Processing method for manufacturing micro PCB laser blind hole at low cost
By forming a multi-layer structure on the copper clad plate, using laser laser technology to form inverted trapezoidal blind holes and performing hole filling electroplating, the problem of difficulty in processing micro blind holes in the existing technology is solved, and low-cost micro PCB blind hole processing is achieved. Improves the production capacity and product density of the factory.
Patent Information
- Application Number
- CN202411086996.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing CO2 laser laser drilling machines are difficult to process tiny blind holes of 50um or less, resulting in the need to purchase high-priced equipment, which limits the factory's advanced product development.
Using a low-cost method, the formation of multi-layer structures on the copper clad plate is carried out, and the inverted trapezoidal blind holes are formed using laser laser technology to penetrate the dry film, and the conductive connection is completed through hole filling electroplating, which improves the production capacity of the blind holes.
The blind hole processing of micro PCBs with a pore size of less than 50μm is realized, which reduces the cost of equipment investment and improves the wiring density and processing efficiency of the printed circuit board.
Smart Images

Figure CN118973140A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of PCB processing, and in particular to a processing method for manufacturing tiny PCB laser blind holes at low cost. Background Art
[0002] With the development of electronic products, they are becoming thinner and denser. The number of components that need to be implanted in printed circuit boards is also constantly decreasing and increasing. As a result, when designing printed circuit boards, it is necessary to increase the wiring density per unit area. HDI products with small holes and fine lines are becoming more and more common, and the level of sophistication is constantly improving.
[0003] For laser micro blind holes, conventional CO2 laser drilling machines can generally stably process 100um laser blind holes. If you need to complete micro blind holes with a diameter of less than 100um, or even 50um and below, the processing capacity of conventional CO2 laser drilling machines can no longer meet the requirements due to the limitation of the CO2 laser beam diameter capacity. You need to purchase very expensive advanced CO2 laser drilling machines, or even UV laser drilling machines. This high investment limits the opportunities for many factories to develop high-end products;
[0004] To this end, the present invention proposes a process method for miniaturizing blind vias without the need for new equipment investment, thereby achieving the purpose of improving the blind via manufacturing capability and increasing the wiring density of printed circuit board products. Summary of the invention
[0005] In view of the deficiencies of the prior art, the present invention provides a low-cost processing method for manufacturing tiny PCB laser blind holes, which solves the problems raised in the background technology.
[0006] To achieve the above objectives, the present invention is implemented by the following technical solutions: a low-cost processing method for making tiny PCB laser blind holes, the steps of which are as follows:
[0007] S1. Feeding, wherein at least one layer of copper clad laminate (CCL) is used as the core layer material, and the CCL is composed of a reinforcing material such as glass fiber cloth and at least one side of copper foil;
[0008] S2. Inner layer circuit production, complete the production of inner layer graphics according to circuit design requirements, including cutting, pre-processing, film pasting, exposure, development, etching and film stripping to form the required circuit pattern;
[0009] S3. Lamination: Use a vacuum laminator to press and cure the multi-layer inner layer circuit board. The material package used for lamination is one of ABF, CBF or NBF build-up dielectric films;
[0010] S4. Lamination: After lamination, a layer of dry film with a certain thickness is pressed on the product to protect the copper layer and prepare for subsequent steps;
[0011] S5. Laser drilling, using laser technology to penetrate the dry film and form blind holes on the underlying copper foil. The laser drilling process adjusts the laser parameters according to the hole size to ensure the quality of the hole;
[0012] S6. De-filming: using a film stripping process to remove the dry film on the surface to prepare for the subsequent electroplating steps;
[0013] S7. Copper deposition and hole-filling electroplating: first, the glue removal process is carried out, and then a copper layer is deposited on the hole wall to achieve hole metallization, and the blind hole is filled by hole-filling electroplating to complete the conductive connection of the circuit board.
