FR4 structure and FPC production process

By adding a nanoparticle layer and a copper-affinity surface layer to the FR4 substrate layer, and combining copper foil bonding, adhesive coating, reinforcement and film coating processes, the rigidity limitation of the FR4 structure is solved, the mechanical strength, thermal stability and flexibility of the FPC are improved, and the reliability and yield of electronic products are increased.

CN118973077APending Publication Date: 2024-11-15JIANGSU XINHONGTAO NEW ENERGY TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410972646.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The traditional FR4 structure FPC manufacturing process suffers from rigidity that limits flexibility and bendability, as well as insufficient mechanical strength, thermal stability, and high-temperature resistance. This affects the design freedom and performance of electronic products and reduces the yield rate.

Method used

A nanoparticle layer is added to the FR4 substrate layer to form a copper-affinity surface layer. Through copper foil bonding, adhesive coating, reinforcement and film coating, combined with micro-hole drilling technology, the mechanical strength and thermal stability are improved, and the flexibility and high temperature resistance are increased.

Benefits of technology

It improves the mechanical strength and thermal stability of FPC, reduces delamination, enhances reliability and service life, and increases the design freedom and yield of electronic products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118973077A_ABST
    Figure CN118973077A_ABST
Patent Text Reader

Abstract

The invention discloses an FR4 structure which comprises an FR4 base material layer, a nano particle layer is uniformly arranged in the FR4 base material layer, a copper-philic surface layer is arranged on the upper surface of the FR4 base material layer, a copper foil layer is arranged on the upper surface of the copper-philic surface layer, an adhesive layer is arranged on the upper surface of the copper foil layer, a reinforcing layer is arranged on the upper surface of the adhesive layer, and the reinforcing layer is arranged on the upper surface of the reinforcing layer. And a protective film layer is arranged on the upper surface of the reinforcing layer. The invention further discloses an FPC production process which comprises the following steps: S1, preparing the FR4 base material; s2, carrying out surface functionalization treatment; s3, copper foil lamination; s4, gluing is carried out; s5, reinforcing is carried out; s6, film covering; and S7, performing micropore drilling. According to the invention, the nano particles with a specific proportion are added into the FR4 base material layer, the nano particle layer is formed through the dispersion strengthening effect, the mechanical strength and thermal stability of the FR4 structure are improved, in addition, the copper-philic surface layer is arranged on the FR4 base material layer, the adhesion to the copper foil is improved, the layering phenomenon is reduced, and the service life of the FR4 structure is prolonged. And the reliability and the service life of the FPC can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of circuit boards, and in particular relates to an FR4 structure and an FPC production process. Background Art

[0002] FPC (flexible printed circuit board) plays an important role in modern electronic devices with its unique advantages such as lightness, bendability, and three-dimensional wiring. However, in the traditional FPC production process, the selection of substrate has a huge impact on the performance of FPC. FR4 material, that is, glass fiber epoxy resin board, is widely used as the substrate of rigid circuit boards due to its good electrical insulation and mechanical strength.

[0003] For example, an FPC production process disclosed in the authorization announcement number CN115023053B uses die-cutting instead of the traditional developing and etching method to make FPC. The entire process does not require the use of chemicals and is environmentally friendly, thus achieving the purpose of environmental protection. However, it does not solve some problems of the existing FR4 structure and FPC production process: in the FPC field, the rigid characteristics of pure FR4 limit the flexibility and bendability of FPC, thereby affecting the design freedom and performance of electronic products. At the same time, the mechanical strength, thermal stability and high temperature resistance of the pure FR4 structure are low, which not only reduces the service life of the FR4 structure, but also reduces the yield rate of the FPC. For this reason, we propose an FR4 structure and FPC production process. Summary of the invention

[0004] The purpose of the present invention is to provide a FR4 structure and FPC production process to solve the problems raised in the above background technology.

[0005] To achieve the above-mentioned purpose, the present invention provides the following technical solution: an FR4 structure, comprising an FR4 substrate layer, a nanoparticle layer is uniformly arranged inside the FR4 substrate layer, a copper-philic surface layer is arranged on the upper surface of the FR4 substrate layer, a copper foil layer is arranged on the upper surface of the copper-philic surface layer, an adhesive layer is arranged on the upper surface of the copper foil layer, a reinforcement layer is arranged on the upper surface of the adhesive layer, and a protective film layer is arranged on the upper surface of the reinforcement layer.

[0006] Preferably, the nanoparticle layer is one of an aluminum oxide nanoparticle layer, a boron nitride nanoparticle layer, a carbon nanotube layer, a graphene layer and a silicon dioxide nanoparticle layer; and the reinforcement layer is configured as a steel plate layer.

[0007] Preferably, the protective film layer includes an upper film layer, a middle film layer and a lower film layer which are laminated together, the upper film layer and the lower film layer are both PBT synthetic layers, a release layer is provided on the outside of the upper film layer, and the upper film layer and the lower film layer are respectively bonded to the middle film layer by polymer compound adhesive.

