the substrate, a second hGAA structure on the substrate, and a third hGAA structure on the substrate, a sacrificial layer on a top surface of the first hGAA structure, the sacrificial layer comprising silicon germanium (SiGe) having a germanium content in a range of greater than 0% to 50% by atoms; and a second hGAA structure, the second hGAA structure being on a top surface of the sacrificial layer. Each of the first hGAA and the second hGAA includes alternating layers of a nanosheet channel layer comprising silicon (Si) and a nanosheet release layer comprising doped silicon germanium (SiGe).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present disclosure are in the field of electronic device manufacturing, and more particularly, relate to transistors. More specifically, embodiments of the present disclosure relate to complementary field effect transistors (CFETs).

[0002] background

[0003] Transistors are key components of most integrated circuits. Since the drive current and speed of a transistor are proportional to the gate width of the transistor, faster transistors generally require larger gate widths. Therefore, there is a trade-off between transistor size and speed, and "fin" field effect transistors (finFETs) have been developed to address the conflicting goals of transistors having maximum drive current and minimum size. FinFETs are characterized by a fin-shaped channel region that significantly increases the size of the transistor without significantly increasing the transistor footprint and is now used in many integrated circuits. However, finFETs have their own disadvantages.

[0004] As the feature size of transistor devices continues to shrink to achieve greater circuit density and higher performance, there is a need to improve transistor device structures to improve electrostatic coupling and reduce negative effects (such as parasitic capacitance and off-state leakage). Examples of transistor device structures include planar structures, fin field effect transistor (FinFET) structures, and surround gate (GAA) structures. The GAA device structure includes several lattice matching trenches suspended in a stacked configuration and connected by source / drain regions. The GAA structure provides good electrostatic control and can be widely used in complementary metal oxide semiconductor (CMOS) wafer manufacturing.

[0005] An example of gate-all-around (GAA) technology is the complementary field effect transistor (CFET), in which nFET and pFET nanowires / nanosheets are stacked vertically on top of each other. CFET transistors increase on-chip device density and reduce area consumption compared to GAA transistors. When nFETs and pFETs are stacked in a monolithic manner, n and p superlattices are deposited sequentially, with the middle sacrificial layer being selectively removed during processing and replaced with an intermediate dielectric isolation. The intermediate dielectric isolation layer is used to electrically isolate the lower-level GAA from the upper-level GAA.

[0006] Each n or p superlattice of a CFET includes alternating layers of channel layers and release layers. The release layers typically include silicon germanium (SiGe) with a low concentration of germanium (Ge). For etching contrast between the middle sacrificial layer and the channel layer and the release layer, the middle sacrificial layer includes SiGe with a high concentration of Ge. However, because the Ge concentration in the middle sacrificial layer is so high, the superlattice relaxes and the strain and mobility are reduced, resulting in poor transistor performance due to reduced drive current.

[0007] Therefore, there is a need for semiconductor devices, particularly CFETs, and methods of fabricating such devices having a fully strained superlattice structure with a defect-free or substantially defect-free channel layer and a release layer with a reduced selective removal rate.

[0008] Overview

[0009] One or more embodiments of the present disclosure relate to semiconductor devices. In one or more embodiments, a semiconductor device includes a vertically stacked superlattice structure on a substrate, the vertically stacked superlattice structure comprising: a first horizontal wraparound gate (hGAA) structure on the substrate; a sacrificial layer on a top surface of the first hGAA structure, the sacrificial layer comprising silicon germanium (SiGe) having a germanium content in a range of greater than 0% to 50% on an atomic basis; and a second horizontal wraparound gate (hGAA) structure on a top surface of the sacrificial layer. Each of the first hGAA and the second hGAA comprises alternating layers of nanosheet channel layers and nanosheet release layers. The nanosheet channel layers comprise silicon (Si), and the nanosheet release layers comprise doped silicon germanium (SiGe).

[0010] Additional embodiments of the present disclosure relate to methods of forming semiconductor devices. In one or more embodiments, a method of forming a semiconductor device includes the following steps: forming a vertically stacked superlattice structure on a substrate by the following steps: forming a first horizontal wraparound gate (hGAA) structure on the substrate; forming a sacrificial layer on a top surface of the first hGAA structure, the sacrificial layer comprising silicon germanium (SiGe) having a germanium content in a range of greater than 0% to 50% by atom; and forming a second horizontal wraparound gate (hGAA) structure on a top surface of the sacrificial layer. Each of the first hGAA and the second hGAA includes alternating layers of nanosheet channel layers and nanosheet release layers. The nanosheet channel layers include silicon (Si), and the nanosheet release layers include doped silicon germanium (SiGe).