[0014] Preferably, the inner layer circuit manufacturing method in step S2 is:
[0015] Cutting: Cut the CCL into a size suitable for processing and subsequent use according to design requirements; the cutting process needs to ensure the accuracy of the size to avoid affecting the assembly and function of the circuit board due to size errors;
[0016] Pretreatment: Clean the surface of CCL to remove oil, dust and other pollutants to ensure that the dry film can be evenly coated and firmly attached to the CCL;
[0017] Film lamination: a layer of photoresist dry film is evenly coated on the surface of CCL, and the thickness of the dry film is controlled within 5μm-20μm according to the process requirements;
[0018] Among them, the function of the dry film is to protect the copper layer that does not need to be etched during the subsequent exposure and development process;
[0019] Exposure: Use image transfer technology to transfer the circuit pattern to the dry film through UV light; precise alignment during the operation ensures the accuracy and integrity of the circuit pattern;
[0020] Development: Use a specific chemical solution in the developing tank to dissolve the dry film in the unexposed area to form grooves for the circuit pattern; precisely control the temperature, speed, and pressure parameters during the development process;
[0021] Etching: Use chemical or mechanical methods to remove the copper foil that is not protected by the dry film to form the desired circuit pattern;
[0022] Among them, the composition, concentration, temperature and etching speed of the etching solution need to be precisely controlled;
[0023] Stripping: Remove the dry film on the formed circuit pattern to prepare for subsequent steps such as copper deposition and electroplating; the stripping process uses a high concentration of sodium hydroxide solution to ensure that the dry film is completely removed.
[0024] Preferably, the etching solution is composed of one of acidic copper chloride, alkaline copper chloride, ferric chloride, ammonium persulfate, sulfuric acid / chromic acid, and sulfuric acid / hydrogen peroxide, wherein the concentration of the alkaline copper chloride etching solution is controlled within the range of 135-165g / L, and the etching is controlled at 45-55°C, wherein the pH value of the alkaline copper chloride etching solution should be maintained at 8.0-8.8, and the temperature is controlled at 45-55°C. Preferably, in S3, during the lamination process, it is necessary to punch the target hole, browning treatment, and punching of the PP sheet (Prepreg), wherein the browning treatment is to activate the copper surface to increase the contact surface area with the resin and ensure reliable bonding of the lamination; then, the lamination is performed, and the inner layer board and the build-up dielectric film are stacked in sequence to form a multilayer structure; finally, a vacuum laminator is used to perform lamination under high temperature and high pressure conditions to tightly combine the layers of material to form a multilayer PCB.
[0025] Preferably, in S5, the laser pulse width is less than 10 picoseconds (ps), the single pulse energy is 70-87 microjoules (μJ), and the pulse frequency is 50-100 kilohertz (kHz).
[0026] Preferably, in the S5 laser drilling process, due to the Gaussian waveform and energy attenuation characteristics of the laser beam, an inverted trapezoidal blind hole is formed in the depth direction of the dielectric layer;
[0027] Among them, the design of the inverted trapezoidal blind hole helps to increase the installation thickness of the circuit board and realize a thinner circuit board design. Under the premise of ensuring the rigidity and flatness of the circuit board, the purpose of thinning the board can be achieved by reducing the number of layers. This design allows the circuit board to achieve higher integration and smaller size while maintaining the necessary physical properties;
[0028] And in the laser drilling process, when the laser beam penetrates the upper dry film and reaches the lower build-up dielectric film, due to the Gaussian waveform characteristics and energy attenuation of the laser, an inverted trapezoidal hole will be formed in the depth direction of the dielectric layer until it extends to the bottom copper barrier layer, thereby forming a second inverted trapezoidal blind hole;
[0029] Among them, the design of the inverted trapezoidal hole can enhance the connection reliability between layers, provide a larger contact area and better electroplating filling effect, and the inverted trapezoidal blind hole helps to reduce the impedance matching problem in signal transmission and improve the data transmission speed. It is especially suitable for high-frequency signal transmission because it can reduce the impact of electromagnetic interference. In the manufacturing process, reducing the processing area and processing circumference can improve the processing efficiency by about 30%. This efficiency improvement is attributed to the fact that the inner layer of colloid does not contact the colloid during the secondary processing, which effectively controls the shrinkage of the colloid, making it easier for electroplated copper to be plated in the hole.