[0008] A FPC production process comprises the following steps:

[0009] S1. FR4 substrate preparation: Select nanoparticles with a moderate particle size, disperse the nanoparticles evenly in the epoxy resin matrix by stirring and ultrasonic treatment, and then cure at a specific temperature to obtain a reinforced FR4 substrate layer;

[0010] S2. Surface functionalization: Plasma treatment is performed on the FR4 substrate to activate the surface activity, and then a copper-philic surface layer is formed through chemical plating or nano-coating technology;

[0011] S3. Copper foil lamination: Use a high-precision laminating machine to make the copper foil closely fit on the copper-philic surface layer to form a copper foil layer;

[0012] S4. Gluing: Using a glue coating machine, a layer of glue is applied on the surface of the copper foil layer to form an adhesive layer;

[0013] S5. Reinforcement: attaching the reinforcing layer to the upper surface of the adhesive layer, and pressing the reinforcing layer and the adhesive layer together by lamination;

[0014] S6. Lamination: Attach a protective film to the reinforcing plate, pre-press the protective film at low temperature and low pressure, so that the protective film wraps around the reinforcing layer, but the protective film does not contact the surface of the FR4 substrate, then apply force to both sides of the protective film extending from the edge of the reinforcing layer in the horizontal direction, so that the protective film effectively shrinks toward the edge of the reinforcing layer, leaving no gap between the protective film and the reinforcing layer, the protective film fits the reinforcing layer and wraps the reinforcing layer tightly, and then presses and cures the protective film at high temperature and high pressure, so that the protective film is in close contact with the FR4 substrate, and the lamination is completed;

[0015] S7. Micro-hole drilling: Use laser ablation, chemical etching or molding technology to form micro-holes in the FR4 substrate layer to balance mechanical strength and flexibility.

[0016] Preferably, the specific method for preparing the FR4 substrate in S1 includes:

[0017] S101. Pretreatment of nanoparticles: performing surface modification treatment on the nanoparticles at a temperature between 20 and 80° C. by chemically modifying the nanoparticles with a silane coupling agent or a surfactant for 4 to 18 hours;

[0018] S102. Dispersion of nanoparticles: The surface-modified nanoparticles are directly added to the epoxy resin, the stirring speed is 500-2000 rpm, the stirring time is 10-80 min, the nanoparticles are fully dispersed, and ultrasonic treatment is performed at an ultrasonic power of 100-200 W for 30-60 min;

[0019] S103. Mixing and curing: Mix the dispersed nanoparticles with epoxy resin and amine curing agent in a ratio of 1:300-500:100-200. After mixing, pour the mixture into a mold and enter the curing stage. The curing temperature is 25-150°C and the curing time is 2-72h to obtain a FR4 substrate.

[0020] Preferably, the pre-pressing conditions at low temperature and low pressure in S6 are 80±10°C and 50±10kg / cm 2 , pre-pressing time 5S, molding time 10S; the high temperature and high pressure conditions are temperature 175±10℃, pressure 50±10kg / cm 2 , pre-pressing time 5S, molding time 300S.

[0021] Preferably, the step S6 further includes preparing a protective film before laminating, which specifically includes the following steps:

[0022] S601. The raw materials of the upper film layer, the middle film layer and the lower film layer are mixed respectively;

[0023] S602. The raw material treated in S601 is subjected to a casting process to obtain each film layer;

[0024] S603. After the processing in S602, the film layers are pressed and shaped to obtain a semi-finished film;

[0025] S604. Cooling and winding the semi-finished film;

[0026] S605. The rolled semi-finished film is subjected to a aging treatment to obtain a finished film.

[0027] Preferably, the temperature of the casting process in 602 is 270°C-290°C, and the casting process includes extrusion operation of a screw extruder. During the extrusion operation of the screw extruder, the temperature is 270°C-290°C, the mold temperature is 50-80°C, and the screw aspect ratio is L / P=20; the shaping speed in 603 is 8-12m / min; the temperature of the aging treatment in 605 is 45°C-60°C, and the time is 5-7 days.

[0028] Preferably, after the copper foil lamination in S4, circuit manufacturing is also included, and the circuit manufacturing specifically includes the following steps:

[0029] S401. Design: Design circuit graphics using CAD software;

[0030] S402. Graphic transfer:

[0031] Lamination: Lamination of dry film photoresist with circuit pattern on FR4 substrate layer, or use of laser direct imaging technology to generate pattern directly on FR4 substrate layer.

[0032] Exposure: Use ultraviolet light to expose the dry film photoresist through a mask to transfer the circuit pattern to the dry film photoresist.

[0033] Development: Use developer to dissolve the unexposed dry film photoresist, leaving the pattern of the circuit graphic;

[0034] S403. Graphic etching:

[0035] Stripping: Remove the residual dry film photoresist to expose the unnecessary copper foil layer;

[0036] Etching: Use an etchant to remove the copper foil layer that is not protected by the dry film photoresist, leaving only the circuit pattern;

[0037] Film removal: completely remove the remaining dry film photoresist and clean the circuit surface;

[0038] S404. Surface treatment: Surface treatment is performed as needed, such as nickel-gold immersion, organic solderability, silver immersion, tin immersion, etc., to enhance solderability and circuit protection.

