Method and system for treating waste gas

By introducing ammonia or ammonia precursor upstream of the Fe-SCR catalyst, controlling the ANR between 2 and 6, and using the Fe-SCR catalyst to treat the exhaust gas of lean internal combustion engines, the problem of insufficient low-temperature NOx conversion performance in the prior art is solved, and the further development is achieved High NOx conversion and low risk of ammonia escape.

CN118973688APending Publication Date: 2024-11-15JOHNSON MATTHEY PLC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380032701.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-27
Filing Date
2023-04-17
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The NOx conversion performance of existing SCR catalysts is insufficient at low temperatures, especially in the treatment of exhaust gas for lean combustion internal combustion engines. When the ANR is controlled between 1 to 1.5, it is difficult to balance the NOx conversion rate and ammonia escape.

Method used

Using Fe-SCR catalyst, including iron and zeolite, the exhaust gas is contacted with the Fe-SCR catalyst by introducing ammonia or ammonia precursor upstream of the Fe-SCR catalyst, and the molar ratio of ammonia to NOx (ANR) is controlled between 2 and 6, so that the exhaust gas is contacted with the Fe-SCR catalyst. To improve NOx conversion performance.

Benefits of technology

The NOx conversion performance is significantly improved, and it performs better at low temperatures compared with Cu-SCR catalysts, and reduces the risk of ammonia escape under high ANR conditions. It is especially suitable for low NOx concentration and low temperature conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005072300330000201
    Figure BDA0005072300330000201
  • Figure BDA0005072300330000202
    Figure BDA0005072300330000202
Patent Text Reader

Abstract

A method of treating exhaust gas from a lean burn internal combustion engine is disclosed. The method comprises: introducing ammonia or an ammonia precursor into the exhaust gas upstream of a Fe-SCR catalyst, the Fe-SCR catalyst comprising iron and a zeolite; and contacting the exhaust gas with the Fe-SCR catalyst; wherein the amount of ammonia or ammonia precursor in the exhaust gas introduced upstream of the Fe-SCR catalyst is controlled to provide an ammonia to NOx molar ratio (ANR) of greater than 2 to 6 in the exhaust gas contacting the Fe-SCR catalyst.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for treating exhaust gas, a system for treating exhaust gas, use of the system and use of an Fe-SCR catalyst. Background Art

[0002] The nitrogen oxides (NO) are oxidized by nitrogen-containing compounds such as ammonia or the ammonia precursor urea. x ) was first developed for processing industrial stationary applications. SCR technology was first used in thermal power plants in Japan in the late 1970s and became widely used in Europe starting in the mid-1980s. In the United States, SCR systems were introduced for use in gas turbines in the 1990s and have more recently been used in coal-fired power plants. In addition to coal-fired thermal power plants and gas turbines, SCR applications include plant and refinery heaters and boilers, heating furnaces, coke ovens, municipal waste treatment plants, and incinerators in the chemical process industry. Recently, SCR-based NO x Reduction systems are being developed in Europe, Japan and the United States for many vehicular (mobile) applications, for example for treating diesel exhaust gases.

[0003] Several chemical reactions occur in the NH3SCR system, all of which represent the conversion of NO x The ideal reaction for reduction to nitrogen gas. The main reaction is represented by reaction (1).

[0004] 4NO + 4NH3 + O2 → 4N2 + 6H2O (1)

[0005] Competing non-selective reactions with oxygen can produce secondary emissions or can consume ammonia non-productively. One such non-selective reaction is the complete oxidation of ammonia, as shown in reaction (2).

[0006] 4NH3 + 5O2 → 4NO + 6H2O (2)

[0007] Additionally, side reactions may lead to undesirable products such as N2O, as represented by reaction (3).

[0008] 4NH3 + 5NO + 3O2 → 4N2O + 6H2O (3)

[0009] Since there is a 1:1 (i.e. stoichiometric) molar relationship between NO and NH3 in reaction (1), in a practical system, the reaction of alumina with NO x The molar ratio (ANR) of the SCR catalyst is controlled to be about 1 to 1.5. This achieves a NO x The desired balance between conversion performance and the possibility of excess ammonia "slipping" through the exhaust system and being released into the atmosphere.

[0010] Aluminosilicate zeolites as NO x Catalysts for SCR with NH3. One application is to control NO from vehicle diesel engines with a reducing agent obtainable from an ammonia precursor such as urea or by injecting ammonia itself. x To promote catalytic activity, transition metals are incorporated into aluminosilicate zeolites. The most commonly tested transition metal zeolites are Cu / ZSM-5, Cu / β, Fe / ZSM-5, and Fe / β because they have relatively wide temperature activity windows. In general, Cu-based zeolite catalysts show better low-temperature NO emissions than iron-based zeolite catalysts. x Reduction activity.

[0011] WO 2008 / 106519 A1 relates to known Cu-CHA zeolite SCR catalysts and particularly to their performance at low temperatures. For example, Comparative Example 11 relates to a Cu / β catalyst, and Example 10 relates to a Cu / Y zeolite catalyst. As expected, in the tested examples, ANR was controlled at about 1.

[0012] Joseph R. Theis, Ford Motor Company, SAE Int. J. Fuels Lubr., Vol. 1, No. 1, pp. 364-375, 2008 relates to a series of performance evaluation tests on SCR catalysts for lean-burn gasoline engines. A number of different parameters were tested under laboratory conditions.

[0013] There is still a need to improve SCR catalysis, and in particular NO x conversion performance, especially at low temperatures. Summary of the invention

[0014] One aspect of the present disclosure is directed to a method of treating exhaust gas from a lean-burn internal combustion engine, the method comprising: introducing ammonia or an ammonia precursor into the exhaust gas upstream of an Fe-SCR catalyst, the Fe-SCR catalyst comprising iron and a zeolite; and contacting the exhaust gas with the Fe-SCR catalyst; wherein the amount of ammonia or an ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide a ratio of ammonia to NO greater than 2 to 6 in the exhaust gas contacting the Fe-SCR catalyst. x Molar ratio (ANR).

[0015] Another aspect of the present disclosure relates to a system for treating exhaust gas from a lean-burn internal combustion engine, the system comprising: a reductant injector for introducing ammonia or an ammonia precursor into the exhaust gas; a substrate; an Fe-SCR catalyst contained within or disposed on the substrate, the Fe-SCR catalyst comprising iron and zeolite; and an engine control unit; wherein the reductant injector is located upstream of the Fe-SCR catalyst; and wherein the engine control unit is configured to control the amount of ammonia or an ammonia precursor introduced into the exhaust gas by the reductant injector during use, so that the ammonia in the exhaust gas contacting the Fe-SCR catalyst is reacted with NO x The molar ratio (ANR) is greater than 2 to 6.

[0016] Another aspect of the present disclosure relates to use of the system of the above aspect in a method according to the first aspect.