[0011] BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Features of the present disclosure have been briefly summarized above and discussed in more detail below, and may be understood by reference to the embodiments of the present disclosure illustrated in the accompanying drawings. However, it should be noted that the accompanying drawings illustrate only typical embodiments of the present disclosure and therefore should not be considered limiting of its scope, as the present disclosure may allow other equally effective embodiments. Embodiments described in the present disclosure are illustrated in the accompanying drawings by way of example and not by way of limitation, and in the accompanying drawings, like reference numerals represent similar elements.

[0013] Figure 1 A process flow chart illustrating a method of forming a semiconductor device according to one or more embodiments;

[0014] Figure 2 A semiconductor structure according to one or more embodiments is shown;

[0015] Figure 3 depicts a semiconductor structure according to one or more embodiments; and

[0016] Figure 4 A vertically stacked superlattice structure is depicted in accordance with one or more embodiments.

[0017] Specific description

[0018] Before describing several exemplary embodiments of the present disclosure, it should be understood that the present disclosure is not limited to the details of construction or processing steps set forth in the following description. The present disclosure is capable of other embodiments and can be practiced or carried out in various ways.

[0019] As used herein, the term "about" means approximately or close to, and in the context of a listed numerical value or range refers to a variation of ±15% or less of the numerical value. For example, values ​​that differ by ±14%, ±10%, ±5%, ±2%, or ±1% will satisfy the definition of about.

[0020] As used in this specification and the appended claims, the term "substrate" or "wafer" refers to a surface or portion of a surface on which a process acts. Those skilled in the art will also understand that, unless the context clearly indicates otherwise, reference to a substrate may refer to only a portion of a substrate. In addition, reference to a deposition on a substrate may refer to both a bare substrate and a substrate having one or more films or features deposited or formed thereon.

[0021] As used herein, "substrate" refers to any substrate or a material surface formed on a substrate to which film processing is applied during a manufacturing process. For example, substrate surfaces on which processing is applied include materials such as silicon, silicon oxide, strained silicon, silicon on insulator (SOI), carbon-doped silicon oxide, amorphous silicon, doped silicon, germanium, gallium arsenide, and any other materials (such as metals, metal nitrides, metal alloys and other conductive materials), depending on the application. Substrates include, but are not limited to, semiconductor wafers. The substrate may be exposed to a pretreatment process to polish, etch, reduce, oxidize, hydroxylate, anneal, and / or bake the substrate surface. In addition to direct film processing directly on the substrate surface itself, in the present disclosure, any film processing step disclosed may also be applied on an underlayer formed on the substrate, as disclosed in more detail below, and the term "substrate surface" is intended to include such an underlayer as indicated by the context. Thus, for example, where a film / layer or a portion of a film / layer has already been deposited on a substrate surface, the exposed surface of the newly deposited film / layer becomes the substrate surface.

[0022] The term "on" indicates that there is direct contact between devices. The term "directly on" indicates that there is direct contact between devices without intervening elements.

[0023] As used in this specification and the appended claims, the terms "precursor", "reactant", "reactant gas" and the like are used interchangeably and refer to any gaseous substance that can react with the surface of a substrate.

[0024] "Epitaxial growth" is a process by which a deposited film is forced into a high degree of crystalline alignment with a substrate. Epitaxial growth is broadly defined as the condensation of a gaseous precursor to form a film on a substrate. Liquid precursors can also be used. Vapor precursors can be obtained by chemical vapor deposition (CVD) and laser ablation. Several epitaxy techniques are available, such as molecular beam epitaxy (MBE), epitaxial CVD or atomic layer epitaxy (ALE).

[0025] A transistor is a circuit component or element that is often formed on a semiconductor device. Depending on the circuit design, a transistor is formed on a semiconductor device in addition to capacitors, inductors, resistors, diodes, wires, or other elements. In general, a transistor includes a gate formed between a source region and a drain region. In one or more embodiments, the source region and the drain region include doped regions of the substrate and exhibit a doping profile suitable for a particular application. The gate is located above the channel region and includes a gate dielectric interposed between a gate electrode and the channel region in the substrate.

[0026] As used herein, the term "field effect transistor" or "FET" refers to a transistor that uses an electric field to control the electrical behavior of the device. A field effect transistor is a voltage-controlled device that changes its current carrying capacity by applying an electric field. Field effect transistors typically exhibit very high input impedance at low temperatures. The conductivity between the drain terminal and the source terminal is controlled by the electric field in the device, which is generated by the voltage difference between the body of the device and the gate. The three terminals of a FET are the source (S), through which carriers enter the channel; the drain (D), through which carriers leave the channel; and the gate (G), which modulates the channel conductivity. Typically, the current entering the channel at the source (S) is designated as IS, and the current entering the channel at the drain (D) is designated as ID. The drain-to-source voltage is designated as VDS. By applying a voltage to the gate (G), the current (ie, ID) entering the channel at the drain can be controlled.