[0039] Preferably, it also includes:

[0040] S8. Inspection and testing: Perform optical inspection to ensure there are no broken wires or short circuits, and perform electrical tests to confirm circuit continuity and performance;

[0041] S9. Finished product processing: Cutting, punching or V-cutting is performed as needed to form the final circuit board size.

[0042] Compared with the prior art, the present invention has the following beneficial effects:

[0043] (1) The present invention adds nanoparticles in a specific proportion to the FR4 substrate layer and forms a nanoparticle layer through dispersion strengthening, which is beneficial to improving the mechanical strength and thermal stability of the FR4 structure. In addition, by providing a copper-philic surface layer on the FR4 substrate layer, the adhesion to the copper foil is improved, the delamination phenomenon is reduced, and the reliability and service life of the FPC are improved;

[0044] (2) The present invention can increase the flexibility and mechanical strength of the FR4 structure by providing a reinforcement layer, and at the same time, by providing a protective film layer, it can increase the high temperature resistance of the FR4 structure, reduce the pollution of the FR4 structure during the processing, and improve the yield rate of the FPC;

[0045] (3) The method of the present invention includes FR4 substrate preparation, surface functionalization treatment, copper foil lamination, gluing, reinforcement, lamination and micro-hole drilling, so that the produced FPC has good mechanical strength and thermal stability, while reducing the delamination phenomenon, which is beneficial to improving the reliability and service life of the FPC. BRIEF DESCRIPTION OF THE DRAWINGS

[0046] Figure 1 It is a structural schematic diagram of the present invention;

[0047] Figure 2 It is a schematic diagram of the structure of the protective film of the present invention;

[0048] Figure 3 It is a flow chart of the present invention.

[0049] In the figure: 1, FR4 substrate layer; 2, nanoparticle layer; 3, copper-philic surface layer; 4, copper foil layer; 5, adhesive layer; 6, reinforcement layer; 7, protective film layer; 71, upper film layer; 72, middle film layer; 73, lower film layer; 74, release layer. DETAILED DESCRIPTION

[0050] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0051] Example 1

[0052] See also Figure 1-Figure 3 The present invention provides a technical solution: an FR4 structure, comprising an FR4 substrate layer 1, a nanoparticle layer 2 is uniformly arranged inside the FR4 substrate layer 1, a copper-philic surface layer 3 is arranged on the upper surface of the FR4 substrate layer 1, a copper foil layer 4 is arranged on the upper surface of the copper-philic surface layer 3, an adhesive layer 5 is arranged on the upper surface of the copper foil layer 4, a reinforcement layer 6 is arranged on the upper surface of the adhesive layer 5, and a protective film layer 7 is arranged on the upper surface of the reinforcement layer 6.

[0053] In this embodiment, preferably, the nanoparticle layer 2 is an aluminum oxide nanoparticle layer; and the reinforcement layer 6 is a steel plate layer.

[0054] In this embodiment, preferably, the protective film layer 7 includes an upper film layer 71, a middle film layer 72 and a lower film layer 73 which are pressed together from top to bottom, the upper film layer 71 and the lower film layer 73 are both PBT synthetic layers, a release layer 74 is provided on the outside of the upper film layer 71, and the upper film layer 71 and the lower film layer 73 are respectively bonded to the middle film layer 72 by polymer compound adhesive.

[0055] A FPC production process comprises the following steps:

[0056] S1. Preparation of FR4 substrate: Select nanoparticles with a moderate particle size, disperse the nanoparticles uniformly in an epoxy resin matrix by stirring and ultrasonic treatment, and then cure at a specific temperature to obtain a reinforced FR4 substrate layer 1;

[0057] S2. Surface functionalization treatment: Plasma treatment is performed on the FR4 substrate to activate the surface activity, and then a copper-philic surface layer is formed by chemical plating or nano-coating technology 3;

[0058] S3. Copper foil lamination: A high-precision laminating machine is used to tightly fit the copper foil on the copper-philic surface layer 3 to form a copper foil layer 4;

[0059] S4. Gluing: Using a glue coating machine, a layer of glue is applied on the surface of the copper foil layer 4 to form an adhesive layer 5;

[0060] S5 reinforcement: The reinforcement layer 6 is attached to the upper surface of the adhesive layer 5, and the reinforcement layer 6 and the adhesive layer 5 are pressed together by lamination;

[0061] S6. Lamination: Attach a protective film to the reinforcing plate, pre-press the protective film at low temperature and low pressure, so that the protective film wraps around the reinforcing layer 6, but the protective film does not contact the surface of the FR4 substrate, then apply force to both sides of the protective film extending from the edge of the reinforcing layer 6 in the horizontal direction, so that the protective film effectively shrinks toward the edge of the reinforcing layer 6, until there is no gap between the protective film and the reinforcing layer 6, the protective film fits the reinforcing layer 6 and wraps the reinforcing layer 6 tightly, and then presses and cures the protective film at high temperature and high pressure, so that the protective film is in close contact with the FR4 substrate, and the lamination is completed;

[0062] S7. Micro-hole drilling: Use laser ablation, chemical etching or molding technology to form micro-holes in the FR4 substrate layer 1 to balance mechanical strength and flexibility.

