Preparation process of dephenolized cottonseed oil

By optimizing the cottonseed oil preparation process, including vaporization, leaching, deacidification and decolorization treatment, the problems of free gossypol, acid value and color in cottonseed oil are solved, efficient removal and improvement are achieved, and product safety and quality are improved. , meets food safety standards and reduces production costs.

CN118956487APending Publication Date: 2024-11-15XINJIANG GUANNONG FRUIT & ANTLER GROUP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411234963.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

During the preparation of cottonseed oil, there are problems such as removing free gossypol, improving color and controlling acid value, which affects the edible safety and quality of the product.

Method used

Through optimized process steps, including adding appropriate amount of water to steam the embryo, selecting specific solvents and conditions for leaching, adopting specific deacidification methods and decolorizing agents, combining vacuum rotary evaporation and degumming, deacidification and decolorization treatments, the high efficiency of free gossypol is achieved by achieving high efficiency of free gossypol Removal, color improvement and acid value control.

Benefits of technology

It effectively reduces the free gossypol content and acid value in cottonseed oil, improves the color, improves the edible safety and quality of the product, meets food safety standards, and reduces production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005027476050000121
    Figure BDA0005027476050000121
Patent Text Reader

Abstract

The invention provides a preparation process of dephenolized cottonseed oil, which comprises the following steps: S1, cleaning smooth cotton seeds, shelling to take embryos, and sequentially crushing, softening, steaming and leaching the embryos to obtain mixed oil; and S2, evaporating the mixed oil until the mass concentration is 60%-70%, and then, carrying out refining treatment. The free gossypol content, the acid value, the color, the smell and the like of the dephenolized cottonseed oil prepared by the method all meet the requirements of first-grade cottonseed oil in GBT1537-2019 cottonseed oil, and are far lower than the stipulation of the gossypol content in vegetable oil in the national food safety standard. The edible safety and quality of the cottonseed oil are improved, the production cost is reduced, and the method has remarkable economic and social benefits.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of cottonseed oil products, and particularly relates to a preparation process of dephenolized cottonseed oil. Background Art

[0002] As an important edible oil resource, cottonseed oil occupies an important position in the food industry and consumer market due to its unique fatty acid composition and nutritional value. However, the preparation of cottonseed oil faces a series of technical challenges, mainly including the removal of free gossypol, the improvement of color and the control of acid value.

[0003] Free gossypol is the main toxic component in cottonseed oil and poses a potential threat to human health. Direct consumption of cottonseed oil containing high concentrations of free gossypol may lead to poisoning reactions, so it must be effectively removed during the preparation process. The color of crude cottonseed oil is dark, which directly affects its commodity value and consumer acceptance. The improvement of color is not only related to the appearance of the product, but also to its intrinsic quality. Acid value is an important indicator to measure the degree of rancidity of oils and fats. High acid value not only affects the storage stability of oils and fats, but may also lead to a decrease in nutritional value.

[0004] Therefore, it is necessary to develop a dephenolized cottonseed oil preparation process. By optimizing each link in the process, efficient removal of free cottonpol, significant improvement in color and effective control of acid value are achieved. This not only improves the edible safety and quality of cottonseed oil, but also reduces production costs, with significant economic and social benefits. Summary of the invention

[0005] The purpose of the present invention is to provide a preparation process of dephenolized cottonseed oil, which realizes efficient removal of free cottonpol, significant improvement of color and effective control of acid value by optimizing various links in the process. It not only improves the edible safety and quality of cottonseed oil, but also reduces production costs, and has significant economic and social benefits.

[0006] In order to achieve the above object, the present invention provides the following technical solutions:

[0007] The preparation process of the dephenolized cottonseed oil comprises the following steps:

[0008] S1. After cleaning the cotton seeds, the husks are peeled and the embryos are taken out, and the embryos are crushed, softened, steamed and leached in sequence to obtain a mixed oil;

[0009] S2. After evaporating the mixed oil to a mass concentration of 60% to 70%, refining is performed to obtain the product.

[0010] Preferably, the softening temperature is 70-75° C., and the softening time is 15-20 min.

[0011] Preferably, the specific steps of steaming the embryos are: adding water to the softened cotton seed embryos, stirring evenly and sealing, and steaming at 93-97° C. for 55-65 minutes.

[0012] Preferably, the amount of water added is 18% to 22% of the weight of the softened cotton seed embryo.