[0017] Another aspect of the present disclosure relates to the use of Fe-SCR catalysts for treating NO containing 100 ppm or less from a lean-burn internal combustion engine. x The Fe-SCR catalyst comprises iron and zeolite, and the ANR is greater than 2 to 6. DETAILED DESCRIPTION

[0018] The present invention seeks to address at least some of the problems associated with the prior art or at least provide a commercially acceptable alternative solution thereto.

[0019] In a first aspect, the present invention provides a method of treating exhaust gas from a lean-burn internal combustion engine, the method comprising:

[0020] introducing ammonia or an ammonia precursor into the exhaust gas upstream of a Fe-SCR catalyst comprising iron and a zeolite; and

[0021] contacting the exhaust gas with the Fe-SCR catalyst;

[0022] wherein the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide a ratio of ammonia to NO greater than 2 to 6 in the exhaust gas contacting the Fe-SCR catalyst. x Molar ratio (ANR).

[0023] Unless expressly indicated to the contrary, each aspect or embodiment as defined herein may be combined with any other aspect or embodiment. In particular, any feature indicated as being preferred or advantageous may be combined with any other feature indicated as being preferred or advantageous.

[0024] Surprisingly, when carrying out the method of this aspect, unexpectedly high NO has been observed, particularly due to the combination of the Fe-SCR catalyst and the particularly high ANR (without wishing to be bound by theory).x Conversion performance. In particular, this improvement has been observed relative to a similar Cu-SCR catalyst. This is in contrast to the current "standard" approach, where the ANR is typically kept below 2, and preferably around 1 to 1.5.

[0025] When increasing the ANR in the SCR reaction, it would be naturally expected that NO x The conversion performance increases slightly. This is because the concentration of the reducing agent ammonia in the exhaust gas is increasing. However, surprisingly, it has been observed that, especially for the Fe-SCR catalyst described herein, when the ANR increases above 2, the NO x The conversion performance is improved by a much greater amount than expected, and importantly, to a greater extent than compared to comparative SCR catalysts such as Cu-SCR catalysts. For example, it can be expected that both Fe-SCR and Cu-SCR catalysts will have a NO x Conversion performance will increase at the same or similar rate with increasing ANR. Cu-SCR catalysts may also be preferred at low temperatures, and therefore it may be expected that Cu-SCR catalysts perform better at low temperatures. However, as ANR increases above 2, especially at low temperatures, it has been observed that Fe-SCR catalysts perform significantly better relative to corresponding Cu-SCR catalysts.

[0026] Increasing ANR and increasing NO x There is also a "trade-off" between performance levels. This is because the higher the ANR, the greater the likelihood of "ammonia slip" in the exhaust system, i.e. the undesirable result of unreacted ammonia reductant passing through the exhaust system and being released into the atmosphere. However, since increased NOx may be exhibited at such ANR in the method of the present invention, x conversion rate, this benefit may outweigh the risk of increased ammonia slip in the system, especially at low temperatures and / or low NO x Therefore, contrary to the teachings of the art, in combination with a Fe-SCR catalyst as described herein, a higher ANR may be beneficial in certain circumstances.

[0027] These advantages cannot be expected from WO 2008 / 106519A1, which can be considered to represent some standard SCR practices in the art. From this document, it can be expected that the use of Cu-SCR catalysts can achieve improvements in SCR catalysis at low temperatures. In addition, no discussion of changing ANR is given. The paper also does not discuss the effect of increasing ANR in combination with Fe-SCR catalysts.

[0028] As used herein, the term "lean-burn internal combustion engine" takes its normal meaning in the art, such as an internal combustion engine that burns fuel in excess air.

[0029] As used herein, the term "ammonia precursor" encompasses any compound that can decompose into ammonia when released into an exhaust system, for example. Typical ammonia precursors used in the field of the present invention include urea, hydrazine, ammonium carbonate, ammonium carbamate, ammonium bicarbonate, and ammonium formate.

[0030] The term "upstream" as used herein refers to the relative position of a feature within an exhaust system. In particular, the term "upstream" as used herein refers to a feature that is closer to the exhaust source along the exhaust path within the exhaust system. Therefore, the term "downstream" as used herein refers to a feature that is farther away from the exhaust source along the exhaust path within the exhaust system. It should also be recognized that an exhaust system including a device (such as an injector for introducing a reductant or a reductant precursor) and an SCR catalyst must be oriented from upstream to downstream so that the introduction of the reductant (or its precursor) is completed upstream of the SCR catalyst. If the orientation is opposite and the reductant (or its precursor) is introduced only downstream of the SCR catalyst, the SCR catalyst will not have a reductant source to perform its function required to reduce nitrogen oxides. Therefore, in this context, the terms "upstream" and "downstream" used in conjunction with the exhaust system impose a clear orientation so that the exhaust system is not only suitable for orientation in any direction.

[0031] The term "SCR" as used herein refers to "selective catalytic reduction", as known in the art. The term "SCR" as used herein encompasses the reduction (i.e., catalytic removal) of NO present in the exhaust gas by a catalyst in the presence of a reducing agent such as ammonia or an ammonia precursor. x .

[0032] The Fe-SCR catalyst comprises iron and a zeolite. Typically, the iron is disposed on the zeolite. For example, in the context of the present invention, the term "disposed on" in the context of a metal "disposed on a zeolite" may encompass having the metal supported on the surface of the zeolite or within its pores, but the zeolite is preferably "ion exchanged" with Fe.

[0033] As used herein, the term "zeolite" takes its ordinary meaning in the art. The term "zeolite" encompasses aluminosilicate molecular sieves, and is further defined and classified by the International Zeolite Association as known to those skilled in the art.

[0034] Preferably, the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR of 3 to 5, more preferably 4 to 5, in the exhaust gas contacting the Fe-SCR catalyst. In some preferred embodiments, the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR of greater than 2.5 in the exhaust gas contacting the Fe-SCR catalyst. It has been surprisingly found that increased NO can be observed even more strongly at such an ANR. xFor example, surprisingly, the Fe-SCR catalysts described herein and comparable SCR catalysts such as Cu-SCR catalysts have a NO conversion performance of 1. x The difference between conversion performance can be even greater at such ratios. This is in contrast to current "standard" methods, where the ANR is typically kept below 2, and preferably around 1 to 1.5.

[0035] NO in exhaust gas contacting Fe-SCR catalyst x The concentration is not particularly limited, and the above effects can also be exerted in high NO x However, preferably, the NO in the exhaust gas contacting the Fe-SCR catalyst x The concentration is 100 ppm or less. More preferably, NO in the exhaust gas contacting the Fe-SCR catalyst x The concentration is 50 ppm or less, even more preferably 10 ppm or less. x In other words, the advantages of the Fe-SCR catalyst described herein over other SCR catalysts such as Cu-SCR catalysts are particularly advantageous at such low NO concentrations. x In addition, the method of the present invention is particularly suitable for such exhaust gas conditions. This is because at such low NO x With a high ANR, the absolute ammonia concentration in the exhaust gas can remain relatively low, even when the ANR is high. Therefore, the risk associated with (absolute) ammonia slip can also be kept low.