[0027] A metal oxide semiconductor field effect transistor (MOSFET) is a type of field effect transistor (FET) and is used in integrated circuits and high-speed switching applications. MOSFETs have an insulated gate, the voltage of which determines the conductivity of the device. This ability to change conductivity with applied voltage is used to amplify or switch electronic signals. MOSFETs are based on the modulation of charge concentration by the metal oxide semiconductor (MOS) capacitance between the body electrode and the gate electrode, which is located above the body and insulated from all other device regions by the gate dielectric layer. Compared to a MOS capacitor, a MOSFET includes two additional terminals (source and drain), each connected to a separate highly doped region separated by the body region. These regions can be either p-type or n-type, but they are all the same type as the body region, as well as the opposite type to the body region. The source and drain (unlike the body) are highly doped, as indicated by the "+" sign after the doping type.

[0028] If the MOSFET is an n-channel, or nMOS FET, the source and drain are the n+ regions, and the bulk is the p-type substrate region. If the MOSFET is a p-channel, or pMOS FET, the source and drain are the p+ regions, and the bulk is the n-type substrate region. The source is so named because it is the source of charge carriers (electrons for n-type channels and holes for p-type channels) that flow through the channel; similarly, the drain is where the charge carriers leave the channel.

[0029] The nMOS FET consists of an n-type source and drain and a p-type substrate. When a voltage is applied to the gate, holes in the bulk (p-type substrate) are driven away from the gate. This allows an n-type channel to form between the source and drain, and current is carried by electrons from the source through the induced n-type channel to the drain. Logic gates and other digital devices implemented using NMOS are said to have NMOS logic. NMOS has three operating modes: cutoff, triode, and saturation. Circuits with NMOS logic gates consume static power when the circuit is idle because DC current flows through the logic gate when the output is low.

[0030] The pMOS FET consists of a p-type source and drain and an n-type substrate. When a positive voltage is applied between the source and gate (negative voltage between the gate and source), a p-type channel of opposite polarity is formed between the source and drain. The current is carried by holes from the source through the induced p-type channel to the drain. A high voltage on the gate will make the PMOS non-conducting, while a low voltage on the gate will make it conduct. Logic gates and other digital devices implemented using PMOS are said to have PMOS logic. PMOS technology is low cost and has good noise immunity.

[0031] In NMOS, the carriers are electrons, while in PMOS, the carriers are holes. When a high voltage is applied to the gate, NMOS will conduct, while PMOS will not conduct. Also, when a low voltage is applied in the gate, NMOS will not conduct, while PMOS will conduct. NMOS is considered faster than PMOS because the carriers in NMOS (which are electrons) move twice as fast as holes (which are carriers in PMOS). But PMOS devices are more resistant to noise than NMOS devices. Also, NMOS ICs will be smaller than PMOS ICs (with the same functionality) because NMOS can provide half the impedance provided by PMOS (with the same geometry and operating conditions).

[0032] As used herein, the term "Fin Field Effect Transistor (FinFET)" refers to a MOSFET transistor built on a substrate where the gate is located on two, three, or four sides of the channel or surrounds the channel to form a dual gate structure. FinFET devices have been given the generic name FinFET because the source / drain regions form a "fin" on the substrate. FinFET devices have fast switching times and high current density.

[0033] As used herein, the term "gate all-around (GAA)" is used to refer to an electronic device, such as a transistor, in which a gate material surrounds a channel region on all sides. The channel region of a GAA transistor may include nanowires or nanoslabs or nanosheets, strip channels, or other suitable channel configurations known to those skilled in the art. In one or more embodiments, the channel region of a GAA device has multiple vertically spaced horizontal nanowires or horizontal strips, making the GAA transistor a stacked horizontal gate-all-around (hGAA) transistor.

[0034] As used herein, the term "complementary field effect transistor (CFET)" refers to a transistor including an NMOS FET device and a PMOS FET device stacked on each other. Each of the NMOS FET device and the PMOS FET device forming the CFET is a GAA transistor or an hGAA transistor.

[0035] As used herein, the term "nanowire" refers to a nanostructure with a diameter of nanometers (10 -9 Nanowires are defined as having a length-to-width ratio greater than 1000. Alternatively, nanowires can be defined as structures with a thickness or diameter limited to tens of nanometers or less and an unlimited length. Nanowires are used in transistors and some laser applications, and in one or more embodiments, are made of semiconductor materials, metal materials, insulating materials, superconducting materials, or molecular materials. In one or more embodiments, nanowires are used in transistors of logic CPUs, GPUs, MPUs, and volatile (such as DRAM) and non-volatile (such as NAND) devices. As used herein, the term "nanosheet" refers to a two-dimensional nanostructure having a thickness ranging from about 0.1 nm to about 1000 nm, or from 0.5 nm to 500 nm, or from 0.5 nm to 100 nm, or from 1 nm to 500 nm, or from 1 nm to 100 nm, or from 1 nm to 50 nm.