[0013] The inventor found that adding an appropriate amount of water and steaming embryo under specific conditions can reduce the content of free cottonpol in cottonseed oil. This may be because in the process of steaming embryo, an appropriate amount of moisture and temperature are conducive to the diffusion of moisture between the internal organizational structure of the material blank, so that more free cottonpol is released, not only can it be combined with protein to generate protein-bound cottonpol that is insoluble in mixed oil and is filtered out in the leaching step, but also can make phospholipid fully absorb water and condense, reduce its solubility in grease, reduce the chance of phospholipid and free cottonpol to generate phospholipid-bound cottonpol that is soluble in grease, and then reduce the content of cottonpol in cottonseed oil. And phospholipid-bound cottonpol color is darker, and residue can affect the color of cottonseed oil. But the temperature is too high in the process of steaming embryo and can cause protein denaturation, and denatured protein-bound cottonpol may be soluble in grease, affecting the free cottonpol removal rate.

[0014] Preferably, the specific steps of leaching are: adding solvent to the steamed cotton seeds, stirring at 52-58°C at a rate of 30 r / min for 25-35 min, then ultrasonicating for 0.5-1.5 h, and vacuum rotary evaporating after filtration until the mass fraction of the mixed oil is 20%-25%.

[0015] Preferably, the mass ratio of the steamed cotton seeds to the solvent is 1:(2-3); more preferably, it is 2:5.

[0016] Preferably, the solvent is n-hexane and ethanol aqueous solution.

[0017] Preferably, the mass ratio of n-hexane to ethanol aqueous solution is (2-3):1; further preferably, it is 7:3.

[0018] Preferably, the mass fraction of ethanol in the ethanol aqueous solution is 85% to 95%.

[0019] Preferably, the power of the ultrasound is 200-250W.

[0020] Preferably, the vacuum degree of the vacuum rotary evaporation is 0.075-0.085 MPa and the temperature is 78-82°C.

[0021] The inventors found that in the leaching process, the selection of specific solvents and leaching conditions can not only greatly reduce the free gossypol content and acid value in cottonseed oil, but also improve the color. This may be because although ethanol aqueous solution and n-hexane are immiscible at room temperature, they are mutually soluble at 52-58°C. The oil in cottonseed is easily soluble in the non-polar n-hexane phase, and polar substances such as free gossypol, free fatty acids, and phospholipids will dissolve in the ethanol aqueous phase. After cooling, the two phases are separated, which can greatly remove the impurity content of free gossypol, free fatty acids, etc. in the mixed oil, thereby reducing the acid value and gossypol content of the prepared cottonseed oil. However, the rotary evaporation temperature still needs to be controlled in this process. If the temperature is too high, the protein will denature, resulting in the formation of denatured protein-bound gossypol and phospholipid-bound gossypol that are soluble in oil and have a dark color, affecting the product color and free gossypol content, while if the temperature is too low, most of the free gossypol, free fatty acids, phospholipids and other polar substances cannot be removed by rotary evaporation.

[0022] Preferably, the evaporation conditions in step S2 are: vacuum degree 0.075-0.085 MPa, evaporation temperature 40-60°C.

[0023] The specific methods of the refining treatment are: degumming, deacidification and decolorization.

[0024] The specific method of degumming is: adding 0.2% to 0.4% phosphoric acid and 4% water by weight to the upper layer oil obtained in step S3, the reaction temperature is 55 to 60° C., the reaction time is 15 to 25 minutes, and after the reaction, the degummed oil is obtained by standing and centrifugation.

[0025] The specific deacidification method is as follows: after heating the degummed oil to 50-60° C., adding a 28wt% sodium hydroxide solution with a concentration of 1%-2% of the oil weight, firstly mixing it at high speed with a knife mixer, and then fully reacting it at 45rpm stirring state for 35-45min, letting it stand after the reaction, and centrifuging to obtain a primary deacidified oil; after heating the primary deacidified oil to 50-60° C., adding a 28wt% sodium hydroxide solution with a concentration of 1%-2% of the oil weight, and then mixing it at high speed with a knife mixer again, and then fully reacting it at 45rpm stirring state for 55-65min, letting it stand after the reaction, and centrifuging to obtain a deacidified oil.