[0036] Preferably, the concentration of NO in the exhaust gas contacting the Fe-SCR catalyst is x The ratio of the concentration of is 0.8 or more, more preferably 0.9 or more. The method of the present invention is particularly applicable to such exhaust gas conditions.

[0037] Preferably, the method further comprises reducing NO in the exhaust gas prior to the step of introducing ammonia or an ammonia precursor into the exhaust gas. x For example, preferably, NO in the exhaust gas discharged from a lean-burn internal combustion engine x The concentration of NO in the exhaust gas is greater than 100 ppm and the step of introducing ammonia or an ammonia precursor into the exhaust gas is preceded by the step of reducing the NO in the exhaust gas x The concentration of NO in the exhaust gas will x The concentration of NO in the exhaust gas is reduced to 100 ppm or less, preferably 50 ppm or less, more preferably 10 ppm or less. The step of reducing NO in the exhaust gas before introducing ammonia or an ammonia precursor into the exhaust gas xThe concentration of NO can be preferably obtained by mixing the exhaust gas with an additional SCR catalyst, an oxidation catalyst and / or a passive NO x The SCR catalyst is preferably contacted with a PNA catalyst. Preferably, the additional SCR catalyst comprises a Cu-SCR catalyst comprising copper and a zeolite. Copper is typically placed on a zeolite. Preferably, the Cu-SCR catalyst comprises copper placed on a small pore zeolite such as AEI or CHA zeolite. Preferably, the oxidation catalyst comprises a diesel oxidation catalyst (DOC). Preferably, the DOC comprises a platinum group metal such as platinum placed on a support material such as alumina. Preferably, the PNA catalyst comprises a platinum group metal (PGM), preferably palladium, placed on a small pore zeolite, and the small pore zeolite preferably has a framework type including CHA and / or AEI. The term "platinum group metal" as used herein may include one or more of iridium, osmium, palladium, platinum, rhodium and ruthenium. For example, the term "passive NO x The term "adsorbent" or "PNA" may include a material that effectively adsorbs NO at cryogenic temperatures or below. x And release the adsorbed NO at temperatures above low temperature x For example, suitable PNAs are discussed in WO 2015 / 085303A1. Such an approach can help achieve low NO that can achieve the above advantages. x Exhaust gas conditions.

[0038] The method of the present invention is particularly applicable to the type of exhaust gas generated by a lean-burn engine, especially a lean-burn engine of a vehicle. For example, preferably, the lean-burn internal combustion engine is a diesel engine, a hydrogen engine, or an engine powered by liquid petroleum gas or natural gas. The lean-burn internal combustion engine is most preferably a diesel engine. Preferably, the lean-burn internal combustion engine is not a gasoline engine.

[0039] Preferably, the temperature of the exhaust gas contacting the Fe-SCR catalyst is 500°C or less. More preferably, the temperature of the exhaust gas contacting the Fe-SCR catalyst is 350°C or less, even more preferably 300°C or less, and still more preferably 200°C or less. Although the surprising and advantageous effects described herein may be observed at higher temperatures, the improved NO reduction of the Fe-SCR catalyst at higher ANRs is x The conversion performance is particularly evident at lower exhaust gas temperatures, especially relative to comparative SCR catalysts. Thus, the method of the present invention may be particularly useful during cold engine starts, while the engine temperature remains relatively cool. For example, there is a strong desire in the art to improve the NO conversion of SCR catalysts during cold starts (low temperature SCR). x The conversion performance, and therefore this advantage, can be very important.

[0040] At such low temperatures, urea (ie, ammonia precursor) hydrolysis may be less likely to occur. However, a heated urea injector may be used.

[0041] Therefore, preferably, in the method of the present invention, when the temperature of the exhaust gas contacting the Fe-SCR catalyst is at a predetermined threshold temperature or lower, the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR greater than 2 to 6 in the exhaust gas contacting the Fe-SCR catalyst; and when the temperature of the exhaust gas contacting the Fe-SCR catalyst is greater than the threshold temperature, the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR of 2 or less in the exhaust gas contacting the Fe-SCR catalyst. More preferably, when the temperature of the exhaust gas contacting the Fe-SCR catalyst is at a predetermined threshold temperature or lower, the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR of 3 to 5 in the exhaust gas contacting the Fe-SCR catalyst. In other words, in some preferred embodiments, the method of the present invention is used only when the engine is in a cold start period, and then once the engine has warmed up so that the temperature of the exhaust gas is above the threshold temperature, a standard method known in the art is used in which the ANR is maintained within a typical range. In this way, once the engine has warmed up and the advantages of high ANR may be less significant, the amount of ANR may be reduced so that the risk of ammonia slip may be reduced.

[0042] For the reasons described above, the threshold temperature is preferably 500°C, more preferably 350°C, even more preferably 300°C, still more preferably 200°C.

[0043] Preferably, the zeolite of the Fe-SCR catalyst comprises a zeolite having a framework type selected from the following: AFX, AEI, BEA, FER, MFI, FAU, LTA, LTL, CHA or one or more of their mixtures or inter-organisms, more preferably AEI, AFX, BEA, FER, MFI, FAU or one or more of their mixtures or inter-organisms. BEA zeolite comprises beta zeolite. The framework topology of zeolite beta is discussed in the following literature: JB Higgins et al., Zeolites 8, 446-452 (1988); and JM Newsam et al., Proc. R. Soc. Lond. A 420, 375-405 (1988). FER zeolite comprises ferrierite. MFI zeolite comprises, for example, ZSM-5. FAU zeolite comprises zeolite X and zeolite Y. AEI zeolite comprises SSZ-39. AFX zeolite comprises SSZ-16. This framework type is known to those skilled in the art and is defined by the International Zeolite Association. Preferably, the zeolite of the Fe-SCR catalyst comprises a medium-pore and / or large-pore zeolite. Such zeolites may be particularly effective in allowing the Fe-SCR catalyst to exhibit the above-mentioned advantageous high NOx at high ANR. x Conversion rate.

[0044] As used herein, the term "small pore zeolite" may encompass zeolites having a maximum ring size of eight tetrahedral atoms. As used herein, the term "medium pore zeolite" may encompass zeolites having a maximum ring size of ten tetrahedral atoms. As used herein, the term "large pore zeolite" may encompass zeolites having a maximum ring size of twelve tetrahedral atoms.

[0045] Preferably, the zeolite of the Fe-SCR catalyst comprises a zeolite having a framework type comprising: AEI, AFX, BEA and / or FER, preferably BEA. Preferably, the zeolite of the Fe-SCR catalyst is a beta zeolite. BEA zeolites (such as beta zeolite) have been shown to be particularly suitable for the method of the present invention to achieve the advantages described herein. Unfortunately, however, BEA zeolite may not be particularly heat resistant, especially in the harsh temperature environment experienced by exhaust gas catalysts. Fe-FER catalysts can achieve similar levels of NO to Fe-BEA catalysts. x conversion, and may exhibit greater thermal durability. Therefore, FER zeolites may also be preferred.