[0036] Without being bound by theory, it is generally believed that relaxation in a vertically stacked superlattice structure including one or more hGAAs leads to defects in the nanosheet channel layer within the structure. Embodiments of the present disclosure advantageously provide semiconductor devices including a fully strained vertically stacked superlattice structure having a defect-free or substantially defect-free nanosheet channel layer. In some embodiments, the presence of defects in the nanosheet channel layer is determined by a reciprocal space mapping (RSM) method. Without being bound by theory, the RSM method is an x-ray diffraction method that collects diffraction data of a vertically stacked superlattice structure in which defects can be observed. As used herein, the term "substantially free" refers to a nanosheet channel layer that is substantially defect-free as determined by a reciprocal space mapping (RSM) method.

[0037] In order to remove the sacrificial layer within the CFET superlattice without etching the nanosheet release layer, a three-color selectivity of >10:1 is required. In a typical patterned wafer, the selectivity of SiGe to Si is very high, meeting the >10:1 requirement. However, the selectivity for SiGe with a high germanium content (i.e., greater than 30% by atom) is much lower than that for SiGe with a low germanium content (i.e., 15-20% by atom) and does not meet the >10:1 requirement. Without intending to be limited to any particular theory of operation, it is believed that doping the SiGe release layer with a dopant (such as carbon (C)) slows the etching rate of SiGe, thereby increasing the differential etching rate in the case of undoped SiGe of the sacrificial layer. Therefore, one or more embodiments of the present disclosure advantageously provide differentiation during etching of the SiGe layers (i.e., the sacrificial layer and the nanosheet release layer) relative to each other and relative to the channel layer.

[0038] In one or more embodiments, the release layer is advantageously doped with carbon (C) to improve strain and mobility by reducing relaxation. At the same time, doping the release layer with carbon (C) reduces the etch rate of the release layer compared to the etch rate of the sacrificial layer. In other words, doping the release layer with carbon (C) advantageously increases the etch rate of the intermediate sacrificial layer to facilitate easier removal without damaging the release layer or the channel layer.

[0039] The embodiments of the present disclosure are described by way of the accompanying drawings, which illustrate devices (such as transistors) and processes for forming transistors according to one or more embodiments of the present disclosure. The processes shown are merely illustrative of possible uses of the disclosed processes, and those skilled in the art will recognize that the disclosed processes are not limited to the described applications.

[0040] Figure 1A process flow chart of a method 100 for manufacturing a monolithic CFET device according to one or more embodiments of the present disclosure is shown. More specifically, Figure 1 A process flow diagram of a method 100 of manufacturing an engineered substrate of an epitaxially grown superlattice composed of alternating silicon (Si) layers and silicon germanium (SiGe) layers for producing a monolithic CFET device is shown. In one or more embodiments, the superlattice is strained and free of lattice defects and allows differential selective removal of two or more different compositions of SiGe. Figure 1 , method 100 begins at operation 102, forming a vertically stacked superlattice structure on a substrate. The vertically stacked superlattice structure is formed on the substrate by the following steps: At operation 104, a first horizontal gate-around (hGAA) structure is formed on the substrate. At operation 106, a sacrificial layer is formed on a top surface of the first hGAA structure. At operation 108, a second horizontal gate-around (hGAA) structure is formed on a top surface of the sacrificial layer. At operation 110, method 100 optionally includes the following steps: selectively removing the sacrificial layer so that an intermediate isolation layer can be formed during subsequent processing.

[0041] Figure 2-4 A cross-sectional view of a vertically stacked superlattice structure of a CFET device 200 is shown. Figure 2-4 The CFET device 200 shown may be Figure 1 A method 100 of manufacturing is shown.

[0042] In one or more embodiments, the CFET device 200 includes a substrate 210 having a top surface 212. The substrate 210 can be any suitable substrate material known to those skilled in the art. In one or more embodiments, the substrate 210 includes a semiconductor material such as silicon (Si), carbon (C), germanium (Ge), silicon germanium (SiGe), gallium arsenide (GaAs), indium phosphate (InP), indium gallium arsenic (InGaAs), indium aluminum arsenic (InAlAs), germanium (Ge), silicon germanium (SiGe), other semiconductor materials, or any combination thereof. In one or more embodiments, the substrate 210 includes one or more of the following: silicon (Si), germanium (Ge), gallium (Ga), arsenic (As), indium (In), phosphorus (P), or selenium (Se). Although several examples of materials that can form the substrate 210 are described herein, any material that can serve as a base on which passive and active electronic devices (such as transistors, memories, capacitors, inductors, resistors, switches, integrated circuits, amplifiers, optoelectronic devices, or any other electronic devices) can be constructed falls within the spirit and scope of the present disclosure.