[0030] Preferably, the film stripping process in S6 is as follows:
[0031] Ultrasonic bulking: First, use ultrasound to bulk up the dry film on the PCB surface, which helps the subsequent stripping solution to penetrate and peel off the dry film more effectively; the ultrasonic frequency is selected at 20-40kHz to ensure that the dry film layer is effectively stripped; spray stripping: After ultrasonic bulking, use stripping liquid to spray the PCB surface to further remove the dry film. The stripping liquid is composed of sodium hydroxide or potassium hydroxide, with a ratio of 15-25g per liter of stripping liquid, 0.2-0.25g of benzotriazole is added, and the rest is water; pressurized water washing: After stripping, the PCB needs to undergo at least two pressurized water washes to remove residual stripping liquid and debris. The pressure of the pressurized water wash is controlled at 1.5-2.5kg / cm2; High-pressure swing water wash: further clean the dry film fragments in the thick copper wire spacing on the PCB surface, using high-pressure swing water wash with a pressure of 10-12kg / cm2; Drying: After cleaning, the PCB needs to be dried to remove surface moisture and prepare for subsequent processes; Inspection: Finally, the PCB is quality checked to ensure that the stripping is thorough and residue-free.
[0032] Preferably, S7 further includes pre-treatment before copper deposition, including plate grinding and activation treatment, wherein the plate grinding is mainly to remove the flash and scratches, clean the plate surface and the dust in the hole, and the activation treatment is to adsorb the palladium ions into the hole wall of the non-conductor to prepare for the subsequent chemical copper deposition;
[0033] The present invention provides a low-cost processing method for making tiny PCB laser blind holes. It has the following beneficial effects:
[0034] This is a low-cost processing method for making tiny PCB laser blind holes. A layer of organic film (such as dry film) that can be peeled off later is pressed on the surface of the circuit board build-up dielectric film, and then conventional CO2 laser drilling is performed on the surface of the organic film. The laser beam first penetrates the organic film, and then penetrates the build-up dielectric film until the bottom copper is exposed. During the whole process, the energy of the laser will weaken as the processing depth increases. By controlling the processing parameters, a laser blind hole is finally formed. The hole shape is generally inverted trapezoidal, and the hole diameter will gradually become smaller (such as Figure 2 As shown in the figure, by utilizing this hole type feature, the aperture on the lower build-up dielectric film is smaller than the aperture on the upper dry film. After the upper organic film is peeled off, a blind hole with an aperture exceeding the processing capacity of a conventional CO2 laser drilling machine can be obtained on the build-up dielectric film. Subsequently, processes such as degumming, copper plating, and electroplating are performed to complete the filling of tiny PCB blind holes. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 It is a schematic diagram of the structure of the present invention;
[0036] Figure 2 It is a schematic diagram of the principle of the present invention;
[0037] Figure 3This is a schematic diagram of laser drilling in comparative example 1 of the present invention;
[0038] Figure 4 This is a schematic diagram of laser drilling in Example 1 of the present invention;
[0039] Figure 5 This is a schematic diagram of the aperture of Comparative Example 1 of the present invention;
[0040] Figure 6 This is a schematic diagram of the aperture of Example 1 of the present invention;
[0041] Figure 7 This is a schematic diagram of the laminated structure of Comparative Example 1 of the present invention;
[0042] Figure 8 This is a schematic diagram of the stacked structure of Example 1 of the present invention. DETAILED DESCRIPTION
[0043] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0044] Embodiment 1:
[0045] See also Figure 1-2 The embodiment of the present invention provides a technical solution: a low-cost processing method for making tiny PCB laser blind holes, the steps of which are as follows:
[0046] S1. Feeding, wherein at least one layer of copper clad laminate (CCL) is used as the core layer material, and the CCL is composed of a reinforcing material such as glass fiber cloth and at least one side of copper foil;
[0047] S2. Inner layer circuit production, complete the production of inner layer graphics according to circuit design requirements, including cutting, pre-processing, film pasting, exposure, development, etching and film stripping to form the required circuit pattern;
[0048] S3. Lamination: Use a vacuum laminator to press and cure the multi-layer inner layer circuit board. The material package used for lamination is one of ABF, CBF or NBF build-up dielectric films;
[0049] S4. Lamination: After lamination, a layer of dry film with a certain thickness is pressed on the product to protect the copper layer and prepare for subsequent steps;
[0050] S5. Laser drilling, using laser technology to penetrate the dry film and form blind holes on the underlying copper foil. The laser drilling process adjusts the laser parameters according to the hole size to ensure the quality of the hole;
[0051] S6. De-filming: using a film stripping process to remove the dry film on the surface to prepare for the subsequent electroplating steps;
[0052] S7. Copper deposition and hole-filling electroplating: first, the glue removal process is carried out, and then a copper layer is deposited on the hole wall to achieve hole metallization, and the blind hole is filled by hole-filling electroplating to complete the conductive connection of the circuit board.
