Cover film NTC bonding pad windowing design structure and production process
The window opening cavity of the cover film is filled by silicone rubber protection method to prevent etching of the etching liquid, and solve the problem of easy breaking of the wire caused by the complex process of the existing pad window opening structure, realize the integrity of the wire and the simplicity of the process, and reduce the cost.
Patent Information
- Application Number
- CN202410989334.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-15
AI Technical Summary
The existing pad window opening structure is complex, and the immersion of the etching liquid can easily cause the line to be etched, the wires are easily broken, and the product reliability is not high.
The silicone rubber protection method is used to fill the silicone rubber into the window opening cavity of the covering film to prevent etching of the etching liquid, and the process flow is simplified by laser cutting and lamination fixing technology.
Ensure conductor integrity, simplify process flow, reduce costs, and improve product reliability.
Smart Images

Figure CN118973134A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of circuit board processing, and in particular to a cover film NTC pad window design structure and a production process. Background Art
[0002] The solder mask layer refers to the part of the printed circuit board that needs to be covered with green ink. In fact, this solder mask layer uses a negative film output, so after the shape of the solder mask layer is mapped to the board, it is not the green solder mask that is applied, but the copper skin is exposed. The pad opening refers to the size of the copper exposed at the location where soldering is required, that is, the size of the part not covered with ink.
[0003] The existing Chinese patent with publication number CN109688700A discloses a solder resist window design for a PCB pad, including a PCB board as a substrate for carrying the pad and a PCB board that needs to be welded or tested. The pad has a solder resist window corresponding to it, the minimum width of the pad is greater than 0.2mm, the solder resist window of the pad is smaller than the pad and the reduction on one side is not less than the alignment deviation value, and the solder resist thickness is less than 20um.
[0004] The existing window structure process is complicated, and the immersion of etching solution will cause the circuit to be etched. In the subsequent use process, the same wire is easy to be broken here, and the product reliability is not high. Summary of the invention
[0005] In view of the problems mentioned in the background technology, the purpose of the present invention is to provide a cover film NTC pad window design structure and production process to solve the problems mentioned in the background technology.
[0006] The above technical objectives of the present invention are achieved through the following technical solutions:
[0007] A cover film NTC pad window design structure comprises a single-sided flexible printed circuit board, wherein the single-sided flexible printed circuit board comprises a top cover film, an intermediate metal layer and a bottom cover film in sequence, and the intermediate metal layer is a hollow copper plate.
[0008] Preferably, the top cover film and the bottom cover film are one of polyimide, polyurea and polyamide.
[0009] Preferably, the bottom cover film is coated with an antifouling coating on a side facing away from the middle metal layer, and the antifouling coating is a polytetrafluoroethylene coating.
[0010] The present invention also discloses a production process of a cover film NTC pad window design structure, comprising the following steps:
[0011] S1. Cutting the bottom cover film: After placing the bottom cover film on the fixture, use a laser cutting machine to cut it at the window opening position;
[0012] S2, laminated copper foil: the copper foil is fixed on the bottom cover film by lamination fixing method;
[0013] S3, Silicone rubber protection: Place the bottom cover film in the silicone rubber tray so that the window opening position is filled and protected by silicone rubber;
[0014] S4, dry film protection: paste dry film on the non-etching area of the copper foil for protection, and control the area between the dry films as the etching area;
[0015] S5, etching: pouring etching liquid on top of the copper foil;
[0016] S6, removing dry film: after cleaning the etched copper foil, remove the dry film;
[0017] S7, pasting the top cover film: attaching the top cover film after laser cutting to the surface of the etched copper foil.
[0018] Preferably, when S2 fixes the copper foil on the bottom cover film by lamination, the temperature of the pressing and fixing is controlled to be 60-75° C., and the pressing and fixing time is controlled to be 30-40 minutes.