[0063] In this embodiment, preferably, the specific method for preparing the FR4 substrate in S1 includes:

[0064] S101. Pretreatment of nanoparticles: Surface modification of nanoparticles was performed at 20°C by chemically modifying the nanoparticles with a silane coupling agent or a surfactant for 4 hours;

[0065] S102. Dispersion of nanoparticles: The surface-modified nanoparticles were directly added to the epoxy resin, with a stirring speed of 500 rpm for 10 min to fully disperse the nanoparticles, and ultrasonic treatment was performed with an ultrasonic power of 100 W for 30 min;

[0066] S103. Mixing and curing: Mix the dispersed nanoparticles with epoxy resin and amine curing agent in a ratio of 1:300:100. After mixing, pour the mixture into a mold and enter the curing stage. The curing temperature is 25°C and the curing time is 72 hours to obtain a FR4 substrate.

[0067] In this embodiment, preferably, the pre-pressing conditions under low temperature and low pressure in S6 are temperature 70°C, pressure 40kg / cm2, pre-pressing time 5S, and molding time 10S; the high temperature and high pressure conditions are temperature 165°C, pressure 40kg / cm2, pre-pressing time 5S, and molding time 300S.

[0068] In this embodiment, preferably, the step S6 further includes preparing a protective film before laminating, which specifically includes the following steps:

[0069] S601. The raw materials of the upper film layer 71, the middle film layer 72 and the lower film layer 73 are mixed respectively;

[0070] S602. The raw material treated in S601 is subjected to a casting process to obtain each film layer;

[0071] S603. After the processing in S602, the film layers are pressed and shaped to obtain a semi-finished film;

[0072] S604. Cooling and winding the semi-finished film;

[0073] S605. The rolled semi-finished film is subjected to a aging treatment to obtain a finished film.

[0074] In this embodiment, preferably, the temperature of the casting process in 602 is 270°C, and the casting process includes extrusion operation of a screw extruder. During the extrusion operation of the screw extruder, the temperature is 270°C, the mold temperature is 50°C, and the screw aspect ratio is L / P=20; the shaping speed in 603 is 8m / min; the temperature of the aging treatment in 605 is 45°C, and the time is 5 days.

[0075] In this embodiment, preferably, after the copper foil lamination in S4, circuit production is also included, and the circuit production specifically includes the following steps:

[0076] S401. Design: Design circuit graphics using CAD software;

[0077] S402. Graphic transfer:

[0078] Lamination: Lamination of dry film photoresist with circuit pattern on FR4 substrate layer 1, or use of laser direct imaging technology to directly generate pattern on FR4 substrate layer 1.

[0079] Exposure: Use ultraviolet light to expose the dry film photoresist through a mask to transfer the circuit pattern to the dry film photoresist.

[0080] Development: Use developer to dissolve the unexposed dry film photoresist, leaving the pattern of the circuit graphic;

[0081] S403. Graphic etching:

[0082] Stripping: removing the residual dry film photoresist to expose the unnecessary copper foil layer 4;

[0083] Etching: Use an etchant to remove the copper foil layer 4 that is not protected by the dry film photoresist, leaving only the circuit pattern;

[0084] Film removal: completely remove the remaining dry film photoresist and clean the circuit surface;

[0085] S404. Surface treatment: Surface treatment is performed as needed, such as nickel-gold immersion, organic solderability, silver immersion, tin immersion, etc., to enhance solderability and circuit protection.

[0086] In this embodiment, preferably, it also includes:

[0087] S8. Inspection and testing: Perform optical inspection to ensure there are no broken wires or short circuits, and perform electrical tests to confirm circuit continuity and performance;

[0088] S9. Finished product processing: Cutting, punching or V-cutting is performed as needed to form the final circuit board size.

[0089] Example 2

[0090] See also Figure 1-Figure 3 The present invention provides a technical solution: an FR4 structure, comprising an FR4 substrate layer 1, a nanoparticle layer 2 is uniformly arranged inside the FR4 substrate layer 1, a copper-philic surface layer 3 is arranged on the upper surface of the FR4 substrate layer 1, a copper foil layer 4 is arranged on the upper surface of the copper-philic surface layer 3, an adhesive layer 5 is arranged on the upper surface of the copper foil layer 4, a reinforcement layer 6 is arranged on the upper surface of the adhesive layer 5, and a protective film layer 7 is arranged on the upper surface of the reinforcement layer 6.

[0091] In this embodiment, preferably, the nanoparticle layer 2 is a boron nitride nanoparticle layer; and the reinforcement layer 6 is configured as a steel plate layer.

[0092] In this embodiment, preferably, the protective film layer 7 includes an upper film layer 71, a middle film layer 72 and a lower film layer 73 which are pressed together from top to bottom, the upper film layer 71 and the lower film layer 73 are both PBT synthetic layers, a release layer 74 is provided on the outside of the upper film layer 71, and the upper film layer 71 and the lower film layer 73 are respectively bonded to the middle film layer 72 by polymer compound adhesive.