[0026] The inventor found that, by selecting a specific deacidification method, the acid value of cottonseed oil can be reduced while the removal rate of cottonpol is greatly improved, thereby improving its stability. This may be because the degummed oil and sodium hydroxide are mixed at a high speed in a knife-type mixer, which can improve the fluidity of grease, so that the sodium hydroxide solution is rapidly dispersed in the grease, and the contact area between the reactants is increased, so that the sodium hydroxide solution is more easily contacted with the acidic substances such as free cottonpol, free fatty acids in the grease and reacts to generate substances such as cottonpol sodium salt, sapodilla and the like, thereby reducing the acid value of cottonseed oil while reducing the free cottonpol content. And the substances such as cottonpol sodium salt, sapodilla generated at a specific low temperature are more likely to agglomerate and be separated, and the specific reaction time enables the raw materials to be fully mixed, greatly improving the removal rate of free cottonpol and free fatty acids. In addition, the secondary deacidification can further reduce the acid value of grease and process the acidic substances such as a small amount of cottonpol that may remain after the initial deacidification, thereby further reducing the acid value and cottonpol content in cottonseed oil.

[0027] The specific decolorization method is: take the deacidified oil and heat it to 100-110° C., add 4%-6% of the oil weight of the decolorizer, stir for 20-30 minutes, filter after reaction, and obtain cottonseed oil after centrifugal separation.

[0028] Preferably, the decolorizing agent is modified activated carbon and activated clay.

[0029] Preferably, the mass ratio of the modified activated carbon to the activated clay is 1:(7-10); further preferably, it is 1:9.

[0030] The preparation method of the activated white clay comprises the following steps: crushing bentonite through a 200-400 mesh sieve and mixing it with a modifier solution, stirring at 90-100°C for 3-5 hours and then cooling to room temperature, removing the upper clear liquid to obtain a lower slurry, washing the lower slurry with water to a pH of 6-7, filtering, drying the filter cake to a constant weight, and crushing to an average particle size of less than 300 meshes.

[0031] Preferably, the montmorillonite content in the bentonite is ≥55%, and the apparent viscosity is 60-70 mPa·s; further preferably, the montmorillonite content in the bentonite is ≥60%, and the apparent viscosity is 65 mPa·s.

[0032] In some preferred embodiments, the bentonite is purchased from Jinhe Minerals (Huizhou) Co., Ltd.

[0033] Preferably, the modifier solution is any one of a sulfuric acid solution and a hydrochloric acid solution.

[0034] Preferably, the concentration of the modifier solution is 18% to 25%.

[0035] Preferably, the solid-liquid ratio of the bentonite and modifier solution is 1 g: 1-3 mL.

[0036] The inventors found that the activated clay prepared by selecting a specific bentonite and modifying it using a specific method has excellent adsorption properties and can also stabilize the acid value of the oil. This may be because sulfuric acid or hydrochloric acid is a strong acid with a high ionization constant, so it is easier to ionize hydrogen ions, and replace with sodium ions, calcium ions and potassium ions between montmorillonite layers in bentonite. The interlayer of montmorillonite forms pores due to the dissolution of metal cations, which increases the crystal interlayer spacing and thus improves the adsorption properties of the activated clay. At the same time, by controlling the modification conditions, the magnesium ions, iron ions and aluminum ions in the octahedron are relatively difficult to dissolve, ensuring the stability of the activated clay structure and avoiding the situation where the acid value rises due to system instability. However, the cottonseed oil decolorized by activated clay has a peculiar smell, which affects the edible experience.

[0037] The preparation method of the modified activated carbon comprises the following steps:

[0038] The activated carbon is mixed with the activated carbon modifier, and calcined at 700-1000°C for 1-3h in a nitrogen atmosphere to obtain the activated carbon.

[0039] Preferably, the activated carbon is coal-based activated carbon.

[0040] Preferably, the particle size of the coal-based activated carbon is 5-20 mesh, and the phenol adsorption capacity is ≥150 mg / g; further preferably, the particle size of the coal-based activated carbon is 8-20 mesh, and the phenol adsorption capacity is ≥160 mg / g.

[0041] In some preferred embodiments, the coal-based activated carbon is purchased from Zhejiang Zhelang Activated Carbon Co., Ltd.

[0042] Preferably, the activated carbon modifier is one or more of sodium hydroxide, potassium hydroxide, disodium ethylenediaminetetraacetate, and tetrasodium ethylenediaminetetraacetate; further preferably, it is sodium hydroxide and disodium ethylenediaminetetraacetate.