[0019] Preferably, when S3 is protected by silicone rubber, the bottom covering film is placed in a silicone rubber tray so that the window position is filled and protected by silicone rubber. During the silicone rubber filling process, the temperature of the silicone rubber is controlled to be 40-50°C, and the downward pressure of the copper foil is controlled to be 500-600Pa.
[0020] Preferably, when etching in S5, the etching liquid used comprises the following components by mass: 20% peroxide, 0.04% fluorine source, and the remainder inorganic acid; etching temperature: 30-40°C.
[0021] Preferably, when S6 removes the dry film and cleans the etched copper foil, it is first cleaned with an alcohol solution with a concentration of 50-60%, then cleaned twice with deionized water, and then dried in a dryer at 60-70°C.
[0022] In summary, the present invention mainly has the following beneficial effects:
[0023] The present invention adopts a silicone rubber protection method to produce a wire of a desired width, and the silicone rubber is completely filled into the window cavity of the covering film, which can block the solution from corroding the wire during etching and ensure the integrity of the wire; and the present invention has a simple structure, a concise process flow and a low cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a processing schematic diagram of the present invention;
[0025] Figure 2 It is a flow chart of the present invention. DETAILED DESCRIPTION
[0026] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0027] Example 1
[0028] refer to Figure 1 and Figure 2 A cover film NTC pad window design structure includes a single-sided flexible printed circuit board, which includes a top cover film, an intermediate metal layer and a bottom cover film in sequence, and the intermediate metal layer is a hollow copper plate.
[0029] Wherein, the top cover film and the bottom cover film are one of polyimide, polyurea and polyamide.
[0030] Wherein, the bottom covering film is coated with an antifouling coating on a side away from the middle metal layer, and the antifouling coating is a polytetrafluoroethylene coating.
[0031] This embodiment also discloses a production process of a cover film NTC pad window design structure, including the following steps:
[0032] S1. Cutting the bottom cover film: After placing the bottom cover film on the fixture, use a laser cutting machine to cut it at the window opening position;
[0033] S2, laminated copper foil: the copper foil is fixed on the bottom cover film by lamination fixing method;
[0034] S3, Silicone rubber protection: Place the bottom cover film in the silicone rubber tray so that the window opening position is filled and protected by silicone rubber;
[0035] S4, dry film protection: paste dry film on the non-etching area of the copper foil for protection, and control the area between the dry films as the etching area;
[0036] S5, etching: pouring etching liquid on top of the copper foil;
[0037] S6, removing dry film: after cleaning the etched copper foil, remove the dry film;
[0038] S7, pasting the top cover film: attaching the top cover film after laser cutting to the surface of the etched copper foil.
[0039] Wherein, when S2 fixes the copper foil on the bottom cover film by lamination fixing, the pressing and fixing temperature is controlled to be 60° C. and the pressing and fixing time is controlled to be 30 minutes.
[0040] Among them, when S3 is protected by silicone rubber, the bottom covering film is placed in the silicone rubber tray so that the window position is filled and protected by silicone rubber. During the silicone rubber filling process, the temperature of the silicone rubber is controlled to be 40-50°C, and the downward pressure of the copper foil is controlled to be 500Pa.
[0041] When etching in S5, the etching liquid used includes the following components by mass: 20% peroxide, 0.04% fluorine source, and the rest is inorganic acid; etching temperature: 30°C.
[0042] Among them, when S6 removes the dry film, when cleaning the etched copper foil, it is first cleaned with an alcohol solution with a concentration of 50-60%, then cleaned twice with deionized water, and then dried at 60-70°C using a dryer.
[0043] Among them, the present invention adopts the silicone rubber protection method to produce wires of required width, and the silicone rubber is completely filled into the window cavity of the covering film, which can block the solution from corroding the wire during etching and ensure the integrity of the wire; and the present invention has a simple structure, a concise process flow and a low cost.