[0093] A FPC production process comprises the following steps:

[0094] S1. Preparation of FR4 substrate: Select nanoparticles with a moderate particle size, disperse the nanoparticles uniformly in an epoxy resin matrix by stirring and ultrasonic treatment, and then cure at a specific temperature to obtain a reinforced FR4 substrate layer 1;

[0095] S2. Surface functionalization treatment: Plasma treatment is performed on the FR4 substrate to activate the surface activity, and then a copper-philic surface layer is formed by chemical plating or nano-coating technology 3;

[0096] S3. Copper foil lamination: A high-precision laminating machine is used to tightly fit the copper foil on the copper-philic surface layer 3 to form a copper foil layer 4;

[0097] S4. Gluing: Using a glue coating machine, a layer of glue is applied on the surface of the copper foil layer 4 to form an adhesive layer 5;

[0098] S5 reinforcement: The reinforcement layer 6 is attached to the upper surface of the adhesive layer 5, and the reinforcement layer 6 and the adhesive layer 5 are pressed together by lamination;

[0099] S6. Lamination: Attach a protective film to the reinforcing plate, pre-press the protective film at low temperature and low pressure, so that the protective film wraps around the reinforcing layer 6, but the protective film does not contact the surface of the FR4 substrate, then apply force to both sides of the protective film extending from the edge of the reinforcing layer 6 in the horizontal direction, so that the protective film effectively shrinks toward the edge of the reinforcing layer 6, until there is no gap between the protective film and the reinforcing layer 6, the protective film fits the reinforcing layer 6 and wraps the reinforcing layer 6 tightly, and then presses and cures the protective film at high temperature and high pressure, so that the protective film is in close contact with the FR4 substrate, and the lamination is completed;

[0100] S7. Micro-hole drilling: Use laser ablation, chemical etching or molding technology to form micro-holes in the FR4 substrate layer 1 to balance mechanical strength and flexibility.

[0101] In this embodiment, preferably, the specific method for preparing the FR4 substrate in S1 includes:

[0102] S101. Pretreatment of nanoparticles: performing surface modification treatment on the nanoparticles at 80°C by chemically modifying the nanoparticles with a silane coupling agent or a surfactant for 18 hours;

[0103] S102. Dispersion of nanoparticles: The surface-modified nanoparticles were directly added to the epoxy resin, with a stirring speed of 2000 rpm for 80 min to fully disperse the nanoparticles, and ultrasonic treatment was performed with an ultrasonic power of 200 W for 60 min;

[0104] S103. Mixing and curing: The dispersed nanoparticles are mixed with epoxy resin and amine curing agent in a ratio of 1:500:200. After the mixing is completed, the mixture is poured into a mold and enters the curing stage. The curing temperature is 150°C and the curing time is 72 hours to obtain a FR4 substrate.

[0105] In this embodiment, preferably, the pre-pressing conditions under low temperature and low pressure in S6 are temperature 90°C, pressure 60kg / cm2, pre-pressing time 5S, and molding time 10S; the high temperature and high pressure conditions are temperature 185°C, pressure 60kg / cm2, pre-pressing time 5S, and molding time 300S.

[0106] In this embodiment, preferably, the step S6 further includes preparing a protective film before laminating, which specifically includes the following steps:

[0107] S601. The raw materials of the upper film layer 71, the middle film layer 72 and the lower film layer 73 are mixed respectively;

[0108] S602. The raw material treated in S601 is subjected to a casting process to obtain each film layer;

[0109] S603. After the processing in S602, the film layers are pressed and shaped to obtain a semi-finished film;

[0110] S604. Cooling and winding the semi-finished film;

[0111] S605. The rolled semi-finished film is subjected to a aging treatment to obtain a finished film.

[0112] In this embodiment, preferably, the temperature of the casting process in 602 is 290°C, and the casting process includes extrusion operation of a screw extruder. During the extrusion operation of the screw extruder, the temperature is 290°C, the mold temperature is 80°C, and the screw aspect ratio is L / P=20; the shaping speed in 603 is 12m / min; the temperature of the aging treatment in 605 is 60°C, and the time is 7 days.

[0113] In this embodiment, preferably, after the copper foil lamination in S4, circuit production is also included, and the circuit production specifically includes the following steps:

[0114] S401. Design: Design circuit graphics using CAD software;

[0115] S402. Graphic transfer:

[0116] Lamination: Lamination of dry film photoresist with circuit pattern on FR4 substrate layer 1, or use of laser direct imaging technology to directly generate pattern on FR4 substrate layer 1.

[0117] Exposure: Use ultraviolet light to expose the dry film photoresist through a mask to transfer the circuit pattern to the dry film photoresist.

[0118] Development: Use developer to dissolve the unexposed dry film photoresist, leaving the pattern of the circuit graphic;

[0119] S403. Graphic etching:

[0120] Stripping: removing the residual dry film photoresist to expose the unnecessary copper foil layer 4;

[0121] Etching: Use an etchant to remove the copper foil layer 4 that is not protected by the dry film photoresist, leaving only the circuit pattern;

[0122] Film removal: completely remove the remaining dry film photoresist and clean the circuit surface;

[0123] S404. Surface treatment: Surface treatment is performed as needed, such as nickel-gold immersion, organic solderability, silver immersion, tin immersion, etc., to enhance solderability and circuit protection.