[0043] In one or more embodiments, substrate 210 is a p-type or n-type substrate. As used herein, the term "n-type" refers to a semiconductor produced by doping an intrinsic semiconductor with an electron donor element during manufacturing. The term n-type comes from the negative charge of the electron. In an n-type semiconductor, electrons are the majority carriers, while holes are the minority carriers. As used herein, the term "p-type" refers to the positive charge of the well (or hole). In contrast to an n-type semiconductor, the hole concentration of a p-type semiconductor is greater than the electron concentration. In a p-type semiconductor, holes are the majority carriers, while electrons are the minority carriers.

[0044] In one or more embodiments, the vertically stacked superlattice structure 260 includes one or more horizontal wraparound gate (hGAA) structures on the substrate 210. In some embodiments, the vertically stacked superlattice structure 260 includes a first or lower horizontal wraparound gate (hGAA) structure 215 on the substrate 210. In some embodiments, at operation 104 of method 100, the vertically stacked superlattice structure 260 includes a first or lower horizontal wraparound gate (hGAA) structure 215 on the top surface 212 of the substrate 210. In some embodiments, the vertically stacked superlattice structure 260 includes a second or upper horizontal wraparound gate (hGAA) structure 255. Without intending to be limited to any particular theory of operation, the first or lower hGAA 215 and the second or upper hGAA 255 may independently include the same structure having the same layers. Figure 3 and 4 In the illustrated embodiment, the vertically stacked superlattice structure 260 includes a first hGAA structure 215 on the top surface 212 of the substrate 210, a sacrificial layer 240 on the top surface 225 of the first hGAA structure 215 (formed in operation 106 of method 100), and a second hGAA structure 255 on the top surface 245 of the sacrificial layer 240 (formed in operation 108 of method 100).

[0045] Reference again Figure 2-4 , in some embodiments, each of the first hGAA 215 and the second hGAA 255 includes alternating layers of nanosheet channel layers 230 and nanosheet release layers 220. In some embodiments, the plurality of nanosheet release layers 220 and the plurality of nanosheet channel layers 230 may include any number of lattice-matched material pairs suitable for forming a vertically stacked superlattice structure 260. In some embodiments, each of the first hGAA 215 and the second hGAA 255 has alternating layers of nanosheet channel layers 230 and nanosheet release layers 220 in the range of 1 to 5 pairs.

[0046] The nanosheet release layer 220 may have any suitable thickness. In one or more embodiments, each nanosheet release layer 220 has a thickness in a range from 5 nm to 15 nm. The nanosheet channel layer 230 may have any suitable thickness. In one or more embodiments, each nanosheet channel layer 230 has a thickness in a range from 5 nm to 15 nm.

[0047] In some embodiments, each nanosheet channel layer 230 independently includes silicon (Si). In some embodiments, each nanosheet release layer 220 independently includes silicon germanium (SiGe) doped with a dopant. In one or more embodiments, the nanosheet release layer 220 includes silicon germanium (SiGe) having a germanium content greater than about 0% to 30% by atom. In a specific embodiment, the nanosheet release layer 220 includes silicon germanium (SiGe) having a germanium content in the range of about 10% to 25% by atom.

[0048] The silicon germanium (SiGe) of the nanosheet release layer 220 may be doped with any suitable dopant including an element having an atomic weight less than that of silicon (Si). In some embodiments, the silicon germanium (SiGe) of the nanosheet release layer 220 is doped with a dopant including one or more of carbon (C) and boron (B). In one or more specific embodiments, the silicon germanium (SiGe) of the nanosheet release layer 220 is doped with carbon (C).

[0049] In one or more embodiments, the dopant of the nanosheet release layer 220 can have any suitable concentration. In some embodiments, the dopant has a concentration in the range of from greater than 0% to less than or equal to 2% dopant by atom. In some embodiments, the dopant has a concentration less than or equal to 2% dopant by atom, including dopant in the range of from 0.1% to 1.99% by atom. In some embodiments, the concentration of the dopant is in the range of 0.1% to 1.99%, including dopants in the range of 0.1% to 1.95%, in the range of 0.1% to 1.9%, in the range of 0.2% to 1.8%, in the range of 0.3% to 1.7%, in the range of 0.4% to 1.6%, in the range of 0.5% to 1.5%, in the range of 0.6% to 1.4%, in the range of 0.7% to 1.3%, in the range of 0.8% to 1.2%, and in the range of 0.9% to 1.1%.