[0046] Preferably, the zeolite of the Fe-SCR catalyst has a silica to alumina molar ratio (SAR) of about 7 to about 50, more preferably about 10 to about 35, even more preferably about 20 to about 30, and still more preferably about 22 to about 28. Such zeolites may be particularly effective in allowing the Fe-SCR catalyst to exhibit the above-described advantageous high NOx at high ANR. xFor example, when the zeolite of the Fe-SCR catalyst includes a zeolite having a framework type including BEA and / or FER, the zeolite of the Fe-SCR catalyst preferably has a SAR of about 25; the AEI preferably has a SAR of 20.

[0047] Preferably, the zeolite of the Fe-SCR catalyst comprises iron disposed on the zeolite at a loading of about 1 wt % to about 7 wt %, preferably about 2 wt % to about 5 wt %, more preferably about 3 wt %, based on the weight of the zeolite.

[0048] In some preferred embodiments, the Fe-SCR catalyst further comprises copper disposed on a zeolite. Thus, the advantages associated with the presence of each of copper and iron, respectively, can be utilized. In this regard, the results of the examples generally indicate that for lean-burn internal combustion engines emitting relatively cold exhaust gases or located in locations where the exhaust gases are relatively cold (e.g., <300° C.), using a Fe-SCR catalyst and contacting the catalyst at an ANR of greater than 2 to 6 can achieve improved NO x Conversion rate.

[0049] However, further, if the exhaust gas of the lean-burn internal combustion engine in dynamic operation spans a temperature range of <300°C and >300°C, the exhaust system can be designed to combine the Fe-SCR zeolite catalyst and the Cu-SCR zeolite catalyst with appropriate control of the ANR to include an ANR greater than 2 to 6, preferably at lower temperatures where the Fe-SCR zeolite catalyst is more active; and a lower ANR at higher temperatures where the Cu-SCR zeolite catalyst can be more active, thereby improving NO over a wider temperature window. x Conversion. Configurations combining the Fe-SCR zeolite catalyst and the Cu-SCR zeolite catalyst include layered arrangements, mixtures of the two catalysts, and zone coated (side-by-side) a single substrate.

[0050] Preferably, the Fe-SCR catalyst is contained within or disposed on a substrate, the substrate comprising two or more catalyst zones, and the Fe-SCR catalyst is contained within a first catalyst zone.

[0051] The term "substrate" as used herein may encompass, for example, a ceramic or metal honeycomb or filter block (e.g., a wall flow filter or a flow-through substrate). The substrate may include a single (or unitary) substrate. The substrate may include a ceramic unitary substrate. The substrate may vary in its material composition, size and configuration, pore shape and density, and wall thickness. Suitable substrates are known in the art.

[0052] In the context of this feature, the term "contained within" may encompass embodiments where the substrate is an extruded substrate, for example, where the Fe-SCR catalyst is incorporated into the extrudate when the extruded substrate is formed.

[0053] In the context of this feature, the term "disposed on" may encompass both having the Fe-SCR catalyst disposed directly on the substrate (i.e., without intervening materials) and / or disposed indirectly on the substrate (i.e., with intervening materials). If the substrate is porous, the term "disposed on" may also encompass having the Fe-SCR catalyst disposed therein, such as within the pores of the substrate, i.e., with the Fe-SCR catalyst disposed thereon and / or therein. The Fe-SCR catalyst may be disposed on the substrate in the form of a washcoat.

[0054] The term "catalyst zone" as used herein encompasses a defined area of ​​a substrate that can be distinguished from another area of ​​the substrate, for example due to having a different catalyst composition contained therein or placed thereon. A "zone" typically has different boundaries or edges (i.e., a zone can be distinguished from another zone using conventional analytical techniques). In addition, the term "zone" as used herein refers to an area having an axial length less than the total axial length of the substrate, such as ≤75% of the total length of the substrate. A "zone" typically has a length (i.e., substantially uniform length) of at least 5% (e.g., ≥5%) (e.g., preferably ≥30%, more preferably ≥40%) of the total length of the substrate.

[0055] The substrate may comprise a wall-flow filter substrate, but in a preferred embodiment, the substrate comprises a flow-through substrate. Prior to applying the Fe-SCR catalyst, the substrate may be a "blank", i.e., a substrate that is not coated with a carrier coating. Alternatively, the substrate may have one or more carrier coatings already loaded thereon. In this case, the final catalyst article may comprise multiple layers of different carrier coatings. The substrate preferably comprises cordierite. However, the composition of the substrate is not particularly limited. The term "carrier coating" as used herein is well known in the art and refers to an adhesion coating that is typically applied to a substrate during catalyst production.

[0056] Preferably, the Cu-SCR catalyst is contained in a second catalyst zone different from the first catalyst zone, and the Cu-SCR catalyst comprises copper and zeolite. The second catalyst zone is usually supported on the surface of the substrate and is adjacent to the Fe-SCR catalyst zone or minimally overlaps the Fe-SCR catalyst (or, depending on the order of application of the Fe-SCR catalyst and the Cu-SCR catalyst carrier coating, the Fe-SCR catalyst may minimally overlap the Cu-SCR catalyst; "minimum overlap" defines an unexpected overlap to allow for coating tolerances of "real world" depths that can be obtained during manufacturing). Copper is usually placed on zeolite. For example, the zeolite may include a small pore zeolite, such as AEI or CHA.

[0057] Preferably, the second catalyst zone is located upstream of the first catalyst zone. This may be a particularly preferred arrangement of the catalyst zones.

[0058] If copper is not necessarily present in the Fe-SCR catalyst, the method preferably further comprises contacting the exhaust gas with a Cu-SCR catalyst prior to contacting the exhaust gas with the Fe-SCR catalyst, the Cu-SCR catalyst comprising copper and a zeolite, wherein the Cu-SCR catalyst is located in a close coupling position upstream of the Fe-SCR catalyst. The preferred Cu-SCR catalysts described elsewhere herein are equally applicable to this embodiment.

[0059] The method preferably also includes contacting the exhaust gas with a Cu-SCR catalyst downstream of the Fe-SCR catalyst, the Cu-SCR catalyst comprising copper and zeolite, wherein the Cu-SCR catalyst is located downstream of the Fe-SCR catalyst in an underfloor position. The preferred Cu-SCR catalysts described elsewhere herein are equally applicable to this embodiment.

[0060] Preferably, the ammonia precursor comprises urea.Other suitable ammonia precursors may comprise hydrazine, ammonium carbonate, ammonium carbamate, ammonium bicarbonate or ammonium formate.

[0061] In another aspect, the present invention provides a system for treating exhaust gas from a lean-burn internal combustion engine, the system comprising:

[0062] a reductant injector for introducing ammonia or an ammonia precursor into the exhaust gas;

[0063] substrate;

[0064] an Fe-SCR catalyst contained within or disposed on the substrate, the Fe-SCR catalyst comprising iron and zeolite; and

[0065] Engine control unit;

[0066] wherein the reductant injector is located upstream of the Fe-SCR catalyst; and

[0067] The engine control unit is configured to control the amount of ammonia or ammonia precursor introduced into the exhaust gas by the reductant injector during use so that the ammonia in the exhaust gas contacting the Fe-SCR catalyst is mixed with NO x The molar ratio (ANR) is greater than 2 to 6.