[0124] In this embodiment, preferably, it also includes:

[0125] S8. Inspection and testing: Perform optical inspection to ensure there are no broken wires or short circuits, and perform electrical tests to confirm circuit continuity and performance;

[0126] S9. Finished product processing: Cutting, punching or V-cutting is performed as needed to form the final circuit board size.

[0127] Example 3

[0128] See also Figure 1-Figure 3 The present invention provides a technical solution: an FR4 structure, comprising an FR4 substrate layer 1, a nanoparticle layer 2 is uniformly arranged inside the FR4 substrate layer 1, a copper-philic surface layer 3 is arranged on the upper surface of the FR4 substrate layer 1, a copper foil layer 4 is arranged on the upper surface of the copper-philic surface layer 3, an adhesive layer 5 is arranged on the upper surface of the copper foil layer 4, a reinforcement layer 6 is arranged on the upper surface of the adhesive layer 5, and a protective film layer 7 is arranged on the upper surface of the reinforcement layer 6.

[0129] In this embodiment, preferably, the nanoparticle layer 2 is a carbon nanotube layer; and the reinforcement layer 6 is a steel plate layer.

[0130] In this embodiment, preferably, the protective film layer 7 includes an upper film layer 71, a middle film layer 72 and a lower film layer 73 which are pressed together from top to bottom, the upper film layer 71 and the lower film layer 73 are both PBT synthetic layers, a release layer 74 is provided on the outside of the upper film layer 71, and the upper film layer 71 and the lower film layer 73 are respectively bonded to the middle film layer 72 by polymer compound adhesive.

[0131] A FPC production process comprises the following steps:

[0132] S1. Preparation of FR4 substrate: Select nanoparticles with a moderate particle size, disperse the nanoparticles uniformly in an epoxy resin matrix by stirring and ultrasonic treatment, and then cure at a specific temperature to obtain a reinforced FR4 substrate layer 1;

[0133] S2. Surface functionalization treatment: Plasma treatment is performed on the FR4 substrate to activate the surface activity, and then a copper-philic surface layer is formed by chemical plating or nano-coating technology 3;

[0134] S3. Copper foil lamination: A high-precision laminating machine is used to tightly fit the copper foil on the copper-philic surface layer 3 to form a copper foil layer 4;

[0135] S4. Gluing: Using a glue coating machine, a layer of glue is applied on the surface of the copper foil layer 4 to form an adhesive layer 5;

[0136] S5 reinforcement: The reinforcement layer 6 is attached to the upper surface of the adhesive layer 5, and the reinforcement layer 6 and the adhesive layer 5 are pressed together by lamination;

[0137] S6. Lamination: Attach a protective film to the reinforcing plate, pre-press the protective film at low temperature and low pressure, so that the protective film wraps around the reinforcing layer 6, but the protective film does not contact the surface of the FR4 substrate, then apply force to both sides of the protective film extending from the edge of the reinforcing layer 6 in the horizontal direction, so that the protective film effectively shrinks toward the edge of the reinforcing layer 6, until there is no gap between the protective film and the reinforcing layer 6, the protective film fits the reinforcing layer 6 and wraps the reinforcing layer 6 tightly, and then presses and cures the protective film at high temperature and high pressure, so that the protective film is in close contact with the FR4 substrate, and the lamination is completed;

[0138] S7. Micro-hole drilling: Use laser ablation, chemical etching or molding technology to form micro-holes in the FR4 substrate layer 1 to balance mechanical strength and flexibility.

[0139] In this embodiment, preferably, the specific method for preparing the FR4 substrate in S1 includes:

[0140] S101. Pretreatment of nanoparticles: performing surface modification treatment on the nanoparticles at 60°C by chemically modifying the nanoparticles with a silane coupling agent or a surfactant for 8 hours;

[0141] S102. Dispersion of nanoparticles: The surface-modified nanoparticles were directly added to the epoxy resin, with a stirring speed of 1000 rpm for 40 min to fully disperse the nanoparticles, and ultrasonic treatment was performed with an ultrasonic power of 150 W for 40 min;

[0142] S103. Mixing and curing: Mix the dispersed nanoparticles with epoxy resin and amine curing agent in a ratio of 1:400:150. After mixing, pour the mixture into a mold and enter the curing stage. The curing temperature is 70°C and the curing time is 8 hours to obtain a FR4 substrate.

[0143] In this embodiment, preferably, the pre-pressing conditions under low temperature and low pressure in S6 are temperature 80°C, pressure 50kg / cm2, pre-pressing time 5S, and molding time 10S; the high temperature and high pressure conditions are temperature 175°C, pressure 50kg / cm2, pre-pressing time 5S, and molding time 300S.

[0144] In this embodiment, preferably, the step S6 further includes preparing a protective film before laminating, which specifically includes the following steps:

[0145] S601. The raw materials of the upper film layer 71, the middle film layer 72 and the lower film layer 73 are mixed respectively;

[0146] S602. The raw material treated in S601 is subjected to a casting process to obtain each film layer;

[0147] S603. After the processing in S602, the film layers are pressed and shaped to obtain a semi-finished film;

[0148] S604. Cooling and winding the semi-finished film;

[0149] S605. The rolled semi-finished film is subjected to a aging treatment to obtain a finished film.