[0050] In a specific embodiment, the dopant is carbon (C), and the carbon concentration is in the range of greater than 0% to less than or equal to 2% carbon (C) by atom. In some embodiments, the nanosheet release layer 220 is doped with carbon (C), and the concentration of carbon (C) in the nanosheet release layer 220 is in the range of greater than 0% to less than or equal to 2% by atom. In some embodiments, the carbon concentration in the nanosheet release layer 220 is less than or equal to 2% carbon by atom, including in the range from 0.1% to 1.99% carbon by atom. In some embodiments, the carbon concentration in the nanosheet release layer 220 is in the range of 0.1% to 1.99%, including carbon in the range of 0.1% to 1.95%, in the range of 0.1% to 1.9%, in the range of 0.2% to 1.8%, in the range of 0.3% to 1.7%, in the range of 0.4% to 1.6%, in the range of 0.5% to 1.5%, in the range of 0.6% to 1.4%, in the range of 0.7% to 1.3%, in the range of 0.8% to 1.2%, and in the range of 0.9% to 1.1% by atom.

[0051] In other embodiments, the nanosheet release layer 220 dopant is boron (B) and the dopant has a concentration in a range from greater than 0% to less than or equal to 2% boron (B) on an atomic basis.

[0052] In one or more embodiments, the nanosheet release layer 220 may include a dopant containing one or more of carbon (C) and boron (B), and the total combined dopant concentration may be in a range of greater than 0% to less than or equal to 2%. Therefore, in some embodiments, the nanosheet release layer 220 is doped with carbon (C) and boron (B).

[0053] In one or more embodiments, it has been advantageously discovered that doping the silicon germanium (SiGe) of the nanosheet release layer 220 allows for control of the strain of the vertically stacked superlattice structure 260. Embodiments of the present disclosure advantageously provide a fully strained vertically stacked superlattice structure 260, wherein each of the nanosheet release layers 220 independently comprises doped silicon germanium (SiGe). More specifically, embodiments of the present disclosure advantageously provide a fully strained vertically stacked superlattice structure 260, wherein each of the nanosheet release layers 220 independently comprises silicon germanium (SiGe) doped with carbon (C).

[0054] In one or more embodiments, it has been surprisingly discovered that doping the silicon germanium (SiGe) of the nanosheet release layer 220 with carbon (C) reduces the strain in the vertically stacked superlattice structure 260 and allows for higher growth temperatures, and thus results in an increased growth rate for forming the vertically stacked superlattice structure 260. As used herein, "increased growth rate" refers to reducing the amount of time to form a layer of the vertically stacked superlattice structure 260. In other words, doping the silicon germanium (SiGe) of the nanosheet release layer 220 with carbon (C) at a temperature of about 600°C increases the growth rate by at least 2 times or at least 3 times as compared to the growth rate at a temperature of about 560°C. Embodiments of the present disclosure advantageously provide a fully strained vertically stacked superlattice structure 260, wherein each of the nanosheet release layers 220 independently comprises silicon germanium (SiGe) doped with carbon (C).

[0055] In one or more embodiments, a sacrificial layer 240 is formed between a first or lower hGAA and a second or upper hGAA. In one or more embodiments, the intermediate sacrificial layer 240 is selectively removed during later processing and replaced with an intermediate dielectric isolation. The intermediate dielectric isolation layer is used to electrically isolate the source / drain region of the lower GAA 215 from the source / drain region of the upper GAA 255. In one or more embodiments, the sacrificial layer 240 includes silicon germanium (SiGe) having a germanium content in the range of greater than 15% to 50% by atom. In a specific embodiment, the nanosheet release layer 220 includes silicon germanium (SiGe) having a germanium content in the range of about 10% to 30% by atom, and the sacrificial layer 240 includes silicon germanium (SiGe) having a germanium content in the range of 20% to 40% by atom. In a particular embodiment, the sacrificial layer 240 includes silicon germanium (SiGe) having a germanium content in the range of approximately 20% to 50% atomically, including 20%, 21%, 22%, 23%, 24%, 25%, 26%, 27%, 28%, 29%, 30%, 31%, 32%, 33%, 34%, 35%, 36%, 37%, 38%, 39%, 40%, 41%, 42%, 43%, 44%, 45%, 46%, 47%, 48%, 49% and 50%.

[0056] In one or more embodiments, the sacrificial layer 240 can have any suitable thickness. In some embodiments, the thickness of the sacrificial layer 240 is in the range of 15 nm to 90 nm, including a range of 15 nm to 80 nm, a range of 20 nm to 75 nm, a range of 15 nm to 60 nm, a range of 15 nm to 50 nm, a range of 15 nm to 75 nm, and a range of 20 nm to 50 nm. In some embodiments, increasing the thickness of the sacrificial layer 240 to greater than 40 nm increases the etch selectivity between the sacrificial layer 240 and the nanosheet release layer 220.