[0053] The inner layer circuit manufacturing method in step S2 is:
[0054] Cutting: Cut the CCL into a size suitable for processing and subsequent use according to design requirements; the cutting process needs to ensure the accuracy of the size to avoid affecting the assembly and function of the circuit board due to size errors;
[0055] Pretreatment: Clean the surface of CCL to remove oil, dust and other pollutants to ensure that the dry film can be evenly coated and firmly attached to the CCL;
[0056] Film lamination: a layer of photoresist dry film is evenly coated on the surface of CCL, and the thickness of the dry film is controlled within 5μm-20μm according to the process requirements;
[0057] Exposure: Use image transfer technology to transfer the circuit pattern to the dry film through UV light; precise alignment during the operation ensures the accuracy and integrity of the circuit pattern;
[0058] Development: Use a specific chemical solution in the developing tank to dissolve the dry film in the unexposed area to form grooves for the circuit pattern; precisely control the temperature, speed, and pressure parameters during the development process;
[0059] Etching: Use chemical or mechanical methods to remove the copper foil that is not protected by the dry film to form the desired circuit pattern;
[0060] Stripping: Remove the dry film on the formed circuit pattern to prepare for subsequent steps such as copper deposition and electroplating; the stripping process uses a high concentration of sodium hydroxide solution to ensure that the dry film is completely removed.
[0061] The etching solution is composed of alkaline copper chloride, wherein the concentration of the alkaline copper chloride etching solution is controlled within the range of 135-165g / L, the etching is controlled at 55°C, wherein the pH value of the alkaline copper chloride etching solution should be maintained at 8.8, and the temperature is controlled at 55°C. In the lamination process of S3, it is necessary to punch the target holes, browning treatment, and punch the PP sheet (Prepreg), and then stack the boards, stack the inner layer boards and the build-up dielectric films in sequence to form a multi-layer structure; finally, a vacuum laminator is used to press under high temperature and high pressure conditions to tightly combine the layers of materials to form a multi-layer PCB.
[0062] The laser pulse width in S5 is less than 10 picoseconds (ps), the single pulse energy is 87 microjoules (μJ), and the pulse frequency is 100 kilohertz (kHz).
[0063] In the S5 laser drilling process, due to the Gaussian waveform and energy attenuation characteristics of the laser beam, an inverted trapezoidal blind hole will be formed in the depth direction of the dielectric layer. In the laser drilling process, when the laser beam penetrates the upper dry film and reaches the lower build-up dielectric film, due to the Gaussian waveform characteristics and energy attenuation of the laser, an inverted trapezoidal hole will be formed in the depth direction of the dielectric layer until it extends to the bottom copper barrier layer, thereby forming a second inverted trapezoidal blind hole.