[0043] Preferably, the mass ratio of the activated carbon to the activated carbon modifier is 1:(2-5); further preferably, it is 1:4.

[0044] Preferably, the mass ratio of sodium hydroxide to disodium ethylenediaminetetraacetate is (1-4):1; further preferably, it is 3:1.

[0045] The inventor creatively discovered that by using sodium hydroxide and disodium ethylenediaminetetraacetate in a mass ratio of (1 to 4): 1 as modifiers to modify a specific activated carbon, and when the mass ratio of the modified activated carbon to activated clay is 1: (7 to 10), the decolorization effect can be further improved, and the odor can also be removed, meeting the requirements of the national standard. This may be because, on the one hand, sodium hydroxide and disodium ethylenediaminetetraacetate jointly modify the activated carbon, and by etching the carbon layer and introducing nitrogen-containing functional groups, the specific surface area and pore volume of the activated carbon are increased, thereby improving its decolorization efficiency. On the other hand, the modified activated carbon and activated clay work synergistically, further improving the decolorization effect while removing the odor, so that the smell and color of the prepared cottonseed oil meet the requirements. However, the amount of modifier added needs to be strictly controlled. Excessive sodium hydroxide will not only destroy the pore structure of the activated carbon, but also remain in the pores of the activated carbon, hindering adsorption, and the residue of excessive disodium ethylenediaminetetraacetate after high-temperature calcination will also block the pores.

[0046] The present invention also includes the dephenolized cottonseed oil prepared by the dephenolized cottonseed oil preparation process.

[0047] Compared with the prior art, the advantages and beneficial effects of the present invention are:

[0048] 1. The present invention provides a preparation process for dephenolized cottonseed oil. By optimizing each link in the process, efficient removal of free cottonpol, significant improvement in color and effective control of acid value are achieved. The free cottonpol content, acid value, color and odor all meet the requirements of first-class cottonseed oil in GBT1537-2019 "Cottonseed Oil", which is far lower than the national food safety standard for the content of cottonpol in vegetable oil. Not only does it improve the edible safety and quality of cottonseed oil, but it also reduces production costs, with significant economic and social benefits.

[0049] 2. The present invention adds an appropriate amount of water and steams the embryo under specific conditions, thereby reducing the content of free cottonpol in cottonseed oil.

[0050] 3. In the leaching process of the present invention, the specific solvent and leaching conditions are selected, which can not only greatly reduce the free cottonpol content and acid value in the cottonseed oil, but also improve the color.

[0051] 4. The present invention selects a specific deacidification method, which can greatly improve the removal rate of cottonphenol while reducing the acid value of cottonseed oil, thereby improving its stability.

[0052] 5. The present invention selects specific bentonite and adopts a specific method to modify it to prepare the activated white clay, which has excellent adsorption performance and can also stabilize the acid value of oil.

[0053] 6. Selecting sodium hydroxide and disodium ethylenediaminetetraacetate in a mass ratio of (1-4):1 as modifiers to modify specific activated carbon, and when the mass ratio of the modified activated carbon to activated clay is 1:(7-10), the decolorization effect can be further improved, and the odor can also be removed, meeting the requirements of the national standard. DETAILED DESCRIPTION

[0054] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0055] The raw materials used in the present invention are all commercially available, specifically:

[0056] The coal-based activated carbon has a particle size of 8 to 20 meshes and a phenol adsorption capacity of ≥160 mg / g, and is purchased from Zhejiang Zhelang Activated Carbon Co., Ltd.

[0057] The weakly acidic cation exchange resin has a total exchange capacity of ≥8 mmol / mL, a total exchange capacity of ≥1.7 mmol / mL, and a water content of 48% to 58%. It was purchased from Hebi Haige Chemical Technology Co., Ltd., D152.

[0058] The bentonite has a montmorillonite content of ≥60% and an apparent viscosity of 65 mPa·s, and is purchased from Jinhe Minerals (Huizhou) Co., Ltd.

[0059] Example 1

[0060] This embodiment provides a preparation process of dephenolized cottonseed oil, the steps are:

[0061] S1. After cleaning the cotton seeds, the husks are peeled and the embryos are taken out, and the embryos are crushed, softened, steamed and leached in sequence to obtain a mixed oil;

[0062] S2. Evaporate the mixed oil to a mass concentration of 65%, and then perform refining treatment to obtain the product.