[0044] Example 2
[0045] refer to Figure 1 and Figure 2 A cover film NTC pad window design structure includes a single-sided flexible printed circuit board, which includes a top cover film, an intermediate metal layer and a bottom cover film in sequence, and the intermediate metal layer is a hollow copper plate.
[0046] Wherein, the top cover film and the bottom cover film are one of polyimide, polyurea and polyamide.
[0047] Wherein, the bottom covering film is coated with an antifouling coating on a side away from the middle metal layer, and the antifouling coating is a polytetrafluoroethylene coating.
[0048] This embodiment also discloses a production process of a cover film NTC pad window design structure, including the following steps:
[0049] S1. Cutting the bottom cover film: After placing the bottom cover film on the fixture, use a laser cutting machine to cut it at the window opening position;
[0050] S2, laminated copper foil: the copper foil is fixed on the bottom cover film by lamination fixing method;
[0051] S3, Silicone rubber protection: Place the bottom cover film in the silicone rubber tray so that the window opening position is filled and protected by silicone rubber;
[0052] S4, dry film protection: paste dry film on the non-etching area of the copper foil for protection, and control the area between the dry films as the etching area;
[0053] S5, etching: pouring etching liquid on top of the copper foil;
[0054] S6, removing dry film: after cleaning the etched copper foil, remove the dry film;
[0055] S7, pasting the top cover film: attaching the top cover film after laser cutting to the surface of the etched copper foil.
[0056] Wherein, when S2 fixes the copper foil on the bottom cover film by lamination fixing, the pressing and fixing temperature is controlled to be 75° C. and the pressing and fixing time is 40 minutes.
[0057] Among them, when S3 is protected by silicone rubber, the bottom covering film is placed in the silicone rubber tray so that the window position is filled and protected by silicone rubber. During the silicone rubber filling process, the temperature of the silicone rubber is controlled to be 50°C, and the downward pressure of the copper foil is controlled to be 560Pa.
[0058] When etching in S5, the etching liquid used includes the following components by mass: 20% peroxide, 0.04% fluorine source, and the rest is inorganic acid; etching temperature: 35°C.
[0059] Among them, when S6 removes the dry film, when cleaning the etched copper foil, it is first cleaned with an alcohol solution with a concentration of 50-60%, then cleaned twice with deionized water, and then dried at 60-70°C using a dryer.
[0060] Among them, the present invention adopts the silicone rubber protection method to produce wires of required width, and the silicone rubber is completely filled into the window cavity of the covering film, which can block the solution from corroding the wire during etching and ensure the integrity of the wire; and the present invention has a simple structure, a concise process flow and a low cost.
[0061] Example 3
[0062] refer to Figure 1 and Figure 2 A cover film NTC pad window design structure includes a single-sided flexible printed circuit board, which includes a top cover film, an intermediate metal layer and a bottom cover film in sequence, and the intermediate metal layer is a hollow copper plate.
[0063] Wherein, the top cover film and the bottom cover film are one of polyimide, polyurea and polyamide.
[0064] Wherein, the bottom covering film is coated with an antifouling coating on a side away from the middle metal layer, and the antifouling coating is a polytetrafluoroethylene coating.
[0065] This embodiment also discloses a production process of a cover film NTC pad window design structure, including the following steps:
[0066] S1. Cutting the bottom cover film: After placing the bottom cover film on the fixture, use a laser cutting machine to cut it at the window opening position;
[0067] S2, laminated copper foil: the copper foil is fixed on the bottom cover film by lamination fixing method;
[0068] S3, Silicone rubber protection: Place the bottom cover film in the silicone rubber tray so that the window opening position is filled and protected by silicone rubber;
[0069] S4, dry film protection: paste dry film on the non-etching area of the copper foil for protection, and control the area between the dry films as the etching area;
[0070] S5, etching: pouring etching liquid on top of the copper foil;
[0071] S6, removing dry film: after cleaning the etched copper foil, remove the dry film;
[0072] S7, pasting the top cover film: attaching the top cover film after laser cutting to the surface of the etched copper foil.