[0068] The term "reductant injector" may encompass any device suitable for releasing or injecting ammonia or an ammonia precursor into the exhaust gas stream. Suitable reductant injectors are known in the art and may include a heated injector nozzle to promote thermal decomposition of an ammonia precursor such as urea.

[0069] An engine control unit configured to control the amount of ammonia or ammonia precursor introduced into the exhaust gas by the reductant injector during use may include the engine control unit being preprogrammed to provide such functionality. For example, the engine control unit may control the amount of NO x The sensor responds to the signal received (i.e., provides information about the NO x The concentration of NO is measured directly and the amount of reductant released by the reductant injector is controlled accordingly, so that the desired ANR is maintained using such a feedback loop. x Concentration of NO x Sensor replacement, NO x The concentration may be determined, for example, by comparing any other suitable parameter of engine condition to the predicted NO in the exhaust gas. x The concentration may be determined indirectly using a pre-associated look-up table or map (stored in the control unit) that correlates the concentration.

[0070] The surprising advantages associated with the method of the first aspect also apply to the present aspect.

[0071] Preferably, the system further comprises a lean burn internal combustion engine.

[0072] Preferably, the engine control unit is configured to control the amount of ammonia or ammonia precursor introduced into the exhaust gas via the reductant injector during use such that the ANR in the exhaust gas contacting the Fe-SCR catalyst is between 3 and 6.

[0073] Preferably, the system comprises an additional SCR catalyst, an oxidation catalyst and / or a PNA catalyst upstream of the Fe-SCR catalyst. x The concentration may be reduced prior to contacting the Fe-SCR catalyst.

[0074] Preferably, the lean-burn internal combustion engine is not a gasoline engine. Use of the system of the present invention may be particularly applicable to the type of exhaust gas generated by such an engine. For example, preferably, the lean-burn internal combustion engine is a diesel engine, a hydrogen engine, or an engine powered by liquid petroleum gas or natural gas. The lean-burn internal combustion engine is most preferably a diesel engine.

[0075] Preferably, the zeolite of the Fe-SCR catalyst comprises a zeolite having a framework type selected from the following: AEI, AFX, BEA, FER, MFI, FAU, LTA, LTL, CHA or one or more of their mixtures or inter-products, more preferably AEI, AFX, BEA, FER, MFI, FAU or one or more of their mixtures or inter-products. BEA zeolites include beta zeolites. FER zeolites include ferrierite. MFI zeolites include, for example, ZSM-5. FAU zeolites include zeolite X and zeolite Y. AEI zeolites include SSZ-39. AFX zeolites include SSZ-16. Such framework types are known to those skilled in the art and are defined by the International Zeolite Association. Preferably, the zeolite of the Fe-SCR catalyst comprises medium-pore and / or large-pore zeolites. Such zeolites may be particularly effective in allowing the Fe-SCR catalyst to exhibit the above-mentioned advantageous high NO at high ANR. x Conversion rate.

[0076] Preferably, the zeolite of the Fe-SCR catalyst comprises a zeolite having a framework type comprising: AEI, AFX, BEA and / or FER, preferably BEA. Preferably, the zeolite of the Fe-SCR catalyst is a beta zeolite. BEA zeolites (such as beta zeolite) have been shown to be particularly suitable for use in the system of the present invention to achieve the advantages described herein. Unfortunately, however, BEA zeolites may not be particularly heat resistant, particularly in the harsh temperature environments experienced by exhaust gas catalysts. Fe-FER catalysts may achieve similar levels of NO to Fe-BEA catalysts. x conversion, and may exhibit greater thermal durability. Therefore, FER zeolites may also be preferred.

[0077] Preferably, the zeolite of the Fe-SCR catalyst has a silica to alumina molar ratio (SAR) of about 15 to about 50, more preferably about 15 to about 35, even more preferably about 20 to about 30, and still more preferably about 22 to about 28. Such zeolites may be particularly effective in allowing the Fe-SCR catalyst to exhibit the above-described advantageous high NOx at high ANR. x For example, when the zeolite of the Fe-SCR catalyst includes a zeolite having a framework type including BEA and / or FER, the zeolite of the Fe-SCR catalyst preferably has a SAR of about 25.

[0078] Preferably, the zeolite of the Fe-SCR catalyst comprises iron disposed on the zeolite at a loading of about 1 wt % to about 7 wt %, preferably about 2 wt % to about 5 wt %, more preferably about 3 wt %, based on the weight of the zeolite.

[0079] In some preferred embodiments, the Fe-SCR catalyst further comprises copper disposed on a zeolite.Thus, the advantages associated with the presence of each of copper and iron, respectively, can be exploited.

[0080] Preferably, the substrate comprises two or more catalyst zones, the Fe-SCR catalyst being contained within a first catalyst zone.

[0081] Preferably, the substrate comprises a wall flow filter substrate. In an alternative preferred embodiment, the substrate comprises a flow-through substrate. The substrate may be a "blank", i.e., a substrate that is not coated with a washcoat. Alternatively, the substrate may have one or more washcoats already loaded thereon. In this case, the final catalyst article may comprise multiple layers of different washcoats. The substrate preferably comprises cordierite. However, the composition of the substrate is not particularly limited.

[0082] Preferably, a Cu-SCR catalyst is contained in a second catalyst zone different from the first catalyst zone, the Cu-SCR catalyst comprising copper and zeolite. The copper is typically placed on the zeolite. For example, the zeolite may include a small pore zeolite, such as AEI or CHA.

[0083] Preferably, the second catalyst zone is located upstream of the first catalyst zone. This may be a particularly preferred arrangement of the catalyst zones.

[0084] If copper is not necessarily present in the Fe-SCR catalyst, the system preferably also includes a Cu-SCR catalyst located in a close coupling position upstream of the Fe-SCR catalyst, the Cu-SCR catalyst comprising copper and a zeolite. The preferred Cu-SCR catalysts described elsewhere herein are also applicable to this embodiment.

[0085] The system preferably also includes a Cu-SCR catalyst located downstream of the Fe-SCR catalyst in an underfloor location, the Cu-SCR catalyst comprising copper and zeolite. The preferred Cu-SCR catalysts described elsewhere herein are equally applicable to this embodiment.

[0086] Preferably, the ammonia precursor comprises urea.

[0087] In another aspect, the present invention provides the use of the system of the above aspect in a method according to the first aspect. Hence, all preferred features and embodiments applicable to the first aspect also apply to the system of the present invention, and vice versa.

[0088] In another aspect, the present invention provides a Fe-SCR catalyst for treating a NO containing 100 ppm or less from a lean-burn internal combustion engine. x The Fe-SCR catalyst comprises iron and zeolite, and the ANR is greater than 2 to 6. In an alternative aspect, NOx There are no particular limitations. Every preferred feature and embodiment that applies to other aspects also applies to this aspect of the invention.