[0064] The film stripping process in S6 is as follows:
[0065] Ultrasonic bulking: First, use ultrasound to bulk up the dry film on the PCB surface, which helps the subsequent film stripping solution to penetrate and peel off the dry film more effectively; the ultrasonic frequency is selected at 20-40kHz to ensure that the dry film layer is effectively peeled off;
[0066] Spray stripping: After ultrasonic expansion, use stripping liquid to spray the PCB surface to further remove the dry film. The stripping liquid is composed of sodium hydroxide or potassium hydroxide, with a ratio of 125g per liter of stripping liquid, 0.25g of benzotriazole, and the rest is water;
[0067] Pressurized water washing: After film stripping, the PCB needs to be washed with pressurized water at least twice to remove the residual film stripping liquid and debris. The pressure of the pressurized water washing is controlled at 2.5kg / cm2;
[0068] High-pressure swing water washing: To further clean the dry film fragments in the gaps between thick copper wires on the PCB surface, high-pressure swing water washing is used with a pressure of 12kg / cm2;
[0069] Drying: After cleaning, the PCB needs to be dried to remove surface moisture and prepare for subsequent processes;
[0070] Inspection: Finally, the PCB is quality checked to ensure that the film is stripped thoroughly and without residue.
[0071] S7 also includes pre-treatment before copper deposition, including grinding and activation treatment, wherein grinding is mainly to remove the flash, scratches, clean the board surface and the dust in the hole, and activation treatment is to make palladium ions adsorbed in the hole wall of the non-conductor to prepare for the subsequent chemical copper deposition; in this embodiment, chemical copper deposition is completed by catalytic oxidation-reduction reaction, and the chemical equation can be expressed as: Cu 2+ +2HCHO+4OH - →Cu+2HCOO - +2H2O+H2↑.
[0072] The rate of the chemical copper deposition process can be calculated by weighing or titration. The calculation formula of the weighing method is:
[0073]
[0074] The titration calculation formula is:
[0075]
[0076] Among them, G1 and G2 are the weights before and after copper deposition, and V consumed during titration. EDTA The volume of the standard solution, V EDTA is the volume constant of the EDTA (ethylenediaminetetraacetic acid) standard solution consumed during titration, 1.97 is the molar ratio of copper reacting with EDTA, 39.37 is the atomic weight of copper in g / mol, 929 and 39.37 are the material densities in this embodiment, and 2.12 and 2 are the area and thickness of the copper deposit in this embodiment.
[0077] In the process of chemical copper deposition, the uniformity and quality of the copper layer must be ensured; the composition and reaction conditions of the chemical copper deposition solution must be precisely controlled, including the copper ion concentration, sodium hydroxide concentration, formaldehyde concentration, and operating temperature.
[0078] In this embodiment, the concentration of copper ions (Cu2+) is controlled at 2.2 g / L, which is the main source of copper deposition; the concentration of sodium hydroxide (NaOH) is maintained at 2 g / L, and sodium hydroxide is used to maintain the pH value of the plating solution and provide the necessary alkaline environment to enable formaldehyde to fully exert its reducing effect; the concentration of formaldehyde (HCHO) is 122 ml / L, and formaldehyde is used as a reducing agent to reduce copper ions to metallic copper; the working temperature is 34°C for the optimal working temperature range of the chemical copper deposition process; within this temperature range, the stability of the bath can be maintained and the copper deposition rate can be optimized; Processing time: The processing time is controlled at 7 minutes to obtain a copper layer with a thickness of 25μ"; Deposition rate: The deposition rate of chemical copper deposition is controlled at 25μ" to ensure the uniformity and density of the copper layer; pH value: The chemical copper deposition solution is strongly alkaline, and the pH value is maintained at 11, which is the optimal pH range for the formaldehyde reducing ability to work; Complexing agent: EDTA is used to prevent the formation of Cu(OH)2 precipitation and maintain the stability of copper ions in the solution; Stabilizer: Organic matter including S and N is used to improve the stability of the chemical copper deposition solution and prevent the autocatalytic reaction from being too fast.
[0079] Comparative Example 1:
[0080] Comparative Example 1 The method steps are:
[0081] Feeding: Feeding of CCL core layer;
[0082] Inner layer circuit: Inner layer graphics are produced according to conventional circuit process
[0083] Lamination: Using a vacuum laminator to laminate the build-up dielectric layer film;
[0084] Laser drilling: laser drilling process is used to complete the production of laser blind holes;
[0085] Hole filling electroplating: laser blind holes and surface electroplating are completed through degumming, copper plating and electroplating processes.