[0057] As known to those skilled in the art, during subsequent processing, the sacrificial layer 240 may be removed and replaced with an intermediate isolation layer. Therefore, at operation 110, the method 100 optionally includes selectively removing the sacrificial layer 240. The sacrificial layer 240 may be selectively removed by any suitable means known to those skilled in the art. In some embodiments, the selective removal of the sacrificial layer 240 includes an etching process that removes the sacrificial layer 240 but does not remove the nanosheet release layer 220. In some embodiments, the etching process includes one or more of a wet etching process or a dry etching process. In some embodiments, the etching process is a directional etching process.

[0058] Each of the nanosheet release layer 220, the nanosheet channel layer 230, and the sacrificial layer 240 within the vertically stacked superlattice structure 260 has its own selective removal rate. Without being bound by theory, it is believed that the high germanium content of the sacrificial layer 240 (e.g., greater than 30% germanium by atom) increases the selective removal rate within the vertically stacked superlattice structure, and that doping the SiGe of the nanosheet release layer 220 with carbon reduces the etch rate of the nanosheet release layer, resulting in a selectivity of >10:1 between the sacrificial layer 240 and the nanosheet release layer 220. In one or more embodiments, increasing the thickness of the sacrificial layer 240 to a thickness greater than 40 nm results in an increased selectivity of greater than 15:1 between the sacrificial layer 240 and the nanosheet release layer 220.

[0059] In one or more embodiments, it has been advantageously found that the silicon germanium (SiGe) of the nanosheet release layer 220 doped with a dopant such as carbon (C), having a dopant concentration in a range of greater than 0% to less than or equal to 2% by atom, allows differentiation of the nanosheet release layer 220, the nanosheet channel layer 230, and the sacrificial layer 240 within the vertically stacked superlattice structure 260. In other words, the silicon germanium (SiGe) of the nanosheet release layer 220 doped with carbon (C) advantageously reduces the selective removal rate of each nanosheet release layer within the vertically stacked superlattice structure 260. Embodiments of the present disclosure advantageously provide a method of selectively removing a sacrificial layer while reducing its selective removal rate without damaging the nanosheet release layer and the nanosheet channel layer within one or more of the first hGAA 215 or the second hGAA 255.

[0060] In one or more embodiments, it has been advantageously found that the carbon (C) doped nanosheet release layer 220 has a reduced etch rate compared to a nanosheet release layer not doped with carbon (C). In some embodiments, the etch rate is reduced by a factor of at least 2.

[0061] The use of spatially relative terms such as "under", "below", "below", "above", "above", etc. may be used in this specification to facilitate description of the relationship of one element or feature shown in the diagram to other elements or features. It will be understood that in addition to the orientation depicted in the diagram, the spatially relative terms are also intended to cover different orientations of the device in use or operation. For example, if the device in the icon is turned over, the elements described as "under" or "under" other elements or features will be oriented as "above" the other elements or features. Therefore, the exemplary term "under" can cover both orientations of above and below. The device can be oriented in other ways (rotated 90 degrees or in other orientations), and the spatially relative terms used herein are interpreted accordingly.

[0062] The use of the terms "a", "an", and "the" and similar reference words in the context of describing the materials and methods discussed in the present specification (especially in the context of the following claims) should be understood to include both the singular and the plural, unless otherwise indicated herein or clearly contradicted by the context. The recitation of ranges of values ​​herein is intended merely to provide a shorthand method of representing the individuality of each separate value falling within the range, unless otherwise indicated herein, and each individual value is incorporated into the specification as if it were individually recited herein. All methods described herein can be performed in any suitable order, unless otherwise indicated herein or clearly contradicted by the context. The use of any and all examples provided herein, or exemplary words (e.g., "for example"), is intended only to better illustrate the materials and methods and is not intended to limit them unless otherwise claimed. No words in the specification should be construed to indicate that any non-claimed element is essential to the practice of the materials and methods of the present disclosure.

[0063] References throughout the specification to "one embodiment," "certain embodiments," "one or more embodiments," or "an embodiment" refer to specific features, structures, materials, or characteristics described in conjunction with that embodiment included in at least one embodiment of the present disclosure. Thus, phrases such as "in one or more embodiments," "certain embodiments," "in an embodiment," or "in an embodiment" appearing throughout the specification do not necessarily refer to the same embodiment of the present disclosure. In one or more embodiments, the specific features, structures, materials, or characteristics are combined in any suitable manner.

[0064] Although the disclosure of this case has been described with reference to specific embodiments, it should be understood that these embodiments are merely illustrative of the principles and applications of the disclosure. It will be apparent to those skilled in the art that various modifications and variations may be made to the methods and apparatus of the disclosure without departing from the spirit and scope of the disclosure. Therefore, the disclosure is intended to include modifications and variations within the scope of the appended claims and their equivalents.