[0089] The invention may also be defined in accordance with one or more of the following claims.

[0090] 1. A method for treating exhaust gas from a lean-burn internal combustion engine, the method comprising: introducing ammonia or an ammonia precursor into the exhaust gas upstream of an Fe-SCR catalyst, the Fe-SCR catalyst comprising iron and a zeolite; and contacting the exhaust gas with the Fe-SCR catalyst; wherein the amount of ammonia or an ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide a ratio of ammonia to NO greater than 2 to 6 in the exhaust gas contacting the Fe-SCR catalyst. x Molar ratio (ANR).

[0091] 2. The method according to 1, wherein the amount of ammonia or an ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR of 3 to 5 in the exhaust gas contacting the Fe-SCR catalyst.

[0092] 3. The method according to 1 or 2, wherein NO in the exhaust gas contacting the Fe-SCR catalyst x The concentration is 100 ppm or less.

[0093] 4. The method according to 3, wherein the NO in the exhaust gas contacting the Fe-SCR catalyst x The concentration is 50 ppm or less, preferably 10 ppm or less.

[0094] 5. The method according to any one of 1 to 4, wherein the concentration of NO in the exhaust gas contacting the Fe-SCR catalyst is x The ratio of the concentration is 0.8 or greater.

[0095] 6. The method according to 5, wherein the concentration of NO in the exhaust gas contacting the Fe-SCR catalyst is x The ratio of the concentration is 0.9 or greater.

[0096] 7. The method according to any one of 1 to 6, wherein the method further comprises reducing NO in the exhaust gas before the step of introducing ammonia or an ammonia precursor into the exhaust gas. x concentration.

[0097] 8. The method according to 7, wherein the exhaust gas from the lean-burn internal combustion engine contains NO x The concentration of NO in the exhaust gas is greater than 100 ppm and the step of introducing ammonia or an ammonia precursor into the exhaust gas is preceded by the step of reducing the NO in the exhaust gas x The concentration of NO in the exhaust gas willx The concentration of is reduced to 100 ppm or less, preferably 50 ppm or less, more preferably 10 ppm or less.

[0098] 9. The method according to item 7 or 8, wherein the step of reducing NO in the exhaust gas is performed before the step of introducing ammonia or an ammonia precursor into the exhaust gas. x The concentration includes mixing the exhaust gas with another SCR catalyst, oxidation catalyst and / or passive NO x Adsorbent (PNA) catalyst contact.

[0099] 10. The method according to 9, wherein the PNA catalyst comprises a platinum group metal (PGM), preferably Pd, disposed on a small pore zeolite, the small pore zeolite preferably having a framework type including CHA and / or AEI.

[0100] 11. The method according to any one of 1 to 10, wherein the lean-burn internal combustion engine is not a gasoline engine.

[0101] 12. The method according to any one of 1 to 11, wherein the lean-burn internal combustion engine is a diesel engine, a hydrogen engine, or an engine powered by liquid petroleum gas or natural gas.

[0102] 13. The method according to any one of 1 to 12, wherein the temperature of the exhaust gas contacting the Fe-SCR catalyst is 500°C or less.

[0103] 14. The method according to 13, wherein the temperature of the exhaust gas contacting the Fe-SCR catalyst is 350°C or lower, preferably 300°C or lower, and more preferably 200°C or lower.

[0104] 15. A method according to any one of 1 to 12, wherein: when the temperature of the exhaust gas contacting the Fe-SCR catalyst is at a predetermined threshold temperature or lower, the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR greater than 2 to 6 in the exhaust gas contacting the Fe-SCR catalyst; and when the temperature of the exhaust gas contacting the Fe-SCR catalyst is greater than the threshold temperature, the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR of 2 or less in the exhaust gas contacting the Fe-SCR catalyst.

[0105] 16. The method according to 15, wherein: when the temperature of the exhaust gas contacting the Fe-SCR catalyst is at a predetermined threshold temperature or lower, the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR of 3 to 5 in the exhaust gas contacting the Fe-SCR catalyst.

[0106] 17. The method according to 15 or 16, wherein the threshold temperature is 500°C.

[0107] 18. The method according to 17, wherein the threshold temperature is 350°C, preferably 300°C, more preferably 200°C.

[0108] 19. The method according to any one of 1 to 18, wherein the zeolite of the Fe-SCR catalyst comprises a zeolite having a framework type selected from the group consisting of: AEI, AFX, BEA, FER, MFI, FAU, LTA, LTL, CHA, or one or more of their mixtures or inter-products.

[0109] 20. The method according to any one of 1 to 19, wherein the zeolite of the Fe-SCR catalyst comprises a medium-pore zeolite and / or a large-pore zeolite.

[0110] 21. The method according to 19 or 20, wherein the zeolite of the Fe-SCR catalyst comprises a zeolite having a framework type comprising: AEI, AFX, BEA and / or FER, preferably BEA.

[0111] 22. The method according to 21, wherein the zeolite of the Fe-SCR catalyst is beta zeolite.

[0112] 23. The method according to any one of 1 to 22, wherein the zeolite of the Fe-SCR catalyst has a silica to alumina molar ratio (SAR) of about 7 to about 50.

[0113] 24. The method according to 23, wherein the zeolite of the Fe-SCR catalyst has a SAR of about 10 to about 35, preferably about 20 to about 30, more preferably about 22 to about 28.

[0114] 25. The method according to 21, wherein the zeolite of the Fe-SCR catalyst has a SAR of about 25.

[0115] 26. The method according to any one of 1 to 25, wherein the zeolite of the Fe-SCR catalyst comprises iron placed on the zeolite at a loading of about 1 wt. % to about 7 wt. %, preferably about 2 wt. % to about 5 wt. %, based on the weight of the zeolite.

[0116] 27. The method according to any one of 1 to 26, wherein the Fe-SCR catalyst further comprises copper disposed on the zeolite.

[0117] 28. The method of any one of 1 to 27, wherein the Fe-SCR catalyst is contained within or disposed on a substrate, the substrate comprising two or more catalyst zones and the Fe-SCR catalyst is contained within a first catalyst zone.

[0118] 29. The method according to 28, wherein a Cu-SCR catalyst is contained in a second catalyst zone different from the first catalyst zone, the Cu-SCR catalyst comprising copper and zeolite.

[0119] 30. The method of claim 29, wherein the second catalyst zone is located upstream of the first catalyst zone.

[0120] 31. A method according to any one of 1 to 26, further comprising contacting the exhaust gas with a Cu-SCR catalyst before contacting the exhaust gas with the Fe-SCR catalyst, the Cu-SCR catalyst comprising copper and zeolite, wherein the Cu-SCR catalyst is located in a close coupling position upstream of the Fe-SCR catalyst.

[0121] 32. A method according to any one of 1 to 31, further comprising contacting the exhaust gas with a Cu-SCR catalyst downstream of the Fe-SCR catalyst, the Cu-SCR catalyst comprising copper and zeolite, wherein the Cu-SCR catalyst is located downstream of the Fe-SCR catalyst in an underfloor position.