[0086] The difference between Comparative Example 1 and Example 1 is that, in Example 1, a layer of dry film with a certain thickness is pressed on the product after lamination, and a laser drilling process is used to drill from the dry film to the next layer of copper to complete the laser blind hole production.
[0087] In summary, after the laser drilling is completed, the hole diameter on the dry film of Example 1 is consistent with the hole diameter on the build-up dielectric film of Comparative Example 1. Figure 3-4 As shown, the effective upper pore diameter of Example 1 after film removal is the waist diameter of Comparative Example 1. Figure 5-6 As shown, the aperture of Example 1 is smaller than that of Comparative Example 1. Therefore, after the hole filling is completed, the blind hole of Example 1 is smaller than that of Comparative Example 1. Figure 7-8 As shown,
[0088] Therefore, this production method can break through the processing capabilities of existing conventional CO2 laser drilling machines in the industry, or the production limits of extremely small blind hole processing, and is suitable for processing tiny PCB blind holes with a hole diameter of ≤50μm.
[0089] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It is obvious to those skilled in the art that the present invention is not limited to the details of the above exemplary embodiments, and the present invention can be implemented in other specific forms without departing from the spirit or basic features of the present invention. Therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the present invention is defined by the attached claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims are included in the present invention. Any figure mark in the claims should not be regarded as limiting the claims involved.
[0090] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. A low-cost method for making tiny PCB laser blind holes, characterized by: The steps are as follows: S1. Feeding, wherein at least one layer of copper clad laminate (CCL) is used as the core layer material, and the CCL is composed of a reinforcing material such as glass fiber cloth and at least one side of copper foil; S2. Inner layer circuit production, complete the production of inner layer graphics according to circuit design requirements, including cutting, pre-processing, film pasting, exposure, development, etching and film stripping to form the required circuit pattern; S3. Lamination, using a vacuum laminator to press and cure the multi-layer inner layer circuit board, the lamination material package used is ABF, CBF or NBF build-up dielectric film one; S4. Lamination: After lamination, a layer of dry film with a certain thickness is pressed on the product to protect the copper layer and prepare for subsequent steps; S5. Laser drilling, using laser technology to penetrate the dry film and form blind holes on the underlying copper foil. The laser drilling process adjusts the laser parameters according to the hole size to ensure the quality of the hole; S6. De-filming: using a film stripping process to remove the dry film on the surface to prepare for the subsequent electroplating steps; S7. Copper deposition and hole-filling electroplating: first, the glue removal process is carried out, and then a copper layer is deposited on the hole wall to achieve hole metallization, and the blind hole is filled by hole-filling electroplating to complete the conductive connection of the circuit board.
2. A low-cost method for making tiny PCB laser blind holes according to claim 1, characterized in that: The inner layer circuit manufacturing method in step S2 is: Cutting: Cut the CCL into a size suitable for processing and subsequent use according to design requirements; the cutting process needs to ensure the accuracy of the size to avoid affecting the assembly and function of the circuit board due to size errors; Pretreatment: Clean the surface of CCL to remove oil, dust and other pollutants to ensure that the dry film can be evenly coated and firmly attached to the CCL; Film lamination: a layer of photoresist dry film is evenly coated on the surface of CCL, and the thickness of the dry film is controlled within 5μm-20μm according to the process requirements; Exposure: Use image transfer technology to transfer the circuit pattern to the dry film through UV light; Precise alignment during operation to ensure the accuracy and integrity of the circuit pattern; Development: Using a specific chemical solution in the developing tank to dissolve the dry film in the unexposed area to form grooves of the circuit pattern; Precise control of temperature, speed, and pressure parameters during the development process; Etching: Use chemical or mechanical methods to remove the copper foil that is not protected by the dry film to form the desired circuit pattern; Stripping: Remove the dry film on the formed circuit pattern to prepare for subsequent steps such as copper deposition and electroplating; the stripping process uses a high concentration of sodium hydroxide solution to ensure that the dry film is completely removed.