[0150] In this embodiment, preferably, the temperature of the casting process in 602 is 280°C, and the casting process includes extrusion operation of a screw extruder. During the extrusion operation of the screw extruder, the temperature is 280°C, the mold temperature is 60°C, and the screw aspect ratio is L / P=20; the shaping speed in 603 is 10m / min; the temperature of the aging treatment in 605 is 50°C, and the time is 6 days.

[0151] In this embodiment, preferably, after the copper foil lamination in S4, circuit production is also included, and the circuit production specifically includes the following steps:

[0152] S401. Design: Design circuit graphics using CAD software;

[0153] S402. Graphic transfer:

[0154] Lamination: Lamination of dry film photoresist with circuit pattern on FR4 substrate layer 1, or use of laser direct imaging technology to directly generate pattern on FR4 substrate layer 1.

[0155] Exposure: Use ultraviolet light to expose the dry film photoresist through a mask to transfer the circuit pattern to the dry film photoresist.

[0156] Development: Use developer to dissolve the unexposed dry film photoresist, leaving the pattern of the circuit graphic;

[0157] S403. Graphic etching:

[0158] Stripping: removing the residual dry film photoresist to expose the unnecessary copper foil layer 4;

[0159] Etching: Use an etchant to remove the copper foil layer 4 that is not protected by the dry film photoresist, leaving only the circuit pattern;

[0160] Film removal: completely remove the remaining dry film photoresist and clean the circuit surface;

[0161] S404. Surface treatment: Surface treatment is performed as needed, such as nickel-gold immersion, organic solderability, silver immersion, tin immersion, etc., to enhance solderability and circuit protection.

[0162] In this embodiment, preferably, it also includes:

[0163] S8. Inspection and testing: Perform optical inspection to ensure there are no broken wires or short circuits, and perform electrical tests to confirm circuit continuity and performance;

[0164] S9. Finished product processing: Cutting, punching or V-cutting is performed as needed to form the final circuit board size.

[0165] Principles and advantages of the present invention:

[0166] The present invention forms a nanoparticle layer 2 by adding a specific proportion of nanoparticles to the FR4 substrate layer 1 and through the dispersion strengthening effect, which is beneficial to improving the mechanical strength and thermal stability of the FR4 structure. In addition, by arranging a copper-philic surface layer 3 on the FR4 substrate layer 1, the adhesion to the copper foil is improved, the delamination phenomenon is reduced, and the reliability and service life of the FPC are improved; by arranging the reinforcement layer 6, the flexibility and mechanical strength of the FR4 structure can be increased; and by arranging the protective film layer 7, the high temperature resistance of the FR4 structure can be increased, the pollution of the FR4 structure during the processing process is reduced, and the yield rate of the FPC is improved;

[0167] The method of the present invention enables the produced FPC to have good mechanical strength and thermal stability through FR4 substrate preparation, surface functionalization treatment, copper foil lamination, gluing, reinforcement, lamination and micro-hole drilling, while reducing the delamination phenomenon, which is beneficial to improving the reliability and service life of the FPC.

[0168] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A FR4 structure, characterized in that: The invention comprises an FR4 substrate layer (1), a nanoparticle layer (2) is uniformly arranged inside the FR4 substrate layer (1), a copper-philic surface layer (3) is arranged on the upper surface of the FR4 substrate layer (1), a copper foil layer (4) is arranged on the upper surface of the copper-philic surface layer (3), an adhesive layer (5) is arranged on the upper surface of the copper foil layer (4), a reinforcing layer (6) is arranged on the upper surface of the adhesive layer (5), and a protective film layer (7) is arranged on the upper surface of the reinforcing layer (6).

2. The FR4 structure according to claim 1, characterized in that: The nanoparticle layer (2) is one of an aluminum oxide nanoparticle layer, a boron nitride nanoparticle layer, a carbon nanotube layer, a graphene layer and a silicon dioxide nanoparticle layer; and the reinforcement layer (6) is configured as a steel plate layer.

3. The FR4 structure according to claim 1, characterized in that: The protective film layer (7) comprises an upper film layer (71), a middle film layer (72) and a lower film layer (73) which are laminated together. The upper film layer (71) and the lower film layer (73) are both PBT synthetic layers. A release layer (74) is provided on the outside of the upper film layer (71). The upper film layer (71) and the lower film layer (73) are respectively bonded to the middle film layer (72) by polymer adhesive.