[0063] The softening temperature is 73° C. and the softening time is 18 min.

[0064] The specific steps of steaming the embryos are: adding water to the softened cotton seed embryos, stirring evenly, sealing, and steaming at 95° C. for 60 minutes.

[0065] The amount of water added is 20% of the weight of the softened cotton seed embryo.

[0066] The specific extraction steps are: adding solvent to the steamed cotton seeds, stirring at 55°C at a rate of 30r / min for 30min and then ultrasonicating for 1h, and vacuum rotary evaporating after filtration until the mass fraction of the mixed oil is 23%.

[0067] The mass ratio of the steamed cotton seeds to the solvent is 2:5.

[0068] The solvents are n-hexane and ethanol aqueous solution.

[0069] The mass ratio of n-hexane to the ethanol aqueous solution is 7:3.

[0070] The mass fraction of ethanol in the ethanol aqueous solution is 90%.

[0071] The power of the ultrasound is 230W.

[0072] The vacuum degree of the vacuum rotary evaporation is 0.08 MPa and the temperature is 80°C.

[0073] The evaporation conditions in step S2 are: vacuum degree 0.08 MPa, evaporation temperature 50°C.

[0074] The specific methods of the refining treatment are: degumming, deacidification and decolorization.

[0075] The specific method of degumming is: adding 0.3% phosphoric acid and 4% water by weight to the upper layer oil obtained in step S3, the reaction temperature is 58° C., the reaction time is 20 min, and after the reaction, the degummed oil is obtained by standing and centrifugation.

[0076] The specific deacidification method is as follows: after heating the degummed oil to 55° C., adding a 28wt% sodium hydroxide solution with a concentration of 1.5% by weight of the oil, firstly mixing it at high speed with a knife mixer, and then fully reacting it at a stirring state of 45 rpm for 40 minutes, letting it stand after the reaction, and centrifuging to obtain a primary deacidified oil; after heating the primary deacidified oil to 55° C., adding a 28wt% sodium hydroxide solution with a concentration of 1.5% by weight of the oil, and then mixing it at high speed with a knife mixer again, and then fully reacting it at a stirring state of 45 rpm for 60 minutes, letting it stand after the reaction, and centrifuging to obtain a deacidified oil.

[0077] The specific decolorization method is: take the deacidified oil and heat it to 105° C., add a decolorizer of 5% by weight of the oil, stir for 25 minutes, filter after reaction, and obtain cottonseed oil after centrifugal separation.

[0078] The decolorizing agent is modified activated carbon and activated clay.

[0079] The mass ratio of the modified activated carbon to the activated clay is 1:9.

[0080] The preparation process of the activated white clay comprises the following steps: crushing bentonite through a 325-mesh sieve and mixing it with a modifier solution, stirring at 95° C. for 4 hours and then cooling to room temperature, removing the upper clear liquid to obtain a lower slurry, washing the lower slurry with water until the pH value is 6.5, filtering it by suction, drying the filter cake to a constant weight, and crushing it to obtain activated white clay with an average particle size of 325 meshes.

[0081] The modifier solution is a sulfuric acid solution.

[0082] The concentration of the modifier solution is 20%.

[0083] The solid-to-liquid ratio of the bentonite and modifier solution is 1 g:2 mL.

[0084] The preparation process of the modified activated carbon comprises the following steps:

[0085] The activated carbon is mixed with the activated carbon modifier and calcined at 900°C for 2h in a nitrogen atmosphere to obtain the product.

[0086] The activated carbon is coal-based activated carbon.

[0087] The activated carbon modifiers are sodium hydroxide and disodium ethylenediaminetetraacetate.

[0088] The mass ratio of the activated carbon to the activated carbon modifier is 1:4.

[0089] The mass ratio of the sodium hydroxide to disodium ethylenediaminetetraacetate is 3:1.

[0090] Example 2

[0091] The specific deacidification method is as follows: after heating the degummed oil to 55° C., adding a 28wt% sodium hydroxide solution with a concentration of 2% by weight of the oil, firstly mixing it at high speed with a knife mixer, and then fully reacting it at a stirring state of 45 rpm for 40 minutes, letting it stand after the reaction, and centrifuging to obtain a primary deacidified oil; after heating the primary deacidified oil to 55° C., adding a 28wt% sodium hydroxide solution with a concentration of 1% by weight of the oil, and again mixing it at high speed with a knife mixer, and then fully reacting it at a stirring state of 45 rpm for 65 minutes, letting it stand after the reaction, and centrifuging to obtain a deacidified oil.