Claims

1. A method for forming a semiconductor device, the method comprising the following steps: The vertically stacked superlattice structure is formed on the substrate by the following steps: forming a first horizontal gate-all-around (hGAA) structure on the substrate; forming a sacrificial layer on a top surface of the first hGAA structure, the sacrificial layer comprising silicon germanium (SiGe) having a germanium content in a range of greater than 0% to 50% by atom; and A second horizontal wraparound gate (hGAA) structure is formed on a top surface of the sacrificial layer, wherein each of the first hGAA structure and the second hGAA structure comprises alternating layers of nanosheet channel layers and nanosheet release layers, the nanosheet channel layers comprising silicon (Si) and each of the nanosheet release layers independently comprising silicon germanium (SiGe) doped with a dopant. 2 . The method of claim 1 , wherein the sacrificial layer comprises silicon germanium (SiGe) having a germanium content in a range of 20 to 50 atomic percent. 3 . The method of claim 2 , wherein the nanosheet release layer comprises silicon germanium (SiGe) having a germanium content in a range of 10 to 30 atomic percent. The method of claim 1 , wherein the sacrificial layer has a thickness in a range of 15 nm to 90 nm. 5 . The method of claim 1 , wherein each of the first hGAA structure and the second hGAA structure has alternating layers of nanosheet channel layers and nanosheet release layers in a range of 1 to 5 pairs.

6. The method of claim 1, wherein the dopant comprises one or more of carbon (C) and boron (B). 7 . The method of claim 6 , wherein the silicon germanium (SiGe) of the nanosheet release layer is doped with carbon (C).

8. The method of claim 6, wherein the dopant has a concentration ranging from greater than 0% to less than or equal to 2% dopant on an atomic basis. 9 . The method of claim 1 , wherein the nanosheet release layer has a reduced etch rate compared to the sacrificial layer.

10. The method of claim 9, wherein the etching rate is reduced by at least 1 / 2.

11. The method of claim 7, wherein doping the silicon germanium (SiGe) of the nanosheet release layer with carbon (C) reduces strain in the vertically stacked superlattice structure and allows for higher growth temperatures and increased growth rates.

12. The method of claim 1, wherein the vertically stacked superlattice structure is fully strained and each nanosheet channel layer is substantially defect-free.

13. The method of claim 3, wherein the sacrificial layer comprises silicon germanium (SiGe) having a germanium content in the range of greater than 30% to 50% by atom, and wherein the nanosheet release layer comprises silicon germanium (SiGe) having a concentration in the range of greater than 15% to 20% by atom and doped with carbon having a carbon concentration in the range of greater than 0% to less than or equal to 2% by atom.

14. The method of claim 1, further comprising the steps of: The sacrificial layer is selectively removed.

15. A semiconductor device comprising: A vertically stacked superlattice structure, the vertically stacked superlattice structure being on a substrate, the vertically stacked superlattice structure comprising: A first horizontal gate-around (hGAA) structure, wherein the first horizontal gate-around (hGAA) structure on the substrate; a sacrificial layer on a top surface of the first hGAA structure, the sacrificial layer comprising silicon germanium (SiGe) having a germanium content in a range of greater than 0% to 50% by atom; and A second horizontal gate-around (hGAA) structure, wherein the second horizontal gate-around (hGAA) structure on the top surface of the sacrificial layer, Each of the first hGAA structure and the second hGAA structure includes alternating layers of nanosheet channel layers and nanosheet release layers, the nanosheet channel layers including silicon (Si) and the nanosheet release layers including silicon germanium (SiGe) doped with a dopant. 16 . The semiconductor device of claim 15 , wherein the dopant comprises one or more of carbon (C) and boron (B). 17 . The semiconductor device of claim 16 , wherein the silicon germanium (SiGe) of the nanosheet release layer is doped with carbon (C).

18. The semiconductor device of claim 16, wherein the dopant has a concentration ranging from greater than 0% to less than or equal to 2% dopant on an atomic basis.

19. The semiconductor device of claim 15, wherein the sacrificial layer comprises silicon germanium (SiGe) having a germanium content in the range of 20% to 50% by atom, and wherein the nanosheet release layer comprises silicon germanium (SiGe) having a concentration in the range of 10% to 30% by atom and doped with carbon having a carbon concentration in the range of greater than 0% to less than or equal to 2% by atom.

20. The semiconductor device of claim 17, wherein doping the silicon germanium (SiGe) of the nanosheet release layer with carbon (C) reduces strain in the vertically stacked superlattice structure and allows for higher growth temperatures and increased growth rates.