3. A low-cost method for making tiny PCB laser blind holes according to claim 1, characterized in that: The etching solution comprises one of acidic cupric chloride, alkaline cupric chloride, ferric chloride, ammonium persulfate, sulfuric acid / chromic acid, and sulfuric acid / hydrogen peroxide. The concentration of the alkaline cupric chloride etching solution is controlled within the range of 135-165 g / L, and the etching is controlled within the range of 45-55° C. The pH value of the alkaline cupric chloride etching solution should be maintained at 8.0-8.8, and the temperature is controlled within the range of 45-55° C.
4. According to claim 1, a low-cost method for making tiny PCB laser blind holes is characterized by: In the lamination process of S3, it is necessary to punch target holes, browning treatment and PP sheet (Prepreg) punching, and then stack the boards, stack the inner layer boards and the build-up dielectric films in sequence to form a multi-layer structure; finally, a vacuum laminator is used to press under high temperature and high pressure conditions to make each layer of material tightly combined to form a multi-layer PCB.
5. According to claim 1, a low-cost method for making tiny PCB laser blind holes is characterized by: The laser pulse width in the S5 is less than 10 picoseconds (ps), the single pulse energy is 70-87 microjoules (μJ), and the pulse frequency is 50-100 kilohertz (kHz).
6. A low-cost method for making tiny PCB laser blind holes according to claim 1, characterized in that: In the S5 laser drilling process, due to the Gaussian waveform and energy attenuation characteristics of the laser beam, an inverted trapezoidal blind hole will be formed in the depth direction of the dielectric layer, and in the laser drilling process, when the laser beam penetrates the upper dry film to reach the lower build-up dielectric film, due to the Gaussian waveform characteristics and energy attenuation of the laser, an inverted trapezoidal hole will be formed in the depth direction of the dielectric layer until it extends to the bottom copper barrier layer, thereby forming a second inverted trapezoidal blind hole.
7. A low-cost method for making tiny PCB laser blind holes according to claim 1, characterized in that: The film stripping process in S6 is as follows: Ultrasonic bulking: First, use ultrasound to bulk up the dry film on the PCB surface, which helps the subsequent film stripping solution to penetrate and peel off the dry film more effectively; the ultrasonic frequency is selected at 20-40kHz to ensure that the dry film layer is effectively peeled off; Spray stripping: After ultrasonic expansion, use a stripping liquid to spray the PCB surface to further remove the dry film. The stripping liquid is composed of sodium hydroxide or potassium hydroxide, with a ratio of 15-25g per liter of stripping liquid, 0.2-0.25g of benzotriazole, and the rest is water; Pressurized water washing: After film stripping, the PCB needs to be washed with pressurized water at least twice to remove the residual film stripping liquid and debris. The pressure of the pressurized water washing is controlled at 1.5-2.5kg / cm²; High-pressure swing water washing: To further clean the dry film fragments in the thick copper wire spacing on the PCB surface, high-pressure swing water washing is used with a pressure of 10-12kg / cm²; Drying: After cleaning, the PCB needs to be dried to remove surface moisture and prepare for subsequent processes; Inspection: Finally, the PCB is quality checked to ensure that the film is stripped thoroughly and without residue.
8. A low-cost method for making tiny PCB laser blind holes according to claim 1, characterized in that: The S7 also includes pre-treatment before copper deposition, including grinding and activation treatment, wherein the grinding is mainly to remove the burrs and scratches, clean the board surface and the dust in the holes, and the activation treatment is to adsorb the palladium ions into the hole wall of the non-conductor to prepare for the subsequent chemical copper deposition.
Citation Information
Patent Citations
Object having through-hole formed therein and laser processing method
CN101448604A
Through hole forming method, and product having through hole
CN102015196A
Manufacturing process of HDI
CN112601371A
Method of obtaining electronic circuitry features
US20100181284A1
Cited By
Millimeter wave radar circuit board processing method and millimeter wave radar circuit board
CN119767559A
Improved manufacturing method of composite cored substrate with embedded circuit
CN120529497A
Improved method for manufacturing a composite core substrate with embedded lines
CN120529497B
High-precision substrate laser processing method
CN121099532A
A high-precision substrate laser processing method
CN121099532B