[0092] Example 3

[0093] The difference between this embodiment and embodiment 1 is that the mass ratio of the modified activated carbon to the activated clay is 1:7.

[0094] Comparative Example 1

[0095] The difference between this comparative example and Example 1 is that the specific steps of steaming the embryos are: adding water to the softened cotton seed embryos, stirring evenly and then sealing, and steaming at 110° C. for 60 minutes.

[0096] Comparative Example 2

[0097] The difference between this comparative example and Example 1 is that the solvent is n-hexane.

[0098] Comparative Example 3

[0099] The difference between this comparative example and Example 1 is that the vacuum degree of the vacuum rotary evaporation is 0.08 MPa and the temperature is 70°C.

[0100] Comparative Example 4

[0101] The difference between this comparative example and Example 1 is that the specific method of deacidification is: after the degummed oil is heated to 55°C, a 28wt% sodium hydroxide solution with a concentration of 1.5% by weight of the oil is added, firstly mixed at high speed by a knife mixer, and then fully reacted for 40 minutes under stirring at 45rpm, and then allowed to stand after the reaction, and deacidified oil is obtained after centrifugal separation.

[0102] Comparative Example 5

[0103] The difference between this comparative example and Example 1 is that the specific method of deacidification is as follows: after the degummed oil is heated to 55°C, a 28wt% sodium hydroxide solution with a concentration of 1.5% by weight of the oil is added, firstly mixed at high speed by a knife mixer, and then fully reacted for 20 minutes under a stirring state of 45rpm, and then allowed to stand after the reaction, and centrifuged to obtain a primary deacidified oil; after the primary deacidified oil is heated to 55°C, a 28wt% sodium hydroxide solution with a concentration of 1.5% by weight of the oil is added, and then mixed at high speed by a knife mixer again, and then fully reacted for 30 minutes under a stirring state of 45rpm, and then allowed to stand after the reaction, and centrifuged to obtain a deacidified oil.

[0104] Comparative Example 6

[0105] The difference between this comparative example and Example 1 is that the specific method of deacidification is as follows: after the degummed oil is heated to 70°C, a 28wt% sodium hydroxide solution with a concentration of 1.5% by weight of the oil is added, firstly mixed at high speed by a knife mixer, and then fully reacted for 40 minutes under a stirring state of 45rpm, and then allowed to stand after the reaction, and centrifuged to obtain a primary deacidified oil; after the primary deacidified oil is heated to 70°C, a 28wt% sodium hydroxide solution with a concentration of 1.5% by weight of the oil is added, and then mixed at high speed by a knife mixer again, and then fully reacted for 60 minutes under a stirring state of 45rpm, and then allowed to stand after the reaction, and centrifuged to obtain a deacidified oil.

[0106] Comparative Example 7

[0107] The difference between this comparative example and Example 1 is that the mass ratio of the modified activated carbon to the activated clay is 1:5.

[0108] Comparative Example 8

[0109] The difference between this comparative example and Example 1 is that the modifier solution is a 20 wt % phosphoric acid solution, which is a medium-strong acid.

[0110] Comparative Example 9

[0111] The difference between this comparative example and Example 1 is that the activated carbon is not modified.

[0112] Comparative Example 10

[0113] The difference between this comparative example and Example 1 is that the mass ratio of the sodium hydroxide to disodium ethylenediaminetetraacetate is 5:1.

[0114] Performance Testing

[0115] The acid value and free cottonpol content were tested according to the method in GB / T 1537-2019 "Cottonseed Oil". The color was determined according to GB / T 22460-2008 "Determination of the color of Lovibond in animal and vegetable oils and fats", and the red value R (25.4 mm) was used to represent the color of cottonseed oil. The results are shown in Table 1.