[0122] 33. The method according to any one of 1 to 32, wherein the ammonia precursor comprises urea.

[0123] 34. A system for treating exhaust gas from a lean-burn internal combustion engine, the system comprising:

[0124] A reductant injector for introducing ammonia or an ammonia precursor into the exhaust gas; a substrate; an Fe-SCR catalyst contained in or disposed on the substrate, the Fe-SCR catalyst comprising iron and zeolite; and an engine control unit; wherein the reductant injector is located upstream of the Fe-SCR catalyst; and wherein the engine control unit is configured to control the amount of ammonia or an ammonia precursor introduced into the exhaust gas by the reductant injector during use, so that the ammonia in the exhaust gas contacting the Fe-SCR catalyst is mixed with NO x The molar ratio (ANR) is greater than 2 to 6.

[0125] 35. The system of claim 34, wherein the system further comprises the lean-burn internal combustion engine.

[0126] 36. A system according to claim 34 or 35, wherein the engine control unit is configured to control the amount of ammonia or ammonia precursor introduced into the exhaust gas through the reductant injector during use so that the ANR in the exhaust gas contacting the Fe-SCR catalyst is 3 to 6.

[0127] 37. A system according to any one of 34 to 36, wherein the system comprises an additional SCR catalyst, an oxidation catalyst and / or a PNA catalyst upstream of the Fe-SCR catalyst.

[0128] 38. A system according to any one of claims 34 to 37, wherein the lean-burn internal combustion engine is not a gasoline engine.

[0129] 39. A system according to any one of claims 34 to 38, wherein the lean-burn internal combustion engine is a diesel engine, a hydrogen engine, or an engine powered by liquid petroleum gas or natural gas.

[0130] 40. A system according to any one of claims 34 to 39, wherein the zeolite of the Fe-SCR catalyst comprises a zeolite having a framework type selected from the group consisting of: AEI, AFX, BEA, FER, MFI, FAU, LTA, LTL, CHA, or one or more of their mixtures or interbionts.

[0131] 41. The system according to any one of claims 34 to 40, wherein the zeolite of the Fe-SCR catalyst comprises a medium pore zeolite and / or a large pore zeolite.

[0132] 42. The system of claim 40 or 41, wherein the zeolite of the Fe-SCR catalyst comprises a zeolite having a framework type comprising AEI, AFX, BEA and / or FER, preferably BEA.

[0133] 43. The system of claim 42, wherein the zeolite of the Fe-SCR catalyst is beta zeolite.

[0134] 44. A system according to any one of claims 34 to 43, wherein the zeolite of the Fe-SCR catalyst has a silica to alumina molar ratio (SAR) of about 15 to about 50.

[0135] 45. The system of claim 44, wherein the zeolite of the Fe-SCR catalyst has a SAR of about 15 to about 35, preferably about 20 to about 30, and more preferably about 22 to about 28.

[0136] 46. ​​The system of claim 42, wherein the zeolite of the Fe-SCR catalyst has a SAR of about 25.

[0137] 47. A system according to any one of 34 to 46, wherein the zeolite of the Fe-SCR catalyst comprises iron placed on the zeolite at a loading of about 1 wt.% to about 7 wt.%, preferably about 2 wt.% to about 5 wt.%, based on the weight of the zeolite.

[0138] 48. The system of any one of claims 34 to 47, wherein the Fe-SCR catalyst further comprises copper disposed on the zeolite.

[0139] 49. The system of any one of claims 34 to 48, wherein the substrate comprises two or more catalyst zones, the Fe-SCR catalyst being contained within a first catalyst zone.

[0140] 50. The system of claim 49, wherein a Cu-SCR catalyst is contained in a second catalyst zone different from the first catalyst zone, the Cu-SCR catalyst comprising copper and zeolite.

[0141] 51. A system according to 50, wherein the second catalyst zone is located upstream of the first catalyst zone.

[0142] 52. The system of any one of claims 34 to 47, further comprising a Cu-SCR catalyst located in a close coupling position upstream of the Fe-SCR catalyst, the Cu-SCR catalyst comprising copper and zeolite.

[0143] 53. The system of any one of claims 34 to 53, further comprising a Cu-SCR catalyst located downstream of the Fe-SCR catalyst in an underfloor location, the Cu-SCR catalyst comprising copper and zeolite.

[0144] 54. A system according to any one of 34 to 53, wherein the ammonia precursor comprises urea.

[0145] 55. Use of a system according to any one of claims 34 to 54 in a method according to any one of claims 1 to 33.

[0146] 56.Fe-SCR catalyst for treating NO containing 100 ppm or less from lean-burn internal combustion engines x The Fe-SCR catalyst comprises iron and zeolite, and the ANR is greater than 2 to 6.

[0147] The invention will now be described with reference to the following non-limiting examples.

[0148] Example

[0149] Example 1 - Preparation of fresh 3.0 wt% Fe / β zeolite catalyst and honeycomb single substrate coated therewith Methods

[0150] Commercially available H-form aluminosilicate beta zeolite was subjected to NH4 + Ion exchange followed by filtration. The resulting material is added to an aqueous solution of Fe(NO3)3 with stirring. The slurry is filtered, then washed and dried. This procedure can be repeated to achieve the desired metal loading. The final product is calcined.

[0151] A cordierite honeycomb (i.e., flow-through) cylindrical single substrate having dimensions of 4.66 inches in diameter and 3 inches in length and a wall thickness of 0.004 inches (4 mils) and a pore density of 400 cpsi (pores per square inch) was coated with a Fe / beta zeolite (silica to alumina ratio (SAR) of 25) catalyst by adding the catalyst to deionized water to produce a catalyst slurry that also contained 10 weight percent water-dispersible boehmite (as a binder) relative to the weight of the zeolite. The solids content of the slurry used to coat each substrate was 30%. The substrates were coated with the substrates using the method disclosed in EP 1064094B1. The resulting catalyst cores each had a 2.4 g / in 3 The entire substrate was first dried in flowing air at 105° C. and then calcined in a muffle furnace at 500° C. for 4 hours. The resulting catalyst was referred to as a “fresh” catalyst.

[0152] The "fresh" catalyst coated substrate was hydrothermally aged at 700°C for a total of 10 hours in an oven in a furnace, wherein the furnace temperature was increased from room temperature and pressure at a "ramp rate" of 10°C / min until a temperature of 700°C was reached. The 10 hour residence time did not start until 700°C was reached. A continuously replenished 10 volume % O2 / 10% H2O / N2 balanced gas mixture controlled by mass flow and liquid flow controllers, respectively, was pumped into the oven at a flow rate of 6 liters / min. The honeycomb substrate cores were arranged in the oven so that the channels extended vertically and the flowing gas mixture was forced from the lower end of the oven into the channels of the individual cores placed in the oven.