[0073] Wherein, when S2 fixes the copper foil on the bottom cover film by lamination fixing, the pressing and fixing temperature is controlled to be 75° C. and the pressing and fixing time is 40 minutes.
[0074] Among them, when S3 is protected by silicone rubber, the bottom covering film is placed in the silicone rubber tray so that the window position is filled and protected by silicone rubber. During the silicone rubber filling process, the temperature of the silicone rubber is controlled to be 40-50°C, and the downward pressure of the copper foil is controlled to be 600Pa.
[0075] When etching in S5, the etching liquid used includes the following components by mass: 20% peroxide, 0.04% fluorine source, and the rest is inorganic acid; etching temperature: 40°C.
[0076] Among them, when S6 removes the dry film, when cleaning the etched copper foil, it is first cleaned with an alcohol solution with a concentration of 50-60%, then cleaned twice with deionized water, and then dried at 60-70°C using a dryer.
[0077] Among them, the present invention adopts the silicone rubber protection method to produce wires of required width, and the silicone rubber is completely filled into the window cavity of the covering film, which can block the solution from corroding the wire during etching and ensure the integrity of the wire; and the present invention has a simple structure, a concise process flow and a low cost.
[0078] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A cover film NTC pad window design structure, characterized in that: The single-sided flexible printed circuit board comprises a top-layer covering film, an intermediate metal layer and a bottom-layer covering film in sequence, and the intermediate metal layer is a hollow copper plate.
2. A cover film NTC pad window design structure according to claim 1, characterized in that: The top cover film and the bottom cover film are one of polyimide, polyurea and polyamide.
3. A cover film NTC pad window design structure according to claim 1, characterized in that: The bottom cover film is coated with an antifouling coating on a side away from the middle metal layer, and the antifouling coating is a polytetrafluoroethylene coating.
4. A production process for a cover film NTC pad window design structure, characterized in that: The following steps are involved: S1. Cutting the bottom cover film: After placing the bottom cover film on the fixture, use a laser cutting machine to cut it at the window opening position; S2, laminated copper foil: the copper foil is fixed on the bottom cover film by lamination fixing method; S3, Silicone rubber protection: Place the bottom cover film in the silicone rubber tray so that the window opening position is filled and protected by silicone rubber; S4, dry film protection: paste dry film on the non-etching area of the copper foil for protection, and control the area between the dry films as the etching area; S5, etching: pouring etching liquid on top of the copper foil; S6, removing dry film: after cleaning the etched copper foil, remove the dry film; S7, pasting the top cover film: attaching the top cover film after laser cutting to the surface of the etched copper foil.
5. The production process of a cover film NTC pad window design structure according to claim 4, characterized in that: When the S2 uses a lamination fixing method to fix the copper foil on the bottom cover film, the pressing and fixing temperature is controlled to be 60-75° C. and the pressing and fixing time is 30-40 minutes.
6. The production process of a cover film NTC pad window design structure according to claim 4, characterized in that: When S3 is protected by silicone rubber, the bottom covering film is placed in the silicone rubber tray so that the window position is filled and protected by silicone rubber. During the silicone rubber filling process, the temperature of the silicone rubber is controlled to be 40-50°C, and the downward pressure of the copper foil is controlled to be 500-600Pa.
7. The production process of a cover film NTC pad window design structure according to claim 1, characterized in that: When etching in S5, the etching liquid used includes the following components by mass: 20% peroxide, 0.04% fluorine source, and the rest is inorganic acid; etching temperature: 30-40°C.
8. The production process of a cover film NTC pad window design structure according to claim 1, characterized in that: When the S6 is used to remove the dry film, the etched copper foil is cleaned by first using an alcohol solution with a concentration of 50-60%, then washing it twice with deionized water, and then drying it at 60-70° C. using a dryer.
Citation Information
Patent Citations
Solder mask opening design for PCB bonding pad
CN109688700A