[0116] Table 1 Measurement results

[0117]

[0118] According to statistics, the dephenolized cottonseed oil prepared in Examples 1 to 3 of the present invention has a low free cottonpol content and acid value and a light color, which meets the requirements of first-grade cottonseed oil in GBT1537-2019 "Cottonseed Oil". In Comparative Example 1, the embryo steaming temperature is too high, in Comparative Example 2, no mixed solvent is used, in Comparative Example 3, the vacuum rotary evaporation temperature is too low, in Comparative Example 4, no secondary deacidification is performed, in Comparative Example 5, the deacidification time is short, in Comparative Example 6, the deacidification temperature is high, in Comparative Example 7, the amount of activated clay added is too low, in Comparative Example 8, medium-strong acid is used to prepare activated clay, and the ionization constant is low, in Comparative Example 9, the activated carbon is not modified, and in Comparative Example 10, the amount of sodium hydroxide added is too high. The prepared cottonseed oils do not fully meet the requirements of the first-class cottonseed oil in GBT1537-2019 "Cottonseed Oil". Therefore, the free cottonphenol content, acid value, color, etc. in the dephenolized cottonseed oil prepared by the method described in the present application meet the requirements of the first-class cottonseed oil in GBT1537-2019 "Cottonseed Oil", which is far lower than the provisions of the national food safety standard on the cottonphenol content in vegetable oil.

[0119] The above is a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principles of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.

Claims

1. A preparation process for dephenolized cottonseed oil, It is characterized in that The following steps are involved: S1. After cleaning the cotton seeds, the husks are peeled and the embryos are taken out, and the embryos are crushed, softened, steamed and leached in sequence to obtain a mixed oil; S2, evaporating the mixed oil to a mass concentration of 60% to 70%, and then refining the mixed oil to obtain; The specific steps of steaming the embryos are: adding water to the softened cotton seed embryos, stirring evenly and sealing, and steaming at 93-97° C. for 55-65 minutes; the amount of water added is 18%-22% of the weight of the softened cotton seed embryos; The specific steps of leaching are: adding solvent to the cotton seeds after embryo steaming, stirring at 52-58°C at a rate of 30r / min for 25-35min, then ultrasonicating for 0.5-1.5h, filtering and vacuum rotary evaporating until the mass fraction of the mixed oil is 20%-25%; The solvent is n-hexane and ethanol aqueous solution; the mass ratio of n-hexane to ethanol aqueous solution is (2-3):

1.

2. The preparation process of dephenolized cottonseed oil according to claim 1, It is characterized in that The mass ratio of the steamed cotton seeds to the solvent is 1:(2-3).

3. The preparation process of dephenolized cottonseed oil according to claim 2, It is characterized in that The vacuum degree of the vacuum rotary evaporation is 0.075-0.085 MPa, and the temperature is 78-82°C.

4. The preparation process of dephenolized cottonseed oil according to claim 1, It is characterized in that The evaporation conditions in step S2 are: vacuum degree 0.075-0.085 MPa, evaporation temperature 40-60°C.

5. The preparation process of dephenolized cottonseed oil according to claim 1, It is characterized in that The specific methods of the refining treatment are: degumming, deacidification and decolorization.

6. The preparation process of dephenolized cottonseed oil according to claim 5, It is characterized in that The specific method of degumming is: adding 0.2% to 0.4% phosphoric acid and 4% water by weight to the upper layer oil obtained in step S3, the reaction temperature is 55 to 60° C., the reaction time is 15 to 25 minutes, and after the reaction, the degummed oil is obtained by standing and centrifugation.

7. The preparation process of dephenolized cottonseed oil according to claim 5, It is characterized in that The specific deacidification method is as follows: after heating the degummed oil to 50-60° C., adding a 28wt% sodium hydroxide solution with a concentration of 1%-2% of the oil weight, firstly mixing it at high speed with a knife mixer, and then fully reacting it at 45rpm stirring state for 35-45min, letting it stand after the reaction, and centrifuging to obtain a primary deacidified oil; after heating the primary deacidified oil to 50-60° C., adding a 28wt% sodium hydroxide solution with a concentration of 1%-2% of the oil weight, and then mixing it at high speed with a knife mixer again, and then fully reacting it at 45rpm stirring state for 55-65min, letting it stand after the reaction, and centrifuging to obtain a deacidified oil.

8. The preparation process of dephenolized cottonseed oil according to claim 5, It is characterized in that The specific decolorization method is: take the deacidified oil and heat it to 100-110° C., add 4%-6% of the oil weight of the decolorizer, stir for 20-30 minutes, filter after reaction, and obtain the dephenolized cottonseed oil after centrifugal separation.

9. The preparation process of dephenolized cottonseed oil according to claim 8, It is characterized in that The decolorizing agent is modified activated carbon and activated clay.