[0153] Sample cores 1 inch in diameter and 3 inches in length were cut from the aged catalyst coated flow-through substrate. The resulting cores were labeled "Catalyst A".

[0154] Comparative Example 2 - Method for preparing fresh Cu / zeolite catalyst and honeycomb single substrate coated therewith

[0155] A commercially available H-form aluminosilicate AEI (SSZ-39) zeolite (SAR 20) was subjected to NH4NO3 solution. + Ion exchange followed by filtration. The resulting material is added to an aqueous solution of copper acetate with stirring. The slurry is filtered and then washed and dried. This procedure can be repeated to achieve the desired copper metal loading of 3.0 wt%. The final product is calcined.

[0156] Similarly, a commercially available aluminosilicate CHA zeolite in H form (SAR 23) was subjected to NH4 + Ion exchange followed by filtration. The resulting material is added to an aqueous solution of copper acetate with stirring. The slurry is filtered and then washed and dried. This procedure can be repeated to achieve the desired copper metal loading of 2.0 wt%. The final product is calcined.

[0157] The Cu / AEI and Cu / CHA zeolite catalysts thus prepared were each coated on a separate bare cordierite honeycomb (i.e., flow-through) cylindrical single substrate identical to the Fe / BEA zeolite catalyst used in Example 1, and both coated substrates were aged in the same manner as the substrates coated with the Fe / BEA zeolite; and cores of the same size were cut from each aged substrate for testing. The comparative Cu / AEI zeolite catalyst was labeled "Catalyst B"; and the comparative Cu / CHA zeolite catalyst was labeled "Catalyst C".

[0158] Example 3-NO x Conversion rate evaluation

[0159] The NO content of the catalyst cores prepared in Example 1 and Comparative Example 2 was evaluated. x Conversion Activity. All aged cores were tested in a laboratory Selective Catalytic Activity Test (SCAT) apparatus using the following gas mixture including an ammonia reductant: 75 ppm NO, "X" ppm NH3 (depending on the ammonia and NO to be used) x Ratio (ANR) (see Tables 1 and 2 below)), 10% O2, 8% CO2, 5% H2O, N2 balance.

[0160] NO under various ANR at 175℃ and 300℃ x The results of the transformation are listed in Tables 1 and 2 below.

[0161] Table 1

[0162]

[0163] Table 2

[0164]

[0165] From the results shown in Tables 1 and 2, it can be seen that at a low temperature of 175°C, surprisingly, the NO x The conversion rate was significantly improved over the two comparative Cu / zeolite samples. At the higher reaction temperature of 300 °C, the NO conversion of Fe / BEA aluminosilicate zeolite catalyst wasx Conversion rates also improved at higher ANRs.

[0166] ****************************

[0167] The foregoing detailed description has been provided by way of explanation and illustration and is not intended to limit the scope of the appended claims. Many variations of the presently preferred embodiments shown herein will be apparent to those of ordinary skill in the art and remain within the scope of the appended claims and their equivalents.

[0168] For the avoidance of any doubt, any and all documents cited herein are hereby incorporated by reference into this application in their entirety.

Claims

1. A method of treating exhaust gas from a lean-burn internal combustion engine, the method comprising: introducing ammonia or an ammonia precursor into the exhaust gas upstream of a Fe-SCR catalyst comprising iron and zeolite; as well as contacting the exhaust gas with the Fe-SCR catalyst; wherein the amount of ammonia or ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide a ratio of ammonia to NO greater than 2 to 6 in the exhaust gas contacting the Fe-SCR catalyst. x Molar ratio (ANR).

2. The method according to claim 1, wherein NO in the exhaust gas contacting the Fe-SCR catalyst x The concentration is 100 ppm or less.

3. The method according to claim 1 or 2, wherein the concentration of NO in the exhaust gas contacting the Fe-SCR catalyst is x The ratio of the concentration is 0.8 or greater.

4. A method according to claim 1, 2 or 3, wherein the lean-burn internal combustion engine is a diesel engine, a hydrogen engine or an engine powered by liquid petroleum gas or natural gas.

5. A method according to any preceding claim, wherein the temperature of the exhaust gas contacting the Fe-SCR catalyst is 500°C or less.

6. The method according to any one of claims 1 to 4, wherein: controlling an amount of ammonia or an ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst to provide an ANR of greater than 2 to 6 in the exhaust gas contacting the Fe-SCR catalyst when the temperature of the exhaust gas contacting the Fe-SCR catalyst is at a predetermined threshold temperature or less; and When the temperature of the exhaust gas contacting the Fe-SCR catalyst is greater than the threshold temperature, the amount of ammonia or an ammonia precursor introduced into the exhaust gas upstream of the Fe-SCR catalyst is controlled to provide an ANR of 2 or less in the exhaust gas contacting the Fe-SCR catalyst.

7. A method according to any preceding claim, wherein the zeolite of the Fe-SCR catalyst comprises a zeolite having a framework type selected from the group consisting of: AEI, AFX, BEA, FER, MFI, FAU, LTA, LTL, CHA or one or more of their mixtures or inter-products, preferably AEI, AFX, BEA and / or FER, most preferably BEA.

8. The method of any preceding claim, wherein the zeolite of the Fe-SCR catalyst has a silica to alumina molar ratio (SAR) of about 7 to about 50.

9. The method of any preceding claim, wherein the zeolite of the Fe-SCR catalyst comprises iron disposed on the zeolite at a loading of about 1 wt% to about 7 wt%, preferably about 2 wt% to about 5 wt%, based on the weight of the zeolite.

10. The method of any preceding claim, wherein the Fe-SCR catalyst further comprises copper disposed on the zeolite.

11. A method according to any preceding claim, wherein the Fe-SCR catalyst is contained within or disposed on a substrate, the substrate comprising two or more catalyst zones and the Fe-SCR catalyst is contained within a first catalyst zone. 12 . The method of claim 11 , wherein a Cu-SCR catalyst is contained in a second catalyst zone different from the first catalyst zone, the Cu-SCR catalyst comprising copper and zeolite.

13. The method of claim 12, wherein the second catalyst zone is located upstream of the first catalyst zone.

14. A system for treating exhaust gas from a lean-burn internal combustion engine, the system comprising: a reductant injector for introducing ammonia or an ammonia precursor into the exhaust gas; substrate; an Fe-SCR catalyst contained within or disposed on the substrate, the Fe-SCR catalyst comprising iron and zeolite; and Engine control unit; wherein the reductant injector is located upstream of the Fe-SCR catalyst; and wherein the engine control unit is configured to control the amount of ammonia or ammonia precursor introduced into the exhaust gas via the reductant injector during use so that the ammonia in the exhaust gas contacting the Fe-SCR catalyst is reacted with NO x The molar ratio (ANR) is greater than 2 to 6.

15. Use of a system according to claim 14 in a method according to any one of claims 1 to 13.

16. Fe-SCR catalyst is used to treat NO containing 100 ppm or less from lean-burn internal combustion engines x The Fe-SCR catalyst comprises iron and zeolite, and the ANR is greater than 2 to 6.