4. A FPC production process, characterized in that: The following steps are involved: S1. Preparation of FR4 substrate: Select nanoparticles with a moderate particle size, disperse the nanoparticles uniformly in an epoxy resin matrix by stirring and ultrasonic treatment, and then cure at a specific temperature to obtain a reinforced FR4 substrate layer (1); S2. Surface functionalization treatment: Plasma treatment of the FR4 substrate to activate the surface activity, and then chemical plating or nano-coating technology to form a copper-philic surface layer (3); S3. Copper foil lamination: using a high-precision laminating machine, the copper foil is closely attached to the copper-philic surface layer (3) to form a copper foil layer (4); S4. Gluing: Using a glue coating machine, a layer of glue is applied on the surface of the copper foil layer (4) to form an adhesive layer (5); S5. Reinforcement: The reinforcing layer (6) is attached to the upper surface of the adhesive layer (5), and the reinforcing layer (6) and the adhesive layer (5) are pressed tightly by lamination; S6. Lamination: A protective film is attached to the reinforcing plate, and the protective film is pre-pressed at low temperature and low pressure so that the protective film wraps around the reinforcing layer (6) but does not contact the surface of the FR4 substrate. Then, force is applied to both sides of the protective film extending from the edge of the reinforcing layer (6) in the horizontal direction so that the protective film effectively shrinks toward the edge of the reinforcing layer (6) until there is no gap between the protective film and the reinforcing layer (6). The protective film fits the reinforcing layer (6) and wraps the reinforcing layer (6). Then, the protective film is pressed and cured at high temperature and high pressure so that the protective film is in close contact with the FR4 substrate, and the lamination is completed. S7. Micro-hole drilling: Micro-holes are formed in the FR4 substrate layer (1) using laser ablation, chemical etching or compression molding technology to balance mechanical strength and flexibility.

5. The FPC production process according to claim 4, characterized in that: The specific method for preparing the FR4 substrate in S1 includes: S101. Pretreatment of nanoparticles: performing surface modification treatment on the nanoparticles at a temperature between 20 and 80° C. by chemically modifying the nanoparticles with a silane coupling agent or a surfactant for 4 to 18 hours; S102. Dispersion of nanoparticles: The surface-modified nanoparticles are directly added to the epoxy resin, the stirring speed is 500-2000 rpm, the stirring time is 10-80 min, the nanoparticles are fully dispersed, and ultrasonic treatment is performed at an ultrasonic power of 100-200 W for 30-60 min; S103. Mixing and curing: Mix the dispersed nanoparticles with epoxy resin and amine curing agent in a ratio of 1:300-500:100-200. After mixing, pour the mixture into a mold and enter the curing stage. The curing temperature is 25-150°C and the curing time is 2-72h to obtain a FR4 substrate.

6. The FPC production process according to claim 4, characterized in that: The pre-pressing conditions under low temperature and low pressure in S6 are temperature 80±10℃, pressure 50±10kg / cm2, pre-pressing time 5S, and molding time 10S; the high temperature and high pressure conditions are temperature 175±10℃, pressure 50±10kg / cm2, pre-pressing time 5S, and molding time 300S.

7. The FPC production process according to claim 4, characterized in that: The step S6 also includes preparing a protective film before laminating, which specifically includes the following steps: S601. The raw materials of the upper film layer (71), the middle film layer (72) and the lower film layer (73) are mixed respectively; S602. The raw material treated in S601 is subjected to a casting process to obtain each film layer; S603. After the processing in S602, the film layers are pressed and shaped to obtain a semi-finished film; S604. Cooling and winding the semi-finished film; S605. The rolled semi-finished film is subjected to a aging treatment to obtain a finished film.

8. The FPC production process according to claim 7, characterized in that: The temperature of the casting process in 602 is 270°C-290°C, and the casting process includes extrusion operation of a screw extruder. During the extrusion operation of the screw extruder, the temperature is 270°C-290°C, the mold temperature is 50-80°C, and the screw aspect ratio is L / P=20; the shaping speed in 603 is 8-12m / min; the temperature of the aging treatment in 605 is 45°C-60°C, and the time is 5-7 days.

9. The FPC production process according to claim 4, characterized in that: The circuit manufacturing step further includes circuit manufacturing after the copper foil lamination in S4, and the circuit manufacturing step specifically includes the following steps: S401. Design: Design circuit graphics using CAD software; S402. Graphic transfer: Laminating: Laminating a dry film photoresist with a circuit pattern on the FR4 substrate layer (1), or using laser direct imaging technology to directly generate a pattern on the FR4 substrate layer (1). Exposure: Use ultraviolet light to expose the dry film photoresist through a mask to transfer the circuit pattern to the dry film photoresist. Development: Use developer to dissolve the unexposed dry film photoresist, leaving the pattern of the circuit graphic; S403. Graphic etching: Stripping: removing the residual dry film photoresist to expose the unnecessary copper foil layer (4); Etching: using an etchant to remove the copper foil layer (4) not protected by the dry film photoresist, leaving only the circuit pattern; Film removal: completely remove the remaining dry film photoresist and clean the circuit surface; S404. Surface treatment: Surface treatment is performed as needed, such as nickel-gold immersion, organic solderability, silver immersion, tin immersion, etc., to enhance solderability and circuit protection.

10. The FPC production process according to claim 4, characterized in that: Also includes: S8. Inspection and testing: Perform optical inspection to ensure there are no broken wires or short circuits, and perform electrical tests to confirm circuit continuity and performance; S9. Finished product processing: Cutting, punching or V-cutting is performed as needed to form the final circuit board size.